Loudspeaker mesh forming method based on etching
Through etching technology, the grid structure is formed on the metal plate, which solves the problem of deformation and fracture during the forming of the horn mesh, and realizes the reliable molding of the horn mesh with small mesh and high density.
Patent Information
- Application Number
- CN202410936992.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-05
AI Technical Summary
When the grid size becomes smaller and the density increases, conventional stamping molding can easily lead to product deformation or breakage, and it is impossible to form reliably.
Using the etching-based horn mesh molding method, a mesh-like mask area is formed on the surface of the metal plate, and an etching process is performed to form a through groove. Combined with the coating mask processing, etching liquid spraying, electropolishing and vacuum coating steps, it is formed. A speaker net with small mesh and high density.
It effectively avoids deformation and breakage of metal plates during molding, ensures reliable molding of the grid structure, and is suitable for producing speaker mesh with small mesh specifications and high density.
Smart Images

Figure CN118900394A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of speaker meshes, and in particular to a speaker mesh forming method based on etching. Background Art
[0002] For products with audio, such as new energy vehicles, a speaker mesh structure is necessary to protect the speakers in the audio and adjust the sound quality.
[0003] Currently, most speaker meshes are formed by stamping. However, as the mesh size of speaker meshes tends to become smaller and the mesh density tends to increase, the force applied to the speaker mesh by conventional stamping can easily cause the product to deform or even break during the forming process, which may make it impossible to reliably form a speaker mesh that meets the requirements. Summary of the invention
[0004] In view of the problems of the prior art, the present invention provides a speaker mesh forming method based on etching, which is suitable for preparing a speaker mesh with small mesh and high density.
[0005] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0006] The present invention provides a speaker mesh forming method based on etching, comprising the following steps:
[0007] A. forming a grid-shaped mask area on the surface of the metal plate, and performing a coating mask treatment on the mask area;
[0008] B. etching the metal plate so that a through groove is formed in the area of the metal plate not subjected to masking due to etching, thereby forming a grid structure;
[0009] C. Cleaning metal plates;
[0010] D. Perform surface treatment on the cleaned metal plate.
[0011] Furthermore, before step A, the method further includes:
[0012] The metal plate is divided into a grid area and a non-grid area, wherein the non-grid area is located at the periphery of the grid area, and the mask area is located in the grid area; the ratio of the area of the non-grid area to the area of the grid area is 1:1-1.5:1.
[0013] Step A also includes: performing a coating mask process on the non-grid area.
[0014] Furthermore, step B specifically includes:
[0015] B1. Move the metal plate to the etching device;
[0016] B2. Spray etching liquid onto the upper surface of the metal plate through an etching device, and use the etching liquid to etch through the mesh area to form a penetrating groove.
[0017] Furthermore, in step A, the upper surface and the lower surface of the mask area of the metal plate are respectively subjected to a coating mask treatment;
[0018] Step B1 specifically includes: moving the metal plate to the etching device, and soaking the lower surface of the metal plate with etching liquid;
[0019] The temperature of the etching solution for immersing the metal plate is 40-60° C., the temperature of the sprayed etching solution is 40-55° C., and the pressure value of the sprayed etching solution is 0.75-0.85 psi.
[0020] Furthermore, in step A, the mask area on the upper surface is mainly composed of multiple first mask strips, and the mask area on the lower surface is mainly composed of multiple second mask strips, and the ratio of the width of the first mask strips to the width of the second mask strips is 1:1.1-1:1.5.
[0021] Furthermore, in step A, the upper surface and the lower surface of the mask area of the metal plate are respectively subjected to a coating mask treatment;
[0022] Step B1 specifically includes:
[0023] B11. Move the metal plate to the etching device, and spray the etching liquid on the upper surface of the metal plate by the etching device;
[0024] B12. Execute step B11 until time t has passed, and then flip the metal plate so that the lower surface of the metal plate faces upward;
[0025] B13. The etching device sprays the etching liquid on the lower surface of the metal plate until a groove penetrating the grid structure is formed;
[0026] Wherein, t is a constant and t>0, the temperature of the sprayed etching solution is 40-55° C., and the pressure value of the sprayed etching solution is 0.75-0.85 psi.
[0027] Furthermore, a fixing mechanism is provided for executing step B12, and the fixing mechanism includes a fixing seat, a top cover, a lifting module, a motor, a gear module and two supporting columns, the two ends of the fixing seat are respectively rotatably set on the two supporting columns, the motor is driven by the gear module to connect to the fixing seat to drive the fixing seat to rotate, the top cover is movably set on the fixing seat, and the lifting module is used to drive the top cover to lift and lower relative to the fixing seat; a plurality of containing holes are provided in the fixing seat, the inner side walls of the containing holes are provided with supporting members, and the top cover is provided with revealing holes; the containing holes are used to accommodate the metal plate and expose the mask area of the metal plate to the outside, the supporting members are used to support the metal plate, and the revealing holes are used to expose the mask area of the metal plate to the outside.
[0028] Furthermore, the motor is provided with an encoder, and the encoder is used to sense the rotation amplitude of the motor's shaft.
[0029] Further, step D specifically includes:
[0030] D1. Mask the non-grid structure parts of the metal plate;
[0031] D2. Electropolishing the grid structure of the metal plate;
[0032] D3. Pickling and washing the electropolished metal plate to remove the liquid and film on the surface of the metal plate;
[0033] D4. Vacuum coating of metal plates.
[0034] Furthermore, between steps D3 and D4, the following steps are also included:
[0035] D31. Processing the metal plate to form a fixed structure;
[0036] D32. Clean the metal plate.
[0037] Beneficial effects of the present invention: The present invention etches a grid structure on a metal plate through an etching process, which applies less pressure to the metal plate than stamping, so that a speaker mesh with a small and dense grid can be reliably formed without deformation or even breakage. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 It is a flow chart of the present invention.
[0039] Figure 2 This is a schematic diagram of the etching device used in Example 1.
[0040] Figure 3 This is a schematic diagram of the etching device used in Example 2.
[0041] Figure 4 This is a top view of the fixing seat described in Example 2.
[0042] Figure numerals: 1—etching device, 2—etching tank, 3—spray module, 4—fixing mechanism, 5—fixing seat, 6—top cover, 7—lifting module, 8—motor, 9—gear module, 10—support column, 11—receiving hole, 12—support member, 13—encoder. DETAILED DESCRIPTION
[0043] In order to facilitate the understanding of those skilled in the art, the present invention is further described below in conjunction with the embodiments and drawings, and the contents mentioned in the embodiments are not intended to limit the present invention. The present invention is described in detail below in conjunction with the drawings.
[0044] Example 1
[0045] like Figure 1 and Figure 2 As shown, this embodiment provides a speaker mesh forming method based on etching, comprising the following steps:
[0046] A. forming a grid-shaped mask area on the surface of the metal plate, and performing a coating mask treatment on the mask area;
[0047] B. etching the metal plate so that a through groove is formed in the area of the metal plate not subjected to masking due to etching, thereby forming a grid structure;
[0048] C. Cleaning metal plates;
[0049] D. The cleaned metal plate is surface treated to produce a speaker mesh.
[0050] The present invention prepares the speaker mesh by etching, specifically, after masking the metal plate so that the through grooves in the speaker mesh are not covered by the film, the etching liquid is sprayed on the metal plate, and the etching liquid etches the position not covered by the film, thereby forming through grooves, so that the metal plate is formed into the speaker mesh. Compared with traditional stamping, the present invention applies less force to the metal plate during the forming process, can reliably avoid deformation of the metal plate or even fracture of the mesh structure during the forming process, and is suitable for reliably producing speaker meshes with small mesh specifications and high density.
[0051] Specifically, before step A, the method further includes:
[0052] The metal plate is divided into a grid area and a non-grid area, wherein the non-grid area is located at the periphery of the grid area, and the mask area is located in the grid area; the ratio of the area of the non-grid area to the area of the grid area is 1:1-1.5:1.
[0053] Step A also includes: performing a coating mask process on the non-grid area.
[0054] That is, the speaker mesh cannot be entirely a grid structure, and there must be non-grid areas, and these non-grid areas also need to be masked to ensure that they will not be etched by the etching solution during the etching process; preferably, the masking of the non-grid area and the mask area is completed at the same time.
[0055] Step B of the present invention specifically comprises:
[0056] B1. Move the metal plate to etching device 1;
[0057] B2. The etching liquid is sprayed onto the upper surface of the metal plate through the spray module 3 of the etching device 1, and the etching liquid etches through the mesh area to form a penetrating groove.
[0058] Specifically, in step A, the upper surface and the lower surface of the mask area of the metal plate are respectively subjected to a coating mask treatment;
[0059] Step B1 specifically includes: moving the metal plate to the etching device 1, specifically moving the metal plate to the etching tank 2 of the etching device 1, wherein the etching tank 2 is filled with a certain amount of etching liquid, and the lower surface of the metal plate is soaked by the etching liquid;
[0060] The temperature of the etching solution for immersing the metal plate is 40-60° C., the temperature of the sprayed etching solution is 40-55° C., and the pressure value of the sprayed etching solution is 0.75-0.85 psi.
[0061] That is, in order to improve efficiency, this embodiment requires masking of both the upper and lower surfaces of the metal plate. When etching is required, the lower surface is immersed in etching solution for etching, while the upper surface is etched by spraying. By etching at both ends simultaneously, the etching time can be effectively shortened, thereby avoiding excessive etching of the side walls of the groove due to etching solution remaining in the groove that has not been penetrated.
[0062] Specifically, in step A, the mask area on the upper surface is mainly composed of a plurality of first mask strips, and the mask area on the lower surface is mainly composed of a plurality of second mask strips, and the ratio of the width of the first mask strips to the width of the second mask strips is 1:1.1-1:1.5.
[0063] Since immersion etching retains more etching liquid than spray etching, the width of the second mask strip needs to be greater than the width of the first mask strip, thereby compensating for the over-etching of the groove sidewall caused by immersion etching.
[0064] In this embodiment, step D specifically includes:
[0065] D1. Mask the non-grid structure parts of the metal plate;
[0066] D2. Electropolishing the grid structure of the metal plate;
[0067] D3. Pickling and washing the electropolished metal plate to remove the liquid and film on the surface of the metal plate;
[0068] D4. Vacuum coating of metal plates.
[0069] That is, after the mesh structure is formed by etching, the mesh structure of the metal plate needs to be electro-polished to make the fine rough surfaces caused by etching smooth, so as to avoid scratches to people during subsequent installation or use, thereby improving safety.
[0070] Since the electropolishing is aimed at the etched grid structure, the unetched positions need to be masked. After the electropolishing is completed, the polishing electrolyte and film on the surface of the metal plate are washed away, and then the metal plate is electroplated to allow the metal plate (i.e. the speaker mesh) surface to have a layer of film for protection. The function of the electroplated film can be determined according to specific needs and will not be repeated here.
[0071] Specifically, between steps D3 and D4, the following steps are also included:
[0072] D31. Processing the metal plate to form a fixed structure;
[0073] D32. Clean the metal plate.
[0074] The fixing structure is a conventional structure, such as a hole position, etc., which is used to fix the speaker mesh to the desired position; taking the hole as an example, since drilling will inevitably produce debris, the hole is cleaned after electropolishing, so that the electrolyte, debris and membrane are washed away together.
[0075] Example 2
[0076] like Figure 1 , Figure 3 and Figure 4 As shown, compared with Example 1, the difference between this embodiment and Example 1 lies in steps A and B, specifically: in step A, the upper surface and the lower surface of the mask area of the metal plate are respectively subjected to a coating mask treatment;
[0077] Step B1 specifically includes:
[0078] B11. The metal plate is moved to the etching device 1, and the etching liquid is sprayed on the upper surface of the metal plate by the spray module 3 of the etching device 1;
[0079] B12. Execute step B11 until time t has passed, and then flip the metal plate so that the lower surface of the metal plate faces upward;
[0080] B13. The etching device 1 sprays the etching liquid on the lower surface of the metal plate until a groove penetrating the grid structure is formed;
[0081] Wherein, t is a constant and t>0, the temperature of the sprayed etching solution is 40-55° C., and the pressure value of the sprayed etching solution is 0.75-0.85 psi.
[0082] That is, the present embodiment adopts a double-sided etching method, that is, after etching at least half the depth of the through groove on the upper surface of the metal plate, the metal plate is turned over and the etching is continued until the through groove is etched through to form. Since the etching liquid in the groove can be separated from the groove by gravity when turning over, the side etching phenomenon caused by the etching liquid staying in the groove for too long can be effectively avoided.
[0083] Specifically, the present embodiment provides a fixing mechanism 4 for executing step B12, the fixing mechanism 4 includes a fixing seat 5, a top cover 6, a lifting module 7, a motor 8, a gear module 9 and two support columns 10, the two ends of the fixing seat 5 are respectively rotatably set on the two support columns 10, the motor 8 is driven by the gear module 9 to connect to the fixing seat 5 to drive the fixing seat 5 to rotate, the top cover 6 is movably set on the fixing seat 5, and the lifting module 7 is used to drive the top cover 6 to rise and fall relative to the fixing seat 5; a plurality of containing holes 11 are provided in the fixing seat 5, the inner side wall of the containing hole 11 is provided with a supporting member 12, and the top cover 6 is provided with an exposing hole; the containing hole 11 is used to accommodate the metal plate and expose the mask area of the metal plate to the outside, the supporting member 12 is used to support the metal plate, and the exposing hole is used to expose the mask area of the metal plate to the outside.
[0084] The fixed seat 5 of this embodiment is covered by the top cover 6 so that only the grid area is exposed to the outside world before and after flipping. The lifting module 7 is preferably a cylinder or an electric cylinder. When in use, the lifting module 7 drives the top cover 6 to rise, so that the robot or the staff can put the metal plate into the container hole 11. The multiple container holes 11 are set to achieve the one-time etching of multiple metal plates; and after the metal plates are placed in each container hole 11, the lifting module 7 controls the top cover 6 to descend so that the top cover 6 covers the fixed seat 5, and then the etching liquid can be sprayed; after the upper surface of the metal plate is etched for time t, the motor 8 is actuated to flip the fixed seat 5, so that the metal plate is flipped to the lower surface facing up, and then the etching liquid can be sprayed until the area of the metal plate that has not been masked is etched through, and the motor 8 is reset to drive the fixed seat 5 to reset, and then the lifting module 7 drives the top cover 6 to open, and the metal plate can be replaced to repeat the above action, achieving the effect of automatic flipping.
[0085] Specifically, the gear module 9 is preferably a reduction box.
[0086] In actual use, the motor 8 is provided with an encoder 13, which is used to sense the rotation amplitude of the rotating shaft of the motor 8, thereby ensuring that the rotation amplitude of the motor 8 is accurate and reliable, and further ensuring that the flip amplitude of the fixing seat 5 is accurate.
[0087] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention is disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with the profession can make some changes or modifications to equivalent embodiments of equivalent changes by using the technical contents disclosed above without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent changes and modifications made to the above embodiments according to the technology of the present invention are within the scope of the technical solution of the present invention without departing from the content of the technical solution of the present invention.
Claims
1. A speaker mesh forming method based on etching, characterized in that: The following steps are involved: A. forming a grid-shaped mask area on the surface of the metal plate, and performing a coating mask treatment on the mask area; B. etching the metal plate so that a through groove is formed in the area of the metal plate not subjected to masking due to etching, thereby forming a grid structure; C. Cleaning metal plates; D. Perform surface treatment on the cleaned metal plate.
2. The method for forming a speaker mesh based on etching according to claim 1, characterized in that: Before step A, also include: The metal plate is divided into a grid area and a non-grid area, wherein the non-grid area is located at the periphery of the grid area, and the mask area is located in the grid area; the ratio of the area of the non-grid area to the area of the grid area is 1:1-1.5:
1. Step A also includes: performing a coating mask process on the non-grid area.
3. The method for forming a speaker mesh based on etching according to claim 1, characterized in that: Step B specifically includes: B1. Move the metal plate to the etching device; B2. Spray etching liquid onto the upper surface of the metal plate through an etching device, and use the etching liquid to etch through the mesh area to form a penetrating groove.
4. The method for forming a speaker mesh based on etching according to claim 3, characterized in that: In step A, the upper surface and the lower surface of the mask area of the metal plate are respectively subjected to a coating mask treatment; Step B1 specifically includes: moving the metal plate to the etching device, and soaking the lower surface of the metal plate with etching liquid; The temperature of the etching solution for immersing the metal plate is 40-60° C., the temperature of the sprayed etching solution is 40-55° C., and the pressure value of the sprayed etching solution is 0.75-0.85 psi.
5. The method for forming a speaker mesh based on etching according to claim 3, characterized in that: In step A, the mask area on the upper surface is mainly composed of a plurality of first mask strips, and the mask area on the lower surface is mainly composed of a plurality of second mask strips, and the ratio of the width of the first mask strips to the width of the second mask strips is 1:1.1-1:1.
5.
6. The method for forming a speaker mesh based on etching according to claim 4, characterized in that: In step A, the upper surface and the lower surface of the mask area of the metal plate are respectively subjected to a coating mask treatment; Step B1 specifically includes: B11. Move the metal plate to the etching device, and spray the etching liquid on the upper surface of the metal plate by the etching device; B12. Execute step B11 until time t has passed, and then flip the metal plate so that the lower surface of the metal plate faces upward; B13. The etching device sprays the etching liquid on the lower surface of the metal plate until a groove penetrating the grid structure is formed; Wherein, t is a constant and t>0, the temperature of the sprayed etching solution is 40-55° C., and the pressure value of the sprayed etching solution is 0.75-0.85 psi.
7. The method for forming a speaker mesh based on etching according to claim 6, characterized in that: A fixing mechanism is provided for executing step B12, the fixing mechanism includes a fixing seat, a top cover, a lifting module, a motor, a gear module and two supporting columns, the two ends of the fixing seat are rotatably set on the two supporting columns respectively, the motor is driven by the gear module to connect to the fixing seat to drive the fixing seat to rotate, the top cover is movably set on the fixing seat, and the lifting module is used to drive the top cover to lift and lower relative to the fixing seat; a plurality of containing holes are provided in the fixing seat, the inner side walls of the containing holes are provided with supporting members, and the top cover is provided with revealing holes; the containing holes are used to accommodate the metal plate and expose the mask area of the metal plate to the outside, the supporting members are used to support the metal plate, and the revealing holes are used to expose the mask area of the metal plate to the outside.
8. The method for forming a speaker mesh based on etching according to claim 7, characterized in that: The motor is provided with an encoder, and the encoder is used to sense the rotation amplitude of the motor's rotating shaft.
9. The method for forming a speaker mesh based on etching according to claim 1, characterized in that: Step D specifically includes: D1. Mask the non-grid structure parts of the metal plate; D2. Electropolishing the grid structure of the metal plate; D3. Pickling and washing the electropolished metal plate to remove the liquid and film on the surface of the metal plate; D4. Vacuum coating of metal plates.
10. The method for forming a speaker mesh based on etching according to claim 9, characterized in that: Also included between steps D3 and D4: D31. Processing the metal plate to form a fixed structure; D32. Clean the metal plate.