A wheel rim forming die and coupled heating spinning method
By using a combination of a semi-annular heating chamber and multiple spray guns in the rim forming mold, an overlapping coupled heating zone is formed, which solves the problem of difficulty in controlling the spray gun heating, and achieves uniform heating and production efficiency improvement in the rim spinning surface area.
Patent Information
- Application Number
- CN202411244719.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-06
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-09-06
AI Technical Summary
During the rim spinning process, the spray gun heating method is used, and the effective range of its heating surface is difficult to control, affecting production efficiency.
A rim forming mold is designed, including a mold body, a spin wheel and a heating assembly. Through the combination of a semi-annular heating chamber and a plurality of spray guns, the flame of the spray gun is sprayed out through the upper and lower spray holes respectively to form an overlapping coupled heating zone. , ensure that the spinning surface is always heated effectively.
Complete coverage heating of the rim rotation surface area is achieved, spinning efficiency and production efficiency are improved, and uniform heating of the rim blank during spinning.
Smart Images

Figure CN118768446B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of metal casting, and more specifically, relates to a rim forming die and a coupled heating spinning method. Background Art
[0002] The rim, commonly known as the wheel ring, is the component for mounting the tire around the wheel. The rim structure is an important component of the automobile wheel and is the basis for assembling and fixing the tire.
[0003] Spinning technology is a metal forming process that achieves plastic deformation of metal by rotating the workpiece and applying pressure. Rim spinning is a manufacturing process for automobile wheels. The rim is processed by spinning technology to improve the strength, rigidity and aesthetics of the wheel. During the rim spinning process, the rim will be fixed on the spinning machine, and then the rotation of the spinning machine and the pressure of the spinning wheel will cause the rim to undergo plastic deformation to form the desired shape and size.
[0004] During the rim spinning process, in order to improve the efficiency of spinning, a spray gun is set on one side of the rim blank. The spray gun sprays flames to heat the spinning surface of the rim. The rim is spun at a high temperature, which can speed up production efficiency. However, when using a spray gun to heat the rim, the effective range of the heating surface is usually difficult to control. Summary of the invention
[0005] The object of the present invention is to provide a rim forming die, aiming to solve the problem that the effective range of the heating surface is usually difficult to control when the rim is heated by a spray gun.
[0006] To achieve the above object, the technical solution adopted by the present invention is: to provide a rim forming mold, comprising:
[0007] A mold body, the mold body comprising a lower mold and an upper mold, the lower mold is mounted on the lower mounting end of the spinning machine, the upper mold is mounted on the upper mounting end of the spinning machine, the lower mold and the upper mold are coaxially arranged and can move axially relative to each other and move synchronously, a plurality of movable blocks are circumferentially arranged on the upper end surface of the lower mold, the outer peripheral surface of the upper mold, the outer peripheral surface of the lower mold and the outer peripheral surfaces of the plurality of movable blocks jointly constitute an assembly surface adapted to the inner peripheral surface of the rim, and the plurality of movable blocks move synchronously along the radial direction of the lower mold to respectively constitute a gathered state for disassembling and assembling the rim and a dispersed state for positioning the rim;
[0008] A spinning wheel, the spinning wheel is arranged at one side of the mold body, the spinning wheel moves horizontally away from the mold body to form a non-working state, and the spinning wheel moves horizontally to abut against the outer peripheral surface of the rim to form a working state, and the contact surface between the spinning wheel and the rim in the working state is defined as the spinning surface;
[0009] A heating assembly, wherein the heating assembly comprises a plurality of spray guns and a semi-annular heating chamber, wherein the plurality of spray guns are connected to the semi-annular heating chamber, wherein the semi-annular heating chamber is coaxially arranged on a side of the mold body away from the spinning wheel, wherein the inner side wall of the semi-annular heating chamber is provided with a flame-spraying hole in accordance with the shape, wherein a partition is horizontally arranged inside the semi-annular heating chamber, wherein the partition divides the inner cavity of the semi-annular heating chamber into an upper chamber and a lower chamber, wherein the partition extends to the inner side wall of the semi-annular heating chamber and divides the flame-spraying hole from top to bottom into an upper spray hole and a lower chamber connected to the upper chamber. A lower spray hole connected to the lower chamber, an upper guide slope is arranged on the side of the upper end surface of the partition close to the inner wall of the semi-annular heating chamber, and the upper guide slope is used to guide the flame sprayed from the upper spray hole to spray toward the spinning surface, and a lower guide slope is arranged on the side of the lower end surface of the partition close to the inner wall of the semi-annular heating chamber, and the lower guide slope is used to guide the flame sprayed from the lower spray hole to spray toward the spinning surface, and the flames sprayed from the upper spray hole and the lower spray hole form overlapping coupling heating areas on the outer wall of the rim to cover the spinning surface.
[0010] In one possible implementation, the lower mold is provided with a plurality of elastic guide components, and the plurality of elastic guide components are connected one by one to the lower ends of the plurality of movable blocks. The elastic guide components are inclined outward from top to bottom and have elastic supporting forces along their own axes. The elastic supporting forces of the plurality of elastic guide components are gathered above the lower mold to form a gathered state, or the plurality of movable blocks are pressed downward by the upper mold and move axially along the corresponding elastic guide components to be distributed in the circumference of the lower mold to form a dispersed state.
[0011] In one possible implementation, the elastic guide assembly includes a plurality of guide slides and a plurality of top blocks, the plurality of guide slides are circumferentially opened on the upper mold, the guide slides are inclined outward from top to bottom, and the plurality of top blocks are arranged in the plurality of guide slides in a one-to-one correspondence, a first elastic member is fixed to the bottom of the guide slide, the upper end of the first elastic member is connected to the corresponding top block and provides elastic force for the top block to move upward along the guide slide.
[0012] In a possible implementation, a top column is provided inside the lower mold, and the top column is coaxially arranged in the middle part of the lower mold. A plurality of telescopic rods are circumferentially arranged on the upper end of the top column. The plurality of telescopic rods are connected to a plurality of movable blocks in a one-to-one correspondence. The telescopic rods shorten or lengthen as the movable blocks are raised or lowered. A second elastic member is connected to the lower end of the top column, and the second elastic member is used to provide an elastic force for the top column to move upward.
[0013] In a possible implementation, a filling groove is provided at one end of the outer side of the partition, an upper insulation sleeve is provided at the upper part of the semi-annular heating chamber from the outside to the inside, and a lower insulation sleeve is provided at the lower part of the semi-annular heating chamber from the outside to the inside, the bottom insulation layer of the upper insulation sleeve and the top insulation layer of the lower insulation sleeve are respectively pressed into the filling groove, the upper insulation sleeve covers an area of not less than 80% of the top of the semi-annular heating chamber, and the lower insulation sleeve covers an area of not less than 80% of the lower part of the semi-annular heating chamber.
[0014] In a possible implementation, a plurality of upper connecting tubes are arranged at equal angles on the upper portion of the outer wall of the semi-annular heating chamber, and the plurality of upper connecting tubes are all connected to the upper chamber; a plurality of lower connecting tubes are arranged at equal angles on the lower portion of the outer wall of the semi-annular heating chamber, and the plurality of lower connecting tubes are all connected to the lower chamber; the plurality of upper connecting tubes and the plurality of lower connecting tubes are alternately arranged on the outer periphery of the semi-annular heating chamber, and the plurality of upper connecting tubes and the plurality of lower connecting tubes are all connected to the plurality of spray guns one by one.
[0015] In a possible implementation, the arc of the semi-annular heating chamber is not less than 60°, and the distance between the inner wall of the semi-annular heating chamber and the inner wall of the rim is not less than 5 times the thickness of the rim wall.
[0016] The rim forming mold provided by the present invention has the beneficial effect that: compared with the prior art, the rim blank is mounted on the lower mold, the upper mold is moved downward for mold closing, the inner peripheral surface of the rim is adapted to be mounted on the outer peripheral surface of the upper mold, the outer peripheral surface of the lower mold and the outer peripheral surface of multiple movable blocks to form an assembly surface, and the multiple movable blocks move radially outward, thereby circumferentially tightening the inner peripheral surface of the rim blank. The spinning wheel is switched from a non-working state to a working state, and the spinning wheel abuts against one side of the rim blank to confirm the initial position of the spinning surface. According to the initial spinning surface position, the semi-annular heating chamber is adjusted so that the upper spray hole and the lower spray hole on the inner side wall of the semi-annular heating chamber are respectively arranged at the upper and lower parts of the spinning surface. Multiple spray guns are installed on the semi-annular heating chamber, and the multiple spray guns are turned on. The flames sprayed from the spray guns are sprayed from the upper spray hole and the lower spray hole through the upper chamber and the lower chamber respectively, and the flame forms a coupled heating zone in the spinning surface area. The rim forming die provided by the present invention can form a coupled heating zone that completely covers the spinning surface by using multiple spray guns in conjunction with a semi-annular heating chamber, thereby ensuring that the spinning surface area of the rim blank is always effectively heated.
[0017] The present invention also provides a coupled heating spinning method, which is applied to the rim forming mold, and comprises the following steps:
[0018] S1: The rim is sleeved on the lower die of the spinning machine from top to bottom, the upper die of the spinning machine moves downward to close the die, and the upper die squeezes multiple movable blocks downward, and the multiple movable blocks move downward and expand radially outward to support the circumference of the inner wall of the rim;
[0019] S2: The spinning wheel on one side of the mold body moves horizontally until its edge abuts against the upper end of the outer wall of the rim, and the semi-annular heating chamber on the other side of the mold body moves toward the side close to the rim, and the inner side of the semi-annular heating chamber reaches a preset distance L from the upper end of the outer wall of the rim, and multiple spray guns are respectively connected to the semi-annular heating chamber;
[0020] S3: Turn on the spinning machine, which drives the rim to rotate, applies a predetermined pressure P to the spinning wheel on one side of the rim and forms a spinning surface with the contact surface of the rim, turns on multiple spray guns, and sprays high-temperature flames into the semi-annular heating chamber and sprays them simultaneously through the upper spray holes and the lower spray holes. The area covered by the flames sprayed from the upper spray holes is the upper heating zone, and the area covered by the flames sprayed from the lower spray holes is the lower heating zone. An overlapping coupling heating zone is formed between the upper heating zone and the lower heating zone to heat the spinning surface;
[0021] S4: The spinning machine drives the rim to rotate and move the rim upward at the same time, and the spinning wheel completes the spinning of the rim from top to bottom in sequence.
[0022] In one possible implementation, in step S2, when the spinning wheel on one side of the mold body moves horizontally to the point where its edge abuts against the upper end of the outer wall of the rim, the contact point between the outer arc end of the spinning wheel and the outer wall of the rim is used as the reference point. The spinning machine is turned on to drive the rim to rotate for at least one circle. The reference point forms a reference line in the circumferential direction of the outer wall of the rim. Two parallel lines are formed after being offset upward and downward by a distance s based on the reference line. The area between the two parallel lines is the spinning surface, s=cota×tana×r, wherein a is half of the preset angle between the outer arc of the spinning wheel and the spinning surface, the value range of a is 10°~20°, and r is the radius of the outer arc end of the spinning wheel.
[0023] In a possible implementation, in step S2, when the preset distance L is set, L=n×d×k, where n≥5, k is in the range of 1 to 1.3, and d is the minimum thickness of the rim in the area where the spinning surface is located; in step S3, when the predetermined pressure P is set, P is in the range of 150 to 250 kgf / mm 2 .
[0024] Compared with the prior art, the coupled heating spinning method provided by the present invention has the following characteristics: when spinning the rim blank, multiple spray guns spray high-temperature flames into the semi-annular heating chamber and spray them out simultaneously through the upper spray hole and the lower spray hole. The area covered by the flames sprayed from the upper spray hole is the upper heating zone, and the area covered by the flames sprayed from the lower spray hole is the lower heating zone. An overlapping coupled heating zone is formed between the upper heating zone and the lower heating zone to heat the spinning surface. By continuously moving the spinning machine upward, the spinning of the rim is completed. The coupled heating spinning method provided by the present invention can use multiple spray guns in conjunction with the semi-annular heating chamber to form a coupled heating zone that completely covers the spinning surface, ensuring that the spinning surface area of the rim blank is always effectively heated. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0026] Figure 1 A front view of a rim forming mold provided by the present invention;
[0027] Figure 2 A top view of a rim forming mold provided by the present invention;
[0028] Figure 3 for Figure 1 A partial enlarged view of the M in the middle;
[0029] Figure 4 A cross-sectional view of a semi-annular heating chamber provided by the present invention;
[0030] Figure 5 A schematic diagram of the spinning surface provided by the present invention.
[0031] In the figure:
[0032] 1. Lower mold; 2. Upper mold; 3. Movable block; 4. Ejector block; 5. First elastic member; 6. Ejector column; 7. Second elastic member; 8. Telescopic rod; 9. Spinning wheel; 10. Semi-circular heating chamber; 11. Spray gun; 12. Partition; 13. Upper chamber; 14. Lower chamber; 15. Upper guide slope; 16. Lower guide slope; 17. Coupled heating zone; 18. Single-side heating zone; 19. Upper insulation sleeve; 20. Lower insulation sleeve; 21. Upper connecting pipe; 22. Nozzle; 23. Spinning surface. DETAILED DESCRIPTION
[0033] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0034] In the claims, description and the above-mentioned drawings of the present invention, unless otherwise clearly defined, the use of terms such as "first", "second" or "third" etc. are for distinguishing different objects rather than for describing a specific order.
[0035] In the claims, specification and the above-mentioned drawings of the present invention, unless otherwise explicitly defined, directional words, such as the terms "center", "lateral", "longitudinal", "horizontal", "vertical", "top", "bottom", "inside", "outside", "up", "down", "front", "back", "left", "right", "clockwise", "counterclockwise", "high", "low", etc., indicating directions or positional relationships are based on the directions and positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction or be constructed and operated in a specific direction, and therefore cannot be understood as limiting the specific protection scope of the present invention.
[0036] See also Figures 1 to 4 Now, a rim forming mold provided by the present invention is described. A rim forming mold comprises a mold body, a spinning wheel 9 and a heating component.
[0037] The mold body includes a lower mold 1 and an upper mold 2, the lower mold 1 is installed at the lower mounting end of the spinning machine, and the upper mold 2 is installed at the upper mounting end of the spinning machine. The lower mold 1 and the upper mold 2 are coaxially arranged and can move axially relative to each other and move synchronously. A plurality of movable blocks 3 are circumferentially arranged on the upper end surface of the lower mold 1. The outer peripheral surface of the upper mold 2, the outer peripheral surface of the lower mold 1, and the outer peripheral surfaces of the plurality of movable blocks 3 jointly constitute an assembly surface adapted to the inner peripheral surface of the rim. The plurality of movable blocks 3 move synchronously along the radial direction of the lower mold 1 to respectively constitute a plurality of movable blocks 3 for disassembling and assembling the wheel rim. The spinning wheel 9 is arranged on one side of the mold body, the spinning wheel 9 moves horizontally away from the mold body to form a non-working state, and the spinning wheel 9 moves horizontally to abut against the outer peripheral surface of the rim to form a working state, and the contact surface between the spinning wheel 9 and the rim in the working state is defined as the spinning surface 23; the heating assembly includes a plurality of spray guns 11 and a semi-annular heating chamber 10, the plurality of spray guns 11 are connected to the semi-annular heating chamber 10, and the semi-annular heating chamber 10 is connected to the semi-annular heating chamber 10. The shaft is arranged on the side of the mold body away from the spinning wheel 9, and the inner wall of the semi-annular heating chamber 10 is provided with a flame hole in accordance with the shape. A partition 12 is arranged horizontally inside the semi-annular heating chamber 10, and the partition 12 divides the inner cavity of the semi-annular heating chamber 10 into an upper chamber 13 and a lower chamber 14. The partition 12 extends to the inner wall of the semi-annular heating chamber 10 and divides the flame hole from top to bottom into an upper spray hole connected to the upper chamber 13 and a lower spray hole connected to the lower chamber 14. The upper end surface of the partition 12 is close to the semi-annular heating chamber 10. An upper guide slope 15 is provided on one side of the inner wall of the annular heating chamber 10, and the upper guide slope 15 is used to guide the flame ejected from the upper nozzle to spray toward the spinning surface 23. A lower guide slope 16 is provided on the lower end surface of the partition 12 close to the inner wall of the semi-annular heating chamber 10, and the lower guide slope 16 is used to guide the flame ejected from the lower nozzle to spray toward the spinning surface 23. The flames ejected from the upper nozzle and the lower nozzle form an overlapping coupling heating area 17 on the outer wall of the rim to cover the spinning surface 23.
[0038] Compared with the prior art, the rim forming mold provided by the present invention is a rim blank that is mounted on the lower mold 1, and the upper mold 2 is moved downward to close the mold. The inner peripheral surface of the rim is adapted to be mounted on the outer peripheral surface of the upper mold 2, the outer peripheral surface of the lower mold 1, and the outer peripheral surfaces of multiple movable blocks 3 to form an assembly surface. The multiple movable blocks 3 move radially outward, thereby circumferentially tightening the inner peripheral surface of the rim blank. The spinning wheel 9 is switched from a non-working state to a working state, and the spinning wheel 9 abuts against one side of the rim blank to confirm the initial position of the spinning surface 23. According to the initial position of the spinning surface 23, the semi-annular heating chamber 10 is adjusted so that the upper spray hole and the lower spray hole on the inner side wall of the semi-annular heating chamber 10 are respectively arranged at the upper and lower parts of the spinning surface 23. A plurality of spray guns 11 are installed on the semi-circular heating chamber 10, and the plurality of spray guns 11 are turned on. The flames sprayed from the spray guns 11 are sprayed from the upper spray hole and the lower spray hole through the upper chamber 13 and the lower chamber 14, respectively. The flames sprayed from the upper spray hole and the lower spray hole respectively form a diffused single-side heating zone 18, and the two single-side heating zones 18 form a coupled heating zone 17 in the spinning surface 23 area. The rim forming mold provided by the present invention can use a plurality of spray guns 11 in conjunction with the semi-circular heating chamber 10 to form a coupled heating zone 17 that completely covers the spinning surface 23, ensuring that the spinning surface 23 area of the rim blank is always effectively heated.
[0039] See also Figure 1 The lower die 1 is provided with a plurality of elastic guide components, which are connected to the lower ends of the plurality of movable blocks 3 one by one. The elastic guide components are inclined outward from top to bottom and have elastic supporting force along their own axial direction. The elastic guide components provide elastic force along their axial direction and act on the corresponding movable blocks 3. Through the elastic supporting force of the plurality of elastic guide components, they gather on the top of the lower die 1 to form a gathered state. In the gathered state, the rim blank is sleeved on the lower die 1. The mold is closed, the upper die 2 and the lower die 1 are close to each other, and the plurality of movable blocks 3 are pressed downward by the upper die 2 and move axially along the corresponding elastic guide components respectively and are distributed in the circumference of the lower die 1 to form a dispersed state. At the same time, the plurality of movable blocks 3 are circumferentially supported on the inner circumference of the rim blank to keep the rim blank stable, and can be driven to rotate and rise and fall by the spinning machine.
[0040] Specifically, the elastic guide assembly includes a plurality of guide slides and a plurality of top blocks 4. The plurality of guide slides are circumferentially opened on the upper mold 2. The guide slides are inclined outward from top to bottom. The plurality of top blocks 4 are arranged in the plurality of guide slides one by one, and the top blocks 4 can slide along the axial direction of the guide slides. A first elastic member 5 is fixed to the bottom of the guide slide. The first elastic member 5 can adopt a structure of a spring and a guide rod. The upper end of the first elastic member 5 is connected to the corresponding top block 4 and provides an elastic force for the top block 4 to move upward along the guide slide. When the first elastic member 5 is not subjected to force, the plurality of movable blocks 3 are in a gathered state and are higher than the upper end surface of the upper mold 2. After the rim mold is assembled, the plurality of top blocks 4 can slide downward along the corresponding guide slides and expand radially through the extrusion of the upper mold 2, and finally reach a dispersed state.
[0041] See also Figure 1 A top column 6 is provided inside the lower mold 1, and the top column 6 is coaxially arranged in the middle part of the lower mold 1. A plurality of telescopic rods 8 are circumferentially arranged on the upper end of the top column 6. The plurality of telescopic rods 8 are connected to the plurality of movable blocks 3 one by one. The telescopic rods 8 automatically shorten or extend with the lifting and lowering of the movable blocks 3. The top column 6 cooperates with the plurality of telescopic rods 8 to ensure that the plurality of movable blocks 3 keep the movements consistent as much as possible. A second elastic member 7 is connected to the lower end of the top column 6. The second elastic member 7 is in the form of a spring cooperating with a fixed plate. When the second elastic member 7 is not under stress, the top column 6 is in an upward ejection state, the plurality of telescopic rods 8 are in an extended state, the plurality of movable blocks 3 are in a gathered state and are higher than the upper end surface of the upper mold 2. After the rim mold is assembled, the plurality of telescopic rods 8 can be shortened by extruding the upper mold 2, the top column 6 moves downward and compresses the second elastic member 7, and finally the plurality of movable blocks 3 are in a dispersed state.
[0042] See also Figure 4 A filling groove is provided at one end of the outer side of the partition 12. The cross section of the semi-annular heating chamber 10 is an M-shaped structure. The upper part of the semi-annular heating chamber 10 is provided with an upper heat insulation sleeve 19 from the outside to the inside, and the lower part of the semi-annular heating chamber 10 is provided with a lower heat insulation sleeve 20 from the outside to the inside. The bottom heat insulation layer of the upper heat insulation sleeve 19 and the top heat insulation layer of the lower heat insulation sleeve 20 are respectively pressed into the filling groove. The upper heat insulation sleeve 19 covers an area of not less than 80% of the top of the semi-annular heating chamber 10, and the lower heat insulation sleeve 20 covers an area of not less than 80% of the lower part of the semi-annular heating chamber 10. The upper heat insulation sleeve 19 and the lower heat insulation sleeve 20 are respectively mounted on the upper and lower parts of the semi-annular heating chamber 10, thereby forming a heat insulation layer on the outer surface of the semi-annular heating chamber 10, reducing heat loss, and also reducing the ambient temperature.
[0043] Preferably, the upper insulation sleeve 19 and the lower insulation sleeve 20 form a double insulation layer inside the partition 12 to reduce heat conduction between the upper chamber 13 and the lower chamber 14. Therefore, the flame temperature in the upper chamber 13 and the lower chamber 14 can be adjusted so that the intensity and temperature of the flame ejected from the upper nozzle hole and the lower nozzle hole are different. That is to say, the power of the spray gun 11 connected to the upper chamber 13 or the lower chamber 14 can be adjusted separately to achieve the purpose of adjusting the heating intensity of the coupled heating zone 17, avoiding adjusting the temperature of the flame in the upper chamber 13 and the lower chamber 14 at the same time. After being superimposed in the coupled heating zone 17, the temperature changes greatly. This method of using a double insulation layer to separate the temperature of the upper chamber 13 and the lower chamber 14 can improve the accuracy of temperature regulation in the coupled heating zone 17.
[0044] See also Figure 2 and Figure 4 A plurality of upper connecting pipes 21 are arranged at equal angles on the upper part of the outer wall of the semi-circular heating chamber 10. The plurality of upper connecting pipes 21 are connected to the upper chamber 13, which can improve the intensity of the flame in the upper chamber 13. At the same time, the flame intensity of the spray gun 11 at different positions can be adjusted to achieve the purpose of adjusting the flame intensity in the upper chamber 13. A plurality of lower connecting pipes are arranged at equal angles on the lower part of the outer wall of the semi-circular heating chamber 10. The plurality of lower connecting pipes are connected to the lower chamber 14, which can improve the intensity of the flame in the lower chamber 14. At the same time, the flame intensity of the spray gun 11 at different positions can be adjusted to achieve the purpose of adjusting the flame intensity in the lower chamber 14. The plurality of upper connecting tubes 21 and the plurality of lower connecting tubes are alternately arranged on the outer periphery of the semi-annular heating chamber 10 to avoid the problem that the temperature of the local area of the semi-annular heating chamber 10 is too high, which affects the service life of the semi-annular heating chamber 10 itself. At the same time, more space is provided for the installation of the plurality of spray guns 11 on the semi-annular heating chamber 10. The plurality of upper connecting tubes 21 and the plurality of lower connecting tubes are connected to the plurality of spray guns 11 one by one, and the spray rods of the spray guns 11 are inserted into the corresponding connecting tubes. The positions of the inner side walls of the upper chamber 13 and the lower chamber 14 corresponding to the connecting tubes are the same. The shaft is provided with a nozzle 22, which is connected to a corresponding connecting pipe. The flame of the spray gun 11 is sprayed into the upper chamber 13 and the lower chamber 14 through the nozzle 22, thereby forming different spray angles, so that the flames sprayed from the multiple nozzles 22 simultaneously located in the upper chamber 13 completely cover the entire area of the upper chamber 13. Similarly, the flames sprayed from the multiple nozzles 22 simultaneously located in the lower chamber 14 completely cover the entire area of the lower chamber 14, and finally the flames sprayed from the upper chamber 13 and the lower chamber 14 can form a uniform heating range on the outer side wall of the rim.
[0045] Specifically, the arc of the semi-annular heating chamber 10 is not less than 60°, ensuring that the semi-annular heating chamber 10 can cover a sufficient area of the outer peripheral wall of the rim, increasing the range of the heating area and ensuring the heating effect. The distance between the inner side wall of the semi-annular heating chamber 10 and the inner side wall of the rim is not less than 5 times the thickness of the rim wall, preventing the flame ejected from the flame ejection hole of the semi-annular heating chamber 10 from being too close to the rim, ensuring the heating effect.
[0046] The present invention also provides a coupled heating spinning method, which is applied to the above-mentioned rim forming mold, comprising the following steps:
[0047] S1: The rim is sleeved on the lower die 1 of the spinning machine from top to bottom, the upper die 2 of the spinning machine moves downward to close the die, the upper die 2 squeezes a plurality of movable blocks 3 downward, and the plurality of movable blocks 3 move downward and expand radially outward to support the circumference of the inner wall of the rim;
[0048] S2: The spinning wheel 9 on one side of the mold body moves horizontally until its edge abuts against the upper end of the outer wall of the rim, and the semi-annular heating chamber 10 on the other side of the mold body moves toward the side close to the rim, and the inner side of the semi-annular heating chamber 10 reaches a preset distance L from the upper end of the outer wall of the rim, and a plurality of spray guns 11 are respectively connected to the semi-annular heating chamber 10;
[0049] S3: Turn on the spinning machine, which drives the rim to rotate, applies a predetermined pressure P to the spinning wheel 9 on one side of the rim, and forms a spinning surface 23 with the contact surface of the rim, and turns on multiple spray guns 11, which spray high-temperature flames into the semi-annular heating chamber 10 and spray them out through the upper spray holes and the lower spray holes at the same time. The area covered by the flames sprayed from the upper spray holes is the upper heating zone, and the area covered by the flames sprayed from the lower spray holes is the lower heating zone. An overlapping coupling heating zone 17 is formed between the upper heating zone and the lower heating zone to heat the spinning surface 23;
[0050] S4: The spinning machine drives the rim to rotate and move the rim upward at the same time, and the spinning wheel 9 completes the spinning of the rim from top to bottom in sequence.
[0051] Compared with the prior art, the coupled heating spinning method provided by the present invention is that when the rim blank is spun, multiple spray guns 11 spray high-temperature flames into the semi-annular heating chamber 10 and spray them out simultaneously through the upper spray hole and the lower spray hole. The area covered by the flames sprayed from the upper spray hole is the upper heating zone, and the area covered by the flames sprayed from the lower spray hole is the lower heating zone. An overlapping coupled heating zone 17 is formed between the upper heating zone and the lower heating zone to heat the spinning surface 23. By continuously moving the spinning machine upward, the spinning of the rim is completed. The coupled heating spinning method provided by the present invention can use multiple spray guns 11 to cooperate with the semi-annular heating chamber 10 to form a coupled heating zone 17 that completely covers the spinning surface 23, ensuring that the spinning surface 23 of the rim blank is always effectively heated.
[0052] See also Figure 5 In step S2, when the spinning wheel 9 on one side of the mold body moves horizontally to the point where its edge abuts against the upper end of the outer wall of the rim, the contact point between the outer arc end of the spinning wheel 9 and the outer wall of the rim is the reference point. The spinning machine is turned on to drive the rim to rotate for at least one circle. The reference point forms a reference line in the circumferential direction of the outer wall of the rim. Two parallel lines are formed after being offset upward and downward by a distance s based on the reference line. The area between the two parallel lines is the spinning surface 23, s=cota×tana×r, where a is half of the preset angle between the outer arc of the spinning wheel 9 and the spinning surface 23, the value range of a is 10°~20°, and r is the radius of the outer arc end of the spinning wheel 9. At this time, the spinning surface 23 takes the reference line as the center line, and after being offset by s on both sides, a spinning surface 23 with a width of 2s is formed. The spinning surface 23 will change the area relative to the outer peripheral surface of the rim at the same time as the axial movement of the rim, but its width is always 2s.
[0053] In step S2, when setting the preset distance L, L=n×d×k, where n≥5, to prevent the flame ejected from the flame ejection hole of the semi-annular heating chamber 10 from being too close to the rim, and to ensure the heating effect. The value range of k is 1 to 1.3, and the value of k is the melting point coefficient of the aluminum alloy. The k value of the aluminum alloy with a melting point of 650°C is defined as 1. The lower the melting point, the larger the k value, and the higher the melting point, the smaller the k value. The change in the melting point of the aluminum alloy is mainly determined by other alloying elements inside, which will not be repeated here. The value of d is the minimum thickness of the rim in the area where the spinning surface 23 is located. When taking the value of d, the value of d in the spoke area or the edge area usually varies greatly, while the value of d in the middle area of the rim has a relatively small deviation, and is generally based on the lower limit of the d value in the middle area of the rim. In step S3, at a predetermined pressure P, the value range of P is 150 to 250 kgf / mm 2 .
[0054] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A rim forming die, It is characterized in that include: A mold body, the mold body comprising a lower mold (1) and an upper mold (2), the lower mold (1) being mounted on the lower mounting end of a spinning machine, the upper mold (2) being mounted on the upper mounting end of the spinning machine, the lower mold (1) and the upper mold (2) being coaxially arranged and capable of axial relative movement and synchronous movement, a plurality of movable blocks (3) being circumferentially arranged on the upper end surface of the lower mold (1), the outer peripheral surface of the upper mold (2), the outer peripheral surface of the lower mold (1) and the outer peripheral surfaces of the plurality of movable blocks (3) jointly forming an assembly surface adapted to the inner peripheral surface of the rim, the plurality of movable blocks (3) being synchronously moved along the radial direction of the lower mold (1) to respectively form a gathered state for disassembling and assembling the rim and a dispersed state for positioning the rim; A spinning wheel (9), wherein the spinning wheel (9) is arranged on one side of the mold body, the spinning wheel (9) moves horizontally away from the mold body to form a non-working state, and the spinning wheel (9) moves horizontally to abut against the outer peripheral surface of the rim to form a working state, and the contact surface between the spinning wheel (9) and the rim in the working state is defined as a spinning surface (23); A heating component, the heating component comprising a plurality of spray guns (11) and a semi-annular heating chamber (10), the plurality of spray guns (11) being connected to the semi-annular heating chamber (10), the semi-annular heating chamber (10) being coaxially arranged on a side of the mold body away from the spinning wheel (9), the inner side wall of the semi-annular heating chamber (10) being provided with a flame jet hole in accordance with the shape, a partition (12) being horizontally arranged inside the semi-annular heating chamber (10), the partition (12) dividing the inner cavity of the semi-annular heating chamber (10) into an upper chamber (13) and a lower chamber (14), the partition (12) extending to the inner side wall of the semi-annular heating chamber (10) and dividing the flame jet hole from top to bottom into a chamber connected to the upper chamber (13) An upper spray hole and a lower spray hole connected to the lower chamber (14); an upper guide bevel (15) is provided on the upper end surface of the partition (12) close to the inner wall of the semi-annular heating chamber (10); the upper guide bevel (15) is used to guide the flame sprayed from the upper spray hole to spray toward the spinning surface (23); a lower guide bevel (16) is provided on the lower end surface of the partition (12) close to the inner wall of the semi-annular heating chamber (10); the lower guide bevel (16) is used to guide the flame sprayed from the lower spray hole to spray toward the spinning surface (23); the flames sprayed from the upper spray hole and the lower spray hole form an overlapping coupling heating zone (17) on the outer side wall of the rim to cover the spinning surface (23).
2. A rim forming mold as claimed in claim 1, It is characterized in that The lower mold (1) is provided with a plurality of elastic guide components, and the plurality of elastic guide components are connected one by one to the lower ends of the plurality of movable blocks (3). The elastic guide components are inclined outward from top to bottom and have elastic supporting forces along their own axes. The elastic supporting forces of the plurality of elastic guide components gather above the lower mold (1) to form a gathered state, or the plurality of movable blocks (3) are pressed downward by the upper mold (2) to move along the axial direction of the corresponding elastic guide components and are distributed in the circumference of the lower mold (1) to form a dispersed state.
3. A rim forming mold as claimed in claim 2, It is characterized in that The elastic guide assembly comprises a plurality of guide slides and a plurality of top blocks (4), wherein the plurality of guide slides are circumferentially opened on the upper mold (2), the guide slides are inclined outward from top to bottom, and the plurality of top blocks (4) are arranged in the plurality of guide slides in a one-to-one correspondence, and a first elastic member (5) is fixed at the bottom of the guide slide, the upper end of the first elastic member (5) is connected to the corresponding top block (4) and provides an elastic force for the top block (4) to move upward along the guide slide.
4. A rim forming mold as claimed in claim 1, It is characterized in that A top column (6) is arranged inside the lower mold (1), and the top column (6) is coaxially arranged in the middle of the lower mold (1). A plurality of telescopic rods (8) are circumferentially arranged at the upper end of the top column (6). The plurality of telescopic rods (8) are connected to a plurality of movable blocks (3) in a one-to-one correspondence. The telescopic rods (8) shorten or lengthen as the movable blocks (3) are raised or lowered. A second elastic member (7) is connected to the lower end of the top column (6), and the second elastic member (7) is used to provide an elastic force for the top column (6) to move upward.
5. A rim forming mold according to any one of claims 1 to 4, It is characterized in that A filling groove is provided at one end of the outer side of the partition (12); an upper heat insulation sleeve (19) is provided on the upper part of the semi-annular heating chamber (10) from the outside to the inside, and a lower heat insulation sleeve (20) is provided on the lower part of the semi-annular heating chamber (10) from the outside to the inside. The bottom heat insulation layer of the upper heat insulation sleeve (19) and the top heat insulation layer of the lower heat insulation sleeve (20) are respectively pressed into the filling groove; the upper heat insulation sleeve (19) covers an area of not less than 80% of the top of the semi-annular heating chamber (10), and the lower heat insulation sleeve (20) covers an area of not less than 80% of the lower part of the semi-annular heating chamber (10).
6. A rim forming mold according to any one of claims 1 to 4, It is characterized in that A plurality of upper connecting tubes (21) are arranged at equal angles on the upper part of the outer wall of the semi-annular heating chamber (10), and the plurality of upper connecting tubes (21) are all connected to the upper chamber (13); a plurality of lower connecting tubes are arranged at equal angles on the lower part of the outer wall of the semi-annular heating chamber (10), and the plurality of lower connecting tubes are all connected to the lower chamber (14); the plurality of upper connecting tubes (21) and the plurality of lower connecting tubes are alternately arranged on the outer periphery of the semi-annular heating chamber (10), and the plurality of upper connecting tubes (21) and the plurality of lower connecting tubes are all connected to the plurality of spray guns (11) in a one-to-one correspondence.
7. A rim forming mold according to any one of claims 1 to 4, It is characterized in that The arc of the semi-annular heating chamber (10) is not less than 60°, and the distance between the inner side wall of the semi-annular heating chamber (10) and the inner side wall of the rim is not less than 5 times the thickness of the rim wall.
8. A coupled heating spinning method, It is characterized in that The rim forming mold according to any one of claims 1 to 7 comprises the following steps: S1: The rim is sleeved on the lower die (1) of the spinning machine from top to bottom, the upper die (2) of the spinning machine moves downward to close the die, the upper die (2) presses a plurality of movable blocks (3) downward, and the plurality of movable blocks (3) move downward and expand radially outward to support the circumference of the inner wall of the rim; S2: The spinning wheel (9) on one side of the mold body moves horizontally until its edge abuts against the upper end of the outer wall of the rim, and the semi-annular heating chamber (10) on the other side of the mold body moves toward the side close to the rim, and the inner side of the semi-annular heating chamber (10) reaches a preset distance L from the upper end of the outer wall of the rim, and a plurality of spray guns (11) are respectively connected to the semi-annular heating chamber (10); S3: Turn on the spinning machine, which drives the rim to rotate, applies a predetermined pressure P to the spinning wheel (9) on one side of the rim and forms a spinning surface (23) with the contact surface of the rim, turns on multiple spray guns (11), and sprays high-temperature flames into the semi-annular heating chamber (10) and sprays them out through the upper spray hole and the lower spray hole at the same time. The area covered by the flame sprayed from the upper spray hole is the upper heating zone, and the area covered by the flame sprayed from the lower spray hole is the lower heating zone. An overlapping coupling heating zone (17) is formed between the upper heating zone and the lower heating zone to heat the spinning surface (23); S4: The spinning machine drives the rim to rotate and move the rim upwards at the same time, and the spinning wheel (9) completes the spinning of the rim from top to bottom in sequence.
9. The coupled heating spinning method according to claim 8, It is characterized in that In step S2, when the spinning wheel (9) on one side of the mold body moves horizontally until its edge abuts against the upper end of the outer wall of the rim, the contact point between the outer arc end of the spinning wheel (9) and the outer wall of the rim is used as the reference point, the spinning machine is turned on to drive the rim to rotate for at least one circle, and the reference point forms a reference line in the circumferential direction of the outer wall of the rim. Two parallel lines are formed after being offset upward and downward by a distance s based on the reference line. The area between the two parallel lines is the spinning surface (23), s=cota×tana×r, wherein a is half of the preset angle between the outer arc of the spinning wheel (9) and the spinning surface (23), the value range of a is 10°~20°, and r is the radius of the outer arc end of the spinning wheel (9).
10. The coupled heating spinning method according to claim 8, It is characterized in that In step S2, when the preset distance L is set, L=n×d×k, wherein n≥5, the value range of k is 1 to 1.3, and the value of d is the minimum thickness of the rim in the area where the spinning surface (23) is located; in step S3, when the predetermined pressure P is set, the value range of P is 150 to 250 kgf / mm 2 .