Wafer cutting method, device and computer readable storage medium

By using two cutting knives during wafer cutting, forming cut marks and adjusting positions, the cutting offset and back collapse caused by the blade cutting method is solved, and the cutting accuracy and quality are improved.

CN118752623BActive Publication Date: 2024-11-15VERIZON UNITED SEMICON (TEXAS) CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411237926.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-11-15
Estimated Expiration
2044-09-05

AI Technical Summary

Technical Problem

During the wafer cutting process, the blade cutting method can easily lead to cutting offset and wafer back collapse or cracking, affecting cutting accuracy and quality.

Method used

Two cutting knives are used to cut separately. The first cutting knives form cut marks and adjust the position of the second cutting knives to ensure the accuracy of cutting, and avoid back collapse or cracks through the deviation detection of the cutting knives.

Benefits of technology

Improves the accuracy of wafer cutting, avoids deviation and back collapse or cracking during cutting, and ensures wafer integrity and quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118752623B_ABST
    Figure CN118752623B_ABST
Patent Text Reader

Abstract

The present invention discloses a wafer cutting method, equipment and computer-readable storage medium. The wafer cutting method includes: determining the positions of non-metallic cutting paths and multiple metal cutting paths in each mask area; determining that the cutting paths included in the current mask area are non-metallic cutting paths, and cutting the non-metallic cutting paths; cutting the non-metallic cutting paths for the first time along the non-metallic cutting paths by a second cutting knife to form a first cut mark; determining the position of the first cut mark; adjusting the position of the second cutting knife when the first cut mark deviates from the center line of the non-metallic cutting paths; cutting the non-metallic cutting paths for the second time by the first cutting knife to a preset depth to form a groove; cutting the non-metallic cutting paths for the third time by the adjusted second cutting knife to penetrate the non-metallic cutting paths. The present invention can improve the offset during cutting, improve the accuracy of cutting, and avoid back collapse or cracking of the wafer during cutting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a wafer cutting method, equipment and computer-readable storage medium. Background Art

[0002] In the wafer preparation process, cutting is the process of dividing the entire chip into single grains of the required size after basic processes such as lithography, coating, and thinning. It is an indispensable post-process in the preparation process. The most widely used cutting method in the industry is blade cutting. Blade cutting is a process in which a high-speed rotating spindle drives the blade installed on it to completely cut the chip into single grains according to a set program. During the cutting process, the cut marks of the blade will shift as the cutting time continues, and it is easy to cause back collapse or cracking when cutting the wafer. Summary of the invention

[0003] The present invention provides a wafer cutting method, a device and a computer-readable storage medium, which can improve the deviation during cutting, improve the cutting accuracy and avoid the wafer from back-breaking or cracking during cutting.

[0004] According to one aspect of the present invention, there is provided a wafer cutting method, comprising:

[0005] Determine a preset cutting image of the wafer; the wafer includes a plurality of mask areas, and the preset cutting image of each mask area is the same;

[0006] According to the preset cutting image of the wafer, the wafer is divided into a plurality of cutting lanes; each mask area also includes a plurality of cutting lanes; the plurality of cutting lanes include metal cutting lanes and non-metal cutting lanes;

[0007] Determine the positions of the non-metallic cutting lanes and the plurality of metal cutting lanes in the current mask area;

[0008] Determine the positions of the non-metallic cutting paths and the plurality of metal cutting paths in each mask area according to the positions of the non-metallic cutting paths and the plurality of metal cutting paths in the current mask area;

[0009] Cutting multiple cutting paths; determining that the cutting paths included in the current mask area are non-metallic cutting paths, and cutting the non-metallic cutting paths; wherein the cutting of the non-metallic cutting paths includes: cutting the non-metallic cutting paths for the first time along the non-metallic cutting paths by a second cutting knife to form a first cut mark; determining the position of the first cut mark; adjusting the position of the second cutting knife when the first cut mark deviates from the center line of the non-metallic cutting paths; cutting the non-metallic cutting paths for the second time by the first cutting knife to a preset depth to form a groove; cutting the non-metallic cutting paths for the third time by the adjusted second cutting knife to penetrate the non-metallic cutting paths.

[0010] Optionally, after determining the position of the first cut, the method further includes:

[0011] When the first cut is located at the center line of the non-metallic cutting path, the non-metallic cutting path is cut a second time by the first cutting knife to a preset depth to form a groove; the non-metallic cutting path is cut a third time by the second cutting knife to penetrate the non-metallic cutting path.

[0012] Optionally, the position of the metal cutting line and the position of the non-metal cutting line in each mask area are the same.

[0013] Optionally, determining the positions of the non-metallic cutting paths and the plurality of metal cutting paths in each mask area according to the positions of the non-metallic cutting paths and the plurality of metal cutting paths in the current mask area includes:

[0014] Determine the spacing between the non-metallic cutting paths in the current mask area and the adjacent next mask area according to the position of the non-metallic cutting paths in the current mask area;

[0015] Determine the position of the non-metallic cutting path of each mask area according to the spacing between the non-metallic cutting path of the current mask area and the adjacent next mask area;

[0016] The position of the metal cutting line in each mask area is determined according to the position of the non-metal cutting line in each mask area.

[0017] Optionally, cutting multiple cutting lanes also includes:

[0018] It is determined that the cutting paths included in the current mask area are metal cutting paths, and the metal cutting paths are cut.

[0019] Optionally, determining that the cutting path included in the current mask area is a metal cutting path, and cutting the metal cutting path includes:

[0020] A first cutting knife is used to perform a first cutting on the metal cutting path along the metal cutting path to form a groove by cutting to a preset depth;

[0021] The metal cutting path is cut for the second time by the second cutting knife, penetrating the metal cutting path.

[0022] Optionally, determining the positions of the metal cutting paths and the non-metal cutting paths in the current mask area includes:

[0023] The positions of the metal cutting lines and non-metal cutting lines in the current mask area are determined by a microscope or visual inspection equipment.

[0024] Optionally, the plurality of cutting paths include a plurality of first cutting paths and a plurality of second cutting paths; each first cutting path extends along a first direction, and the plurality of first cutting paths are arranged along a second direction; each second cutting path extends along a second direction, and the plurality of second cutting paths are arranged along the first direction; the first direction and the second direction are perpendicular to each other; the first cutting paths and the second cutting paths both include metal cutting paths and non-metal cutting paths;

[0025] Cut multiple lanes, including:

[0026] cutting a plurality of first cutting paths;

[0027] After the cutting of the plurality of first cutting streets is completed, the plurality of second cutting streets are cut.

[0028] According to another aspect of the present invention, there is provided a wafer cutting device, the wafer cutting device comprising:

[0029] at least one processor; and a memory in communication with the at least one processor; wherein,

[0030] The memory stores a computer program that can be executed by at least one processor. The computer program is executed by at least one processor so that the at least one processor can execute the wafer cutting method described in any embodiment of the present invention.

[0031] According to another aspect of the present invention, a computer-readable storage medium is provided, wherein the computer-readable storage medium stores computer instructions, and the computer instructions are used to implement the wafer cutting method described in any embodiment of the present invention when executed by a processor.

[0032] The wafer cutting method provided by the technical solution of the embodiment of the present invention includes: along the non-metallic cutting path, a second cutting knife is used to perform a first cutting on the non-metallic cutting path to form a first cut mark; the position of the first cut mark is determined; when the first cut mark deviates from the center line of the non-metallic cutting path, the position of the second cutting knife is adjusted; the non-metallic cutting path is cut for a second time by the first cutting knife to form a groove by cutting to a preset depth; the non-metallic cutting path is cut for a third time by the adjusted second cutting knife to penetrate the non-metallic cutting path. The embodiment of the present invention uses the first cutting knife and the second cutting knife for cutting, which can avoid back collapse or cracks when the same cutting knife is used to cut the wafer. At the same time, when cutting the non-metallic cutting path, the position of the first cut mark produced by the second cutting knife is first determined, and then cutting is performed, which can avoid the second cutting knife from being offset, improve the cutting accuracy, and also avoid back collapse or cracks when the wafer is cut.

[0033] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0035] Figure 1 It is a flow chart of a wafer cutting method provided by an embodiment of the present invention.

[0036] Figure 2 It is a schematic diagram of a photomask area for forming a wafer provided by an embodiment of the present invention.

[0037] Figure 3 It is a schematic diagram of a mask area of ​​a wafer provided by an embodiment of the present invention.

[0038] Figure 4 It is a schematic diagram of a mask area of ​​another wafer provided by an embodiment of the present invention.

[0039] Figure 5 It is a schematic diagram of a cut provided by an embodiment of the present invention.

[0040] Figure 6 yes Figure 1 A detailed flow chart included in S140.

[0041] Figure 7 It is a schematic diagram of a mask area of ​​another wafer provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0042] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0043] It should be noted that the terms "first", "second", etc. in the present invention are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product, or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products, or devices.

[0044] The embodiment of the present invention provides a wafer cutting method. Figure 1 is a flow chart of a wafer cutting method provided by an embodiment of the present invention, with reference to Figure 1 , wafer dicing methods include:

[0045] S110, determining a preset cutting image of the wafer; the wafer includes a plurality of mask areas, and the preset cutting image of each mask area is the same.

[0046] in, Figure 2 is a schematic diagram of a photomask region for forming a wafer provided by an embodiment of the present invention, with reference to Figure 2 , set the preset cutting image of wafer 01 according to actual needs, and the preset cutting image can be the circuit pattern actually needed; place wafer 01 in the lithography machine, which includes a light source component, a mask platform module and a wafer platform module; the light source component is fixed in the lithography machine, so that the preset cutting image on the mask 05 can be completely projected onto various parts of wafer 01, the mask platform module carries the same mask 05 and moves back and forth, the wafer platform module accurately locates the position of wafer 01 and moves, ensuring that each mask area (block) in wafer 01 is the same, a layer of oxide film 02 will be covered on wafer 01 to protect wafer 01, a layer of photoresist 03 is covered on the oxide film 02, and a lens 04 is also provided on the side of the photoresist 03 away from wafer 01 to form the preset cutting image in wafer 01.

[0047] S120, dividing the wafer into a plurality of cutting lanes according to a preset cutting image of the wafer; each mask area also includes a plurality of cutting lanes; the plurality of cutting lanes include metal cutting lanes and non-metal cutting lanes.

[0048] In order to divide the wafer into single chips, the wafer needs to be divided into multiple cutting lanes according to the preset cutting image of the wafer. Each cutting lane needs to be cut, so the number of cuts in each mask area is the same, so that each chip inside the wafer is the same. Figure 3is a schematic diagram of a mask area of ​​a wafer provided by an embodiment of the present invention, with reference to Figure 3 , Figure 3 The left picture in the figure shows nine mask areas of the wafer, namely Block 1 to Block 9. The mask area in the center is Block 5. Figure 3 The right picture in the figure is a partial enlarged picture of Block 5. In Block 5, multiple cutting paths 10 are included. The multiple cutting paths may include multiple first cutting paths 11 extending along the first direction X and multiple second cutting paths 12 extending along the second direction Y. Since the wafer includes a stacked silicon layer and a metal layer, the metal layer covers part of the silicon layer, and the first cutting paths 11 and the second cutting paths 12 both include metal cutting paths and non-metal cutting paths. Figure 3 The right picture in the figure shows the metal cutting path and non-metal cutting path by example. The cutting path in the red frame is the metal cutting path, which is the cutting path with a metal layer covering the silicon layer; the cutting path in the blue frame is the non-metal cutting path, which is the cutting path without a metal layer covering the silicon layer. The positions of the metal cutting path and the non-metal cutting path in each mask area are the same.

[0049] S130, determining the positions of the non-metal cutting lanes and the plurality of metal cutting lanes in the current mask area.

[0050] The current mask area may be any cut mask area in the wafer, and the positions of the non-metallic cutting paths and the plurality of metal cutting paths in the current mask area may be determined by a microscope or a visual inspection device.

[0051] S140, determining the positions of the non-metallic cutting lines and the plurality of metal cutting lines in each mask area according to the positions of the non-metallic cutting lines and the plurality of metal cutting lines in the current mask area.

[0052] Among them, each mask area can include one non-metallic cutting line and multiple metal cutting lines. The positions of the non-metallic cutting lines and the multiple metal cutting lines in each mask area are the same. According to the position of the non-metallic cutting line in the current mask area, the distance between the non-metallic cutting line of the current mask area and the next adjacent mask area can be determined; according to the distance between the non-metallic cutting line of the current mask area and the next adjacent mask area, the position of the non-metallic cutting line of each mask area is determined; according to the position of the non-metal in each mask area, the position of the metal cutting line of each mask area is determined.

[0053] S150, cutting multiple cutting paths; determining that the cutting paths included in the current mask area are non-metallic cutting paths, and cutting the non-metallic cutting paths; wherein the cutting of the non-metallic cutting paths includes: cutting the non-metallic cutting paths for the first time along the non-metallic cutting paths by a second cutting knife to form a first cut mark; determining the position of the first cut mark; adjusting the position of the second cutting knife when the first cut mark deviates from the center line of the non-metallic cutting paths; cutting the non-metallic cutting paths for the second time by the first cutting knife to a preset depth to form a groove; cutting the non-metallic cutting paths for the third time by the adjusted second cutting knife to penetrate the non-metallic cutting paths.

[0054] Among them, reference Figure 3 , the wafer can be cut in different directions, and all the first cutting streets 11 extending along the first direction X can be cut first, or all the second cutting streets 12 extending along the second direction Y can be cut first; Figure 4 is a schematic diagram of a mask area of ​​another wafer provided by an embodiment of the present invention, referring to Figure 4 , Figure 4 The left picture in the figure shows nine mask areas of the wafer, namely Block 1 to Block 9. The mask area in the center is Block 5. Figure 3 The right figure in the figure includes the cutting lane distribution diagram of Block 5. In Block 5, 14 cutting lanes may be included, of which the 12th cutting lane is a non-metallic cutting lane, and the rest are metallic cutting lanes.

[0055] Specifically, the embodiment of the present invention adopts two cutting knives for cutting, wherein the first cutting knife mainly grooves the cutting path to eliminate the metal layer in the cutting path, and the second cutting knife mainly cuts through the silicon layer of the wafer. The cutting width of the first cutting knife is greater than the cutting width of the second cutting knife. Since the second cutting knife performs a second cutting in the cut mark of the first cutting knife, it is impossible to determine whether the second cutting knife is offset. The present invention selects to check the position offset of the second cutting knife in the non-metallic cutting path, which can prevent the second cutting knife from touching the metal layer in the metal cutting path during the first cutting. If the metal layer adheres to the second cutting knife, it will cause back collapse of the wafer or cracks due to back collapse. Therefore, the embodiment of the present invention detects whether the second cutting knife is offset while cutting the non-metallic cutting path. Specifically, the second cutting knife first cuts the non-metallic cutting path for a distance to form a first cut mark; the position of the first cut mark is determined by a visual inspection device. Figure 5 is a schematic diagram of a cut provided by an embodiment of the present invention, with reference to Figure 5, the cut mark 20 should be located on the center line of the cutting path. If the first cut mark offsets the center line of the non-metallic cutting path, the position of the second cutting knife can be directly adjusted; then the non-metallic cutting path is cut for the second time by the first cutting knife, and cut to a preset depth to form a groove. The first cutting knife is mainly used for grooving; after the first cutting knife completes the cutting, the visual inspection equipment can be used to detect whether the position of the first cutting knife is offset. If no offset occurs, continue cutting. If offset occurs, the position of the first cutting knife needs to be adjusted; the non-metallic cutting path is cut for the third time by the adjusted second cutting knife. The second cutting knife can cut the silicon layer of the wafer and penetrate the non-metallic cutting path. The cutting is performed by the adjusted second cutting knife. Therefore, the present invention can avoid the offset of the second cutting knife, improve the cutting accuracy, and also avoid the back collapse or cracking of the wafer during cutting.

[0056] The wafer cutting method provided by the technical solution of the embodiment of the present invention includes: along the non-metallic cutting path, a second cutting knife performs a first cutting on the non-metallic cutting path to form a first cut mark; determines the position of the first cut mark; when the first cut mark deviates from the center line of the non-metallic cutting path, adjusts the position of the second cutting knife; performs a second cutting on the non-metallic cutting path by the first cutting knife to form a groove by cutting to a preset depth; performs a third cutting on the non-metallic cutting path by the adjusted second cutting knife to penetrate the non-metallic cutting path. The embodiment of the present invention can avoid the deviation of the second cutting knife by first determining the position of the first cut mark produced by the second cutting knife when cutting the non-metallic cutting path, and then performs cutting, thereby improving the cutting accuracy, and also avoiding the back collapse or cracking of the wafer during cutting.

[0057] Optionally, after determining the position of the first cut, it also includes: when the first cut is located at the center line of the non-metallic cutting line, cutting the non-metallic cutting line for a second time by the first cutting knife, cutting to a preset depth to form a groove; cutting the non-metallic cutting line for a third time by the second cutting knife, penetrating the non-metallic cutting line.

[0058] Among them, when detecting whether the second cutting knife is offset, if the first cut mark produced by the second cutting knife is located at the center line of the non-metallic cutting path, there is no need to adjust the position of the second cutting knife, and the groove is directly formed by cutting through the first cutting knife; the second cutting knife penetrates the non-metallic cutting path to complete the cutting of the non-metallic cutting path.

[0059] Optionally, the position of the metal cutting line and the position of the non-metal cutting line in each mask area are the same.

[0060] Since the preset cutting patterns of each mask area are the same, each mask area includes the same cutting paths, so the positions of the metal cutting paths and the non-metal cutting paths in each mask area are the same, thereby cutting to form single chips with the same performance.

[0061] Optional, Figure 6 yes Figure 1 A detailed flow chart included in S140, refer to Figure 6 S140, determining the positions of the non-metallic cutting paths and the plurality of metal cutting paths in each mask area according to the positions of the non-metallic cutting paths and the plurality of metal cutting paths in the current mask area, including:

[0062] S141. Determine the spacing between the non-metallic cutting lines in the current mask area and the adjacent next mask area according to the position of the non-metallic cutting lines in the current mask area.

[0063] Among them, the position of the non-metallic cutting path in the current mask area can be determined by a microscope or a visual inspection device. Since the distance between adjacent mask areas in the same direction is the same, the spacing between the non-metallic cutting paths of the current mask area and the next adjacent mask area is the sum of the distance between the adjacent mask areas and the size of the mask area in the same direction. For example, reference Figure 4 In the second direction Y, each mask area includes 14 cutting lanes, the 12th cutting lane is a non-metallic cutting lane, and the rest are metal cutting lanes. The distance between adjacent mask areas is zero, so the spacing between the non-metallic cutting lane of the next mask area and the cutting lane of the current mask area is 14 cutting lanes. Therefore, the first detection is performed at the 12th cutting lane, and the second cutting knife is detected every 14 cutting lanes to see if it is offset.

[0064] S142, determining the position of the non-metallic cutting line of each mask area according to the distance between the non-metallic cutting line of the current mask area and the adjacent next mask area.

[0065] Among them, exemplary, reference Figure 4 , in the second direction Y, the spacing between the non-metallic cutting road of the next mask area and the cutting road of the current mask area is 14 cutting roads. Therefore, in the second direction, the spacing between the non-metallic cutting roads in adjacent mask areas is 14 cutting road spacings, so that the position of the non-metallic cutting road of each mask area can be determined. It can be set by the knife mark self-reading detection (kerf check) in the wafer cutting equipment. After determining the position of the non-metallic cutting road of each mask area, it can be set to detect whether the position of the second cutting knife is offset in the non-metallic cutting road of each mask area. For example, the second cutting knife can be set to detect in the number of cutting roads in the mask area, and then detect every certain number of cutting roads.

[0066] S143, determining the position of the metal cutting line in each mask area according to the position of the non-metal cutting line in each mask area.

[0067] Among them, the position of the non-metal cutting line of each mask area is determined, and the rest are the positions of the metal cutting lines. Similarly, the first direction X can also be determined according to this method.

[0068] Optionally, S150, cutting the plurality of cutting paths, further includes: determining that the cutting paths included in the current mask area are metal cutting paths, and cutting the metal cutting paths.

[0069] Among them, exemplary, reference Figure 4 , along the second direction Y, there are multiple cutting lanes, the 12th cutting lane is a non-metallic cutting lane, and the 1-11, 13, and 14 are all metal cutting lanes. The cutting lanes are cut in sequence according to the order of the 1-14, and it is determined that the cutting lanes included in the current mask area are metal cutting lanes, and the metal cutting lanes are cut.

[0070] Optionally, it is determined that the cutting path included in the current mask area is a metal cutting path, and the metal cutting path is cut, including: along the metal cutting path, the metal cutting path is cut for the first time by a first cutting knife, cutting to a preset depth to form a groove; and the metal cutting path is cut for the second time by a second cutting knife, penetrating the metal cutting path.

[0071] Among them, when cutting the metal cutting path, the first cutting knife can be used to cut the metal cutting path for the first time, cutting to a preset depth to form a groove, the preset depth is mainly the depth that can eliminate the metal layer in the metal cutting path, after the first cutting knife is finished cutting, the visual inspection equipment can be used to detect whether the position of the first cutting knife is offset, if not, continue cutting, if offset, it is necessary to adjust the position of the first cutting knife; the second cutting knife is used to cut the metal cutting path for the second time, the second cutting knife mainly cuts the silicon layer of the wafer, the second cutting knife cuts inside the groove formed by the first cutting knife, and penetrates the metal cutting path. The embodiment of the present invention uses two cutting knives for cutting, which can avoid back collapse or cracks when cutting the wafer.

[0072] Optionally, determining the positions of the metal cutting paths and the non-metal cutting paths in the current mask area includes:

[0073] The positions of the metal cutting lines and non-metal cutting lines in the current mask area are determined by a microscope or visual inspection equipment.

[0074] Optionally, the plurality of cutting paths include a plurality of first cutting paths and a plurality of second cutting paths; each first cutting path extends along a first direction, and the plurality of first cutting paths are arranged along a second direction; each second cutting path extends along a second direction, and the plurality of second cutting paths are arranged along the first direction; the first direction and the second direction are perpendicular to each other; the first cutting paths and the second cutting paths both include metal cutting paths and non-metal cutting paths;

[0075] Cutting the plurality of cutting paths includes: cutting the plurality of first cutting paths; and after the cutting of the plurality of first cutting paths is completed, cutting the plurality of second cutting paths.

[0076] Among them, reference Figure 3 and Figure 4 The plurality of cutting lanes include a plurality of first cutting lanes 11 and a plurality of second cutting lanes 12. Each first cutting lane 11 extends along a first direction X, and each second cutting lane 12 extends along a second direction Y. The wafer can be cut in different directions. All the first cutting lanes 11 extending along the first direction X are cut first, and then all the second cutting lanes 12 are cut. Alternatively, all the second cutting lanes 12 extending along the second direction Y are cut first, and then all the first cutting lanes 11 are cut. Figure 7 is a schematic diagram of a mask area of ​​another wafer provided by an embodiment of the present invention, referring to Figure 7 In the first direction X, each mask area includes 16 cutting lanes, the 6th cutting lane is a non-metallic cutting lane, and the rest are metal cutting lanes. The distance between adjacent mask areas is zero, so the spacing between the non-metallic cutting lane of the next mask area and the cutting lane of the current mask area is 16 cutting lanes. Therefore, the first detection is set at the position of the 6th cutting lane, and the second cutting knife is detected every 16 cutting lanes to see if it is offset.

[0077] An embodiment of the present invention provides a wafer cutting device based on the above embodiment, and the wafer cutting device includes: at least one processor; and a memory communicatively connected to the at least one processor; wherein the memory stores a computer program executable by the at least one processor, and the computer program is executed by the at least one processor so that the at least one processor can execute the wafer cutting method described in any embodiment of the present invention.

[0078] The wafer cutting device provided by the embodiment of the present invention has the same beneficial effects as the wafer cutting method described in any embodiment of the present invention.

[0079] An embodiment of the present invention provides a computer-readable storage medium based on the above embodiments. The computer-readable storage medium stores computer instructions. The computer instructions are used to enable a processor to implement the wafer cutting method described in any embodiment of the present invention when executed.

[0080] The computer-readable storage medium provided by the embodiment of the present invention has the same beneficial effects as the wafer cutting method described in any embodiment of the present invention.

[0081] It should be understood that the various forms of processes shown above can be used to reorder, add or delete steps. For example, the steps described in the present invention can be executed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.

[0082] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A wafer cutting method, characterized in that: include: Determine a preset cutting image of the wafer; The wafer includes a plurality of mask areas, and the preset cutting images of each mask area are the same; According to the preset cutting image of the wafer, the wafer is divided into a plurality of cutting lanes; each mask area also includes a plurality of cutting lanes; the plurality of cutting lanes include metal cutting lanes and non-metal cutting lanes; Determine the positions of the non-metallic cutting lanes and the plurality of metal cutting lanes in the current mask area; Determine the positions of the non-metallic cutting paths and the plurality of metal cutting paths in each mask area according to the positions of the non-metallic cutting paths and the plurality of metal cutting paths in the current mask area; Cutting multiple cutting lanes; Determine that the cutting path included in the current mask area is a non-metallic cutting path, and cut the non-metallic cutting path; wherein, cutting the non-metallic cutting path includes: cutting the non-metallic cutting path for the first time along the non-metallic cutting path by a second cutting knife to form a first cut mark; determining the position of the first cut mark; adjusting the position of the second cutting knife when the first cut mark offsets the center line of the non-metallic cutting path; cutting the non-metallic cutting path for the second time by the first cutting knife to a preset depth to form a groove; cutting the non-metallic cutting path for the third time by the adjusted second cutting knife to penetrate the non-metallic cutting path.

2. The wafer cutting method according to claim 1, characterized in that: After determining the location of the first cut, it also includes: When the first cut mark is located at the center line of the non-metallic cutting road, the non-metallic cutting road is cut for the second time by the first cutting knife to a preset depth to form a groove; the non-metallic cutting road is cut for the third time by the second cutting knife to penetrate the non-metallic cutting road.

3. The wafer cutting method according to claim 1, characterized in that: The positions of the metal cutting lines and the non-metal cutting lines in each of the mask areas are the same.

4. The wafer cutting method according to claim 3, characterized in that: According to the positions of the non-metallic cutting paths and the plurality of metal cutting paths in the current mask area, the positions of the non-metallic cutting paths and the plurality of metal cutting paths in each mask area are determined, including: Determine the spacing between the non-metallic cutting lines in the current mask area and the adjacent next mask area according to the position of the non-metallic cutting lines in the current mask area; Determine the position of the non-metallic cutting path of each mask area according to the spacing between the non-metallic cutting path of the current mask area and the adjacent next mask area; The position of the metal cutting line in each mask area is determined according to the position of the non-metal cutting line in each mask area.

5. The wafer cutting method according to claim 1, characterized in that: Cutting multiple cutting lanes also includes: It is determined that the cutting paths included in the current mask area are metal cutting paths, and the metal cutting paths are cut.

6. The wafer cutting method according to claim 5, characterized in that: Determining that a cutting path included in the current mask area is a metal cutting path, and cutting the metal cutting path, including: Performing a first cutting on the metal cutting path along the metal cutting path by a first cutting knife, cutting the metal cutting path to a preset depth to form a groove; The metal cutting path is cut for the second time by a second cutting knife, penetrating the metal cutting path.

7. The wafer cutting method according to claim 1, characterized in that: Determine the location of metal cutting lines and non-metal cutting lines in the current mask area, including: The positions of the metal cutting lines and non-metal cutting lines in the current mask area are determined by a microscope or visual inspection equipment.

8. The wafer cutting method according to claim 1, characterized in that: The plurality of cutting paths include a plurality of first cutting paths and a plurality of second cutting paths; each of the first cutting paths extends along a first direction, and the plurality of first cutting paths are arranged along a second direction; each of the second cutting paths extends along the second direction, and the plurality of second cutting paths are arranged along the first direction; the first direction and the second direction are perpendicular to each other; the first cutting paths and the second cutting paths both include metal cutting paths and non-metal cutting paths; Cut multiple lanes, including: cutting a plurality of first cutting paths; After the cutting of the plurality of first cutting streets is completed, the plurality of second cutting streets are cut.

9. A wafer cutting device, characterized in that: The wafer cutting equipment comprises: at least one processor; and a memory in communication with the at least one processor; wherein, The memory stores a computer program executable by the at least one processor, and the computer program is executed by the at least one processor so that the at least one processor can perform the wafer cutting method according to any one of claims 1 to 8.

10. A computer-readable storage medium, characterized in that: The computer-readable storage medium stores computer instructions, and the computer instructions are used to enable a processor to implement the wafer cutting method according to any one of claims 1 to 8 when executed.

Citation Information

Patent Citations

  • Twice shear mark detection device and method, terminal and storage medium

    CN113989365A

  • Wafer splitting processing method, wafer processing equipment and storage medium

    CN115139419A

  • Wafer cutting method, scribing machine and storage medium

    CN116038527A

  • Wafer cutting method

    CN117727694A

  • Wafer processing method

    US20170186646A1