Surface processing technology of mylar material
By forming an anti-glare AG layer and a wear-resistant AF layer on the surface of the Maila material and printing an ink layer on it, the problem of low durability and quality of the Maila material is solved, the wear resistance and aesthetics of the material are improved, and the Reliability of notebooks.
Patent Information
- Application Number
- CN202410934061.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-01
AI Technical Summary
The existing Maila materials cannot withstand under long-term friction, resulting in low durability and quality in the mouse board area of the notebook, and a processing technology is needed to improve the wear resistance of Maila materials on the surface.
By forming an anti-glare AG layer and a wear-resistant AF layer on the surface of the Maila material, the surface roughness of the AG layer is 0.3 μm to 0.7 μm, the thickness of the AF layer is 10-25 nm, the AF layer is obtained by coating technology, and A colorful ink layer is printed on it to improve the aesthetics and wear resistance of the material.
It improves the surface wear resistance and aesthetics of the Maila material, enhances the reliability and durability of the notebook, reduces the coefficient of dynamic and static friction, has high hardness on the surface and no scratches, making it suitable for manual operation.
Smart Images

Figure CN118876562A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wear-resistant Mylar materials, in particular to a surface processing technology of Mylar materials. Background Art
[0002] The mouse pad area of a laptop is made of thick Mylar material. Due to the long-term sliding friction of the user's fingers, the Mylar material in this area needs to have wear-resistant properties. The existing Mylar material cannot currently withstand long-term friction. To ensure the reliable quality of the laptop, it is urgent to develop a processing technology to improve the wear resistance of the Mylar material surface. Summary of the Invention
[0003] In response to the above problems, the present invention provides a surface processing technology for Mylar material, which improves the surface wear resistance of the Mylar material and thereby improves the reliability and durability of the notebook.
[0004] A surface processing process for Mylar material is characterized in that: an anti-glare AG layer is pre-laminated on the upper layer of the Mylar material, and the surface roughness of the AG layer is 0.3μm to 0.7μm. Then, a wear-resistant AF layer is compounded on the upper surface of the AG layer, and the thickness of the AF layer is 10-25nm.
[0005] The further feature is that the AG layer is specifically a texture layer with a surface roughness of 0.4 μm to 0.6 μm obtained by pressing the upper surface of the Mylar material through a UV mold;
[0006] The AF layer is obtained by placing the Mylar material that has been pressed to form the AG layer in a coating machine for coating;
[0007] The coating time of AF layer in the coating machine is 15min~20min;
[0008] The thickness of the AF layer obtained by coating in the coating machine is 15 to 20 nm;
[0009] Mylar material is a transparent material. After the AF layer is obtained by coating, a colorful ink layer is printed on the lower surface of the Mylar material, thereby improving the aesthetics of the entire Mylar material.
[0010] The upper surface of the AF layer was rubbed 10,000 times with an EF74 eraser (100g weight) at a rubbing speed of 60 cycles / min. No obvious marks were left on the surface after rubbing. The change in water drop angle before and after rubbing was less than 10%, and the change in glossiness was less than 2°.
[0011] The surface hardness of the AF layer is high, with a pencil hardness of ≥2H / 500g and no scratches;
[0012] The dynamic and static friction coefficient of the obtained material surface is less than 0.1um.
[0013] The internal composition ratio of the printing ink, the ratio of the color ink and the varnish, is calculated and mixed in proportion so that the original color ink is converted into the color of the corresponding transmittance through the dilution of the varnish, so that the entire Mylar material looks beautiful when the back light source is turned on.
[0014] After adopting the above technical solution, the surface roughness of the AG layer is 0.3μm~0.7μm, and the thickness of the AF layer is 10~25nm. The adjustment improves the surface roughness of the AG layer while thickening the film thickness of the AF layer. This makes the surface of the Mylar material have a skin feel and high wear resistance. It improves the surface wear resistance of the Mylar material, thereby improving the reliability and durability of the notebook. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 Schematic diagram of a process applicable to the present invention;
[0016] The names corresponding to the serial numbers in the figure are as follows:
[0017] Mylar material 10 , AG layer 20 , AF layer 30 , ink layer 40 . DETAILED DESCRIPTION
[0018] A surface processing process for Mylar material, comprising the following steps:
[0019] a. An anti-glare AG layer 20 is formed on the upper layer of the Mylar material 10 by UV mold lamination. The surface roughness of the AG layer 20 is 0.55±0.1μm, and the roughness of the UV mold is 0.5μm.
[0020] b. The AF layer 30 is obtained by placing the Mylar material that has been pressed to form the AG layer 20 in a coating machine for coating. The coating time of the AF layer 30 in the coating machine is 15 minutes to 20 minutes. The thickness of the AF layer 30 obtained by coating in the coating machine is 15 to 20 nm.
[0021] c. The Mylar material 10 is a transparent material. After the AF layer 30 is obtained by coating, a colorful ink layer 40 is printed on the lower surface of the Mylar material, thereby improving the aesthetics of the entire Mylar material.
[0022] The upper surface of the Mylar material obtained after the specific implementation was rubbed 10,000 times with an EF74 rubber load of 100g at a rubbing speed of 60 cycles / min. No obvious marks were left on the surface after the rubbing. The change in water drop angle before and after rubbing was less than 10%, and the change in glossiness was less than 2°.
[0023] The surface hardness of the whole material is high, with pencil hardness ≥2H / 500g without scratches;
[0024] The dynamic and static friction coefficient of the obtained material surface is less than 0.1um.
[0025] The internal composition ratio of the printing ink, the ratio of the color ink and the varnish, is calculated and mixed in proportion so that the original color ink is converted into the color of the corresponding transmittance through the dilution of the varnish, so that the entire Mylar material looks beautiful when the back light source is turned on.
[0026] In specific implementation, after the AG layer 20 is formed, the Mylar material 10 changes from a previously glossy surface to a matte surface. Simultaneously, the light transmittance of the transparent Mylar is reduced. The AF layer 30 is then formed by coating. The resulting material surface has a dynamic and static friction coefficient of less than 0.1 μm, making it suitable for touch operation. When the set color is translucent blue, the internal component ratio of the printing ink is calculated to be blue ink: varnish = 3:2. After mixing according to the ratio, the original blue ink becomes semi-transparent through dilution of the varnish, while the ink properties remain unchanged. The product is then printed using a 420# screen to obtain an ink layer 40. Testing has shown that using a screen with a larger mesh size will produce a screen print, which is extremely obvious under backlighting. Therefore, a 420# screen print is selected for printing.
[0027] After adopting the process of the present invention, the surface roughness of the AG layer is 0.55±0.1μm, and the thickness of the AF layer is 10-25nm. The adjustment improves the surface roughness of the AG layer while thickening the film thickness of the AF layer. This makes the surface of the Mylar material have a skin feel and high wear resistance. This improves the surface wear resistance of the Mylar material, thereby improving the reliability and durability of the notebook.
[0028] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the invention can be embodied in other specific forms without departing from the spirit or essential characteristics of the invention. Therefore, the embodiments should be considered in all respects as illustrative and non-restrictive, and the scope of the invention is defined by the appended claims, not the foregoing description, and all variations within the meaning and range of equivalents of the claims are intended to be included therein. Any reference sign in a claim should not be construed as limiting the claim to which it relates.
[0029] In addition, it should be understood that although this specification is described in terms of implementation methods, not every implementation method contains only one independent technical solution. This narrative method of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.
Claims
1. A surface processing technology of Mylar material, characterized by: The anti-glare AG layer is pre-laminated on the upper layer of the Mylar material, and the surface roughness of the AG layer is 0.3μm to 0.7μm. Then, a wear-resistant AF layer is compounded on the upper surface of the AG layer, and the thickness of the AF layer is 10-25nm.
2. The surface processing technology of Mylar material according to claim 1, characterized in that: The AG layer is specifically a texture layer having a surface roughness of 0.4 μm to 0.6 μm obtained by pressing a UV mold on the upper surface of the Mylar material.
3. The surface processing technology of Mylar material according to claim 1, characterized in that: The AF layer is obtained by placing the Mylar material that has been pressed to form the AG layer in a coating machine for coating.
4. The surface processing technology of Mylar material according to claim 3 is characterized by: The coating time of the AF layer in the coating machine is 15min to 20min.
5. The surface processing technology of Mylar material according to claim 4, characterized in that: The AF layer is coated in a coating machine to obtain a layer thickness of 15 to 20 nm.
6. The surface processing technology of Mylar material according to claim 1, characterized in that: Mylar material is a transparent material. After the AF layer is obtained by coating, a colorful ink layer is printed on the lower surface of the Mylar material.
7. The surface processing technology of Mylar material according to claim 1, characterized in that: The upper surface of the AF layer was rubbed 10,000 times with an EF74 rubber with a load of 100g and a rubbing speed of 60 cycles / min. There was no obvious mark on the surface after the friction. The change in water drop angle before and after friction was less than 10%, and the change in glossiness was less than 2°.
8. The surface processing technology of Mylar material according to claim 1, characterized in that: The surface of the AF layer has high hardness, with a pencil hardness of ≥2H / 500g and no scratches.
9. The surface processing technology of Mylar material according to claim 1, characterized in that: The dynamic and static friction coefficient of the obtained material surface is less than 0.1um.
10. The surface processing technology of Mylar material according to claim 1, characterized in that: The internal composition ratio of the printing ink, the ratio of the color ink and the varnish, is calculated and mixed in proportion so that the original color ink is diluted with the varnish to become the color of the corresponding transmittance, so that when the back light source is turned on, the entire Mylar material looks beautiful.
Citation Information
Patent Citations
Multifunctional optical film and composite thereof, as well as multifunctional optical plate and manufacturing method thereof
CN103360709A
Anti-dazzle electronic grade glass and manufacture technology thereof
CN108549502A
Cover glass used for keyboards and computer touch pads
CN109704587A
Micro-nano transfer printing material based on matrix material and preparation method of micro-nano transfer printing material
CN115895008A
Integrated color printing process for AG (anti-glare) glass