Calcium carbide solid waste resource utilization process and system
Through multi-field coupling combined with enhanced leaching and calcium and magnesium directional cascade enrichment technology, the problem of slime water treatment problems and poor dry coal preparation effects in underground coal preparation has been solved, and the deep and clean utilization of calcium carbide solid waste and waste heat resources have been achieved. Recycling reduces environmental pressure and costs.
Patent Information
- Application Number
- CN202410857560.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-15
AI Technical Summary
Among the existing underground coal preparation methods, wet coal preparation results in the production of a large amount of coal slurry water, which is difficult to handle and causes environmental pressure. The application effect of dry coal preparation is poor, resulting in equipment being idle.
Multi-field coupling combined enhanced leaching technology and calcium and magnesium directional cascade enrichment technology are used to realize resource utilization of calcium carbide solid waste through the process of calcination-dissociation-leaching-directional enrichment, including kiln calcination and rod mill Dissociation, hydraulic classification cyclone classification, multi-field coupling enhanced separation, multi-phase reaction tower cascade precipitation and waste heat utilization drying.
It improves the leaching efficiency of calcium carbide purification ash and the recovery rate of calcium and magnesium components, reduces product moisture, realizes waste heat resource utilization, reduces accumulation and landfill costs, avoids dust and groundwater pollution, and meets environmental protection requirements.
Smart Images

Figure CN118771431A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of calcium carbide solid waste treatment, and specifically relates to a calcium carbide solid waste resource utilization process and system. Background Art
[0002] Existing underground coal preparation methods include dry coal preparation represented by wind coal preparation and heavy medium fluidized bed coal preparation, and wet coal preparation represented by jigging coal preparation and heavy medium cyclone coal preparation. Both coal preparation methods have their own advantages and disadvantages: dry coal preparation uses air or air heavy medium as the sorting medium. The advantages are saving a lot of water resources, reducing equipment investment and energy consumption, high efficiency and environmental protection, and simplifying the sorting process. The disadvantages are strong dependence on environmental stability, high requirements for raw coal moisture, and a high lower limit of sorting particle size; wet coal preparation uses water and heavy medium suspension as the sorting medium, with high sorting accuracy, low lower limit of sorting particle size, mature technology, and is currently the most widely used coal preparation method; the disadvantages are high heavy medium consumption, rapid wear of pipelines and equipment, and the most important problem is that a large amount of coal slime water is generated, the circulating water volume is large, difficult to handle, causing great pressure on the surrounding environment, and difficult to control. At present, the main method of coal preparation at the mine is wet method, and the effect of dry coal preparation on site is poor, so that the established dry coal preparation technology has been idle or replaced. In most cases, dry coal preparation is used as pre-discharge of gangue.
[0003] The process of resource utilization of calcium carbide solid waste adopts the method of calcination decarbonization-mechanical dissociation-multi-field coupling combined enhanced leaching-directional gradient enrichment. Calcination decarbonization reduces the load and cost of leaching equipment, and the reduction method improves the process processing capacity. At the same time, it can also provide carbon sources for calcium and magnesium enrichment processes and the energy required for product drying; after mechanical dissociation, the hydraulic classification method is used to fully release the inclusions of calcium and magnesium valuable components; multi-field coupling combined enhanced leaching ensures the leaching efficiency of fine-grained calcium carbide purification ash generated by dissociation; based on nano-target directional gradient enrichment technology, the purity of calcium carbonate and magnesium carbonate products can be further improved. Summary of the invention
[0004] In view of the shortcomings of the existing technology, a multi-field coupling combined enhanced leaching technology and a calcium and magnesium directional step-by-step enrichment technology were adopted. According to the packaging characteristics of valuable components after calcination of calcium carbide solid waste, a process and system for resource utilization of calcium carbide solid waste was provided, realizing the resource utilization of calcium carbide solid waste through "calcination-dissociation-leaching-directional enrichment".
[0005] In order to achieve the above technical purpose, the present invention provides a process for resource utilization of calcium carbide solid waste, the steps of which are as follows:
[0006] Calcium carbide solid waste is collected from the acetylene production workshop, and the residual carbon in the calcium carbide solid waste is removed by calcination in kiln A. The solid residue after calcination is white calcium carbide purified ash with a diameter of 2-4 mm, which is spherical particles;
[0007] The calcium carbide purified ash and water are fed into the rod mill B for dissociation, and the grinding product of the rod mill B is fed into the mill tailings pool C, and is classified according to a diameter of 0.1 mm by the hydraulic classification cyclone D connected to the mill tailings pool C. The bottom flow after the separation of the hydraulic classification cyclone D is fed into the cyclone bottom flow pool E, and then returns to the rod mill B. The overflow of the hydraulic classification cyclone D enters the multi-field coupling enhanced separation equipment F;
[0008] The drug adding box S is used to add the extractant to the multi-field coupling enhanced separation device F and mix them. The overflow is mixed with the drug and then processed by the multi-field coupling enhanced separation device F to generate a leachate, which is stored in the leachate pool G. The leachate in the leachate pool G is separated into solid and liquid by the hydraulic classification cyclone H. The overflow of the hydraulic classification cyclone H is fed into the multiphase reaction tower I. The bottom flow residue of the hydraulic classification cyclone H is used as a building material raw material or returned to the rod mill B according to the dissociation effect and product characteristics.
[0009] A calcium acid targeted chelating agent and a magnesium carbonate targeted chelating agent are added to the overflow in the multiphase reaction tower I through the dosing box T and the dosing box U through the cascade, and after the chelation reaction, concentrated carbon dioxide gas is introduced to cascadely precipitate calcium carbonate and magnesium carbonate. The calcium carbonate precipitate enters the calcium carbonate precipitation tank J, and the magnesium carbonate precipitate enters the magnesium carbonate precipitation tank K. The residual gas returns to the gas purifier V;
[0010] The calcium carbonate precipitate is dehydrated by the filter press L and collected in the feed bin N. The magnesium carbonate precipitate is dehydrated by the filter press M and collected in the feed bin O. The filtrate produced by the filter press enters the circulating water pool R.
[0011] The dehydrated calcium carbonate precipitate and magnesium carbonate precipitate are dried separately to finally obtain dried calcium carbonate product and magnesium carbonate product.
[0012] Further, the waste heat is used to utilize the dryer P to dry the calcium carbonate precipitate in the feed bin N, and the waste heat is used to utilize the dryer Q to dry the magnesium carbonate precipitate in the feed bin O; the heat source used for drying is the hot waste gas generated during the calcination process.
[0013] Furthermore, the waste gas after heat release passes through the heat-containing waste and passes through the calcium carbonate waste heat utilization dryer N and the magnesium carbonate waste heat utilization dryer Q to release heat to obtain exothermic waste gas. The exothermic waste gas passes through the gas purifier V and then passes through the carbon dioxide concentrator W to produce carbon dioxide concentrated gas.
[0014] Furthermore, in the process that the overflow of the hydraulic classification cyclone D enters the multi-field coupling enhanced separation device F, water is replenished from the circulating water tank R to the multi-field coupling enhanced separation device F.
[0015] Furthermore, the filtered calcium carbonate is fed into a waste heat drying machine P by a vibration feeding method to obtain calcium carbonate; the filtered magnesium carbonate is fed into a waste heat drying machine Q by a vibration feeding method to obtain magnesium carbonate.
[0016] Furthermore, the underflow of the hydraulic grading cyclone H has two processes to choose from according to the dissociation and leaching conditions. If the dissociation is poor and no leaching is performed, the underflow of the hydraulic grading cyclone H is fed into the cyclone underflow tank E and then fed into the rod mill B for grinding; if the dissociation is good and the leaching is thorough, the underflow of the hydraulic grading cyclone H enters the concentrator X, and after sedimentation and concentration, the overflow of the concentrator is generated and flows into the circulating water tank R. The underflow of the concentrator is filtered through the residue filter press Y to obtain the residue and the residue filter press filtrate, and the residue filter press filtrate is also fed into the circulating water tank R.
[0017] A system for resource utilization of calcium carbide solid waste, comprising a kiln A, a rod mill B, a mill tailings pool C, a hydraulic classification cyclone D, a cyclone underflow pool E, a multi-field coupling enhanced separation device F, a leachate pool G, a hydraulic classification cyclone H, a multiphase reaction tower I, a calcium carbonate precipitation tank J, a magnesium carbonate precipitation tank K, a filter press L, a filter press M, a feed bin N, a feed bin O, a waste heat utilization dryer P, a waste heat utilization dryer Q, a circulating water pool R, a dosing box S, a dosing box T, a dosing box U, a gas purifier V, a carbon dioxide concentrator W, a concentrator X, a residue filter press Y, a slurry pump Z, a slurry pump AA, a slurry pump AB, a slurry pump AC, a slurry pump AD, and a clean water pump AE;
[0018] After the calcium carbide solid waste is calcined in the kiln A, calcium carbide purified ash and heat-containing waste are generated. The heat-containing waste is released through the calcium carbonate waste heat utilization dryer N and the magnesium carbonate waste heat utilization dryer Q to obtain exothermic waste gas and exothermic waste gas respectively. The exothermic waste gas passes through the gas purifier V to generate purified waste gas, and then passes through the carbon dioxide concentrator W to obtain carbon dioxide concentrated gas;
[0019] The rod mill B is mixed with water and carbide purified ash through the clean water pump AE and enters the rod mill B. The carbide purified ash is dissociated to obtain rod mill discharge, which enters the mill tailings pool C for storage. The slurry pump Z pumps the mill discharge as cyclone feed into the Φ0.1mm hydraulic grading cyclone D. After grading according to 0.1mm, the bottom flow of the Φ0.1mm hydraulic grading cyclone D containing coarse particles and the overflow of the Φ0.1mm hydraulic grading cyclone D containing fine particles are generated. The bottom flow of the hydraulic grading cyclone D flows into the cyclone bottom flow pool E and is returned to the pulp by the slurry pump AA to return to the rod mill B for dissociation again.
[0020] The overflow of the hydraulic grading cyclone D is mixed with the water replenishment of the multi-field coupling enhanced separation device from the circulating water pool R and the leaching agent from the leaching agent dosing box, and then added to the multi-field coupling enhanced separation device F. The leachate flows out from the bottom of the multi-field coupling enhanced separation device F and is stored in the leachate pool G. The slurry pump AB adds the hydraulic grading cyclone feed to the hydraulic grading cyclone H, and after grading the hydraulic grading cyclone feed, a hydraulic grading cyclone bottom flow containing residue and a hydraulic grading cyclone overflow 10 containing calcium and magnesium extracts are generated; the cyclone overflow 10 is mixed with the calcium carbonate targeted chelating agent from the calcium chelating agent dosing box T and the magnesium carbonate targeted chelating agent from the carbon magnesium chelating agent dosing box U, and then enters the multiphase reaction tower I. The carbon dioxide concentrated gas is introduced into the multiphase reaction tower to react with calcium and magnesium ions respectively. The calcium carbonate precipitate precipitated in the first stage enters the calcium carbonate precipitation tank J, and the magnesium carbonate precipitate precipitated in the second stage enters the magnesium carbonate precipitation tank K. The reaction tail gas returns to the gas purifier V for circulation;
[0021] The slurry pump AC pumps the material in the calcium chloride precipitation tank J to the calcium carbonate filter press L as the feed of the calcium carbonate filter press, and obtains wet calcium carbonate and filtrate after filtration. The filtrate is returned to the circulating water pool R, and the wet calcium carbonate enters the calcium carbonate feeding bin N, and then is fed to the calcium carbonate waste heat utilization dryer P by a vibration feeding method to obtain calcium carbonate 23; the slurry pump AD pumps the material in the magnesium chloride precipitation tank K to the magnesium chloride filter press M as the feed of the magnesium chloride filter press, and obtains wet magnesium carbonate and filtrate after filtration. The filtrate is returned to the circulating water pool R, and the wet magnesium carbonate enters the magnesium carbonate feeding bin O, and enters the magnesium carbonate waste heat utilization dryer Q by a vibration feeding method to obtain magnesium carbonate;
[0022] The cyclone underflow depends on the dissociation and leaching conditions. If the leaching dissociation is poor or no leaching occurs, the cyclone underflow enters the cyclone underflow pool E for further grinding. If the dissociation is good and the leaching is thorough, the cyclone underflow enters the concentrator X. After sedimentation and concentration, the concentrator overflow is generated and flows into the circulating water pool R. The concentrator underflow is filtered through the residue filter press Y to obtain the residue and the residue filter press filtrate. The residue filter press filtrate also flows into the circulating water pool R. The water in the circulating water pool R is supplied to various equipment through the hydrophilic pump AE.
[0023] In multi-field coupled enhanced separation equipment, the solution is usually weakly alkaline, and the production equipment needs to consider alkali resistance or corrosion resistance to avoid frequent replacement of equipment and related accessories; the gas purifier needs to ensure that the acid gas content in the purified gas is less than 5%, and the carbon dioxide concentrator needs to increase the carbon dioxide concentration to more than 50%. The calcium carbide purification ash resource utilization process proposed in the present invention, and other modifications, replacements and optimization of some process links based on this process, all fall within the scope of protection of the present invention.
[0024] Beneficial effects:
[0025] The present invention realizes deep and efficient clean utilization of calcium carbide purified ash through grinding dissociation, multi-field coupled leaching and gradient directional enrichment. The advantages of the present invention are as follows:
[0026] By grinding and dissociating the coarse-grained carbide purification ash, calcium and magnesium oxide inclusions are released, fresh surfaces and valuable components are exposed, and the leaching efficiency is improved; the dissociated carbide purification ash particles are leached using multi-field coupling enhanced separation equipment, which can increase the calcium and magnesium leaching rate and the recovery rate of calcium and magnesium components.
[0027] Through the chelating reaction between targeted nanocarrier molecules and calcium ions in a multiphase reaction tower, calcium carbonate is precipitated preferentially, and magnesium carbonate is further precipitated from the magnesium-containing extract after the calcium ions are precipitated, thereby achieving gradient directional enrichment of calcium and magnesium components and improving the product purity of calcium carbonate and magnesium carbonate.
[0028] The heat released by the combustion of residual carbon in calcium carbide purification ash is used to dry the calcium carbonate and magnesium carbonate products, realizing the resource utilization of waste heat, reducing product moisture, improving product quality, and facilitating material transportation, storage and application.
[0029] The carbon dioxide produced by the combustion of calcium carbide purification ash is purified and concentrated to provide a carbon source for the multiphase reaction tower, achieving carbon element fixation and circulation, which meets environmental protection requirements and the needs of the national dual carbon strategy.
[0030] The resource utilization of calcium carbide purification ash reduces the cost of stacking and landfilling, avoids the generation of dust and groundwater pollution, and produces better economic and social benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 It is a schematic diagram of the process for resource utilization of calcium carbide solid waste of the present invention;
[0032] Figure 2 It is a schematic diagram of the structure of the calcium carbide solid waste resource utilization system of the present invention.
[0033] In the figure: 1-calcium carbide purification ash, 2-rod mill discharge, 3-hydraulic classification cyclone feed, 4-hydraulic classification cyclone underflow, 5-hydraulic classification cyclone overflow, 6-cyclone underflow return slurry, 7-leachate, 8-hydraulic classification cyclone feed, 9-hydraulic classification cyclone underflow, 10-hydraulic classification cyclone overflow, 11-calcium carbonate precipitation, 12-magnesium carbonate precipitation, 13-multiphase reaction tower discharge liquid, 14-calcium carbonate filter press feed, 15-magnesium carbonate filter press feed, 16-humid calcium carbonate, 17-calcium carbonate filter press filtrate, 18-humid carbonate Magnesium, 19-magnesium carbonate filter press filtrate, 20-wet calcium carbonate feed, 21-wet magnesium carbonate feed, 22-exothermic waste gas, 23-calcium carbonate, 24-exothermic waste gas, 25-magnesium carbonate, 26-extraction agent, 27-calcium carbonate targeted chelating agent, 28-magnesium carbonate targeted chelating agent, 29-rod mill make-up water, 30-multi-field coupling enhanced separation equipment make-up water, 31-hot waste gas, 32-purified waste gas, 33-carbon dioxide concentrated gas, 34-concentrator underflow, 35-concentrator overflow, 36-residue, 37-residue filter press filtrate, 38-reaction tail gas.
[0034] A-kiln, B-rod mill, C-mill tailings pond, D-Φ0.1mm hydraulic classification cyclone, E-cyclone underflow tank, F-multi-field coupling enhanced separation equipment, G-leachate tank, H-hydraulic classification cyclone, I-multiphase reaction tower, J-calcium carbonate precipitation tank, K-magnesium carbonate precipitation tank, L-calcium carbonate filter press, M-magnesium carbonate filter press, N-calcium carbonate feeding bin, O-magnesium carbonate feeding bin, P-calcium carbonate waste heat utilization dryer, Q-magnesium carbonate waste heat utilization dryer, R-circulating water pool, S-leaching agent dosing box, T calcium chelating agent dosing box, U-magnesium chelating agent dosing box, V-gas purifier, W-carbon dioxide concentrator, X-concentrator, Y-residue filter press, Z-slurry pump AA-slurry pump, AB-slurry pump, AC-slurry pump, AD-slurry pump, AE-clean water pump. DETAILED DESCRIPTION
[0035] The specific embodiments of the present invention are further described below in conjunction with the accompanying drawings:
[0036] like Figure 1 and Figure 2 As shown, the present invention discloses a process for resource utilization of calcium carbide solid waste, and the implementation steps are as follows:
[0037] After the calcium carbide solid waste is discharged from the acetylene production workshop, it is calcined in kiln A to remove the residual carbon in the solid waste. A large amount of hot waste gas 31 is generated as the heat source for product drying, and the heat is released through the waste heat utilization dryers P and Q; the gases 22 and 24 after heat release pass through the gas purifier and V carbon dioxide concentrator W to provide the carbon dioxide carbon source of the process; the solid residue after calcination is spherical particles of white calcium carbide purification ash 1 with a diameter of 2-4mm.
[0038] The calcium carbide purified ash 1 enters the rod mill B for dissociation, and the rod mill discharge 2 of the rod mill B enters the tailings pond C to form a Φ0.1mm hydraulic classification cyclone feed 3, which is classified according to a diameter of about 0.1mm through the hydraulic classification cyclone D. The bottom flow 4 of the hydraulic classification cyclone returns to the slurry 6 as the cyclone bottom flow through the cyclone bottom flow pool and returns to the rod mill B. The cyclone overflow 5 enters the multi-field coupling enhanced separation equipment F.
[0039] The cyclone overflow 5 is mixed with the leaching agent and treated by the multi-field coupling enhanced separation device F to produce the leachate 7. The leachate 7 is stored in the leachate pool G. The leachate pool G inputs the hydraulic classification cyclone feed 8 to the hydrocyclone H for solid-liquid separation. The hydrocyclone overflow 10 enters the multiphase reaction tower I. The hydrocyclone underflow 9 residue is used as a building material raw material or returned to the rod mill B according to the dissociation effect and product characteristics.
[0040] The overflow 10 of the hydraulic classification cyclone is added with calcium carbonate targeted chelating agent 27 and magnesium carbonate targeted chelating agent 28 in a multiphase reaction tower I through a calcium chelating agent dosing box T and a magnesium chelating agent dosing box U in a stepwise manner. After the chelation reaction, concentrated carbon dioxide is introduced to precipitate calcium carbonate precipitate 11 and magnesium carbonate precipitate 12 in a stepwise manner. The calcium carbonate precipitate 11 enters a calcium carbonate precipitation tank J, and the magnesium carbonate precipitate 12 enters a magnesium carbonate precipitation tank K. The reaction tail gas 38 returns to the upper gas purifier V.
[0041] The calcium carbonate precipitate 11 is dehydrated by the filter press L, the wet calcium carbonate 16 enters the feed bin N, and the calcium carbonate filter press filtrate 17 enters the circulating water pool R; the magnesium carbonate precipitate 12 is dehydrated by the filter press M, and the wet magnesium carbonate 18 enters the feed bin O, and the magnesium carbonate filter press filtrate 19 enters the circulating water pool R.
[0042] The calcium carbonate feeding bin N uses a vibrating feeder to feed the wet calcium carbonate feed 20 into the waste heat utilization dryer P to obtain dry calcium carbonate 23; the magnesium carbonate feeding bin O uses a vibrating feeder to feed the wet magnesium carbonate feed 21 into the waste heat utilization dryer Q to obtain dry magnesium carbonate 25.
[0043] The solution in the multi-field coupled enhanced separation equipment F is usually weakly alkaline, and the production equipment needs to consider alkali resistance or corrosion resistance to avoid frequent replacement of equipment and related accessories; the gas purifier V needs to ensure that the acid gas content in the purified gas is less than 5%, and the carbon dioxide concentrator W needs to increase the carbon dioxide concentration to more than 50%.
[0044] Pretreatment of calcium carbide solid waste: After calcination in kiln A, calcium carbide solid waste produces calcium carbide purified ash 1 and heat-containing waste 31. The heat-containing waste releases heat through calcium carbonate waste heat utilization dryer N and magnesium carbonate waste heat utilization dryer Q to obtain exothermic waste gas 24 and exothermic waste gas 22 respectively. The exothermic waste gas passes through gas purifier V to produce purified waste gas 32, and then passes through carbon dioxide concentrator W to produce carbon dioxide concentrated gas 33.
[0045] Dissociation and classification of calcium carbide purified ash: Rod mill supplementary water 29 and calcium carbide purified ash 1 are mixed and enter rod mill B. After dissociation, calcium carbide purified ash 1 obtains rod mill discharge 2, which enters mill tailings pool C for storage. Slurry pump Z pumps mill discharge 2 as cyclone feed 3 into Φ0.1mm hydraulic grading cyclone D, and after classification according to 0.1mm, Φ0.1mm hydraulic grading cyclone underflow 4 containing coarse particles and Φ0.1mm hydraulic grading cyclone overflow 5 containing fine particles are generated. Cyclone underflow 4 flows into cyclone underflow pool E and returns the cyclone underflow to slurry 6 through slurry pump AA to rod mill B for further dissociation.
[0046] Calcium and magnesium component leaching and directional step enrichment: the cyclone overflow 5 is mixed with the multi-field coupling enhanced separation equipment make-up water 30 from the circulating water pool R and the leaching agent 26 from the leaching agent dosing box and then enters the multi-field coupling enhanced separation equipment F. The leachate 7 flows out from the bottom of the multi-field coupling enhanced separation equipment F and is stored in the leachate pool G. The slurry pump AB pumps the hydraulic grading cyclone feed 8 into the hydraulic grading cyclone H to grade the hydraulic grading cyclone feed 8 to produce a hydraulic grading cyclone bottom flow 9 containing residue and a hydraulic grading cyclone overflow 10 containing calcium and magnesium leachates. The cyclone overflow 10 is mixed with the calcium carbonate targeted chelating agent 27 from the calcium chelating agent dosing box T and the magnesium carbonate targeted chelating agent 28 from the carbon magnesium chelating agent dosing box and then enters the multiphase reaction tower I. The carbon dioxide concentrated gas 33 is introduced into the multiphase reaction tower to react with calcium and magnesium ions respectively. The first stage calcium carbonate precipitate 11 enters the calcium carbonate precipitation tank J, and the second stage magnesium carbonate precipitate 12 enters the magnesium carbonate precipitation tank K. The reaction tail gas 38 returns to the gas purifier V for circulation.
[0047] Post-processing of calcium and magnesium products: slurry pump AC pumps the material in calcium chloride precipitation tank J to calcium carbonate filter press L as feed for calcium carbonate filter press, and obtains wet calcium carbonate 16 and calcium carbonate filter press filtrate 17 after filtration. The calcium carbonate filter press filtrate 17 returns to the circulating water pool R, and the wet calcium carbonate enters the calcium carbonate feeding bin N, and then is fed to the calcium carbonate waste heat utilization dryer P by a vibration feeding method to obtain calcium carbonate 23; slurry pump AD feeds the material in magnesium chloride precipitation tank K to magnesium chloride filter press M as feed for magnesium chloride filter press 15, and obtains wet magnesium carbonate 18 and magnesium carbonate filter press filtrate 17 after filtration. The magnesium carbonate filter press filtrate 17 returns to the circulating water pool R, and the wet magnesium carbonate 18 enters the magnesium carbonate feeding bin O, and enters the magnesium carbonate waste heat utilization dryer Q by a vibration feeding method to obtain magnesium carbonate 25.
[0048] Treatment of leaching residue: There are two processes for the cyclone underflow 9 to choose from according to the dissociation and leaching conditions. If the dissociation is poor and no leaching occurs, the cyclone underflow 9 enters the cyclone underflow pool E for further grinding; if the dissociation is good and the leaching is thorough, the cyclone underflow 9 enters the concentrator X, and after sedimentation and concentration, the concentrator overflow 35 is generated and flows into the circulating water pool R. The concentrator underflow 34 is filtered by the residue filter press Y to obtain the residue 36 and the residue filter press filtrate 37, and the residue filter press filtrate 37 also flows into the circulating water pool R. The water in the circulating water pool R is supplied to each device through the hydrophilic pump AE.
[0049] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any simple modification, transformation and modification made to the above embodiment based on the technical essence of the present invention shall fall within the scope of the technical solution of the present invention.
Claims
1. A process for resource utilization of calcium carbide solid waste, characterized in that: Here are the steps: Calcium carbide solid waste is collected from the acetylene production workshop, and the residual carbon in the calcium carbide solid waste is removed by calcination in kiln A. The solid residue after calcination is white calcium carbide purified ash with a diameter of 2-4 mm, which is spherical particles; The calcium carbide purified ash and water are fed into the rod mill B for dissociation, and the grinding product of the rod mill B is fed into the mill tailings pool C, and is classified according to a diameter of 0.1 mm by the hydraulic classification cyclone D connected to the mill tailings pool C. The bottom flow after the separation of the hydraulic classification cyclone D is fed into the cyclone bottom flow pool E, and then returns to the rod mill B. The overflow of the hydraulic classification cyclone D enters the multi-field coupling enhanced separation equipment F; The drug adding box S is used to add the extractant to the multi-field coupling enhanced separation device F and mix them. The overflow is mixed with the drug and then processed by the multi-field coupling enhanced separation device F to generate a leachate, which is stored in the leachate pool G. The leachate in the leachate pool G is separated into solid and liquid by the hydraulic classification cyclone H. The overflow of the hydraulic classification cyclone H is fed into the multiphase reaction tower I. The bottom flow residue of the hydraulic classification cyclone H is used as a building material raw material or returned to the rod mill B according to the dissociation effect and product characteristics. A calcium acid targeted chelating agent and a magnesium carbonate targeted chelating agent are added to the overflow in the multiphase reaction tower I through the dosing box T and the dosing box U through the cascade, and after the chelation reaction, concentrated carbon dioxide gas is introduced to cascadely precipitate calcium carbonate and magnesium carbonate. The calcium carbonate precipitate enters the calcium carbonate precipitation tank J, and the magnesium carbonate precipitate enters the magnesium carbonate precipitation tank K. The residual gas returns to the gas purifier V; The calcium carbonate precipitate is dehydrated by the filter press L and collected in the feed bin N. The magnesium carbonate precipitate is dehydrated by the filter press M and collected in the feed bin O. The filtrate produced by the filter press enters the circulating water pool R. The dehydrated calcium carbonate precipitate and magnesium carbonate precipitate are dried separately to finally obtain dried calcium carbonate product and magnesium carbonate product.
2. A process for resource utilization of calcium carbide solid waste according to claim 1, characterized in that: The waste heat is used to utilize the dryer P to dry the calcium carbonate precipitate in the feed bin N, and the waste heat is used to utilize the dryer Q to dry the magnesium carbonate precipitate in the feed bin O; the heat source used for drying is the hot waste gas generated during the calcination process.
3. The process for resource utilization of calcium carbide solid waste according to claim 2, characterized in that: The waste gas after heat release passes through the heat-containing waste and passes through the calcium carbonate waste heat utilization dryer N and the magnesium carbonate waste heat utilization dryer Q to release heat to obtain exothermic waste gas. The exothermic waste gas passes through the gas purifier V and then passes through the carbon dioxide concentrator W to produce carbon dioxide concentrated gas.
4. The process for resource utilization of calcium carbide solid waste according to claim 1, characterized in that: In the process that the overflow of the hydraulic classification cyclone D enters the multi-field coupling enhanced separation device F, water is replenished from the circulating water tank R to the multi-field coupling enhanced separation device F.
5. The process for recycling calcium carbide solid waste as claimed in claim 1, characterized in that: The filtered calcium carbonate is fed into the waste heat drying machine P by a vibration feeding method to obtain calcium carbonate; the filtered magnesium carbonate is fed into the waste heat drying machine Q by a vibration feeding method to obtain magnesium carbonate.
6. The process for resource utilization of calcium carbide solid waste according to claim 1, characterized in that: There are two processes for the bottom flow of the hydraulic grading cyclone H to choose from according to the dissociation and leaching conditions. If the dissociation is poor and no leaching is performed, the bottom flow of the hydraulic grading cyclone H is fed into the cyclone bottom flow pool E and then fed into the rod mill B for grinding. If the dissociation is good and the leaching is thorough, the bottom flow of the hydraulic grading cyclone H enters the concentrator X, and after sedimentation and concentration, the overflow of the concentrator is generated and flows into the circulating water pool R. The bottom flow of the concentrator is filtered through the residue filter press Y to obtain the residue and the residue filter press filtrate, and the residue filter press filtrate is also fed into the circulating water pool R.
7. A calcium carbide solid waste resource utilization system of the calcium carbide solid waste resource utilization process according to claim 1, characterized in that: Including kiln A, rod mill B, mill tailings pool C, hydraulic classification cyclone D, cyclone underflow pool E, multi-field coupling enhanced separation equipment F, leachate pool G, hydraulic classification cyclone H, multiphase reaction tower I, calcium carbonate precipitation tank J, magnesium carbonate precipitation tank K, filter press L, filter press M, feed bin N, feed bin O, waste heat utilization dryer P, waste heat utilization dryer Q, circulating water pool R, dosing box S, dosing box T, dosing box U, gas purifier V, carbon dioxide concentrator W, concentrator X, residue filter press Y, slurry pump Z, slurry pump AA, slurry pump AB, slurry pump AC, slurry pump AD, clean water pump AE; After the calcium carbide solid waste is calcined in the kiln A, calcium carbide purified ash and heat-containing waste are generated. The heat-containing waste is released through the calcium carbonate waste heat utilization dryer N and the magnesium carbonate waste heat utilization dryer Q to obtain exothermic waste gas and exothermic waste gas respectively. The exothermic waste gas passes through the gas purifier V to generate purified waste gas, and then passes through the carbon dioxide concentrator W to obtain carbon dioxide concentrated gas; The rod mill B is mixed with water and carbide purified ash through the clean water pump AE and enters the rod mill B. The carbide purified ash is dissociated to obtain rod mill discharge, which enters the mill tailings pool C for storage. The slurry pump Z pumps the mill discharge as cyclone feed into the Φ0.1mm hydraulic grading cyclone D. After grading according to 0.1mm, the bottom flow of the Φ0.1mm hydraulic grading cyclone D containing coarse particles and the overflow of the Φ0.1mm hydraulic grading cyclone D containing fine particles are generated. The bottom flow of the hydraulic grading cyclone D flows into the cyclone bottom flow pool E and is returned to the pulp by the slurry pump AA to return to the rod mill B for dissociation again. The overflow of the hydraulic grading cyclone D is mixed with the water replenishment of the multi-field coupling enhanced separation device from the circulating water pool R and the leaching agent from the leaching agent dosing box, and then added to the multi-field coupling enhanced separation device F. The leachate flows out from the bottom of the multi-field coupling enhanced separation device F and is stored in the leachate pool G. The slurry pump AB adds the hydraulic grading cyclone feed to the hydraulic grading cyclone H, and after grading the hydraulic grading cyclone feed, a hydraulic grading cyclone bottom flow containing residue and a hydraulic grading cyclone overflow 10 containing calcium and magnesium extracts are generated; the cyclone overflow 10 is mixed with the calcium carbonate targeted chelating agent from the calcium chelating agent dosing box T and the magnesium carbonate targeted chelating agent from the carbon magnesium chelating agent dosing box U, and then enters the multiphase reaction tower I. The carbon dioxide concentrated gas is introduced into the multiphase reaction tower to react with calcium and magnesium ions respectively. The calcium carbonate precipitate precipitated in the first stage enters the calcium carbonate precipitation tank J, and the magnesium carbonate precipitate precipitated in the second stage enters the magnesium carbonate precipitation tank K. The reaction tail gas returns to the gas purifier V for circulation; The slurry pump AC pumps the material in the calcium chloride precipitation tank J to the calcium carbonate filter press L as the feed of the calcium carbonate filter press, and obtains wet calcium carbonate and filtrate after filtration. The filtrate is returned to the circulating water pool R, and the wet calcium carbonate enters the calcium carbonate feeding bin N, and then is fed to the calcium carbonate waste heat utilization dryer P by a vibration feeding method to obtain calcium carbonate 23; the slurry pump AD pumps the material in the magnesium chloride precipitation tank K to the magnesium chloride filter press M as the feed of the magnesium chloride filter press, and obtains wet magnesium carbonate and filtrate after filtration. The filtrate is returned to the circulating water pool R, and the wet magnesium carbonate enters the magnesium carbonate feeding bin O, and enters the magnesium carbonate waste heat utilization dryer Q by a vibration feeding method to obtain magnesium carbonate; The cyclone underflow depends on the dissociation and leaching conditions. If the leaching dissociation is poor or no leaching occurs, the cyclone underflow enters the cyclone underflow pool E for further grinding. If the dissociation is good and the leaching is thorough, the cyclone underflow enters the concentrator X. After sedimentation and concentration, the concentrator overflow is generated and flows into the circulating water pool R. The concentrator underflow is filtered through the residue filter press Y to obtain the residue and the residue filter press filtrate. The residue filter press filtrate also flows into the circulating water pool R. The water in the circulating water pool R is supplied to various equipment through the hydrophilic pump AE.