Attachment of object to base through intermediate heat sink
Through a two-stage fixation method, using a combination of pressure sintering and welding, the deficiencies of welding and pressure sintering when fixing semiconductor power modules are solved, high-quality heat transfer and mechanical connection are achieved, and production flexibility and quality control are improved.
Patent Information
- Application Number
- CN202410508256.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-26
- Filing Date
- 2024-04-25
- Publication Date
- 2024-10-29
AI Technical Summary
When fixing semiconductor power modules to base components in the existing technology, the welding method can easily cause the solder layer to become soft and damaged, the pressure sintering method is complex and difficult to achieve high-quality uniform heat transfer and mechanical solidity, and lacks effective non-destructive quality. measurement technology, resulting in production flexibility and quality control difficulties.
A two-stage fixing method is adopted: first, the middle heat sink is fixed to the interface side of the attached object by pressure sintering to form a pressure sintered body layer, and then the middle heat sink is fixed to the base part by welding, forming a solder layer, and on each Non-destructive measurements and electrical performance testing are performed at each stage to ensure quality.
It improves the heat transfer performance of attached objects and the reliability of mechanical connections, reduces production waste, enhances production flexibility and quality control feasibility, and avoids the need for complex tooling for welding and pressure sintering.
Smart Images

Figure CN118866698A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a manufacturing method for fixing an attachment object (e.g., a semiconductor power module) to a base component (e.g., to a heat sink, a heat sink, and / or a cooler (a part for a cooler)). It also relates to an assembly comprising a base component and an attachment object fixed relative to the base component. Background Art
[0002] The manufacturing method is applicable to the manufacture of a power module assembly. Such a power module assembly (hereinafter referred to as an "assembly") may include several attached objects fixed to a base component. Typically, the assembly is configured to form a part of an electrical circuit, such as a powertrain circuit of an electric vehicle. Nowadays, the demand for electric vehicles (especially electric vehicles) is growing rapidly.
[0003] The power module assembly, in particular the objects to which it is attached, is adapted to exhibit the required electrical functions. At least some of the attached objects may be semiconductor power modules. These may include insulated gate bipolar transistors (IGBTs) and / or metal oxide semiconductor field effect transistors (MOSFETs).
[0004] During operation of the circuit, the attached object generates heat, in particular due to the current. In order to avoid overheating and damage of the attached object, the attached object is fixed to the base component. Usually, the base component is a heat sink, a heat sink and / or a cooler (a part for a cooler). The base component receives a considerable part of the heat generated by the attached object and dissipates it further.
[0005] The attachment object should be fixed to the base component in a manner that allows sufficient heat transfer from the attachment object to the base component. In addition, the mechanical connection between the attachment object and the base component should be reliable.
[0006] Typically, the attached object is fixed directly to the base component by welding. Fixing by welding is relatively easy and has low manufacturing cost. However, the solder layer between the attached object and the base component tends to soften and is eventually damaged due to high temperature peaks occurring at the interface side of the attached object directly facing the solder layer. During operation, the attached object (e.g., a semiconductor power module) is sometimes "pulsed" heated. The heat generation of the attached object may be uneven over time. In addition, the heat generated by the internal components of a single attached object may be spatially unevenly distributed at the interface side of the attached object.
[0007] Alternatively, the attached object can also be fixed directly to the base component by pressure sintering. A sintering layer consisting of a sintering material is provided between the attached object and the base component. During the subsequent curing step, the sintering material is heated to a maximum sintering temperature. In addition, the attached object and the base component are pressed together, for example, along a normal direction, which can be perpendicular to the interface side. The curing step densifies and solidifies the sintered material. A pressure sintered body layer is formed directly between the attached object and the base component by the sintering layer. The pressure sintered body layer permanently fixes the attached object directly to the base component. The pressure sintered body layer is less susceptible to damage by high temperature peaks occurring at the interface side of the attached object. However, it is relatively difficult and demanding to fix the semiconductor power module directly to the base component by pressure sintering. It requires more complex tools and is generally more expensive than fixing by welding. In particular, since the attached object and the base component must be pressed together evenly to obtain a thin and uniform pressure sintered body layer, the tool should be adapted to the individual shapes of the attached object and the base component. This results in a high workload and low production flexibility for manufacturing different types of components.
[0008] Often, different secondary manufacturers (hereinafter referred to as customers) use the same type of attachment object (e.g., semiconductor power module) for different purposes, such as for manufacturing different customer-specific components. Since pressure sintering is difficult and demanding, some customers have problems with adequate quality when fixing the attachment object to their customer-specific base component by means of pressure sintering.
[0009] A high quality of the pressure sintered body layer must be ensured, so that sufficient heat transfer from the attached object to the base component is exhibited and the fixation is mechanically strong. No voids or delaminations should be noticeable in or at the pressure sintered body layer. Currently, there are no adequate measurement techniques to check the quality of the pressure sintered body connection formed directly between the attached object and the base component in sufficient detail in a non-destructive manner in industrial production. The measurement techniques are either too slow or too expensive for reasonable quality control in industrial production, or the measurement resolution is too low to detect smaller voids or delaminations of the pressure sintered body layer, or the measurement is hampered by the complex and / or irregular internal structure of the attached object and the base component.
[0010] Typically, several attachment objects are fixed to the base component simultaneously by pressure sintering in one common curing step. However, due to the increased temperature and pressure required for pressure sintering, some of the attachment objects become at risk of damage during the pressure sintering process. Since the resulting pressure sintered body layer is rigid and permanently fixes the attachment objects to the base component, if only one attachment object is damaged during pressure sintering, the entire assembly must be discarded. Summary of the invention
[0011] The problem is to provide a way of fixing an attachment object to a base part which exhibits high reliability in operation and flexibility in production.
[0012] This problem is solved by a production method for fixing an attachment object to a base component according to claim 1 .
[0013] The manufacturing method comprises the following steps:
[0014] - providing an intermediate heat sink as a supplement to the attached object;
[0015] - fixing the intermediate heat sink to the interface side of the attachment object by pressure sintering, thereby forming a pressure sintered body layer between the interface side and the object side of the intermediate heat sink; and
[0016] - The intermediate heat sink, to which the attachment object is pressure-sintered, is fixed to the base member by soldering, thereby forming a solder layer between the base member and a base side of the intermediate heat sink opposite to the object side.
[0017] In other words, the attached object is fixed to the base component by a two-stage fixing process. The first stage includes fixing the intermediate heat sink to the interface side of the attached object by pressure sintering. The second stage includes fixing the intermediate heat sink to the base component by pressure sintering the attached object to the intermediate heat sink. The first stage and the second stage can be performed at different locations and / or by different tools. For example, the first stage can be performed at a primary manufacturing facility and the second stage can be performed at a secondary manufacturing facility. The first stage and the second stage, the corresponding tools and the corresponding quality checks can be optimized separately.
[0018] The intermediate heat sink to which the attachment object is pressure sintered may be referred to as a "first stage subassembly." An "assembly" may include a base component having at least one first stage subassembly fixed thereto (according to the second stage).
[0019] On the one hand, the pressure sintered body layer is less susceptible to damage by excessively high temperatures during operation than the solder layer. On the other hand, forming the pressure sintered body layer is more demanding than forming the solder layer. It requires more complex tools and checking the quality can be more difficult. Vice versa, forming the solder layer requires less complex tools and is easier.
[0020] Using the disclosed method, the more demanding first stage can be performed centrally, such as at the same primary manufacturing facility, while the second stage can be performed at different secondary manufacturing facilities. For example, different customers can manufacture their final components at their own secondary manufacturing facilities.
[0021] In the final assembly (e.g., as described below), the attached object (e.g., semiconductor power module) typically generates heat during operation. The heat should be transferred to the base component and further dissipated through the base component. Spatial temperature peaks and / or temporal temperature peaks may occur at the interface side of the attachment side.
[0022] The pressure sintered body layer adjacent to the heat generating attachment object is more temperature resistant and exhibits a good heat transfer from the attachment object to the intermediate heat sink. The connection directly adjacent to the interface side must be of very good quality.
[0023] The intermediate heat sink is configured to protect the solder layer from high temperatures.
[0024] The intermediate heat sink spreads the heat received from the attached object. The intermediate heat sink flattens the spatial and / or temporal high temperature peaks (and corresponding spatial and / or temporal heat flow peaks) generated by the attached object. Typically, the temperature and heat flow at the base side of the intermediate heat sink are more uniform than at the interface side of the attached object. The risk of high temperature peaks at the base side is much lower than the risk of high temperature peaks at the interface side. Therefore, the connection between the intermediate heat sink and the base component can be formed by a solder layer (rather than a pressure sintered body layer) without compromising the reliability of the final assembly.
[0025] Typically, during operation, a temperature gradient between the object side and the susceptor side, i.e., a temperature gradient along the normal direction within the intermediate heat sink, occurs anyway. Even without taking into account spatial and / or temporal high temperature peaks, the temperature at the susceptor side is typically lower than the temperature at the object side.
[0026] The normal direction may be perpendicular to the intermediate heat sink, in particular perpendicular to its object side surface (at least where the pressure sintered body layer is formed).
[0027] There are no very strict requirements on the quality of the solder layer, for example on voids in the solder layer. Firstly, the solder layer is shielded against high temperature peaks by the intermediate heat sink. Secondly, the heat flow is introduced more uniformly into the solder layer rather than into the pressure sintered body layer. Thirdly, the solder layer is cooled directly by the base component. Therefore, inhomogeneities and / or local defects in the solder layer are less likely to impair the performance and / or reliability of the component.
[0028] The pressure sintered body layer is made of a sintered material by pressure sintering. The sintered material is disposed between the attached object and the intermediate heat sink, more specifically, between the interface side and the object side. Pressure sintering includes applying heat and pressure to the sintered material. Pressure sintering densifies and solidifies the sintered material. As a result, a pressure sintered body layer is produced from the sintered material.
[0029] According to one aspect, the manufacturing method may include (the following steps):
[0030] After the intermediate heat sink is fixed to the attachment object by pressure sintering, but before the intermediate heat sink is fixed to the base member by pressure sintering the attachment object to the intermediate heat sink,
[0031] - non-destructive measurement of the pressure sintered body layer and / or
[0032] - Testing of electrical properties exhibited by said attached object.
[0033] If the non-destructive measurement shows that the quality of the pressure sintered body layer in a first-stage assembly is unacceptable, only the relevant first-stage subassembly needs to be discarded. No base component should be wasted. Furthermore, if multiple first-stage subassemblies should be fixed to the same base component, only the first-stage subassembly with the unacceptable pressure sintered body layer must be discarded; the other ones of the first-stage subassemblies do not need to be wasted. The non-destructive measurement of the pressure sintered body layer can be performed for each first-stage subassembly individually.
[0034] During the pressure sintering process, the attached object is subjected to increased pressure and elevated temperature. During the pressure sintering process, it may be damaged. Even if it exhibits the desired electrical properties before pressure sintering, this may no longer be guaranteed after the pressure sintering is completed (i.e., when the attached object becomes part of the first stage subassembly). According to this aspect, each first stage subassembly can be individually tested for the electrical characteristics exhibited by the attached object, and any defective first stage subassembly can be selectively sorted before it becomes fixed to the base component (even before additional first stage subassemblies can be fixed to the base component). This helps to reduce production waste.
[0035] The non-destructive measurement of the pressure sintered body layer may include scanning acoustic microscopy (SAM) of the pressure sintered body layer. SAM can be performed after the intermediate heat sink is fixed to the interface side of the attached object by pressure sintering, but before the intermediate heat sink to which the attached object is pressure sintered is fixed to the base component by welding. The measurement can be implemented from the side of the intermediate heat sink. In particular, an acoustic detection wave can be emitted from the side of the intermediate heat sink toward the pressure sintered body layer, for example, at least substantially along the normal direction, and a reflection carrying the information to be measured can be detected at one side of the intermediate heat sink. SAM checks the quality of the completed pressure sintered body layer in a non-destructive manner.
[0036] It would be difficult to inspect the pressure sintered body layer by applying the SAM from the side of the attached object. The attached object may include a complex and / or irregular structure, which may impair the measurement if the sound waves (e.g., incident waves and / or reflections) must pass through the attached object. In addition, the base component may have a complex and / or irregular structure, such as having multiple cooling fins and / or multiple coolant channels, etc. The complex and / or irregular structure of the base component may impair the measurement if the sound waves (e.g., incident sound waves and / or reflections) must pass through the base component.
[0037] Therefore, if the attached object is fixed directly to the base component by means of a conventionally positioned pressure sintered body layer, it is difficult or even impossible to reliably check the quality of such a conventionally positioned pressure sintered body layer by means of SAM. The two-stage fixing according to the invention allows reliable non-destructive measurement of the final pressure sintered body layer between the attached object and the intermediate heat sink before the intermediate heat sink to which the attached object has been fixed is further fixed to the base component.
[0038] According to another aspect, the manufacturing method may include (the following steps):
[0039] - Non-destructive measurement of solder layers using X-rays.
[0040] Despite any complex and / or irregular structure of the base component and any complex and / or irregular structure of the attached object, non-destructive measurement of the solder layer can be performed using X-rays. It is fast and cost-effective.
[0041] As mentioned above, there are no very strict requirements for voids in the solder layer. The required quality can be adequately checked by measurement using X-rays.
[0042] The manufacturing method may include the following steps:
[0043] - arranging a sintering slurry and / or a sintering paste between the intermediate heat sink and the attachment object.
[0044] More generally, the sintering material may include (especially consist of) a sintering paste and / or a sintering slurry.
[0045] The sintered material may include metal particles and at least one volatile component. The metal particles may include silver particles and / or copper particles, or may be silver particles and / or copper particles. The volatile component(s) may be organic. The density of the sintered material may be 2.5 g / cm 3 Up to 3.5g / cm 3 The sintering material can be applied in a wet state in the application step, for example, to the object side and / or the interface side.
[0046] The sintering material may be pre-dried. In particular, the manufacturing method may include a step of pre-drying the sintering material, for example after the applying step and before placing the attachment object on the object side, the sintering material between the attachment object and the object side. At least a portion of the volatile organic components evaporates during the pre-drying process, for example at least 70%.
[0047] According to one aspect, forming a pressure sintered body layer (for permanently fixing the attached object to the intermediate heat sink) may include sintering at a maximum sintering temperature in the range of 200°C to 300°C and / or at a maximum sintering pressure in the range of 10MPa to 40MPa. This ensures proper sintering and therefore ensures a rigid and secure fixation of the attached object to the intermediate heat sink. The increased pressure reduces the risk of voids in the pressure sintered body layer and helps the pressure sintered body layer to become particularly dense and thin. This facilitates good thermal conductivity from the attached object to the intermediate heat sink. Ultimately, this improves the reliability of the final assembly in operation.
[0048] In one embodiment, the thickness of the pressure sintered body layer (e.g., along the normal direction) is a maximum of 70 μm. Additionally or alternatively, the thickness of the pressure sintered body layer may be at least 20 μm. The thickness of the pressure sintered body layer may be 50 μm ± V. For example, V may be 10 μm or 6 μm. The thickness of the pressure sintered body layer may be less than the thickness of the previous sintered layer (i.e., the sintered material layer before pressure sintering occurs). The density of the pressure sintered body layer may be higher than the density of the previous sintered layer. The pressure sintered body layer may be made of at least 90% (by weight), at least 96% (by weight) metal, for example resulting from the metal material proportion of the sintered material. The density of the pressure sintered body layer may at least substantially correspond to the density of the metal material proportion of the sintered material.
[0049] In one embodiment, the base component is made of metal. Additionally or alternatively, the base component may be a heat sink, a heat sink and / or a cooler (part for a cooler).
[0050] The base component may be configured to dissipate heat to at least one fluid, such as to ambient air and / or a coolant.
[0051] The base component may comprise cooling fins, such as rectangular fins / ribs and / or pin fins. Additionally or alternatively, the base component may comprise grooves and / or walls for forming coolant channels.
[0052] In particular, the base component can be made of aluminum (including aluminum alloys). This facilitates the manufacture of complex structures of the base component by stamping and forging, such as cooling fins and / or grooves for forming coolant channels. In addition, aluminum is cheaper than copper. In contrast, copper (including copper alloys) promotes a firm and reliable fixation of the pressure sintered body layer and exhibits higher thermal conductivity. Since the base component is indirectly fixed to the accessory via the solder layer, the intermediate heat sink and the pressure sintered body layer, in other words, since the pressure sintered body layer is not directly fixed to the base component, and since the intermediate heat sink protects the base component from high temperatures, the present invention allows the advantages of both materials to be utilized.
[0053] According to a more general aspect, the intermediate heat sink may be made of a different material than the base member.
[0054] Fixing the intermediate heat sink with the attached object pressure sintered thereto to the base component by welding may include (i.e., be performed by or assisted by) heating the base component with a hot fluid, such as hot air. Since the base component may be configured to dissipate heat to at least one fluid and vice versa, it may be easily heated by subjecting it to a hot fluid. This allows for inexpensive welding and non-complex tools. Furthermore, it facilitates the use of the same heating tool for base components with different complex cooling structures.
[0055] According to one aspect, the attachment object may be or may include at least one of the following:
[0056] -Heating components;
[0057] - electronic components, such as semiconductor components; and
[0058] -Semiconductor power modules.
[0059] In particular, the attachment object may be a semiconductor power module.A semiconductor power module may include at least one semiconductor component.
[0060] Electronic components and semiconductor power modules may generate heat during operation; therefore they may also be considered as heat-generating components, respectively.
[0061] The semiconductor component may include or consist of a semiconductor switch, an insulated gate bipolar transistor (IGBT), a metal oxide semiconductor field effect transistor (MOSFET), etc.
[0062] Such an attached object, for example such a semiconductor power module, may include different layers and / or components.
[0063] In particular, the attached object may include or consist of a molded semiconductor power module. This is a semiconductor power module with a resin cover. The resin cover can be manufactured by resin transfer molding. If a plurality of attached objects form part of an assembly, at least one of them, a part of them or all of them may include or consist of a molded semiconductor power module, respectively.
[0064] The manufacturing method may include the step of forming a resin cover.
[0065] The resin cover may be formed before the intermediate heat sink with the attachment object pressure-sintered thereto is fixed to the base member by welding.
[0066] The resin cover may be formed before the intermediate heat sink is fixed to the interface side of the attachment object by pressure sintering.
[0067] Alternatively, the resin cover may be formed after the intermediate heat sink is fixed to the interface side of the attached object by pressure sintering. In this case, it may be advantageous to perform non-destructive measurement of the pressure sintered body layer and / or testing of the electrical properties exhibited by the attached object after (the step of) forming the resin cover. By doing so, damage to the attached object caused by forming the resin cover after the heat sink is fixed to the attached object will also be detected.
[0068] According to one aspect, the attachment object may comprise an integrated heat sink at the interface side, wherein the pressure sintered body layer fixes the intermediate heat sink (directly) to the integrated heat sink.
[0069] In one embodiment, the attachment object includes an insulating layer, an internal circuit layer (directly) fixed to the insulating layer, and at least one semiconductor component fixed to the insulating layer and / or the internal circuit layer.
[0070] In particular, the insulating layer may be (directly) fixed to the integrated heat sink (at a side of the integrated heat sink facing away from the interface side). The insulating layer may be arranged between the integrated heat sink and the inner circuit layer. The insulating layer may be made of a ceramic material.
[0071] The attached object may further include any, several or all of the following:
[0072] - an internal fixing layer (e.g., an internal pressure sintered body layer) for fixing the semiconductor component to the insulating layer and / or the internal circuit layer,
[0073] - bonding wires, and
[0074] -Resin cover ("Molded semiconductor power module").
[0075] The internal pressure sintered body layer (within the semiconductor power module) and the pressure sintered body layer can be cured by the same curing step. In this case, it is advantageous to form the resin cover after fixing the intermediate heat sink to the interface side of the attachment object by pressure sintering.
[0076] In one embodiment, the attached object (e.g., a semiconductor power module) includes a direct copper bond (DCB) structure. It may include a substrate, such as a ceramic substrate, forming an insulating layer. In addition, the DCB structure may include an insulating layer and one or both of an internal circuit layer and an integrated heat sink.
[0077] In one embodiment, the intermediate heat sink is made of copper, is planar, and / or has a thickness in the range of 2 mm to 4 mm.
[0078] In this case, "copper" may include pure copper and copper alloys. It is particularly easy to form a strong mechanical connection and good thermal conductivity between the intermediate heat sink and the pressure sintered body layer of the intermediate heat sink made of copper (including copper alloys).
[0079] The intermediate heat sink may have no (additional) metallization. For example, the intermediate heat sink may be made of one single bulk material. This reduces costs.
[0080] Forming the intermediate heat sink may include rolling. In other words, the intermediate heat sink may be made of rolled material, in particular rolled metal. This is a cost-effective and reliable way of ensuring the planarity and smoothness of the intermediate heat sink. This in turn helps to obtain a particularly thin and uniform pressure sintered body layer.
[0081] The intermediate heat sink can have a simple geometry. Pressure sintering requires the use of a suitable pressure sintering tool. Using an intermediate heat sink with a simple geometry allows the use of a simple and efficient sintering tool. In addition, the intermediate heat sink can be manufactured quickly and cost-effectively. In particular, as described above, the intermediate heat sink can be flat (planar). It can have a rectangular shape, a polygonal shape, a disc shape, etc. In one embodiment, it has a rectangular shape.
[0082] For example, the intermediate heat exchanger may be free of cooling fins and cooling channels.
[0083] If the intermediate heat sink is flat (planar), this facilitates uniform transfer of heat from the pressure sintering tool to the sintering material via the intermediate heat sink during pressure sintering. Furthermore, it is particularly easy to apply uniform pressure to the sintering material during pressure sintering. The flat shape allows the use of efficient planar sintering tools for pressure sintering.
[0084] The plan shape of the intermediate heat sink can be adapted to the plan shape of the attached object at the interface side. This simplifies the handling of the first stage subassembly. Furthermore, the first stage subassembly can be easily fitted into a corresponding recess in the base component.
[0085] In particular, the area size of the intermediate heat sink may be at least substantially the same as the area size of the interface surface. For example, the area size of the intermediate heat sink may deviate from the area size of the interface surface by at most 10%.
[0086] According to one aspect, the intermediate heat sink may cover at least the complete integrated heat sink. This ensures a good heat transfer to the intermediate heat sink.
[0087] According to another aspect, when the intermediate heat sink is fixed to the attached object by the pressure sintered body layer, the intermediate heat sink can cover the attached object in a fitting manner at the interface side. In other words, the intermediate heat sink can be configured so that the attached object overlaps with the intermediate heat sink in a fitting manner. According to another aspect, the pressure sintered body layer can also be shaped accordingly.
[0088] In particular, the side walls of the intermediate heat sink (which may be parallel to the normal direction) and the attached object may be flush with each other.
[0089] In one embodiment, the base component comprises a recess for receiving the intermediate heat sink, wherein the shape of the recess at least substantially matches the planar shape of the intermediate heat sink. This facilitates the correct positioning of the first stage subassembly at the base component. Furthermore, the solder layer may (at least partially) extend between the side walls of the intermediate heat sink and the side walls of the recess. By doing so, the heat transfer from the intermediate heat sink to the base component may be enhanced. Furthermore, the recess may help ensure a correct position of the soldering material.
[0090] In particular, the area dimension of the recess may be in the range of 1.01 to 1.20 times the area dimension of the intermediate heat sink. This tolerance is large enough to facilitate insertion of the intermediate heat sink, small enough to ensure sufficient correct alignment of the first stage subassembly with the base component, and small enough that the solder layer may (at least partially) extend between the sidewalls of the intermediate heat sink and the sidewalls of the recess.
[0091] The above mentioned problems are further solved by an assembly comprising a base member and an attachment object fixed relative to the base member,
[0092] wherein the assembly comprises an additional intermediate heat sink (additional interconnecting heat sink) arranged between the base member and the attachment object, and
[0093] wherein the pressure sintered body layer fixes the object side of the intermediate heat sink to the attachment object, and the solder layer fixes the base side of the intermediate heat sink opposite to the object side to a base member.
[0094] Features and advantages described with regard to the production method apply correspondingly to the component and vice versa.
[0095] According to one aspect, the attachment object and the intermediate heat sink may be (permanently) fixed to the base component by the manufacturing method disclosed herein.
[0096] The attachment object may be a semiconductor power module comprising at least one semiconductor component. Additionally or alternatively, the base component is a heat sink, a heat sink and / or a cooler.
[0097] In one embodiment, the attachment product includes:
[0098] - an integrated heat sink fixed (directly) to an intermediate heat sink via a pressure sintered body layer,
[0099] - an insulating layer fixed (directly) to an integrated heat sink, and
[0100] - an inner circuit layer fixed (directly) to said insulating layer.
[0101] In particular, the attachment object may be a semiconductor power module, and at least one semiconductor component is fixed to the insulation layer and / or the circuit layer (eg, by an internal fixing layer of the semiconductor power module, such as an internal pressure sintered body layer).
[0102] According to one aspect, the above-mentioned problem is solved by an assembly comprising a base component and at least two sub-assemblies, wherein each of the sub-assemblies comprises an attachment object, an intermediate heat sink (additional interconnected heat sink) arranged between its attachment object and the base component, and a pressure sintered body layer, wherein the pressure sintered body layer fixes the object side of the intermediate heat sink to the attachment object, wherein the base sides of the intermediate heat sinks opposite to their object sides are respectively fixed to the base component by welding.
[0103] Additional features, advantages and possible applications of the invention are derived from the following description of exemplary embodiments and the accompanying drawings. All features described and / or illustrated graphically herein form the subject matter of the invention individually or in any desired combination, regardless of how they are combined in the claims or in their reference to previous claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0104] Preferred embodiments of the present invention will now be described with reference to the accompanying drawings, in which:
[0105] Figure 1Schematically illustrates an example of a manufacturing method with a two-stage fixing process, the two-stage fixing process comprising a first stage including pressure sintering for forming a first-stage subassembly having an attachment object fixed to an intermediate heat sink by a pressure sintered body layer, and a second stage including fixing the first-stage subassembly to a base component by welding;
[0106] Figure 2 The first stage is symbolically illustrated;
[0107] Figure 3 An embodiment of a first stage subassembly is shown in which the interface side of the attached object is attached to the object side of the intermediate heat sink via a pressure sintered body layer;
[0108] Figure 4 Schematically shows a non-destructive measurement for checking the quality of a pressure sintered body layer;
[0109] Figure 5 An exemplary embodiment of a base component is shown;
[0110] Figure 6 The second stage is symbolically illustrated;
[0111] Figure 7 A first embodiment of an assembly formed by the manufacturing method is shown;
[0112] Figure 8 schematically illustrates a non-destructive measurement for checking the quality of a solder layer; and
[0113] Fig. 9 A second embodiment of an assembly formed by the manufacturing method is shown. DETAILED DESCRIPTION
[0114] Figure 1 An example of a manufacturing method according to the present disclosure is shown.
[0115] Step S10 is intended to provide an intermediate radiator 30. For example, Figure 2 One embodiment of an intermediate radiator 30 can be seen in FIG.
[0116] The intermediate heat sink 30 should be made of a material with high thermal conductivity. For example, the intermediate heat sink 30 is made of metal. Figure 2 In the exemplary embodiment shown, the intermediate heat sink 30 is made of copper (which may also include copper alloys).
[0117] The intermediate heat sink 30 is flat (planar). The normal direction N may be perpendicular to the intermediate heat sink 30. In particular, the normal direction N is perpendicular to the object side 32 of the intermediate heat sink 30.
[0118] The intermediate heat sink 30 has a shape conforming to the shape of the interface side 51 of the attachment object 50 to be fixed to the object side 32 of the intermediate heat sink 30 in a plane perpendicular to the normal direction N. For example, the intermediate heat sink 30 has a rectangular shape.
[0119] The intermediate radiator 30 may be made of a rolled material. Therefore, the thickness T is particularly uniform and can be precisely controlled. In addition, the base side 31 (which faces away from the object side 32) and the object side 32 of the intermediate radiator 30 are smooth and planar, respectively. Step S10 may include manufacturing the intermediate radiator 30 by rolling and / or cutting a rolled material.
[0120] Furthermore, the manufacturing method may include a step S20 for applying a sintered material. The sintered material is disposed between the object side 32 of the intermediate heat sink 30 and the interface side 51 of the attached object. Figure 2 As shown, a sintering slurry 41 can be applied to the object side 32 to which the attached object 50 is to be fixed. The sintering slurry 41 includes metal particles, such as silver particles and / or copper particles. This ensures high thermal conductivity of the post-sintered body layer 40 formed by pressure sintering of the sintering slurry 41. The sintering slurry 41 includes at least one organic volatile component and is applied in a wet state. This facilitates the application of the sintering slurry 41. The applied sintering material can form a sintered layer with a thickness in the range of 80μm to 200μm, for example, 150μm±V, where V can be 10μm or 6μm. The temporary sintering layer must not be confused with the final pressure sintered body layer 40.
[0121] In the embodiment shown, the attachment object 50 is a semiconductor power module. It includes a direct copper bonding (DCB) structure 52. The DCB structure 52 includes an insulating layer 54 formed by a ceramic substrate. The DCB structure 52 also includes an integrated heat sink 53 directly fixed to the insulating layer 54 at the interface side 51. On the side opposite to the interface side 51 (along the normal direction N), the internal circuit layer 55 of the DCB structure 52 is directly fixed to the insulating layer 54. The integrated heat sink 53 must not be confused with the intermediate heat sink 30.
[0122] Furthermore, the attachment object 50, e.g. Figure 2 The semiconductor power module shown may include at least one semiconductor component 57, such as a semiconductor switch, an insulated gate bipolar transistor (IGBT), a metal oxide semiconductor field effect transistor (MOSFET), etc. The semiconductor component 57 may include a die or be composed of a die. The semiconductor component 57 may be fixed to the DCB structure 52, for example, by an internal pressure sintered body layer 56. In some embodiments (not shown), the attached object 50 may include a plurality of semiconductor components 57. They may all be of the same type or may be of different types.
[0123] The attachment object 50 may further include bonding wires, such as bonding wires 60 for electrically connecting the semiconductor component 57 to the internal circuit layer 55, such as Figure 2 and Figure 3 Optionally, it may include a mechanical buffer layer 59 attached to the corresponding semiconductor component 57. The bonding buffer layer 59 may help to bond the bonding wire relative to the corresponding semiconductor component 57. For example, the bonding buffer layer 59 may be fixed to the corresponding semiconductor component 57 by another internal pressure sintered body layer 58.
[0124] The attachment object 50 may include an electrical connector 61. The electrical connector 61 may be used to connect to the same final assembly 210 (see Fig. 9 , with a plurality of first-stage subassemblies 80, each subassembly including at least one semiconductor power module) to establish electrical connections with other attachment objects 50, such as other semiconductor power modules, and / or with other electrical components, such as other electrical components of a powertrain circuit. In one embodiment, the electrical connector(s) 61 may be formed by a lead frame.
[0125] The attachment object 50 may be Figure 2 It may even include a prefabricated resin cover 62 '(such as Figure 2 as shown by the dashed line in the figure).
[0126] However, the manufacturing method may include one or more steps of forming / manufacturing the attachment object 50 .
[0127] For example, the manufacturing method may include a step S50 of forming the resin covers 62', 62 of the attached object 50. Forming the resin covers 62', 62 may include resin transfer molding.
[0128] The resin cover 62' may be formed before the intermediate heat sink 30 is fixed to the attachment object 50 by pressure sintering (see Figure 2 In this case, with Figure 1 Differently, step S50 may be performed before step S30.
[0129] The resin covers 62', 62 protect the internal components of the attachment object 50 from physical and / or chemical damage. In another variation, the attachment object 50 does not include any resin covers 62', 62 at all.
[0130] Step S30 is related to pressure sintering, which is used to form the first stage subassembly 80 (see Figure 3 ), wherein the attachment object 50 is fixed to the intermediate heat sink 30 through the pressure sintered body layer 40.
[0131] exist Figure 2, arrow A1 symbolically shows that the intermediate heat sink 30 is fixed to the interface side 51 of the attached object 50 by pressure sintering, thereby forming a pressure sintered body layer 40 between the interface side 51 of the intermediate heat sink 30 and the object side 32 (see Figure 3 ). This occurs during step S30.
[0132] Figure 3 The pressure sintered body layer 40 is composed of Figure 2 The sintering slurry 41 at the object side 32 shown in FIG. 3 is formed. Step S30 comprises a curing step performed by means of a pressure sintering tool.
[0133] The curing step may include applying pressure to the sintered material (e.g., by a pressure sintering tool) within a sintering pressure range of 10 MPa to 40 MPa, in variations of 15 MPa to 30 MPa. This may include subjecting the sintered material to a high temperature treatment, particularly while the sintering temperature ranges from 200° C. to 300° C. The temperature may be maintained within the sintering temperature range and / or the applied pressure may be maintained within the sintering pressure range for a duration of 2 minutes to 10 minutes.
[0134] The thickness of the resulting pressure sintered body layer 40 may be in the range of 20 μm to 70 μm.
[0135] The pressure sintered body layer 40 permanently and rigidly fixes the attached object 50 to the intermediate heat sink 30. It exhibits high thermal conductivity from the attached object 50 (particularly from the integrated heat sink 53) to the intermediate heat sink 30.
[0136] According to another aspect, step S30 may also include fixing the semiconductor component(s) 57 to the DCB structure 52 by pressure sintering and / or fixing the joint buffer 59 to the respective semiconductor component 57 by pressure sintering. In other words, one, several or all of the internal pressure sintered body layers 56, 58 of the same attached object 50 may be formed together with the pressure sintered body layer 40, in particular in a common curing process and / or within the same pressure sintering tool.
[0137] Thus, the step S20 for applying a sintering material may include providing a sintering material, such as a sintering paste and / or sintering slurry(s) for forming one, more or all of the internal pressure sintered body layers 56 , 58 .
[0138] Of course, step S30 may include arranging all the components to be pressure sintered together in a kit to be sintered, and placing the kit into a pressure sintering tool.
[0139] Optionally, the manufacturing method may include a bonding and / or welding step S40 for attaching bonding wire(s) 60 and / or electrical connector(s) 61. Of course, this should be done before forming the resin covers 62', 62.
[0140] The resin cover 62 may be formed after step S30 (and, if applicable, after step S40). This facilitates forming the inner pressure sintered body layers 56, 58 together with the pressure sintered body layer 40 within the attached object 50, and in particular curing them together in a single curing step.
[0141] Pressure sintering requires providing heat to the sintering material. Typically, the resin caps 62, 62' provide only limited thermal conductivity. Therefore, if the resin caps 62 are formed after pressure sintering, pressure sintering can become easier and more efficient. However, forming the resin caps 62' before pressure sintering can facilitate processing at the location where pressure sintering occurs.
[0142] Figure 3 The resulting first stage subassembly 80 is shown, which includes fixing the intermediate heat sink 30 to the interface side 51 of the attached object 50 by pressure sintering, thereby forming a permanent and rigid pressure sintered body layer 40 between the interface side 51 and the object side 32 of the intermediate heat sink 30. Figure 3 , the first stage subassembly includes an optional resin cover 62 .
[0143] Optionally, the manufacturing method includes a step S60 of testing the electrical characteristics exhibited by the attached object 50, for example, the desired switching function. Since there is some risk of damage to components of the attached object 50 during step S30 and / or step S40 (if applicable), step S50 may be performed afterwards. In other words, step S60 may be used to test the electrical characteristics of the first-stage subassembly 80.
[0144] Additionally or alternatively, the manufacturing method may include a step S70 of performing non-destructive measurements on the pressure sintered body layer 40. Step S70 may include inspecting the quality of the pressure sintered body layer 40. The testing may reveal voids within the pressure sintered body layer 40, thickness variations of the pressure sintered body layer 40, and / or delamination between the pressure sintered body layer 40 and any one of the interface side 51 and the object side 32.
[0145] A suitable exemplary measurement method is scanning acoustic microscopy (SAM) from the base side 31 of the intermediate heat sink 30. An acoustic probe wave can be emitted from the base side 31 toward the pressure sintered body layer 40. The reflected acoustic wave portion can be detected. SAM can be performed using a SAM head 90, such as Figure 4The SAM head 90 can be moved at the base side 31 in an xy plane perpendicular to the normal direction N. Of course, other methods can be used to obtain spatial resolution in addition or alternatively.
[0146] Evaluation unit 91 may automatically evaluate signals detected by SAM head 90 to determine the quality of pressure sintered body layer 40. Optionally, discard mechanism 92 automatically instructs and / or performs discarding of any first stage subassembly 80 where the quality of pressure sintered body layer 40 is deemed insufficient by evaluation unit 91.
[0147] Since the configuration of the DCB structure 52 (especially the integrated heat sink 53 and the insulating layer 54 ) is relatively uniform in the xy plane, step S70 may even include non-destructive measurement of the internal pressure sintered body layer 56 in the same manner.
[0148] Of course, step S70 must be performed after step S30 and before step S100 explained below. Figure 1 In a variation of the present invention, step S70 may be performed before any one of steps S40, S50, S60, S80, S90 and S100.
[0149] The manufacturing method may optionally include a step S80 of delivering the first stage subassembly 80 to another manufacturing facility. For example, at least step S30 may be performed in a primary manufacturing facility, and step S80 is intended to deliver the first stage subassembly 80 to a secondary manufacturing facility. For example, Figure 1 Steps S90 to S110 in may be performed at a secondary manufacturing facility, for example, where a customer purchases the first stage subassembly to be fixed to the manufacture of a customer-specific base component 10 , 210 .
[0150] Step S90 involves providing a base component 10 , 210 . Figure 5 An exemplary base component 10 in the form of a heat sink is shown. The base component 10 is made of aluminum (including aluminum alloys). It includes a side 12 to which the base side 31 of the intermediate heat sink 30 is fixed by welding in step S100. This side can be referred to as the heat sink side 12. The side 11 of the base component 10 opposite to the heat sink side 12 can be referred to as the dissipation side 11, which includes a plurality of cooling fins 14, for example, pin fins and / or rectangular fins.
[0151] exist Figure 5 In the illustrated embodiment, a recess 13 for receiving the intermediate radiator 30 is formed at the radiator side 1 2. The size and shape of the recess 13 are configured to help secure the first stage subassembly 80 in place and properly aligned. The bottom of the recess 13 is flat.
[0152] In other variations (not shown), the heat sink side 12 may be at least substantially flat.
[0153] Step S100 is directed to welding the first stage subassembly 80 to the base member 10. The second stage of manufacturing consists of Figure 6 The solder material 21 to be transformed into the solder layer 20 is provided between the base side 31 of the intermediate heat sink 30 and the bottom of the corresponding recess 13 at the heat sink side 12 of the base component 10. The first-stage subassembly 80, the solder material 21 and the base component 10 are joined together so that the base side 31 directly abuts the solder material 21 at a first side along the normal direction N, and the bottom of the recess 13 directly abuts the solder material 21 at a second side opposite to the first side.
[0154] Figure 7 The assembly 100 resulting from step S100 is shown. The attachment object 50 is permanently fixed to the base member 10 via the pressure sintered body layer 40, the intermediate heat sink 30, and the solder layer 20. At this point, the attachment object 50 is fixed to the base member 10 indirectly.
[0155] Compared to the solder layer 20, the pressure sintered body layer 40 is less susceptible to damage by spatial and / or temporal high temperature peaks that may occur at the interface surface 51 during operation. For example, the semiconductor component(s) 57, the bonding wire(s) 60, the internal circuit layer 55 and / or the electrical connector 61 may generate heat in operation. Due to the internal structure of the attached object 50, the heat is generated spatially non-uniformly. In addition, since the operation of the attached object 50 may include switching currents, such as currents of a powertrain circuit, the generation of heat may be non-uniform in time.
[0156] The intermediate heat sink 51 protects the solder layer 20 from high temperatures. Even in the case where the heat generation is constant in time during operation, a temperature gradient generally occurs along the normal direction N. The temperature at the base side 31 (and therefore at the solder layer 20) is generally lower than the temperature at the interface side 51 (and therefore at the pressure sintered body layer 40). In addition, the intermediate heat sink 51 dissipates spatial and temporal heat peaks.
[0157] The assembly 100 may be configured for high current operation, however, the solder layer 20 is produced by soldering without increasing the risk of failure in operation.
[0158] The intermediate heat sink 30 may completely cover the interface side 51 of the attached object 50, e.g. Figure 3In particular, the intermediate heat sink 30 can completely overlap the integrated heat sink 53. In addition, the pressure sintered body layer 40 can at least completely cover the integrated heat sink 53 (at the interface side 51). This allows the heat generated by the attached object 50 during operation to be optimally transferred to the intermediate heat sink 30.
[0159] Typically, it is much easier for secondary production facilities to fasten components together by welding than by pressure sintering. The required tools and processing are less complex. In addition, the disclosed manufacturing method and assembly 80 allow for reduced quality requirements on the solder layer 20.
[0160] The fixation directly at the interface surface 51 is most critical due to the high temperature peaks and the corresponding thermal stresses. With the disclosed method, the more complex and difficult process of pressure sintering the fixation layer (i.e., the pressure sintered body layer 40) directly adjacent to the interface side 31 can be centralized at one single primary manufacturing facility. However, even at different secondary manufacturing facilities, the same type of first stage subassembly 80 can be easily welded to various customer-specific base components 10, 210 by cost-effective welding.
[0161] In addition to this, the pressure sintering step S30 is more efficient, more flexible and cheaper than in the case where different customers fix the attachment object directly to their customer-specific base component by pressure sintering. There is no need to adapt the pressure sintering tool to the shape of the base component 10. In addition, the intermediate heat sink 30 has a smaller thickness and / or a smaller heat capacity than the base component 10. Therefore, heating the sintered material in step S30 can be carried out faster and with less energy than in the case where the pressure sintered body layer is formed directly at the base component 10. In addition to this, the heat transfer from the pressure sintering tool in step S30 is particularly high because the base side 31 is flat and does not have cooling fins 14 with interposed gaps.
[0162] For example, the thickness T of the intermediate heat sink 30 may be in the range of 2 mm to 4 mm (see Figure 3 ). On the one hand, the thickness T is large enough to provide a beneficial shielding for the solder layer 20. On the other hand, it is thinner than the base member 10.
[0163] Compared to the case where the attachment object is directly fixed to the base member by pressure sintering, the quality requirements of the solder layer 20 can be more easily checked in a non-destructive manner.
[0164] Step S110 involves non-destructive measurement of the solder layer 20. One suitable exemplary measurement method is X-ray measurement. The X-ray source 95 can emit X-rays, and the X-rays can pass through the component 100 having the solder layer 20. The X-rays that have passed through the component 100 can be detected by the X-ray detector 96. The X-ray detector 96 can exhibit spatial resolution. Naturally, as a supplement or alternative, other methods can be used to obtain spatial resolution.
[0165] Evaluation unit 97 may automatically evaluate the signals detected by X-ray detector 96 to determine the quality of solder layer 20. Optionally, rejection mechanism 98 automatically instructs and / or performs the rejection of any component 100 in which the quality of solder layer 20 is deemed insufficient by evaluation unit 97.
[0166] Fig. 9 A further embodiment of a (semiconductor power module) assembly 200 is shown. The same reference numerals are used for the same elements and the above explanations apply correspondingly. Only the differences are pointed out.
[0167] exist Fig. 9 In the embodiment of the present invention, the base member 210 of the assembly 200 is a cooler. It includes a channel structure having a fluid inlet 216, a fluid outlet 217 and internal fluid channels 215. Inner walls 214 are formed between adjacent fluid channels 215.
[0168] The base member 210 may be configured to be cooled by a coolant, such as water.
[0169] However, step S100 may include heating the base component 210 for welding by passing a hot fluid (eg, hot air) through the channel structure. Fig. 9 This is schematically shown by the arrow HF in the middle.
[0170] According to another aspect, the assembly 200 includes three first-stage subassemblies 80. Each of them is fixed to the base component 210 by welding, particularly including step S100. One, two or all of the first-stage subassemblies 80 may conform to Figure 3 The embodiment shown.
[0171] Reference numerals:
[0172] 10, 210 base parts
[0173] 11 Dissipation side
[0174] 12 Radiator side
[0175] 13 recess
[0176] 14 Cooling fins
[0177] 20 Solder layer
[0178] 21. Welding materials
[0179] 30 Intermediate radiator
[0180] 31 Base side
[0181] 32 Object side
[0182] 40 Pressure sintered body layer
[0183] 41. Sintering paste (sintering material)
[0184] 50 Attached object (e.g. semiconductor power module)
[0185] 51 Interface side
[0186] 52 Direct Copper Bonding (DCB) Structure
[0187] 53 Integrated heat sink
[0188] 54 Insulation layer
[0189] 55 Internal circuit layer
[0190] 56, 58 Internal pressure sintered body layer
[0191] 57 Semiconductor components
[0192] 59 Joint buffer
[0193] 60 Bonding wire
[0194] 61 Electrical connector
[0195] 62', 62 resin cover
[0196] 80 First stage subcomponents
[0197] 90 Scanning Acoustic Microscopy (SAM) Head
[0198] 91, 97 Evaluation Units
[0199] 92, 98 discard mechanism
[0200] 95 X-ray source
[0201] 96 X-ray detector
[0202] 100, 200 Components
[0203] 214 Inner wall
[0204] 215 Internal fluid passage
[0205] 216 Fluid inlet
[0206] 217 Fluid outlet
[0207] A1 Arrow (Phase 1)
[0208] A2 Arrow (Phase 2)
[0209] HF Arrow (Hot Fluid)
[0210] N Normal direction
[0211] T Thickness.
Claims
1. A manufacturing method for fixing an attachment object (50) to a base component (10, 210), the method comprising the following steps: - providing an intermediate heat sink (30) as a supplement to the attachment object (50); - fixing the intermediate heat sink (30) to the interface side (51) of the attachment object (50) by pressure sintering, thereby forming a pressure sintered body layer (40) between the interface side (51) and the object side (32) of the intermediate heat sink (30); and - fixing the intermediate heat sink (30) - wherein the attachment object (50) is pressure-sintered to the intermediate heat sink (30) - to the base component (10, 210) by welding, thereby forming a solder layer (20) between the base component (10, 210) and a base side (31) of the intermediate heat sink (30) opposite to the object side (32).
2. The manufacturing method according to claim 1, characterized in that: After the intermediate heat sink (30) is fixed to the attachment object (50) by pressure sintering, but before the intermediate heat sink (30) - wherein the attachment object (50) is pressure sintered to the intermediate heat sink (30) - is fixed to the base member (10, 210), - non-destructive measurement of the pressure sintered body layer (40) and / or - Testing of electrical properties exhibited by said attached object (50).
3. The manufacturing method according to claim 2, wherein the non-destructive measurement of the pressure sintered body layer (40) comprises scanning acoustic microscopy of the pressure sintered body layer (40).
4. The manufacturing method according to any one of the preceding claims, characterized in that: - Non-destructive measurement of the solder layer (20) using X-rays.
5. The manufacturing method according to any one of the preceding claims, characterized in that: - a sintering slurry and / or sintering paste (41) is arranged between the intermediate heat sink (30) and the attachment object (50).
6. A method of manufacturing according to any one of the preceding claims, wherein: Forming the pressure sintered body layer (40) includes: sintering at a maximum sintering temperature in the range of 200°C to 300°C and a maximum sintering pressure in the range of 10MPa to 40MPa.
7. The manufacturing method according to any of the preceding claims, wherein the base component is made of metal and is a heat sink, a heat sink (10) and / or a cooler (210).
8. The manufacturing method according to any one of the preceding claims, wherein the attachment object (50) is or includes at least one of the following: -Heating components (55, 57, 59, 60, 61); - a semiconductor component (57); and - A semiconductor power module (50).
9. A manufacturing method according to any one of the preceding claims, wherein the attached object (50) includes an integrated heat sink (53) at the interface side (51), wherein the pressure sintered body layer (40) fixes the intermediate heat sink (30) to the integrated heat sink (53).
10. The manufacturing method according to any one of the preceding claims, wherein the attachment object (50) comprises: An insulating layer (54), an internal circuit layer (55) fixed to the insulating layer (54), and at least one semiconductor component (57) fixed to the insulating layer (54) and / or the internal circuit layer (55).
11. The manufacturing method according to any of the preceding claims, wherein the intermediate heat sink (30) is made of copper, is formed flat, and has a thickness (T) ranging from 2 mm to 4 mm.
12. The manufacturing method according to any one of the preceding claims, wherein a planar shape of the intermediate heat sink (30) is adapted to a planar shape of the attachment object (50) at the interface side (51).
13. The manufacturing method according to any one of the preceding claims, wherein the base component (10, 210) comprises a recess (13) for receiving the intermediate heat sink (30), wherein the shape of the recess (13) is at least substantially adapted to the planar shape of the intermediate heat sink (30).
14. An assembly (100, 200) comprising a base component (10, 210) and an attachment object (50) fixed relative to the base component (10, 210), It is characterized in that The assembly (100, 200) comprises an additional intermediate heat sink (30) arranged between the base component (10, 210) and the attached object (50); The pressure sintered body layer (40) fixes the object side (32) of the intermediate heat sink (30) to the attached object (50), and the solder layer (20) fixes the base side (31) of the intermediate heat sink (30) opposite to the object side (32) to the base component (10, 210).
15. The assembly (100, 200) according to claim 14, wherein the attachment object (50) is a semiconductor power module comprising at least one semiconductor component (57), wherein the base component is a heat sink, a heat sink (10) and / or a cooler (210).
16. The assembly (10, 210) of claim 15, wherein the attachment object (50) further comprises - an integrated heat sink (53) fixed to the intermediate heat sink (30) by means of the pressure sintered body layer (40), - an insulating layer (54) fixed to the integrated heat sink (53), and - an internal circuit layer (55) fixed to the insulating layer (54), The at least one semiconductor component (57) is fixed to the insulating layer (54) and / or the internal circuit layer (55).
Citation Information
Patent Citations
Method for low-temperature pressure sintering
CN101952960A
Power module, power semiconductor device, and method for manufacturing power semiconductor device
CN115939061A
Power module substrate, power module substrate with metal part, power module with metal part, method for producing power module substrate, and method for producing power module substrate with metal part
US20160219693A1