Composite material and preparation method thereof

By pre-treating the copper-aluminum composite material, adding emulsion and silicon powder layers, and performing composite rolling and forging annealing treatments, the problems of high process complexity, high cost and low bonding quality in the existing technology are solved, achieving Provides more efficient substrate bonding and improved conductivity.

CN118769664AInactive Publication Date: 2024-10-15CHONGQING COLLEGE OF ELECTRONICS ENG
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410844073.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing copper-aluminum composite material preparation methods have problems such as high process complexity, high cost, low safety, and low base material bonding quality.

Method used

By pre-treating the base material to form multiple protrusions, adding emulsion and silicon powder layers, using a roller mill to perform 50-60% composite rolling, and performing at least one forging and annealing treatment to form a mortise and tenon interlocking structure. Improve bonding quality.

Benefits of technology

It reduces process complexity and cost, improves the coordinated deformation and bonding quality between substrates, avoids high temperatures and noise, and enhances the conductivity and structural stability of the material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118769664A_ABST
    Figure CN118769664A_ABST
Patent Text Reader

Abstract

The preparation method of the composite material disclosed by the invention comprises the following steps: during manufacturing, firstly, pre-treating a base material needing to be compounded, so that a plurality of bulges are formed on the bonding surface of the base material needing to be compounded; then, the multiple layers of base materials are stacked in sequence, and emulsion is added between every two adjacent combination faces; carrying out composite rolling on the multi-layer laminated base material pile through a rolling mill at a pressing rate of 50-60%; forging and pressing the integrally compounded composite material for at least one time; and finally, the forged and pressed composite material is subjected to annealing treatment. According to the method, the process complexity can be reduced, the input cost can be reduced, the safety can be improved, and meanwhile, coordinated deformation between the base materials can be realized, so that the overall bonding quality of the manufactured composite material can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of composite materials, and in particular to a copper-aluminum composite material and a preparation method thereof. Background Art

[0002] Composite materials refer to a material composed of two or more metals or other materials with suitable properties, such as bimetallic strips. Bimetallic strips are also called thermal bimetallic strips. Since the thermal expansion coefficients of the component layers are different, when the temperature changes, the deformation of the active layer is greater than that of the passive layer, so the entire bimetallic strip will bend toward the passive layer, and the curvature of the composite material will change, resulting in deformation.

[0003] Copper-aluminum composite material refers to a multi-layer composite plate made of copper and aluminum. It is a copper-aluminum composite material with composite, layered and metal-metal bonding made by multiple rolling.

[0004] In the prior art, the following methods are usually used to prepare copper-aluminum composite materials: friction welding, flash welding, and explosion welding. Specifically:

[0005] 1) Friction welding: expensive equipment, complex tooling design, difficult to predict welding quality, and high requirements for equipment and operators;

[0006] 2) Flash welding: Flash welding requires heating, which will change the properties of metal materials. The equipment cost of flash welding is high, and special equipment and technology are required. For metal materials with small plate thickness and high hardness, the effect is not good, the requirements for operators are high, and it is easy to inhale harmful gases and cause eye damage.

[0007] 3) Explosion welding method: It generates impact force and noise, which can easily cause damage to the surrounding environment and equipment. The impact force and thermal deformation generated during the explosion can cause deformation and cracking of the material. Due to the high risk of explosion, special protective measures need to be taken, which places high demands on operators.

[0008] At the same time, these three methods also have the problem of low bonding quality between the welded composite material substrates. Summary of the invention

[0009] In view of the deficiencies in the prior art, the technical problem to be solved by the present invention is to provide a composite material and a preparation method thereof, which can reduce process complexity, reduce investment costs, and improve safety, while enabling coordinated deformation between substrates, thereby improving the overall bonding quality of the composite material.

[0010] In order to achieve the above object, the present invention is implemented by the following technical scheme: a method for preparing a composite material, comprising: pre-treating a substrate to be composited so that a plurality of protrusions are formed on the bonding surface of the substrate to be composited;

[0011] stacking multiple layers of the substrate in sequence and adding an emulsion between two adjacent bonding surfaces;

[0012] After the multi-layer stack is stacked, the substrate stack is subjected to composite rolling with a pressing rate of 50-60% by a rolling mill;

[0013] Forging the composite material combined into one piece at least once;

[0014] The composite material after forging is subjected to annealing treatment.

[0015] Furthermore, the pretreatment also includes grinding the bonding surface of the substrate and cleaning it after grinding.

[0016] Furthermore, the protrusion is formed by a single synchronous rolling process with a rolling mill having a pressing rate of 50%.

[0017] Furthermore, the protrusion has a shape that can be easily inserted into and locked in the combining surface to be combined with it.

[0018] Furthermore, the size of the root of the protrusion is larger than the size of the top, and the top of the protrusion is inclined toward the forward or backward direction of the roller shaft.

[0019] Furthermore, the protrusions include longitudinal ribs parallel to the roller axis direction, or transverse ribs perpendicular to the roller axis direction, or the transverse ribs and the longitudinal ribs are staggered to form a grid state.

[0020] Furthermore, the protrusions are a plurality of protrusions.

[0021] Furthermore, a silicon powder layer is added between two adjacent bonding surfaces.

[0022] Furthermore, the amount of the silicon powder layer is 2-4% of the sum of the masses of the two adjacent substrates to be composited.

[0023] A composite material, a composite material prepared by the method.

[0024] Beneficial effects of the present invention:

[0025] The preparation method of the composite material has the following advantages:

[0026] 1. It can reduce process complexity and equipment investment cost;

[0027] 2. No heating is required during the processing, which can avoid changes in the properties of the metal substrate. At the same time, it can avoid the generation of harmful gases due to high heat and avoid damage to the operator's eyes due to high light;

[0028] 3. It can avoid the impact and noise, which may cause damage to the surrounding environment, equipment and other equipment;

[0029] 4. Multiple protrusions are formed on the bonding surface of the substrate. During the rolling and compounding process, the mortise and tenon interlocking structure can accelerate the rupture of the interface hardened layer, and a large amount of new metal is squeezed out from it, forcing the coordinated deformation between the two substrates to improve the overall bonding quality;

[0030] 5. The emulsion can form a lubricating film on the surface of the substrate, which can reduce the probability of scratches, wear and other adverse conditions on the surface of the substrate, thereby improving the quality of the substrate.

[0031] The composite material prepared by the above composite material method has good composite effect and stable structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the specific implementation of the present invention, the following will briefly introduce the drawings required for use in the specific implementation. In all the drawings, each element or part is not necessarily drawn according to the actual scale.

[0033] Figure 1 A schematic diagram of a method for preparing a composite material provided by one embodiment of the present invention;

[0034] Figure 2 A schematic diagram of a substrate with protrusions pressed thereon;

[0035] Figure 3 The morphology of the mortise and tenon interlocking structure of the copper-aluminum composite plate;

[0036] Figure 4 This is the surface scan result of the rolled mortise and tenon interlocking structure, where the gray is aluminum and the dark black is copper;

[0037] Figure 5 This is the shear strength curve of the copper-aluminum composite plate in the rolling plane;

[0038] Figure 6 The morphology of the copper-aluminum composite interface, the left side is a structure without mortise and tenon interlocking, and the right side is a structure with mortise and tenon interlocking;

[0039] Figure 7 This is the metallographic diagram of copper-aluminum composite material;

[0040] Figure 8 This is the distribution diagram of metal compounds at the interface of copper and aluminum materials. The upper part is the material with silicon powder added, and the lower part is the material without silicon powder added.

[0041] Fig. 9 Comparison of the electrical conductivity of the joint before and after heat treatment at 300°C. DETAILED DESCRIPTION

[0042] The following embodiments of the technical solution of the present invention are described in detail in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and are therefore only used as examples, and cannot be used to limit the protection scope of the present invention.

[0043] See also Figures 1 to 9 The present invention provides a method for preparing a composite material, comprising the following steps:

[0044] S110, pre-treating the substrate to be composited so that a plurality of protrusions are formed on the bonding surface of the substrate to be composited.

[0045] It should be noted that, in the pre-treatment process, before processing the protrusions, the substrate needs to be polished and cleaned. The polishing can be done with sandpaper, and the cleaning can be done with ultrasonic cleaning. The composite effect can be improved by polishing and cleaning.

[0046] At the same time, the substrate is preferably a plate with a regular shape, which is convenient for compounding regular composite materials. If the substrate is a metal plate, its edge can be cut into regular shapes by a spark wire cutting machine, which is convenient for subsequent processing.

[0047] In this embodiment, the protrusion is formed by a single synchronous rolling process with a pressing rate of 50% by a rolling mill. The rolling process can be hot rolling, hot rolling or warm rolling. The rolling pattern of the rolling mill should be determined according to the shape of the protrusion required, and the shape of the protrusion should be a shape that is easy to enter and be stuck in the bonding surface to be bonded with it. That is, the root size of the protrusion is larger than the top size, and the top of the protrusion is inclined toward the side where the roller shaft moves forward or backward (see Figure 2 ).

[0048] With this shape, since the size of the protrusion root is larger than the size of the top, it is convenient for the protrusion to be inserted into the joint surface to be combined with it; at the same time, the top of the protrusion is inclined toward the forward or backward direction of the roller shaft, and when the protrusion is inserted into the corresponding joint surface, a mortise and tenon interlocking structure can be formed ( Figure 3 ), the bonding strength between the two can be improved, thereby improving the bonding effect. In this embodiment, the protrusion can be a longitudinal rib parallel to the roller axis, or a transverse rib perpendicular to the roller axis, or the transverse rib and the longitudinal rib are staggered to form a grid state. In addition, the protrusion can also be a plurality of convex points. Multiple convex points are arranged regularly and evenly, which can also achieve the same effect (see Figure 2 ).

[0049] For example, when the two substrates are copper plate and aluminum plate, the above-mentioned protrusions are processed on the copper plate, and then the two are composite rolled. Due to the low rheological stress, the aluminum plate will first produce work hardening, so that the deformation of the copper layer and the aluminum layer gradually tends to be consistent, which will be more conducive to the interface bonding of the copper layer and the aluminum layer. During rolling, it can be found that: the protrusions on the copper plate are first pressed into the aluminum plate and form grooves during the rolling composite process, so that the protrusions on the copper plate and the grooves on the aluminum plate are embedded together to form a mortise and tenon interlocking structure. The mortise and tenon interlocking structure can accelerate the rupture of the interface hardened layer, and a large amount of new metal is squeezed out, forcing the coordinated deformation between the two metals, improving the overall bonding quality, and improving the bonding strength (see the mortise and tenon interlocking structure). Figure 5 ).

[0050] Can attend Figure 4 , is the surface scan result of the copper-aluminum composite rolled mortise and tenon interlocking structure, in which the gray is aluminum and the dark black is copper. Figure 5 In the microscopic interface morphology, large gaps appeared in some positions of the interface of the composite plate without mortise and tenon interlocking structure, and effective bonding could not be achieved. This shows that the interface of the composite plate with mortise and tenon interlocking structure has been bonded in the plane position, thus having better mechanical properties. Figure 6 The left side has no mortise and tenon interlocking structure, and the right side has mortise and tenon interlocking structure. Figure 7 This is the metallographic diagram of copper-aluminum composite material.

[0051] S120, stacking multiple layers of substrates in sequence, and adding an emulsion between two adjacent bonding surfaces.

[0052] When stacking in sequence, it can be assisted by relevant clamps. At the same time, it can be stacked in sequence from left to right horizontally or stacked in sequence from bottom to top vertically. Preferably, it can be stacked in sequence from bottom to top vertically, which is convenient for rolling by a roller mill. An emulsion is added between the adjacent bonding surfaces. The emulsion can form a lubricating film on the surface of the material, which can reduce the probability of adverse conditions such as scratches and wear on the surface of the substrate. In addition, the emulsifier does not contain harmful substances such as organic solvents, does not pollute the environment, and ensures the environmental friendliness of the entire preparation process.

[0053] S130, subjecting the multi-layered substrate stack to composite rolling with a pressing rate of 50-60% through a rolling mill.

[0054] When performing composite rolling, the roller mill can be a two-roller reversible rolling mill. During the rolling process, the protrusions are pressed into and clamped into the corresponding bonding surfaces, and the two substrates are firmly composited together.

[0055] It should be noted that when two different metal sheets are laminated, a silicon powder layer can be added between two adjacent bonding surfaces. The weight of the silicon powder layer can be 2-4% of the sum of the weights of the two adjacent substrates to be laminated. The silicon powder is placed between the bonding surfaces to inhibit the formation of metal compounds between the copper and aluminum bonding surfaces (see Figure 8 ), which makes the electron scattering rate lower, thereby improving conductivity. For example:

[0056] When the base materials are copper plates and aluminum plates respectively, metal compounds will be produced when the copper and aluminum materials are pressed. The more metal compounds are produced, the higher the electron scattering rate will be, thereby reducing the conductivity of the material. By adding silicon powder to the copper and aluminum plates, the formation of metal compounds between copper and aluminum can be inhibited.

[0057] S140, performing at least one forging on the composite material that is combined into one.

[0058] The composite effect between the substrates can be further improved by forging. The forging times are preferably three or more. The forging pressure can be increased gradually.

[0059] S150, annealing the composite material after forging.

[0060] Since the base material will produce work hardening after composite, it is not conducive to subsequent processing and use. The appropriate annealing process can release residual stress, eliminate work hardening, promote the mutual diffusion of material atoms, and form a strong metallurgical bond at the composite interface, thereby improving the bonding strength of the composite plate, which is beneficial to the subsequent bending, stamping and other processing procedures of the composite plate.

[0061] For example, when the substrate is copper plate and aluminum plate, we use an annealing furnace to anneal the copper-aluminum composite plate with a pressing rate of 55%. Through multiple experiments, the microstructure of the material before and after heat treatment is analyzed. The heat treatment makes the diffusion between aluminum and copper atoms more complete, thus forming a continuous intermetallic compound layer, which greatly improves the conductivity of the material (see Fig. 9 ). Through experiments, the annealing temperature is 300℃ and the treatment time is 2h, which is the best. Figure 5 As shown in the figure, it is a schematic diagram that the electrical conductivity of the material can reach a higher level when the annealing temperature is 300°C and the annealing time is 2h.

[0062] In addition, the present invention also provides a composite material, and the composite material is prepared by the above-mentioned composite material preparation method.

[0063] The above composite material preparation method and composite material:

[0064] Beneficial effects of the present invention:

[0065] The preparation method of the composite material has the following advantages:

[0066] 1. It can reduce process complexity and equipment investment cost;

[0067] 2. No heating is required during the processing, which can avoid changes in the properties of the metal substrate. At the same time, it can avoid the generation of harmful gases due to high heat and avoid damage to the operator's eyes due to high light;

[0068] 3. It can avoid the impact and noise, which may cause damage to the surrounding environment, equipment and other equipment;

[0069] 4. Multiple protrusions are formed on the bonding surface of the substrate. During the rolling and compounding process, the mortise and tenon interlocking structure can accelerate the rupture of the interface hardened layer, and a large amount of new metal is squeezed out from it, forcing the coordinated deformation between the two substrates to improve the overall bonding quality;

[0070] 5. The emulsion can form a lubricating film on the surface of the substrate, which can reduce the probability of scratches, wear and other adverse conditions on the surface of the substrate, thereby improving the quality of the substrate.

[0071] 6. By adding a silicon powder layer, the formation of metal compounds between the copper and aluminum bonding surfaces is suppressed, so that the electron scattering rate is lowered, thereby improving the conductivity.

[0072] The composite material prepared by the above composite material method has good composite effect and stable structure.

[0073] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. These modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present invention, and they should all be included in the scope of the claims and specification of the present invention.

Claims

1. A method for preparing a composite material, characterized in that: include: Pre-treating the substrate to be composited so that a plurality of protrusions are formed on the bonding surface of the substrate to be composited; stacking multiple layers of the substrate in sequence and adding an emulsion between two adjacent bonding surfaces; After the multi-layer stack is stacked, the substrate stack is subjected to composite rolling with a pressing rate of 50-60% by a rolling mill; Forging the composite material combined into one piece at least once; The composite material after forging is subjected to annealing treatment.

2. The method for preparing a composite material according to claim 1, characterized in that: The pretreatment also includes grinding the bonding surface of the substrate and cleaning it after grinding.

3. The method for preparing a composite material according to claim 1, characterized in that: The protrusions are formed by a single synchronous rolling process with a rolling mill having a pressing rate of 50%.

4. The method for preparing a composite material according to claim 1 or 3, characterized in that: The protrusion has a shape that is easy to enter and be stuck in the combination surface with which it is combined.

5. The method for preparing a composite material according to claim 4, characterized in that: The root size of the protrusion is larger than the top size, and the top of the protrusion is inclined toward the forward or backward direction of the roller shaft of the rolling mill.

6. The method for preparing a composite material according to claim 5, characterized in that: The protrusions are longitudinal ribs parallel to the roller axis direction, or transverse ribs perpendicular to the roller axis direction, or the transverse ribs and the longitudinal ribs are staggered to form a grid state.

7. The method for preparing a composite material according to claim 4, characterized in that: The protrusions are a plurality of protrusions.

8. The method for preparing a composite material according to claim 1, characterized in that: Add a layer of silicon powder between two adjacent bonding surfaces.

9. The method for preparing a composite material according to claim 8, characterized in that: The amount of the silicon powder layer is 2-4% of the sum of the masses of the two adjacent substrates to be composited.

10. A composite material, characterized in that: A composite material prepared by the method according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Copper / aluminum composite strip and preparation method thereof

    CN104669705A

  • Welding method for improving aluminum and steel weldment welding effect

    CN107283058A

  • Copper-nanpsilicon carbide-aluminum sandwich structure composite material and preparation method thereof

    CN109174995A

  • Compound strip material with high bonding strength and making method thereof

    CN110756582A

  • Gradient composite material and preparation method thereof

    CN112223888A