Manufacturing method of deposition additive BD roller

By using a composite BD roll with a low-carbon alloy steel support layer and a high-alloy powder working layer, combined with additive manufacturing and optimized processes, the failure and high roll consumption problems of BD rolls in harsh environments have been solved, resulting in extended roll life and resource conservation.

CN118893215APending Publication Date: 2024-11-05SINOSTEEL XINGTAI MACHINERY & MILL ROLL +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410784478.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-18
Publication Date
2024-11-05
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a deposition additive BD roller, which belongs to the technical field of composite roller manufacturing, and comprises the following steps of: manufacturing a steel ingot, sequentially adding pig iron, scrap steel and a material head into an electric arc furnace according to the requirements of chemical components of each part of the composite BD roller supporting layer, adjusting the components, and pouring; 2, forging and forming, namely heating the steel ingot in a heating furnace, taking out of the furnace and forging at the forging ratio of more than or equal to 4 after the temperature is reached, and annealing after the blank is formed; thirdly, rough turning is carried out, the machining process is carried out according to a drawing to obtain the minimum size, and the hole shape size is machined; 4, heat treatment is conducted, specifically, the composite BD roller is directly subjected to thermal refining after being discharged out of the furnace, water serves as a quenching medium, then knife polishing is conducted, and oxide skin is removed; and 5, cladding additive manufacturing: preparing alloy powder according to the requirements of the chemical components of the working layer of the composite BD roller, vibrating and mixing, putting the alloy powder into a powder feeding system, and carrying out cladding additive manufacturing on the supporting layer of the composite BD roller. According to the BD roller, the strength and toughness are improved, reutilization can be achieved, and resource consumption is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of composite roller manufacturing, and in particular relates to a method for manufacturing a BD roller with a fusion-bonded material. Background Art

[0002] The function of the BD rolling mill is to perform multiple reversible rolling of the steel billet. During the rolling process, the transmission system frequently rotates forward and reversely. The BD roller is in direct contact with the steel billet, and the surface is cooled by circulating water. The BD roller is in a complex stress and fatigue state for a long time. According to measurements and calculations, the roller directly bears a rolling force of 10000-12000KN, and the temperature of the rolled steel billet is about 950-1100℃. In this way, the roller is subjected to local force back and forth on the contact surface with the steel billet during the rolling process, and the roller will generate local thermal shock force, steel billet contact stress and residual stress, etc. At the same time, due to the large temperature difference between the roller and the cooling water, the working environment of the BD roller is relatively harsh, which makes the roller surface easy to fail.

[0003] In addition, cast rolls often have defects such as sand holes, pores, inclusions, etc. on the roll surface. The complex rolling process will increase the failure rate of the roll surface. During the rolling process of back and forth contact with the steel billet, the defects will be magnified exponentially, and eventually wear, fatigue and even cracks will occur on the roll surface, resulting in high BD roll consumption.

[0004] In addition, when conventional cast BD rolling rolls reach the scrap process size, the remaining weight accounts for about 60%-70% of the new rolls, resulting in huge waste. For steel mills, the roll consumption is relatively high.

[0005] Therefore, there is an urgent need to improve the manufacturing method of the BD roller to solve the current problem of large BD roller loss. Summary of the invention

[0006] The technical problem to be solved by the present invention is to provide a method for manufacturing a BD rolling roller by melt-deposited additive, and to develop a new production method and combined material. The supporting layer is produced by forging with low-carbon alloy steel to improve strength and toughness, and can be reused to reduce resource consumption. The working layer is formed by additive manufacturing and melt-deposited high-alloy composite material to improve its wear resistance. According to the heat treatment conditions in the preparation process of the additive high-alloy material, a BD rolling roller and a manufacturing method thereof are provided.

[0007] To achieve the above purpose, the technical solution adopted by the present invention is: A method for manufacturing a BD roller by melt-cladding additive includes a support layer and a working layer, and the specific steps are as follows: Step 1: Ingot production: according to the requirements of the chemical composition of each part of the composite BD roller support layer, pig iron, scrap steel, and head are added to the electric arc furnace in sequence, and the composition is adjusted for pouring; Step 2: Forging and forming: put the steel ingot into a heating furnace for heating. After reaching the temperature, take it out of the furnace for forging. The forging ratio is ≥4. After the blank is formed, annealing is performed. Step 3: Rough turning, process according to the drawing and process the hole size; Step 4: Heat treatment: the composite BD roll is directly subjected to quenching and tempering treatment after it comes out of the furnace. The quenching medium is water, and then the oxide scale is removed by polishing. Step 5: Additive deposition: prepare alloy powder and vibrate and mix it according to the requirements of the chemical composition of the composite BD roller working layer, put it into the powder feeding system, and perform additive deposition on the composite BD roller support layer.

[0008] The further improvement of the technical solution of the present invention is that the chemical composition of the supporting layer and the mass percentage of each component are C 0.3-0.5%, Si 0.2-0.4%, Mn 0.6-0.8%, Cr 0.8-1.0%, Ni1.0-1.5%, Mo 0.15-0.30%, P≤0.03%, S≤0.03%, and the rest are Fe and inevitable impurities; the working layer uses 90% Ni55A alloy powder + 10% WC powder, the powder particle size is: 100-300 mesh, the main components of Ni55A alloy powder are: C0.4~0.8%, Si3.5-5.5%, B3.0-4.5%, Cr14-17%, Fe≤5%, and the rest are Ni.

[0009] A further improvement of the technical solution of the present invention is that the hardness of the prepared composite BD roller is HSD75-85, and after one rolling cycle of the working layer roller of the composite BD roller, the fatigue layer is removed, and step five is repeated on the supporting layer to achieve another cycle rolling, until the intermediate rolling volume reaches 500,000 tons, the roller is scrapped, and no more deposition and material addition is performed.

[0010] The further improvement of the technical solution of the present invention is that the specific steps in step one are: A1. According to the requirements of the chemical composition of each part of the composite BD roll support layer, pig iron, scrap steel, and head are added to the electric arc furnace in order to obtain primary molten steel; A2. The primary molten steel is transferred to the LF ladle refining furnace for further adjustment of the composition to obtain finished molten steel for ingot casting.

[0011] The further improvement of the technical solution of the present invention is that: in step 2, two upsetting and drawing processes are adopted, and after the blank is formed, a stress relief annealing process at 600-700°C is performed.

[0012] A further improvement of the technical solution of the present invention is that the tempering temperature in step 4 is 850-900°C.

[0013] The further improvement of the technical solution of the present invention is that the specific steps of step five are: E1. Select the additive material and vibrate and mix the alloy powder according to the requirements of the chemical composition of each part of the working layer of the composite BD roller; E2. Preheat the composite BD roller support layer to 300-400°C and keep it warm for 10-16h; E3. After the insulation is completed, place the BD roller ring support layer on the automatic rotating device; E4. Implement melt deposition additive manufacturing, feed the additive alloy powder through the powder feeding system, set the computer program, and perform automatic additive manufacturing.

[0014] The further improvement of the technical solution of the present invention is that in step E4, the gas flow rate is 8L / min, the powder flow rate is 40g / min, a 5kw fiber laser is selected, the scanning speed is 20mm / s, the interval distance is controlled at 10mm, and 5 layers of automatic additive are achieved according to the hole size.

[0015] Due to the adoption of the above technical solution, the technical progress achieved by the present invention is: The BD roller prepared by the present invention has high strength, good red hardness, good wear resistance, good accident resistance, small wear after being used on the machine, and the online time is extended by 2 times compared with conventional cast steel materials. The high red hardness and wear resistance of the outer layer are achieved through additive manufacturing. By optimizing the forging and heat treatment process parameters, the strength, toughness and other mechanical properties of the BD roller support layer are further improved. At the same time, after the BD roller working layer is consumed in the rolling process, the support layer can repeat the above operation many times to achieve reuse.

[0016] The BD roller of the present invention adopts 3D additive manufacturing method, which is essentially different from conventional cast steel materials. Conventional cast steel is produced by static casting, and the roller size is large, which is prone to defects such as sand holes and inclusions, and the wear and fatigue during the rolling process are also serious. The above conventional materials are rolled at 20,000-25,000 tons per time, while the 3D additive bimetallic composite BD roller of the present invention is rolled at 40,000-50,000 tons per time, achieving exponential growth.

[0017] The BD roller support layer of the present invention can be reused 3-5 times. According to the calculation based on 3 times, the roller consumption can be reduced to 1 / 6 of that of conventional materials, and the cost can be reduced by more than 50%, which brings huge economic benefits to the steel mill. DETAILED DESCRIPTION

[0018] The present invention is further described in detail below in conjunction with embodiments: Example 1 The components and weight percentages of a BD roller working layer and a supporting layer are as follows: C 0.38%, Si0.3%, Mn 0.7%, Cr 0.95%, Ni1.10%, Mo 0.25%, P≤0.03%, S≤0.03%, the rest are Fe and inevitable impurities. The working layer uses 90% Ni55A alloy powder + 10% WC powder, powder size: 200 mesh, Ni55A alloy powder main components: C0.6%, Si4.0%, B4.0%, Cr15%, Fe≤5%, the rest is Ni.

[0019] The preparation of a BD roller includes the following process: A. Ingot production A1. According to the requirements of the chemical composition of the BD roll support layer, pig iron, scrap steel, and head are added to the 30t electric arc furnace in order, slag-making materials are added, oxygen is blown to make slag, decarbonize, and dephosphorize to obtain primary molten steel; A2. Put the primary molten steel into LF refining bag, heat the deoxidizer Al cake, add lime, silicon carbide, fluorite, make white slag, make S≤0.010%, adjust the final product composition, and cast steel ingots.

[0020] B. Forging B1. After the steel ingot is kept warm for 48 hours, it is unpacked and transferred to a gas furnace. After it is heated to temperature, it is taken out of the furnace for forging. The forging is divided into two fires. The first fire removes the riser and the ingot tail, and performs a pulling process. The second fire uses the pulling process again and corrects it to the blank shape. The actual forging ratio is 6.25; B3. After the blank is formed, it is transferred to a resistance furnace, heated to 680°C, kept warm for 25 hours, and subjected to stress relief annealing process; C. Rough turning After stress relief is completed, the roller blank is transferred to the processing workshop for rough turning and hole punching.

[0021] D. Heat treatment D1. After the seamless BD roll support is taken out of the furnace, it is loaded into a 30t high-temperature resistance furnace and heated to 880℃. Then it is taken out of the furnace and placed in a water pool with stirring. After 1h20min, the water is removed and loaded into a low-temperature resistance furnace and heated to 600℃. Then it is taken out of the furnace and air-cooled to complete the quenching and tempering treatment. Then it is polished and the oxide scale is removed. E. Additive Deposition According to the requirements of the chemical composition of the BD roller working layer, the alloy powder is prepared and vibrated and mixed, and placed in the powder feeding system. The computer program is set, the gas flow rate is 8L / min, the powder flow rate is 40g / min, a 5kw fiber laser is selected, the scanning speed is 20mm / s, the interval distance is controlled to 10mm, and 5 layers of melt deposition are realized on the composite BD roller support layer according to the hole shape.

[0022] Example 2 The components and weight percentages of a BD roller working layer and supporting layer are as follows: The chemical composition of the supporting layer and the mass percentage of each component are C 0.45%, Si 0.34%, Mn 0.65%, Cr0.8%, Ni1.4%, Mo 0.15%, P≤0.03%, S≤0.03%, and the rest are Fe and unavoidable impurities; the working layer uses 90% Ni55A alloy powder + 10% WC powder, powder particle size: 100 mesh, the main components of Ni55A alloy powder are: C0.8%, Si5.5%, B4.5%, Cr17%, Fe≤5%, and the rest is Ni.

[0023] The preparation of a BD roller includes the following process: A. Ingot production A1. According to the requirements of the chemical composition of each part of the BD roll, pig iron, scrap steel, and head are added to the 30t electric arc furnace in order, slag-making materials are added, oxygen is blown to make slag, decarbonize, and dephosphorize to obtain primary molten steel; A2. Put the primary molten steel into LF refining bag, heat the deoxidizer Al cake, add lime, silicon carbide, fluorite, make white slag, make S≤0.009%, adjust the final product composition, and cast steel ingots.

[0024] B. Forging B1. After the steel ingot is kept warm for 42 hours, it is unpacked and transferred to a gas furnace. After being heated to room temperature, it is taken out of the furnace for forging. The forging is divided into two fires. The first fire removes the riser and the ingot tail, and performs a pulling process. The second fire uses the pulling process again and corrects it to the blank shape. The actual forging ratio is 5.0; B3. After the blank is formed, it is transferred to a resistance furnace, heated to 680°C, kept warm for 20 hours, and subjected to stress relief annealing process; C. Rough turning After stress relief is completed, the roller blank is transferred to the processing workshop for rough turning and hole punching.

[0025] D. Heat treatment D1. After the seamless BD roll support is taken out of the furnace, it is loaded into a 30t high-temperature resistance furnace and heated to 880℃. Then it is taken out of the furnace and placed in a water pool with stirring. After 1h10min, the water is discharged and loaded into a low-temperature resistance furnace and heated to 580℃. Then it is taken out of the furnace and air-cooled to complete the quenching and tempering treatment. Then the oxide scale is removed by a polishing knife. E. Additive Deposition According to the requirements of the chemical composition of the BD roller working layer, the alloy powder is prepared and vibrated and mixed, and placed in the powder feeding system. The computer program is set, the gas flow rate is 8L / min, the powder flow rate is 40g / min, a 5kw fiber laser is selected, the scanning speed is 20mm / s, the interval distance is controlled to 10mm, and 5 layers of melt deposition are realized on the composite BD roller support layer according to the hole shape.

[0026] The BD roller prepared by the present invention has high strength, hardness HSD75-85, good red hardness, good wear resistance, good accident resistance, small wear after being used on the machine, and single rolling is increased from 20000t to 44000t.

[0027] After a rolling cycle of the working layer roll of the composite BD roll, the fatigue layer is removed and the operation of depositing and adding materials (step E) is repeated on the supporting layer to achieve another cyclic rolling. After the intermediate rolling volume reaches 500,000 tons, the roll is scrapped and no more depositing and adding materials are performed.

Claims

1. A method for manufacturing a BD roller by depositing additive, characterized in that: Including the support layer and the working layer, the specific steps are as follows: Step 1: Ingot production: according to the requirements of the chemical composition of each part of the composite BD roller support layer, pig iron, scrap steel and head are added to the electric arc furnace in sequence, and the composition is adjusted for pouring; Step 2: Forging and forming: put the steel ingot into a heating furnace for heating. After reaching the temperature, take it out of the furnace for forging. The forging ratio is ≥4. After the blank is formed, annealing is performed. Step 3: Rough turning, process according to the drawing and process the hole size; Step 4: Heat treatment: the composite BD roll is directly subjected to quenching and tempering treatment after it comes out of the furnace. The quenching medium is water, and then the oxide scale is removed by polishing. Step 5: Additive deposition: prepare alloy powder and vibrate and mix it according to the requirements of the chemical composition of the composite BD roller working layer, put it into the powder feeding system, and perform additive deposition on the composite BD roller support layer.

2. A method for manufacturing a BD roller by depositing additive according to claim 1, characterized in that: The chemical composition of the supporting layer and the mass percentage of each component are C 0.3-0.5%, Si 0.2-0.4%, Mn 0.6-0.8%, Cr 0.8-1.0%, Ni1.0-1.5%, Mo 0.15-0.30%, P≤0.03%, S≤0.03%, and the rest are Fe and unavoidable impurities; the working layer uses 90% Ni55A alloy powder + 10% WC powder, and the powder particle size is 100-300 mesh.

3. A method for manufacturing a BD roller by depositing additive according to claim 1, characterized in that: The hardness of the prepared composite BD roller is HSD75-85. After one rolling cycle of the working layer of the composite BD roller, the fatigue layer is removed and step five is repeated on the supporting layer to achieve another cyclic rolling. After the medium rolling volume reaches 500,000 tons, the roller is scrapped and no more deposition and material addition is performed.

4. A method for manufacturing a BD roller by depositing additive according to claim 1, characterized in that: The specific steps in step one are: A1. According to the requirements of the chemical composition of each part of the composite BD roll support layer, pig iron, scrap steel, and head are added to the electric arc furnace in order to obtain primary molten steel; A2. The primary molten steel is transferred to the LF ladle refining furnace for further adjustment of the composition to obtain finished molten steel for ingot casting.

5. The method for manufacturing a BD roller by depositing additive according to claim 1, characterized in that: In step 2, two upsetting and drawing processes are adopted. After the blank is formed, a stress relief annealing process at 600-700°C is performed.

6. A method for manufacturing a BD roller by depositing additive according to claim 1, characterized in that: In step 4, the tempering temperature is 850-900°C.

7. A method for manufacturing a BD roller by depositing additive according to claim 1, characterized in that: The specific steps of step five are: E1. Select the additive material and vibrate and mix the alloy powder according to the requirements of the chemical composition of each part of the working layer of the composite BD roller; E2. Preheat the composite BD roller support layer to 300-400°C and keep it warm for 10-16h; E3. After the insulation is completed, place the BD roller ring support layer on the automatic rotating device; E4. Implement melt deposition additive manufacturing, feed the additive alloy powder through the powder feeding system, set the computer program, and perform automatic additive manufacturing.

8. A method for manufacturing a BD roller by depositing additive according to claim 7, characterized in that: In step E4, the gas flow rate is 8 L / min, the powder flow rate is 40 g / min, a 5 kW fiber laser is selected, the scanning speed is 20 mm / s, the interval distance is controlled at 10 mm, and 5 layers of automatic additive are achieved according to the hole size.

9. A method for manufacturing a BD roller by depositing additive according to claim 2, characterized in that: The main components of Ni55A alloy powder are: C0.4~0.8%, Si3.5~5.5%, B3.0~4.5%, Cr14~17%, Fe≤5%, and the rest is Ni.