Method for cleaning aviation kerosene pipeline attached with high-temperature coke layer

Through combined reagents and ultrasonic cleaning technology, the problem of poor removal of high-temperature coke layer attached to aviation kerosene pipelines is solved, and efficient cleaning effect is achieved, with an error of milligram level, which is better than traditional methods.

CN118904812AActive Publication Date: 2024-11-08TIANMUSHAN LABORATORY +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411184872.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-08
Estimated Expiration
2044-08-27

AI Technical Summary

Technical Problem

The existing aviation kerosene pipeline cleaning method has poor removal effect on the attached high-temperature coke layer, resulting in reduced engine heat exchange efficiency and blocked runners.

Method used

Combination reagents/combination reagents combined with ultrasonic cleaning methods, including dipping or ultrasonic cleaning of oxidants and alkaline agents, combined with ultrasonic technology, remove the coke layer in the pipeline.

Benefits of technology

It significantly improves the cleaning effect of aviation kerosene pipelines, ensures that the error is at the milligram level, effectively removes the coke layer, and is better than gas blowing and single chemical reagent method.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904812A_ABST
    Figure CN118904812A_ABST
Patent Text Reader

Abstract

A method for cleaning an aviation kerosene pipeline attached with a high-temperature coke layer belongs to the field of pipeline cleaning, and comprises the following steps: firstly, judging whether the aviation kerosene pipeline to be cleaned can be put into an ultrasonic cleaning machine, and for the aviation kerosene pipeline which cannot be put into the ultrasonic cleaning machine, adopting a combined reagent cleaning method: flushing residual aviation kerosene; soaking with an oxidizing agent; removing the residual oxidant; immersion cleaning with an alkaline agent; treating waste liquid. For the aviation kerosene pipeline which can be placed in an ultrasonic cleaning machine, a combined reagent combined ultrasonic cleaning method is adopted, ultrasonically cleaning with an oxidant; ultrasonic cleaning with an alkaline agent; performing direct ultrasonic cleaning; treating waste liquid. According to the method, combined reagent / combined reagent combined ultrasonic cleaning is adopted, effective cleaning of the aviation kerosene pipeline attached with the high-temperature coke layer can be achieved, it is guaranteed that the error is at the milligram level, the coke layer can be effectively removed, and the problem that an existing cleaning method for the coke layer attached to the aviation kerosene pipeline is poor in coke removing effect is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of pipeline cleaning, and in particular relates to a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer attached thereto. Background Art

[0002] In the new generation of aircraft engines, using its own fuel, namely aviation kerosene, as a heat sink to cool the hot end components of the engine is considered to be an effective way to solve the problem of engine thermal protection. However, during the heat exchange process of aviation kerosene, when its temperature reaches above 150°C, an oxidation coking reaction will occur, forming a coke layer with low thermal conductivity attached to the wall of the aviation kerosene pipeline, which will lead to deterioration of heat exchange and even cause blockage of the flow channel, resulting in engine failure. Therefore, timely cleaning and blowing off the coke layer attached to the wall of the aviation kerosene pipeline is the key to ensuring the heat exchange effect of aviation kerosene.

[0003] At present, the cleaning methods for the coke layer attached to aviation kerosene pipelines mainly include gas blowing cleaning method, chemical reagent cleaning method, etc. Among them, the chemical reagents in the chemical reagent cleaning method mainly include: dissolving reagents such as dichloromethane, oxidizing cleaning agents such as hydrogen peroxide and alkaline oxidizing cleaning agents such as sodium nitrate.

[0004] Since the oxidation coking reaction of aviation kerosene involves hundreds of elementary reactions, the generated coke has a variety of microscopic morphologies such as needle-shaped, mesh-shaped, spherical, and amorphous ( Figure 1 ), cokes of various microscopic morphologies are interconnected and closely attached to the wall surface, and the above-mentioned existing aviation kerosene pipeline cleaning methods are less effective in removing cokes. Summary of the invention

[0005] In order to solve the problem of poor coke removal effect in the existing cleaning method of aviation kerosene pipeline with attached coke layer, the present invention provides a cleaning method of aviation kerosene pipeline with attached high-temperature coke layer. The present invention is a method of using a combined reagent / combined reagent combined with ultrasonic cleaning, which can effectively clean the aviation kerosene pipeline with attached high-temperature coke layer.

[0006] The technical solution adopted by the present invention to solve the technical problem is as follows:

[0007] The present invention provides a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer, comprising the following steps: first, determining whether the aviation kerosene pipeline to be cleaned can be placed in an ultrasonic cleaning machine; for aviation kerosene pipelines that cannot be placed in an ultrasonic cleaning machine, a combined reagent cleaning method is used, and the specific implementation process is as follows:

[0008] S1. Residual aviation kerosene flushing;

[0009] Use n-hexane to flush the aviation kerosene pipeline to be cleaned to remove the residual aviation kerosene in the pipeline, and then flush it with tap water;

[0010] S2. Oxidant leaching;

[0011] Use the configured oxidant to soak and wash the aviation kerosene pipeline to be cleaned;

[0012] S3. Residual oxidant removal;

[0013] Use ferrous sulfate to soak the aviation kerosene pipeline to be cleaned, and then soak it with dilute hydrochloric acid until the discharged solution is clear;

[0014] S4. Alkaline agent leaching;

[0015] Use 10% sodium hydroxide solution to soak the aviation kerosene pipeline to be cleaned, and then rinse it with tap water;

[0016] S5. Waste liquid treatment;

[0017] Add sodium bicarbonate powder to the last discharged alkaline waste liquid until the sodium bicarbonate powder no longer dissolves;

[0018] For aviation kerosene pipelines that can be placed in an ultrasonic cleaning machine, a combined reagent combined with ultrasonic cleaning method is used. The specific implementation process is as follows:

[0019] S1. Direct ultrasonic cleaning;

[0020] Place the aviation kerosene pipeline to be cleaned into the cleaning cylinder of the ultrasonic cleaning machine and directly perform ultrasonic cleaning with tap water;

[0021] S2. Oxidant ultrasonic cleaning;

[0022] Use the configured oxidant to add into the cleaning cylinder of the ultrasonic cleaning machine for ultrasonic cleaning; after ultrasonic cleaning, pour the waste liquid in the cleaning cylinder of the ultrasonic cleaning machine into the waste liquid tank, and rinse the cleaning cylinder of the ultrasonic cleaning machine with tap water;

[0023] S3. Alkaline agent ultrasonic cleaning;

[0024] Add 10% sodium hydroxide solution to the cleaning cylinder of the ultrasonic cleaning machine, heat it to 70-90°C for ultrasonic cleaning; after ultrasonic cleaning, pour the waste liquid in the cleaning cylinder of the ultrasonic cleaning machine into the waste liquid tank, and rinse the cleaning cylinder of the ultrasonic cleaning machine with tap water;

[0025] S4. Direct ultrasonic cleaning;

[0026] Add tap water to the cleaning cylinder of the ultrasonic cleaning machine and heat it to 70-90°C for ultrasonic cleaning;

[0027] S5. Waste liquid treatment;

[0028] For potassium permanganate waste liquid, add ferrous sulfate first and then dilute hydrochloric acid, and stir until it becomes clear; for sodium hydroxide waste liquid, add sodium bicarbonate powder until the sodium bicarbonate powder no longer dissolves.

[0029] As a preferred embodiment, the oxidant is prepared in a volume ratio of saturated potassium permanganate solution to distilled water of (1.5-2.5):(2.5-3.5).

[0030] As a preferred embodiment, in the step S1 of direct ultrasonic cleaning of the combined reagent and ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 30min-60min.

[0031] As a preferred embodiment, in the step S2 oxidant ultrasonic cleaning of the combined reagent combined with the ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 60min-180min.

[0032] As a preferred embodiment, in the alkaline agent ultrasonic cleaning in step S3 of the combined reagent combined ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 60min-120min.

[0033] As a preferred embodiment, in the direct ultrasonic cleaning in step S4 of the combined reagent and ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 30min-60min.

[0034] The beneficial effects of the present invention are:

[0035] The present invention provides a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer. Compared with the existing gas blowing method (nitrogen) and the single oxidant cleaning method, the cleaning method of the present invention has obvious advantages in the cleaning effect of the aviation kerosene pipeline. The present invention provides a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer. The method adopts a combination reagent / combination reagent combined with ultrasonic cleaning, which can effectively clean the aviation kerosene pipeline with a high-temperature coke layer, and the error is guaranteed to be at the milligram level. The coke layer can be effectively removed, and the problem of poor coke removal effect in the existing cleaning method for the aviation kerosene pipeline with a coke layer is solved. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 This is an electron microscope photograph of a high-temperature coke layer with complex and varied microscopic morphology.

[0037] Figure 2 The present invention provides a flow chart of a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer attached thereto.

[0038] Figure 3The electron microscope photos of the aviation kerosene pipeline before and after cleaning by different methods are shown in the figure, (a) before cleaning, (b) after cleaning by the method of the present invention, (c) after cleaning by gas blowing method, and (d) after cleaning by single chemical reagent method. DETAILED DESCRIPTION

[0039] The present invention is further described in detail below in conjunction with the accompanying drawings.

[0040] like Figure 2 As shown, the present invention provides a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer, which mainly includes a combined reagent cleaning method and a combined reagent combined ultrasonic cleaning method. First, it is necessary to determine whether the aviation kerosene pipeline to be cleaned can be placed in an ultrasonic cleaning machine. For aviation kerosene pipelines that cannot be placed in an ultrasonic cleaning machine, a combined reagent cleaning method is used, and the specific implementation process is as follows:

[0041] S1. Residual aviation kerosene flushing;

[0042] Use n-hexane to flush the aviation kerosene pipeline to be cleaned to remove the residual aviation kerosene in the pipeline, and then flush it with tap water;

[0043] S2. Oxidant leaching;

[0044] A saturated potassium permanganate solution is prepared into an oxidant in a volume ratio of (1.5-2.5) to distilled water, and the prepared oxidant is used to immerse the aviation kerosene pipeline to be cleaned;

[0045] S3. Residual oxidant removal;

[0046] Use ferrous sulfate to soak the aviation kerosene pipeline to be cleaned, and then soak it with dilute hydrochloric acid until the discharged solution is clear;

[0047] S4. Alkaline agent leaching;

[0048] Use 10% sodium hydroxide solution to soak the aviation kerosene pipeline to be cleaned, and then rinse it with tap water;

[0049] S5. Waste liquid treatment;

[0050] Sodium bicarbonate powder is added to the last discharged alkaline waste liquid until the sodium bicarbonate powder no longer dissolves.

[0051] Among them, for aviation kerosene pipelines that can be placed in an ultrasonic cleaning machine, a combined reagent combined with ultrasonic cleaning method is used, and the specific implementation process is as follows:

[0052] S1. Direct ultrasonic cleaning;

[0053] The aviation kerosene pipeline to be cleaned is placed in the cleaning cylinder of an ultrasonic cleaning machine and directly cleaned with tap water. The ultrasonic power is preferably 1000W-2000W, more preferably 1500W, and the ultrasonic time is preferably 30min-60min, more preferably 30min.

[0054] S2. Oxidant ultrasonic cleaning;

[0055] A saturated potassium permanganate solution is prepared into an oxidant in a ratio of (1.5-2.5) to distilled water by volume; the prepared oxidant is added into a cleaning barrel of an ultrasonic cleaning machine for ultrasonic cleaning, wherein the ultrasonic power is preferably 1000W-2000W, more preferably 1500W, and the ultrasonic time is preferably 60min-180min, more preferably 180min; after ultrasonic cleaning, the waste liquid in the cleaning barrel of the ultrasonic cleaning machine is poured into a waste liquid tank, and the cleaning barrel of the ultrasonic cleaning machine is rinsed with tap water;

[0056] S3. Alkaline agent ultrasonic cleaning;

[0057] Add 10% sodium hydroxide solution to the cleaning cylinder of the ultrasonic cleaning machine, heat it to 70-90°C for ultrasonic cleaning, the ultrasonic power is preferably 1000W-2000W, more preferably 1500W, the ultrasonic time is preferably 60min-120min, more preferably 60min; after ultrasonic cleaning, pour the waste liquid in the cleaning cylinder of the ultrasonic cleaning machine into the waste liquid tank, and rinse the cleaning cylinder of the ultrasonic cleaning machine with tap water;

[0058] S4. Direct ultrasonic cleaning;

[0059] Add tap water to the cleaning cylinder of the ultrasonic cleaning machine and heat it to 70-90°C for ultrasonic cleaning; the ultrasonic power is preferably 1000W-2000W, more preferably 1000W, and the ultrasonic time is preferably 30min-60min, more preferably 30min;

[0060] S5. Waste liquid treatment;

[0061] For potassium permanganate waste liquid, add ferrous sulfate first and then dilute hydrochloric acid, and stir until it becomes clear; for sodium hydroxide waste liquid, add sodium bicarbonate powder until the sodium bicarbonate powder no longer dissolves.

[0062] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0063] Example 1: Method for cleaning aviation kerosene pipeline with high-temperature coke layer of the present invention

[0064] Specifically, for a group of circular cross-section aviation kerosene pipelines with an outer diameter of 3mm, an inner diameter of 2mm, and a length of 500mm, which have been subjected to high-temperature oxidation and coking for two hours, a combined reagent combined with ultrasonic cleaning method can be adopted. The specific operation steps are as follows:

[0065] (1) Put enough tap water into the cleaning cylinder of the ultrasonic cleaning machine. The tap water level should be about 2-3 cm higher than the heating rod. Put the circular cross-section aviation kerosene pipeline to be cleaned into the cleaning cylinder of the ultrasonic cleaning machine and directly use tap water for ultrasonic cleaning. The ultrasonic power is 1500W and the ultrasonic time is 30 minutes.

[0066] (2) Place the pipe cleaning rack into the cleaning cylinder of the ultrasonic cleaning machine, add about 350 ml of potassium permanganate cleaning solution for ultrasonic cleaning, the ultrasonic power is 1500W, and the ultrasonic time is 180 minutes (due to equipment limitations, the actual time is 60 minutes × 3 times or 90 minutes × 2 times); the amount of potassium permanganate cleaning solution added can be adjusted appropriately, preferably about 1 cm higher than the upper end of the experimental tube. Among them, the potassium permanganate cleaning solution is prepared according to the volume ratio of saturated potassium permanganate solution to distilled water of 2:3;

[0067] (3) Add 10% sodium hydroxide solution to the cleaning cylinder of the ultrasonic cleaning machine, heat it to 80° C. for ultrasonic cleaning, the ultrasonic power is 1500 W, the ultrasonic time is 60 min, and the ultrasonic cleaning machine is not covered during cleaning;

[0068] (4) Drain the potassium permanganate cleaning liquid in the cleaning cylinder into the waste liquid tank, add 350 ml of tap water to the cleaning cylinder, rotate the pipe cleaning rack slightly to clean the potassium permanganate in the pipe section for 10-15 seconds, and then drain the water into the waste liquid tank, keep the drain valve of the cleaning cylinder open, and then rinse the inner wall of the cleaning cylinder, the pipe cleaning rack and the pipe section with 100-200 ml of tap water;

[0069] (5) Add ferrous sulfate to the waste liquid tank and stir until the purple color of the solution fades, then add dilute hydrochloric acid to the solution and stir until it becomes clear, pour the waste liquid into the sewer and clean the waste liquid tank with tap water;

[0070] (6) Add about 300 ml of 10% sodium hydroxide solution into the cleaning cylinder. The liquid level should be about 2 mm above the upper end of the test tube.

[0071] (7) Add 10% sodium hydroxide solution to the cleaning cylinder of the ultrasonic cleaning machine, heat to 80° C. for ultrasonic cleaning, the ultrasonic power is 1500 W, and the ultrasonic time is 60 min;

[0072] (8) Pour the sodium hydroxide solution in the cleaning cylinder into the waste liquid tank, keep the drain valve of the cleaning cylinder open, and then rinse the inner wall of the cleaning cylinder, the pipeline cleaning rack and the pipe section with 100-200ml of tap water;

[0073] (9) adding sodium bicarbonate powder to the waste liquid until it no longer dissolves, pouring the waste liquid into the sewer and cleaning the waste liquid tank with tap water;

[0074] (10) Add about 300 ml of tap water into the cleaning cylinder. The liquid level should be about 2 mm higher than the top of the test tube.

[0075] (11) Add tap water to the cleaning cylinder of an ultrasonic cleaning machine, heat it to 80° C. and perform ultrasonic cleaning at an ultrasonic power of 1000 W and an ultrasonic time of 30 min;

[0076] (12) Drain the waste liquid in the cleaning cylinder into the sewer and clean all experimental instruments with tap water;

[0077] (13) The mass of coke removed from the aviation kerosene pipeline before and after cleaning is measured using the cutoff weighing method.

[0078] The above test was repeated three times under the same conditions, and the results were averaged. After calculation, the error in the mass of coke washed away did not exceed 1% and 0.2 mg, and the error was guaranteed to be at the milligram level. This proves that the aviation kerosene pipeline cleaning method with a high-temperature coke layer attached to the present invention can effectively remove the coke layer, and the coke removal effect is good.

[0079] Comparative Example 1 Gas Blowing Method (Nitrogen)

[0080] For a group of circular cross-section aviation kerosene pipelines with an outer diameter of 3mm, an inner diameter of 2mm, and a length of 500mm, which had been subjected to two hours of high-temperature oxidation and coking, a gas blowing method (nitrogen) was used for cleaning.

[0081] Comparative Example 2: Single Oxidant Cleaning Method

[0082] For a group of circular cross-section aviation kerosene pipelines with an outer diameter of 3mm, an inner diameter of 2mm, and a length of 500mm, which had been subjected to two hours of high-temperature oxidation and coking, a single oxidant cleaning method was used for cleaning.

[0083] The cleaning method of the present invention, the gas blowing method (nitrogen), and the single oxidant cleaning method were used to clean the circular cross-section aviation kerosene pipeline that had undergone the same coking process. The aviation kerosene pipeline was observed under an electron microscope before and after cleaning. The results are as follows: Figure 3As shown, it was found that the gas method and the single oxidant method had obvious coking residues, while the aviation kerosene pipeline cleaning method with attached high-temperature coke layer of the present invention did not find obvious coking residues, and the coke removal effect was good, which proved that the cleaning method of the present invention has certain reliability and obvious cleaning effect advantages. In summary, the existing technologies for cleaning aviation kerosene pipelines include gas blowing method or simple chemical reagent removal method, which have poor removal effects on the high-temperature coke layer attached to the wall of the aviation kerosene pipeline after complex oxidation coking reaction. The aviation kerosene pipeline cleaning method with attached high-temperature coke layer provided by the present invention can effectively remove the coke layer, ensuring that the error is at the milligram level.

[0084] The present invention discloses a method for cleaning an aviation kerosene pipeline with a high-temperature coke layer attached thereto. Those skilled in the art can refer to the contents of this article and appropriately improve the process parameters to achieve the cleaning method. It should be particularly noted that all similar substitutions and modifications are obvious to those skilled in the art and are considered to be included in the present invention. The product of the present invention has been described through preferred embodiments, and relevant personnel can obviously modify or appropriately change and combine the product described herein without departing from the content, spirit and scope of the present invention to implement and apply the technology of the present invention.

Claims

1. Cleaning method of aviation kerosene pipeline with high temperature coke layer. It is characterized in that The method comprises the following steps: firstly, determining whether the aviation kerosene pipeline to be cleaned can be placed in an ultrasonic cleaning machine; for aviation kerosene pipelines that cannot be placed in an ultrasonic cleaning machine, a combined reagent cleaning method is used, and the specific implementation process is as follows: S1. Residual aviation kerosene flushing; Use n-hexane to flush the aviation kerosene pipeline to be cleaned to remove the residual aviation kerosene in the pipeline, and then flush it with tap water; S2. Oxidant leaching; Use the configured oxidant to soak and wash the aviation kerosene pipeline to be cleaned; S3. Residual oxidant removal; Use ferrous sulfate to soak the aviation kerosene pipeline to be cleaned, and then soak it with dilute hydrochloric acid until the discharged solution is clear; S4. Alkaline agent leaching; Use 10% sodium hydroxide solution to soak the aviation kerosene pipeline to be cleaned, and then rinse it with tap water; S5. Waste liquid treatment; Add sodium bicarbonate powder to the last discharged alkaline waste liquid until the sodium bicarbonate powder no longer dissolves; For aviation kerosene pipelines that can be placed in an ultrasonic cleaning machine, a combined reagent combined with ultrasonic cleaning method is used. The specific implementation process is as follows: S1. Direct ultrasonic cleaning; Place the aviation kerosene pipeline to be cleaned into the cleaning cylinder of the ultrasonic cleaning machine and directly perform ultrasonic cleaning with tap water; S2. Oxidant ultrasonic cleaning; Use the configured oxidant to add into the cleaning cylinder of the ultrasonic cleaning machine for ultrasonic cleaning; after ultrasonic cleaning, pour the waste liquid in the cleaning cylinder of the ultrasonic cleaning machine into the waste liquid tank, and rinse the cleaning cylinder of the ultrasonic cleaning machine with tap water; S3. Alkaline agent ultrasonic cleaning; Add 10% sodium hydroxide solution to the cleaning cylinder of the ultrasonic cleaning machine, heat it to 70-90°C for ultrasonic cleaning; after ultrasonic cleaning, pour the waste liquid in the cleaning cylinder of the ultrasonic cleaning machine into the waste liquid tank, and rinse the cleaning cylinder of the ultrasonic cleaning machine with tap water; S4. Direct ultrasonic cleaning; Add tap water to the cleaning cylinder of the ultrasonic cleaning machine and heat it to 70-90°C for ultrasonic cleaning; S5. Waste liquid treatment; For potassium permanganate waste liquid, add ferrous sulfate first and then dilute hydrochloric acid, and stir until it becomes clear; for sodium hydroxide waste liquid, add sodium bicarbonate powder until the sodium bicarbonate powder no longer dissolves.

2. The method for cleaning an aviation kerosene pipeline with a high-temperature coke layer according to claim 1, It is characterized in that The oxidant is prepared according to the volume ratio of saturated potassium permanganate solution to distilled water of (1.5-2.5):(2.5-3.5).

3. The method for cleaning an aviation kerosene pipeline with a high-temperature coke layer according to claim 1, It is characterized in that In the step S1 of direct ultrasonic cleaning of the combined reagent and ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 30min-60min.

4. The method for cleaning an aviation kerosene pipeline with a high-temperature coke layer according to claim 1, It is characterized in that In the step S2 of the combined reagent and ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 60min-180min.

5. The method for cleaning an aviation kerosene pipeline with a high-temperature coke layer according to claim 1, It is characterized in that In the alkaline agent ultrasonic cleaning of step S3 of the combined reagent combined ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 60min-120min.

6. The method for cleaning an aviation kerosene pipeline with a high-temperature coke layer according to claim 1, It is characterized in that In the direct ultrasonic cleaning of step S4 of the combined reagent and ultrasonic cleaning method, the ultrasonic power is 1000W-2000W, and the ultrasonic time is 30min-60min.

Citation Information

Patent Citations

  • Method for ultrasonic removal of carbon deposition

    CN103757650A

  • Engine duct carbon deposit removing method

    CN108150288A

  • Cleaning solution and cleaning method for coke on inner surface of renewable pipeline

    CN112626528A

  • Impurity removal and modification method for pyrolysis carbon black of waste tires

    US20230242769A1