MEMS piezoelectric resonator manufacturing method and MEMS piezoelectric resonator

By using SOI wafers and forming electrical connection points and channel structures during the manufacturing process of MEMS piezoelectric resonators, the high manufacturing cost and wafer warping problems caused by Cavity SOI processing method are solved, and the Q value of the device is improved and performance.

CN118900105APending Publication Date: 2024-11-05MST MICROELECTRONICS (SHENZHEN) CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410989852.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The manufacturing cost of MEMS piezoelectric resonators is high, and the Cavity SOI processing method increases the risk of wafer warping and overall thickness, affecting performance.

Method used

Using SOI wafers, the second insulating layer is removed by forming the first and second release ports, and a MEMS piezoelectric resonator is formed to reduce manufacturing costs, and the Q value is increased by forming electrical connection points and channel structures in the device layer.

Benefits of technology

The manufacturing cost of MEMS piezoelectric resonator is reduced, the problems of wafer warping and overall thickness increase are avoided, and the Q value of the device is improved, which improves the low-frequency noise performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900105A_ABST
    Figure CN118900105A_ABST
Patent Text Reader

Abstract

The embodiment of the invention discloses a manufacturing method of an MEMS (Micro Electro Mechanical System) piezoelectric resonator and the MEMS piezoelectric resonator. The manufacturing method of the MEMS piezoelectric resonator comprises the steps that an SOI wafer is provided, and the SOI wafer comprises a first insulating layer, a substrate, a second insulating layer and a device layer which are sequentially arranged in a stacked mode from bottom to top; sequentially forming a first electrode layer, a piezoelectric layer and a second electrode layer exposing part of the piezoelectric layer on the device layer from bottom to top; patterning the first electrode layer, the piezoelectric layer and the second electrode layer to form a first electrode, a piezoelectric structure and a second electrode, and exposing part of the device layer; etching the exposed device layer to form a first release port and a second release port; and removing part of the second insulating layer through the first release port and the second release port to form the MEMS piezoelectric resonator. According to the scheme, the manufacturing cost of the MEMS piezoelectric resonator can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present application relate to the field of micro-electromechanical technology, and more particularly to a method for manufacturing a MEMS piezoelectric resonator and a MEMS piezoelectric resonator. Background Art

[0002] Micro-Electro-Mechanical System (MEMS) is a high-tech field based on microelectronics and micromachining technology. MEMS technology can integrate mechanical components, drive components, electronic control systems, digital processing systems, etc. into an integrated micro unit. MEMS devices have many advantages such as being small, intelligent, executable, integrable, having good process compatibility, and low cost. The development of MEMS technology has opened up a new technological field and industry. Micro sensors, micro actuators, micro components, micromechanical optical devices, vacuum microelectronic devices, power electronic devices, etc. made using MEMS technology have very broad application prospects in the fields of aviation, aerospace, automobiles, biomedicine, environmental monitoring, military, and the Internet of Things.

[0003] MEMS piezoelectric resonators generally rely on the processing method of buried cavity SOI (Cavity SOI). The advantage of Cavity SOI is that the cavity is made at the bottom of the MEMS piezoelectric resonator in advance to avoid a series of problems such as side drilling and footing effect caused by release and other issues in the final stage of the production process, which lead to poor performance of the MEMS piezoelectric resonator. However, the manufacturing cost of Cavity SOI is relatively high. Summary of the invention

[0004] The embodiments of the present application provide a method for manufacturing a MEMS piezoelectric resonator and a MEMS piezoelectric resonator, which can reduce the manufacturing cost of the MEMS piezoelectric resonator.

[0005] The present application provides a method for manufacturing a MEMS piezoelectric resonator, comprising:

[0006] Providing an SOI wafer, the SOI wafer comprising a first insulating layer, a substrate, a second insulating layer and a device layer stacked in sequence from bottom to top;

[0007] Forming a first electrode layer, a piezoelectric layer, and a second electrode layer exposing a portion of the piezoelectric layer in sequence from bottom to top on the device layer;

[0008] Patterning the first electrode layer, the piezoelectric layer and the second electrode layer to form a first electrode, a piezoelectric structure and a second electrode, and exposing a portion of the device layer;

[0009] Etching the exposed device layer to form a first release opening and a second release opening;

[0010] A portion of the second insulating layer is removed through the first release opening and the second release opening to form a MEMS piezoelectric resonator.

[0011] In the method for manufacturing a MEMS piezoelectric resonator provided in an embodiment of the present application, after the first electrode layer, the piezoelectric layer, and the second electrode layer exposing a portion of the piezoelectric layer are sequentially formed on the device layer from bottom to top, the first electrode layer, the piezoelectric layer, and the second electrode layer are patterned to form a first electrode, a piezoelectric structure, and a second electrode, and before a portion of the device layer is exposed, the method further includes:

[0012] A first electrical connection point penetrating through the piezoelectric layer and connected to the first electrode layer and a second electrical connection point covering a portion of the second electrode layer are formed.

[0013] In the method for manufacturing a MEMS piezoelectric resonator provided in an embodiment of the present application, after etching the device layer to form a first release port and a second release port, a portion of the second insulating layer is removed through the first release port and the second release port before forming the MEMS piezoelectric resonator, the method further includes:

[0014] A photoresist layer is formed on a side wall of the second release opening away from the second electrical connection point, penetrating through the second insulating layer and connected to the substrate.

[0015] In the method for manufacturing a MEMS piezoelectric resonator provided in an embodiment of the present application, etching the exposed device layer to form a first release port and a second release port includes:

[0016] The exposed device layer is etched by deep reactive ion etching process to form a first release port and a second release port.

[0017] In the method for manufacturing a MEMS piezoelectric resonator provided in an embodiment of the present application, removing the second insulating layer through the first release port and the second release port to form the MEMS piezoelectric resonator includes:

[0018] A dry etching process or a wet etching process is used to etch a portion of the second insulating layer through the first release opening and the second release opening to form a cavity, thereby obtaining a MEMS piezoelectric resonator.

[0019] In a second aspect, an embodiment of the present application provides a MEMS piezoelectric resonator, which is manufactured using the above-mentioned method for manufacturing a MEMS piezoelectric resonator, and the MEMS piezoelectric resonator includes:

[0020] a first insulating layer;

[0021] a substrate, wherein the substrate is disposed on the first insulating layer;

[0022] a second insulating layer, wherein the second insulating layer is disposed on the substrate;

[0023] A device layer, wherein the device layer is arranged on the second insulating layer, a cavity is provided between the device layer and the substrate, the device layer comprises a coupling structure, a coupling beam, a connecting beam, at least one pair of anchor points and at least one pair of resonators, the resonators are connected to the coupling structure through the coupling beam, the anchor points are connected to the coupling structure through the connecting beam, the resonators have first release ports arranged in an array, and an auxiliary structure is provided at the center of the coupling structure.

[0024] The MEMS piezoelectric resonator provided in the embodiment of the present application also includes:

[0025] A first channel is disposed in the connecting beam and extends from the anchor point to the auxiliary structure.

[0026] In the MEMS piezoelectric resonator provided in the embodiment of the present application, a second channel is provided between the coupling beam and the auxiliary structure.

[0027] In the MEMS piezoelectric resonator provided in the embodiment of the present application, a second channel is provided between the connecting beam and the auxiliary structure.

[0028] In the MEMS piezoelectric resonator provided in the embodiment of the present application, a phononic crystal is provided at the intersection of the connecting beam and the auxiliary structure.

[0029] In summary, the manufacturing method of the MEMS piezoelectric resonator provided in the embodiment of the present application includes providing an SOI wafer, wherein the SOI wafer includes a first insulating layer, a substrate, a second insulating layer, and a device layer stacked in sequence from bottom to top; forming a first electrode layer, a piezoelectric layer, and a second electrode layer exposing a portion of the piezoelectric layer in sequence from bottom to top on the device layer; patterning the first electrode layer, the piezoelectric layer, and the second electrode layer to form a first electrode, a piezoelectric structure, and a second electrode, and exposing a portion of the device layer; etching the exposed device layer to form a first release port and a second release port; removing a portion of the second insulating layer through the first release port and the second release port to form a MEMS piezoelectric resonator. This solution forms a MEMS piezoelectric resonator by using SOI. Compared with using Cavity SOI to form a MEMS piezoelectric resonator, the manufacturing cost of using SOI to form a MEMS piezoelectric resonator is lower. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.

[0031] Figure 1 It is a schematic flow chart of a method for manufacturing a MEMS piezoelectric resonator provided in an embodiment of the present application.

[0032] Figure 2-Figure 7 It is a schematic diagram of the intermediate component structure of the MEMS piezoelectric resonator provided in an embodiment of the present application.

[0033] Figure 8 It is a schematic diagram of the structure of the MEMS piezoelectric resonator provided in an embodiment of the present application.

[0034] Fig. 9 yes Figure 8 Schematic diagram of the top view structure.

[0035] Fig.10 It is a schematic diagram of the shape of the auxiliary structure provided in the embodiment of the present application.

[0036] Fig.11 This is a forward phase simulation diagram of the MEMS piezoelectric resonator provided in an embodiment of the present application.

[0037] Fig.12 This is an inverse phase simulation diagram of the MEMS piezoelectric resonator provided in an embodiment of the present application. DETAILED DESCRIPTION

[0038] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The implementations described in the following exemplary embodiments do not represent all implementations consistent with the present application. Instead, they are merely examples of devices and methods consistent with some aspects of the present application as detailed in the appended claims.

[0039] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used in this application and in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used in this application includes any and all combinations of one or more related listed items.

[0040] It should be noted that, in this article, the terms "include", "comprises" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "includes a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element. In addition, components, features, and elements with the same name in different embodiments of the present application may have the same meaning or different meanings, and their specific meanings need to be determined by their explanation in the specific embodiment or further combined with the context of the specific embodiment.

[0041] It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0042] In the subsequent description, the suffixes such as "module", "component" or "unit" used to represent elements are only used to facilitate the description of the present application, and have no specific meanings. Therefore, "module", "component" or "unit" can be used in a mixed manner.

[0043] In the description of the present application, it should be noted that the terms "upper", "lower", "left", "right", "inner", "outer", "longitudinal", "lateral", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0044] Low Q value (quality factor) has always been one of the problems to be solved for MEMS piezoelectric resonators. For MEMS piezoelectric resonators used as low-jitter products, under the condition of the same feedthrough capacitance, a high Q value means that when the frequency is adjusted through the load capacitance, the load capacitance has a higher resolution for frequency adjustment. At the same time, a higher Q value also brings better low-frequency noise performance. Therefore, for MEMS piezoelectric resonators, improving the Q value is very important for improving the performance of MEMS piezoelectric resonators.

[0045] MEMS piezoelectric resonators generally rely on the Cavity SOI processing method. The advantage of Cavity SOI is that a cavity is made at the bottom of the MEMS piezoelectric resonator in advance to avoid poor performance of the MEMS piezoelectric resonator due to side drilling, footing effect and other problems caused by release and other issues in the final stage of the production process. However, the problems brought by Cavity SOI are also very significant. Compared with SOI (Silicon-On-Insulator), Cavity SOI has a higher cost. In addition, when making Cavity SOI, the increase in the number of bonding times will cause the wafer warpage to further increase, which has a greater impact on the multi-pair stacked structure of the MEMS piezoelectric resonator. Finally, when using Cavity SOI, the overall thickness of the MEMS piezoelectric resonator will inevitably increase, so it is necessary to add multiple thinning steps in the process steps to increase the processing risk.

[0046] Based on this, the embodiment of the present application provides a method for manufacturing a MEMS piezoelectric resonator and a MEMS piezoelectric resonator. The technical solution shown in the present application will be described in detail through specific embodiments. It should be noted that the description order of the following embodiments does not limit the priority order of the embodiments.

[0047] See also Figure 1 , Figure 1 : is a schematic diagram of a method for manufacturing a MEMS piezoelectric resonator provided in an embodiment of the present application. The specific process of the method for manufacturing a MEMS piezoelectric resonator may be as follows:

[0048] 101. Provide an SOI wafer, wherein the SOI wafer includes a first insulating layer, a substrate, a second insulating layer, and a device layer stacked in sequence from bottom to top.

[0049] In some embodiments, the SOI wafer 10 may be Figure 2 shown.

[0050] The materials of the first insulating layer 11 and the second insulating layer 13 may be silicon oxide, aluminum nitride, aluminum oxide, etc. The material of the substrate 12 may be single crystal silicon.

[0051] In a specific implementation process, after step 101 , the device layer 14 may be doped with PSG and annealed.

[0052] 102. Form a first electrode layer, a piezoelectric layer, and a second electrode layer exposing a portion of the piezoelectric layer in sequence from bottom to top on the device layer.

[0053] The first electrode layer 20 and the second electrode layer 40 can be prepared by sputtering or electron beam evaporation, and the piezoelectric layer 30 can be prepared by low pressure chemical vapor deposition (LPCVD) or molecular beam epitaxy (MBE).

[0054] In the specific implementation process, the first electrode layer 20, the piezoelectric layer 30 and the second electrode layer 40 can be formed sequentially from bottom to top on the device layer 14. Then, a patterned first photoresist layer is formed on the second electrode layer 40 by a photolithography process, and then a portion of the second electrode layer 40 is etched by ion beam etching (IBE) to expose a portion of the piezoelectric layer 30, and finally the first photoresist layer is removed to form a Figure 3 The structure shown.

[0055] The materials of the first electrode layer 20 and the second electrode layer 40 can be molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof. The material of the piezoelectric layer 30 can be aluminum nitride, zinc oxide, lead zirconate titanate (PZT), etc.

[0056] 103. Pattern the first electrode layer, the piezoelectric layer, and the second electrode layer to form a first electrode, a piezoelectric structure, and a second electrode, and expose a portion of the device layer.

[0057] In some embodiments, a patterned third photoresist layer can be formed on the surface of the second electrode layer 40 and the piezoelectric layer 30 by a photolithography process, and then the first electrode layer 20, the piezoelectric layer 30 and the second electrode layer 40 are etched by ion beam etching (IBE) to form a first electrode, a piezoelectric structure and a second electrode. At the same time, a portion of the device layer 14 is exposed to form a Figure 6 The structure shown.

[0058] Before step 103, the first electrical connection point 50 connected to the first electrode layer 20 through the piezoelectric layer 30 and the second electrical connection point 60 covering a portion of the second electrode layer 40 are formed, so as to form Figure 5 Specifically, a patterned second photoresist layer can be formed on the surface of the piezoelectric layer 30 by a photolithography process, and then the piezoelectric layer 30 is etched by ion beam etching (IBE) to expose a portion of the first electrode layer 20, and then the second photoresist layer is removed to form a structure as shown. Figure 4 Finally, the first electrical connection point 50 and the second electrical connection point 60 are deposited to form the structure shown in FIG. Figure 5 The structure shown.

[0059] The first electrical connection point 50 and the second electrical connection point 60 can be prepared by sputtering or electron beam evaporation. The material of the first electrical connection point 50 and the second electrical connection point 60 can be gold or aluminum.

[0060] 104. Etch the exposed device layer to form a first release opening and a second release opening.

[0061] Specifically, the third photoresist layer can be used as a protective layer, and then the exposed device layer 14 can be etched using a deep reactive ion etching process to form a first release port 15 and a second release port 16, so as to obtain Figure 7 The structure shown.

[0062] 105. Remove a portion of the second insulating layer through the first release port and the second release port to form a MEMS piezoelectric resonator.

[0063] In some embodiments, before step 105, a photoresist layer may be formed on the side wall of the second release port 16 away from the second electrical connection point 60 to pass through the second insulating layer 13 and connect to the substrate 12. Specifically, a patterned fourth photoresist layer may be formed on the side wall of the second release port 16 away from the second electrical connection point 60 by a photolithography process to protect the second insulating layer 13 on the non-etched side. Then, a dry etching process or a wet etching process is used to etch part of the second insulating layer 13 through the first release port 15 and the second release port 16 to form a cavity, so that the device is suspended, and finally the third photoresist layer and the fourth photoresist layer are removed to obtain the following. Figure 8 The MEMS piezoelectric resonator shown.

[0064] In summary, the manufacturing method of the MEMS piezoelectric resonator provided in the embodiment of the present application forms the MEMS piezoelectric resonator by using SOI. Compared with the MEMS piezoelectric resonator formed by using Cavity SOI, the manufacturing cost of the MEMS piezoelectric resonator formed by using SOI is lower. It can also avoid the problem that when making Cavity SOI, the warping of the SOI wafer will be further increased due to the increase in the number of bonding times, which has a greater impact on the multiple pairs of stacked structures of the MEMS piezoelectric resonator. It can also avoid the problem that when using Cavity SOI, the overall thickness of the MEMS piezoelectric resonator will inevitably increase, so it is necessary to add multiple thinning steps in the process steps, which increases the processing risk.

[0065] The following will specifically describe the MEMS piezoelectric resonator manufactured by the above-mentioned method for manufacturing a MEMS piezoelectric resonator. The meanings of the terms are the same as those in the above-mentioned method for manufacturing a MEMS piezoelectric resonator, and the specific implementation details can refer to the description of the above-mentioned method for manufacturing a MEMS piezoelectric resonator.

[0066] See also Figure 8 and Fig. 9 ,in Fig. 9 yes Figure 8 The MEMS piezoelectric resonator may include a first insulating layer 11, a substrate 12, a second insulating layer 13 and a device layer 14 stacked in sequence from bottom to top.

[0067] There is a cavity between the device layer 14 and the substrate 12; the device layer 14 includes a coupling structure 108, a coupling beam 103, a connecting beam 104, at least one pair of anchor points 102 and at least one pair of resonators 101, the resonator 101 is connected to the coupling structure 108 through the coupling beam 103, the anchor point 102 is connected to the coupling structure 108 through the connecting beam 104, the resonator 101 has an array-arranged first release port 15, and an auxiliary structure 107 is arranged at the center of the coupling structure 108.

[0068] Each pair of anchor points 102 is symmetrically arranged about the coupling structure 108, and each pair of resonators 101 is symmetrically arranged about the coupling structure 108. It can be understood that there is a second insulating layer 13 between the substrate 12 and the device layer 14. A first insulating layer 11 is arranged on the side of the substrate 12 away from the device layer 14.

[0069] In the specific implementation process, the auxiliary structure 107 located at the center of the coupling structure 108 can effectively form an energy propagation band gap, so that the coupling structure 108 is generally ring-shaped, and a path is established for energy transfer, so that energy can be transmitted along the ring-shaped coupling structure 108, reducing energy loss and improving the Q value.

[0070] It should be noted that the auxiliary structure 107 includes but is not limited to Fig. 9 The fan-shaped and rod-shaped structures of the array arrangement shown may also include Fig.10 The shown square shape, circular array convex shape, cross block shape, square four-corner array square shape or square center penetrating shape, etc.

[0071] In some embodiments, the MEMS piezoelectric resonator may further include a first channel 105, which is disposed in the connecting beam 104 and extends from the anchor point 102 to the auxiliary structure 107. The first channel 105 can prevent energy loss at the anchor point 102, reduce the loss of the anchor point 102, and improve the Q value of the resonator.

[0072] In one embodiment, the MEMS piezoelectric resonator may further include a second channel 106 disposed between the coupling beam 103 and the auxiliary structure 107, and a second channel 106 between the connecting beam 104 and the auxiliary structure 107. The second channel 106 can prevent the coupling structure 108 from distributing energy due to an excessively large non-displacement area, thereby improving the Q value.

[0073] In another embodiment, a phononic crystal is disposed at the intersection of the connecting beam 104 and the auxiliary structure 107. The phononic crystal can effectively form an energy propagation band gap, avoid energy loss at the anchor point 102, reduce the loss at the anchor point 102, and improve the Q value.

[0074] In addition, the MEMS piezoelectric resonator works in an in-plane mode, which may specifically include an SE mode, a LE mode, a breathing mode, a Wine glass mode, and a WE mode.

[0075] It should be noted that the first release port 15 , the first channel 105 , the second channel 106 , the gap between the auxiliary structure 107 , and the gap between the auxiliary structure 107 and the coupling structure 108 are formed synchronously, and the specific formation process is not repeated here.

[0076] It can be understood that in order to ensure the consistency of etching load during synchronous processing, the width of the first release port 15, the width of the first channel 105, the width of the second channel 106, the gap width between the auxiliary structures 107, and the gap width between the auxiliary structure 107 and the coupling structure 108 are roughly kept consistent.

[0077] See also Fig.11 and Fig.12 , Fig.11 is a forward phase simulation diagram of a MEMS piezoelectric resonator provided in an embodiment of the present application, Fig.12 is a reverse phase simulation diagram of a MEMS piezoelectric resonator provided in an embodiment of the present application. Fig.11 The Q value of the MEMS piezoelectric resonator in the positive phase reaches 7.1987e5. Fig.12 The Q value of the medium inverse-phase MEMS piezoelectric resonator is reduced to 2260.2, which proves that the performance of the MEMS piezoelectric resonator provided in the embodiment of the present application is significantly improved.

[0078] In summary, the MEMS piezoelectric resonator provided in the embodiment of the present application may include a first insulating layer 11, a substrate 12, a second insulating layer 13 and a device layer 14 stacked in sequence from bottom to top. Among them, there is a cavity between the device layer 14 and the substrate 12; the device layer 14 includes a coupling structure 108, a coupling beam 103, a connecting beam 104, at least one pair of anchor points 102 and at least one pair of resonators 101, the resonator 101 is connected to the coupling structure 108 through the coupling beam 103, the anchor point 102 is connected to the coupling structure 108 through the connecting beam 104, the resonator 101 has a first release port 15 arranged in an array, and an auxiliary structure 107 is provided at the center of the coupling structure 108. This solution can effectively form an energy propagation bandgap through the auxiliary structure 107 located at the center of the coupling structure 108, so that the coupling structure 108 is generally annular, a path is set for energy transfer, and energy can be transmitted along the annular coupling structure 108, reducing energy loss and improving the Q value.

[0079] The above is a detailed introduction to the manufacturing method of the MEMS piezoelectric resonator and the MEMS piezoelectric resonator provided by the present application. Specific examples are used in the present application to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the core idea of ​​the present application. At the same time, for technical personnel in this field, according to the idea of ​​the present application, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A method for manufacturing a MEMS piezoelectric resonator, characterized in that: include: Providing an SOI wafer, the SOI wafer comprising a first insulating layer, a substrate, a second insulating layer and a device layer stacked in sequence from bottom to top; Forming a first electrode layer, a piezoelectric layer, and a second electrode layer exposing a portion of the piezoelectric layer in sequence from bottom to top on the device layer; Patterning the first electrode layer, the piezoelectric layer and the second electrode layer to form a first electrode, a piezoelectric structure and a second electrode, and exposing a portion of the device layer; Etching the exposed device layer to form a first release opening and a second release opening; A portion of the second insulating layer is removed through the first release opening and the second release opening to form a MEMS piezoelectric resonator.

2. The method for manufacturing a MEMS piezoelectric resonator according to claim 1, wherein: After forming a first electrode layer, a piezoelectric layer, and a second electrode layer exposing a portion of the piezoelectric layer in sequence from bottom to top on the device layer, patterning the first electrode layer, the piezoelectric layer, and the second electrode layer to form a first electrode, a piezoelectric structure, and a second electrode, and before exposing a portion of the device layer, the method further includes: A first electrical connection point penetrating through the piezoelectric layer and connected to the first electrode layer and a second electrical connection point covering a portion of the second electrode layer are formed.

3. The method for manufacturing a MEMS piezoelectric resonator according to claim 1, wherein: After etching the device layer to form a first release port and a second release port, a portion of the second insulating layer is removed through the first release port and the second release port before forming the MEMS piezoelectric resonator, the method further includes: A photoresist layer is formed on a side wall of the second release opening away from the second electrical connection point, penetrating through the second insulating layer and connected to the substrate.

4. The method for manufacturing a MEMS piezoelectric resonator according to claim 1, wherein: The step of etching the exposed device layer to form a first release port and a second release port comprises: The exposed device layer is etched by deep reactive ion etching process to form a first release port and a second release port.

5. The method for manufacturing a MEMS piezoelectric resonator according to claim 1, wherein: The method of removing the second insulating layer through the first release port and the second release port to form a MEMS piezoelectric resonator includes: A dry etching process or a wet etching process is used to etch a portion of the second insulating layer through the first release opening and the second release opening to form a cavity, thereby obtaining a MEMS piezoelectric resonator.

6. A MEMS piezoelectric resonator, manufactured by the method for manufacturing a MEMS piezoelectric resonator according to any one of claims 1 to 5, characterized in that: The MEMS piezoelectric resonator comprises: a first insulating layer; a substrate, wherein the substrate is disposed on the first insulating layer; a second insulating layer, wherein the second insulating layer is disposed on the substrate; A device layer, wherein the device layer is arranged on the second insulating layer, a cavity is provided between the device layer and the substrate, the device layer comprises a coupling structure, a coupling beam, a connecting beam, at least one pair of anchor points and at least one pair of resonators, the resonators are connected to the coupling structure through the coupling beam, the anchor points are connected to the coupling structure through the connecting beam, the resonators have first release ports arranged in an array, and an auxiliary structure is provided at the center of the coupling structure.

7. The MEMS piezoelectric resonator according to claim 6, wherein: Also includes: A first channel is disposed in the connecting beam and extends from the anchor point to the auxiliary structure.

8. The MEMS piezoelectric resonator according to claim 6, wherein: A second channel is provided between the coupling beam and the auxiliary structure.

9. The MEMS piezoelectric resonator according to claim 6, wherein: A second channel is provided between the connecting beam and the auxiliary structure.

10. The MEMS piezoelectric resonator according to claim 6, wherein: A phononic crystal is arranged at the intersection of the connecting beam and the auxiliary structure.

Citation Information

Cited By

  • Piezoelectric MEMS device and preparation method and application thereof

    CN122079066A