Paper diaper with multiple layers of core bodies

Through the multi-layer core structure, the combination of high-expanded water-absorbing resin and high-magnification water-absorbing resin is used to solve the problems of poor water absorption and insufficient skin care effect of diapers, and the good water absorption and buttock protection effect of diapers are achieved, keeping the surface of diapers dry , comfortable to use.

CN118892399APending Publication Date: 2024-11-05HANGZHOU QIANDAOHU TIANXIN CO LTD

Patent Information

Application Number
CN202410891440.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-04
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

When existing diapers fit on the baby's buttocks for a long time, the water absorption is poor, resulting in redness and inflammation on the baby's buttocks. The pearl powder is prone to fall off and oxidation during transportation and storage, which cannot effectively improve the water absorption effect.

Method used

Using a multi-layer core structure, including a conductive layer, a skin care layer, a support layer and a reinforcement layer. A high-expansion water-absorbing resin and a skin care room are set up in the skin care layer. The support layer is polyester fiber, and a high-magnification water-absorbing resin in the reinforcement layer. The membrane is made of Made of wood pulp and polyester resin, it is easy to break and release skin care substances after exposure to water, keeping the surface of the diapers dry.

Benefits of technology

It achieves good water absorption and buttock protection effect of diapers, keeps the surface of diapers dry, is comfortable to use, and effectively alleviates skin problems on the baby's buttocks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118892399A_ABST
    Figure CN118892399A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of paper diaper manufacturing, and provides a paper diaper with a multi-layer core in order to solve the problem that a paper diaper in the prior art does not have a skin care effect, the multi-layer core of the paper diaper comprises a conducting layer and a water absorption layer, and the water absorption layer sequentially comprises a skin care layer, a supporting layer and a reinforcing layer from top to bottom. The skin care layer is composed of a plurality of non-woven fabrics which are arranged in parallel, a plurality of water absorption chambers and skin care chambers are alternately arranged in the space between the adjacent non-woven fabrics, high-expansion water absorption resin is arranged in the water absorption chambers, diaphragms containing wood pulp are arranged on all faces of the skin care chambers, skin care substances are arranged in the skin care chambers, the supporting layer is made of polyester fibers, and high-magnification water absorption resin is arranged in the reinforcing layer. The paper diaper has a skin care effect on the buttocks of a baby and is good in water absorption, and the surface of the paper diaper can be kept dry.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of diaper manufacturing, and in particular to a diaper with a multi-layer core. Background Art

[0002] Diapers are daily necessities commonly used by babies. The main structures of conventional diapers are the surface coating layer, the absorbent core layer and the base fabric. The coating layer is close to the baby's body, which can promote the rapid penetration of urine and effectively prevent back-seepage, so that the surface of the diaper remains dry. The main function of the absorbent core layer is to capture and quickly absorb urine, disperse urine or diffuse it into the entire core layer through capillary action, and finally absorb and store urine.

[0003] Diapers fit the baby's buttocks for a long time, and when the water absorption is poor, it is easy to cause redness and inflammation of the baby's buttocks. The molded multi-V belt improves the durability and NVH performance of the rubber by adding a layer of spandex sweat cloth or flocking on the wedge surface. For example, the invention patent with publication number CN109009670A discloses a diaper containing pearl powder and its preparation method. The diaper is coated with pearl powder on the surface to prevent skin redness and diaper rash that are easy to occur when using diapers. However, the pearl powder is easy to fall off and oxidize during the transportation and storage of the diaper, and it cannot improve the water absorption effect. Summary of the invention

[0004] In order to overcome the problem that diapers in the prior art do not have a skin care effect, the present invention provides a diaper with a multi-layer core, which has a skin care effect on the baby's buttocks and has good water absorption to keep the surface of the diaper dry.

[0005] In order to achieve the above object, the present invention adopts the following technical solutions: A diaper with a multi-layer core, the multi-layer core of the diaper comprising a conductive layer and a water-absorbing layer, the water-absorbing layer comprising a skin-care layer, a supporting layer and a reinforcing layer from top to bottom, the skin-care layer being a plurality of parallel non-woven fabrics, a plurality of water-absorbing chambers and skin-care chambers being alternately arranged in the space between adjacent non-woven fabrics, a high-expansion water-absorbing resin being arranged in the water-absorbing chamber, each surface of the skin-care chamber being a diaphragm containing wood pulp, a skin-care substance being arranged in the skin-care chamber, the supporting layer being polyester fiber, and the reinforcing layer being provided with a high-rate water-absorbing resin.

[0006] The present invention has a multi-layer structure. The first layer is a conductive layer for conducting liquid. The second layer is used to absorb liquid. The water absorption chamber equipped with high expansion water-absorbing resin in the skin care layer structure of the second layer can initially absorb urine, and expand rapidly after absorbing liquid, tearing the diaphragm adjacent to the water absorption chamber to release the skin care substance in the skin care chamber. The skin care substance is dissolved in the liquid and slowly released to the surface of the diaper, thereby playing a skin care role. The supporting layer of the second layer can separate the upper and lower layers of water-absorbing resins with different functions, and play a role in supporting their skeleton to prevent the core from being too soft and causing the entire core to collapse. The reinforcing layer is equipped with high-rate water-absorbing resin, which can fully absorb the urine that has not been absorbed by the skin care layer that has seeped into the reinforcing layer through gravity, so as to ensure that the entire core is dry.

[0007] Preferably, the high expansion water-absorbing resin is a SAP resin with a particle size of 400-600 μm.

[0008] Preferably, the high-rate water-absorbing resin is a SAP resin having a particle size of 125-250 μm.

[0009] When the particle size of SAP resin is 400-600 μm, its expansion ratio is relatively large; when the particle size is 125-250 μm, its absorption ratio is relatively large.

[0010] Preferably, the diaphragm is obtained by mixing wood pulp and polyester resin in a mass ratio of (80-100): (0-20) and then pressing, and the thickness of the diaphragm is 0.01-0.05 mm.

[0011] The diaphragm is pressed from wood pulp or a mixture of wood pulp and polyester resin. It can isolate skin care substances and high-expansion water-absorbing resin before use. After contacting water, the bonding effect between wood pulp fibers decreases, making the diaphragm easily damaged by external forces.

[0012] Preferably, the surface of the diaphragm located on the skin care room side is coated with a polyvinyl alcohol coating.

[0013] The polyvinyl alcohol coating prevents oily skin care substances from penetrating the membrane.

[0014] Preferably, the skin care substance is diaper cream or diaper oil.

[0015] Preferably, the width ratio of the water absorption chamber and the skin care chamber is (3-10):1.

[0016] Preferably, the thickness ratio of the skin care layer, the support layer and the reinforcement layer is (3-5):1:(5-10).

[0017] Preferably, the conductive layer material is bio-based fiber.

[0018] Preferably, the multi-layer core further comprises a buffer layer, and the buffer layer is disposed at the bottom of the water-absorbing reinforcement layer.

[0019] The buffer layer can prevent the high-rate water-absorbent resin from piercing the bottom layer of the multi-layer core body, thereby causing urine leakage.

[0020] Preferably, the buffer layer material is ES fiber.

[0021] ES fiber has a certain degree of fluffiness, which can effectively accommodate high-rate water-absorbent resin in its fluffiness gaps, playing a buffering role.

[0022] Therefore, the present invention has the following beneficial effects: good water absorption can keep the surface of the diaper dry, good comfort in use, and has a hip protection effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a structural schematic diagram of the present invention.

[0024] Among them, 1-conducting layer, 2-water absorbing layer, 21-skin care layer, 211-water absorbing chamber, 212-skin care chamber, 22-supporting layer, 23-reinforcement layer, 3-buffering layer. DETAILED DESCRIPTION

[0025] The present invention is further described below in conjunction with specific implementation methods and drawings.

[0026] The present invention provides a diaper with a multi-layer core. The multi-layer core of the diaper includes a conductive layer and a water-absorbing layer. The water-absorbing layer includes a skin-care layer, a supporting layer and a reinforcing layer from top to bottom. The skin-care layer is a plurality of non-woven fabrics arranged in parallel. A plurality of water-absorbing chambers and skin-care chambers are alternately arranged in the space between adjacent non-woven fabrics. A high-expansion water-absorbing resin is arranged in the water-absorbing chamber. Each surface of the skin-care chamber is a diaphragm containing wood pulp. A skin-care substance is arranged in the skin-care chamber. The supporting layer is polyester fiber. The reinforcing layer is provided with a high-rate water-absorbing resin.

[0027] In an embodiment of the present invention, the high expansion water-absorbing resin is a SAP resin with a particle size of 400-600 μm, and the high rate water-absorbing resin is a SAP resin with a particle size of 125-250 μm.

[0028] In an embodiment of the present invention, the separator is obtained by mixing wood pulp and polyester resin in a mass ratio of (80-100): (0-20) and then pressing, and the thickness of the separator is 0.01-0.05 mm.

[0029] In an embodiment of the present invention, the surface of the membrane located on the skin care chamber side is coated with a polyvinyl alcohol coating.

[0030] In an embodiment of the present invention, the skin care substance is a diaper cream or diaper oil, the diaper oil is composed of camellia seed oil, bisabolol and tocopherol acetate, and the diaper cream is composed of camellia seed oil, bisabolol, tocopherol acetate and beeswax.

[0031] In an embodiment of the present invention, the width ratio of the water absorption chamber and the skin care chamber is (3-10):1.

[0032] In an embodiment of the present invention, the thickness ratio of the skin care layer, the support layer and the reinforcement layer is (3-5):1:(5-10).

[0033] In an embodiment of the present invention, the conductive layer material is a bio-based fiber.

[0034] In an embodiment of the present invention, the multi-layer core further comprises a buffer layer, and the buffer layer is disposed at the bottom of the water-absorbent reinforcing layer.

[0035] In an embodiment of the present invention, the buffer layer material is ES fiber.

[0036] Example 1 A diaper with a multi-layer core, wherein the structure of the multi-layer core in the diaper is as follows Figure 1 As shown, it includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.5 mm. The skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm. The diaphragm is pressed from virgin wood pulp and has a thickness of 0.05 mm. The surface of one side of the diaphragm is coated with a polyvinyl alcohol coating, and then the surface coated with the polyvinyl alcohol coating is folded inward to obtain a skin care room 212. The top and bottom outer sides of the skin care room 212 are combined with the non-woven fabric by hot melt adhesive. The skin care material is filled in the skin care room 212, and the skin care material is a diaphragm cream prepared from 10 parts of camellia seed oil, 3 parts of bisabolol, 6 parts of tocopherol acetate and 6 parts of beeswax. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, in which a high expansion water absorption resin is provided, and the high expansion water absorption resin is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 8:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber and has a thickness of 0.5mm.

[0037] Before use, the skin care substance is isolated by the diaphragm and does not contact the outside world. During use, urine flows into the skin care layer 21 under the guidance of the conductive layer 1. The high expansion water-absorbing resin in the skin care layer 21 absorbs urine and expands in the water absorption chamber 211, driving the non-woven fabrics on the upper and lower sides of the water absorption chamber 211 away from each other, so that the diaphragm adjacent to the water absorption chamber 211 receives vertical tension. In addition, the mechanical properties of the diaphragm itself decrease after absorbing water. After the diaphragm is damaged, the skin care substance in the skin care chamber 212 is released. The skin care substance dissolves in the liquid and is slowly released to the surface of the diaper, thereby playing a skin care role. Urine that is not absorbed by the skin care layer 21 flows into the reinforcing layer 23 through the supporting layer 22 under the action of gravity and is absorbed by the high-rate water-absorbing resin in the reinforcing layer 23.

[0038] Detect the re-seepage amount of Example 1. Use three pressurizations, and the specific steps are: lay the diaper flat and fixed on the workbench, place the test cylinder in the center of the diaper, pour in 80mL of physiological saline and start timing, measure the absorption time, and after 5 minutes, quickly put several layers of filter paper with a known mass of ф110mm (until the top layer of filter paper has no liquid absorption) on the surface of the sample liquid absorption, and at the same time press a 5kg briquette on the filter paper. After 5 minutes, remove the standard briquette, weigh the increased weight of the filter paper (i.e., the re-seepage amount) with a balance and measure the diffusion length. The above steps are repeated three times, and the absorption time, re-seepage amount, and diffusion length are calculated three times respectively. The detection result of the re-seepage amount after three pressurizations in Example 1 is 2.8g, which shows that the absorption effect of the present invention is good, and the high-rate water-absorbent resin can lock urine and keep the surface coating layer dry.

[0039] Comparative Example 1 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of Example 1 in that the water-absorbing layer 2 does not contain a support layer 22, and its specific structure includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, a skin care layer 21 and a reinforcement layer 23 are arranged from close to the conductive layer 1 to far away from the conductive layer 1. The thickness of the skin care layer 21 is 0.6 mm, and the skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is arranged in the space of each layer. The skin care room 212 is surrounded by a diaphragm, and the diaphragm is pressed from virgin wood pulp, and its thickness is 0.05 mm. The surface of one side of the diaphragm is coated with a polyvinyl alcohol coating, and then the surface coated with the polyvinyl alcohol coating is folded inward to obtain the skin care room 212, and the top and bottom outer sides of the skin care room 212 are combined with the non-woven fabric by hot melt adhesive. The skin care chamber 212 is filled with a skin care substance, which is a diaper cream prepared from 10 parts of camellia oil, 3 parts of bisabolol, 6 parts of tocopherol acetate and 6 parts of beeswax. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, and the water absorption chamber 211 is provided with a high expansion water absorption resin, which is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 8:1. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and a fluff pulp, and its thickness is 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber, and its thickness is 0.5mm.

[0040] In the diaper prepared in Comparative Example 1, the core lacks support, causing the entire core to collapse, and the high-rate water-absorbent resin in the reinforcement layer is unevenly distributed, resulting in a decrease in the local water absorption performance of the diaper and thus poor dryness performance of the diaper.

[0041] Example 2 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of Example 1 in that the particle sizes of the high expansion water-absorbing resin and the high rate water-absorbing resin are different; Its specific structure includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.6 mm. The skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm. The diaphragm is pressed from virgin wood pulp and has a thickness of 0.05 mm. The surface of one side of the diaphragm is coated with a polyvinyl alcohol coating, and then the surface coated with the polyvinyl alcohol coating is folded inward to obtain the skin care room 212. The top and bottom outer sides of the skin care room 212 are combined with the non-woven fabric by hot melt adhesive. The skin care material is filled in the skin care room 212, and the skin care material is a diaphragm cream prepared from 10 parts of camellia seed oil, 3 parts of bisabolol, 6 parts of tocopherol acetate and 6 parts of beeswax. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, in which a high expansion water absorption resin is provided, and the high expansion water absorption resin is a SAP resin with a particle size of 400μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 8:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber and has a thickness of 0.5mm.

[0042] The back permeation amount of Example 2 was detected using the same method as Example 1, and the detection result was 2.6 g.

[0043] Example 3 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of the embodiment 1 in that the structure of the water-absorbing layer 2 is different; Its specific structure includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.6 mm. The skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm. The diaphragm is pressed from virgin wood pulp and has a thickness of 0.05 mm. The surface of one side of the diaphragm is coated with a polyvinyl alcohol coating, and then the surface coated with the polyvinyl alcohol coating is folded inward to obtain the skin care room 212. The top and bottom outer sides of the skin care room 212 are combined with the non-woven fabric by hot melt adhesive. The skin care material is filled in the skin care room 212, and the skin care material is a diaphragm cream prepared from 10 parts of camellia seed oil, 3 parts of bisabolol, 6 parts of tocopherol acetate and 6 parts of beeswax. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, in which a high expansion water absorption resin is provided, and the high expansion water absorption resin is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 8:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber and has a thickness of 0.5mm.

[0044] Example 4 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of the embodiment 1 in that the structure of the water-absorbing layer 2 is different; Its specific structure includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.5 mm. The skin care layer 21 is divided into four layers by three parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm. The diaphragm is pressed from virgin wood pulp and has a thickness of 0.04 mm. The surface of one side of the diaphragm is coated with a polyvinyl alcohol coating, and then the surface coated with the polyvinyl alcohol coating is folded inward to obtain the skin care room 212. The top and bottom outer sides of the skin care room 212 are combined with the non-woven fabric by hot melt adhesive. The skin care material is filled in the skin care room 212, and the skin care material is a diaphragm cream prepared from 10 parts of camellia seed oil, 3 parts of bisabolol, 6 parts of tocopherol acetate and 6 parts of beeswax. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, in which a high expansion water absorption resin is provided, and the high expansion water absorption resin is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 3:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber and has a thickness of 0.5mm.

[0045] Example 5 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of Example 1 in that the diaphragm structure is different; its specific structure includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.6 mm, and the skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm. The diaphragm is pressed from virgin wood pulp and has a thickness of 0.05 mm. The skin care room 212 is then folded to obtain the skin care room 212, and the top and bottom outer sides of the skin care room 212 are bonded to the non-woven fabric by hot melt adhesive. The skin care chamber 212 is filled with a skin care substance, which is a diaper cream prepared from 10 parts of camellia seed oil, 3 parts of bisabolol, 6 parts of tocopherol acetate and 6 parts of beeswax. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, and the water absorption chamber 211 is provided with a high expansion water absorption resin, which is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 8:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber and has a thickness of 0.5mm.

[0046] Example 6 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of Example 1 in that the diaphragm structure is different and the skin care substance is diaper oil; Its specific structure includes a conductive layer 1, a water-absorbing layer 2 and a buffer layer 3. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.6 mm. The skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm. The diaphragm is pressed from virgin wood pulp, and its thickness is 0.05 mm. Then, the skin care room 212 is folded to obtain the skin care room 212. The top and bottom outer sides of the skin care room 212 are combined with the non-woven fabric by hot melt adhesive. The skin care material is filled in the skin care room 212, and the skin care material is a diaphragm oil prepared from 10 parts of camellia seed oil, 3 parts of bisabolol and 6 parts of tocopherol acetate. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, in which a high expansion water absorption resin is provided, and the high expansion water absorption resin is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 8:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm. The buffer layer 3 is obtained by pressing ES fiber and has a thickness of 0.5mm.

[0047] Example 7 A diaper with a multi-layer core, the structure of the multi-layer core of the diaper is different from that of Example 1 in that it does not contain a buffer layer 3; its specific structure includes a conductive layer 1 and a water-absorbing layer 2. The conductive layer 1 is located below the surface coating layer of the diaper, and is obtained by weaving and pressing polylactic acid fibers, with a thickness of 0.2 mm. In the structure of the water-absorbing layer 2, from close to the conductive layer 1 to far away from the conductive layer 1, there are a skin care layer 21, a support layer 22 and a reinforcement layer 23. The thickness of the skin care layer 21 is 0.5 mm, and the skin care layer 21 is divided into four layers by five parallel non-woven fabrics. A skin care room 212 is set in the space of each layer. The skin care room 212 is surrounded by a diaphragm, and the diaphragm is pressed from virgin wood pulp, and its thickness is 0.05 mm. The surface of one side of the diaphragm is coated with a polyvinyl alcohol coating, and then the surface coated with the polyvinyl alcohol coating is folded inward to obtain the skin care room 212, and the top and bottom outer sides of the skin care room 212 are bonded to the non-woven fabric by hot melt adhesive. The skin care chamber 212 is filled with a skin care substance, which is a diaper oil prepared from 10 parts of camellia seed oil, 3 parts of bisabolol and 6 parts of tocopherol acetate. The remaining space of each layer in the skin care layer 21 is the water absorption chamber 211, and the water absorption chamber 211 is provided with a high expansion water absorption resin, which is a SAP resin with a particle size of 600μm. The total width ratio of the water absorption chamber 211 and the skin care chamber 212 is 10:1. The support layer 22 is obtained by pressing polyester fiber and has a thickness of 0.15mm. The reinforcement layer 23 is obtained by mixing and pressing a high-rate water absorption resin and a fluff pulp, and has a thickness of 1.5mm. The high-rate water absorption resin is a SAP resin with a particle size of 200μm.

[0048] When Example 1-7 is immersed in physiological saline, it can be observed that an oily substance (camellia seed oil) appears in the physiological saline, which indicates that the diapers obtained in Example 1-7 can release diaper cream or diaper oil after absorbing urine.

Claims

1. A diaper with a multi-layer core, characterized in that: The multi-layer core of the diaper comprises a conductive layer (1) and a water-absorbing layer (2), wherein the water-absorbing layer comprises a skin-care layer (21), a support layer (22) and a reinforcing layer (23) from top to bottom, the skin-care layer being a plurality of non-woven fabrics arranged in parallel, a plurality of water-absorbing chambers (211) and skin-care chambers (222) being alternately arranged in the space between adjacent non-woven fabrics, a high-expansion water-absorbing resin being arranged in the water-absorbing chamber, each surface of the skin-care chamber being a diaphragm containing wood pulp, a skin-care substance being arranged in the skin-care chamber, the support layer being polyester fiber, and the reinforcing layer being provided with a high-rate water-absorbing resin.

2. A diaper with a multi-layer core according to claim 1, characterized in that: The high expansion water-absorbing resin is a SAP resin with a particle size of 400-600 μm.

3. A diaper with a multi-layer core according to claim 1, characterized in that: The high-rate water-absorbing resin is a SAP resin with a particle size of 125-250 μm.

4. A diaper with a multi-layer core according to claim 1, characterized in that: The diaphragm is obtained by mixing wood pulp and polyester resin in a mass ratio of (80-100): (0-20) and then pressing the mixture. The thickness of the diaphragm is 0.01-0.05 mm.

5. A diaper with a multi-layer core according to claim 4, characterized in that: The surface of the diaphragm located at the skin care room side is coated with a polyvinyl alcohol coating.

6. A diaper with a multi-layer core according to claim 4 or 5, characterized in that: The skin care substance is diaper cream or diaper oil.

7. A diaper with a multi-layer core according to claim 1, characterized in that: The width ratio of the water absorption chamber and the skin care chamber is (3-10):

1.

8. The multi-layer core diaper according to claim 1, characterized in that: The thickness ratio of the skin care layer, the support layer and the reinforcement layer is (3-5):1:(5-10).

9. A diaper with a multi-layer core according to claim 1, 2, 3 or 8, characterized in that: The multi-layer core also includes a buffer layer (3), which is placed at the bottom of the water-absorbing reinforcement layer.

10. A diaper with a multi-layer core according to claim 9, characterized in that: The buffer layer material is ES fiber.

Citation Information

Patent Citations

  • Diaper containing pearl powder and preparation method thereof

    CN109009670A

  • Skin-care anti-allergic baby diaper

    CN204092345U

  • Environmental protection skin care panty -shape diapers

    CN207654327U

  • Absorbent article

    JP2022037490A

  • Nonwoven fabric for skin care product

    JP2023061379A

Cited By

  • Composite core body and absorption product

    CN121489736A

  • Composite core paper diaper with core supporting structure

    CN224056189U