Stirring friction continuous additive manufacturing device and method based on directional solidification

Through directional solidification technology combined with friction stir additive manufacturing, continuous feeding and additive deposition of metal liquids is achieved, which solves the problem of not being able to achieve continuous additive and personalized manufacturing in the prior art, and improves production efficiency and complex material forming. sex.

CN118905253APending Publication Date: 2024-11-08NANJING UNIV OF SCI & TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410868231.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-01
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing friction stir additive manufacturing devices cannot realize the continuous process directly from raw materials to additive components, cannot customize personalized materials, and it is difficult to manufacture complex large structural parts.

Method used

Directional solidification technology combined with friction stir additive manufacturing, through insulation furnace, heating device, water-cooled crystallizer, traction and feeding mechanism, spindle drive device and stirring head, continuous feeding and directional solidification of metal liquid is achieved, forming rod material, and Rotating stirring deposition is performed on the additive manufacturing substrate to achieve continuous additive manufacturing.

Benefits of technology

The continuous additive manufacturing of the machine is realized, the production efficiency is improved, and the additive can be directly applied on the existing additive layer, overcoming the problem that traditional friction stir additive manufacturing cannot achieve continuous cast alloys, and achieving personality Chemical material ratio and the formation of complex large components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905253A_ABST
    Figure CN118905253A_ABST
Patent Text Reader

Abstract

The invention discloses a stirring friction continuous additive manufacturing device and method based on directional solidification, and the device comprises a heat preservation furnace which is used for pouring molten metal; the heating device is used for heating the molten metal, so that gas is discharged from the molten metal; the valve is used for controlling the molten metal in the heat preservation furnace to flow out; the water cooling crystallizer is used for providing a temperature gradient environment for directional solidification, so that the molten metal forms a bar material; the detection unit is used for detecting the position of the bar so as to control the traction and feeding mechanism and the main shaft to work; the traction and feeding mechanism is used for clamping the bar and applying downward pressure to the bar and can rotate along with the main shaft; the spindle driving device is used for driving the spindle to rotate; the main shaft is used for driving the bar and the stirring head to rotate, so that the bar forms an additive layer on the additive manufacturing substrate; the stirring head is used for increasing the plastic flowability of the additive layer; and the cooling device is used for cooling the stirring head. The continuous feeding friction stir additive manufacturing device realizes continuous feeding friction stir additive manufacturing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of friction stir additive manufacturing, and in particular to a friction stir continuous additive manufacturing device and method based on directional solidification. Background Art

[0002] Additive manufacturing (AM), also known as 3D printing technology, is a revolutionary rapid prototyping technology. Its basic principle is to use a discrete-stacking method to discretize the digital model and continuously stack the materials to form the required solid model. It has the advantages of short processing cycle, simple process, high efficiency, small grain size, dense structure and excellent mechanical properties. It has been applied in many fields such as aerospace, biomedicine, and automobile manufacturing. Friction stir deposition additive manufacturing (AFSD) technology is an emerging solid-phase additive technology in recent years. The material does not melt during the additive process, avoiding the processing defects such as pores and thermal cracks based on traditional molten additives. Its high additive efficiency is suitable for additive manufacturing of large-sized parts, and it has low requirements for the manufacturing environment, no polluting gas generation, and is green and environmentally friendly. The existing friction stir additive manufacturing device cannot realize the process directly from raw materials to additive components. The current device is also difficult to carry out the continuous additive process of supplying raw materials, and cannot realize personalized material customization.

[0003] To address the above problems, it is necessary to develop a device for directional solidification and continuous friction stir additive manufacturing, which can realize friction stir additive manufacturing of raw materials with a variety of different proportions, overcome the inherent limitations of existing friction stir additive manufacturing technology, and broaden the breadth and depth of application of this additive manufacturing technology. Summary of the invention

[0004] The object of the present invention is to provide a device and method for continuous friction stir additive manufacturing with directional solidification, so as to realize friction stir additive manufacturing with continuous feeding.

[0005] The technical solution to achieve the purpose of the present invention is:

[0006] A friction stir continuous additive manufacturing device based on directional solidification, comprising:

[0007] A holding furnace for pouring molten metal;

[0008] A heating device, used to heat the molten metal so that the molten metal discharges gas;

[0009] The valve is used to control the outflow of the molten metal in the holding furnace. When directional solidification is required, the valve is opened so that the heat flow of the molten metal is mainly transmitted in one direction along the casting direction;

[0010] A water-cooled crystallizer is used to provide a temperature gradient environment for directional solidification so that the molten metal forms a bar;

[0011] A detection unit is used to detect the position of the bar material to control the operation of the traction and feeding mechanism and the spindle;

[0012] The traction and feeding mechanism is used to clamp the bar material and apply pressure to the bar material along the axial direction of the bar material, and can rotate with the main shaft;

[0013] A spindle driving device, used for driving the spindle to rotate;

[0014] A spindle, used to drive the rod and the stirring head to rotate, so that the rod forms an additive layer on the additive manufacturing substrate;

[0015] A stirring head, used to increase the plastic fluidity of the additive layer;

[0016] The cooling device is used to cool the stirring head.

[0017] A friction stir continuous additive manufacturing device based on directional solidification is used in an additive manufacturing method, comprising:

[0018] Step 1: Before the equipment starts working, first prepare the molten metal that needs to be stir-friction additively manufactured, start the heating device and water-cooled crystallizer for directional solidification, preheat and exhaust the gas in the molten metal, and ensure that the directional solidification area has a stable temperature gradient; pour the molten metal that has been adjusted into the insulation furnace. When the temperature of the molten metal is stable, open the valve at the bottom of the insulation furnace, and the molten metal flows through the heating device and the water-cooled crystallizer according to gravity;

[0019] Step 2: When the bar material is discharged from the water-cooled crystallizer, the traction and feeding mechanism is started. When the position detection unit detects that the bar material enters the traction and feeding mechanism, the traction and feeding mechanism starts to operate, the spindle drive device drives the spindle to rotate, and the traction and feeding mechanism holds the bar material and applies downward pressure to the bar material;

[0020] Step 3: Start the cooling device of the stirring head. After the material is discharged from the end of the stirring head, it stays until the rod material undergoes plastic deformation, softening and deposition. The spindle is controlled to move along the additive manufacturing direction path. During this process, the traction and feeding mechanisms are continuously operated, so that the rod material is continuously discharged from between the stirring head and the additive manufacturing substrate. At the same time, the additive layer gradually forms a flat surface under the stirring action of the stirring head.

[0021] Step 4: The stirring head continuously trims the plane. When the spindle reaches the end of the planned path, the spindle is lifted and starts printing the original second layer. This cycle is repeated until the component is printed.

[0022] Compared with the prior art, the present invention has the following significant advantages:

[0023] (1) By integrating the directional solidification method and the friction stir additive manufacturing method, continuous additive manufacturing without stopping the machine is achieved, which can work continuously and produce large-sized complex structural parts. At the same time, this method can directly add material on the existing additive layer, greatly improving production efficiency and having excellent economy; it can realize the forming of complex large components, overcoming the current problem that friction stir additive manufacturing cannot achieve continuous casting alloys.

[0024] (2) Through the directional solidification device, the specific composition ratio of the alloy material is personalized, and by adjusting the cooling rate of the alloy bar, the bar for stir friction additive manufacturing can be produced in real time, realizing uninterrupted stir friction additive manufacturing, shortening the time required to adjust the raw materials, and realizing personalized manufacturing. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 This is a schematic structural diagram of a friction stir continuous additive manufacturing device based on directional solidification described in the present invention. DETAILED DESCRIPTION

[0026] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0027] Combination Figure 1 The present invention is a friction stir continuous additive manufacturing device based on directional solidification, which mainly includes a heat preservation furnace 1, a heating device 2, a valve 4, a water-cooled crystallizer 5, a traction and feeding mechanism 7, a spindle motor 15, a synchronous pulley 10, a stirring head 11, a water cooling device 12 and an additive manufacturing substrate 14. The device for producing a directionally solidified cast alloy includes a heat preservation furnace 1, a heating device 2, a valve 4, and a water-cooled crystallizer 5. Next is the equipment for friction stir additive manufacturing, which mainly includes a traction and feeding mechanism 7, a spindle motor 15, a synchronous pulley 10, a stirring head 11, a water cooling device 12 and an additive manufacturing substrate 14. The traction and feeding mechanism 7 mainly performs rotational clamping and axial propulsion actions on the cast alloy bar 8 produced by directional solidification above, and the stirring head 11 cooperates with the spindle 6 to drive the alloy bar 8 to rotate, thereby realizing the friction stir deposition between the bar and the additive manufacturing substrate, and achieving the purpose of additive manufacturing.

[0028] The holding furnace 1 is used to shape the cast alloy, and the heating device 2 is evenly distributed outside the holding furnace to ensure that the molten body exists in a liquid state in the heating area, wherein the lower end adopts a chamfered structure, and the chamfering can facilitate the molten body to flow downward and will not be retained in the holding furnace; the heating device 2 is used to reheat the alloy and discharge the bubbles in the alloy melt to ensure that there are no pore defects in the finished cast alloy rod; a valve 4 is arranged at the lower end of the holding furnace 1 to control the flow of the molten metal in the holding furnace 1, and when directional solidification is required, the valve is opened, and vice versa; the water-cooled crystallizer 5 has a large temperature difference and a high temperature gradient, and the cooling rate and temperature gradient can be adjusted according to alloys with different proportions, and the heat flow of the molten metal in the holding furnace 1 is mainly transmitted unidirectionally along the casting direction, which meets the conditions of directional solidification and can obtain an infinitely long columnar structure solidified in one direction. The process is optimized and controlled to facilitate the elimination and growth of grains and realize the continuous casting of single crystals; the traction and feeding mechanism 7 uses two pairs of clamping structures with power sources to clamp the cast alloy bar and apply downward pressure to it, and the clamping structure also rotates with the main shaft; the displacement sensor 9 is arranged in the main shaft 6, mainly used to detect the specific position of the alloy bar 8 in the traction and feeding mechanism 7; the main shaft motor 15 mainly provides stable power for the rotation of the main shaft 6. It can use a servo motor to accurately adjust the main shaft speed to meet the main shaft speed required by alloy bars of different compositions. The synchronous pulley 10 is mainly connected to the main shaft motor 15 through a belt drive to drive the main shaft 6 to rotate. The stirring head 11 includes a connection part between the rotating main shaft 6 and a stirring head part used for additive manufacturing below. The large end face of the connection part faces upward and the small end face faces downward. A plurality of protrusions may be used on the small end face of the stirring head, including but not limited to cylinders, bosses, cones, etc., to accelerate the plastic flow of alloy bars during stir friction additive manufacturing; the material of the stirring head may be high-speed tool steel, cemented carbide, etc. The cooling device 12 mainly cools the stirring head 11 to prevent the stirring head 11 from generating high temperature due to high-speed rotation and stirring friction, causing the internal bars to expand and block the discharge port, thereby ensuring the stability of the overall stir friction additive manufacturing.

[0029] Example

[0030] The embodiment of the present invention provides a friction stir continuous additive manufacturing device based on directional solidification, such as Figure 1 As shown, it includes a heat preservation furnace 1, a heating device 2, a valve 4, a water-cooled crystallizer 5, a spindle 6, a traction and feeding mechanism 7, a spindle motor 15, a displacement sensor 9, a pulley 10, a stirring head 11, a cooling device 12 and an additive manufacturing substrate 14; combined Figure 1The continuous directional solidification device provides a temperature gradient environment for stable directional solidification of the alloy solution 3 with a good proportion (the temperature gradient is determined by the actual material). The spindle motor 15 can drive the synchronous pulley 10 fixed on the spindle 6 to rotate at high speed through the synchronous belt drive, thereby driving the entire spindle 6 to rotate. The traction and feeding mechanism 7 is composed of two pairs of clamping structures, which hold the alloy bar 8 in the spindle 6 and continuously provide a downward force, while ensuring that the alloy bar 8 rotates with the spindle 6. The stirring head 11 can drive the alloy bar 8 to rotate and stir and frictionally deposit the additive with the additive manufacturing substrate 14. During the entire additive process, the alloy bar 8 always keeps synchronous rotation with the spindle 6;

[0031] The directional solidification device mainly consists of two areas. One area is the heating area of ​​the insulation furnace 1 by the heating device 2, which can ensure that the alloy solution 3 is in a liquid state in the insulation furnace 1; the other area is the water-cooled crystallizer 5, which has a stable temperature gradient to ensure that the alloy solution 3 is directionally solidified in this area, and a sufficient length is reserved to ensure that the liquid core is located in this area, ensuring that the alloy rod 8 enters the rotating main shaft 6 in a solid form.

[0032] The spindle 6 can drive the stirring head 11 and the alloy bar 8 to rotate. The stirring head 11 is connected with bolts and nuts. The spindle 6 is fixed on a three-axis motion platform, so the spindle 6 can move in three directions of freedom, which is convenient for producing components of various models and sizes.

[0033] The traction and feeding mechanism 7 can be operated by a clamping structure fixed on the main shaft 6 and distributed on both sides of the alloy bar 8, and its working principle is as follows: when the displacement sensor 9 detects that the alloy bar 8 enters the traction and feeding mechanism 7, the clamping structures on both sides are driven by the power source to firmly clamp and lock the alloy bar 8, and apply downward pressure, and when the clamping mechanism moves axially to the limit position, it will release the bar, move upward and return to the initial position. Among them, when the upper and lower pairs of clamping structures are reset, the other pair of clamping structures should ensure that the alloy bar 8 is clamped, so that alternating and uninterrupted feeding can be achieved. At the same time, the clamping structures on both sides rotate with the main shaft 6 at the same time, so as to achieve the purpose of continuously depositing additives by the alloy bar 8 downward.

[0034] The stirring head 11 includes an overall stepped structure from large to small, and fine protrusion structures are evenly distributed on the smallest cross-section in contact with the additive manufacturing substrate 14. It can be a truncated cone, hemisphere, cone or other structure, and is opened at the center of the stirring head 11 to make it consistent with the cross-sectional size of the alloy rod 8.

[0035] The cooling device 12 is mainly used to cool the stirring head 11 to prevent the internal alloy rod 8 from expanding due to the high temperature caused by the high-speed rotation and stirring of the stirring head 11, which can reduce the deformation of the alloy rod 8 caused by temperature rise and ensure the stability of the overall stir friction additive manufacturing.

[0036] An additive manufacturing method based on a friction stir continuous additive manufacturing device for directional solidification, the specific implementation of which includes the following steps:

[0037] Step 1: Before the equipment starts working, first prepare the alloy solution 3 that needs to be stir-friction additively manufactured, start the heating device 2 and water-cooled crystallizer 5 for directional solidification, preheat for 20 minutes, and exhaust the gas in the alloy solution 3 to prevent defects and ensure that the directional solidification area has a stable temperature gradient. Pour the adjusted alloy solution 3 into the insulation furnace 1 through a crucible. When the temperature of the alloy solution 3 stabilizes, open the valve 4 at the bottom of the insulation furnace 1, and the alloy solution 3 flows through the heating device 2 and the water-cooled crystallizer 5 by gravity;

[0038] Step 2: When the alloy bar 8 is discharged from the water-cooled crystallizer 4 in the directional solidification device according to the action of gravity and the principle of directional solidification, the traction and feeding mechanism 7 is started. When the displacement sensor 9 detects that the alloy bar 8 enters the traction and feeding mechanism 7, the clamping structures on both sides start to operate, and the spindle motor 15 is started. The synchronous belt drive drives the synchronous pulley 10 to rotate, thereby driving the spindle 6 to rotate. The clamping structure holds the alloy bar 8 and rotates synchronously with the spindle 6, and at the same time exerts downward pressure on the alloy bar 8.

[0039] Step three: Start the cooling device 12 of the stirring head 11. After the stirring head 11 discharges the material from the end, it stays until the alloy rod 8 undergoes plastic deformation, softening and deposition. The spindle 6 is controlled to move along the additive manufacturing direction path. During this process, the clamping structure in the traction and feeding mechanism 7 does not stop operating continuously, so that the alloy rod 8 is continuously discharged from between the stirring head 11 and the additive manufacturing substrate 14. At the same time, the additive layer 13 gradually forms a smooth surface under the stirring action of the stirring head 11.

[0040] Step 4: The protruding structure on the stirring head 11 continuously trims the plane. When the spindle 6 reaches the end of the planned path, the spindle 6 is lifted and starts printing the originally planned second layer. This cycle is repeated until the component printing is completed.

[0041] Furthermore, the rotation speed of the stirring head can be adjusted by the spindle servo motor. After the bar is pressed down, the preheating is maintained for about 3-30 seconds.

[0042] Furthermore, when additive manufacturing begins, the three-axis motion platform needs to be controlled to lift the main axis upward relative to the additive manufacturing substrate 14 to the required additive thickness to ensure the thickness of the additive layer.

Claims

1. A friction stir additive continuous manufacturing device based on directional solidification, characterized in that: include: A holding furnace for pouring molten metal; A heating device, used to heat the molten metal so that the molten metal discharges gas; The valve is used to control the outflow of the molten metal in the holding furnace. When directional solidification is required, the valve is opened so that the heat flow of the molten metal is mainly transmitted in one direction along the casting direction; A water-cooled crystallizer is used to provide a temperature gradient environment for directional solidification so that the molten metal forms a bar; A detection unit is used to detect the position of the bar material to control the operation of the traction and feeding mechanism and the spindle; The traction and feeding mechanism is used to clamp the bar material and apply pressure to the bar material along the axial direction of the bar material, and can rotate with the main shaft; A spindle driving device, used for driving the spindle to rotate; A spindle, used to drive the rod and the stirring head to rotate, so that the rod forms an additive layer on the additive manufacturing substrate; A stirring head, used to increase the plastic fluidity of the additive layer; The cooling device is used to cool the stirring head.

2. The friction stir continuous additive manufacturing device based on directional solidification according to claim 1, characterized in that: The spindle drive device includes a spindle motor and a synchronous pulley; The synchronous pulley is connected to the main shaft, and the main shaft motor is connected to the synchronous pulley through a belt drive, thereby driving the main shaft to rotate.

3. The friction stir continuous additive manufacturing device based on directional solidification according to claim 1, characterized in that: The stirring head comprises a connection part between the rotating main shaft and a stirring head part used for additive manufacturing below, wherein the large end face of the connection part faces upward and the small end face faces downward; the stirring head part is provided with a protrusion structure.

4. The friction stir continuous additive manufacturing device based on directional solidification according to claim 1, characterized in that: The lower end of the insulation furnace adopts a chamfered structure.

5. The friction stir continuous additive manufacturing device based on directional solidification according to claim 1, characterized in that: The main shaft is fixed on a three-axis motion platform.

6. The friction stir continuous additive manufacturing device based on directional solidification according to claim 1, characterized in that: The detection unit adopts a displacement sensor and is arranged in the main shaft.

7. The stir friction continuous additive manufacturing device based on directional solidification according to claims 1-6 is used in an additive manufacturing method, characterized in that: include: Step 1: Before the equipment starts working, first prepare the molten metal that needs to be stir-friction additively manufactured, start the heating device and water-cooled crystallizer for directional solidification, preheat and exhaust the gas in the molten metal, and ensure that the directional solidification area has a stable temperature gradient; pour the molten metal that has been adjusted into the insulation furnace. When the temperature of the molten metal is stable, open the valve at the bottom of the insulation furnace, and the molten metal flows through the heating device and the water-cooled crystallizer according to gravity; Step 2: When the bar material is discharged from the water-cooled crystallizer, the traction and feeding mechanism is started. When the position detection unit detects that the bar material enters the traction and feeding mechanism, the traction and feeding mechanism starts to operate, the spindle drive device drives the spindle to rotate, and the traction and feeding mechanism holds the bar material and applies downward pressure to the bar material; Step 3: Start the cooling device of the stirring head. After the material is discharged from the end of the stirring head, it stays until the rod material undergoes plastic deformation, softening and deposition. The spindle is controlled to move along the additive manufacturing direction path. During this process, the traction and feeding mechanisms are continuously operated, so that the rod material is continuously discharged from between the stirring head and the additive manufacturing substrate. At the same time, the additive layer gradually forms a flat surface under the stirring action of the stirring head. Step 4: The stirring head continuously trims the plane. When the spindle reaches the end of the planned path, the spindle is lifted and starts printing the original second layer. This cycle is repeated until the component is printed.

8. The additive manufacturing method according to claim 7, characterized in that: The rotation speed of the stirring head is regulated by the spindle drive device. After the bar is pressed down, the preheating is maintained for about 3-30 seconds.

9. The additive manufacturing method according to claim 7, characterized in that: When additive manufacturing begins, the spindle is lifted up to the desired additive thickness via a multi-axis motion platform.

Citation Information

Cited By

  • Coaxial powder feeding friction stir additive manufacturing and polishing device

    CN121083065A