Manufacturing method of heterojunction battery

By using high-temperature silver paste and laser removal technology in heterojunction solar cells, the problems of low welding tension and high paste consumption caused by low-temperature silver paste are solved, the welding effect and service life of the components are improved, and the production cost is reduced. cost.

CN118763129APending Publication Date: 2024-10-11JIANGSU RUISHENG LIGHT ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410798819.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-20
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The low-temperature silver paste of existing heterojunction solar cells results in low welding tension, which affects the assembly effect and service life of the components. At the same time, the paste consumption is high, which increases the cost.

Method used

High-temperature silver paste is used for printing and sintering. By plating doped polysilicon and transparent metal conductive film on both sides of the silicon wafer, combined with laser removal of amorphous silicon and conductive film, the welding strength is improved and the amount of silver paste used is reduced.

Benefits of technology

The welding pull force is enhanced, the service life of the component is extended, and the production cost is reduced by reducing the amount of silver paste used.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118763129A_ABST
    Figure CN118763129A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a heterojunction battery. The manufacturing method comprises the following steps: step 1, carrying out heterojunction texturing on an N-type silicon wafer through the prior art; step 2, plating doped polycrystalline silicon on the two surfaces of the silicon wafer; 3, performing double-sided high-temperature silver paste printing and sintering according to the target pattern; 4, printing ink at the electrode position; step 5, removing the polycrystalline silicon and the printing ink; step 6, plating amorphous silicon on the two surfaces of the silicon wafer; 7, plating transparent metal conductive films ITO on the two surfaces of the silicon wafer; and step 8, removing the amorphous silicon and the transparent metal conductive film ITO at the welding point position by using laser. High-temperature silver paste is adopted for printing and sintering, and metal and a silicon wafer can be better fused due to the high temperature of the silver paste, so that the welding tension is enhanced, the welding effect of the assembly is improved, and the service life of the assembly is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of heterojunction battery manufacturing, and in particular to a method for manufacturing a heterojunction battery. Background Art

[0002] In recent years, the photovoltaic industry has developed rapidly, and people have proposed many new structures and preparation methods of solar cells with excellent electrical properties. Among them, heterojunction solar cells (HJT solar cells) have high photoelectric conversion efficiency, low temperature coefficient and low cost, and have been widely and deeply studied by many scientific research institutions and enterprises. The typical manufacturing process of heterojunction solar cells is to deposit intrinsic amorphous silicon, doped amorphous silicon and transparent conductive oxide film on both sides of the n-type silicon wafer in sequence, and then screen print silver paste on both sides as electrodes, and then perform thermal curing. The current process uses low-temperature silver paste. The disadvantages of low-temperature silver paste are: 1. The welding tension is relatively low, which will affect the welding effect of the component and the subsequent component life. After all, the component needs to be used stably for decades; 2. The special structure of low-temperature silver paste leads to high paste consumption and high cost. Summary of the invention

[0003] The purpose of the present invention is to solve at least one of the technical problems existing in the prior art and to provide a method for manufacturing a heterojunction battery with good welding effect and low slurry consumption.

[0004] A method for manufacturing a heterojunction battery according to an embodiment of the present invention comprises the following steps:

[0005] Step 1, performing heterojunction texturing on an N-type silicon wafer;

[0006] Step 2, coating doped polysilicon on both sides of the silicon wafer;

[0007] Step 3, double-sided high-temperature silver paste printing and sintering according to the target pattern;

[0008] Step 4, printing ink at the electrode position;

[0009] Step 5, removing polysilicon and ink;

[0010] Step 6, coating amorphous silicon on both sides of the silicon wafer;

[0011] Step 7, coating transparent metal conductive film ITO on both sides of the silicon wafer;

[0012] Step 8: Use laser to remove the amorphous silicon and transparent metal conductive film ITO at the welding point.

[0013] According to some embodiments of the present invention, in step 2, tubular PECVD is used to coat 100 nm of doped polysilicon on both sides of the silicon wafer.

[0014] According to some embodiments of the present invention, in step 5, HF and HNO 3 are used to remove polysilicon, and KOH is used to remove ink.

[0015] According to some embodiments of the present invention, in step 6, amorphous silicon / microcrystalline silicon is plated on both sides of the silicon wafer.

[0016] According to some embodiments of the present invention, in step 7, a transparent metal conductive film ITO / silicon nitride is plated on both sides of the silicon wafer.

[0017] According to some embodiments of the present invention, in step 8, amorphous silicon / microcrystalline silicon and transparent metal conductive film at the welding point are removed by laser.

[0018] The manufacturing method of the heterojunction battery according to the embodiment of the present invention has at least the following beneficial effects: high-temperature silver paste is used for printing and sintering. Due to the high temperature of the silver paste, the metal and the silicon wafer can be better melted, thereby enhancing the welding tension, improving the welding effect of the component and extending the service life of the component. Secondly, compared with low-temperature silver paste, the high-temperature silver paste itself has a small resistance, and its contact resistance with other components is also small. Effective printing and sintering can be achieved without the accumulation of a large amount of silver paste, and the paste consumption is significantly low, thereby reducing costs.

[0019] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] The specific embodiments of the present invention will be further described below in conjunction with the accompanying drawings;

[0021] Figure 1 It is a flow chart of the method for manufacturing a heterojunction battery. DETAILED DESCRIPTION

[0022] This section will describe in detail the specific embodiments of the present invention. The preferred embodiments of the present invention are shown in the accompanying drawings. The purpose of the accompanying drawings is to supplement the description of the text part of the specification with graphics, so that people can intuitively and vividly understand each technical feature and the overall technical solution of the present invention, but it cannot be understood as a limitation on the scope of protection of the present invention.

[0023] In the description of the present invention, it should be understood that descriptions involving orientations, such as up, down, front, back, left, right, etc., and orientations or positional relationships indicated are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0024] In the description of the present invention, “several” means one or more, “more” means more than two, “greater than”, “less than”, “exceed”, etc. are understood as not including the number itself, and “above”, “below”, “within”, etc. are understood as including the number itself.

[0025] Reference Figure 1 The present invention provides a method for manufacturing a heterojunction battery, comprising the steps of:

[0026] Step 1, performing heterojunction texturing on an N-type silicon wafer using existing technology;

[0027] Step 2, coating doped polysilicon on both sides of the silicon wafer;

[0028] Step 3, double-sided high-temperature silver paste printing and sintering according to the target pattern;

[0029] Step 4, printing ink at the electrode position;

[0030] Step 5, removing polysilicon and ink;

[0031] Step 6, coating amorphous silicon on both sides of the silicon wafer;

[0032] Step 7, coating transparent metal conductive film ITO on both sides of the silicon wafer;

[0033] Step 8: Use laser to remove the amorphous silicon and transparent metal conductive film ITO at the welding point.

[0034] Furthermore, in step 2, tubular PECVD is used to coat 100 nm of doped polysilicon on both sides of the silicon wafer to improve manufacturing efficiency.

[0035] In some embodiments, in step 5, HF and HNO3 are used to remove polysilicon, and KOH is used to remove ink, and the removal effect is good.

[0036] In some embodiments, in step 6, in addition to amorphous silicon, microcrystalline silicon may also be plated on both sides of the silicon wafer. In step 8, amorphous silicon or microcrystalline silicon at the welding point position needs to be removed by laser.

[0037] In some embodiments, in step 7, in addition to coating the transparent metal conductive film ITO on both sides of the silicon wafer, silicon nitride can also be coated to improve light absorption and reduce costs.

[0038] The present invention uses high-temperature silver paste for printing and sintering. Due to the high temperature of the silver paste, the metal and the silicon wafer can be melted better, thereby enhancing the welding tension, improving the welding effect of the component and extending the service life of the component. Secondly, compared with the low-temperature silver paste, the high-temperature silver paste itself has a small resistance, and its contact resistance with other components is also small. Effective printing and sintering can be achieved without the accumulation of a large amount of silver paste, and the slurry consumption is significantly low, thereby reducing costs.

[0039] It is easy for those skilled in the art to understand that the above preferred embodiments can be freely combined and superimposed without conflict.

[0040] The above are only preferred embodiments of the present invention, and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the contents of the present invention's specification and drawings under the inventive concept of the present invention, or directly or indirectly applied in other related technical fields, are included in the patent protection scope of the present invention.

Claims

1. A method for manufacturing a heterojunction battery, characterized in that: Includes steps: Step 1, performing heterojunction texturing on an N-type silicon wafer; Step 2, coating doped polysilicon on both sides of the silicon wafer; Step 3, double-sided high-temperature silver paste printing and sintering according to the target pattern; Step 4, printing ink at the electrode position; Step 5, removing polysilicon and ink; Step 6, coating amorphous silicon on both sides of the silicon wafer; Step 7, coating transparent metal conductive film ITO on both sides of the silicon wafer; Step 8: Use laser to remove the amorphous silicon and transparent metal conductive film ITO at the welding point.

2. The method for manufacturing a heterojunction battery according to claim 1, characterized in that: In step 2, 100 nm of doped polysilicon is plated on both sides of the silicon wafer using tubular PECVD.

3. The method for manufacturing a heterojunction battery according to claim 1, characterized in that: In step 5, HF and HNO3 are used to remove polysilicon, and KOH is used to remove ink.

4. The method for manufacturing a heterojunction battery according to claim 1, characterized in that: In step 6, amorphous silicon / microcrystalline silicon is plated on both sides of the silicon wafer.

5. The method for manufacturing a heterojunction battery according to claim 4, characterized in that: In step 7, a transparent metal conductive film ITO / silicon nitride is coated on both sides of the silicon wafer.

6. The method for manufacturing a heterojunction battery according to claim 5, characterized in that: In step 8, the amorphous silicon / microcrystalline silicon and the transparent metal conductive film at the welding point are removed by laser.