Micro injection molding integrated testing machine for metal-plastic interface coated workpiece
By integrating a micro temperature/pressure sensor and a mechanical/ultrasonic vibration system into the metal-plastic interface coating testing machine, the problem of in-mold parameter detection in the existing technology is solved, and the coating area is continuously adjustable and the testing efficiency is improved. Optimized the metal-plastic interface coating effect.
Patent Information
- Application Number
- CN202411066678.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-08-06
AI Technical Summary
The existing technology is difficult to effectively control and detect the pressure, temperature and vibration in the mold during the metal-plastic interface coating test, resulting in complex research, high cost and difficulty in optimizing the coating effect.
A micro-injection molding integrated testing machine for metal-plastic interface coated parts is designed, which integrates a high-precision micro temperature/pressure sensor and a mechanical/ultrasonic vibration system to monitor and adjust the temperature, pressure and vibration parameters during the injection molding process. Optimize the metal-plastic interface coating effect.
It achieves continuous adjustment of the coating area, improves experimental efficiency and sample preparation efficiency, reduces costs, and can simultaneously study the effects of temperature, pressure and vibration on the interface bonding form and bonding strength.
Smart Images

Figure CN118769495A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of injection molding, and in particular to a micro-injection molding integrated testing machine for metal-plastic interface coated parts. Background Art
[0002] Insert molding is an advanced plastic processing technology. Its basic principle is to pre-fix one or more auxiliary materials (metal, plastic or ceramic parts) in the injection mold, and then inject molten plastic material to cover and fix the insert. After the mold is opened, the insert is wrapped by the cooled and solidified plastic to form a composite part. In the secondary processing and subsequent use scenarios of metal-plastic parts, such as stamping, cutting, long-term operation of parts in high temperature environment, radiation environment and cyclic load, the composite parts will fail due to interface separation. At present, the samples used for metal-plastic interface coating are prone to the situation that the interface is not damaged but the plastic breaks first during testing. Different molds need to be replaced according to different coating areas for different plastics. The research process is complicated, difficult and costly. At the same time, the only controllable variables are temperature, pressure and the difference in the types of plastic and metal, ignoring the influence of other factors on the metal-plastic interface coating. So far, there are no reports at home and abroad on the metal-plastic interface coating test device for injection molding that integrates in-mold pressure detection, in-mold temperature detection and in-mold vibration. Summary of the invention
[0003] In view of the deficiencies in the prior art, the present invention provides a micro-injection molding integrated testing machine for metal-plastic interface coated parts. The integrated testing machine accurately monitors the temperature / pressure parameters of the molding process by setting high-precision micro-temperature / pressure sensors in the mold cavity, thereby avoiding the error between the machine setting temperature / pressure and the actual data caused by the dissipation of energy during the molding process. The obtained data is more conducive to the accurate analysis of the metal-plastic interface coating effect; the in-mold mechanical / ultrasonic vibration system applies high-frequency / low-frequency combined vibration to the polymer melt flowing through the flow channel during the molding process, thereby improving the metal-plastic interface coating effect by affecting the uniformity and microstructure of the polymer melt. This testing machine can be used to study the influencing factors and optimization methods of the interface coating of metal-plastic composite parts under the injection molding process. The specific technical scheme is as follows:
[0004] A micro-injection integrated testing machine for metal-plastic interface coated parts, comprising a testing machine mold, and an in-mold pressure and temperature detection system, an ultrasonic vibration system and a mechanical vibration system integrated in the testing machine mold;
[0005] The testing machine mold comprises a fixed mold bottom plate, a fixed mold plate, a front mold core, a rear mold core, a movable mold plate, an upper ejector plate, a square iron, a lower ejector plate, an ejector, and a movable mold bottom plate; a flow channel is arranged in the middle of the fixed mold plate and the movable mold plate after the mold is closed;
[0006] The ultrasonic vibration system and the mechanical vibration system are arranged relatively between the fixed platen and the movable platen;
[0007] The rear mold core is provided with a metal-plastic sample cavity and a standard tensile sample cavity at the same time. The metal-plastic sample cavity is provided with an ejector pin hole, a raised pad, a sample metal part positioning block and a tail positioning pin. The raised pad is used to support the metal part of the metal-plastic interface coated part so that the melt can coat the metal part; the sample metal part positioning block is used to limit the metal part of the metal-plastic interface coated part in the width direction, and the tail positioning pin is installed at the tail of the metal-plastic sample cavity and is used to limit the metal part of the metal-plastic interface coated part in the length direction;
[0008] The in-mold pressure and temperature detection system includes an in-mold temperature sensor 1, an in-mold temperature sensor 2, an in-mold temperature sensor 3, an in-mold pressure sensor 1, an in-mold pressure sensor 2, an in-mold pressure sensor 3, a data connector, a precision calibrator and a data acquisition terminal; the in-mold temperature sensor 1, the in-mold temperature sensor 2, the in-mold temperature sensor 3 and the in-mold pressure sensor 3 are all installed on the front mold core, the in-mold pressure sensor 1 and the in-mold pressure sensor 2 are installed on the rear mold core, and the in-mold temperature sensor 1 and the in-mold temperature sensor 2 are arranged at different points of the flow channel on the cavity side of the standard tensile specimen, and are used to measure the temperature changes at different distances from the glue inlet in the flow channel; the in-mold temperature sensor 3 is arranged at the metal-plastic specimen The pressure sensor 1 and the pressure sensor 2 are arranged at different points of the flow channel on one side of the standard tensile specimen cavity, the pressure sensor 1 corresponds to the position of the in-mold temperature sensor 1, the pressure sensor 2 corresponds to the position of the in-mold temperature sensor 2, the pressure sensor 3 is fixed in the metal-plastic specimen cavity, and is symmetrically arranged with the temperature sensor 3 to monitor the pressure state in the metal-plastic specimen cavity; each sensor is connected to the data connector, the precision calibrator and the data acquisition terminal in sequence through a single-line cable, and the data acquisition terminal organizes and analyzes the collected temperature or pressure data to provide process optimization suggestions.
[0009] Furthermore, the testing machine mold also includes a mechanical vibration guide block and an ultrasonic vibration guide block, which are relatively arranged and fixed on the rear mold core; the flow channel is located between the mechanical vibration guide block and the ultrasonic vibration guide block.
[0010] Furthermore, sensor fixing holes are provided on the fixed mold plate, front mold core, movable mold plate and rear mold core, and sensor pressure plates are fixedly connected to the fixed mold plate and the movable mold plate, and the axial movement of all in-film temperature sensors and pressure sensors is limited by the front mold core, rear mold core and the sensor pressure plate.
[0011] Furthermore, the mechanical vibration system includes a voice coil motor, a sleeve, a connecting rod and a mechanical vibration block, the voice coil motor is placed in the sleeve, the voice coil motor is fixedly connected to the connecting rod, and the connecting rod is cooperatively connected to the mechanical vibration block arranged near the flow channel in the mold cavity; the sleeve and the voice coil motor are fixedly connected to the surface of the testing machine mold; the mechanical vibration block maintains stable axial motion through the mechanical vibration guide blocks fixed on both sides, and applies low-frequency and high-amplitude vibration to the melt flowing through the flow channel.
[0012] Furthermore, the ultrasonic vibration system includes an ultrasonic vibration generator, a gasket, a fixed block and an ultrasonic vibration block connected in sequence, the fixed block is fixed on the surface of the testing machine mold, the ultrasonic vibration block is fixedly connected to the ultrasonic vibration generator, and the ultrasonic vibration block is arranged near the flow channel in the mold cavity, symmetrically with the mechanical vibration block, and applies high-frequency and low-amplitude vibration to the melt flowing through the flow channel.
[0013] Furthermore, in the testing machine mold, the fixed mold plate is fixed on the fixed mold bottom plate, the front mold core is fixed on the fixed mold plate, the rear mold core is fixed on the movable mold plate, the upper ejector plate and the lower ejector plate are fixed together, the ejector is fixed between the upper ejector plate and the lower ejector plate, and passes through the movable mold plate upward; the square iron is fixed between the movable mold plate and the movable mold bottom plate.
[0014] The beneficial effects of the present invention are as follows:
[0015] 1. The micro-injection molding integrated testing machine for metal-plastic interface coated parts provided by the present invention realizes continuous adjustment of the coating area within a certain range by changing the length of the metal insert extending into the plastic during the injection molding process. It can be used for testing the interface coating strength, interface damage form, etc. of various materials under the injection molding process, thereby improving the experimental efficiency and reducing the cost of sample production.
[0016] 2. The micro-injection molding integrated testing machine for metal-plastic interface coated parts provided by the present invention can simultaneously prepare heterogeneous interface coated specimens and pure plastic tensile specimens, thereby improving the sample preparation efficiency. Moreover, the two specimens are prepared simultaneously in the same set of molds, which is conducive to controlling variables.
[0017] 3. The present invention can be used to study the action mechanism of vibration, temperature and pressure on the plastic-metal interface bonding form and interface bonding strength under injection molding process conditions by integrating an in-mold temperature detection system, an in-mold pressure detection system, a mechanical vibration system and an ultrasonic vibration system in a testing machine. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a schematic diagram of the structure of the metal-plastic interface coating specimen.
[0019] Figure 2 This is the overall schematic diagram of the testing machine.
[0020] Figure 3 This is the main cross-sectional view of the testing machine.
[0021] Figure 4 Exploded view of the testing machine mold core.
[0022] Figure 5 This is a schematic diagram of the sensor fixing structure of the testing machine.
[0023] Figure 6 Schematic diagram of sensor distribution.
[0024] Figure 7 This is a schematic diagram of the sensor interface.
[0025] Figure 8 This is a schematic diagram showing the arrangement of the ultrasonic vibration system 4 and the mechanical vibration system 5.
[0026] Fig. 9 It is a schematic diagram of the principle of the in-mold pressure and temperature detection system 3.
[0027] Fig.10 Schematic diagram of the mechanical vibration system structure.
[0028] Fig.11 Schematic diagram of the installation position of the mechanical vibration guide block.
[0029] Fig.12 This is a schematic diagram of the ultrasonic vibration system structure.
[0030] In the figure, the test specimen 1, the test machine mold 2, the in-mold pressure and temperature detection system 3, the ultrasonic vibration system 4, the mechanical vibration system 5; 101-plastic part, 102-metal part, 103-standard tensile specimen; 201-fixed mold bottom plate, 202-fixed mold plate, 203-front mold core, 204-flow channel, 205-rear mold core, 206-movable mold plate, 218-upper ejector plate, 207-square iron, 208-lower ejector plate, 209-movable mold bottom plate, 210-standard tensile specimen cavity, 211-ejector, 212-sensor pressure plate, 213-sensor wiring groove, 214-specimen metal part tail shaped positioning pin, 215-specimen metal part positioning block, 216- 6- ejector hole, 217- raised pad, 219- ultrasonic vibration guide block, 220- sensor fixing hole, 221- mechanical vibration guide block; the in-mold pressure / temperature detection system includes: 301- temperature sensor 1, 302- temperature sensor 2, 303- data connector, 304- precision calibrator, 305- data acquisition terminal, 306- pressure sensor 1, 307- pressure sensor 2, 308- temperature sensor 3, 309- pressure sensor 3; 401- ultrasonic vibration generating rod, 402- washer, 403- fixing block, 404- ultrasonic vibration block; 501- sleeve, 502- voice coil motor, 503- connecting rod, 504- mechanical vibration block. DETAILED DESCRIPTION
[0031] The present invention will be described in detail below according to the accompanying drawings and preferred embodiments, and the purpose and effect of the present invention will become more clear. The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0032] As shown in the figure, the test specimen and testing machine system for studying metal-plastic interface coating under injection molding process of the present invention includes a test specimen, a testing machine mold, an in-mold pressure detection system, an in-mold temperature detection system, a mechanical vibration system, and an ultrasonic vibration system;
[0033] like Figure 1As shown, sample 1 includes a tensile specimen 103 of GB / T 37426-2019 standard and a metal-plastic interface coating specimen. The metal-plastic interface coating specimen consists of a metal part 102 and a plastic part 101. The front end of the metal part 102 is wrapped by the plastic part 101. A symmetrical circular hole 104 with a radius of 1 mm is opened at the exposed end of the metal part 102, which is used to position and fix the metal part 102 when preparing the metal-plastic interface coating specimen in the testing machine. The metal part 102 has different lengths to choose from, and the length of the metal-plastic bonding part is adjusted accordingly. By adjusting the length of the metal insert, the metal-plastic coating area can be continuously adjusted. The sample is provided with a U-shaped groove of about 7 mm long and about 1 mm wide on both sides of the junction of the metal and the plastic, which is used to fix the metal insert so that it does not displace or bend when the polymer melt is filled into the mold. Different lengths of inserts can be selected for different materials to avoid the situation where the plastic strength is lower than the bonding surface strength and the experimental purpose cannot be achieved, and to ensure that the metal-plastic bonding surface is destroyed in the subsequent tensile test of the metal-plastic interface coated specimen, and the stress-strain curve of the specimen is obtained to observe the microscopic scale of the destroyed interface.
[0034] like Figure 2 , 3 As shown in , 4, the test machine mold 2 includes a fixed mold base plate 201, a fixed mold plate 202, a front mold core 203, a runner 204, a rear mold core 205, a movable mold plate 206, an upper ejector plate 218, an ejector 211, a square iron 207, a lower ejector plate 208, a movable mold base plate 209, an ultrasonic vibration guide block 219, a mechanical vibration guide block 221, an in-mold temperature detection system, an in-mold pressure detection system, a mechanical vibration system 5, and an ultrasonic vibration system 4. The fixed mold plate 202 is fixed on the fixed mold base plate 201, the front mold core 203 is fixed on the fixed mold plate 202, the rear mold core 205 is fixed on the movable mold plate 206, the upper ejector plate 218 and the lower ejector plate 208 are fixed together by bolts, and the ejector 211 is fixed between the upper ejector plate 218 and the lower ejector plate 208, and passes through the movable mold plate 206 upward. The square iron 207 is fixed between the movable mold plate 206 and the movable mold base plate 209.
[0035] like Figure 3 As shown, the mechanical vibration system 5 and the ultrasonic vibration system 4 are relatively installed between the fixed plate 202 and the movable plate 206. Figure 4 and 5 As shown, the in-mold temperature sensor 1 301, the in-mold temperature sensor 2 302, the in-mold temperature sensor 3 308 and the in-mold pressure sensor 1 306, the in-mold pressure sensor 2 307, the in-mold pressure sensor 3 309 are fixed on the front mold core 203 and the rear mold core 205 respectively. Figure 4It can be seen that in this embodiment, the in-mold temperature sensor 1 301, the in-mold temperature sensor 2 302, the in-mold temperature sensor 3 308 and the in-mold pressure sensor 3 309 are all installed on the front mold core 203, and the in-mold pressure sensor 1 306 and the in-mold pressure sensor 2 307 are installed on the rear mold core 205.
[0036] The rear mold core 205 is provided with a metal-plastic sample cavity and a standard tensile sample cavity 210. The metal-plastic sample cavity is provided with a pinhole 216, a raised pad 217, a sample metal part positioning block 215 and a tail positioning pin 214. The ultrasonic vibration guide block 219 and the mechanical vibration guide block 221 are arranged opposite to each other and are both fixed on the rear mold core 205. The flow channel 204 is located between the mechanical vibration guide block 221 and the ultrasonic vibration guide block 219. The raised pad 217 is used to support the metal part of the metal-plastic interface coated part so that the melt can coat the metal part to form a metal insert. The sample metal part positioning block 215 is used to limit the metal part of the metal-plastic interface coated part in the width direction; the tail positioning pin 214 is installed at the tail of the metal-plastic sample cavity, and is used to limit the metal part of the metal-plastic interface coated part in the length direction. Figure 6 As shown, the fixed mold plate 202, the front mold core 203, the movable mold plate 206, and the rear mold core 205 are all provided with sensor fixing holes 220. The axial movement of the temperature sensor and the pressure sensor in the membrane is limited by the front mold core 203, the rear mold core 205 and the sensor pressure plate 212, thereby achieving the fixation of the sensors.
[0037] like Figures 7 to 9 As shown, in order to realize temperature and pressure measurement, the in-mold pressure and temperature detection system 3 includes a temperature detection unit and a pressure detection unit. In addition to the in-mold temperature sensor 1 301, the in-mold temperature sensor 2 302, the in-mold temperature sensor 3 308 and the in-mold pressure sensor 1 306, the in-mold pressure sensor 2 307, and the in-mold pressure sensor 3 309, the temperature detection unit also includes a data connector 303 connected by a single-line cable, a precision calibrator 304, and a data acquisition terminal 305. Figure 7As shown, temperature sensor 1 301 and temperature sensor 2 307 are arranged at different points on the flow channel of the standard sample side, and are used to measure the temperature changes at different distances from the glue inlet in the flow channel. Temperature sensor 3 308 is arranged in the metal-plastic sample mold cavity, and is used to monitor the temperature state in the mold cavity. Pressure sensor 1 306 and pressure sensor 2 307 are arranged at different points on the flow channel of the standard sample side, and pressure sensor 3 309 is fixed in the mold cavity on the metal-plastic interface coated spline side, and is arranged symmetrically with temperature sensor 3 308, and is used to monitor the pressure state in the mold cavity. The pressure sensor arrangement points correspond one-to-one with the temperature sensor points, and are used to measure the pressure changes at different distances from the glue inlet in the flow channel. Temperature sensors and pressure sensors are arranged at the same point at the same time, so as to achieve the purpose of simultaneously monitoring the temperature and pressure data of the same point. The sensor probe has a diameter of 1 mm, is flush with the inner surface of the mold cavity and directly contacts the melt. The collected temperature and pressure data are transmitted to the data acquisition terminal 305 through a single-line connection cable and a matching multi-channel data connector 303, and then through a matching precision calibrator 304. The data acquisition terminal 305 organizes and analyzes the acquired data and gives process optimization suggestions.
[0038] like Fig.10 As shown, the mechanical vibration system 5 includes a voice coil motor 502, a sleeve 501, a connecting rod 503, and a mechanical vibration block 504. The voice coil motor 502 is placed in the sleeve 501 and connected to the connecting rod 503 by bolts. The connecting rod 503 is connected to the mechanical vibration block 504 set in the mold cavity. The sleeve 501 and the voice coil motor 502 are fixed to the mold surface by bolts. Fig.11 As shown, the mechanical vibration block 504 maintains stable axial motion through the mechanical vibration guide blocks 221 fixed on both sides, and the mechanical vibration block 504 is arranged near the flow channel 204. Fig.12 As shown, the ultrasonic vibration system 4 includes an ultrasonic vibration generator 401, a gasket 402, a fixed block 403, and an ultrasonic vibration block 404 connected in sequence. The fixed block 403 is fixed on the mold surface by matching and threading. The ultrasonic vibration block 404 is threadedly connected to the ultrasonic vibration generator 401. The ultrasonic vibration block 404 is arranged near the flow channel 204 in the mold cavity, symmetrically with the mechanical vibration block 504, and the ultrasonic vibration generator 401 is connected to an external power supply and a controller. The ultrasonic vibration system 4 and the mechanical vibration system 5 are symmetrically distributed on both sides of the flow channel 204, and two-dimensional composite vibrations are applied to the melt flowing through the flow channel 204. The mechanical vibration system 5 applies low-frequency and high-amplitude vibrations to the polymer melt flowing through the flow channel, which can accelerate the process of polymer disentanglement; the ultrasonic vibration system 4 applies high-frequency and low-amplitude vibrations to the polymer melt flowing through the flow channel 204, which can cause the polymer to have an overall orientation. The two can be applied simultaneously or separately, and the heterogeneous coating interface is affected by the disentanglement and overall orientation of the polymer chain.
[0039] The working process of the metal-plastic interface coating testing machine of the present invention is as follows:
[0040] S1: Heat the temperature of the test machine mold 2 to 90-110°C;
[0041] S2: Start the mechanical vibration system 5 and the ultrasonic vibration system 4, and set the vibration amplitude and vibration frequency respectively;
[0042] S3: Connect the in-mold pressure and temperature detection system 3 to the data acquisition terminal to calibrate the current temperature and pressure;
[0043] S4: Adjust the process parameters of the injection molding machine, taking the polymer material LCP VT94HT as an example, such as: injection speed 180mm / s, holding time 0.5s, melt temperature 345℃, holding pressure 50MPa, etc., place the insert and set it to semi-automatic mode;
[0044] S5: close the mold and start the injection molding process. After the injection and pressure holding stages are completed, open the mold to take out the sample to check whether the sample is normal and usable, and whether the in-mold pressure and temperature detection system 3, mechanical vibration system 5, and ultrasonic vibration system 4 are working normally. After checking that everything is correct, turn on the full automatic mode;
[0045] S6: After orthogonal tests on process parameters such as injection speed (150-180 mm / s), holding time (0.3-0.8 s), melt temperature (300-345 ° C), holding pressure (30-80 MPa) and external vibration conditions, tensile tests were performed on the interface coated samples and pure plastic samples to obtain the stress-strain curves of the samples. At the same time, the fracture of the sample was placed on a scanning electron microscope (SEM) to observe the microscopic morphology of the port surface and compared with the incision made manually at the coating;
[0046] S7: Evaluate the quality of the interface coating based on the test and microscopic characterization results, and combine the test variables to establish a material parameter-process parameter-external condition-actual parameter-coating quality database. Use deep learning methods to train the data and determine the influencing factors of each factor to provide support for subsequent experiments, and repeat this cycle. Finally, the model can give the optimal injection molding machine process parameters based on material parameters, actual process parameters and external conditions with the goal of optimizing the metal-plastic interface coating quality.
[0047] Those skilled in the art can understand that the above are only preferred examples of the invention and are not intended to limit the invention. Although the invention is described in detail with reference to the above examples, those skilled in the art can still modify the technical solutions recorded in the above examples or replace some of the technical features therein with equivalents. Any modification, equivalent replacement, etc. made within the spirit and principle of the invention shall be included in the protection scope of the invention.
Claims
1. A micro-injection molding integrated testing machine for metal-plastic interface coated parts, characterized in that: It includes a testing machine mold, and an in-mold pressure and temperature detection system, an ultrasonic vibration system and a mechanical vibration system integrated in the testing machine mold; The testing machine mold comprises a fixed mold bottom plate, a fixed mold plate, a front mold core, a rear mold core, a movable mold plate, an upper ejector plate, a square iron, a lower ejector plate, an ejector, and a movable mold bottom plate; a flow channel is arranged in the middle of the fixed mold plate and the movable mold plate after the mold is closed; The ultrasonic vibration system and the mechanical vibration system are arranged relatively between the fixed platen and the movable platen; The rear mold core is provided with a metal-plastic sample cavity and a standard tensile sample cavity at the same time. The metal-plastic sample cavity is provided with an ejector pin hole, a raised pad, a sample metal part positioning block and a tail positioning pin. The raised pad is used to support the metal part of the metal-plastic interface coated part so that the melt can coat the metal part; the sample metal part positioning block is used to limit the metal part of the metal-plastic interface coated part in the width direction, and the tail positioning pin is installed at the tail of the metal-plastic sample cavity and is used to limit the metal part of the metal-plastic interface coated part in the length direction; The in-mold pressure and temperature detection system includes an in-mold temperature sensor 1, an in-mold temperature sensor 2, an in-mold temperature sensor 3, an in-mold pressure sensor 1, an in-mold pressure sensor 2, an in-mold pressure sensor 3, a data connector, a precision calibrator and a data acquisition terminal; the in-mold temperature sensor 1, the in-mold temperature sensor 2, the in-mold temperature sensor 3 and the in-mold pressure sensor 3 are all installed on the front mold core, the in-mold pressure sensor 1 and the in-mold pressure sensor 2 are installed on the rear mold core, and the in-mold temperature sensor 1 and the in-mold temperature sensor 2 are arranged at different points of the flow channel on the cavity side of the standard tensile specimen, and are used to measure the temperature changes at different distances from the glue inlet in the flow channel; the in-mold temperature sensor 3 is arranged at the metal-plastic specimen The pressure sensor 1 and the pressure sensor 2 are arranged at different points of the flow channel on one side of the standard tensile specimen cavity, the pressure sensor 1 corresponds to the position of the in-mold temperature sensor 1, the pressure sensor 2 corresponds to the position of the in-mold temperature sensor 2, the pressure sensor 3 is fixed in the metal-plastic specimen cavity, and is symmetrically arranged with the temperature sensor 3 to monitor the pressure state in the metal-plastic specimen cavity; each sensor is connected to the data connector, the precision calibrator and the data acquisition terminal in sequence through a single-line cable, and the data acquisition terminal organizes and analyzes the collected temperature or pressure data to provide process optimization suggestions.
2. The micro-injection molding integrated testing machine for metal-plastic interface coated parts according to claim 1 is characterized in that: The testing machine mold also includes a mechanical vibration guide block and an ultrasonic vibration guide block, which are arranged relatively to each other and are fixed on the rear mold core; the flow channel is located between the mechanical vibration guide block and the ultrasonic vibration guide block.
3. The micro-injection molding integrated testing machine for metal-plastic interface coated parts according to claim 1, characterized in that: The fixed mold plate, front mold core, movable mold plate and rear mold core are all provided with sensor fixing holes, and the fixed mold plate and movable mold plate are fixedly connected with sensor pressure plates, and the axial movement of all the in-film temperature sensors and pressure sensors is limited by the front mold core, rear mold core and the sensor pressure plate.
4. The micro-injection molding integrated testing machine for metal-plastic interface coated parts according to claim 2, characterized in that: The mechanical vibration system includes a voice coil motor, a sleeve, a connecting rod and a mechanical vibration block. The voice coil motor is placed in the sleeve, the voice coil motor is fixedly connected to the connecting rod, and the connecting rod is cooperatively connected to the mechanical vibration block arranged near the flow channel in the mold cavity; the sleeve and the voice coil motor are fixedly connected to the surface of the testing machine mold; the mechanical vibration block 504 maintains stable axial movement through the mechanical vibration guide blocks fixed on both sides, and applies low-frequency and high-amplitude vibration to the melt flowing through the flow channel.
5. The micro-injection molding integrated testing machine for metal-plastic interface coated parts according to claim 4, characterized in that: The ultrasonic vibration system includes an ultrasonic vibration generator, a gasket, a fixed block and an ultrasonic vibration block connected in sequence, the fixed block is fixed on the surface of the testing machine mold, the ultrasonic vibration block is fixedly connected to the ultrasonic vibration generator, and the ultrasonic vibration block is arranged near the flow channel in the mold cavity, symmetrically with the mechanical vibration block, and applies high-frequency and low-amplitude vibration to the melt flowing through the flow channel.
6. The micro-injection molding integrated testing machine for metal-plastic interface coated parts according to claim 4, characterized in that: In the testing machine mold, the fixed mold plate is fixed to the fixed mold bottom plate, the front mold core is fixed to the fixed mold plate, the rear mold core is fixed to the movable mold plate, the upper ejector plate and the lower ejector plate are fixed together, the ejector is fixed between the upper ejector plate and the lower ejector plate, and passes through the movable mold plate upward; the square iron is fixed between the movable mold plate and the movable mold bottom plate.
Citation Information
Patent Citations
Testing machine with broadband amplitude vibration test / rheological measurement integrated function
CN114633448A
Micro injection mold with mechanical and ultrasonic composite vibration function
CN116352957A
Micro injection mold of adjustable-amplitude combined variable-angle vibration runner structure
CN116852655A
Using ultrasound in injection molding cavities, comprises directing ultrasound at critical cavity points using a system comprising a transducer, booster and a sonotrode
DE10153706A1
Apparatus for controlling gas assisted injection molding to produce hollow and non-hollow plastic parts and modify their physical characteristics