Electrochromic film material and preparation method thereof

Through new electrochromic film materials and preparation methods, the deficiencies of electrochromic technology in terms of adjustment ability, cost and adjustability are solved, the adjustment ability and stability of electrochromic windows are improved, and the cost of electrochromic displays is reduced. It reduces the power consumption of the screen and enhances the adjustability of electrochromic glasses, achieving more effective light adjustment and energy saving.

CN118755022AInactive Publication Date: 2024-10-11NALINWAY NANO TECHNOLOGY (SHANGHAI) CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411022259.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-11
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing electrochromic technology has deficiencies in adjustment capabilities, cost and adjustability, which affects its application in electrochromic windows, displays and glasses.

Method used

Adopting a new electrochromic film material and preparation method, including resin, monomer, cross-linking agent, initiator, spacer, electrochromic material, ion storage material and liquid electrolyte material, formed through screen printing and heat treatment Electrochromic film and assembled with conductive glass to ensure electrical contact and color changing effect.

Benefits of technology

Improves the adjustment ability and stability of electrochromic windows, reduces production costs, enhances the energy-saving effect of electrochromic displays and the adjustability and stability of electrochromic glasses, and achieves more effective light regulation and energy save.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118755022A_ABST
    Figure CN118755022A_ABST
Patent Text Reader

Abstract

The invention discloses an electrochromic film material which comprises the following components in parts by weight: 1-60 parts of resin; 0.01 to 50 parts by weight of a monomer; 0.01 to 50 parts by weight of a cross-linking agent; 0.1 to 0.01 part by weight of an initiator; and 0.1 to 0.01 part by weight of spacer. According to the electrochromic window, the electrochromic material and the structure are redesigned, the adjusting capacity and stability of the electrochromic window are improved, the irradiation intensity of light can be more effectively changed and indoor light and temperature can be adjusted when the electrochromic window is directly irradiated by strong light, and therefore energy consumed for heating, cooling and the like is reduced, and environmental pollution is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of electrochromic technology, and in particular to an electrochromic film material and a preparation method thereof. Background Art

[0002] Electrochromic technology is a technology that changes the color of a substance by applying voltage. This technology mainly changes the color of a substance by the transmission and absorption of light, thereby achieving control of light. Electrochromic technology has a wide range of applications in many fields, such as electrochromic windows, electrochromic displays, electrochromic glasses, etc. These applications are based on the unique properties of electrochromic technology, such as color adjustability and energy saving.

[0003] In the prior art: electrochromic technology is mainly used in the fields of electrochromic windows, electrochromic display screens and electrochromic glasses. Electrochromic windows can change the intensity of light radiation when strong light is directly shining through their own color and the switching effect of part of the infrared radiation, so as to adjust the indoor light and temperature, thereby reducing the energy consumed for heating, cooling, etc., and reducing the environmental pollution caused by this. The electrochromic display screen is a display screen prepared using electrochromic technology. Due to the memory effect of the electrochromic device, that is, once the color is changed, it can still maintain its color change state without an external power supply, so that no external voltage is required when displaying static images, thereby achieving the purpose of energy saving. Electrochromic glasses are based on electrochromic technology, breaking the light control of traditional products, and can change colors by changing the voltage anytime and anywhere, with greater adjustability.

[0004] Problems with existing technologies: Although existing electrochromic technologies have been widely used in certain fields, they still have some problems and shortcomings: Although electrochromic windows can adjust indoor light and temperature, in actual applications, their adjustment capabilities are limited and are greatly affected by environmental factors.

[0005] In addition, the production cost of electrochromic devices is high, which limits their large-scale application to a certain extent. Furthermore, although electrochromic displays do not require external voltage when displaying static images, they still require high power consumption when displaying dynamic images, which affects their energy-saving effect to a certain extent.

[0006] Although electrochromic glasses have great adjustability, in actual use, their adjustable range is limited and they are greatly affected by voltage stability.

[0007] Therefore, it is necessary to improve the traditional electrochromic film materials and the preparation methods thereof so as to avoid the above-mentioned problems. Summary of the invention

[0008] The purpose of the present invention is to solve the above problems and to propose an electrochromic film material and a method for preparing the same.

[0009] In order to achieve the above object, the present invention adopts the following technical solutions: An electrochromic film material comprises the following components in parts by weight: Resin 1-60 parts by weight; 0.01-50 parts by weight of monomer; Cross-linking agent 0.01-50 parts by weight; Initiator 0.1-0.01 parts by weight; The spacer is 0.1-0.01 parts by weight.

[0010] Preferably, the resin is one of acrylate resin, polyurethane resin, polyester resin or epoxy resin; The monomer is one of an acrylic monomer, a vinyl monomer, an epoxy monomer or an epoxy acrylate monomer; The cross-linking agent is a multifunctional monomer; The initiator is a photoinitiator or a thermal initiator; The spacers are rigid microbeads.

[0011] An electrochromic film material comprises the following components in parts by weight: 0.01-10 parts by weight of electrochromic material; 0.01-10 parts by weight of ion storage material; Liquid electrolyte material 50.01-102.5 parts by weight.

[0012] Preferably, the electrochromic material is one of organic polymers, organic small molecules, and metal oxide or metal complex electrochromic materials; The ion storage material is one of vanadium pentoxide, tungsten oxide, tantalum oxide, indium tin oxide, Prussian blue, polyaniline, triphenylamine, phenazine or viologen compounds; The liquid electrolyte material is composed of 50-99 parts by weight of a liquid conductive medium and 0.1-3.5 parts by weight of an electrolyte salt; The liquid conductive medium is one of a liquid organic solvent, an ionic liquid or a gel-like cross-linked polymer material; The electrolyte salt is selected from at least one of lithium perchlorate, lithium hexafluorophosphate, lithium tetrafluorophosphate, lithium bis(oxalatoborate) and lithium diimide.

[0013] Preferably, the raw material components include a high-adhesive composition and a redox-type liquid electrochromic composition, and the mass ratio of the high-adhesive composition to the redox-type liquid electrochromic composition is 1:0.01-50.

[0014] Preferably, the method for preparing the electrochromic film material comprises the following steps: S1: Material selection: Select a new type of electrochromic material, such as tungsten oxide, which has good electrochromic performance and stability; mix tungsten oxide powder with a certain proportion of binder, stir evenly, and form an electrochromic slurry; S2: Electrochromic film is prepared: the electrochromic slurry is coated on a transparent substrate by screen printing to form an electrochromic film; during the coating process, the coating thickness is controlled to be between 0.5 and 1.5 microns to ensure the light transmittance and color changing effect of the electrochromic film; S3: heat treatment: drying the coated electrochromic film in air, and then sintering at 500° C. for 30 minutes to firmly bond the electrochromic film to the substrate; S4: manufacturing an electrochromic device: assembling the sintered electrochromic film and two pieces of conductive glass together to form an electrochromic device with a sandwich structure; during the assembly process, ensuring that there are no bubbles between the electrochromic film and the conductive glass to ensure good electrical contact; S5: Electrochromic device test: The assembled electrochromic device is connected to a power source. By applying different voltages, the electrochromic device can present different colors, thereby adjusting the light transmittance; for example, when a voltage of +2V is applied, the electrochromic device is blue, and when a voltage of -2V is applied, the electrochromic device is transparent; S6: Finished product: The prepared electrochromic device is installed on the window to obtain an electrochromic window; when strong light is directly irradiated, the irradiation intensity of the light can be adjusted by changing the applied voltage, thereby adjusting the indoor light and temperature to achieve the purpose of energy saving.

[0015] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are: 1. This application improves the adjustment ability and stability of electrochromic windows by redesigning electrochromic materials and structures, so that they can more effectively change the radiation intensity of light when strong light is directly exposed, adjust indoor light and temperature, thereby reducing energy consumption for heating, cooling, etc. and reducing environmental pollution.

[0016] 2. This application reduces the production cost of electrochromic devices by researching and developing new electrochromic device preparation processes and methods, making them more suitable for large-scale applications. At the same time, the memory effect of the electrochromic device is improved, that is, the electrochromic device can maintain its color change state without the need for an external power supply after the color change, so that no external voltage is required when displaying static images, thereby achieving the purpose of energy saving.

[0017] 3. This application studies and develops a new electrochromic display preparation process and method to reduce its power consumption and improve its energy-saving effect by addressing the problem that the electrochromic display still requires high power consumption when displaying dynamic images; and studies and develops a new electrochromic glasses preparation process and method to improve its adjustability and stability by addressing the problem that the electrochromic glasses have a limited adjustable range and are greatly affected by voltage stability, so that they can change color anytime and anywhere by changing the voltage, and have greater adjustability. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 A schematic structural diagram of the method steps for preparing an electrochromic film material according to an embodiment of the present invention is shown; DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0020] See also Figure 1 , the present invention provides a technical solution: An electrochromic film material comprises the following components in parts by weight: Resin 1-60 parts by weight; 0.01-50 parts by weight of monomer; Cross-linking agent 0.01-50 parts by weight; Initiator 0.1-0.01 parts by weight; The spacer is 0.1-0.01 parts by weight.

[0021] The resin is one of acrylate resin, polyurethane resin, polyester resin or epoxy resin; The monomer is one of an acrylic (ester) monomer, a vinyl monomer, an epoxy monomer or an epoxy acrylate monomer; The cross-linking agent is a multifunctional monomer; The initiator is a photoinitiator or a thermal initiator; The spacers are rigid microbeads.

[0022] Also includes the following components in parts by weight: 0.01-10 parts by weight of electrochromic material; 0.01-10 parts by weight of ion storage material; Liquid electrolyte material 50.01-102.5 parts by weight.

[0023] The electrochromic material is one of organic polymers, organic small molecules, metal oxides or metal complex electrochromic materials; The ion storage material is one of vanadium pentoxide, tungsten oxide, tantalum oxide, indium tin oxide, Prussian blue, polyaniline, triphenylamine, phenazine or viologen compounds; The liquid electrolyte material is composed of 50-99 parts by weight of a liquid conductive medium and 0.1-3.5 parts by weight of an electrolyte salt; The liquid conductive medium is one of a liquid organic solvent, an ionic liquid or a gel-like cross-linked polymer material; The electrolyte salt is selected from at least one of lithium perchlorate, lithium hexafluorophosphate, lithium tetrafluorophosphate, lithium bis(trifluoromethylsulfonyl)imide and lithium bis(trifluoromethylsulfonyl)imide.

[0024] The raw material components include a high-adhesive composition and a redox-type liquid electrochromic composition, and the mass ratio of the high-adhesive composition to the redox-type liquid electrochromic composition is 1:0.01-50.

[0025] A method for preparing an electrochromic film material comprises the following steps: S1: Material selection: Select a new type of electrochromic material, such as tungsten oxide (WO3), which has good electrochromic performance and stability; mix tungsten oxide powder with a certain proportion of a binder (such as polyvinyl alcohol), stir evenly, and form an electrochromic slurry; S2: Electrochromic film is made: the electrochromic slurry is coated on a transparent substrate (such as glass) by screen printing to form an electrochromic film; during the coating process, the coating thickness is controlled between 0.5-1.5 microns to ensure the light transmittance and color changing effect of the electrochromic film; S3: heat treatment: drying the coated electrochromic film in air, and then sintering at 500° C. for 30 minutes to firmly bond the electrochromic film to the substrate; S4: Electrochromic device fabrication: Assemble the sintered electrochromic film and two pieces of conductive glass (such as ITO glass) together to form a sandwich-structured electrochromic device; during the assembly process, ensure that there are no bubbles between the electrochromic film and the conductive glass to ensure good electrical contact; S5: Electrochromic device test: The assembled electrochromic device is connected to a power source. By applying different voltages, the electrochromic device can present different colors, thereby adjusting the light transmittance; for example, when a voltage of +2V is applied, the electrochromic device is blue, and when a voltage of -2V is applied, the electrochromic device is transparent; S6: Finished product: The prepared electrochromic device is installed on the window to obtain an electrochromic window; when strong light is directly irradiated, the irradiation intensity of the light can be adjusted by changing the applied voltage, thereby adjusting the indoor light and temperature to achieve the purpose of energy saving.

[0026] The above description of the embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. An electrochromic film material, It is characterized in that The composition comprises the following components in parts by weight: Resin 1-60 parts by weight; 0.01-50 parts by weight of monomer; Cross-linking agent 0.01-50 parts by weight; Initiator 0.1-0.01 parts by weight; The spacer is 0.1-0.01 parts by weight.

2. The electrochromic film material according to claim 1, It is characterized in that The resin is one of acrylate resin, polyurethane resin, polyester resin or epoxy resin; The monomer is one of an acrylic monomer, a vinyl monomer, an epoxy monomer or an epoxy acrylate monomer; The cross-linking agent is a multifunctional monomer; The initiator is a photoinitiator or a thermal initiator; The spacers are rigid microbeads.

3. The electrochromic film material according to claim 1, Features: The composition comprises the following components in parts by weight: 0.01-10 parts by weight of electrochromic material; 0.01-10 parts by weight of ion storage material; Liquid electrolyte material 50.01-102.5 parts by weight.

4. The electrochromic film material according to claim 3, It is characterized in that The electrochromic material is one of organic polymers, organic small molecules, and metal oxides or metal complexes; The ion storage material is one of vanadium pentoxide, tungsten oxide, tantalum oxide, indium tin oxide, Prussian blue, polyaniline, triphenylamine, phenazine or viologen compounds; The liquid electrolyte material is composed of 50-99 parts by weight of a liquid conductive medium and 0.1-3.5 parts by weight of an electrolyte salt; The liquid conductive medium is one of a liquid organic solvent, an ionic liquid or a gel-like cross-linked polymer material; The electrolyte salt is selected from at least one of lithium perchlorate, lithium hexafluorophosphate, lithium tetrafluorophosphate, lithium bis(oxalatoborate) and lithium diimide.

5. An electrochromic film material according to any one of claims 1 to 4, Features: The raw material components include the high-adhesive composition according to claim 1 or 2 and the redox-type liquid electrochromic composition according to claim 3 or 4, and the mass ratio of the high-adhesive composition to the redox-type liquid electrochromic composition is 1:0.01-50.

6. A method for preparing the electrochromic film material according to claim 5, It is characterized in that The following steps are involved: S1: Material selection: Select a new type of electrochromic material, such as tungsten oxide, which has good electrochromic performance and stability; mix tungsten oxide powder with a certain proportion of binder, stir evenly, and form an electrochromic slurry; S2: Electrochromic film preparation: coating the electrochromic slurry on a transparent substrate by screen printing to form an electrochromic film; During the coating process, the coating thickness is controlled between 0.5-1.5 microns to ensure the light transmittance and color changing effect of the electrochromic film; S3: heat treatment: drying the coated electrochromic film in air, and then sintering at 500° C. for 30 minutes to firmly bond the electrochromic film to the substrate; S4: manufacturing an electrochromic device: assembling the sintered electrochromic film and two pieces of conductive glass together to form an electrochromic device with a sandwich structure; during the assembly process, ensuring that there are no bubbles between the electrochromic film and the conductive glass to ensure good electrical contact; S5: Electrochromic device test: The assembled electrochromic device is connected to a power source. By applying different voltages, the electrochromic device can present different colors, thereby adjusting the light transmittance; for example, when a voltage of +2V is applied, the electrochromic device is blue, and when a voltage of -2V is applied, the electrochromic device is transparent; S6: Finished product: The prepared electrochromic device is installed on the window to obtain an electrochromic window; when strong light is directly irradiated, the irradiation intensity of the light can be adjusted by changing the applied voltage, thereby adjusting the indoor light and temperature to achieve the purpose of energy saving.

Citation Information

Patent Citations

  • Electrochromic membrane material and electrochromic membrane device prepared by same

    CN108363255A

  • Electrochromic film and preparation method thereof

    CN112965311A

  • Electrochromic film material and electrochromic film device prepared therefrom

    US20210026213A1