Nuclear power plant pipeline defect detection method
Through magnetic field sensors and ultrasonic detection technology, the problem of corrosion detection of rubber lining pipelines in nuclear power plants has been solved, comprehensive inspection of nuclear power plants has been achieved, defects have been discovered in the early stage, and system safety has been improved.
Patent Information
- Application Number
- CN202410874762.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-01
- Publication Date
- 2024-11-08
AI Technical Summary
The lining pipes in the three-loop system of the nuclear power plant are damaged and fall off due to factors such as process and long-term service, which causes seawater to corrode the metal matrix, lack of effective corrosion detection technology, affecting system safety.
A magnetic field sensor is used to collect magnetic signals on the surface of the pipeline, and the suspected defect area is determined through analysis, and ultrasonic detection is used for review to determine the existence and properties of the defect area.
A comprehensive and blind spot detection of nuclear power plant pipelines has been achieved, and the early detection of lining damage and metal corrosion has been detected, which avoids misjudgment and misjudgment, provides a basis for timely handling, and improves system safety.
Smart Images

Figure CN118914340A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of nuclear power plant pipelines, and in particular to a method for detecting corrosion of nuclear power plant pipelines. Background Art
[0002] The tertiary circuit of a nuclear power plant, also called the cooling circuit, is the ultimate heat sink of the nuclear power plant and plays an important role in the safe operation of the nuclear power plant. Its related systems need to resist seawater corrosion, so rubber-lined pipes are often used. However, due to factors such as the rubber lining process, long-term service, and fluid scouring, the rubber lining is damaged and falls off, and then the seawater directly corrodes the metal matrix, which in severe cases causes the pipeline to be perforated and the three-circuit system loses its integrity. Therefore, the integrity of these rubber-lined pipes determines the safety of the three-circuit system of the nuclear power plant to a certain extent. Nuclear power plants also attach great importance to the anti-corrosion management of these systems, and ensure the safety of these rubber-lined equipment through daily inspections and overhauls. However, daily inspections are mainly based on visual inspections, and there is a lack of a technical method for corrosion detection. Summary of the invention
[0003] The technical solution adopted by the present invention to solve its technical problem is: a method for detecting defects in nuclear power plant pipelines.
[0004] The technical solution adopted by the present invention to solve the technical problem is: the pipeline comprises a rubber lining layer, a metal layer and a coating layer arranged in sequence from the inside to the outside, and the rubber lining layer is bonded and connected to the metal layer; the method comprises the following steps:
[0005] S1: collecting magnetic signals on the surface of the pipeline to be inspected area through a magnetic field sensor, analyzing the magnetic signals, and obtaining suspected defect areas;
[0006] S2: Using ultrasonic testing to review the suspected defective area to determine whether the suspected defective area has defects, and if so, determine it as a defective area.
[0007] Preferably, S1 includes: the surface of the pipeline to be inspected area includes at least one block, the width of the block is a preset ratio of the magnetic field sensor coverage width, the magnetic signal of the block is collected by the magnetic field sensor, and the magnetic signal is analyzed to obtain a suspected defect area.
[0008] Preferably, collecting the magnetic signal of the block by the magnetic field sensor, analyzing the magnetic signal, and obtaining the suspected defect area includes: collecting the magnetic signal of the block at least once by the magnetic field sensor, analyzing each magnetic signal, and obtaining the suspected defect area.
[0009] Preferably, the analyzing each magnetic signal to obtain the suspected defect area includes: filtering each magnetic signal, extracting the low-frequency signal therein as a low-frequency scanning signal, and performing differential processing on all the low-frequency scanning signals to obtain the suspected defect area.
[0010] Preferably, the magnetic field sensor is a three-axis fluxgate sensor.
[0011] Preferably, the reviewing of the suspected defect area includes: reviewing the suspected defect area using an ultrasonic resonance review method.
[0012] Preferably, the verification method using ultrasonic resonance method comprises: performing ultrasonic detection on the suspected defect area according to emitting an ultrasonic signal with a preset pulse duration and a preset frequency domain scanning range.
[0013] Preferably, the method further comprises: performing ultrasonic thickness measurement on the defective area to determine the defect type of the defective area.
[0014] Preferably, the use of ultrasonic thickness measurement to perform thickness measurement detection on the defect position includes: emitting thickness measurement ultrasonic waves, collecting thickness measurement ultrasonic transmission waves, obtaining thickness measurement values and thickness measurement reflection waveform data of the defect area according to the thickness measurement ultrasonic transmission waves, and analyzing the thickness measurement values and the thickness measurement reflection waveform data to obtain the defect type of the defect area.
[0015] Preferably, the analyzing the thickness measurement value and the thickness measurement reflection waveform data to obtain the defect type of the defect area includes: judging whether the thickness measurement value is less than a preset pipe metal layer wall thickness value; if so, judging that the rubber lining layer is damaged and the metal layer is corroded; judging whether the thickness measurement value is equal to the preset pipe metal layer wall thickness value, and the reflection peak of the thickness measurement reflection waveform data is clear and evenly distributed in the time domain; if so, judging that the rubber lining layer is detached or bubbled, and the metal layer is not corroded; judging whether the thickness measurement value is unstable, and the reflection peak of the thickness measurement reflection waveform data has an accompanying peak phenomenon; if so, judging that the rubber lining layer is not firmly bonded or the rubber lining is missing but not damaged.
[0016] The implementation of the present invention has the following beneficial effects: The present invention relates to a method for detecting defects in pipelines of nuclear power plants, the method comprising: collecting magnetic signals on the surface of the pipeline to be inspected area by means of a magnetic field sensor, analyzing the magnetic signals to obtain a suspected defective area; reviewing the suspected defective area by means of ultrasonic detection to determine whether there is a defect in the suspected defective area, and if so, determining it as a defective area. The magnetic field sensor can realize comprehensive and blind-angle detection of the surface of the pipeline to be inspected area, effectively avoiding the limitations of visual inspection. By analyzing the magnetic signals, problems such as lining damage and metal corrosion can be discovered at an early stage, providing a basis for timely processing. Reviewing the suspected defective area by means of ultrasonic detection can more accurately determine the existence and nature of the defect, avoiding misjudgment and missed judgment. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solution of the present invention, the accompanying drawings required for use in the description of the present invention will be briefly introduced below. Obviously, the accompanying drawings in the following description are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0018] Figure 1 The present invention is a flowchart of a method for detecting pipeline defects in a nuclear power plant according to an embodiment;
[0019] Figure 2 An embodiment provides a schematic diagram of sample dimensions with rubber lining defects;
[0020] Figure 3 is an embodiment original signal curve;
[0021] Figure 4 is a curve after the differential processing of the embodiment signal;
[0022] Figure 5 An ultrasonic resonance waveform at a damaged rubber lining of an embodiment;
[0023] Figure 6 The present invention is an ultrasonic resonance waveform with a perfect rubber lining. DETAILED DESCRIPTION
[0024] In order to make the purpose, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0025] like Figure 1As shown, in some embodiments, the method does not need to be tested when the unit is shut down, and can be carried out in a time window outside the overhaul time of the unit or equipment, which can save the overhaul time cost. The pipeline applicable to the present invention includes a rubber lining layer, a metal layer and a coating arranged in sequence from the inside to the outside. The rubber lining layer is bonded to the metal layer, and the coating is sprayed on the metal layer. The coating does not need to be removed during detection. The coating is about 0.2mm. In the present invention, a metal layer is arranged under the coating. The metal layer can be specifically made of carbon steel material, and under the carbon steel layer, a rubber lining layer is further arranged to enhance the stability and sealing of the structure. The damage of the coating can be easily found by general visual inspection. The detection of the metal layer and the rubber lining layer includes: S1: collecting the magnetic signal on the surface of the pipeline to be inspected area through a magnetic field sensor, analyzing the magnetic signal, and obtaining a suspected defect area; S2: using ultrasonic detection to review the suspected defect area to determine whether the suspected defect area has defects, and if so, it is determined to be a defect area. In order to more accurately detect the conditions of the metal layer and rubber lining layer under the coating, the present invention adopts a passive magnetic detection method, which does not require additional magnetization operations on the pipeline. The probe structure is simple, which greatly reduces the requirements for detection space, making the detection process more convenient and efficient.
[0026] Specifically, the method uses a magnetic field sensor to collect magnetic signals from the surface of the pipeline area to be inspected, and captures the magnetic signal distortion caused by pipeline defects. The suspected defect area is preliminarily determined by magnetic signal distortion, and then ultrasonic detection technology is used to review these areas. If the ultrasonic detection confirms the existence of defects, the area will be officially determined as a defective area. The present invention has no requirements on the outer diameter of the pipeline when inspecting the pipeline. It is suitable for small-diameter pipelines that cannot be entered for inspection by people. This method is also fully applicable to large-diameter pipelines with complex structures that cannot be reached by manpower, providing a daily pipeline inspection method for nuclear power plants.
[0027] In some embodiments, in order to more accurately simulate the detection environment of the actual pipeline and optimize the detection effect, the present invention manufactures a simulation part of the pipeline to be inspected for simulating defects. The types of rubber lining defects for pipelines with different metal wall thicknesses are formulated as shown in Table 1. By utilizing the electromagnetic and acoustic properties of the pipeline to be inspected, various types of defects that may occur in the pipeline are simulated, such as debonding, lack of meat, and bubbling. When the rubber lining on the pipeline is damaged or debonded, there are two main factors that affect the magnetic signal distribution near the surface of the pipeline. One is that the local stress distribution state is changed, and the other is that the local structure changes, which has a very weak effect on the magnetic field distribution. By using a high-precision magnetic sensor, the magnetic field distribution state near the surface is detected and scanned and drawn. By analyzing the abnormal magnetic field distribution, the abnormal point of the rubber lining is determined. The pipeline can be regarded as a double-layer structure of metal and rubber lining. Compared with a single-layer metal, the rubber lining changes the overall acoustic properties, and defects such as debonding and bubbling are equivalent to introducing an air layer between the metal and rubber lining, which is different from the acoustic properties of the intact rubber lining. The damaged rubber lining also changes the acoustic characteristics of the pipeline. Sound waves are reflected and transmitted at different interfaces between the two media. If the rubber lining is damaged and debonded, the transmittance is significantly lower than the transmittance when the rubber lining is intact. This difference can be used to confirm the location of the rubber lining defect. Through the detection of simulated parts, the minimum detection accuracy and effect of the detection method can be clarified, providing strong support for subsequent actual detection.
[0028] Table 1
[0029]
[0030]
[0031] In one embodiment, during the pipeline detection process, the surface of the pipeline to be inspected is first divided into several blocks, and the width of each block is determined by presetting a suitable ratio according to the coverage width of the magnetic field sensor. Specifically, the scanning intervals can be divided on the surface of the pipeline to be inspected according to the width that the sensor can cover. Usually, the width of these intervals will be set to 80% of the sensor coverage width to ensure that the sensor can fully scan each block. When all the equipment is properly connected, the staff will record the specific location of the detection function and the number of the detection file on the computer, and confirm that the surface condition of the pipeline to be inspected meets the detection requirements to ensure the accuracy and effectiveness of the detection. Next, the magnetic field sensor is used to collect magnetic signals from each block. The sensor will capture the magnetic signal distortion caused by potential defects inside the pipeline. Then, by conducting in-depth analysis of these magnetic signals, it can be preliminarily determined which blocks may have defects, that is, suspected defect areas. These suspected defect areas will be the focus of subsequent further detection.
[0032] In one embodiment, collecting magnetic signals of a block by means of a magnetic field sensor, analyzing the magnetic signals, and obtaining suspected defective areas includes: collecting magnetic signals of a block at least once by means of a magnetic field sensor, analyzing the magnetic signals each time, and obtaining suspected defective areas.
[0033] Specifically, first, in order to verify the performance of the magnetic field sensor, the sensor is placed on a carbon steel plate and gradually lifted. At this time, it should be observed that the display signal shows an exponential downward trend, which proves that the sensor can respond normally to changes in the magnetic field. Next, the probe is placed close to the surface of the carbon steel plate and scanned evenly from one side of the steel plate to the other. In this process, the absolute value of the tangential signal should show a trend of decreasing first and then increasing, because the magnetic field distribution changes with the movement of the probe position. Before officially starting the test, it is necessary to ensure that the surface state of the object to be tested is clean, without any foreign protrusions or corrosion products, to ensure the accuracy of the test results. After clicking to start the test, the operator should push the sensor to scan the surface of the pipeline at a uniform speed and pay close attention to the changes in the signal. If a defect signal is found on the test cloud map, the suspected defect position should be scanned back and forth at least three times, and it should be confirmed that the corresponding defect signal appears in each scan, so as to accurately mark the defect position. After completing a scanning interval, the above scanning steps should be repeated in the next interval until the entire pipeline surface is scanned. In this way, potential defects on the pipeline can be detected comprehensively and accurately.
[0034] In one embodiment, electromagnetic noise is a problem that cannot be ignored during the actual measurement process. These noises are not only numerous, but may also cover up weak defect signals, resulting in an insufficient signal-to-noise ratio for detection. In order to solve this problem, two strategies are adopted. The first is to suppress environmental noise. Specifically, the sensor and the signal transmission line are covered with an electromagnetic shielding layer to reduce the interference of the external electromagnetic field on the signal. This can reduce the noise level to a certain extent and improve the purity of the signal. The second is to identify and eliminate environmental noise from the perspective of signal processing. It is known that noise signals are often high-frequency, while magnetic signals are stable low-frequency signals. Therefore, the signal can be pre-processed at the hardware level through filtering design to filter out high-frequency noise. At the same time, at the software level, the uploaded acquisition signal is further processed, and a pure detection signal is further extracted through algorithm optimization and data analysis. In particular, this method adopts the second strategy to suppress noise. Specifically, each magnetic signal is filtered and processed, and the low-frequency signal therein is extracted as a low-frequency scanning signal. Subsequently, all low-frequency scanning signals are differentially processed to identify possible defect areas. The above strategy significantly improves the signal-to-noise ratio of the detection, thereby more accurately identifying the suspected defect areas in the pipeline. This improvement not only improves the accuracy of the detection, but also enhances the reliability and practicality of the detection method.
[0035] In one embodiment, a three-axis fluxgate sensor is used for magnetic field detection. This sensor has a wide range of more than 10Gs and a very high resolution of 5nT, ensuring the accuracy and precision of the detection. By integrating the magnetic induction intensity vectors of the X and Y direction components, the normal magnetic field intensity and tangential magnetic field intensity of the pipeline surface can be intuitively displayed on the detection interface, providing strong data support for subsequent defect detection.
[0036] In one embodiment, the verification method of the ultrasonic resonance method is used to verify the suspected defect area. In one embodiment, the suspected defect area is detected by ultrasonic detection based on the ultrasonic signal of the preset pulse duration and the preset frequency domain scanning range. Specifically, a vertically incident ultrasonic probe is placed on one side of the metal layer, and the duration of the ultrasonic pulse is set to 10 microseconds. Under this condition, due to multiple reflections of the pulse, aliasing may occur between the bottom surface reflection echoes. When the phases of these reflected waves are the same, they will be superimposed in the same phase, resulting in a great enhancement of the amplitude of the signal, which is the so-called resonance phenomenon. In order to conduct an in-depth analysis of the resonance phenomenon, the frequency domain scanning range can be set to 1 to 9 MHz. According to the actual detection situation, a certain section of the curve within this frequency range can be intercepted for detailed resonance analysis. In this way, it is possible to more accurately determine whether there are defects inside the metal plate and determine the specific location and size of the defects.
[0037] In one embodiment, the method further includes: performing ultrasonic thickness measurement on the defective area to determine the defect type of the defective area.
[0038] In one embodiment, the process of using ultrasonic thickness measurement technology to measure the thickness of the defect position is as follows: First, transmit the thickness measurement ultrasonic wave, which will pass through the material being measured and encounter the internal defects. Then, collect the returned thickness measurement ultrasonic transmission wave (also called reflection wave). By analyzing the reflection wave, the thickness measurement value of the defect area and the corresponding thickness measurement reflection waveform data can be obtained. These thickness measurement values and thickness measurement reflection waveform data are deeply analyzed. By comparing and analyzing these data, the defect type of the defect area can be determined.
[0039] In one embodiment, when analyzing the thickness measurement value and the thickness measurement reflection waveform data, the defect type of the defect area can be determined by the following steps: First, determine whether the thickness measurement value is less than the preset pipe metal layer wall thickness value. If the thickness measurement value is less than this preset value, it can be preliminarily determined that the rubber lining layer has been damaged and the metal layer has been corroded. Secondly, check whether the thickness measurement value is equal to the preset pipe metal layer wall thickness value, and at the same time observe whether the reflection peak of the thickness measurement reflection waveform data is clear and whether the distribution interval in the time domain is uniform. If both conditions are met, it can be inferred that the rubber lining may have fallen off or bubbled, but the metal layer has not been corroded. Finally, analyze whether the thickness measurement value is unstable, and observe whether the reflection peak of the thickness measurement reflection waveform data has a companion peak phenomenon. If the thickness measurement value is unstable and the reflection peak has a companion peak, it can be determined that the rubber lining may have a loose bond or the rubber lining is missing but not damaged. Through the above analysis steps, the defect type of the defect area can be determined more accurately, providing an important basis for subsequent maintenance and treatment.
[0040] like Figure 2 Method verification: In order to verify the accuracy of the detection method, a 250mm×250mm rubber-lined steel plate was selected as the experimental object. A Φ10mm circular hole was artificially cut out in the center of the rubber-lined surface of the steel plate to simulate the real rubber-lined defect. Figure 2 As shown in the figure. Two mutually perpendicular scanning directions are marked on the sample to enable comprehensive inspection from the carbon steel surface. First, the magnetic sensor is scanned from the lower left corner to the upper right corner and from the lower right corner to the upper left corner. Subsequently, ultrasonic inspection is performed on the carbon steel surface using the ultrasonic method to observe the signal characteristics.
[0041] like Figure 3 and Figure 4 As shown in the experimental results: The scanning results based on the magnetic sensor are as follows Figure 3 shown. Figure 3 The original signal of the scan is shown in the figure. It can be seen from the figure that there is an obvious signal anomaly in the middle part of the original signal. In order to make the defect signal more prominent, the original signal is differentially processed. The processing results are shown in the figure below. Figure 4 As shown. From the signal after differential processing, it can be clearly seen that the signal changes on two channels are the most significant. Combining the position of the defect on the rubber lining board and the position of the defect signal on the scanning curve, and through multiple scanning confirmations at the defect position, it is confirmed that the signal distortion is indeed caused by the rubber lining defect.
[0042] like Figure 5 and Figure 6 As shown in the figure, the ultrasonic resonance method was used to measure the resonance signals of the rubber lining defects and the rubber lining intact areas on the side of the carbon steel plate. Figure 5This is the ultrasonic resonance waveform at the damaged part of the rubber lining. Figure 6 The ultrasonic resonance waveform of the rubber lining is intact. The results show that when the rubber lining is damaged, the resonance signal is stronger than when the rubber lining is intact, which is consistent with the reflection resonance principle. This result further verifies the effectiveness and accuracy of the detection method in identifying rubber lining defects.
[0043] The present invention relates to a method for detecting defects in pipelines of nuclear power plants, the method comprising: collecting magnetic signals on the surface of a pipeline to be inspected area by means of a magnetic field sensor, analyzing the magnetic signals to obtain a suspected defective area; and rechecking the suspected defective area by means of ultrasonic detection to determine whether the suspected defective area has defects, and if so, determining it as a defective area. The magnetic field sensor can realize comprehensive and blind-angle detection of the surface of the pipeline to be inspected area, effectively avoiding the limitations of visual inspection. By analyzing the magnetic signals, problems such as lining rubber damage and metal corrosion can be discovered at an early stage, providing a basis for timely processing. Rechecking the suspected defective area by means of ultrasonic detection can more accurately determine the existence and nature of defects, avoiding misjudgment and missed judgment.
[0044] It can be understood that the above embodiments only express the preferred implementation modes of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, the above technical features can be freely combined without departing from the concept of the present invention, and several deformations and improvements can be made, which all belong to the protection scope of the present invention. Therefore, all equivalent changes and modifications made to the scope of the claims of the present invention should belong to the coverage of the claims of the present invention.
Claims
1. A method for detecting defects in pipelines of a nuclear power plant, wherein the pipeline comprises a rubber lining layer, a metal layer and a coating layer arranged in sequence from the inside to the outside, wherein the rubber lining layer is bonded to the metal layer, and wherein: include: S1: collecting magnetic signals on the surface of the pipeline to be inspected area through a magnetic field sensor, analyzing the magnetic signals, and obtaining suspected defect areas; S2: Using ultrasonic testing to review the suspected defective area to determine whether the suspected defective area has defects, and if so, determine it as a defective area.
2. The method for detecting defects in nuclear power plant pipelines according to claim 1, characterized in that: The S1 includes: The surface of the pipeline to be inspected area includes at least one block, the width of the block is a preset ratio of the magnetic field sensor coverage width, the magnetic signal of the block is collected by the magnetic field sensor, and the magnetic signal is analyzed to obtain a suspected defect area.
3. The method for detecting defects in nuclear power plant pipelines according to claim 2, characterized in that: The collecting of magnetic signals of the block by the magnetic field sensor and analyzing the magnetic signals to obtain suspected defect areas include: The magnetic signal of the block is collected at least once by a magnetic field sensor, and each magnetic signal is analyzed to obtain a suspected defect area.
4. The method for detecting defects in nuclear power plant pipelines according to claim 3, characterized in that: The suspected defect areas obtained by analyzing each magnetic signal include: Each magnetic signal is filtered, a low-frequency signal is extracted as a low-frequency scanning signal, and all the low-frequency scanning signals are differentially processed to obtain a suspected defect area.
5. The method for detecting defects in nuclear power plant pipelines according to claim 1, characterized in that: include: The magnetic field sensor is a three-axis fluxgate sensor.
6. The method for detecting defects in nuclear power plant pipelines according to claim 1, characterized in that: The review of the suspected defect area includes: The suspected defect area is reviewed by using an ultrasonic resonance review method.
7. The method for detecting defects in nuclear power plant pipelines according to claim 6, characterized in that: The verification method using ultrasonic resonance method comprises: The suspected defect area is ultrasonically inspected based on the emission of an ultrasonic signal with a preset pulse duration and a preset frequency domain scanning range.
8. The method for detecting defects in nuclear power plant pipelines according to claim 6, characterized in that: Also includes: An ultrasonic thickness measurement is performed on the defective area to determine the defect type of the defective area.
9. The method for detecting defects in nuclear power plant pipelines according to claim 8, characterized in that: The use of ultrasonic thickness measurement to measure the thickness of the defect position includes: Transmit thickness measurement ultrasonic waves, collect thickness measurement ultrasonic transmission waves, obtain thickness measurement values and thickness measurement reflection waveform data of the defect area according to the thickness measurement ultrasonic transmission waves, and analyze the thickness measurement values and the thickness measurement reflection waveform data to obtain the defect type of the defect area.
10. The method for detecting defects in nuclear power plant pipelines according to claim 9, characterized in that: The defect type of the defect area obtained by analyzing the thickness measurement value and the thickness measurement reflection waveform data includes: Determine whether the thickness value is less than a preset pipe metal layer wall thickness value. If so, it is determined that the rubber lining layer is damaged and the metal layer is corroded. Determine whether the thickness measurement value is equal to the preset pipe metal layer wall thickness value, and whether the reflection peak of the thickness measurement reflection waveform data is clear and evenly distributed in the time domain; if so, it is determined that the rubber lining layer is falling off or bubbling, and the metal layer is not corroded; It is determined whether the thickness measurement value is unstable and whether the reflection peak of the thickness measurement reflection waveform data has a companion peak phenomenon; if so, it is determined that the rubber lining layer is not firmly bonded or the rubber lining is missing but not damaged.