Metal molding powder spraying process and device
Through surface treatment, fine polishing and spraying workpieces, metal flash plastic powder spraying on the rotating fixture, combined with high-temperature curing and airflow circulation, the problems of poor spraying uniformity and adhesion in traditional processes are solved, and the efficiency of stainless steel insulation containers is achieved , aesthetics and durability.
Patent Information
- Application Number
- CN202410974242.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-08
AI Technical Summary
During the traditional metal flash plastic powder spraying stainless steel insulation container, there are problems such as insufficient spray uniformity, large surface roughness, poor coating adhesion, and easy to produce leveling and sagging, which affects the aesthetics and usage performance of the product, resulting in high production costs and Market competitiveness is reduced.
Using surface treatment and fine polishing, it is installed on a rotatable fixture tool for full-mouth spraying of metal flash plastic powder, and is cured through high temperature, combined with airflow circulation and spray speed control, ensuring coating uniformity and adhesion, avoiding leveling and Slope.
It achieves uniformity and strong bonding power of the surface coating of the workpiece, has good corrosion resistance and durability, and has a unique metal flash effect, which reduces production costs and improves market competitiveness.
Smart Images

Figure CN118904682A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of stainless steel heat-insulating containers, and in particular to a metal plastic powder spraying process and a device. Background Art
[0002] With the rapid development of the industrial field, metal powder spraying technology plays an increasingly important role in the automotive, home appliance, construction and other industries. In the field of home appliances, metal flash powder spraying is widely used in the surface treatment of the shells of various home appliances such as refrigerators, washing machines, air conditioners, and televisions. Its unique metal flash effect not only gives the product a fashionable and high-end appearance, but also enhances the durability and corrosion resistance of the product.
[0003] However, in the actual process of spraying stainless steel insulation containers with metallic flash plastic powder, the traditional process faces the problems of insufficient spraying uniformity, large surface roughness, poor coating adhesion, poor coating uniformity, and easy leveling and sagging. These problems not only affect the aesthetics and performance of the product, but also lead to increased production costs and low production efficiency, thereby reducing market competitiveness. Summary of the invention
[0004] In view of this, the purpose of the present invention is to provide a metal plastic powder spraying process and device, which can make the surface coating of the sprayed workpiece uniform and the bonding force between the coating and the workpiece strong, so that it has good corrosion resistance and durability, and also has a unique metallic flash effect.
[0005] The present invention solves the above technical problems by the following technical means:
[0006] A metal plastic powder spraying process comprises the following steps:
[0007] S1. Surface treatment of the workpiece to be processed is performed, and the surface treated workpiece to be processed is dried;
[0008] S2. Install the dried workpiece to be processed on a rotatable fixture;
[0009] S3. The workpiece to be processed is transferred to the spraying area and sprayed with metal flash plastic powder;
[0010] S4. The sprayed workpiece is transferred to the curing area for high temperature curing;
[0011] S5. Cool and unload the solidified workpiece to obtain a workpiece sprayed with metallic glitter plastic powder.
[0012] According to the above-mentioned technical means, by first performing surface treatment on the workpiece, dirt and defects on the surface of the workpiece can be removed, corrosion resistance and wear resistance can be improved, and it is beneficial to improve the adhesion and uniformity of the paint, which is beneficial to the subsequent spraying. The surface-treated workpiece is then mounted on the fixture, and the workpiece and the fixture are then transferred to the spraying area for full spraying of metallic glitter plastic powder. The outer surface of the workpiece can be fully sprayed with metallic glitter plastic powder, and the problems of leveling, sagging and accumulation can be avoided during the spraying process. At the same time, the paint will not enter the interior of the workpiece, so that the surface coating of the workpiece after spraying is uniform and has strong bonding strength. Finally, through high-temperature curing, the workpiece surface has a unique metallic glitter effect.
[0013] Preferably, in the step S1, when the workpiece to be processed is subjected to surface treatment, electrolysis and surface polishing operations are performed in sequence.
[0014] More preferably, during the electrolytic operation, electrolytic polishing is performed using a phosphoric acid-based electrolyte.
[0015] Further preferably, during the surface fine polishing operation, fine polishing is performed by using one or more combinations of corundum, white corundum, brown corundum, ceramic particles, and stainless steel shots, and after fine polishing, the surface is cleaned and then dried.
[0016] According to the above technical means, through fine polishing operation, not only the corrosion resistance, wear resistance and anti-fingerprint properties of the workpiece can be improved, but also the adhesion between the workpiece surface and the coating can be improved, which is beneficial to subsequent spraying.
[0017] Further preferably, in the step S2, when the workpiece is mounted on the fixture, the workpiece is mounted on the fixture through threads and is tightly sealed against the fixture.
[0018] According to the above technical means, the workpiece can be fixedly installed on the fixture by threaded installation and sealing against the fixture, and the paint can be prevented from entering the interior of the workpiece during spraying.
[0019] Further preferably, before the workpiece to be processed is transported to the spraying area, a purging and impurity removal operation is performed.
[0020] Further preferably, when performing the purging and impurity removal operation, each workpiece is purged by providing an air pump and a connecting pipe, and each workpiece is fully purged by controlling the rotation of the fixture.
[0021] According to the above technical means, dust and other impurities attached during the installation process can be removed by blowing the workpiece to avoid affecting the subsequent spraying operation.
[0022] Preferably, in the step S3, when the metallic glitter plastic powder is fully sprayed, the workpiece is first heated, and then the metallic glitter plastic powder is fully sprayed.
[0023] Further preferably, when the workpiece is heated, the workpiece is heated to 100-120° C. by a high-temperature drying tunnel or external coil heating or natural gas heating, and external air flow circulation is performed on the workpiece.
[0024] Further preferably, when external air flow circulation is performed on the workpiece, the heating of the high-temperature drying tunnel is stopped first, and the gas expanded by heat in the workpiece is discharged so that high pressure is not generated in the workpiece, and then spraying is performed. After spraying, cold air with a gradually decreasing temperature is introduced to contact the outer surface of the workpiece. After the cold air continues for a period of time, the cold air introduction is closed, and the high-temperature drying tunnel is opened again. The air flow circulation process continues until the spraying is completed.
[0025] According to the above technical means, the hot air that expands due to heat is discharged first so that high pressure will not be generated in the workpiece, and then spraying is carried out, so as to avoid the product mouth from detaching from the fixture and vibration during the spraying process, and to avoid the spray powder from entering the workpiece and affecting the powder hanging on the spraying surface, thereby improving the surface finish of the workpiece; and then introducing cold air with a gradually decreasing temperature, which can maintain the heating temperature of the workpiece within a stable range, which is beneficial to avoid the workpiece temperature from being too high, causing deformation of the workpiece and stress concentration. At the same time, by continuously introducing cold air with a reduced temperature, the strength and toughness of the workpiece can also be improved.
[0026] By continuously circulating the hot air and then introducing the cold air with gradually lowered temperature, the metallic glitter plastic powder can be pre-solidified after spraying, which is beneficial to the combination of the metallic glitter plastic powder and the surface of the workpiece, and can also reduce the chance of leveling and sagging of the coating on the surface of the workpiece.
[0027] Further preferably, when the cold air with gradually decreasing temperature is introduced, the temperature is reduced from 25±2°C to 20±2°C, the air flow rate is 6-10m / s, the pressure is 1-100Pa, and the duration is 60-100s.
[0028] According to the above technical means, by introducing air that has been lowered from room temperature to low temperature and controlling the conditions of the introduction, the temperature in the high-temperature drying tunnel is maintained at 60±5°C, which also helps the pre-solidification of the coating.
[0029] Further preferably, when the metallic glitter plastic powder is sprayed full mouthful, the liquid metallic glitter plastic powder is sprayed over a large area from top to bottom and then from bottom to top through a spray gun.
[0030] According to the above technical means, spraying from top to bottom and then from bottom to top is beneficial to improving the uniformity of the coating and reducing the chance of leveling and sagging. Combined with pre-solidification, leveling and sagging can be avoided as much as possible, and paint accumulation can be avoided.
[0031] Further preferably, when spraying a large area, the spraying pressure of the spray gun is 0.3-0.8 MPa, the spraying speed is 8-15 m / min, the distance between the spray gun and the workpiece is 20-30 cm, and the speed of the spray gun movement is 200-500 mm / s.
[0032] Further preferably, in the process of spraying from top to bottom, the spraying speed is 10 to 15 m / min, and in the process of spraying from bottom to top, the spraying speed is 8 to 12 m / min.
[0033] According to the above technical means, by controlling the difference in spraying speed from top to bottom and from bottom to top, in conjunction with the rotating workpiece, it is beneficial to further improve the uniformity of the coating and reduce the leveling, sagging and accumulation phenomena.
[0034] Preferably, in the step S4, during high temperature curing, a high temperature oven is used for high temperature curing, the temperature in the high temperature oven is 190-220° C., and a plurality of sensors are arranged in the high temperature oven for dynamic feedback adjustment of the temperature of the high temperature oven and the transmission speed of the workpiece.
[0035] Further preferably, the sensor includes a temperature sensor and a speed sensor, and the temperature sensor and the speed sensor are arranged at multiple points in the high-temperature drying tunnel and are electrically connected to an external industrial control machine.
[0036] According to the above technical means, the temperature at different positions in the high-temperature drying oven is monitored in real time by temperature sensors, which is conducive to real-time feedback of the real-time heating temperature of the workpiece and the coating. The speed sensor is used to monitor the speed of the workpiece in the high-temperature drying oven in real time, so as to feedback the curing condition of the coating to avoid premature or over-maturity. It can also feedback the working condition of the high-temperature drying oven and provide timely feedback when a problem occurs.
[0037] During the high-temperature curing process, the heated and expanded gas in the workpiece is discharged so that high pressure will not be generated in the workpiece. It can also avoid the uneven thermal stress generated when the metallic flash plastic powder coating combines with the workpiece surface during the high-temperature curing process, which will lead to a decrease in adhesion.
[0038] Preferably, in the step S5, natural cooling is used to cool the material, and then the material is unloaded by a robot.
[0039] The present application also discloses a metal plastic powder spraying device, including a fixture and a spraying unit, the fixture including a fixed part, a rotating part and an exhaust part, the fixed part is assembled on the rotating part, a workpiece to be processed is sealed on the fixed part, the exhaust part is arranged in the fixed part and is connected to the workpiece to be processed, and the spraying unit is used to spray the workpiece to be processed.
[0040] According to the above-mentioned technical means, by setting the fixture tooling as a fixed part, a rotating part and an exhaust part, on the one hand, the workpiece to be processed can be sealed and assembled through the fixed part, which can prevent the paint from entering the workpiece when the metal flash plastic powder is sprayed all over the mouth, and then the fixed part and the workpiece to be processed are driven to rotate through the rotating part, which is beneficial to the subsequent spraying of the workpiece; on the other hand, through the exhaust part, the workpiece sprayed with metal flash plastic powder can be discharged during the spraying process of the workpiece, which is beneficial to the combination of metal flash plastic powder and the surface of the workpiece, and can also reduce the probability of leveling and sagging of the coating on the surface of the workpiece.
[0041] Preferably, the fixing portion comprises a connecting seat and a fixing seat, the connecting seat and the fixing seat are fixedly connected, an annular platform is fixedly provided on the connecting seat, an elastic gasket is provided on the annular platform, and an external thread is provided on the outer wall of the connecting seat.
[0042] According to the above-mentioned technical means, through the cooperation of the connecting seat, the elastic gasket and the external thread, the workpiece can be sealed and stably installed on the fixed part, thereby preventing the paint from entering the interior of the workpiece during spraying. When the workpiece is heated, it can also reduce the high pressure inside the workpiece caused by the expansion of the gas due to heat, thereby causing the loosening of the workpiece and the connecting seat, thereby avoiding affecting the processing effect of the contact surface between the workpiece and the connecting seat.
[0043] Preferably, the rotating part includes a transmission member and a driving member, one end of the transmission member is connected to the fixed part, and the other end is connected to the driving member.
[0044] According to the above technical means, when the driving member is working, it can drive the fixed part to rotate through the transmission member, thereby driving the workpiece to rotate, which is beneficial to the subsequent spraying of the workpiece.
[0045] Preferably, the exhaust portion includes a mounting plate and a control component, wherein the mounting plate is fixedly disposed in the fixing portion, a through hole is disposed on the mounting plate, and the control component is mounted at the through hole for controlling the opening and closing of the through hole and the discharge of airflow.
[0046] According to the above technical means, by setting a control part at the through hole to control the discharge of airflow between the upper part of the fixture and the workpiece, the heated gas inside the workpiece can be discharged when the workpiece is heated, which is beneficial to the adhesion of the metal flash plastic powder during the spraying process and the control of leveling and sagging, and can also prevent the powder coating from entering the interior of the workpiece.
[0047] Preferably, the fixture further comprises a magnetic attraction portion, which comprises a bracket and a plurality of magnets, the bracket is detachably mounted on the fixed portion, the plurality of magnets are respectively arranged on the peripheral side of the bracket, and the bracket is provided with a plurality of through slots.
[0048] According to the above technical means, through the setting of several magnets, the metal in the paint can be magnetically attracted during the process of spraying metallic glitter plastic powder on the surface of the workpiece. Different shapes can be formed by combining different combinations of multiple magnets, thereby forming a unique metallic glitter effect on the surface of the workpiece.
[0049] Preferably, the spraying unit includes a material storage tank, a pipe, a lifting member and a spray gun, one end of the pipe is connected to the material storage tank, and the other end is connected to the spray gun, and the spray gun is mounted on the lifting member for spraying the workpiece to be processed mounted on the fixture.
[0050] According to the above technical means, the metal flash plastic powder is loaded into a storage tank, and the metal flash plastic powder can be melted through the storage tank, or it can be melted first and then loaded into a storage tank with a heat-insulating effect, and then transported to the spray gun through a pipeline. The lifting part lifts and lowers the spray gun to spray the workpiece to be processed.
[0051] The present application adopting the above scheme has the following beneficial effects:
[0052] 1. In the present application, in the process of spraying the metal flash plastic powder on the workpiece to be processed, the workpiece to be processed is firstly subjected to surface treatment, which can remove dirt and defects on the surface of the workpiece, improve corrosion resistance and wear resistance, and help to improve the adhesion and uniformity of the spray paint, which is beneficial to the subsequent spraying, and then the workpiece after the surface treatment is mounted on the fixture, and then the workpiece and the fixture are transferred to the spraying area, and the metal flash plastic powder is sprayed all over the mouth, so that the outer surface of the workpiece can be sprayed with the metal flash plastic powder, and the problems of leveling, sagging and accumulation can be avoided during the spraying process. At the same time, the paint will not enter the interior of the workpiece, so that the surface coating of the workpiece after spraying is uniform, the bonding force is strong, and it also has a unique metal flash texture, and finally, through high temperature curing, the workpiece surface has a unique metal flash effect;
[0053] 2. When the workpiece is sprayed with metal flash plastic powder, an airflow circulation process is added during the heating and spraying process. During the airflow circulation process, the hot air that expands due to heat in the workpiece is first discharged so that high pressure will not be generated in the workpiece before spraying. This prevents the mouth of the product from detaching from the fixture and vibrating during the spraying process, and prevents the spray powder from entering the workpiece and affecting the powder hanging on the spraying surface, thereby improving the surface finish of the workpiece; then, by introducing cold air with a gradually decreasing temperature, the heating temperature of the workpiece can be maintained within a stable range, which can improve the strength, toughness and surface finish of the workpiece, and can also pre-solidify the metal flash plastic powder after spraying, which is beneficial to the combination of the metal flash plastic powder and the workpiece surface, and can also reduce the probability of leveling and sagging of the coating on the workpiece surface;
[0054] 3. During the spraying process, adopt a large-area spraying method from top to bottom and then from bottom to top, and control the difference in spraying speed between the two methods, which is conducive to further reducing the phenomenon of leveling, sagging and accumulation;
[0055] 4. In the present application, by improving the fixture, the fixture can meet the requirements of full mouth spraying of the workpiece during the metal flash plastic powder spraying process, preventing the paint from entering the workpiece, and the exhaust device can be arranged in the fixture to discharge the heated gas in the workpiece and improve the compactness of the fixture;
[0056] 5. By adding a magnetic suction part in the fixture, the spraying effect of the metal flash plastic powder can be adjusted, and a unique metal flash effect can be formed on the surface of the workpiece, making the appearance of the product better. BRIEF DESCRIPTION OF THE DRAWINGS
[0057] The present application may be further illustrated by non-limiting examples given in the accompanying drawings;
[0058] Figure 1 It is a schematic diagram of the structure of the fixture in the metal plastic powder spraying device in the embodiment of the application;
[0059] Figure 2 It is a partial cross-sectional structural schematic diagram of a metal plastic powder spraying device in an embodiment of the application;
[0060] Figure 3 It is a partial cross-sectional structural schematic diagram of a fixed part in a metal plastic powder spraying device in an embodiment of the application;
[0061] Figure 4 It is a schematic diagram of the structure of the elastic gasket in the metal plastic powder spraying device in the embodiment of the application;
[0062] Figure 5 It is a schematic diagram of the structure of the bracket in the metal plastic powder spraying device in the embodiment of the application;
[0063] Figure 6 It is a schematic diagram of the structure of the tension wheel in the metal plastic powder spraying device in the embodiment of the application;
[0064] Figure 7 It is a partial structural schematic diagram of a spraying unit in a metal plastic powder spraying device in an embodiment of the application;
[0065] Figure 8 This is a rendering of a stainless steel heat-insulating container after being processed by a metal plastic powder spraying process in an application embodiment;
[0066] Description of main symbols and components:
[0067] 10. fixing part; 11. fixing seat; 12. annular platform; 13. elastic washer; 131. annular protrusion; 14. connecting seat; 20. workpiece;
[0068] 30. Rotating part; 31. First gear; 32. Second gear; 33. Speed reduction motor; 34. Tensioning wheel;
[0069] 40. Exhaust part; 41. Mounting plate; 42. Through hole; 421. Bearing; 43. Joint; 44. Exhaust pipe; 45. Silicone one-way valve;
[0070] 50. Magnetic attraction portion; 51. Bracket; 52. Snap-fit slot; 53. Through slot;
[0071] 60. Spraying unit; 61. Power source; 62. Screw rod; 63. Base; 64. Mounting seat; 65. Spray gun; 651. Pipe; 66. Guide rod. DETAILED DESCRIPTION
[0072] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention:
[0073] like Figure 1-7 As shown, an embodiment of the present application discloses a metal plastic powder spraying device, including a fixture and a spraying unit 60. The fixture includes a fixed part 10, a rotating part 30 and an exhaust part 40. The fixed part 10 is assembled on the rotating part 30, and a workpiece 20 to be processed is sealed and assembled on the fixed part 10. The rotating part 30 rotates to drive the fixed part 10 and the workpiece 20 to be processed to rotate. The exhaust part 40 is arranged in the fixed part 10 and is connected to the workpiece 20 to be processed. It is used to discharge the heated and expanded gas in the workpiece 20 to be processed during the spraying process of the workpiece 20 to be processed. The spraying unit 60 is used to perform a full mouth spray on the workpiece 20 to be processed assembled on the fixed part 10.
[0074] In this embodiment, the workpiece 20 to be processed is a stainless steel heat-insulating container, and may also be a cylindrical stainless steel container, etc. Full mouth spraying means spraying the outer surface of the workpiece 20 and the cup mouth, thereby achieving full mouth spraying.
[0075] In some optional embodiments, such as Figure 1-4 As shown, the fixing part 10 includes a connecting seat 14 and a fixing seat 11. The connecting seat 14 and the fixing seat 11 are fixedly connected, and an annular platform 12 is fixedly arranged on the connecting seat 14, and an elastic gasket 13 is arranged on the annular platform 12, which is used to abut against the mouth of the workpiece 20. An external thread is arranged on the outer wall of the connecting seat 14, which is used to be threadedly connected with the mouth of the workpiece 20, so as to fix the workpiece 20 on the fixture.
[0076] In this embodiment, the connecting seat 14, the fixing seat 11 and the annular platform 12 are integrally formed, and the processing and forming is convenient. The elastic gasket 13 is made of high temperature resistant silicone material and can withstand 150-350°C. The connecting seat 14 has an annular groove, and the elastic gasket 13 is assembled in the annular groove. The inner ring of the elastic gasket 13 has an annular protrusion 131, and the annular protrusion 131 is partially located outside the annular groove, so that the workpiece 20 can be better sealed when it is threadedly connected to the connecting seat 14 and abuts against the elastic gasket 13.
[0077] In this embodiment, if Figure 1-2 and Figure 6 As shown, the rotating part 30 includes a transmission member and a driving member. One end of the transmission member is connected to the fixed part 10, and the other end is connected to the driving member. When the driving member is working, the fixed part 10 can be driven to rotate through the transmission member, thereby driving the workpiece 20 to rotate.
[0078] In this embodiment, when each fixture is driven individually, the transmission member may be the first gear 31, the driving member may be the reduction motor 33 and the second gear 32, the first gear 31 is connected to the fixing seat 11 via a spline, the second gear 32 is fixedly connected to the output shaft of the reduction motor 33, and then meshes with the first gear 31, so as to control each fixture to rotate individually and reserve installation space for the exhaust part 40. Of course, in actual operation, the transmission member may also be a geared disc, etc., and the driving member may be a reduction motor 33 and a chain, etc.
[0079] In another embodiment, when multiple fixtures are driven together, the transmission member may be a tension wheel 34, and the driving member may be a reduction motor 33 and a belt. By installing a tension wheel 34 on the fixed seat 11 of each fixture, and then tensioning each tension wheel 34 through a belt, and tensioning with the output shaft of the reduction motor 33, when the reduction motor 33 is working, it can drive multiple fixtures to move together. In actual situations, the transmission member may be a sprocket, and the driving member may be a reduction motor 33 and a chain. Appropriate transmission members and driving members may also be selected according to actual situations.
[0080] In this embodiment, not only the reduction motor 33 but also a servo motor, a permanent magnet synchronous motor, etc. can be selected.
[0081] In some optional embodiments, such as Figure 2-3 As shown, the exhaust part 40 includes a mounting plate 41 and a control member. The mounting plate 41 is fixedly arranged in the fixing part 10, and a through hole 42 is arranged on the mounting plate 41. The control member is installed at the through hole 42 to control the opening and closing of the through hole 42 and the exhaust of the airflow.
[0082] In this embodiment, the mounting plate 41 is fixedly connected to the fixing seat 11 by spot welding or bolts, and the control parts are the joint 43, the exhaust pipe 44 and the silicone check valve 45. The joint 43 is rotatably arranged at the through hole 42 through the bearing 421, so that when the fixing part 10 rotates, the joint 43 will not rotate. One end of the exhaust pipe 44 is fixedly connected to the joint 43, and the other end is connected to the outside. The silicone check valve 45 is fixedly arranged on the exhaust pipe 44 to control the opening and closing of the branch pipe, so as to discharge the gas expanded by heat in the workpiece. In order to monitor the temperature of the air inside the workpiece 20, a temperature sensor can also be arranged on the joint 43. The silicone check valve 45 and the temperature sensor are both connected to the external industrial control machine and are used to control the temperature transmitted by the temperature sensor and control the operation of the silicone check valve 45. Of course, the motor can also be connected to the industrial control machine and control the speed of the motor, thereby controlling the rotation speed of the workpiece 20 to be processed.
[0083] In this embodiment, the silicone one-way valve 45 is a high-temperature resistant silicone one-way valve, and other high-temperature resistant valves may be selected according to actual conditions.
[0084] In some optional embodiments, such as Figure 2 and Figure 5As shown, the fixture also includes a magnetic attraction portion 50. The magnetic attraction portion 50 includes a bracket 51 and a plurality of magnets. The bracket 51 is detachably mounted in the connecting seat 14 by means of threads. The plurality of magnets are arranged on the peripheral side of the bracket 51. By controlling the shapes of different magnet combinations, the metal powder in the metallic glitter plastic powder coating can be magnetically attracted, thereby controlling the shape of the metal powder on the coating, so that the coating can show a unique metallic glitter effect after curing. A plurality of through grooves 53 are provided on the bracket 51, which are staggered with the positions of the magnets, and are used to communicate with the inside of the workpiece 20 and the joint 43, which is conducive to the discharge of hot air.
[0085] In this embodiment, the magnet can be fixedly mounted on the bracket 51 by bolts or fasteners or by snapping the fastening groove 52, so as to adjust the position and combination of the magnets according to different customer needs, thereby forming different shapes on the coating. The shape of the magnet can be bar, block or arc, etc., which can be selected according to actual conditions.
[0086] In some optional embodiments, such as Figure 7 As shown, the spraying unit 60 includes a material storage tank, a pipe 651, a lifting member and a spray gun 65. One end of the pipe 651 is connected to the material storage tank, and the other end is connected to the spray gun 65, which is used to transport liquid metal flash plastic powder to the spray gun 65. The spray gun 65 is assembled on the lifting member, and is used to lift and spray the workpiece 20 to be processed assembled on the fixture.
[0087] In this embodiment, the storage tank can be one or more, and can be used to fill the same type of paint or corresponding matching paint. The storage tank can be a reaction tank with a high-temperature heating function, which can melt the metallic glitter plastic powder; it can also be a storage tank with a heat preservation function, which can keep the molten metallic glitter plastic powder warm to avoid solidification; it can also be just a medium storage tank, which stores the metallic glitter plastic powder in liquid or powder form. In this application, the metallic glitter plastic powder is metallic glitter paint, which can be Baoyoute Chameleon paint.
[0088] In this embodiment, the lifting member includes a power source 61, a screw rod 62, a base 63, a guide rod 66 and a mounting seat 64. The screw rod 62 is rotatably mounted between two bases 63, and a light rod portion at one end of the screw rod 62 passes through one of the bases 63. The power source 61 is in transmission connection with the light rod portion passing through the base 63 to control the rotation of the screw rod 62. The mounting seat 64 is screwed to the screw rod 62, and the guide rod 66 slides through the mounting seat 64. The spray gun 65 is fixedly mounted on the mounting seat 64 by bolts.
[0089] In this embodiment, when the power source 61 drives each screw rod 62 independently, that is, each spray gun 65 is raised and lowered separately, the output shaft of the power source 61 can be fixedly connected with the polished rod of each screw rod 62 passing through the base 63; when the power source 61 needs to drive multiple screw rods 62, that is, multiple spray guns 65 are raised and lowered synchronously, the output shaft of the power source 61 can be driven by the gear, belt or chain, and the polished rod part of each screw rod 62 passing through the base 63 in cooperation with the gear or tension wheel 34 or toothed disc. It can be understood that gears cooperate with gears, belts cooperate with tension wheels 34, and chains cooperate with toothed discs.
[0090] The present application also discloses a metal plastic powder spraying process, comprising the following steps:
[0091] S1. The workpiece 20 to be processed is subjected to surface treatment, and the surface treated workpiece 20 to be processed is dried;
[0092] S11. The workpiece 20 to be processed is first subjected to an electrolytic operation and then to a fine polishing operation;
[0093] S12. During the electrolytic operation, electrolytic polishing is performed using an electrolyte to remove oil stains, dirt and rust from the surface of the workpiece 20;
[0094] S13. During the fine polishing operation, the electrolyzed workpiece 20 is placed in a polishing machine, polished by stainless steel shot, and then cleaned and dried to obtain a finely polished workpiece 20;
[0095] S2. The dried workpiece 20 to be processed is installed on the connecting seat 14 of the fixture, and the mouth of the workpiece 20 to be processed is against the elastic gasket 13 to form a sealed installation;
[0096] S3. The workpiece 20 to be processed and the fixture are transferred to the spraying area, and the metal flash plastic powder is sprayed full;
[0097] S31. Before the workpiece 20 to be processed is transferred to the spraying area, a purge and impurity removal operation is performed;
[0098] S32. The workpiece 20 to be processed after being purged and cleaned is heated to 100-120°C by a high-temperature drying tunnel or an external coil or natural gas, and the workpiece 20 is circulated with an external airflow;
[0099] S33. During the heating process, the gas expanded by the heat in the workpiece 20 is discharged through the exhaust part 40, and then the high-temperature drying tunnel is stopped, and cold air with a gradually lowered temperature is introduced. After the cold air lasts for 65±2s, the cold air is turned off to maintain the temperature of the workpiece at 60±5°C, and then the high-temperature drying tunnel is opened to discharge the gas expanded by the heat in the workpiece. The airflow cycle process continues until the spraying is completed;
[0100] S34. When the workpiece 20 is heated to 100 to 120°C, the workpiece 20 is sprayed with a large area of metallic flash plastic powder liquid coating from top to bottom and from bottom to top by a spray gun 65;
[0101] S4. The sprayed workpiece 20 is transferred to the curing area for high temperature curing;
[0102] S41. The workpiece 20 sprayed with the metallic flash plastic powder liquid coating is transferred to a high-temperature oven for high-temperature curing. The temperature in the high-temperature oven is 190 to 220°C. A plurality of temperature sensors and speed sensors are arranged in the high-temperature oven for dynamic feedback adjustment of the high-temperature oven temperature and the transmission speed of the workpiece 20;
[0103] S5. The solidified workpiece 20 is naturally cooled to room temperature, and the workpiece 20 is unloaded to obtain a workpiece 20 sprayed with metallic glitter plastic powder.
[0104] In this embodiment, in step S12, electrolytic polishing is performed using a phosphoric acid electrolyte, the components of which are phosphoric acid, sulfuric acid, and a brightener, the mass percentage of phosphoric acid is 52±2%, the mass percentage of sulfuric acid is 45±2%, and the brightener is polyethylene glycol, the mass percentage is 3±0.5%, and during electrolysis, the current density is 8-15A / dm 2 , the voltage is 7~9V.
[0105] In this embodiment, in step S13, the particle size of the stainless steel shot is 0.1-1 mm, and then it is washed with soft water 2-3 times, and finally dried at 100±5° C. to obtain a finely polished workpiece 20.
[0106] In this embodiment, in step S31, when the purge and impurity removal operation is performed, an air pump is arranged outside, the output end of the air pump is connected to a connecting pipe, and a nozzle is installed on the connecting pipe at a position corresponding to each workpiece 20. Then, by controlling the rotation of the rotating part 30, the fixed part 10 and the workpiece 20 are driven to rotate, and each workpiece 20 is fully purged to remove dust and other impurities attached during the installation process.
[0107] In this embodiment, in step S33, when the temperature of the workpiece 20 in the high-temperature drying tunnel reaches 110±5°C, the silicone one-way valve 45 is opened, and the air in the workpiece 20 that is heated and expanded is discharged through the exhaust pipe 44. In the process of discharging the hot air, the paint is sprayed through the spray gun 65. After spraying one circle on the surface of the workpiece, the spray gun 65 is closed, the heat supply in the high-temperature drying tunnel is stopped, and cold air with a temperature reduced from 25±2°C to 20±2°C is introduced at the end of the drying tunnel. In this process, the inlet flow rate of the cold air is 6-10m / s, the pressure is 60±5Pa, and the duration is 65±2s. After the cold air is introduced, the high-temperature drying tunnel is opened again, and when the temperature of the workpiece 20 rises to 110±5°C, the hot air is discharged through the silicone one-way valve 45 again, and the above steps are repeated until the spraying is completed.
[0108] In this embodiment, in step S34, when spraying by the spray gun 65, the base paint is first sprayed on the workpiece 20, and then the metallic glitter plastic powder paint is sprayed, and the spray gun 65 is controlled by the power source 61 to rise and fall on the screw 62. The moving speed of the spray gun 65 is 300mm / s. During the spraying process of the spray gun 65 from top to bottom, the spraying speed is 13~15m / min, and during the spraying process from bottom to top, the spraying speed is 8~10m / min, so that the thickness of the entire coating is 4~6mm, the spraying pressure of the spray gun 65 is 0.5MPa, and the distance between the spray gun 65 and the workpiece 20 is 25cm.
[0109] In this embodiment, in step S41, after the product enters the high-temperature oven, the temperature in the high-temperature oven is monitored by a temperature sensor, and the temperature in the high-temperature oven is adjusted to 200±10°C by feedback control. The transmission speed of the conveyor belt in the high-temperature oven is monitored by a speed sensor to be 0.1~0.3m / s, and the curing time of the workpiece 20 in the high-temperature oven is controlled to be 12min.
[0110] Through the spraying process of this application, the sprayed products such as Figure 8 As shown in the attached Figure 8 It can be seen that the present application can prepare a stainless steel insulation container with a full-mouth spray effect, and the surface coating of the stainless steel insulation container is uniform, and the bonding force between the coating and the workpiece 20 is strong, so it has good corrosion resistance and durability, and also has a unique metallic flash effect.
[0111] The above is a detailed introduction to a metal plastic powder spraying process and device provided by the present invention. The description of the specific embodiment is only used to help understand the method of the present invention and its core idea. It should be pointed out that for ordinary technicians in this technical field, without departing from the principle of the present invention, several improvements and modifications can be made to the present invention, and these improvements and modifications also fall within the scope of protection of the claims of the present invention.
[0112] It should be noted that if no specific experimental steps or conditions are specified in the examples, the conventional experimental steps or conditions described in the literature in the field can be used. If no manufacturer is specified for the reagents or instruments used, they are all conventional reagent products that can be purchased commercially.
[0113] The above examples are intended to provide a better understanding of the present invention, and are not intended to be limiting of the best implementation mode described herein, nor are they intended to limit the content and protection scope of the present invention. Any product identical or similar to the present invention that is derived by anyone under the inspiration of the present invention or by combining the present invention with features of other prior arts shall fall within the protection scope of the present invention.
Claims
1. A metal plastic powder spraying process, characterized in that: The following steps are involved: S1. Surface treatment is performed on the workpiece to be processed (20), and the surface-treated workpiece to be processed (20) is dried; S2. The dried workpiece to be processed (20) is mounted on a rotatable fixture; S3. The workpiece to be processed (20) is transferred to the spraying area and sprayed with a mouthful of metallic flash plastic powder; S4. The sprayed workpiece (20) is transferred to a curing area for high temperature curing; S5. Cooling and unloading the solidified workpiece (20) to obtain a workpiece (20) sprayed with metal plastic powder.
2. The metal plastic powder spraying process according to claim 1, characterized in that: In the step S1, when the workpiece (20) to be processed is subjected to surface treatment, electrolysis and surface finishing polishing operations are performed in sequence.
3. The metal plastic powder spraying process according to claim 1, characterized in that: In the step S3, when the metal glitter plastic powder is fully sprayed, the workpiece (20) is first heated, and then the metal glitter plastic powder is fully sprayed.
4. The metal plastic powder spraying process according to claim 3, characterized in that: When the workpiece (20) is heated, the workpiece (20) is heated to 100-120° C. by a high-temperature drying tunnel or external coil heating or natural gas heating, and external air flow circulation is performed on the workpiece (20).
5. The metal plastic powder spraying process according to claim 1, characterized in that: In the step S3, when the metal flash plastic powder is sprayed full mouth, the liquid metal flash plastic powder is sprayed on a large area from top to bottom and then from bottom to top through the spray gun (65).
6. The metal plastic powder spraying process according to claim 1, characterized in that: In the step S4, when high temperature curing is performed, a high temperature oven is used for high temperature curing, the temperature in the high temperature oven is 190-220° C. A plurality of sensors are arranged in the high temperature oven for dynamic feedback adjustment of the temperature of the high temperature oven and the transmission speed of the workpiece (20).
7. A metal plastic powder spraying device, characterized in that: Used to execute the metal plastic powder spraying process described in any one of claims 1 to 6, the device comprises a fixture and a spraying unit (60), the fixture comprises a fixed part (10), a rotating part (30) and an exhaust part (40), the fixed part (10) is assembled on the rotating part (30), the fixed part (10) is sealed with a workpiece to be processed (20), the exhaust part (40) is arranged in the fixed part (10) and is connected to the workpiece to be processed (20), and the spraying unit (60) is used to spray the workpiece to be processed (20).
8. The metal plastic powder spraying device according to claim 7, characterized in that: The fixing portion (10) comprises a connecting seat (14) and a fixing seat (11), the connecting seat (14) and the fixing seat (11) are fixedly connected, an annular platform (12) is fixedly arranged on the connecting seat (14), an elastic washer (13) is arranged on the annular platform (12), and an external thread is arranged on the outer wall of the connecting seat (14); The rotating part (30) comprises a transmission member and a driving member, one end of the transmission member is connected to the fixed part (10), and the other end is connected to the driving member.
9. The metal plastic powder spraying device according to claim 7, characterized in that: The exhaust portion (40) comprises a mounting plate (41) and a control member, wherein the mounting plate (41) is fixedly arranged in the fixing portion (10), a through hole (42) is arranged on the mounting plate (41), and the control member is installed at the through hole (42) and is used to control the opening and closing of the through hole (42) and the exhaust of airflow.
10. The metal plastic powder spraying device according to claim 7, characterized in that: The fixture tooling also includes a magnetic attraction portion (50), the magnetic attraction portion (50) includes a bracket (51) and a plurality of magnets, the bracket (51) is detachably mounted on the fixing portion (10), the plurality of magnets are respectively arranged on the peripheral side of the bracket (51), and the bracket (51) is provided with a plurality of through slots (53).