Method for improving CO removal rate of sintering flue gas

By dividing the sintered flue gas into two categories: high CO and low CO, and performing optimization treatments respectively, metal catalysts and activated carbon adsorbents, the problem of easy deactivation of CO catalysts in traditional processes is solved, and efficient CO removal and The reduction of pollutants extends the life of the catalyst and reduces the treatment cost.

CN118904071APending Publication Date: 2024-11-08BAOSTEEL ZHANJIANG IRON & STEEL CO LTD

Patent Information

Application Number
CN202411187105.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-08

Smart Images

  • Figure CN118904071A_ABST
    Figure CN118904071A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of sintering flue gas purification, and discloses a method for improving the CO removal rate of sintering flue gas, which comprises the following steps: S1, dividing the sintering air box flue gas into high-CO flue gas and low-CO flue gas according to different CO concentrations in the flue gas of each air box of a sintering machine; s2, carrying out dust removal, water removal, desulfurization, decarbonization and denitration on the high-CO flue gas, and then discharging the flue gas through a chimney; and S3, the low-CO flue gas is discharged through a chimney after being subjected to dust removal, desulfurization and denitration. The sintering flue gas is divided into the high-CO flue gas and the low-CO flue gas according to the release rule of each pollutant in the sintering process, and the high-CO flue gas and the low-CO flue gas are respectively treated, so that the flue gas amount in the CO removal process is reduced by half, the treatment efficiency is improved, and meanwhile, the aim of CO emission reduction is fulfilled. Besides, the concentration of SO2, HCl and VOCs in the flue gas can reach extremely low values before decarbonization of the high-CO flue gas, the influence on the activity of a CO catalyst is reduced, and the service life of the catalyst is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of sintering flue gas purification, and more specifically discloses a method for improving the CO removal rate of sintering flue gas. Background Art

[0002] The sintering process refers to the process in which raw materials, fuel, flux, return ore and water are mixed and granulated, then added to the sintering machine through the distribution system, the ignition furnace ignites the fuel, and the exhaust locomotive draws air to complete the reaction. After the sintered ore is cooled and screened, it can enter the blast furnace to smelt molten iron. The sintering process is a very important step in the steel manufacturing process.

[0003] Since the flue gas produced during the sintering process contains a large amount of SO 2 , NOx, dust, CO, VOCs pollutants, and the emission of these pollutants accounts for 90% of the total pollutant emissions in the steel process. Sintering flue gas must be dusted, desulfurized, and denitrified before being discharged. CO removal from sintering flue gas is becoming more and more important.

[0004] Catalytic oxidation of CO is one of the best methods for flue gas with a CO concentration below 2%. However, even after desulfurization and denitrification, sintering flue gas still contains a small amount of SO 2 , trace amounts of VOCs and HCl, which can have a serious impact on the catalytic efficiency and life of CO oxidation catalysts. In sintering flue gas with a water content of up to 10%, SO 2 Sulfite is formed by adsorption on the catalyst surface, and then stable sulfate is formed by the hydroxide formed by dissociation of water, which will cover the active sites on the catalyst surface. Trace amounts of VOCs are attached to the catalyst surface by forming carbon deposits through incomplete oxidation. HCl will dissociate into chloride ions that are strongly adsorbed on the active sites and further form chloride salts. Sulfate and carbon deposits begin to decompose at high temperatures above 300 and 400°C respectively, while the decomposition of chloride salts requires a high temperature of more than 800°C. To reduce their impact, the reaction temperature of CO oxidation should be higher than 400°C, or the SO 2 , VOCs, and HCl concentrations. High temperature reaction and adding flue gas treatment equipment after the existing desulfurization and denitrification equipment will increase costs. The best solution is to reduce SO by optimizing process conditions and system control methods. 2 , VOCs, and HCl concentrations so that the flue gas will not quickly poison the CO oxidation catalyst.

[0005] In the traditional sintering flue gas treatment process, the flue gas extracted by each wind box is often collected and then uniformly subjected to dust removal, desulfurization, and denitrification, and then discharged after meeting the emission standards. The same is true for existing CO removal schemes, such as CN201921889301.9. The disadvantages of this method are large flue gas volume, many types of pollutants, and high concentrations, which make the CO catalyst easily deactivated and CO oxidation removal difficult.

[0006] In summary, there is an urgent need for a flue gas treatment method for CO in sintering flue gas, which can prevent other components in the flue gas from poisoning the CO oxidation catalyst while minimizing the flue gas treatment volume and treatment procedures to reduce costs. Summary of the invention

[0007] The present invention mainly provides a method for improving the CO removal rate of sintering flue gas, which can solve the problems that the traditional sintering flue gas treatment process causes the CO catalyst to be easily deactivated and the CO oxidation removal is difficult.

[0008] To solve the above technical problems, according to one aspect of the present invention, more specifically, a method for improving the CO removal rate of sintering flue gas comprises the following steps:

[0009] S1. Divide the sintering bellows flue gas into high CO flue gas and low CO flue gas according to the different CO concentrations in the flue gas of each bellows of the sintering machine;

[0010] S2, remove dust, water, desulfurize, decarbonize and denitrify the high CO flue gas and then discharge it through the chimney;

[0011] S3. The low CO flue gas is discharged through the chimney after dust removal, desulfurization and denitrification.

[0012] Furthermore, the high CO flue gas refers to sintering bellows flue gas with a CO concentration of 0.5-2 vol.%, preferably sintering bellows flue gas with a CO concentration of 1-1.8 vol.%.

[0013] Furthermore, the SO 2 Concentration less than 250 mg / m 3 、VOCs concentration is greater than 30mg / m 3 And the HCl concentration is less than 5 mg / m 3 More preferably, SO 2 Concentration less than 230 mg / m 3 , VOCs concentration is greater than 40mg / m 3 And the HCl concentration is less than 4 mg / m 3 ; Except for high CO flue gas, all other sintering bellows flue gases are low CO flue gases.

[0014] Furthermore, the diversion method of the sintering bellows flue gas is: the bellows under the sintering machine are numbered in sequence, with the serial numbers being 1, 2, 3, ..., x, ..., y; wherein the SO in the flue gas from bellows No. 1 to No. x is 2 The concentration was less than 250 mg / m 3 (Preferably less than 230 mg / m 3 ) and the HCl concentration is less than 5 mg / m 3(Preferably less than 4 mg / m 3 ); The flue gases from the 1st to the xth bellows are collected to form high CO flue gases, and the flue gases from the (x+1)th to the yth bellows are collected to form low CO flue gases. Further preferably, a is set to be an integer greater than or equal to 1 and less than x, and when the average CO concentration of the flue gases from the 1st to the ath bellows is not higher than the average CO concentration of the flue gases from the (x+1)th to the yth bellows, the flue gases from the (a+1)th to the xth bellows are collected to form high CO flue gases, and the flue gases from the 1st to the ath bellows and the (x+1)th to the yth bellows are collected to form low CO flue gases.

[0015] Furthermore, the dehydration in step S2 is to cool the high CO flue gas to 35-55°C for condensation dehydration, preferably to 40-50°C for condensation dehydration; the water vapor concentration of the high CO flue gas after dehydration is 5-13%, preferably 7-12;

[0016] The denitration in step S2 is SCR denitration;

[0017] The heating in step S2 is to heat the high CO flue gas to 160-200° C., preferably 160-180° C.;

[0018] The decarbonization in step S2 is to remove CO by catalytic oxidation of CO; the catalyst used for the catalytic oxidation of CO is a metal catalyst containing any one or more of Cu, Mn, Co, Ce, Pt, Pd, and Au;

[0019] The desulfurization in step S2 is activated carbon adsorption desulfurization, including the synergistic removal of HCl and VOCs; desulfurization is to remove SO in high CO flue gas. 2 The concentration is reduced to 0-10 mg / m 3 , preferably 0 to 5 mg / m 3 ; Reduce the VOCs concentration in high CO flue gas to 0-15 mg / m 3 , preferably 0 to 10 mg / m 3 ; Reduce the HCl concentration in high CO flue gas to 0-3 mg / m 3 , preferably 0 to 2 mg / m 3 .

[0020] Furthermore, the method further comprises: S4, using the heat of the low-CO flue gas to increase the temperature of the high-CO flue gas after desulfurization in step S2.

[0021] Furthermore, the activated carbon circulation amount W in the desulfurization process of step S2 is 1 for:

[0022]

[0023] Where W1 is the activated carbon circulation amount in the desulfurization process, t / h; Q 1 is the flue gas volume of high CO flue gas, m 3 / h; SO in high CO flue gas 2 Initial concentration, mg / m 3 ; C 1HCl is the initial concentration of HCl in high CO flue gas, mg / m 3 ; C 1VOCs is the initial concentration of VOCs in high CO flue gas, mg / m 3 ; SO after desulfurization of high CO flue gas 2 Concentration, mg / m 3 ; C 1outHCl is the HCl concentration after high CO flue gas desulfurization, mg / m 3 ; C 1outVOCs is the VOCs concentration after high CO flue gas desulfurization, mg / m 3 ; a is the activated carbon to SO 2 Adsorption capacity, mg / g; a HCl is the adsorption capacity of activated carbon for HCl, mg / g; a VOCs is the adsorption capacity of activated carbon for VOCs, mg / g; Preferably <5 mg / m 3 ; C 1outHCl <3mg / m 3 , preferably 2 mg / m 3 ; C 1outVOCs <15mg / m 3 , preferably <10 mg / m 3 .

[0024] Furthermore, the denitration in step S2 and the denitration in step S3 are respectively denitration of high CO flue gas after decarbonization and low CO flue gas after desulfurization;

[0025] During the decarbonization process, the temperature of high CO flue gas changes as follows:

[0026]

[0027] In the formula, ΔT 1 is the temperature change of high CO flue gas during decarbonization, ℃; C 1CO is the CO concentration in high CO flue gas, %; C out1CO is the CO concentration in high CO flue gas after decarbonization, %, C out1CO The value of M is 0 to 0.05%, preferably 0 to 0.03%; WCOis the molar mass of CO, g / mol; λ is the heat of combustion of CO, kJ / g; b is the molar volume, m 3 / mol; ρ is the smoke density, kg / m 3 ;c 1 is the specific heat capacity of high CO flue gas, kJ / (kg〃℃);

[0028] In addition, before the decarbonization step, when only the low CO flue gas is heat exchanged with the high CO flue gas after desulfurization, the temperature of the high CO flue gas after heat exchange is:

[0029]

[0030] Where, T 1 is the temperature of high CO flue gas after desulfurization, ℃; T 2 is the temperature of low CO flue gas before heat exchange, ℃; t 1 is the temperature of high CO flue gas after heat exchange, ℃; where T 1 The value of T is 40~50℃; 2 The value of c is 280~320℃; 2 is the specific heat capacity of low CO flue gas, kJ / (kg〃℃);

[0031] According to equation 2 and equation 3, assuming the denitration temperature is T 3 When t 1 +ΔT 1 ≥T 3 When t 1 +ΔT 1 <T 3 When the heat is supplemented, T 3 The value range is 270~290℃, preferably 278~285℃.

[0032] Furthermore, the denitration in step S2 and the denitration in step S3 are to denitrate by mixing the high CO flue gas after decarbonization with the low CO flue gas after desulfurization;

[0033] CO oxidation in high CO flue gas can increase the temperature of the mixed gas by ΔT 2 :

[0034]

[0035] In the formula, Q 1 is the flue gas volume of high CO flue gas, m 3 / h;Q 2 is the flue gas volume of low CO flue gas, m 3 / h; C 1CO is the CO concentration in high CO flue gas, %; C out1CO is the CO concentration in high CO flue gas after decarbonization, %; C out1COThe value of M is 0 to 0.05%, preferably 0 to 0.03%; WCO is the molar mass of CO, g / mol; λ is the heat of combustion of CO, kJ / g; b is the molar volume, m 3 / mol; ρ is the smoke density, kg / m 3 ; c is the specific heat capacity of the mixed gas, kJ / (kg〃℃);

[0036] After the high CO flue gas after decarbonization is mixed with the low CO flue gas after desulfurization, the temperature of the mixed gas is:

[0037]

[0038] Where, T 1 is the temperature of high CO flue gas after desulfurization, ℃; T 2 is the temperature of low CO flue gas before heat exchange, ℃; t 1 is the temperature of high CO flue gas after heat exchange, ℃; t 2 is the temperature of low CO flue gas after heat exchange; Q 1 is the flue gas volume of high CO flue gas, m 3 / h;Q 2 is the flue gas volume of low CO flue gas, m 3 / h; where T 1 The value of T is 40~50℃; 2 The value of t is 280~320℃; 2 The value is 160~180℃;

[0039] According to equations 4, 5 and 6, assuming the denitrification temperature is T 3 When t 3 +ΔT 1 ≥T 3 When t 3 +ΔT 1 <T 3 When the heat is supplemented, T 3 The value range is 270~290℃, preferably 278~285℃.

[0040] Furthermore, the supplementary heat is provided by a heater and / or the high CO flue gas after denitration in step S2 is used for supplementary heat.

[0041] Furthermore, the activated carbon circulation amount in the desulfurization process in step S3 is W 2 for:

[0042]

[0043] Where W 2 is the activated carbon circulation amount in the desulfurization process, t / h; Q 2is the flue gas volume of low CO flue gas, m 3 / h; For SO in low CO flue gas 2 Initial concentration, mg / m 3 ; SO after low CO flue gas desulfurization 2 Concentration, mg / m 3 ; a is the activated carbon to SO 2 Adsorption capacity, mg / g.

[0044] The beneficial effect of the method for improving the CO removal rate of sintering flue gas of the present invention is as follows: according to the release law of each pollutant in the sintering process, the sintering flue gas is divided into high CO flue gas and low CO flue gas, and they are treated separately, so that the flue gas volume in the CO removal process is reduced by half, the treatment efficiency is improved, and the purpose of CO emission reduction is achieved at the same time. In addition, it can ensure that SO in the flue gas is reduced to 0.05% before decarbonization of high CO flue gas. 2 , HCl and VOCs concentrations all reach extremely low values, reducing the impact on the activity of the CO catalyst and extending the service life of the catalyst. BRIEF DESCRIPTION OF THE DRAWINGS

[0045] The present invention is further described in detail below with reference to the accompanying drawings and specific implementation methods.

[0046] Figure 1 A schematic diagram of the process of removing CO from sintering flue gas provided by the present invention;

[0047] Figure 2 This is a diagram showing the release patterns of various pollutants during the sintering process. DETAILED DESCRIPTION

[0048] The present invention will be described in detail below with reference to the accompanying drawings and in combination with embodiments. It should be noted that the embodiments and features in the embodiments of the present application can be combined with each other without conflict.

[0049] According to one aspect of the present invention, there is provided a method for improving the CO removal rate of sintering flue gas, comprising the following steps:

[0050] S1. Divide the sintering bellows flue gas into high CO flue gas and low CO flue gas according to the different CO concentrations in the flue gas of each bellows of the sintering machine;

[0051] S2, remove dust, water, desulfurize, decarbonize and denitrify the high CO flue gas and then discharge it through the chimney;

[0052] S3. The low CO flue gas is discharged through the chimney after dust removal, desulfurization and denitrification.

[0053] Preferably, the high CO flue gas refers to sintering bellows flue gas with a CO concentration of 0.5-2 vol.%, preferably sintering bellows flue gas with a CO concentration of 1-1.8 vol.%.

[0054] Preferably, the SO of the high CO flue gas 2 Concentration less than 250 mg / m 3 、VOCs concentration is greater than 30mg / m 3 And the HCl concentration is less than 5 mg / m 3 More preferably, SO 2 Concentration less than 230 mg / m 3 , VOCs concentration is greater than 40mg / m 3 And the HCl concentration is less than 4 mg / m 3 ; Except for high CO flue gas, all other sintering bellows flue gases are low CO flue gases.

[0055] Preferably, the sintering bellows flue gas is divided in the following manner: the bellows under the sintering machine are numbered in sequence as 1, 2, 3, ..., x, ..., y; wherein the SO in the flue gas from bellows No. 1 to No. x is 2 The concentration was less than 250 mg / m 3 (Preferably less than 230 mg / m 3 ) and the HCl concentration is less than 5 mg / m 3 (Preferably less than 4 mg / m 3 ); The flue gases from the 1st to the xth bellows are collected to form high CO flue gases, and the flue gases from the (x+1)th to the yth bellows are collected to form low CO flue gases. Further preferably, a is set to be an integer greater than or equal to 1 and less than x, and when the average CO concentration of the flue gases from the 1st to the ath bellows is not higher than the average CO concentration of the flue gases from the (x+1)th to the yth bellows, the flue gases from the (a+1)th to the xth bellows are collected to form high CO flue gases, and the flue gases from the 1st to the ath bellows and the (x+1)th to the yth bellows are collected to form low CO flue gases.

[0056] Preferably, the dehydration in step S2 is to cool the high CO flue gas to 35-55°C for condensation dehydration, preferably to 40-50°C for condensation dehydration; the water vapor concentration of the high CO flue gas after dehydration is 5-13%, preferably 7-12;

[0057] The denitration in step S2 is SCR denitration;

[0058] The heating in step S2 is to heat the high CO flue gas to 160-200° C., preferably 160-180° C.;

[0059] The decarbonization in step S2 is to remove CO by catalytic oxidation of CO; the catalyst used for the catalytic oxidation of CO is a metal catalyst containing any one or more of Cu, Mn, Co, Ce, Pt, Pd, and Au;

[0060] The desulfurization in step S2 is activated carbon adsorption desulfurization, including the synergistic removal of HCl and VOCs; desulfurization is to remove SO in high CO flue gas. 2 The concentration is reduced to 0-10 mg / m 3 , preferably 0 to 5 mg / m 3 ; Reduce the VOCs concentration in high CO flue gas to 0-15 mg / m 3 , preferably 0 to 10 mg / m 3 ; Reduce the HCl concentration in high CO flue gas to 0-3 mg / m 3 , preferably 0 to 2 mg / m 3 .

[0061] Preferably, the method further comprises: S4, using the heat of the low-CO flue gas to increase the temperature of the high-CO flue gas after desulfurization in step S2.

[0062] Preferably, the activated carbon circulation amount W in the desulfurization process of step S2 is 1 for:

[0063]

[0064]

[0065] Where W 1 is the activated carbon circulation amount in the desulfurization process, t / h; Q 1 is the flue gas volume of high CO flue gas, m 3 / h; SO in high CO flue gas 2 Initial concentration, mg / m 3 ; C 1HCl is the initial concentration of HCl in high CO flue gas, mg / m 3 ; C 1VOCs is the initial concentration of VOCs in high CO flue gas, mg / m 3 ; SO after desulfurization of high CO flue gas 2 Concentration, mg / m 3 ; C 1outHCl is the HCl concentration after high CO flue gas desulfurization, mg / m 3 ; C 1outVOCs is the VOCs concentration after high CO flue gas desulfurization, mg / m 3 ; a is the activated carbon to SO 2 Adsorption capacity, mg / g; aHCl is the adsorption capacity of activated carbon for HCl, mg / g; a VOCs is the adsorption capacity of activated carbon for VOCs, mg / g; Preferably <5 mg / m 3 ; C 1outHCl <3mg / m 3 , preferably 2 mg / m 3 ; C 1outVOCs <15mg / m 3 , preferably <10 mg / m 3 .

[0066] Preferably, the denitration in step S2 and the denitration in step S3 are respectively denitration of high CO flue gas after decarbonization and low CO flue gas after desulfurization;

[0067] During the decarbonization process, the temperature of high CO flue gas changes as follows:

[0068]

[0069] In the formula, ΔT 1 is the temperature change of high CO flue gas during decarbonization, ℃; C 1CO is the CO concentration in high CO flue gas, %; C out1CO is the CO concentration in high CO flue gas after decarbonization, %, C out1CO The value of M is 0 to 0.05%, preferably 0 to 0.03%; WCO is the molar mass of CO, g / mol; λ is the heat of combustion of CO, kJ / g; b is the molar volume, m 3 / mol; ρ is the smoke density, kg / m 3 ;c 1 is the specific heat capacity of high CO flue gas, kJ / (kg〃℃);

[0070] In addition, before the decarbonization step, when only the low CO flue gas is heat exchanged with the high CO flue gas after desulfurization, the temperature of the high CO flue gas after heat exchange is:

[0071]

[0072] Where, T 1 is the temperature of high CO flue gas after desulfurization, ℃; T 2 is the temperature of low CO flue gas before heat exchange, ℃; t 1 is the temperature of high CO flue gas after heat exchange, ℃; where T 1 The value of T is 40~50℃; 2 The value of c is 280~320℃; 2 is the specific heat capacity of low CO flue gas, kJ / (kg〃℃);

[0073] According to equation 2 and equation 3, assuming the denitration temperature is T 3 When t 1 +ΔT 1 ≥T 3 When t 1 +ΔT 1 <T 3 When the heat is supplemented, T 3 The value range is 270~290℃, preferably 278~285℃.

[0074] Preferably, the denitration in step S2 and the denitration in step S3 are performed by mixing the high CO flue gas after decarbonization and the low CO flue gas after desulfurization for denitration;

[0075] CO oxidation in high CO flue gas can increase the temperature of the mixed gas by ΔT 2 :

[0076]

[0077] In the formula, Q 1 is the flue gas volume of high CO flue gas, m 3 / h;Q 2 is the flue gas volume of low CO flue gas, m 3 / h; C 1CO is the CO concentration in high CO flue gas, %; C out1CO is the CO concentration in high CO flue gas after decarbonization, %; C out1CO The value of M is 0 to 0.05%, preferably 0 to 0.03%; WCO is the molar mass of CO, g / mol; λ is the heat of combustion of CO, kJ / g; b is the molar volume, m 3 / mol; ρ is the smoke density, kg / m 3 ; c is the specific heat capacity of the mixed gas, kJ / (kg〃℃);

[0078] After the high CO flue gas after decarbonization is mixed with the low CO flue gas after desulfurization, the temperature of the mixed gas is:

[0079]

[0080]

[0081] Where, T 1 is the temperature of high CO flue gas after desulfurization, ℃; T 2 is the temperature of low CO flue gas before heat exchange, ℃; t 1 is the temperature of high CO flue gas after heat exchange, ℃; t 2 is the temperature of low CO flue gas after heat exchange; Q 1 is the flue gas volume of high CO flue gas, m3 / h;Q 2 is the flue gas volume of low CO flue gas, m 3 / h; where T 1 The value of T is 40~50℃; 2 The value of t is 280~320℃; 2 The value is 160~180℃;

[0082] According to equations 4, 5 and 6, assuming the denitrification temperature is T 3 When t 3 +ΔT 1 ≥T 3 When t 3 +ΔT 1 <T 3 When the heat is supplemented, T 3 The value range is 270~290℃, preferably 278~285℃.

[0083] Preferably, the supplementary heat is provided by a heater and / or the high CO flue gas after denitration in step S2 is used for supplementary heat.

[0084] Preferably, the activated carbon circulation amount in the desulfurization process in step S3 is W 2 for:

[0085]

[0086] Where W 2 is the activated carbon circulation amount in the desulfurization process, t / h; Q 2 is the flue gas volume of low CO flue gas, m 3 / h; For SO in low CO flue gas 2 Initial concentration, mg / m 3 ; SO after low CO flue gas desulfurization 2 Concentration, mg / m 3 ; a is the activated carbon to SO 2 Adsorption capacity, mg / g.

[0087] In the present invention, the release patterns of various pollutants during the sintering process are studied, such as Figure 2 There are multiple bellows under the sintering trolley to extract the flue gas generated by sintering. Each bellows corresponds to a different material layer state, and the flue gas composition is quite different. 2 O concentration is high, starting from the end of the first stage (such as the flue gas of bellows No. 19), H 2The concentration of O gradually decreases. On the contrary, the concentration of HCl in the first section of flue gas is low, and from the end of the first section, the concentration of HCl slowly increases. 2 The concentrations of the flue gas increased first and then decreased. The CO concentration in the middle flue gas (such as the flue gas from bellows 10-18) was the highest, and the SO concentration in the middle and rear flue gas (such as the flue gas from bellows 19-21) was the highest. 2 In addition, the concentration changes of VOCs are consistent with that of CO.

[0088] In the present invention, if the flue gas from the above-mentioned bellows No. 1-18 is used as high CO flue gas, and the flue gas from the bellows No. 19-29 is used as low CO flue gas, it can be calculated according to the flue gas volume of each bellows that the CO concentration in the high CO flue gas is as high as 1-1.5%, while the CO concentration in the low CO flue gas is only 0.1-0.3%. Therefore, only the high CO flue gas can be decarbonized, and the flue gas volume in the CO removal process can be reduced by half, thereby improving the treatment efficiency and achieving the purpose of CO emission reduction.

[0089] In the present invention, according to the above research on the pollutant release law during the sintering process, the sintering flue gas is divided into high CO flue gas and low CO flue gas, and the two flue gases are treated separately. 2 O, SO 2 , VOCs and HCl. Before CO removal, these pollutants in high CO flue gas need to be removed or reduced. The high CO flue gas is cooled, dehydrated and desulfurized before being sent to the CO removal process. The desulfurization is done by using activated carbon desulfurization. At a low temperature of 40 to 50 ° C, the activated carbon process is used to remove SO 2 The removal efficiency of CO, HCl and VOCs can reach more than 98%. Compared with the unified treatment of all flue gases, the SO 2 The concentration of HCl is lower than that of HCl, which makes it easy to remove it to an ultra-low concentration, which is beneficial to the catalytic oxidation of CO.

[0090] In the present invention, conventional treatment is performed on the low CO flue gas, and the low CO flue gas is discharged after being desulfurized and denitrified.

[0091] In the present invention, the classification of high CO flue gas and low CO flue gas is further refined. Since the CO concentration in some front wind boxes (i.e., wind boxes 1 to a) is low, the flue gas therein is mixed with the flue gas in wind boxes x+1 to y as low CO flue gas, and the flue gas in the remaining wind boxes is used as high CO flue gas. The amount of flue gas in the CO removal process is further reduced.

[0092] In the present invention, after the high CO flue gas is desulfurized, the presence of various trace impurities in the flue gas will increase the activation temperature of CO oxidation, so before the flue gas is decarbonized or denitrified, the temperature of the high CO flue gas needs to be increased. At this time, the heat of the low CO flue gas can be fully utilized to exchange heat with the high CO flue gas after desulfurization.

[0093] In the present invention, a method for calculating the high CO flue gas temperature and the activated carbon circulation amount is further proposed. According to the temperature and flow rate of the high CO flue gas and the low CO flue gas, the temperature of the high CO flue gas (or mixed flue gas) after heat exchange with the low CO flue gas and the temperature increased during the CO catalytic oxidation process are calculated to accurately control the heating of the high CO flue gas (or mixed flue gas). At the same time, according to the pollutant content in the flue gas, the activated carbon circulation amount in different flue gas desulfurization processes is accurately controlled.

[0094] In the present invention, the sintering flue gas with high CO concentration and low concentration of other pollutants is processed in stages, so as to ensure that SO in the flue gas is reduced before decarburization of the high CO flue gas. 2 , HCl and VOCs concentrations all reach extremely low values, reducing the impact on the activity of the CO catalyst and extending the service life of the catalyst.

[0095] In the present invention, the denitrification is to use SCR reaction to remove NOx in the flue gas to 50mg / m 3 the following.

[0096] Example 1

[0097] A method for improving the CO removal rate of sintering flue gas, removing multiple pollutants from the sintering flue gas:

[0098] 1. Detect CO and SO in the No. 1 to No. 29 wind boxes under the sintering machine 2 , HCl concentration, according to the SO2 of the flue gas of No. 1 to No. x bellows in the sintering bellows <250mg / m 3 And HCl < 5 mg / m 3 The position of x is determined to be 18 according to the requirement that the average CO concentration of the flue gas from bellows 1 to a should not be higher than the average CO concentration of the flue gas from bellows x+1 to y. The flue gas extracted from the bellows of the sintering trolley is divided into the first section with high CO and low SO 2 , HCl high CO flue gas and second stage high SO 2 , HCl low CO flue gas. The measured flow rate of high CO flue gas is 405142m 3 / h, the flow rate of low CO flue gas is 577982m 3 / h.

[0099] 2. After the high CO flue gas is dusted, it is introduced into the condensation dehumidifier to reduce the temperature of the high CO flue gas to 45°C, and then it is sent to the desulfurization tower for desulfurization, and the following is obtained:

[0100] W 1

[0101] In the formula, Q 1 is the flue gas volume of high CO flue gas, Q 1 =405142m 3 / h; SO in high CO flue gas 2 The initial concentration of C 1HCl is the initial concentration of HCl in high CO flue gas, C 1HCl =5mg / m 3 ; C 1VOCs is the initial concentration of VOCs in high CO flue gas, C 1VOCs =47mg / m 3 ; SO after desulfurization of high CO flue gas 2 concentration, C 1outHCl is the HCl concentration after high CO flue gas desulfurization, C 1outHCl =1mg / m 3 ; C 1outVOCs is the VOCs concentration after high CO flue gas desulfurization, C 1outVOCs =5mg / m 3 ; a is the activated carbon to SO 2 Adsorption capacity, a = 150 mg / g; a HCl is the adsorption capacity of activated carbon for HCl, a HCl =120mg / g; a VOCs is the adsorption capacity of activated carbon for VOCs, a VOCs =200mg / g. According to the above data, W 1 =0.7t / h.

[0102] After desulfurization, high CO flue gas exchanges heat with low CO flue gas to increase temperature:

[0103]

[0104] In the formula, Q 1 is the flue gas volume of high CO flue gas, Q 1 =405142m 3 / h;Q 2 is the flue gas volume of low CO flue gas, Q 2 =577982m 3 / h; T 1is the temperature of high CO flue gas after desulfurization, T 1 =46℃; T 2 is the temperature of low CO flue gas before heat exchange, T 2 =302℃; t 1 is the temperature of high CO flue gas after heat exchange, t 1 =199℃; t 2 is the temperature of low CO flue gas after heat exchange, t 2 =199℃;c 2 is the specific heat capacity of low CO flue gas, c 2 =1.122 kJ / (kg〃℃); c 1 is the specific heat capacity of high CO flue gas, c 1 =1.068kJ / (kg〃℃).

[0105] The hot high CO flue gas enters the decarbonization process and heats up during the decarbonization process.

[0106]

[0107] In the formula, C 1CO is the CO concentration in high CO flue gas, C 1CO =1.07%; C out1CO is the CO concentration in high CO flue gas after decarbonization, C out1CO =0.02%; M WCO is the molar mass of CO, M WCO =28g / mol; λ is the heat of combustion of CO, λ=10.1kJ / g; b is the molar volume, b=0.0224m3 / mol; ρ is the flue gas density, ρ=0.748kg / m 3 ; ΔT 1 is the temperature change of high CO flue gas during decarbonization, ΔT 1 =166℃;

[0108] After decarbonization is completed, the temperature of high CO flue gas is t 1 +ΔT 1 =365℃, the temperature required for denitrification is T 3 =280℃,t 1 +ΔT 1 >T 3 , directly pass the high CO flue gas into the denitrification process (NOx concentration 600mg / m 3 ), reducing NOx concentration to 50mg / m 3 the following.

[0109] 3. After the low CO flue gas is dust-removed and heat-exchanged with the high CO flue gas, it enters the desulfurization process through the induced draft fan. The activated carbon circulation amount in the desulfurization process is:

[0110]

[0111] In the formula, Q 2 is the flue gas volume of low CO flue gas, Q 2 =577982m 3 / h; For SO in low CO flue gas 2 The initial concentration of SO after low CO flue gas desulfurization 2 concentration, a is the activated carbon to SO 2 Adsorption capacity, a = 150 mg / g; W 2 is the activated carbon circulation amount in the desulfurization process, W 2 =6.6t / h.

[0112] Then the low CO flue gas (NOx content is 40mg / m 3 ) and the high CO flue gas after decarbonization and denitrification (the NOx concentration after mixing is less than 50mg / m 3 ). After the above treatment, the flue gas meets the emission standard, and the CO content in the flue gas is 0.08%.

[0113] Example 2

[0114] A method for improving the CO removal rate of sintering flue gas, removing multiple pollutants from the sintering flue gas:

[0115] 1. Detect CO and SO in the No. 1 to No. 29 wind boxes under the sintering machine 2 , HCl concentration, according to the SO 2 <250 mg / m 3 And HCl < 5 mg / m 3 The position of x is determined to be 19 according to the requirement that the average CO concentration of the flue gas from bellows 1 to a should not be higher than the average CO concentration of the flue gas from bellows x+1 to y. The flue gas extracted from the bellows of the sintering trolley is divided into the first section with high CO and low SO 2 , HCl high CO flue gas and second stage high SO 2 , HCl low CO flue gas. The measured flow rate of high CO flue gas is 430254m 3 / h, the flow rate of low CO flue gas is 552870m 3 / h.

[0116] 2. After the high CO flue gas is dusted, it is introduced into the condensation dehumidifier to reduce the temperature of the high CO flue gas to 45°C, and then it is sent to the desulfurization tower for desulfurization, and the following is obtained:

[0117] W1

[0118] In the formula, Q 1 is the flue gas volume of high CO flue gas, Q 1 =430254m 3 / h; SO in high CO flue gas 2 The initial concentration of C 1HCl is the initial concentration of HCl in high CO flue gas, C 1HCl =5mg / m 3 ; C 1VOCs is the initial concentration of VOCs in high CO flue gas, C 1VOCs =47mg / m 3 ; SO after desulfurization of high CO flue gas 2 concentration, C 1outHCl is the HCl concentration after high CO flue gas desulfurization, C 1outHCl =1mg / m 3 ; C 1outVOCs is the VOCs concentration after high CO flue gas desulfurization, C 1outVOCs =5mg / m 3 ; a is the activated carbon to SO 2 Adsorption capacity, a = 150 mg / g; a HCl is the adsorption capacity of activated carbon for HCl, a HCl =120mg / g; a VOCs is the adsorption capacity of activated carbon for VOCs, a VOCs =200mg / g. According to the above data, W 1 =0.8t / h.

[0119] After desulfurization, high CO flue gas exchanges heat with low CO flue gas to increase temperature:

[0120]

[0121] In the formula, Q 1 is the flue gas volume of high CO flue gas, Q 1 =430254m 3 / h;Q 2 is the flue gas volume of low CO flue gas, Q 2 =552870m 3 / h; T 1 is the temperature of high CO flue gas after desulfurization, T 1 =48℃; T 2 is the temperature of low CO flue gas before heat exchange, T 2 =311℃; t 1is the temperature of high CO flue gas after heat exchange, t 1 =203℃; t 2 is the temperature of low CO flue gas after heat exchange, t 2 =204℃;c 2 is the specific heat capacity of low CO flue gas, c 2 =1.201 kJ / (kg〃℃); c 1 is the specific heat capacity of high CO flue gas, c 1 =1.053kJ / (kg〃℃).

[0122] After heat exchange, the high CO flue gas enters the decarbonization process. The CO oxidation in the high CO flue gas can increase the temperature of the two mixed gases by ΔT. 2 :

[0123]

[0124] In the formula, C 1CO is the CO concentration in high CO flue gas, C 1CO =1.18%; C out1CO is the CO concentration in high CO flue gas after decarbonization, C out1CO =0.02%;;M WCO is the molar mass of CO, M WCO =28g / mol; λ is the heat of combustion of CO, λ = 10.1kJ / g; b is the molar volume, b = 0.0224m 3 / mol; ρ is the smoke density, ρ = 0.748 kg / m 3 ; c is the specific heat capacity of the mixed gas, 1.097 kJ / (kg〃℃); ΔT 2 =78℃.

[0125] After the high CO flue gas after decarbonization is mixed with the low CO flue gas after desulfurization, the temperature of the mixed gas is:

[0126]

[0127] Where, t 1 is the temperature of high CO flue gas after heat exchange, t 1 =203℃; t 2 The temperature of low CO flue gas after heat exchange = 204℃.

[0128] After high CO flue gas is mixed with low CO flue gas, the temperature of the mixed flue gas is t 3 +ΔT 2 =281℃, the temperature required for denitrification is T 3 =280℃,t 1 +ΔT 1 >T 3There is no need to heat the mixed flue gas, and it can be directly passed into the denitrification process to reduce the NOx concentration to 50mg / m 3 The following is discharged after denitrification is completed.

[0129] 3. After the low CO flue gas is dust-removed and heat-exchanged with the high CO flue gas, it enters the desulfurization process through the induced draft fan. The activated carbon circulation amount in the desulfurization process is:

[0130]

[0131] In the formula, Q 2 is the flue gas volume of low CO flue gas, Q 2 =552870m 3 / h; For SO in low CO flue gas 2 The initial concentration of SO after low CO flue gas desulfurization 2 concentration, a is the activated carbon to SO 2 Adsorption capacity, a = 150 mg / g. W 2 is the activated carbon circulation amount in the desulfurization process, W 2 =6.2t / h.

[0132] Then the low CO flue gas is mixed with the high CO flue gas and denitrified to reduce the NOx concentration to 50 mg / m 3 After denitration is completed, the flue gas is mixed with the high CO flue gas after decarbonization and denitration and discharged. The flue gas after the above treatment meets the emission standard, and the CO content in the flue gas is 0.05%.

[0133] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by ordinary technicians in this technical field within the essential scope of the present invention also fall within the protection scope of the present invention.

Claims

1. A method for improving the CO removal rate of sintering flue gas, characterized in that: It includes the following steps: S1.分流烧结风箱烟气:分流烧结风箱烟气,根据烧结机各风箱烟气中CO浓度的不同,将烧结风箱烟气分流为高CO烟气和低CO烟气; S2.高CO烟气处理:将高CO烟气进行除尘、除水、脱硫、脱碳及脱硝后经烟囱排放; S3.低CO烟气处理:将低CO烟气进行除尘、脱硫及脱硝后经烟囱排放。 2. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The high-CO flue gas refers to the sintering wind box flue gas with a CO concentration of 0.5-2 vol.%.

3. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The SO2 concentration of the high CO flue gas is less than 250 mg / m 3 , VOCs concentration is greater than 30mg / m 3 And the HCl concentration is less than 5 mg / m 3 ; Except for high CO flue gas, all other sintering bellows flue gases are low CO flue gases.

4. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The diversion method of the sintering bellows flue gas is as follows: the bellows under the sintering machine are numbered in sequence, with the serial numbers being 1, 2, 3, ..., x, ..., y; wherein the SO2 concentration in the flue gas from bellows No. 1 to No. x is less than 250 mg / m 3 And the HCl concentration is less than 5 mg / m 3 ; The flue gases from bellows No. 1 to No. x are collected to form high CO flue gas, and the flue gases from bellows No. (x+1) to No. y are collected to form low CO flue gas.

5. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: In step S2, the water removal is to cool the high-CO flue gas to 35-55 °C for condensation and water removal; the water vapor concentration of the high-CO flue gas after water removal is 5-13%; The denitrification in step S2 is SCR denitrification; The temperature increase in step S2 is to increase the temperature of the high-CO flue gas to 160-200 °C; The decarbonization in step S2 is to remove CO by catalytic oxidation of CO; the catalyst used for the catalytic oxidation of CO is a metal catalyst containing any one or more of Cu, Mn, Co, Ce, Pt, Pd, and Au; The desulfurization in step S2 is activated carbon adsorption desulfurization, including the synergistic removal of HCl and VOCs; the desulfurization is to reduce the SO2 concentration in the high CO flue gas to 0-10 mg / m 3 ; Reduce the VOCs concentration in high CO flue gas to 0-15 mg / m 3 ; Reduce the HCl concentration in high CO flue gas to 0-3 mg / m 3 .

6. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The method further includes: S4.利用低CO烟气热量:将低CO烟气的热量用于步骤S2中高CO烟气脱硫后的升温。 7. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The activated carbon circulation amount W1 in the desulfurization process of step S2 is: Where W1 is the activated carbon circulation amount in the desulfurization process, t / h; Q1 is the flue gas volume of high CO flue gas, m 3 / h; is the initial concentration of SO2 in high CO flue gas, mg / m 3 ; C 1HCl is the initial concentration of HCl in high CO flue gas, mg / m 3 ; C 1VOCs is the initial concentration of VOCs in high CO flue gas, mg / m 3 ; is the SO2 concentration after desulfurization of high CO flue gas, mg / m 3 ; C 1outHCl is the HCl concentration after high CO flue gas desulfurization, mg / m 3 ; C 1outVOCs is the VOCs concentration after high CO flue gas desulfurization, mg / m 3 ; a is the adsorption capacity of activated carbon for SO2, mg / g; a HCl is the adsorption capacity of activated carbon for HCl, mg / g; a VOCs is the adsorption capacity of activated carbon for VOCs, mg / g; where C 1outSO2 <10mg / m 3 ; C 1outHCl <3mg / m 3 ; C 1outVOCs <15mg / m 3 .

8. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The denitrification in step S2 and the denitrification in step S3 are respectively denitrifying the high-CO flue gas after decarbonization and the low-CO flue gas after desulfurization; During the decarbonization process, the temperature change of the high-CO flue gas is: Where ΔT1 is the temperature change of high CO flue gas during the decarbonization process, ℃; 1CO is the CO concentration in high CO flue gas, %; C out1CO is the CO concentration in high CO flue gas after decarbonization, %, C out1CO The value of M is 0~0.05%; WCO is the molar mass of CO, g / mol; λ is the heat of combustion of CO, kJ / g; b is the molar volume, m 3 / mol; ρ is the smoke density, kg / m 3 ; c1 is the specific heat capacity of high CO flue gas, kJ / (kg·℃); In addition, before the decarbonization step, when only the low-CO flue gas exchanges heat with the high-CO flue gas after desulfurization, the temperature of the high-CO flue gas after heat exchange is: In the formula, T1 is the temperature of the high-CO flue gas after desulfurization, °C; T2 is the temperature of the low-CO flue gas before heat exchange, °C; t1 is the temperature of the high-CO flue gas after heat exchange, °C; among them, the value of T1 is 40-50 °C; the value of T2 is 280-320 °C; c2 is the specific heat capacity of the low-CO flue gas, kJ / (kg·°C); According to formula 2 and formula 3, let the denitrification temperature be T3; when t1 + ΔT1 ≥ T3, no heat supplement is required; when t1 + ΔT1 < T3, heat supplement is required; among them, the value range of T3 is 270-290 °C.

9. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The denitrification in step S2 and the denitrification in step S3 are to mix and denitrify the high-CO flue gas after decarbonization and the low-CO flue gas after desulfurization; The oxidation of CO in the high-CO flue gas can increase the temperature of the mixed gas by ΔT2: Where Q1 is the flue gas volume of high CO flue gas, m 3 / h; Q2 is the flue gas volume of low CO flue gas, m 3 / h; C 1CO is the CO concentration in high CO flue gas, %; C out1CO is the CO concentration in high CO flue gas after decarbonization, %; C out1CO The value of M is 0~0.05%; WCO is the molar mass of CO, g / mol; λ is the heat of combustion of CO, kJ / g; b is the molar volume, m 3 / mol; ρ is the smoke density, kg / m 3 ; c is the specific heat capacity of the mixed gas, kJ / (kg·℃); After mixing the high-CO flue gas after decarbonization and the low-CO flue gas after desulfurization, the temperature of the mixed gas is: Where, T1 is the temperature of high CO flue gas after desulfurization, °C; T2 is the temperature of low CO flue gas before heat exchange, °C; t1 is the temperature of high CO flue gas after heat exchange, °C; t2 is the temperature of low CO flue gas after heat exchange; Q1 is the flue gas volume of high CO flue gas, m 3 / h; Q2 is the flue gas volume of low CO flue gas, m 3 / h; wherein, the value of T1 is 40~50℃; the value of T2 is 280~320℃; the value of t2 is 160~180℃; According to formula 4, formula 5 and formula 6, let the denitrification temperature be T3; when t3 + ΔT1 ≥ T3, no heat supplement is required; when t3 + ΔT1 < T3, heat supplement is required; among them, the value range of T3 is 270-290 °C.

10. The method for improving CO removal rate of sintering flue gas according to claim 1, characterized in that: The activated carbon circulation amount W2 in the desulfurization process of step S3 is: Where W2 is the activated carbon circulation amount in the desulfurization process, t / h; Q2 is the flue gas volume of low CO flue gas, m 3 / h; is the initial concentration of SO2 in low CO flue gas, mg / m 3 ; is the SO2 concentration after low CO flue gas desulfurization, mg / m 3 ; a is the adsorption capacity of activated carbon for SO2, mg / g.

Citation Information

Patent Citations

  • Carbon monoxide and nitrogen oxide co-processing system

    CN211753932U

Cited By

  • A control system and method for deCOing of sintering flue gas

    CN120274556B

  • Method for removing CO after flue gas desulfurization and before ammonia spraying and flue gas treatment system

    CN121731956A