Pre-sintered silver soldering lug for protecting power module and processing method of pre-sintered silver soldering lug
Through the multi-layer structure of pre-sintered silver solder sheets and the use of hot pressing forming of sintered silver solder layers and other layers, the problems of insufficient conductivity and welding reliability of existing silver solder sheets are solved, and stable welding under high temperature and high pressure is achieved. performance.
Patent Information
- Application Number
- CN202410870894.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-01
- Publication Date
- 2024-10-22
AI Technical Summary
The electrical conductivity and welding reliability of existing silver solder sheets have not yet been improved, especially in high temperature and high pressure environments, where there is insufficient stability.
The pre-sintered silver solder sheet adopts a multi-layer structure, including a sintered silver solder layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold solder layer. Compression molding creates a dense structure to ensure conductivity and reliability of welding.
It improves the conductivity and reliability of welding, ensures stable welding under high temperature and high pressure, and is suitable for high-power IGBT and SiC power modules.
Smart Images

Figure CN118808983A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to raw materials for producing power modules, and in particular to a pre-sintered silver solder sheet for protecting power modules and a processing method thereof. Background Art
[0002] Silicon carbide power modules integrate power devices and drive circuits for controlling, regulating and converting electrical energy. They have good high-temperature characteristics and can work stably in high-temperature environments, improving the reliability and life of the system. They can effectively buffer voltage shocks, reduce the system's dependence on external power supplies, achieve high integration, and are extremely small in size, making them easy to integrate, install and maintain. Silver solder sheets are cast from metals such as silver and copper, and are rolled into thin sheets for welding power modules. This reliable welding connection is essential for the stable operation and long life of power modules. Patent document CN117248197A discloses a silver solder sheet, which is prepared by ion beam reaction, in-situ electrochemical reaction and sputtering reaction on a silver sheet to obtain a silver solder sheet with a micro-nano structure on the surface, which can increase the contact area with other materials, provide more binding sites, enhance bonding strength and interface affinity, form micro-nano-level bumps or textures, increase surface area, and enhance physical properties such as light, electricity and heat. However, this silver solder sheet adopts a single silver sheet structure, and its conductive properties and welding reliability need to be improved. Therefore, it is necessary to optimize its structure to overcome the above-mentioned defects. Summary of the invention
[0003] The purpose of the present invention is to provide a pre-sintered silver solder sheet for protecting a power module and a processing method thereof.
[0004] The technical solution adopted by the present invention to solve the technical problem is:
[0005] A pre-sintered silver solder sheet for protecting a power module, comprising:
[0006] A sintered silver soldering layer, which can be connected to a lead-out point of a power module by welding;
[0007] A gold conductive layer, the gold conductive layer being attached to the top surface of the sintered silver solder layer;
[0008] A palladium conductive inner layer, the palladium conductive inner layer is attached to the top surface of the gold conductive layer;
[0009] a silver conductive layer, the silver conductive layer being attached to a top surface of the palladium conductive inner layer;
[0010] A copper foil conductive layer, the copper foil conductive layer being attached to the top surface of the silver conductive layer;
[0011] A nickel conductive layer, the nickel conductive layer being attached to the top surface of the copper foil conductive layer;
[0012] A palladium conductive outer layer, the palladium conductive outer layer attached to the top surface of the nickel conductive layer;
[0013] A gold soldering layer is attached to the top surface of the palladium conductive outer layer, and the lead wire can be soldered to the gold soldering layer.
[0014] In one embodiment of the present invention, the sintered silver solder layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold solder layer are bonded to each other by hot pressing.
[0015] In one embodiment of the present invention, the pre-sintered silver solder sheet is cut and formed by hot-pressing and bonding a sintered silver solder layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold solder layer to form a sheet.
[0016] In one embodiment of the present invention, the pre-sintered silver solder sheet is in a rectangular shape.
[0017] In one embodiment of the present invention, the size of the pre-sintered silver solder sheet is 5 mm×5 mm.
[0018] In one embodiment of the present invention, the size of the pre-sintered silver solder sheet is 10 mm×10 mm.
[0019] In one embodiment of the present invention, the dimensional accuracy of the pre-sintered silver solder sheet is controlled within ±0.03 mm.
[0020] In one embodiment of the present invention, the corners of the pre-sintered silver solder sheet are provided with arc chamfers to reduce stress concentration.
[0021] A method for processing a pre-sintered silver solder sheet, used for making the pre-sintered silver solder sheet for protecting a power module, comprising:
[0022] Preparing a sintered silver soldering layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold soldering layer, and stacking the sintered silver soldering layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold soldering layer in sequence;
[0023] The stacked sintered silver solder layer, gold conductive layer, palladium conductive inner layer, silver conductive layer, copper foil conductive layer, nickel conductive layer, palladium conductive outer layer and gold solder layer are subjected to hot pressing and forming to bond them to each other;
[0024] The sheet formed by hot pressing the sintered silver solder layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold solder layer is cut to form a rectangular pre-sintered silver solder sheet.
[0025] During the hot pressing process, the hot pressing pressure used is 3-30 MPa, the hot pressing time is 1-30 minutes, and the hot pressing temperature is 100-300°C.
[0026] The advantages of the present invention are:
[0027] This pre-sintered silver solder sheet is formed by hot-pressing a sintered silver soldering layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold soldering layer to form a sheet body that can be placed in a packaging box that matches its shape for quick access. The sintered silver soldering layer is pre-sintered to form a dense structure, which can provide good electrical conductivity during the welding process, ensure smooth flow of module current and reduce energy loss. It has good welding performance, can stably weld under high temperature and high pressure, ensure the reliability of the welding point, and is suitable for high-power IGBT power modules or SiC power modules. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 The figure is a schematic diagram of the structure of the pre-sintered silver solder sheet for protecting the power module proposed by the present invention. DETAILED DESCRIPTION
[0029] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings here can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents selected embodiments of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of the present invention.
[0030] like Figure 1 As shown, the pre-sintered silver solder sheet for protecting the power module proposed by the present invention comprises a sintered silver soldering layer 1, a gold conductive layer 2, a palladium conductive inner layer 3, a silver conductive layer 4, a copper foil conductive layer 5, a nickel conductive layer 6, a palladium conductive outer layer 7 and a gold soldering layer 8. The sintered silver soldering layer can be connected to the wire lead-out point of the power module by welding. The gold conductive layer is attached to the top surface of the sintered silver soldering layer, the palladium conductive inner layer is attached to the top surface of the gold conductive layer, the silver conductive layer is attached to the top surface of the palladium conductive inner layer, the copper foil conductive layer is attached to the top surface of the silver conductive layer, the nickel conductive layer is attached to the top surface of the copper foil conductive layer, the palladium conductive outer layer is attached to the top surface of the nickel conductive layer, the gold soldering layer is attached to the top surface of the palladium conductive outer layer, and the lead-out wire can be soldered to the gold soldering layer.
[0031] In this embodiment, the sintered silver solder layer 1, the gold conductive layer 2, the palladium conductive inner layer 3, the silver conductive layer 4, the copper foil conductive layer 5, the nickel conductive layer 6, the palladium conductive outer layer 7 and the gold solder layer 8 are bonded to each other by hot pressing.
[0032] In this embodiment, the pre-sintered silver solder sheet is cut and formed by hot-pressing and bonding a sintered silver solder layer 1, a gold conductive layer 2, a palladium conductive inner layer 3, a silver conductive layer 4, a copper foil conductive layer 5, a nickel conductive layer 6, a palladium conductive outer layer 7 and a gold solder layer 8 to form a sheet.
[0033] In this embodiment, the pre-sintered silver solder sheet is in a rectangular shape.
[0034] In one embodiment, the size of the pre-sintered silver solder sheet is 5 mm×5 mm.
[0035] In another embodiment, the size of the pre-sintered silver solder sheet is 10 mm×10 mm.
[0036] In this embodiment, the dimensional accuracy of the pre-sintered silver solder sheet is controlled within ±0.03 mm.
[0037] In this embodiment, arc chamfers are provided at the corners of the pre-sintered silver solder sheet to reduce stress concentration.
[0038] The processing method for making the above-mentioned pre-sintered silver solder sheet for protecting the power module includes:
[0039] Preparing a sintered silver soldering layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold soldering layer, and stacking the sintered silver soldering layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold soldering layer in sequence;
[0040] The stacked sintered silver solder layer, gold conductive layer, palladium conductive inner layer, silver conductive layer, copper foil conductive layer, nickel conductive layer, palladium conductive outer layer and gold solder layer are subjected to hot pressing and forming to bond them to each other;
[0041] The sheet formed by hot pressing the sintered silver solder layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold solder layer is cut to form a rectangular pre-sintered silver solder sheet.
[0042] During the hot pressing process, the hot pressing pressure used is 3-30 MPa, the hot pressing time is 1-30 minutes, and the hot pressing temperature is 100-300°C.
[0043] In the description of the present invention, it should be noted that when terms such as "upper", "lower", "inner", "outer", "left", "right" and the like indicating orientation or positional relationship appear, it should be understood that the orientation or positional relationship shown in the drawings, or the orientation or positional relationship in which the invention product is usually placed when in use, or the orientation or positional relationship commonly understood by those skilled in the art, is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the equipment or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. In addition, when terms such as "first" and "second" appear, they are only used to distinguish the description, and cannot be understood as indicating or implying relative importance. In the description of the present invention, it should also be noted that, unless otherwise clearly specified and limited, terms such as "installation", "setting", and "connection" should be understood in a broad sense. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be a connection between the two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
Claims
1. A pre-sintered silver solder sheet for protecting power modules, It is characterized in that include: A sintered silver soldering layer, which can be connected to a lead-out point of a power module by welding; A gold conductive layer, the gold conductive layer being attached to the top surface of the sintered silver solder layer; A palladium conductive inner layer, the palladium conductive inner layer is attached to the top surface of the gold conductive layer; a silver conductive layer, the silver conductive layer being attached to a top surface of the palladium conductive inner layer; A copper foil conductive layer, the copper foil conductive layer being attached to the top surface of the silver conductive layer; A nickel conductive layer, the nickel conductive layer being attached to the top surface of the copper foil conductive layer; A palladium conductive outer layer, the palladium conductive outer layer attached to the top surface of the nickel conductive layer; A gold soldering layer is attached to the top surface of the palladium conductive outer layer, and the lead wire can be soldered to the gold soldering layer.
2. A pre-sintered silver solder sheet for protecting a power module according to claim 1, Features: The sintered silver solder layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold solder layer are bonded to each other by heat pressing.
3. A pre-sintered silver solder sheet for protecting a power module according to claim 2, Features: The pre-sintered silver solder sheet is cut and formed by hot-pressing and bonding a sintered silver solder layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold solder layer to form a sheet.
4. A pre-sintered silver solder sheet for protecting a power module according to claim 3, Features: The pre-sintered silver solder sheet is in a rectangular shape.
5. A pre-sintered silver solder sheet for protecting a power module according to claim 4, Features: The size of the pre-sintered silver solder sheet is 5 mm×5 mm.
6. A pre-sintered silver solder sheet for protecting a power module according to claim 4, Features: The size of the pre-sintered silver solder sheet is 10 mm×10 mm.
7. A pre-sintered silver solder sheet for protecting a power module according to claim 5 or 6, Features: The dimensional accuracy of the pre-sintered silver solder sheet is controlled within ±0.03 mm.
8. The pre-sintered silver solder sheet for protecting a power module according to claim 4, Features: The corners of the pre-sintered silver solder sheet are provided with arc chamfers to reduce stress concentration.
9. A method for processing a pre-sintered silver solder sheet, used for making a pre-sintered silver solder sheet for protecting a power module as claimed in any one of claims 1 to 8, It is characterized in that include: Preparing a sintered silver soldering layer, a gold conductive layer, a palladium conductive inner layer, a silver conductive layer, a copper foil conductive layer, a nickel conductive layer, a palladium conductive outer layer and a gold soldering layer, and stacking the sintered silver soldering layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold soldering layer in sequence; The stacked sintered silver solder layer, gold conductive layer, palladium conductive inner layer, silver conductive layer, copper foil conductive layer, nickel conductive layer, palladium conductive outer layer and gold solder layer are subjected to hot pressing and forming to bond them to each other; The sheet formed by hot pressing the sintered silver solder layer, the gold conductive layer, the palladium conductive inner layer, the silver conductive layer, the copper foil conductive layer, the nickel conductive layer, the palladium conductive outer layer and the gold solder layer is cut to form a rectangular pre-sintered silver solder sheet.
10. A method for processing a pre-sintered silver solder sheet according to claim 9, Features: During the hot pressing process, the hot pressing pressure used is 3-30 MPa, the hot pressing time is 1-30 minutes, and the hot pressing temperature is 100-300°C.