Seaweed nano grey alkali as well as preparation method and application thereof

By coordinating natural sea limestone and other components with seaweed ash and nano-treated treatment, seaweed nano-grain alkali was prepared, which solved the problems of low efficiency and high cost of traditional water treatment technology, and achieved efficient and low-cost water pollutants Removal effect.

CN118908380AActive Publication Date: 2024-11-08GUANGDONG FUZHI ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411153516.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-08
Estimated Expiration
2044-08-20

AI Technical Summary

Technical Problem

Traditional water treatment technology has limited effectiveness in removing water pollutants, and is cost-effective and inefficient. The application efficiency of seaweed ash is easily affected by water conditions, so its performance needs to be optimized to improve water treatment efficiency.

Method used

Seaweed nano-grain alkali is prepared by synergistically combining natural sea limestone, seaweed ash, carboxymethylcellulose sodium, porous graphene, activator, scale cleaner, plasticizer and diatomaceous earth, and then mix and grind and high-pressure homogenization treatment achieves nanoification, enhancing its adsorption and flocculation capabilities.

Benefits of technology

It achieves the effect of efficient removal of pollutants in water bodies, reduces costs, improves treatment efficiency, is suitable for large-scale applications, and improves the uniformity and stability of materials in water bodies.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005004970740000021
    Figure BDA0005004970740000021
  • Figure BDA0005004970740000031
    Figure BDA0005004970740000031
  • Figure BDA0005004970740000071
    Figure BDA0005004970740000071
Patent Text Reader

Abstract

The invention provides seaweed nano ash alkali as well as a preparation method and application thereof. The seaweed nano ash alkali is prepared from the following components: natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, an activating agent, a scale remover, a plasticizer and diatomite. The preparation method comprises the following steps: (1) mixing natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, an activator, a scale remover, a plasticizer and diatomite in parts by weight, and grinding to obtain a premix; and (2) performing high-pressure homogenization treatment on the premix obtained in the step (1) to obtain the seaweed nano ash alkali. The seaweed nano grey alkali provided by the invention can efficiently remove pollutants in a water body, and compared with a traditional water treatment method, the seaweed nano grey alkali has lower cost and higher treatment efficiency, and is beneficial to large-scale popularization and application.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of water treatment, and relates to a water treatment agent, in particular to a seaweed nano-ash alkali and a preparation method and application thereof. Background Art

[0002] There are many types of water pollutants, mainly including organic matter, inorganic matter, heavy metals, microorganisms, pesticide residues, etc. Each pollutant has different chemical properties and biodegradability, which puts forward different requirements for water treatment technology.

[0003] Traditional water treatment technologies are mainly divided into sedimentation, filtration, adsorption, oxidation, etc., and generally have limited effectiveness in removing specific pollutants. There is also much room for improvement in treatment efficiency, cost, energy consumption and secondary pollution.

[0004] Seaweed ash is a kind of ash left after burning seaweed. It contains a variety of minerals and trace elements, which make it have certain application potential in water treatment. For example, seaweed ash is rich in minerals such as calcium and magnesium, which can form precipitation with heavy metal ions such as lead, cadmium, and mercury in water, thereby removing these pollutants; seaweed ash has a certain alkalinity and can be used to adjust the pH value of water bodies, especially in the neutralization treatment of acidic water bodies; some components in seaweed ash have a flocculation effect, which helps to aggregate suspended particles in water and facilitate their removal by sedimentation or filtration; seaweed ash contains components that inhibit the growth of microorganisms, which helps to control bacteria and algae in water bodies.

[0005] However, the adsorption and flocculation capabilities of seaweed ash are far inferior to those of professional water treatment chemicals. Under normal circumstances, it needs to be used in combination with other treatment methods. In addition, the efficiency of seaweed ash in water treatment is easily affected by factors such as water conditions, pH value, temperature, etc. Therefore, how to optimize the performance of seaweed ash and how to effectively apply it to water treatment processes have become issues that technicians in this field urgently need to solve. Summary of the invention

[0006] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a seaweed nano-lime alkali and a preparation method and application thereof. The seaweed nano-lime alkali can efficiently remove pollutants in water bodies. Compared with traditional water treatment methods, it has lower costs and higher treatment efficiency, which is conducive to large-scale promotion and application.

[0007] To achieve this object, the present invention adopts the following technical solutions:

[0008] In a first aspect, the present invention provides a seaweed nano-ash alkali, the components of which include natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, an activator, a descaling agent, a plasticizer and diatomaceous earth.

[0009] The present invention achieves the purpose of efficiently removing pollutants from water bodies through the synergistic cooperation between specific components and seaweed ash. Among them, natural sea limestone helps to neutralize acidic substances and adjust the pH value of water bodies; sodium carboxymethyl cellulose can promote the aggregation of suspended particles in water, accelerate the sedimentation process through flocculation, and improve the transparency of water bodies; porous graphene has a very high specific surface area and enhances adsorption capacity; the activator can fully activate the potential activity of other components and enhance the effectiveness of the overall material; the descaling agent and seaweed ash work together to further improve the ability to remove dirt; the plasticizer is used to improve the plasticity of the material, making it easier to process and use; diatomaceous earth, as a porous material, provides additional adsorption surface area and fully removes suspended particles and organic matter in the water body. Compared with traditional water treatment methods, the seaweed nano-ash alkali provided by the present invention has lower costs and higher treatment efficiency, which is conducive to large-scale promotion and application.

[0010] Preferably, the seaweed nano-ash base comprises the following components in parts by weight:

[0011]

[0012]

[0013] The weight proportion of the natural sea limestone is 55-69 parts, for example, 55 parts, 56 parts, 57 parts, 58 parts, 59 parts, 60 parts, 61 parts, 62 parts, 63 parts, 64 parts, 65 parts, 66 parts, 67 parts, 68 parts or 69 parts, and the weight proportion of the seaweed ash is 8-12 parts, for example, 8 parts, 8.5 parts, 9 parts, 9.5 parts, 10 parts, 10.5 parts, 11 parts, 11.5 parts or 12 parts, the weight proportion of the sodium carboxymethyl cellulose is 3-7 parts, for example, it can be 3 parts, 3.5 parts, 4 parts, 4.5 parts, 5 parts, 5.5 parts, 6 parts, 6.5 parts or 7 parts, and the weight proportion of the porous graphene is 12-18 parts, for example, it can be 12 parts, 12.5 parts, 13 parts, 13.5 parts, 14 parts, 14.5 parts, 15 parts, 15.5 parts, 16 parts, 16.5 parts, 17 parts, 17.5 parts or 18 parts, the weight portion of the activator is 1-3 parts, for example, it can be 1 part, 1.2 parts, 1.4 parts, 1.6 parts, 1.8 parts, 2 parts, 2.2 parts, 2.4 parts, 2.6 parts, 2.8 parts or 3 parts, the weight portion of the descaling agent is 2-5 parts, for example, it can be 2 parts, 2.5 parts, 3 parts, 3.5 parts, 4 parts, 4.5 parts or 5 parts, the weight portion of the plasticizer is 1-3 parts, for example, it can be 1 part, 1.2 parts, 1.4 parts, 1.6 parts, 1.8 parts, 2 parts, 2.2 parts, 2.4 parts, 2.6 parts, 2.8 parts or 3 parts, the weight proportion of the diatomaceous earth is 1-3 parts, for example, it can be 1 part, 1.2 parts, 1.4 parts, 1.6 parts, 1.8 parts, 2 parts, 2.2 parts, 2.4 parts, 2.6 parts, 2.8 parts or 3 parts, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0014] Preferably, the activator comprises any one of sodium carbonate, aluminum oxide, potassium nitrate, cobalt dioxide, titanium dioxide, magnesium oxide or calcium oxide, or a combination of at least two thereof. Typical but non-limiting combinations include a combination of sodium carbonate and aluminum oxide, a combination of aluminum oxide and potassium nitrate, a combination of potassium nitrate and cobalt dioxide, a combination of cobalt dioxide and titanium dioxide, a combination of titanium dioxide and magnesium oxide, or a combination of magnesium oxide and calcium oxide.

[0015] Preferably, the average particle size of the activator is 10-500 nm, for example, 10 nm, 50 nm, 100 nm, 150 nm, 200 nm, 250 nm, 300 nm, 350 nm, 400 nm, 450 nm or 500 nm, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0016] Preferably, the descaling agent includes any one of sodium dodecylbenzene sulfonate, sodium hydroxide, hydrochloric acid, citric acid, sodium phosphate or acrylic acid, or a combination of at least two thereof. Typical but non-limiting combinations include a combination of sodium dodecylbenzene sulfonate and sodium hydroxide, a combination of sodium hydroxide and hydrochloric acid, a combination of hydrochloric acid and citric acid, a combination of citric acid and sodium phosphate, or a combination of sodium phosphate and acrylic acid.

[0017] Preferably, the average particle size of the descaling agent is 100-500 nm, for example, 100 nm, 150 nm, 200 nm, 250 nm, 300 nm, 350 nm, 400 nm, 450 nm or 500 nm, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0018] Preferably, the plasticizer comprises any one of lignin sulfonate, polycarboxylic acid, naphthalene sulfonate, aromatic aminosulfonate or sulfonated melamine formaldehyde resin, or a combination of at least two thereof. Typical but non-limiting combinations include a combination of lignin sulfonate and polycarboxylic acid, a combination of polycarboxylic acid and naphthalene sulfonate, a combination of naphthalene sulfonate and aromatic aminosulfonate, or a combination of aromatic aminosulfonate and sulfonated melamine formaldehyde resin.

[0019] Preferably, the average particle size of the plasticizer is 100-500 nm, for example, 100 nm, 150 nm, 200 nm, 250 nm, 300 nm, 350 nm, 400 nm, 450 nm or 500 nm, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0020] In a second aspect, the present invention provides a method for preparing the seaweed nano-ash base as described in the first aspect, the preparation method comprising the following steps:

[0021] (1) mixing natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, an activator, a descaling agent, a plasticizer and diatomaceous earth according to weight proportions, and grinding to obtain a premix;

[0022] (2) subjecting the premix obtained in step (1) to high-pressure homogenization to obtain the seaweed nano-ash alkali.

[0023] The present invention achieves sufficient mixing and nano-size of the obtained products through sequential mixing, grinding and high-pressure homogenization treatment, and the nano-scale particles have a larger specific surface area, which helps to improve the adsorption capacity and reaction activity of the material, and at the same time fully improves the uniformity and stability of the material in the water environment, avoids the influence of excessively large particles on the water treatment effect, and ultimately improves the water treatment efficiency.

[0024] Preferably, the grinding process in step (1) is performed until the average particle size of the premix is ​​50-1500nm, for example, it can be 50nm, 100nm, 200nm, 300nm, 400nm, 500nm, 600nm, 700nm, 800nm, 900nm, 1000nm, 1100nm, 1200nm, 1300nm, 1400nm or 1500nm, and the saturation magnetization is 10-100emu / g, for example, it can be 10emu / g, 20emu / g, 30emu / g, 40emu / g, 50emu / g, 60emu / g, 70emu / g, 80emu / g, 90emu / g or 100emu / g, but it is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0025] Preferably, the mixing temperature of the high-pressure homogenization treatment in step (2) is 60-70°C, for example, it can be 60°C, 61°C, 62°C, 63°C, 64°C, 65°C, 66°C, 67°C, 68°C, 69°C or 70°C, the mixing pressure is 19-22MPa, for example, it can be 19MPa, 19.5MPa, 20MPa, 20.5MPa, 21MPa, 21.5MPa or 22MPa, and the treatment time is 20-30min, for example, it can be 20min, 21min, 22min, 23min, 24min, 25min, 26min, 27min, 28min, 29min or 30min, but it is not limited to the listed values, and other values ​​not listed within the numerical range are also applicable.

[0026] As a preferred technical solution of the second aspect of the present invention, the preparation method comprises the following steps:

[0027] (1) mixing 55-69 parts of natural sea limestone, 8-12 parts of seaweed ash, 3-7 parts of sodium carboxymethyl cellulose, 12-18 parts of porous graphene, 1-3 parts of activator, 2-5 parts of descaling agent, 1-3 parts of plasticizer and 1-3 parts of diatomaceous earth, and grinding to obtain a premix having an average particle size of 50-1500 nm and a saturation magnetization of 10-100 emu / g;

[0028] (2) The premix obtained in step (1) is subjected to high-pressure homogenization for 20-30 min, and the mixing temperature of the high-pressure homogenization is controlled to be 60-70° C. and the mixing pressure is controlled to be 19-22 MPa to obtain the seaweed nano-ash alkali.

[0029] In a third aspect, the present invention provides an application of the seaweed nano-lime alkali as described in the first aspect, wherein the seaweed nano-lime alkali is used to remove pollutants in water.

[0030] The numerical range described in the present invention not only includes the point values ​​listed above, but also includes any point values ​​between the above numerical ranges that are not listed. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0031] Compared with the prior art, the present invention has the following beneficial effects:

[0032] (1) The present invention achieves the purpose of efficiently removing pollutants from water bodies through the synergistic cooperation between specific components and seaweed ash. Among them, natural sea limestone helps to neutralize acidic substances and adjust the pH value of water bodies; sodium carboxymethyl cellulose can promote the aggregation of suspended particles in water, accelerate the sedimentation process through flocculation, and improve the transparency of water bodies; porous graphene has a very high specific surface area and enhances adsorption capacity; the activator can fully activate the potential activity of other components and enhance the effectiveness of the overall material; the descaling agent and seaweed ash work together to further improve the ability to remove dirt; the plasticizer is used to improve the plasticity of the material, making it easier to process and use; diatomaceous earth, as a porous material, provides additional adsorption surface area and fully removes suspended particles and organic matter in the water body. Compared with traditional water treatment methods, the seaweed nano-ash alkali provided by the present invention has lower costs and higher treatment efficiency, which is conducive to large-scale promotion and application.

[0033] (2) The present invention achieves sufficient mixing and nano-sizing of the obtained products by sequentially performing mixing, grinding and high-pressure homogenization. The nano-scale particles have a larger specific surface area, which helps to improve the adsorption capacity and reaction activity of the material. At the same time, it fully improves the uniformity and stability of the material in the water environment, avoids the influence of excessively large particles on the water treatment effect, and ultimately improves the water treatment efficiency. DETAILED DESCRIPTION

[0034] The technical solution of the present invention is further illustrated below through specific implementation methods.

[0035] Example 1

[0036] This embodiment provides a seaweed nano-lime alkali and a preparation method thereof. The seaweed nano-lime alkali comprises the following components in parts by weight:

[0037]

[0038] The specific surface area of ​​the porous graphene is 562 m 2 / g, the average particle size of the sodium carbonate is 200nm, the average particle size of the sodium dodecylbenzene sulfonate is 300nm, and the average particle size of the sodium lignin sulfonate is 300nm.

[0039] The preparation method provided in this embodiment comprises the following steps:

[0040] (1) mixing natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, sodium carbonate, sodium dodecylbenzene sulfonate, sodium lignin sulfonate and diatomaceous earth according to weight parts, and grinding to obtain a premix with an average particle size of 1200 nm and a saturation magnetization intensity of 50 emu / g;

[0041] (2) The premix obtained in step (1) is subjected to high-pressure homogenization for 25 minutes, and the mixing temperature of the high-pressure homogenization is controlled to be 65° C. and the mixing pressure is controlled to be 20 MPa, to obtain the seaweed nano-ash alkali.

[0042] Example 2

[0043] This embodiment provides a seaweed nano-lime alkali and a preparation method thereof. The seaweed nano-lime alkali comprises the following components in parts by weight:

[0044]

[0045]

[0046] The specific surface area of ​​the porous graphene is 651 m 2 / g, the average particle size of the aluminum oxide is 10 nm, the average particle size of the sodium hydroxide is 100 nm, and the average particle size of the sodium 1-naphthalenesulfonate is 100 nm.

[0047] The preparation method provided in this embodiment comprises the following steps:

[0048] (1) mixing natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, aluminum oxide, sodium hydroxide, sodium 1-naphthalenesulfonate and diatomaceous earth according to weight parts, and grinding to obtain a premix with an average particle size of 50 nm and a saturation magnetization of 10 emu / g;

[0049] (2) The premix obtained in step (1) is subjected to high-pressure homogenization for 20 minutes, and the mixing temperature of the high-pressure homogenization is controlled to be 70° C. and the mixing pressure is controlled to be 22 MPa, to obtain the seaweed nano-ash alkali.

[0050] Example 3

[0051] This embodiment provides a seaweed nano-lime alkali and a preparation method thereof. The seaweed nano-lime alkali comprises the following components in parts by weight:

[0052]

[0053]

[0054] The specific surface area of ​​the porous graphene is 483 m 2 / g, the average particle size of the calcium oxide is 500nm, the average particle size of the sodium phosphate is 500nm, and the average particle size of the aromatic sodium aminosulfonate is 500nm.

[0055] The preparation method provided in this embodiment comprises the following steps:

[0056] (1) mixing natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, calcium oxide, sodium phosphate, aromatic sodium aminosulfonate and diatomaceous earth according to weight proportions, and grinding to obtain a premix having an average particle size of 1500 nm and a saturation magnetization of 100 emu / g;

[0057] (2) The premix obtained in step (1) is subjected to high-pressure homogenization for 30 minutes, and the mixing temperature of the high-pressure homogenization is controlled to be 60° C. and the mixing pressure is controlled to be 19 MPa, to obtain the seaweed nano-ash alkali.

[0058] Example 4

[0059] This embodiment provides a seaweed nano-lime alkali and a preparation method thereof. Except that sodium carbonate is replaced with potassium nitrate of equal mass, the remaining steps and conditions are the same as those in Example 1, so they are not described here in detail.

[0060] Example 5

[0061] This embodiment provides a seaweed nano-lime alkali and a preparation method thereof. Except that sodium lignin sulfonate is replaced with an equal mass of sulfonated melamine formaldehyde resin (with a degree of polymerization of 3500), the remaining steps and conditions are the same as those in Example 1, so they are not repeated here.

[0062] Example 6

[0063] This embodiment provides a seaweed nano-ash alkali and a preparation method thereof. Except for changing the average particle size of the premix to 2000 nm by adjusting the grinding conditions described in step (1), the remaining steps and conditions are the same as those in Example 1 and are not described in detail here.

[0064] Example 7

[0065] This embodiment provides a seaweed nano-ash alkali and a preparation method thereof. Except that the mixing temperature of the high-pressure homogenization treatment in step (2) is changed to 50° C., the remaining steps and conditions are the same as those in Example 1 and are not described in detail here.

[0066] Example 8

[0067] This embodiment provides a seaweed nano-ash alkali and a preparation method thereof. Except that the mixing pressure of the high-pressure homogenization treatment in step (2) is changed to 15 MPa, the remaining steps and conditions are the same as those in Example 1, and therefore are not described in detail here.

[0068] Comparative Example 1

[0069] This comparative example provides a seaweed nano-ash alkali and a preparation method thereof. Except that sodium carboxymethyl cellulose is not added, the remaining steps and conditions are the same as those in Example 1, so they are not described here in detail.

[0070] Comparative Example 2

[0071] This comparative example provides a seaweed nano-ash alkali and a preparation method thereof. Except that porous graphene is not added, the remaining steps and conditions are the same as those in Example 1, so they are not described here in detail.

[0072] Comparative Example 3

[0073] This comparative example provides a seaweed nano-lime alkali and a preparation method thereof. Except that sodium carbonate is not added, the remaining steps and conditions are the same as those in Example 1, so they are not described in detail here.

[0074] Comparative Example 4

[0075] This comparative example provides a seaweed nano-ash alkali and a preparation method thereof. Except that sodium dodecylbenzene sulfonate is not added, the remaining steps and conditions are the same as those in Example 1, so they are not described here in detail.

[0076] Comparative Example 5

[0077] This comparative example provides a seaweed nano-lime alkali and a preparation method thereof. Except that sodium lignin sulfonate is not added, the remaining steps and conditions are the same as those in Example 1, so they are not described here in detail.

[0078] Performance Testing

[0079] 13 groups of sewage samples were prepared with 1L, and the pH of the sewage was controlled to be 6, the particle concentration was 10mg / L, and the chemical oxygen demand COD was 500mg / L. The seaweed nano-lime alkali obtained in Examples 1-8 and Comparative Examples 1-5 was added to the above 13 groups of sewage samples respectively, and the addition amount was 10g, and the seaweed nano-lime alkali was fully stirred to make the seaweed nano-lime alkali suspended and fully contacted with the sewage. After stirring for 5 hours, the pH value of the sewage, the concentration of residual particles and the chemical oxygen demand were detected. The relevant physical properties and decontamination test results of the seaweed nano-lime alkali are shown in Table 1 below.

[0080] Table 1

[0081]

[0082] It can be seen that the present invention achieves the purpose of efficiently removing pollutants from water bodies through the synergistic cooperation between specific components and seaweed ash. Among them, natural sea limestone helps to neutralize acidic substances and adjust the pH value of water bodies; sodium carboxymethyl cellulose can promote the aggregation of suspended particles in water, accelerate the sedimentation process through flocculation, and improve the transparency of water bodies; porous graphene has a very high specific surface area and enhances adsorption capacity; the activator can fully activate the potential activity of other components and enhance the effectiveness of the overall material; the descaling agent and seaweed ash work together to further improve the ability to remove dirt; the plasticizer is used to improve the plasticity of the material, making it easier to process and use; diatomaceous earth, as a porous material, provides additional adsorption surface area and fully removes suspended particles and organic matter in the water body. Compared with traditional water treatment methods, the seaweed nano-ash alkali provided by the present invention has lower costs and higher treatment efficiency, which is conducive to large-scale promotion and application.

[0083] In addition, the present invention achieves sufficient mixing and nano-sizing of the obtained products through the sequential mixing, grinding and high-pressure homogenization treatments, and the nano-scale particles have a larger specific surface area, which helps to improve the adsorption capacity and reaction activity of the material, and at the same time fully improves the uniformity and stability of the material in the water environment, avoiding the influence of excessively large particles on the water treatment effect, and ultimately improving the water treatment efficiency.

[0084] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A seaweed nano-lime alkali, It is characterized in that The components of the seaweed nano-ash alkali include natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, an activator, a descaling agent, a plasticizer and diatomaceous earth.

2. The seaweed nano-ash base according to claim 1, It is characterized in that The seaweed nano-ash base comprises the following components in parts by weight:

3. The seaweed nano-ash base according to claim 1 or 2, It is characterized in that The activator includes any one of sodium carbonate, aluminum oxide, potassium nitrate, cobalt dioxide, titanium dioxide, magnesium oxide or calcium oxide, or a combination of at least two thereof; Preferably, the average particle size of the activator is 10-500 nm.

4. The seaweed nano-ash base according to any one of claims 1 to 3, It is characterized in that The descaling agent includes any one or a combination of at least two of sodium dodecylbenzene sulfonate, sodium hydroxide, hydrochloric acid, citric acid, sodium phosphate or acrylic acid; Preferably, the average particle size of the descaling agent is 100-500 nm.

5. The seaweed nano-ash base according to any one of claims 1 to 4, It is characterized in that The plasticizer includes any one or a combination of at least two of lignin sulfonate, polycarboxylic acid, naphthalene sulfonate, aromatic aminosulfonate or sulfonated melamine formaldehyde resin; Preferably, the average particle size of the plasticizer is 100-500 nm.

6. A method for preparing seaweed nano-ash alkali as claimed in any one of claims 1 to 5, It is characterized in that The preparation method comprises the following steps: (1) mixing natural sea limestone, seaweed ash, sodium carboxymethyl cellulose, porous graphene, an activator, a descaling agent, a plasticizer and diatomaceous earth according to weight proportions, and grinding to obtain a premix; (2) subjecting the premix obtained in step (1) to high-pressure homogenization to obtain the seaweed nano-ash alkali.

7. The preparation method according to claim 6, It is characterized in that The grinding process in step (1) is performed until the average particle size of the premix is ​​50-1500 nm and the saturation magnetization is 10-100 emu / g.

8. The preparation method according to claim 6 or 7, It is characterized in that The mixing temperature of the high-pressure homogenization treatment in step (2) is 60-70° C., the mixing pressure is 19-22 MPa, and the treatment time is 20-30 min.

9. The preparation method according to any one of claims 6 to 8, It is characterized in that The preparation method comprises the following steps: (1) mixing 55-69 parts of natural sea limestone, 8-12 parts of seaweed ash, 3-7 parts of sodium carboxymethyl cellulose, 12-18 parts of porous graphene, 1-3 parts of activator, 2-5 parts of descaling agent, 1-3 parts of plasticizer and 1-3 parts of diatomaceous earth, and grinding to obtain a premix having an average particle size of 50-1500 nm and a saturation magnetization of 10-100 emu / g; (2) The premix obtained in step (1) is subjected to high-pressure homogenization for 20-30 min, and the mixing temperature of the high-pressure homogenization is controlled to be 60-70° C. and the mixing pressure is controlled to be 19-22 MPa to obtain the seaweed nano-ash alkali.

10. An application of the seaweed nano-ash alkali as claimed in any one of claims 1 to 5, It is characterized in that The seaweed nano-ash alkali is used for removing pollutants in water bodies.

Citation Information

Patent Citations

  • Heavy metal sewage treating agent

    CN107324415A

  • Composite oil adsorption material and preparation method and application thereof

    CN107442079A

  • Seawater desalination process

    CN116789331A

  • Water quality improvement module type cartridge

    JP3003524U