Semiconductor device and forming method thereof

By introducing a compound semiconductor structure with compression stress type into the semiconductor device, the influence of the through-substrate guide hole stress on the circuit performance is solved, the circuit design area is reduced, and more efficient current matching and space utilization is achieved.

CN118899283APending Publication Date: 2024-11-05WINBOND ELECTRONICS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311058683.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-02
Filing Date
2023-08-22
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

In a stereoscopic circuit, the tensile stresses through the substrate guide holes cause a current mismatch between the P-type metal oxide semiconductor and the N-type metal oxide semiconductor, affecting the circuit performance, and the existing discharge area settings are added The circuit design area offsets the benefits of the three-volume circuit.

Method used

A compound semiconductor structure is introduced into a semiconductor device, which is arranged around the periphery of a plurality of through-substrate guide holes. The structure has a different type of compression stress from the through-substrate guide holes, which cancels the tensile stress of the guide holes and passes through shallow grooves The trough isolation region is isolated from the through substrate guide holes, reducing the discharge area from other devices.

Benefits of technology

The impact of stress through the substrate guide holes on other devices is effectively avoided, the overall device performance is improved, and the area requirement of the overall wafer is reduced by reducing the size of the discharge area.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118899283A_ABST
    Figure CN118899283A_ABST
Patent Text Reader

Abstract

The invention provides a semiconductor device and a forming method thereof. The device comprises a substrate; the source electrode region and the drain electrode region are arranged in the substrate; the shallow trench isolation region is arranged in the substrate and surrounds the source region and the drain region; a plurality of through-substrate vias through the substrate, where the through-substrate vias are adjacent to the shallow trench isolation regions; and a compound semiconductor structure which isolates the shallow trench isolation region from the through-substrate via. The through substrate via has a first stress type, and the compound semiconductor structure has a second stress type different from the first stress type.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a semiconductor device and a method for forming the same, and in particular to a compound semiconductor structure and a method for forming the same. Background Art

[0002] In recent years, in order to further increase the functional density of semiconductor integrated circuits, the configuration of three-dimensional circuits has been explored. In order to achieve effective electrical connection in three-dimensional circuits, through-substrate vias extend from the front surface of the substrate into the substrate and are exposed from the back surface of the substrate. However, due to the tensile stress of the through-substrate vias, other devices of the semiconductor integrated circuit will be impacted.

[0003] For example, since the on-currents of the N-type metal oxide semiconductor and the P-type metal oxide semiconductor are not connected due to the impact of tensile stress and compressive stress, the through substrate via will cause current mismatch between the P-type metal oxide semiconductor and the N-type metal oxide semiconductor. In detail, when the semiconductor device has both a P-type metal oxide semiconductor and an N-type metal oxide semiconductor, the through substrate via with tensile stress can increase the on-current of the N-type metal oxide semiconductor and reduce the on-current of the P-type metal oxide semiconductor, thereby causing current mismatch between the P-type metal oxide semiconductor and the N-type metal oxide semiconductor.

[0004] In existing circuit designs, multiple through-substrate vias are grouped together and separated from other semiconductor devices to a distance (keep out zone (KOZ)) to reduce the impact on other devices. Generally speaking, when multiple through-substrate vias are separated from other devices to a defined keep out zone or beyond its keep out zone, the impact of the stress of the multiple through-substrate vias on other devices can be minimized. For example, the current between the P-type metal oxide semiconductor and the N-type metal oxide semiconductor can be well matched by setting the keep out zone. However, the setting of the keep out zone increases the area required for the circuit design, offsetting the benefits of the three-dimensional circuit (such as reducing the occupied circuit area). Summary of the invention

[0005] A semiconductor device includes: a substrate; a source region and a drain region disposed in the substrate; a shallow trench isolation (STI) region disposed in the substrate and surrounding the source region and the drain region; a plurality of through substrate vias (TSVs) penetrating the substrate, wherein the through substrate vias are adjacent to the shallow trench isolation region; and a compound semiconductor structure isolating the shallow trench isolation region and the through substrate vias. The through substrate vias have a first stress type, and the compound semiconductor structure has a second stress type, which is different from the first stress type.

[0006] A method for forming a semiconductor device includes: providing a substrate; forming a shallow trench isolation region, a source region, and a drain region in the substrate, wherein the shallow trench isolation region surrounds the source region and the drain region; forming an expansion trench in the substrate, and isolating the shallow trench isolation region from the source region and the drain region; filling a compound semiconductor structure in the expansion trench; and forming a plurality of through-substrate vias extending from above the front side surface of the substrate into the substrate, wherein the compound semiconductor structure surrounds the through-substrate vias. The through-substrate vias have a first stress type, and the compound semiconductor structure has a second stress type, which is different from the first stress type.

[0007] The semiconductor device of the present invention has a novel compound semiconductor structure, which is arranged around the periphery of multiple through-substrate vias and has a second stress type that can offset the first stress type of the multiple through-substrate vias, so as to prevent the stress of the multiple through-substrate vias from impacting other devices in the substrate and affecting the performance of the overall device. In addition, through the arrangement of the compound semiconductor structure, the discharge area between the multiple through-substrate vias and other devices can also be effectively reduced, thereby reducing the area required for the overall chip. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Figures 1 to 20 FIG. 4 is a cross-sectional view showing an intermediate stage of forming a semiconductor device according to some embodiments of the present invention.

[0009] Fig.21 FIG. 1 is a top view of a semiconductor device according to some embodiments of the present invention.

[0010] Fig. 22 FIG. 4 is a cross-sectional view of a semiconductor device according to another embodiment of the present invention.

[0011] Reference Numbers

[0012] 10: Semiconductor devices

[0013] 10A: Device area

[0014] 10B: Peripheral area

[0015] 20: Semiconductor devices

[0016] 20A: Device area

[0017] 20B: Peripheral area

[0018] 100: substrate

[0019] 102: Shallow Trench Isolation Area

[0020] 104: Source region

[0021] 106: drain region

[0022] 110: passivation layer

[0023] 120: pad oxide layer

[0024] 130: Hard mask layer

[0025] 140: Patterned photoresist layer

[0026] 150: Opening

[0027] 151: Opening

[0028] 152: Opening

[0029] 160: Initial groove

[0030] 170: Expansion groove

[0031] 180: Compound Semiconductor Structure

[0032] 190: Covering layer

[0033] 200: Gate structure

[0034] 210: Gate dielectric

[0035] 220: Gate electrode

[0036] 230: Gate spacer

[0037] 300: Interlayer dielectric layer

[0038] 310: Source contact plug

[0039] 320: drain contact plug

[0040] 410: Etching stop layer

[0041] 420: Intermetallic dielectric layer

[0042] 430: Source contact via

[0043] 440: Drain contact via

[0044] 450: Gate contact via

[0045] 480: Opening

[0046] 500: through-substrate via

[0047] 510: Diffusion barrier layer

[0048] 520: conductive layer

[0049] 530:Metal cover

[0050] 610: Etching stop layer

[0051] 620: Intermetallic dielectric layer

[0052] 630: Source metal via

[0053] 640: Drain metal via

[0054] 650: Gate metal vias

[0055] 660: Substrate metal vias

[0056] 730: Source metal layer

[0057] 740: Drain metal layer

[0058] 750: Gate metal layer

[0059] 760: substrate metal layer

[0060] A-A': Line segment DETAILED DESCRIPTION

[0061] The semiconductor device of the present invention is a device in which an innovative compound semiconductor structure is added between a plurality of through-substrate vias and other devices.

[0062] Figures 1 to 20 FIG. 1 is a cross-sectional view of an intermediate stage of forming a semiconductor device 10 according to some embodiments of the present invention. In one embodiment, the semiconductor device 10 may include any number of active components and passive components, which are omitted and not shown.

[0063] Reference Figure 1, the semiconductor device 10 of the present invention can be divided into a device area 10A and a peripheral area 10B. In the subsequent process, a metal oxide semiconductor (P-type or N-type) can be formed in the device area 10A, and a plurality of through-substrate vias and compound semiconductor structures can be formed in the peripheral area 10B. The initial structure of the semiconductor device may include a substrate 100, a shallow trench isolation region 102, a source region 104, and a drain region 106. The substrate 100 may be, for example, a wafer or a grain. In one embodiment, the substrate 100 may be a semiconductor substrate, such as a silicon substrate or a germanium substrate; a compound semiconductor substrate, including gallium nitride, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, or a combination thereof; an alloy semiconductor, including a silicon-germanium alloy, a phosphorus-arsenic-gallium alloy, an arsenic-aluminum-indium alloy, an arsenic-aluminum-gallium alloy, an arsenic-gallium-indium alloy, a phosphorus-gallium-indium alloy, an arsenic-phosphorus-gallium-indium alloy, or a combination thereof. In other embodiments, the substrate 100 may also be a semiconductor substrate on an insulating layer.

[0064] The device region 10A may include a shallow trench isolation region 102, a source region 104, and a drain region 106. The shallow trench isolation region 102 may define the range of the active region and electrically isolate the active region components in or on the substrate 100. In other embodiments, the shallow trench isolation region 102 may also be replaced by other isolation structures such as a deep trench isolation region and a local silicon oxide structure.

[0065] The source region 104 and the drain region 106 extend from the front surface of the substrate 100 into the substrate 100. In one embodiment, the source region 104 and the drain region 106 may be P-type or N-type. The depth of the source region 104 and the drain region 106 in the substrate 100 may be approximately between 20 nm and 100 nm. The source region 104 and the drain region 106 may be formed by methods such as ion implantation, diffusion process, in-situ doping, etc.

[0066] Reference Figure 2 , a passivation layer 110 and a pad oxide layer 120 are sequentially formed on the front side surface of the substrate 100. The passivation layer 110 only covers the device area 10A, while the pad oxide layer 120 covers the device area 10A and the peripheral area 10B. The material of the passivation layer 110 may include silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, silicon oxynitride carbide, etc. The material of the pad oxide layer 120 may include oxide. The passivation layer 110 and the pad oxide layer 120 may be formed by chemical vapor deposition. Since the subsequent etching process may completely consume the pad oxide layer 120, the provision of the passivation layer 110 can ensure that the components of the device area 10A are not damaged by the subsequent etching process. In other embodiments, the passivation layer 110 may be omitted, and only the pad oxide layer 120 is provided on the substrate 100.

[0067] Reference Figure 3 and Figure 4, a hard mask layer 130 is formed on the pad oxide layer 120, and a patterned photoresist layer 140 is formed on the hard mask layer 130. For example, the hard mask layer 130 can be formed by a deposition process, and the patterned photoresist layer 140 can be formed by a deposition and photolithography process. Figure 4 As shown, the patterned photoresist layer 140 has an opening 150 .

[0068] Reference Figure 5 , the pattern of the patterned photoresist layer 140 is transferred to the underlying hard mask layer 130 to form an opening 151. Specifically, the hard mask layer 130 may be etched using the patterned photoresist layer 140 as a mask to form the opening 151. The etching process may include dry etching, wet etching, or other similar methods. In one embodiment, the width of the opening 151 may be approximately between 1 μm and 5 μm.

[0069] Reference Figure 6 , the pattern of the hard mask layer 130 is transferred to the pad oxide layer 120 and the substrate 100 below to form an opening 152 and an initial trench 160. For example, the pad oxide layer 120 can be etched using the patterned hard mask layer 130 as a mask to form the opening 152, and then the substrate 100 can be etched using the patterned pad oxide layer 120 as a mask to form the initial trench 160. The initial trench 160 extends from the front side surface of the substrate 100 into the substrate 100, and its depth can be approximately between 1 μm and 5 μm. In this embodiment, the provision of the pad oxide layer 120 can relieve the stress of the substrate 100.

[0070] Reference Figure 7 Then, an isotropic wet etching process is performed on the initial trench 160 to further expand the initial trench 160 into an expanded trench 170. For example, the isotropic wet etching process can be performed by immersion, spraying, other suitable methods, or a combination thereof. The width of the expanded trench 170 can be approximately between 1 μm and 5 μm. The depth of the expanded trench 170 can be approximately between 1 μm and 5 μm. It is worth noting that in addition to expanding the initial trench 160, the wet etching process will also further reduce the remaining thickness of the pad oxide layer 120.

[0071] From the top view (see Fig.21 ), the expansion groove 170 in the peripheral area 10B is a ring structure, which surrounds a plurality of through-substrate vias to be formed subsequently. It is particularly noted that the conditions of the wet etching process can be controlled so that the expansion groove 170 is designed to have a preset profile, so that the compound semiconductor structure to be formed subsequently can more effectively eliminate the impact of the stress of the plurality of through-substrate vias on other devices.

[0072] In one embodiment, the etchant of the wet etching process may include ammonium hydroxide, diluted hydrofluoric acid, tetramethylammonium hydroxide, ammonia, ethylenediamine catechol, nitric acid, acetic acid, potassium hydroxide, or a combination thereof. In a specific embodiment, the wet etching process may be performed using tetramethylammonium hydroxide, followed by cleaning with diluted hydrofluoric acid. In this embodiment, the etching conditions (e.g., concentration, process time, cycle, or other similar parameters) of tetramethylammonium hydroxide may be designed so that the expanded trench 170 presents a U-shaped final profile.

[0073] Reference Figure 8 , a compound semiconductor structure 180 is formed in the expanded trench 170. In addition, the compound semiconductor structure 180 can be applied to the profile of the expanded trench 170, so as to have a U-shaped profile. The width and depth of the compound semiconductor structure 180 can be similar to the width and depth of the expanded trench 170, and will not be repeated here.

[0074] From the top view, since the expansion trench 170 is designed as a ring structure, the compound semiconductor structure 180 formed in the substrate 100 also has a ring structure, which surrounds the multiple through-substrate vias formed subsequently. In other words, the compound semiconductor structure 180 isolates the multiple through-substrate vias from other components in the substrate 100. As mentioned previously, since the multiple through-substrate vias have tensile stress (first stress type), the compound semiconductor structure 180 may have compressive stress (second stress type), so that the compressive stress of the compound semiconductor structure 180 can offset the tensile stress of the multiple through-substrate vias, thereby eliminating the stress of the multiple through-substrate vias from omnidirectionally impacting other devices in the substrate.

[0075] In one embodiment, the material of the compound semiconductor structure 180 may include a compound semiconductor, such as silicon germanium or other similar materials. Silicon germanium can be regarded as native silicon atoms (the same material as the substrate 100) doped with foreign germanium atoms. Since the mass of germanium atoms is greater than the mass of silicon atoms, a second stress type is generated. In other embodiments, silicon germanium can be further doped with, for example, boron to form a ternary compound of boron-doped silicon germanium. It should be understood that doped silicon germanium was originally widely used in logic wafer fabs, mainly to help improve the mobility of electrons / holes in active devices, such as doped silicon germanium and undoped silicon germanium lining its surface. However, dopants do not significantly change the second stress type in silicon germanium, so doping is not a necessary step. The compound semiconductor structure 180 can be formed by any suitable deposition method.

[0076] Reference Fig. 9, a cap layer 190 is formed on the compound semiconductor structure 180. The cap layer 190 may be formed by any suitable deposition method. The material of the cap layer 190 may include a material similar to that of the substrate 100, such as silicon or other similar materials. The thickness of the cap layer 190 may be approximately between 20 nm and 200 nm. The cap layer 190 may seal the compound semiconductor structure 180 in the substrate 100 to prevent the compound semiconductor structure 180 from being affected by subsequent processes. Since the previous etching process has reduced the thickness of the pad oxide layer 120 to a very thin thickness, the thickness of the cap layer 190 should be greater than the remaining thickness of the pad oxide layer 120 to effectively seal the compound semiconductor structure 180.

[0077] Reference Fig.10 After forming the cap layer 190, the passivation layer 110 and the pad oxide layer 120 are removed. An appropriate etching process can be performed using an etchant having a high etching selectivity ratio for nitride and oxide to remove the passivation layer 110 and the pad oxide layer 120, while leaving the cap layer 190 on the front side surface of the substrate 100.

[0078] Reference Fig.11 , a gate structure 200 is formed in the device region 10A, and then a gate spacer 230 is formed on the sidewall of the gate structure 200. For example, a gate dielectric layer and a gate electrode layer may be sequentially formed on the front side surface of the substrate 100. The method of forming the gate dielectric layer may include, for example, chemical vapor deposition, atomic layer deposition, etc. The method of forming the gate electrode layer may include, for example, physical vapor deposition, atomic layer deposition, electroplating, etc. Then, the gate dielectric layer and the gate electrode layer are patterned to form a gate dielectric 210 and a gate electrode 220, respectively. The patterning step may include a photolithography etching process. Thereafter, a gate spacer layer may be conformally deposited on the front side surface of the substrate 100, on the sidewall of the gate structure 200, and on the top surface of the gate structure 200. Then, the horizontal portion of the gate spacer layer (including the portion on the substrate 100 and the portion on the top surface of the gate structure 200) may be etched by an anisotropic etch-back process. The remaining portion of the gate spacer layer located on the sidewall of the gate structure 200 becomes the gate spacer 230 .

[0079] like Fig.11As shown, the gate structure 200 (including the gate dielectric 210 and the gate electrode 220) and the gate spacer 230 may be located on the front side surface of the substrate 100 and laterally located between the source region 104 and the drain region 106. The material of the gate dielectric 210 may include a high dielectric constant (e.g., K value greater than 7) material, such as hafnium oxide, hafnium silicate, hafnium silicon oxynitride, hafnium aluminum oxide, hafnium lanthanum oxide, hafnium zirconium oxide, hafnium tantalum oxide, hafnium titanium oxide, lanthanum oxide, aluminum oxide, silicon aluminum oxide, zirconium oxide, titanium oxide, tantalum oxide, yttrium oxide, silicon oxynitride, or other similar materials. The material of the gate electrode may include amorphous silicon, polycrystalline silicon, polycrystalline silicon germanium, metal, metal nitride, metal silicide, metal carbide, metal oxide, or other similar materials. The metal may include cobalt, ruthenium, aluminum, palladium, platinum, tungsten, copper, titanium, tantalum, silver, gold, nickel, the above materials, or a combination thereof.

[0080] Reference Fig.12 , an interlayer dielectric layer 300 is formed on the front side surface of the substrate 100. The interlayer dielectric layer 300 may surround the gate structure 200 and the gate spacer 230, and expose the top of the gate structure 200 and / or the gate spacer 230. For example, a dielectric material covering the cap layer 190 of the peripheral area 10B, and the gate structure 200 and the gate spacer 230 of the device area 10A may be blanket formed on the substrate 100. Then, the dielectric material 300 is chemically mechanically polished or mechanically ground to expose the top of the gate structure 200 and / or the gate spacer 230. The material of the interlayer dielectric layer 300 may include silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, silicon oxynitride carbide, tetraethoxysilane, undoped silicate glass, doped silicon oxide, low dielectric constant dielectric material, etc. The thickness of the interlayer dielectric layer 300 may be similar to the overall thickness of the gate structure 200.

[0081] Reference Fig.13 After forming the interlayer dielectric layer 300, a source contact plug 310 and a drain contact plug 320 may be formed in the device region 10A through the interlayer dielectric layer 300. For example, a plurality of openings corresponding to the source region 104 and the drain region 106 may be formed in the interlayer dielectric layer 300, and then the source contact plug 310 and the drain contact plug 320 may be formed in the openings. The material of the source contact plug 310 and the drain contact plug 320 may be similar to the material of the gate electrode 220. In one embodiment, a barrier layer (not shown) may be formed between the source contact plug 310 and the drain contact plug 320 and the sidewalls and bottom of the opening to prevent the material of the source contact plug 310 and the drain contact plug 320 from diffusing into the interlayer dielectric layer 300. The material of the barrier layer may include titanium nitride, titanium, tantalum, tantalum nitride, tungsten, tungsten nitride, or a combination thereof. In one embodiment, the barrier layer may be formed by physical vapor deposition, atomic layer deposition, electroplating, or other similar methods.

[0082] Reference Fig.14 , an etch stop layer 410 and an intermetallic dielectric layer 420 may be sequentially formed on the interlayer dielectric layer 300. The etch stop layer 410 may prevent subsequent processes from damaging the components below and the influence of the plasma of the back-end process on the front-end transistors. The intermetallic dielectric layer 420 may isolate the metal material above from the metal material below to avoid an electrical short circuit. The materials and formation methods of the etch stop layer 410 and the intermetallic dielectric layer 420 may be similar to those of the interlayer dielectric layer 300, and will not be described in detail here. It is worth noting that the material selected for the etch stop layer 410 should have a desired etching selectivity for certain specific components.

[0083] Reference Fig.15 Then, a source contact via 430, a drain contact via 440, and a gate contact via 450 may be formed in the device region 10A through the intermetallic dielectric layer 420 and the etch stop layer 410. The source contact via 430, the drain contact via 440, and the gate contact via 450 may physically contact the source contact plug 310, the drain contact plug 320, and the gate structure 200, respectively. The materials and formation methods of the source contact via 430, the drain contact via 440, and the gate contact via 450 may be similar to those of the source contact plug 310 and the drain contact plug 320, and will not be described in detail herein.

[0084] Continue to refer to Fig.15 After forming the intermetallic dielectric layer 420, a plurality of openings 480 may be formed in the peripheral region 10B through the intermetallic dielectric layer 420, the etch stop layer 410, and the interlayer dielectric layer 300, and extend into the substrate 100. Fig.15 Two openings 480 are shown in the figure, but the present invention is not limited thereto. The peripheral region 10B may include any number of openings 480, and may have suitable sizes and spacings. The width of the openings 480 may be approximately between 1 μm and 20 μm. The method for forming the plurality of openings 480 may be similar to the method for forming the initial trench 160 and / or the expanded trench 170, and will not be described in detail herein.

[0085] Reference Fig.16 , a plurality of through-substrate vias 500 are formed in the plurality of openings 480. For example, a diffusion barrier layer 510 may be conformally deposited on the bottom and sidewalls of the plurality of openings 480, and then a conductive layer 520 may be deposited to fill the remaining openings 480. Then, chemical mechanical polishing or mechanical grinding may be performed to make the top surfaces of the plurality of through-substrate vias 500 coplanar with the top surface of the intermetallic dielectric layer 420. Fig.16As shown, the through substrate vias 500 may include a diffusion barrier layer 510 and a conductive layer 520. The overall width of the plurality of through substrate vias 500 may be similar to the width of the opening 480. The materials of the diffusion barrier layer 510 and the conductive layer 520 may be similar to the gate dielectric 210 and the gate electrode 220, respectively.

[0086] Reference Fig.17 , a metal capping layer 530 is formed on the plurality of through-substrate vias 500. Although the metal capping layer 530 is illustrated as a single structure, the present invention is not limited thereto. The metal capping layer 530 may be a composite structure including a plurality of film layers. According to some embodiments of the present invention, the metal capping layer 530 may have good thermal stability and may effectively control the morphology of the plurality of through-substrate vias 500 to prevent the conductive layer 520 from being squeezed to cause gaps in the vias, cracks in the dielectric material, and loss of thickness. The material of the metal capping layer 530 may be similar to that of the gate electrode 220, such as an alloy mainly composed of cobalt. The metal capping layer 530 may be formed by any suitable deposition method.

[0087] Reference Fig.18 , an etch stop layer 610 and an intermetal dielectric layer 620 may be sequentially formed on the intermetal dielectric layer 420 and the metal cap layer 530. The etch stop layer 610 covers the metal cap layer 530. The materials and formation methods of the etch stop layer 610 and the intermetal dielectric layer 620 may be similar to those of the interlayer dielectric layer 300. It is worth noting that one or more sets of etch stop layers and intermetal dielectric layers may be additionally inserted between the intermetal dielectric layer 420 and the etch stop layer 610, depending on the application and design requirements.

[0088] Reference Fig.19, a source metal via 630, a drain metal via 640, and a gate metal via 650 may be formed in the intermetal dielectric layer 620 of the device region 10A and extend through the etch stop layer 610. The source metal via 630, the drain metal via 640, and the gate metal via 650 may respectively physically contact the source contact via 430, the drain contact via 440, and the gate contact via 450. In addition, a source metal layer 730, a drain metal layer 740, and a gate metal layer 750 may be formed in the intermetal dielectric layer 620. In one embodiment, the source metal layer 730 is electrically coupled to the source region 104 through the source metal via 630, the source contact via 430, and the source contact plug 310, the drain metal layer 740 is electrically coupled to the drain region 106 through the drain metal via 640, the drain contact via 440, and the drain contact plug 320, and the gate metal layer 750 is electrically coupled to the gate structure 200 through the gate metal via 650 and the gate contact via 450. The source metal layer 730, the drain metal layer 740, and the gate metal layer 750 can serve as the source terminal, the drain terminal, and the gate terminal of the metal oxide semiconductor transistor, respectively.

[0089] Continue to refer to Fig.19 , a substrate metal via 660 may be formed in the intermetal dielectric layer 620 of the peripheral region 10B and extend through the etch stop layer 610. The substrate metal via 660 may physically contact the metal cap layer 530. In other embodiments, the substrate metal via 660 may extend through the metal cap layer 530 and physically contact the through-substrate via 500. In addition, a substrate metal layer 760 may be formed in the intermetal dielectric layer 620. In one embodiment, the substrate metal layer 760 is electrically coupled to the through-substrate via 500 through the substrate metal via 660 and / or the metal cap layer 530. It should be understood that the source metal layer 730, the drain metal layer 740, the gate metal layer 750, and the substrate metal layer 760 may be regarded as metal traces of the back-end process.

[0090] The source metal via 630, the drain metal via 640, the gate metal via 650, the substrate metal via 660, the source metal layer 730, the drain metal layer 740, the gate metal layer 750, and the substrate metal layer 760 may be integrally formed and thus include the same material, which may be similar to the material of the gate electrode 220. First, a plurality of openings (including via openings and metal layer openings) may be formed in the etch stop layer 610 and the intermetallic dielectric layer 620, corresponding to the source contact via 430, the drain contact via 440, the gate contact via 450, and the through-substrate via 500 (or the metal cap layer 530), respectively. Next, the above materials may be filled into the plurality of openings through a suitable deposition process or a damascene process to form a source metal via 630 , a drain metal via 640 , a gate metal via 650 , a substrate metal via 660 , a source metal layer 730 , a drain metal layer 740 , a gate metal layer 750 , and a substrate metal layer 760 .

[0091] Reference Fig. 20 The substrate 100 can be thinned from the back surface of the substrate 100 until the bottoms of the plurality of through-substrate vias 500 in the peripheral region 10B are exposed, thereby completing the semiconductor device 10 of this embodiment. The substrate 100 can be thinned by a Taiko grinding process, a non-Taiko grinding process, or the like.

[0092] Fig.21 FIG. 1 is a top view of a semiconductor device 10 according to some embodiments of the present invention. It should be noted that Fig. 20 for Fig.21 Schematic diagram of the cross-section obtained by the line segment AA'. Fig.21 Only the front surface of the substrate 100 is shown. The corresponding positions of the gate structure 200 and the gate spacer 230 are marked with dotted lines. For illustrative purposes, only the shallow trench isolation region 102, the source region 104, the drain region 106, the gate structure 200, the gate spacer 230, the compound semiconductor structure 180, and the through-substrate via 500 are shown, and other components are omitted.

[0093] Reference Fig.21, the shallow trench isolation region 102 of the device region 10A defines an active region (e.g., a metal oxide semiconductor transistor formed by the source region 104, the drain region 106, the gate structure 200, and the gate spacer 230), and the compound semiconductor structure 180 of the peripheral region 10B surrounds a plurality of through-substrate vias 500. As mentioned previously, the compound semiconductor structure 180 of the embodiment of the present invention may have a compressive stress (a second stress type), which produces a mutually offsetting effect for the tensile stress (a first stress type) of the plurality of through-substrate vias 500, thereby preventing the stress of the plurality of through-substrate vias 500 from omnidirectionally impacting other devices in the substrate 100. In addition, due to the arrangement of the compound semiconductor structure 180, the plurality of through-substrate vias 500 do not need to maintain an excessively large spacing with the device region 10A to prevent the metal oxide semiconductor transistor from being impacted, thereby reducing the circuit area required for the entire chip. Here, although the compound semiconductor structure 180 is illustrated as a square ring, the present invention is not limited thereto. The compound semiconductor structure 180 may have a ring structure of any suitable geometric shape.

[0094] Fig. 22 FIG. 2 is a cross-sectional view of a semiconductor device 20 according to another embodiment of the present invention. The semiconductor device 20 can be divided into a device region 20A and a peripheral region 20B. Fig. 20 The embodiment of FIG. 1 is similar to the embodiment of FIG. 2 , except that the compound semiconductor structure 180 in the peripheral region 20B has a hexagonal profile. In this embodiment, the conditions of the wet etching can be adjusted to form an expansion trench 170 having a hexagonal profile (see FIG. 2 ). Figure 7 ), so that the compound semiconductor structure 180 can have a hexagonal profile. In other embodiments, the wet etching conditions can be further adjusted to make the expansion trench 170 and the compound semiconductor structure 180 have a rhombus, diamond, or other polygonal profiles.

[0095] Here, it is worth mentioning that when the compound semiconductor structure 180 has a U-shaped profile, the second stress type can be distributed across the sidewall of the compound semiconductor structure 180, and the sidewall surface can be used to offset the first stress type of the plurality of through-substrate vias 500. However, when the compound semiconductor structure 180 has a profile such as a hexagon or other polygon, the second stress type can be focused on the side corners (which have the maximum stress value) of the compound semiconductor structure 180, and the corner ends can be used to offset the first stress type of the plurality of through-substrate vias 500. The second stress type of the compound semiconductor structure 180 with a polygonal profile is greater than the second stress type of the compound semiconductor structure 180 with a U-shaped profile. The compound semiconductor structure 180 with an appropriate profile can be selected according to design requirements.

[0096] In summary, the semiconductor device of the present invention has a novel compound semiconductor structure, which is arranged around the periphery of the plurality of through-substrate vias and has a second stress type that can offset the first stress type of the plurality of through-substrate vias, so as to prevent the stress of the plurality of through-substrate vias from impacting other devices in the substrate and affecting the performance of the overall device. In addition, through the arrangement of the compound semiconductor structure, the discharge area between the plurality of through-substrate vias and other devices can also be effectively reduced, thereby reducing the area required for the overall chip.

[0097] In particular, Figures 1 to 22 In the figure, the structures of the devices are not drawn in actual proportion for the sake of clarity. For example, the size of the metal oxide semiconductor transistor (composed of the source region 104, the drain region 106, the gate structure 200, and the gate spacer 230) drawn in the device region 10A is much smaller than the size of the through-hole conductor via 500 and the compound semiconductor structure 180.

[0098] Although the present invention is disclosed in the above embodiments, it is not intended to limit the present invention. Those skilled in the art may make some modifications and improvements without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be determined by the above claims.

Claims

1. A semiconductor device, characterized in that: include: a substrate; A source region and a drain region are disposed in the substrate; A shallow trench isolation region is disposed in the substrate and surrounds the source region and the drain region; A plurality of through-substrate vias penetrate the substrate, wherein the through-substrate vias are adjacent to the shallow trench isolation region and have a first stress type; as well as A compound semiconductor structure isolates the shallow trench isolation region and the through substrate vias, wherein the compound semiconductor structure has a second stress type, which is different from the first stress type.

2. The semiconductor device according to claim 1, wherein The shallow trench isolation region defines a device region.

3. The semiconductor device according to claim 2, wherein: The through substrate vias are located in a peripheral area outside the device area.

4. The semiconductor device according to claim 1, wherein: The compound semiconductor structure is arranged in the substrate and surrounds the through-substrate vias.

5. The semiconductor device according to claim 1, wherein: The shallow trench isolation region, the source region, the drain region, and the compound semiconductor structure extend from a front side surface of the substrate into the substrate.

6. The semiconductor device according to claim 5, wherein: The invention further comprises a gate structure, which is disposed on the front surface of the substrate and is laterally located between the source and the drain regions.

7. The semiconductor device according to claim 6, wherein: Also includes: an interlayer dielectric layer, located on the front surface of the substrate and surrounding the gate structure; a first etch stop layer disposed on the interlayer dielectric layer; a first intermetallic dielectric layer disposed on the first etch stop layer; a second etch stop layer disposed on the first intermetal dielectric layer; and A second intermetal dielectric layer is disposed on the second etch stop layer.

8. The semiconductor device according to claim 7, wherein: Also includes: A source contact plug and a drain contact plug are disposed through the interlayer dielectric layer and connected to the source region and the drain region, respectively; A source contact via, a drain contact via, and a gate contact via are disposed through the first intermetallic dielectric layer and the first etch stop layer and are connected to the source contact plug, the drain contact plug, and the gate structure, respectively; a source metal via, a drain metal via, and a gate metal via, disposed through the second intermetallic dielectric layer and the second etch stop layer, and connected to the source contact via, the drain contact via, and the gate contact via, respectively; and A source metal layer, a drain metal layer, and a gate metal layer are located in the second intermetallic dielectric layer and are respectively coupled to the source metal via, the drain metal via, and the gate metal via.

9. A method for forming a semiconductor device, characterized in that: include: providing a substrate; Forming a shallow trench isolation region, a source region, and a drain region in the substrate, wherein the shallow trench isolation region surrounds the source region and the drain region; forming an extended trench in the substrate and isolating the source region and the drain region by the shallow trench isolation region; Filling a compound semiconductor structure in the expansion trench; as well as A plurality of through substrate vias are formed extending from above a front surface of the substrate into the substrate, wherein the compound semiconductor structure surrounds the through substrate vias, wherein the through substrate vias have a first stress type, and the compound semiconductor structure has a second stress type, the second stress type being different from the first stress type.

10. The method for forming a semiconductor device according to claim 9, wherein: Forming the expansion groove includes: forming a pad oxide layer, a hard mask layer, and a patterned photoresist layer in sequence on the front surface of the substrate; patterning the hard mask layer and the pad oxide layer using the patterned photoresist layer; The substrate is etched using the patterned pad oxide layer as a mask.

11. The method for forming a semiconductor device according to claim 10, wherein: Etching the substrate comprises: performing a dry etching process to form an initial trench; and After the dry etching process is completed, a wet etching process is performed to expand the initial trench into the expanded trench.

12. The method for forming a semiconductor device according to claim 9, wherein: The method further includes forming a cap layer on the compound semiconductor structure.

13. The method for forming a semiconductor device according to claim 9, wherein: The method further includes sequentially depositing an interlayer dielectric layer, a first etch stop layer, a first intermetallic dielectric layer, a second etch stop layer, and a second intermetallic dielectric layer on the front surface of the substrate.

14. The method for forming a semiconductor device according to claim 13, wherein: Forming the through substrate vias includes: After depositing the first intermetallic dielectric layer, etching a plurality of openings through the first intermetallic dielectric layer, the first etch stop layer, and the interlayer dielectric layer and extending into the substrate; depositing a diffusion barrier layer on the bottom and sidewalls of the openings; and A conductive layer is formed to fill the openings.

15. The method for forming a semiconductor device according to claim 14, wherein: The method further includes forming a metal capping layer on the top surfaces of the diffusion barrier layer and the conductive layer.

16. The method for forming a semiconductor device according to claim 15, wherein: Also includes: forming a substrate metal via through the second intermetallic dielectric layer and the second etch stop layer and connected to the metal cap layer; and A substrate metal layer is formed in the second intermetallic dielectric layer and coupled to the substrate metal via.