Manufacturing method of four-order HDI high-speed board for server

By adopting strict control process steps such as multiple laminations, drilling, plasma glue removal, copper deposition, exposure and development, etching and solder mask in the production of HDI high-speed boards, the low yield and cost of HDI high-speed boards in the existing technology are solved. High-volume production with high transmission rate and high reliability is achieved.

CN118829104APending Publication Date: 2024-10-22LONGYAN JINSHIYU ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411006144.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

It is difficult to effectively produce high-end HDI high-speed boards with existing technology, resulting in low yield, high cost and low reliability. Especially in communication products, the process control is complex and the details are cumbersome.

Method used

Use multiple lamination steps to use copper foil with a specific thickness, strictly control the expansion and contraction process, and perform expansion and contraction testing and marking; control the hole shape and roughness when drilling, use a new tool to drill and measure the CPK value; plasma glue removal and leveling Control the glue removal rate and copper plating uniformity when depositing copper; outer layer Lines use high-sensitivity dry film for exposure and development to ensure line width and spacing consistency; grinding and brushing are prohibited during etching and solder mask pre-processing, and impedance testing is performed; tolerances and quality are strictly controlled during appearance processing and flying probe testing; finally passed OSP processing ensures consistent copper thickness of the line.

Benefits of technology

It achieves the high transmission rate of the fourth-order HDI high-speed board, with simple process, high reliability and high production yield. It is suitable for mass production and lays the foundation for the development of HDI boards with higher transmission rates.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118829104A_ABST
    Figure CN118829104A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of high-speed board preparation, in particular to a manufacturing method of a four-order HDI high-speed board for a server, which comprises the following steps of: pressing for multiple times, using a copper foil with a specific thickness, ensuring that the distance from an inner layer hole to a line meets the design requirement, strictly controlling the expansion and shrinkage in the pressing process, and carrying out expansion and shrinkage testing and marking; the manufacturing method, the manufacturing process and the process control details of the fourth-order HDI high-speed board for the server have the advantages that the transmission rate of manufactured fourth-order HDI finished products can reach 1GHZ or above, due to the fact that the process is simple, reliability is high, the production yield is high, cost is low, the fourth-order HDI high-speed board is suitable for mass production, meanwhile, the high-speed requirement can be met, and the service life of the fourth-order HDI high-speed board is prolonged. Most importantly, a solid foundation can be laid for further development of HDI boards with higher transmission rates in the future, and the method has great reference significance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of high-speed board preparation, and in particular to a method for preparing a fourth-order HDI high-speed board for a server. Background Art

[0002] HDI is the abbreviation of High Density Inverter, which is a circuit board with a relatively high line distribution density that uses micro blind / buried hole technology to produce printed circuit boards. In the PCB industry, the definition of HDI boards is usually that the minimum line width / spacing is 75 / 75μm or less, the minimum via hole diameter is 150μm or less, it contains blind holes or blind buried holes, the minimum pad is 400μm or less, and the pad density is greater than

[0003] 20 / cm2 PCB board is a high-end PCB type;

[0004] At present, the third-order, fourth-order or Anylayer HDi motherboards are more widely used in electronic terminal products. With the development of 5G communication and AI intelligence, consumers' requirements for transmission speed are also gradually shifting towards lighter and thinner HDI motherboards and finer line width and spacing. The requirements for production processes are also getting higher and higher. It is difficult for general factories to make such products, especially high-speed boards for communications. There are many technologies that need to be tackled in the process, and the management and control details are extremely cumbersome, which directly leads to a lot of problems such as low yield, high cost, and low reliability. Summary of the invention

[0005] The object of the present invention is to provide a method for manufacturing a four-level HDI high-speed board for a server, so as to solve the problems raised in the above background technology.

[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a method for manufacturing a fourth-order HDI high-speed board for a server, the method comprising multiple lamination steps, using copper foil of a specific thickness, ensuring that the distance from the inner hole to the line meets the design requirements, strictly controlling the expansion and contraction during the lamination process, and performing expansion and contraction testing and marking.

[0007] Preferably, a browning step is also included, the amount of micro-etching is strictly controlled, mixed pressing is not allowed, and pressing is carried out strictly in accordance with the process procedure to ensure the quality of the hole wall.

[0008] Preferably, it also includes a drilling step, controlling the hole shape to 100-105um, the hole bottom to be larger than 85um, the hole wall roughness to be controlled to ≤25um, using a new drill, reducing the feed speed, limiting the life of the drill bit, and measuring the CPK value to ensure the drilling quality.

[0009] Preferably, it also includes plasma degumming and horizontal copper deposition steps, and the degumming rate is controlled at 0.15-0.35 mg / cm2 To ensure the surface cleanliness before copper plating; after copper plating, the blind holes must be filled, the DP value must be controlled ≤10um, and the surface copper must be controlled at the median value to ensure uniform copper plating.

[0010] Preferably, it also includes multiple copper reduction steps, controlling the copper foil thickness to 8-12um, controlling the extreme value of copper thickness on the board surface to within 3um, and paying attention to controlling the scratch phenomenon.

[0011] Preferably, it also includes the outer layer circuit production step, using high-sensitivity dry film for exposure and development, controlling the exposure PE value to 60um, and the pre-processing production speed to operate under specific conditions to ensure the best exposure environment and development conditions; the minimum line width and line spacing of the production draft

[0012] It is .101 / 0.066mm, and the minimum spacing is 0.051MM.

[0013] Preferably, it also includes an etching step to ensure that there are no burrs in the etching. After the pattern is etched, it is forbidden to open the grinding brush. The impedance line width and the ordinary line width are measured to ensure that they are consistent with the actual line width of the inner layer. Preferably, it also includes solder mask pre-treatment and character production steps. Before the solder mask is processed, it is forbidden to open the grinding brush and sandblast. The characters are white and the text is clear. PAD cannot be used, and the finished product impedance test is performed after the characters are written.

[0014] Preferably, it also includes the steps of shape processing and flying probe testing, and the shape tolerance is controlled within ±

[0015] 0.1MM, flying probe test strictly controls scratches, board warping and test leakage.

[0016] Preferably, OSP processing and final quality control steps are also included, and OSP rework is strictly controlled to ensure the consistency of circuit copper thickness; the pads and BGA of the same component have the same shape and size to meet the high quality requirements of server high-speed boards.

[0017] Compared with the prior art, the present invention has the following beneficial effects:

[0018] The invention proposes a method for manufacturing a fourth-order HDI high-speed board for a server, a manufacturing process and process control details, and a fourth-order HDI finished product with a transmission rate of more than 1 GHZ. Due to the simple process, high reliability, high production yield and low cost, it is suitable for mass production and can also meet high-speed requirements. Most importantly, it can lay a solid foundation for the further development of HDI boards with higher transmission rates in the future, which is of great reference significance.

[0019] The etching line width compensation test board made according to the present invention can effectively confirm the influence of different equipment and different factors on the line width of high-frequency high-speed boards and other PCB boards, so as to find out the appropriate compensation parameters, provide strong guidance for the consistency of the line width of the entire PCB, and be of great help in impedance control and other aspects. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 The figure is a flow chart of the method of the present invention. DETAILED DESCRIPTION

[0021] In order to make the purpose and technical solution of the present invention clearly and completely described, and the advantages more clearly understood, the embodiments of the present invention are further described in detail with reference to the accompanying drawings. It should be understood that the specific embodiments described herein are part of the embodiments of the present invention, rather than all of the embodiments, and are only used to explain the embodiments of the present invention, and are not used to limit the embodiments of the present invention. All other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] Embodiment 1

[0023] See also Figure 1 The present invention provides a technical solution: a method for manufacturing a fourth-order HDI high-speed board for a server, the method comprising multiple lamination steps, using copper foil of a specific thickness, ensuring that the distance from the inner hole to the line meets the design requirements, strictly controlling the expansion and contraction during the lamination process, and performing expansion and contraction testing and marking.

[0024] It also includes the browning step, strictly controls the amount of micro-etching, does not allow mixed pressing, and strictly follows the process procedure to press to ensure the quality of the hole wall.

[0025] It also includes the drilling steps, controlling the hole shape to 100-105um, the hole bottom to be greater than 85um, the hole wall roughness to be controlled to ≤25um, using a new drill, reducing the feed speed, limiting the life of the drill tip, and measuring the CPK value to ensure the drilling quality.

[0026] It also includes plasma degumming and horizontal copper deposition steps, and the degumming rate is controlled at 0.15-0.35mg / cm 2 To ensure the surface cleanliness before copper plating; after copper plating, the blind holes must be filled, the DP value must be controlled ≤10um, and the surface copper is controlled at the median value to ensure uniform copper plating.

[0027] It also includes multiple copper reduction steps to control the copper foil thickness to 8-12um, the extreme value of copper thickness on the board surface to be controlled within 3um, and pay attention to controlling the scratch phenomenon.

[0028] It also includes the steps of making the outer layer circuits, using high-sensitivity dry film for exposure and development, controlling the exposure PE value to 60um, and the pre-processing production speed to operate under specific conditions to ensure the best exposure environment and development conditions; the minimum line width and line spacing of the production draft is .101 / 0.066mm, and the minimum spacing is 0.051MM.

[0029] It also includes the etching step to ensure that there are no burrs in the etching. It is forbidden to use the grinding brush after etching. The impedance line width and the normal line width are measured to ensure that they are consistent with the actual line width of the inner layer.

[0030] It also includes solder mask pre-treatment and character production steps. Brushing and sandblasting are prohibited in solder mask pre-treatment. White characters are used for characters, and the text is clear. PAD cannot be used, and the finished product impedance test is carried out after the characters are written.

[0031] It also includes shape processing and flying probe test steps. The shape tolerance is controlled at ±0.1MM, and the flying probe test strictly controls scratches, board warping and test leakage.

[0032] It also includes OSP processing and final quality control steps, strictly controlling OSP rework to ensure the consistency of circuit copper thickness; the pads and BGA shapes and sizes of the same component are consistent to meet the high quality requirements of server high-speed boards.

[0033] Embodiment 2

[0034] Based on the first embodiment, a method for manufacturing a fourth-order HDI high-speed board for a server is proposed, and the electroplating hole filling method comprises the following steps:

[0035] Step 1: Cut the material, cut the 12-layer four-stage four-step pressing HDI blind hole board. The core board thickness is 0.15MM H / H OZ. One large material is produced by cutting 6 working boards (Shengyi / Lianmao two types of boards).

[0036] Step 2: Inner layer lines L5-L6 / L7-L8; the minimum line width and line spacing of the inner layer line manuscript is 0.060 / 0.060mm, the minimum line width and line spacing of the production manuscript is 0.070 / 0.050mm, the minimum spacing: 0.050MM, the routing compensation of the original manuscript 0.06MM is 0.01MM, the customer accepts the minimum line width of the finished product is 0.03MM, and the other routing compensation is 0.025MM.

[0037] Step 3: Inner layer inspection L6 / L7-L8; inner layer inspection is prohibited from patching.

[0038] Step 4: Press once; pay attention to controlling expansion and contraction, use 1 / 3OZ copper foil for pressing, the inner hole to the line of the laser hole is 0.1MM, and the inner hole to the line of the through hole and buried hole is 0.15MM.

[0039] Step 5: One laser for L4-L9; One laser for L8-9 layers: The laser is only used to drill the electroplating side holes in order to burn out the inner target for the circuit layer alignment.

[0040] Step 6: Horizontal copper deposition L4-L9; plasma degumming is required before horizontal copper deposition, and the degumming rate is controlled at 0.15-0.35mg / cm 2 .

[0041] Step 7: Fill L4-L9 holes at one time; the blind holes must be filled and leveled when filling holes at one time, the DP value must be controlled to be ≤10um, and the surface copper must be controlled to the median value (measure 9 points, control ≤22um, to ensure uniform copper plating).

[0042] Step 8: Reduce copper L4-L9 at one time; after reducing copper once, the thickness of copper foil is 8-12um, the extreme value of copper thickness on the board surface is controlled at 3UM, and it is managed according to the median value, and attention is paid to controlling scratches.

[0043] Step nine: Drill tool holes L4-L9; Use a ≤4 drill tip to drill tool holes 2.004, lower the feed speed by 0.20, and control the scratches during the process.

[0044] Step 10: L4-L9 of the primary circuit; the copper foil of the entire board of the primary circuit, the minimum copper bridge is 0.127MM, and this copper bridge cannot be disconnected, otherwise it will be open. Minimum spacing: 0.064MM, the outer layer is produced with high-sensitivity dry film, the exposure LDI machine grabs the internal target exposure, the PE value uses 60um exposure, the pre-processing production speed is operated according to the P1.25 light board conditions, the speed is 2.5 meters, and the film pressing is 3 meters; Quality control points: The circuit production of this board must ensure the best exposure environment and the best development conditions, and it is best to produce it 2 hours after the new cylinder.

[0045] Step 11: Primary electroplating L4-L9; surface copper thickness is controlled at 20-25um, and the copper plating extreme difference is controlled at 3-5um.

[0046] Step 12: Etch L4-L9 at one time; there should be no burrs during etching, and brushing is prohibited after etching. Measure the impedance line width and ordinary line width and refer to the actual line width of the inner layer to ensure consistency and matching of each layer.

[0047] Step 13: Check L4-L9 once; the high-speed board cannot be patched.

[0048] Step 14: Secondary lamination; During the secondary lamination, pay attention to controlling the expansion and shrinkage, use 1 / 3OZ copper foil for lamination, the inner hole of the laser hole is 0.1MM to the line, and the inner hole of the through hole and buried hole is 0.15MM to the line. The amount of micro-etching of browning is controlled to be 1.2~1.5um; mixed pressing is not allowed, and the pressing is strictly carried out according to the pressing program provided by the process. 00% expansion and shrinkage are measured, and the piles are processed and marked according to the process requirements. Use new steel plates for lamination, and the PP powder and PP fiber wefts of the transport vehicle must be cleaned up. The outer layer AOI with small spacing cannot be repaired. 100% check for browning white spots before outsourcing laser.

[0049] Step 15: Secondary laser L3-L10; Secondary laser, L9-10 layer laser is only used to make electroplating side holes, in order to burn out the inner target for the circuit layer alignment, the second hole type is 105-110UM, and the bottom of the hole is larger than 85UM.

[0050] Step 16: Horizontal copper deposition L3-L10; external plasma degumming is also required.

[0051] Step 17; Secondary filling of L3-L10 holes; Blind holes must be filled and leveled during filling, DP value control ≤10um, surface copper control median management (measure 9 points, control ≤22um, ensure uniform copper plating).

[0052] Step 18: Secondary copper reduction L3-L10; after the secondary copper reduction, the copper foil thickness is 8-12um, the extreme value of the copper thickness on the board is controlled at 3UM, and it is managed according to the median value, paying attention to controlling scratches.

[0053] Step 19: Drill buried holes L3-L10; buried hole diameter 0.225MM, hole wall roughness controlled at ≤25UM, thickness-diameter ratio 4.89:1; drill buried hole 0.225 with a new drill, feed speed down 0.2, measure CPK≥1.33 or above. Quality control points: specify the machine with the highest temperature and set the machine to drill holes, 1 piece 1 stack; each PNL is illuminated at the four corners to ensure no biased holes; hole roughness is controlled to be less than 22UM; control scratches. Step 20: Second copper deposition board electroplating L3-L10; external plasma degumming, vertical copper deposition; board electroplating twice, positive and negative clamping, using 0.75ASD*25min, control the uniformity of the bottom copper (COV≥90%). Step 21; Secondary lines L3-L10; Minimum line width and line spacing of original manuscript: 0.060 / 0.060mm, minimum line width and line spacing of production manuscript: 0.070 / 0.050mm, minimum spacing 0.050MM, use high-sensitivity dry film (1630SN), the routing compensation of 0.06MM of original manuscript is 0.01MM, the minimum line width of the finished product accepted by the customer is 0.03MM, and the other routing compensation is 0.025MM; the outer layer is produced with high-sensitivity dry film, the exposure LDI machine grabs the internal target exposure, the PE value uses 60um exposure, the pre-processing production speed is operated according to the P1.25 light board conditions, the speed is 2.5 meters, and the film is pressed for 3 meters. Quality control points: The circuit production of this board must ensure the best exposure environment and the best development conditions, and it is best to produce it 2 hours after the new cylinder.

[0054] Step 22: Secondary electroplating L3-L10; hole copper control ≥10um, surface copper thickness 20-25um. Step 23: Secondary etching L3-L10; etching should not have burrs, and brushing is prohibited after etching. Measure the impedance line width and ordinary line width and refer to the actual line width of the inner layer to ensure consistency and matching of each layer.

[0055] Step 24: Secondary inspection of L3-L10; high-speed boards cannot be patched.

[0056] Step 25; Three times of pressing; Three times of pressing, pay attention to control the expansion and shrinkage, use 1 / 3OZ copper foil for pressing, the inner hole of the laser hole is 0.1MM to the line, and the inner hole of the through hole and the buried hole is 0.15MM to the line. Pay attention to control the expansion and shrinkage during the three pressings, use 1 / 3OZ copper foil for pressing, the inner hole of the laser hole is 0.1MM to the line, and the inner hole of the through hole and the buried hole is 0.15MM to the line. Browning controls the micro-etching amount of 1.2~1.5um; cannot be mixed, and must be pressed strictly according to the pressing program provided by the process. 00% measurement of expansion and shrinkage, and mark the piles according to the process requirements. Use new steel plates for pressing and arranging plates, and clean the PP powder and PP fiber weft wires on the transport vehicle. The outer layer AOI with small spacing cannot be repaired. 100% inspection of browning white spots before outsourcing laser.

[0057] Step 26: Three times of laser L2-L11; three times of hole type according to 100-105UM, the bottom of the hole is greater than 85UM; control the scratching; parameter control according to different materials to make blind holes and slice the first piece.

[0058] Step 27: Horizontal copper deposition L2-L11; plasma degumming is required before horizontal copper deposition, and the degumming rate is controlled at 0.15-0.35mg / cm 2 .

[0059] Step 28: Fill holes L2-L11 three times; fourth-order HDI, three lasers.

[0060] Step 29; reduce copper L2-L11 three times; after three times of copper reduction, the copper foil thickness is 8-12um, the extreme value of copper thickness on the board surface is controlled at 3UM, and it is managed according to the median value, and attention is paid to controlling scratches.

[0061] Step 30: Drill the peripheral tool holes L2-L11; use a ≤4 drill bit to drill the tool hole 2.004, and reduce the feed speed by 0.20; control the scratches.

[0062] Step 31: Three-time circuit L2-L11; large copper foil on the whole board, the minimum copper bridge is 0.09MM, this copper bridge cannot be disconnected, otherwise it will be open. Use high-sensitivity dry film (1630SN), minimum spacing: 0.05MM; the outer layer is produced with high-sensitivity dry film, exposure LDI machine grabs the internal target exposure, PE value uses 60um exposure, pre-processing production speed is operated according to P1.25 light board conditions, speed 2.5 meters, lamination 3 meters. Quality control points: The circuit production of this board must ensure the best exposure environment and the best development conditions, and it is best to produce it 2 hours after the new cylinder.

[0063] Step 32: Electroplating L2-L11 three times; surface copper thickness is controlled at 20-25um.

[0064] Step 33: Etch L2-L11 three times; there should be no burrs on the etching, and grinding and brushing are prohibited after etching. Measure the impedance line width and ordinary line width and refer to the actual line width control of the inner layer to ensure consistency and matching of each layer.

[0065] Step 34: Check L2-L11 three times; high-speed boards cannot be patched.

[0066] Step 35: Lamination for four times; Lamination for four times, pay attention to control the expansion and shrinkage, use 1 / 3OZ copper foil for lamination, the inner hole of the laser hole is 0.1MM to the line, and the inner hole of the through hole and buried hole is 0.15MM to the line. Browning controls the micro-etching amount to 1.2~1.5um; mixed pressing is not allowed, and lamination is strictly carried out according to the lamination program provided by the process. 00% expansion and shrinkage are measured, and the piles are processed and marked according to the process requirements. Use new steel plates for lamination and layout, and the PP powder and PP fiber wefts of the transport vehicle must be cleaned up. The outer layer AOI with small spacing cannot be repaired. 100% check for browning white spots before outsourcing laser.

[0067] Step 36: Four times of laser blasting; the fourth hole type is 100-105UM, the bottom of the hole is larger than 85UM, and the scratching is controlled.

[0068] Step 37: Horizontal copper deposition; Plasma degumming is required before horizontal copper deposition, and the degumming rate is controlled at 0.15-0.35mg / cm 2 .

[0069] Step 38: Fill the holes four times; the blind holes must be filled when filling the holes, the DP value must be controlled to be ≤10um, and the surface copper must be controlled to the median value (measure 9 points, control ≤22um, to ensure uniform copper plating).

[0070] Step 39: Reduce copper four times; after four times of copper reduction, the thickness of the copper foil is 8-12um, and the extreme value of the copper thickness on the board is controlled at 3UM. Manage it according to the median value and pay attention to controlling scratches.

[0071] Step 40: Drilling; buried hole diameter 0.25MM, hole wall roughness controlled at ≤25UM, thickness-to-diameter ratio 6:1; drill 0.25 with a new drill, feed speed reduced by 0.40, drill tip life reduced by 500 hole limits, measured CPK ≥ 1.33 or above; quality control points: specify the machine temperature to set the machine for drilling; each PNL illuminates the four corners to ensure no deflected holes; hole roughness is controlled to be less than 22UM.

[0072] Step 41: Electroplating of copper-plated board; plasma degumming is required, vertical copper deposition, copper thickness of board ≥6um; board electroplating twice, front and back clamping, using 0.75ASD*25min, to control the uniformity of bottom copper. Step 42: Outer layer circuit; the minimum line width and line spacing of the original manuscript: 0.076 / 0.091mm, the minimum line width and line spacing of the production manuscript: 0.101 / 0.066mm, the minimum spacing is 0.051MM, the outer layer is produced using high-sensitivity dry film, the exposure LDI machine grabs the internal target exposure, the PE value uses 60um exposure, the pre-processing production speed is operated according to the P1.25 light board conditions, the speed is 2.5 meters, and the film pressing is 3 meters. Quality control points: The circuit production of this board needs to ensure the best exposure environment and the best development conditions, and it is best to produce it 2 hours after the new cylinder.

[0073] Step 43: Graphic electroplating; hole copper 10um, surface copper thickness 20-25um, original minimum line width and line spacing: 0.076 / 0.091mm, production minimum line width and line spacing: 0.101 / 0.066mm, minimum spacing 0.051MM, control copper plating extreme difference 3-5um.

[0074] Step 44: alkaline etching; there should be no burrs during etching, and brushing is prohibited after etching. Measure the impedance line width and ordinary line width and refer to the actual line width of the inner layer to ensure consistency and matching of each layer.

[0075] Step 45; Mid-term inspection: High-speed boards cannot be patched, and consistency must be ensured during impedance testing.

[0076] Step 46: Solder mask; grinding, brushing and sand blasting are prohibited before solder mask treatment.

[0077] Step 47: Characters: Use white characters, the text should be clear, and no PAD should be used. After the characters are printed, the impedance of the finished product is tested.

[0078] Step 48: Molding; shape tolerance ±0.1MM.

[0079] Step 49: Testing: Flying probe test, control scratches, board warping, and strictly control test leakage. Step 50: OSP: Strictly control OSP rework to ensure the consistency of circuit copper thickness.

[0080] Step 51: FQC; the pads of the same component must be of the same size, and the BGA shape must be of the same size.

[0081] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for manufacturing a fourth-order HDI high-speed board for a server, Features: The method includes multiple lamination steps, using copper foil of specific thickness, ensuring that the distance from the inner hole to the line meets the design requirements, strictly controlling the expansion and contraction during the lamination process, and performing expansion and contraction testing and marking.

2. A method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes a browning step, strictly controls the amount of micro-etching, does not allow mixed pressing, and strictly follows the process procedure for pressing to ensure the quality of the hole wall.

3. A method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes the drilling steps, controlling the hole shape to 100-105um, the hole bottom to be larger than 85um, the hole wall roughness to be controlled at ≤25um, using a new drill, reducing the feed speed, limiting the life of the drill tip, and measuring the CPK value to ensure the drilling quality.

4. A method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes plasma degumming and horizontal copper deposition steps, and the degumming rate is controlled at 0.15-0.35mg / cm 2 To ensure the surface cleanliness before copper plating; after copper plating, the blind holes must be filled, the DP value must be controlled ≤10um, and the surface copper must be controlled at the median value to ensure uniform copper plating.

5. The method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes multiple copper reduction steps to control the copper foil thickness to 8-12um, the extreme value of copper thickness on the board surface to be controlled within 3um, and pay attention to controlling the scratch phenomenon.

6. A method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes the steps of making the outer layer circuits, using high-sensitivity dry film for exposure and development, controlling the exposure PE value to 60um, and the pre-processing production speed to operate under specific conditions to ensure the best exposure environment and development conditions; the minimum line width and line spacing of the production draft is .101 / 0.066mm, and the minimum spacing is 0.051MM.

7. A method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes the etching step to ensure that there are no burrs in the etching. It is forbidden to use the grinding brush after etching. The impedance line width and the normal line width are measured to ensure that they are consistent with the actual line width of the inner layer.

8. A method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes solder mask pre-treatment and character production steps. Brushing and sandblasting are prohibited in solder mask pre-treatment. White characters are used for characters, and the text is clear. PAD cannot be used, and the finished product impedance test is carried out after the characters are written.

9. The method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes shape processing and flying probe test steps. The shape tolerance is controlled at ±0.1MM, and the flying probe test strictly controls scratches, board warping and test leakage.

10. The method for manufacturing a fourth-order HDI high-speed board for a server according to claim 1, Features: It also includes OSP processing and final quality control steps, strictly controlling OSP rework to ensure the consistency of circuit copper thickness; the pads and BGA shapes and sizes of the same component are consistent to meet the high quality requirements of server high-speed boards.