Manufacturing method of trigger type ignition semiconductor bridge chip
Determine the polysilicon thickness through simulation modeling, use negative photoresist and high-contrast developer to reduce jaggedness, and combine with metal nanoparticle-assisted wet etching and anti-reflective coating to solve the problem of ultra-thick polysilicon and metal electrode layer engraving in SCB pyrotechnics. Solve the problem of difficult corrosion and achieve high-quality preparation of pyrotechnics.
Patent Information
- Application Number
- CN202410954688.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-15
AI Technical Summary
It is difficult to achieve etching of ultra-thick polysilicon films and ultra-thick metal electrode layers in existing SCB pyrotechnics, resulting in low quality consistency and poor reliability.
The thickness is determined through simulation and experimental modeling of polysilicon thickness and resistance. Negative photoresist and high-contrast developer are used to reduce the sawtooth phenomenon. Metal nanoparticles are used to assist the wet etching process to increase the uniformity and selectivity of etching. Add an anti-reflective coating to the photoresist surface to reduce light reflection interference.
Realized the production of sharp lines in the H-bridge of SCB pyrotechnics, etched ultra-thick polysilicon and metal electrode layers, ensured high-step etching at the overlap of polysilicon and metal electrodes, and improved the preparation quality and reliability of pyrotechnics. sex.
Smart Images

Figure CN118776399A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of initiating explosives, and further relates to the technical field of SCB initiating explosives, and specifically, to a method for manufacturing a trigger-type ignition semiconductor bridge chip. Background Art
[0002] Traditional pyrotechnics trigger igniters using resistors, which have poor controllability and long ignition response time. SCB pyrotechnics refer to a type of pyrotechnics that use semiconductor films (or metal-semiconductor composite films) as ignition elements and then develop into pyrotechnics that use microelectronic integration technology to give pyrotechnics logic control functions. They are key components of weapons, ammunition and other combustion and explosion systems. They are stimulated by small external energy, complete their effects, and achieve their intended functions. They are mainly used to ignite gunpowder and detonate explosives.
[0003] In the prior art, such as Figure 1-2 As shown, due to the limitations of the basic principles and basic structure of SCB pyrotechnics, there are the following problems: 1. In order to make the H-bridge of SCB explosives quickly generate Joule heat and thermal plasma, it is necessary to use the electric field concentration effect to design the electrodes at both ends of the bridge into sharp corners. In conventional semiconductor etching processes, it is difficult to achieve sharp corners.
[0004] 2. In order to reduce the ignition time and ignition energy of SCB explosives, ultra-thick polysilicon films and ultra-thick metal electrode layers of 10,000 angstroms to 50,000 angstroms are required (relative to 5000A in conventional semiconductor processes). For ultra-thick polysilicon films and ultra-thick metal electrode layers, the existing semiconductor processes are difficult to control in terms of growth quality and etching, with low quality consistency and poor reliability.
[0005] 3. For wet etching of ultra-thick polysilicon films and ultra-thick metal electrode layers, ordinary photoresists are too thin to meet the requirements of polysilicon etching.
[0006] 4. Since wet etching has isotropic characteristics, during the wet etching of the metal electrode layer, there is a high step where the polysilicon and the metal overlap in the bridge area, resulting in uneven etching at the step and irregular bridge area.
[0007] In view of this, the present invention is proposed. Summary of the invention
[0008] The technical problem to be solved by the present invention is to solve the problem that it is difficult to etch an ultra-thick polysilicon film and an ultra-thick metal electrode layer in the existing SCB pyrotechnics H-bridge.
[0009] To this end, the present invention provides a method for manufacturing a trigger-type ignition semiconductor bridge chip, including the following method: 1. Method for determining polysilicon thickness Through simulation and experimental modeling of polysilicon thickness and resistance, the relationship between polysilicon thickness and resistance was determined, thereby determining the polysilicon thickness.
[0010] 2. Methods to solve photoresist sawtooth When etching ultra-thick polysilicon, it is inevitable that jagged edges will appear on the photoresist, which will cause jagged edges on the polysilicon lines. To this end, the following methods are used: (1) Use negative photoresist instead of positive photoresist because the sidewalls of negative photoresist are steeper and it is easier to achieve sharp-angle graphics.
[0011] (2) Use a high-contrast developer to increase the difference between the exposed and non-exposed areas of the photoresist and reduce the occurrence of dark corrosion.
[0012] Description of High Contrast Developer: Contrast Factor (γ): The contrast factor γ is defined as the ratio of the logarithm of the change in thickness of the photoresist during the development process to the logarithm of the change in exposure dose.
[0013] The higher the gamma value, the higher the contrast of the developer. In practical applications, the gamma value of high-contrast developers is usually between 4 and 8.
[0014] Parameter range of high contrast developer: Specific high-contrast developer parameters may vary depending on the application scenario and photoresist type, but generally have the following characteristics: High gamma: usually between 4 and 8.
[0015] Narrow exposure dose window: The developer is highly sensitive to a specific range of exposure doses.
[0016] Fast Developing Times: Typically developing times are shorter to avoid overdevelopment of areas outside the exposure dose.
[0017] Use low concentration developer to improve the positive photoresist film to obtain higher contrast, reduce corrosion in unexposed areas or have a longer development time for only partially exposed cross-sectional areas.
[0018] Description of low concentration developer: Normal concentration of developer in the photolithography process usually refers to the standard concentration, that is, the developer concentration widely used and recommended in the photolithography process. These concentrations are usually optimized to provide good contrast and resolution within a reasonable development time.
[0019] The standard concentration range of commonly used developer solutions is as follows: 1. TMAH (Tetramethylammonium hydroxide): Standard concentration: 2.38% (2.38% TMAH is usually used as the standard developer concentration, suitable for most positive photoresists).
[0020] Application: Widely used in semiconductor and microelectronics manufacturing.
[0021] 2. KOH (Potassium Hydroxide): Standard concentration: 2% to 5%.
[0022] Application: Commonly used in photolithography processes that require stronger development effects.
[0023] 3. NaOH (sodium hydroxide): Standard concentration: 0.1 M to 0.2 M (approximately 0.4% to 0.8%).
[0024] Application: Suitable for specific types of photoresists and specific process requirements.
[0025] The concentration range of the low concentration developer of the present invention is as follows: 1. TMAH (Tetramethylammonium hydroxide): TMAH is a commonly used developer for positive photoresists. Low concentrations of TMAH are usually between 0.1% and 0.26%.
[0026] 2. KOH (Potassium Hydroxide): KOH is also a common solution used in photoresist development. Low concentrations of KOH are usually between 0.1% and 1%.
[0027] 3. NaOH (sodium hydroxide): Low concentrations of NaOH typically range from 0.1% to 0.5%.
[0028] Advantages of low concentration developer: Improve contrast: Low concentration developer can better control the development process and improve the contrast of positive photoresist films.
[0029] Reduce corrosion: Reduce the corrosiveness of the developer and reduce the degree of corrosion in the unexposed areas, thereby protecting the integrity of the unexposed areas.
[0030] Finer patterns: Low-concentration developer can produce finer and more accurate lithography patterns, suitable for high-precision micro-nanoscale manufacturing processes.
[0031] (4) Add anti-reflective coating (ARC) on the upper and lower surfaces of the photoresist to reduce light reflection and interference and reduce the impact of the standing wave effect.
[0032] 3. Wet etching of metal electrode layer In order to solve the problem of sawtooth in wet etching of aluminum-titanium-gold, metal nanoparticles assisted wet etching process was adopted.
[0033] Technical effects of the present invention: (1) Realize the production of sharp angle lines in the H-bridge of SCB pyrotechnics.
[0034] (2) Achieve etching of ultra-thick polysilicon films for SCB pyrotechnic H-bridges.
[0035] (3) Realize the etching of the ultra-thick metal electrode layer film of the SCB pyrotechnics H-bridge.
[0036] (4) Achieve etching of the high steps where the polysilicon and metal electrodes of the H-bridge of SCB pyrotechnics overlap.
[0037] The method can be widely used in the preparation of SCB pyrotechnics fire semiconductor bridge chips. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 This is a schematic diagram of the planar structure of the triggered ignition semiconductor bridge chip.
[0039] Figure 2 This is a schematic diagram of the vertical structure of the triggered ignition semiconductor bridge chip.
[0040] Figure 3 Schematic diagram of modeling the relationship between H-bridge polysilicon thickness and resistance.
[0041] In the figure: 1 is the silicon substrate, 2 is the bridge region, 3 is the heavily doped polysilicon, and 4 is the metal electrode layer. DETAILED DESCRIPTION
[0042] The manufacturing method of the trigger-type ignition semiconductor bridge chip is specifically implemented as follows: The polysilicon is heavily doped with phosphorus.
[0043] The metal electrode layer is an aluminum-titanium-gold alloy layer.
[0044] The polysilicon is grown by using a CVD process.
[0045] 1. Determination of polysilicon thickness Through simulation and experimental modeling of polysilicon thickness and resistance, the relationship between polysilicon thickness and resistance was determined, thereby determining the polysilicon thickness.
[0046] As shown in Table 1, through multiple simulations and experiments, the relationship between polysilicon thickness and resistance is determined as follows: Figure 3 As shown, the thickness was finally determined to be 21000-24000 angstroms.
[0047] Table 1 Relationship between polysilicon thickness and resistance
[0049] 2. Selection of etching solution in wet etching method (1) For acidic etching solution: use HNO 3 A mixed solution of HF and MgO in a ratio of 1:6 or 1:10, the temperature is controlled at room temperature or slightly higher, and the etching time is 5 minutes to 100 minutes. The role of acidic etching solution is a faster etching rate, but the disadvantage is that the etching selectivity is low, and it also has a certain etching effect on silicon oxide and silicon nitride.
[0050] (2) Regarding alkaline etching solution: Use KOH, NH4OH or TMAH solution with a concentration of 10% to 30%, control the temperature at 50℃ to 80℃, and the etching time is 5 minutes to 10 hours. The function of alkaline etching solution is high etching selectivity, and it has almost no etching effect on silicon oxide and silicon nitride. The disadvantage is that the etching rate is slow, and it may be affected by the crystal orientation, and irregular etching morphology may occur.
[0051] 3. Selection of etchant in dry etching method of aluminum-titanium-gold alloy layer Method 1: Dry etching of the AlTiAu alloy layer using a Cl 2 , BCl 3 , Ar, N2, CHF 3 and C 2 H 4 The plasma of gases such as Cl2 and BCl3 reacts chemically with aluminum to produce volatile AlCl 3 , Ar and N 2 Provides physical vertical bombardment, CHF 3 and C 2 H 4 A passivation layer is formed on the sidewalls to prevent lateral etching. The disadvantages are that the etching rate is slow, the etching uniformity is poor, and the silicon wafer surface needs to be cleaned after etching to remove residual etchant and reaction products.
[0052] Method 2: Use plasma containing hydrogen fluoride and oxygen as an etchant. Hydrogen fluoride can react chemically with the aluminum-titanium-gold alloy layer to generate volatile AlF3 and TiF4, and oxygen can provide physical vertical bombardment and generate oxide to protect the sidewalls. The advantages are fast etching rate, good etching uniformity, and no need to clean the silicon wafer surface after etching. The disadvantage is that the etchant is highly corrosive, which has a certain impact on the safety of operators and equipment.
[0053] 4. Preparation of anti-reflective coating (1) Bottom anti-reflective coating (BARC): It is a coating applied between the silicon wafer or wafer and the photoresist. Its main components are cross-linked resin, thermal acid generator, surfactant and solvent. The preparation process is to first clean the surface of the silicon wafer or wafer, apply a layer of BARC material, then bake and cure it, and then apply a layer of photoresist on it, and finally perform photolithography exposure, development and cleaning steps.
[0054] (2) Top anti-reflective coating (TARC): It is a coating applied on the top of the photoresist. It completely relies on optical destructive interference to control the reflection of the photoresist surface. It can only control the reflectivity of the photoresist surface and cannot suppress the reflection at the photoresist / substrate interface. The preparation process is to first apply a layer of photoresist on the surface of the silicon wafer or wafer, bake and cure it, then apply a layer of TARC material, bake and cure it again, and finally perform photolithography exposure, development and cleaning steps.
[0055] (3) Developable bottom anti-reflective coating (DBARC): There are two main types, one is an anti-reflective coating that can be directly dissolved in the developer, and the other is a photosensitive anti-reflective coating. The preparation process of the former is similar to that of BARC, except that the coating does not need to be removed during development. The preparation process of the latter is to first apply a layer of photosensitive anti-reflective coating on the surface of the silicon wafer or wafer, bake and cross-link it, and then apply a layer of photoresist on it. When performing photolithography exposure, light will pass through the photoresist and irradiate the coating, stimulating the photochemical reaction in the coating to remove the cross-linking and dissolve it in the developer, and finally perform development and cleaning steps.
[0056] (4) Spin-coated Si anti-reflective coating (SiARC): The main material is organic siloxane. The preparation process is to first coat a layer of SiARC material on the surface of the silicon wafer or wafer, bake and cure it, then coat a layer of photoresist on it, and finally perform photolithography exposure, development and cleaning steps.
[0057] 5. Metal nanoparticle-assisted wet etching process The role of metal nanoparticles in wet etching: (1) Nanoparticles can act as catalysts in the etching solution, increasing the activity of the etching reaction and thus accelerating the etching rate.
[0058] (2) Nanoparticles act as carriers in the etching solution, increasing the contact area between the etching solution and the silicon wafer surface and improving the uniformity of etching.
[0059] (3) Nanoparticles act as masks in the etching solution, increasing the selectivity of etching.
[0060] Nanoparticle selection method: It is determined by the properties of the etchant and the requirements of the etched object. Nanoparticles should have the following characteristics: It has good chemical stability with etchants and will not react or dissolve with them.
[0061] It has a good catalytic effect with the metal electrode layer and can promote the etching reaction.
[0062] It has good wettability with the aluminum metal electrode layer and can be evenly dispersed and attached to its surface.
[0063] It has a good masking effect with the metal electrode layer and can prevent the etchant from corroding its side wall.
[0064] With proper size and shape, the efficiency and accuracy of etching can be improved.
[0065] For the aluminum-titanium-gold alloy layer, the selection of metal nanoparticles is as follows: (1) Metal nanoparticles, such as gold, silver, copper, iron, nickel, palladium, etc., can undergo redox reactions with hydrofluoric acid or hydrogen peroxide in the etchant, thereby accelerating the etching rate.
[0066] (2) Metal oxide nanoparticles, such as aluminum oxide, zirconium oxide, iron oxide, manganese oxide, titanium oxide, etc., can react with hydrofluoric acid or hydrogen peroxide in the etchant to accelerate the etching rate.
[0067] (3) Metal sulfide nanoparticles, such as cadmium sulfide, zinc sulfide, copper sulfide, iron sulfide, molybdenum sulfide, etc., can undergo double decomposition reaction with hydrofluoric acid or hydrogen peroxide in the etchant, thereby accelerating the etching rate.
[0068] (4) Metal nitride nanoparticles, such as aluminum nitride, boron nitride, titanium nitride, silicon nitride, gallium nitride, etc., which can undergo hydrolysis reaction with hydrofluoric acid or hydrogen peroxide in the etchant, thereby accelerating the etching rate.
[0069] (5) Metal carbide nanoparticles, such as aluminum carbide, boron carbide, titanium carbide, silicon carbide, tungsten carbide, etc., can undergo hydrolysis reaction with hydrofluoric acid or hydrogen peroxide during etching, thereby accelerating the etching rate.
[0070] 6. Process control method for uniformity of wet etching of polysilicon (1) Before etching, clean the wafer thoroughly to remove impurities and contaminants on the surface to avoid affecting the uniformity of etching.
[0071] (2) Stir or circulate the etching solution during the etching process to maintain the consistency of the concentration and temperature of the etching solution to avoid local excessive or insufficient etching.
[0072] (3) After etching, rinse the wafer thoroughly to remove the etching products and residual etching solution to avoid subsequent corrosion or damage.
[0073] (4) Accurately measure the thickness of the wafer before and after etching, and calculate the appropriate etching time based on the etching rate to avoid excessive or insufficient etching.
[0074] Finally, it should be noted that the above embodiments are merely examples for the purpose of clear explanation. The present invention includes but is not limited to the above embodiments. It is not necessary and impossible to list all implementation methods exhaustively. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. All implementation methods that meet the requirements of the present invention belong to the protection scope of the present invention.
Claims
1. A method for manufacturing a triggered ignition semiconductor bridge chip, characterized in that: The following methods are included: (1) Method for determining polysilicon thickness Through simulation and experimental modeling of polysilicon thickness and resistance, the relationship between polysilicon thickness and resistance is determined, thereby determining the polysilicon thickness; (2) Methods to solve photoresist sawtooth problems 1) Use negative photoresist instead of positive photoresist; 2) Use a high contrast developer with a contrast factor of 4-8; 3) Use low concentration developer; 4) Add anti-reflective coating to the upper and lower surfaces of the photoresist; (3) Wet etching of metal electrode layer A nanoparticle-assisted wet etching process is used.
2. The method for manufacturing a triggered ignition semiconductor bridge chip according to claim 1, characterized in that: The thickness of the polysilicon is 21000 angstroms to 24000 angstroms.
3. The method for manufacturing a triggered ignition semiconductor bridge chip according to claim 1, characterized in that: The polysilicon is heavily doped with phosphorus.
4. The method for manufacturing a triggered ignition semiconductor bridge chip according to claim 1, characterized in that: The metal electrode layer is an aluminum-titanium-gold alloy layer.
5. The method for manufacturing a triggered ignition semiconductor bridge chip as claimed in claim 1, characterized in that: The polysilicon is grown by using a CVD process.
6. The method for manufacturing a triggered ignition semiconductor bridge chip as claimed in claim 1, characterized in that: The wet etching solution is: For acidic etching solution: use a mixed solution of HNO3 and HF, the ratio of HNO3 to HF is 1:6 or 1:10, the temperature is in the room temperature range, and the etching time is 5 minutes to 100 minutes; For alkaline etching solution: use KOH, NH4OH or TMAH solution with a concentration of 10% ~ 30%, a temperature of 50℃ ~ 80℃, and an etching time of 5 minutes to 10 hours.
7. The method for manufacturing a triggered ignition semiconductor bridge chip as claimed in claim 1, characterized in that: The selection of dry etchant for aluminum-titanium-gold alloy layer is as follows: Using a plasma containing Cl2, BCl3, Ar, N2, CHF3 and C2H4 gases as an etchant; or A plasma containing hydrogen fluoride and oxygen is used as an etchant.
8. The method for manufacturing a triggered ignition semiconductor bridge chip as claimed in claim 1, characterized in that: The preparation methods of the anti-reflective coating are as follows: Method 1: Bottom anti-reflective coating (BARC): It is a coating applied between the silicon chip or wafer and the photoresist. Its main components are cross-linkable resin, thermal acid generator, surfactant and solvent. The preparation process is to first clean the surface of the silicon chip or wafer, apply a layer of BARC material, then bake and cure it, then apply a layer of photoresist on it, and finally perform photolithography exposure, development and cleaning steps; Method 2: Top anti-reflective coating (TARC): It is a coating applied on top of the photoresist. The preparation process is to first apply a layer of photoresist on the surface of the silicon wafer or wafer, bake and cure it, then apply a layer of TARC material, bake and cure it again, and finally perform photolithography exposure, development and cleaning steps; Method 3: Developable Bottom Anti-Reflective Coating (DBARC): The first type is an anti-reflective coating that can be directly dissolved in the developer and does not need to be removed during development; The second type is a photosensitive anti-reflective coating. The preparation process is to first apply a layer of photosensitive anti-reflective coating on the surface of the silicon chip or wafer, bake and cross-link it, and then apply a layer of photoresist on it. When performing photolithography exposure, light will pass through the photoresist and irradiate the coating, stimulating the photochemical reaction in the coating to remove the cross-linking and dissolve it in the developer, and finally perform the development and cleaning steps; Method 4: Spin-coated Si anti-reflective coating (SiARC): The main material is organic siloxane. The preparation process is to first apply a layer of SiARC material on the surface of the silicon wafer or wafer, bake and cure it, then apply a layer of photoresist on it, and finally perform photolithography exposure, development and cleaning steps.
9. The method for manufacturing a triggered ignition semiconductor bridge chip as claimed in claim 1, characterized in that: For the aluminum-titanium-gold alloy layer, the nanoparticles are one or more of the following: (1) Metal nanoparticles; (2) Metal oxide nanoparticles; (3) Metal sulfide nanoparticles; (4) Metal nitride nanoparticles; (5) Metal carbide nanoparticles.
10. The method for manufacturing a triggered ignition semiconductor bridge chip as claimed in claim 9, characterized in that: The metal nanoparticles are gold, silver, copper, iron, nickel or palladium; The metal oxide nanoparticles are aluminum oxide, zirconium oxide, iron oxide, manganese oxide or titanium oxide; The metal sulfide nanoparticles are cadmium sulfide, zinc sulfide, copper sulfide, iron sulfide or molybdenum sulfide; The metal nitride nanoparticles are aluminum nitride, boron nitride, titanium nitride, silicon nitride or gallium nitride; The metal carbide nanoparticles are aluminum carbide, boron carbide, titanium carbide, silicon carbide or tungsten carbide.
Citation Information
Cited By
Method for preparing super-thick coating through dynamic compensation optimization chemical vapor deposition
CN119876918A
3D integrated SCB-VO2 current protection device based on TSV interconnection and preparation method thereof
CN122448031A
3D Integrated SCB-VO2 Current Protection Device Based on TSV Interconnect and Its Fabrication Method
CN122448031B