Napping processing method of light and thin knitted fabric containing wool
Through double-sided composite and double-sided woven woven treatment, the problems of holes and tension changes in the woven fabric during the woven woven process are solved, which improves the woven effect and efficiency, ensuring the warmth and overall quality of the fabric.
Patent Information
- Application Number
- CN202411230136.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-11-05
AI Technical Summary
Light and thin knitted fabrics are prone to holes, pilling hair loss and local tension changes during the hair extraction process, resulting in the expansion of defect area. Due to the good elasticity, single-sided hair removal is difficult to effectively deal with, affecting warmth.
The double-sided woven is used to woven and combine adhesive composite and sewing to reduce the elasticity of the fabric. The double-sided woven woven is used to form a single-sided woven effect, and it is washed with flat web, pre-shaped, dyed, and dry. The steps of adding additives to shape, compounding, reverse woven hair pulling, reverse woven hair shearing, split cleaning and final whisking improve the effect and efficiency of fleece lifting.
It effectively reduces the probability of holes and the impact of local tension, improves the wooling efficiency and the warmth of the fabric, and ensures the overall quality and performance of the fabric.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of textiles and relates to a method for raising the pile of a thin and light knitted fabric containing wool. Background Art
[0002] With the rise of the outdoor market and people's increasing requirements for health and comfort, the need for light and thin thermal fabrics is constantly being developed. If you want the fabric to be light and thin, the fabric weight should be light, but the strength will also be reduced. In order to keep the fabric warm, it is necessary to nap and raise it. Because the fabric strength is reduced, it is very easy to have holes, pilling and shedding during the napping process. In addition, due to local holes and other situations, it will also cause changes in fabric tension in a larger range outside the hole area. Therefore, the area of defects during the napping process will be greatly expanded due to local holes; in addition, many light and thin knitted fabrics (especially those used for thermal insulation) only need to be napped on one side (the inner side needs to maintain good skin-friendliness), and double-sided napping machines cannot be used. Finally, due to the good elasticity of wool-containing fabrics, the area of fabric with tension relaxation caused by local holes is expanded. Summary of the invention
[0003] The purpose of the present invention is to provide a method for raising the pile of thin and light knitted fabrics containing wool in view of the above-mentioned problems existing in the prior art. The technical problem to be solved by the present invention is how to improve the raising effect and efficiency.
[0004] The object of the present invention can be achieved by the following technical scheme: A method for raising the pile of a light and thin knitted fabric containing wool, characterized in that it comprises the following steps:
[0005] 1) Open-width washing: Wash the woven fabric in open width;
[0006] 2) Pre-setting: pre-setting the washed fabric;
[0007] 3) Dyeing: Put the fabric into the dyeing vat for dyeing;
[0008] 4) Drying: put the fabric into the setting machine for drying;
[0009] 5) Add additives to fix the shape;
[0010] 6) Compounding: Use the front sides of two rolls of light and thin knitted fabric as compounding surfaces, and perform detachable compounding on the two rolls of fabric;
[0011] 7) Back side napping: napping the two sides of the composite fabric to form the back side napping effect of a single knitted fabric;
[0012] 8) Shearing on the reverse side: Raise the two sides of the composite fabric to form the shearing effect of the reverse side of a single knitted fabric;
[0013] 9) Split and clean: Split and clean the composite fabric to form two single-sided fleece knitted fabrics;
[0014] 10) Final shaping: Final shaping of the fabric.
[0015] As an option, the fabrics may be bonded by dot-matrix stitching.
[0016] As another possibility, the fabrics may be bonded together by gluing.
[0017] Compared with the prior art, the present invention has the following advantages:
[0018] 1. It is not difficult to see that the napping is performed after double-sided lamination, which increases the thickness of the napped fabric. The elasticity of the fabric can be reduced by combining adhesive lamination and sewing, which reduces the impact of holes on the fabric caused by the napping process. Specifically, single-sided holes will hardly affect the local tension of the fabric.
[0019] 2. The fabrics are napped after lamination, which obviously reduces the probability of holes in the napping process;
[0020] 3. For fabrics that only need to be napped on one side, they can be processed by a double-sided napping machine after lamination to improve the napping efficiency. DETAILED DESCRIPTION
[0021] The following are specific embodiments of the present invention, which further describe the technical solutions of the present invention, but the present invention is not limited to these embodiments.
[0022] The fabric is made of 50s acrylic viscose blended yarn (containing 7% wool) and 40D spandex (1*1) ribbing, with spandex fully lined in the middle.
[0023] Example 1
[0024] Set the workshop temperature to 25°C and the humidity to 75%
[0025] 1. Open-width washing: Wash the woven fabric in open-width water, set the temperature to 95°C and the speed to 40m / min.
[0026] 2. Pre-setting: Pre-set the washed fabric, set the temperature to 182℃, and the speed to 30m / min.
[0027] 3. Dyeing: Put the fabric into the dye vat for dyeing.
[0028] 4. Drying: Put the fabric into the setting machine for drying, the drying temperature is 155℃, and the speed is set to 50m / min.
[0029] 5. Add auxiliary agents for shaping: add 35g / L raising agent, 0.5g / L penetrant, set the shaping temperature to 150℃, and set the speed to 50m / min.
[0030] 6. Composite: The two rolls of fabric are composited by dot stitching, with the non-brushed surface as the composite surface.
[0031] 7. Back side napping: Use a double-sided napping machine for napping. The first napping machine has a curved needle value of 20RPM, a straight needle value of 0RPM, and a fabric speed of 25m / min. The second napping machine has a curved needle value of 12RPM, a straight needle value of 5RPM, and a fabric speed of 25m / min.
[0032] 8. Back side shearing: Use Lafer shearing machine for double side shearing, with circular knife speed of 1100 rpm, circular knife distance of 0.6mm, flat knife distance of 0.2mm. Machine speed of 30m / min;
[0033] 9. Separate and clean the suture threads.
[0034] 10. Final shaping: The fabric is finally shaped at a shaping temperature of 150°C and a speed of 40m / min.
[0035] Example 2
[0036] Set the workshop temperature to 25°C and the humidity to 75%
[0037] 1. Open-width washing: Wash the woven fabric in open-width water, set the temperature to 95°C, and the speed to 40m / min.
[0038] 2. Pre-setting: Pre-set the washed fabric, set the temperature to 200℃ and the speed to 30m / min.
[0039] 3. Dyeing: Put the fabric into the dye vat for dyeing.
[0040] 4. Drying: Put the fabric into the setting machine for drying, the drying temperature is 150℃, and the speed is set to 30m / min.
[0041] 5. Add auxiliary agents for shaping: add 28g / L raising agent, 0.3g / L penetrant, set the shaping temperature to 150℃, and the speed to 50m / min.
[0042] 6. Composite: Use heat-removable glue or starch paste to composite the fabrics, with the non-napped side as the composite side.
[0043] 7. Back side napping: Use a double-sided napping machine for napping. The first napping machine has a curved needle value of 25RPM, a straight needle value of -2RPM, and a fabric speed of 18m / min. The second napping machine has a curved needle value of 15RPM, a straight needle value of 0RPM, and a fabric speed of 18m / min.
[0044] 8. Back side shearing: Use Lafer shearing machine for double side shearing, with circular knife speed of 1100 rpm, circular knife distance of 0.5mm, flat knife distance of 0.2mm. Machine speed of 18m / min;
[0045] 9. Split and clean: Split by hot cleaning.
[0046] 10. Final shaping: The fabric is finally shaped at a shaping temperature of 160°C and a speed of 35m / min.
[0047] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
Claims
1. A method for raising the pile of a light and thin knitted fabric containing wool, characterized in that: The steps include: 1) Open-width washing: Wash the woven fabric in open width; 2) Pre-setting: pre-setting the washed fabric; 3) Dyeing: Put the fabric into the dyeing vat for dyeing; 4) Drying: put the fabric into the setting machine for drying; 5) Add additives to fix the shape; 6) Compounding: Use the front sides of two rolls of light and thin knitted fabric as compounding surfaces, and perform detachable compounding on the two rolls of fabric; 7) Back side napping: napping the two sides of the composite fabric to form the back side napping effect of a single knitted fabric; 8) Shearing on the reverse side: Raise the two sides of the composite fabric to form the shearing effect of the reverse side of a single knitted fabric; 9) Split and clean: Split and clean the composite fabric to form two single-sided fleece knitted fabrics; 10) Final shaping: Final shaping of the fabric.
2. A method for raising the fleece of a light and thin knitted fabric containing wool according to claim 1, characterized in that: The fabric bonding method can be dot matrix stitching.
3. The method for raising the fleece of a light and thin knitted fabric containing wool according to claim 1, characterized in that: The fabric bonding method can be gluing.