Ceramic production process parameter control method

The ceramic blanks are prepared through the ball milling mechanism and the firing parameters are optimized using database and wavelet transformation technology, which solves the problem of inaccurate temperature control in traditional ceramic firing processes, improves the ceramic firing accuracy and efficiency, and improves the yield rate.

CN118915671AActive Publication Date: 2024-11-08CHAOZHOU DAXIN CRAFT FACTORY CO LTD

Patent Information

Application Number
CN202411074503.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-11-08
Estimated Expiration
2044-08-07

AI Technical Summary

Technical Problem

Traditional ceramic firing processes rely on the operator's experience, resulting in insufficient precision in firing temperature control, affecting product quality, and are time-consuming and error-prone, reducing production efficiency and cost-effectiveness.

Method used

The ceramic blank is prepared by using the ball milling mechanism. By obtaining the characteristic parameters of the blank and performing cluster analysis with the historical database, an initial firing scheme is generated, and the temperature change trend is extracted using wavelet transformation, real-time monitoring and comparison of the actual and reference curves, and firing parameters are adjusted. , combine image processing and defect recognition technology to compensate and optimize the firing solution.

Benefits of technology

It improves firing accuracy and process efficiency, predicts the quality of finished ceramic products in advance, reduces waste of manpower and material resources, and improves yield and process energy efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118915671A_ABST
    Figure CN118915671A_ABST
Patent Text Reader

Abstract

The invention discloses a ceramic production process parameter control method which comprises the following steps: performing compression molding on a blank to obtain a ceramic blank, and performing clustering analysis according to the ceramic blank and a database to obtain an initial firing scheme which comprises a reference temperature change curve and reference heat preservation time of each firing stage; acquiring an actual temperature change curve of the current stage, and extracting a main trend by adopting wavelet transform so as to divide the actual curve and the reference curve into a plurality of curve segments; based on each curve segment, respectively determining a first change trend of the actual curve and a second change trend of the reference curve, calculating trend similarity, calculating data similarity of each temperature data on the actual curve and the reference curve, and determining target similarity according to the trend similarity and the data similarity; and if the target similarity is greater than a first preset threshold value, executing the next firing stage according to the initial firing scheme. Through real-time monitoring and parameter adjustment, the effects of improving the firing precision, enhancing the product quality stability and improving the production efficiency are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of ceramic production, and in particular to a method for controlling process parameters of ceramic production. Background Art

[0002] Traditional ceramic firing processes usually rely on the operator's experience and manual adjustment, that is, before firing, a rough firing plan is made based on past experience, and then during the firing process, the temperature is adjusted and controlled by manual observation and actual conditions. However, relying on the operator to manually adjust the temperature during the firing process will result in inaccurate control of the firing temperature, which is easily affected by personal experience. The fluctuation of the firing temperature will lead to unstable product quality, thus affecting the yield rate; in addition, this manual adjustment is not only time-consuming and error-prone, but also reduces production efficiency and cost-effectiveness. Summary of the invention

[0003] In order to solve at least one of the above-mentioned technical problems, the present invention provides a method for controlling process parameters of ceramic production.

[0004] The present invention provides a method for controlling process parameters of ceramic production, the method comprising:

[0005] A ball mill is used to prepare a ceramic blank, and the prepared blank is pressed and formed to obtain a ceramic body;

[0006] Acquire characteristic parameters of the ceramic body and a database generated according to a historical ceramic preparation process, perform cluster analysis on the characteristic parameters and the database, and obtain an initial firing scheme for the ceramic body, wherein the initial firing scheme includes a reference temperature change curve and a reference holding time at each firing stage;

[0007] Obtaining an actual temperature change curve of the ceramic in the current firing stage and a corresponding reference temperature change curve as an actual curve and a reference curve; extracting the temperature change trends of the actual curve and the reference curve by wavelet transform, so as to divide the actual curve and the reference curve into a plurality of curve segments;

[0008] Determine a first change trend of each curve segment in the actual curve and a second change trend of each curve segment in the reference curve; calculate the trend similarity of the first change trend and the second change trend, and calculate the data similarity of each temperature data on the actual curve and the reference curve, and determine the target similarity according to the trend similarity and the data similarity;

[0009] It is determined whether the target similarity is greater than a first preset threshold value. If the target similarity is greater than the first preset threshold value, the next firing stage is executed according to the initial firing scheme.

[0010] Preferably, the method further comprises:

[0011] If the target similarity is less than or equal to a first preset threshold, calculating a deviation between the target similarity and the first preset threshold, and determining whether the deviation is within a preset range;

[0012] If yes, the reference temperature change curve and the reference holding time of the next firing stage in the initial firing plan are optimized, and the next firing stage is executed according to the optimized firing plan;

[0013] If not, the firing process of the current ceramic body is stopped and a new ceramic body is replaced for firing.

[0014] Preferably, before executing the next firing stage according to the optimized firing scheme, the method further includes:

[0015] Acquire the ceramic product image after the current firing stage is completed, perform denoising, image enhancement and grayscale processing on the ceramic product image to obtain a grayscale image;

[0016] Extract features from grayscale images, including texture features, edge features, and spectral features; input the extracted features into the preset RNN model for defect recognition and generate recognition results;

[0017] The optimized firing scheme is compensated according to the identification results.

[0018] Preferably, compensating the optimized firing scheme according to the recognition result comprises:

[0019] Determining defect types according to the recognition results, wherein the defect types include cracks, bubbles, and uneven colors;

[0020] Performing correlation analysis on the defect type and the reference temperature change curve and reference holding time of the current firing stage in the initial firing scheme, and screening out the target defect type with a correlation greater than a second preset threshold value;

[0021] The firing temperature and holding time to be adjusted are determined according to the target defect type, and the optimized firing scheme is compensated according to the firing temperature and holding time to be adjusted.

[0022] Preferably, the pressure during the compression molding is:

[0023] P=C(ρ g -ρ0) n

[0024] In the formula, P represents pressure, C represents the response degree of the ceramic blank to pressure, and ρ g represents the target density of the ceramic body after pressing, ρ0 represents the density of the ceramic body before pressing, and n represents the relationship between the density of the body and the pressure, satisfying 2≤n≤5.

[0025] Preferably, the characteristic parameters include the material type and actual density of the ceramic body and the theoretical density of the finished ceramic product.

[0026] Preferably, the method further comprises:

[0027] After all firing stages are completed to obtain a finished ceramic product, the quality parameters of the current finished ceramic product are obtained, and the initial firing plan for the next ceramic production is determined according to the quality parameters;

[0028] The quality parameters of the finished ceramic product include dimensional change, porosity and tensile strength.

[0029] Preferably, determining the initial firing scheme for the next ceramic production according to the quality parameters comprises:

[0030] Establish a multi-objective optimization function for firing temperature, holding time and heating rate, and establish corresponding constraints based on dimensional change, porosity and tensile strength;

[0031] The multi-objective optimization function is solved according to the firefly algorithm, and the initial firing plan for the next ceramic production is determined according to the solution result.

[0032] Compared with the prior art, the present invention has the following beneficial effects:

[0033] 1) The present invention uses the characteristic parameters of the ceramic body and the historical database for cluster analysis to obtain an initial firing plan suitable for the current body, so that a reference can be quickly provided for the current firing plan to make it more consistent with the characteristics of the actual body. The trend of the actual temperature change curve and the reference curve is extracted by wavelet transform, so as to accurately divide the curve segments. When comparing the reference curve and the actual curve, the temperature trends of different curve segments can be more finely compared, so as to more accurately find deviations and match corresponding processing strategies, thereby improving firing accuracy and accelerating process efficiency.

[0034] 2) When comparing the reference curve and the actual curve, the present invention will compare the similarity of the change trend of each curve segment, and will also combine the data similarity of the discrete temperature points in the curve segment, so as to determine the target similarity according to the trend similarity and the data similarity, and compare the target similarity with the first preset threshold after obtaining it. If it is greater than the first preset threshold, it means that the current actual firing temperature is normal, and the next firing stage can be executed according to the initial firing scheme. On the contrary, if it is less than or equal to the first preset threshold, it means that the actual firing process is abnormal. At this time, the deviation between the target similarity and the first preset threshold is determined to determine whether the deviation is within the preset range. If so, the reference temperature change curve and the reference holding time of the next firing stage in the initial firing scheme are adjusted before executing the next firing stage. If not, it means that the current firing abnormality cannot be remedied, so there is no need to continue firing, and another blank can be replaced and fired again. The present invention can timely discover the deviation and make adjustments by monitoring the actual temperature change in real time and comparing it with the reference curve. By considering the similarity of continuous trend change and the similarity of discrete values, the difference between the actual curve and the reference curve can be analyzed more accurately. When it is found that the deviation range is controllable, it can be remedied by adjusting the parameters in the next stage. Conversely, if the deviation is uncontrollable, there is no need to continue wasting manpower and material resources to replace the new body and re-fire it. In this way, the quality of the finished ceramic product can be predicted in advance, and when the firing problem is irreversible, it can be replaced in time to avoid wasting energy, thereby greatly improving the process energy efficiency of ceramic processing.

[0035] 3) After obtaining the finished ceramic product, the present invention will obtain the quality parameters of the current finished ceramic product, establish constraints based on the quality parameters, establish constraints based on the temperature, insulation time and heating rate in the firing plan, and determine the initial firing plan before the next ceramic firing by optimizing. Through this self-learning feedback control and adjustment mechanism, the quality of ceramic firing is continuously improved, and ultimately the yield rate of the entire ceramic firing process is greatly improved.

[0036] It is to be understood that both the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the disclosure. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the technical solutions in the embodiments of the present invention or the background technology, the drawings required for use in the embodiments of the present invention or the background technology will be described below.

[0038] The drawings herein are incorporated into the specification and constitute a part of the specification. These drawings illustrate embodiments consistent with the present disclosure and are used to illustrate the technical solutions of the present disclosure together with the specification.

[0039] Figure 1 A schematic diagram of a process flow of a ceramic production process parameter control method provided by an embodiment of the present invention;

[0040] Figure 2 A comparative analysis diagram of an actual curve of temperature variation over time and a reference curve provided in an embodiment of the present invention;

[0041] Figure 3 A schematic flow chart of a ceramic production process parameter control method provided by another embodiment of the present invention;

[0042] Figure 4 The embodiment of the present invention provides Figure 3 A schematic flow chart of the sub-steps of step S80;

[0043] Figure 5 The embodiment of the present invention provides Figure 4 Schematic diagram of the flow of sub-steps of step S803. DETAILED DESCRIPTION

[0044] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0045] It should be noted that ceramic production mainly includes the following links:

[0046] 1) Material preparation: Select appropriate raw materials such as clay, quartz, feldspar, etc. according to the performance requirements of the required ceramics; mix the various raw materials evenly according to the formula ratio;

[0047] 2) Blank making: Processing the ceramic raw materials into clay and forming them through slip injection, dry pressing, manual throwing, etc. to obtain a blank;

[0048] 3) Drying: remove moisture from the green body to prevent cracking during firing;

[0049] 4) Trimming: Trim the dried green body to achieve the desired shape and surface smoothness.

[0050] 5) Biscuit firing: gradually raise the temperature from room temperature, keep it at high temperature for a period of time to ensure that the green body is completely sintered, and then slowly cool it to room temperature;

[0051] 6) Glazing: After bisque firing and when the ceramic body is completely cooled, the surface of the ceramic body is covered with glaze by dipping, spraying, brushing, etc.

[0052] 7) Glaze firing: The glazed green body is fired at high temperature in a kiln to harden it and form a glassy surface.

[0053] At present, the quality control of each link in ceramic production mostly relies on manual experience, such as raw material preparation, molding and drying, and temperature control of firing schemes, which leads to unsatisfactory yield. To this end, the present invention provides a ceramic production process parameter control method, which improves the process efficiency and yield rate by accurately controlling the temperature at different firing stages, and greatly increases the process energy efficiency of ceramic preparation.

[0054] See also Figure 1 , Figure 1 A flow chart of a ceramic production process parameter control method provided by an embodiment of the present invention. Figure 1 As shown, the method comprises the following steps:

[0055] S10, using a ball mill to prepare a ceramic blank, and pressing the prepared blank to obtain a ceramic body.

[0056] In this embodiment, the required raw materials, such as alumina powder, adhesives and other additives, are first placed in a ball mill. The raw materials are ground by steel balls or other types of grinding media in the ball mill to achieve the desired particle size distribution and uniform mixing. Then, an appropriate amount of water or other solvent is added to form a slurry with a certain fluidity, and the prepared slurry is dried to an appropriate water content for subsequent molding. Finally, a pressing device is used to press the dried blank into the desired shape and size to form a ceramic body.

[0057] In one embodiment, the pressure during the compression molding is:

[0058] P=C(ρ g -ρ0) n

[0059] In the formula, P represents pressure, C represents the response degree of the ceramic blank to pressure, and ρ g represents the target density of the ceramic body after pressing, ρ0 represents the density of the ceramic body before pressing, and n represents the relationship between the density of the body and the pressure, satisfying 2≤n≤5.

[0060] The above formula describes the relationship between pressure and density of ceramic green body during the pressing process. C represents the degree of response of ceramic green body to pressure, which is a constant related to material properties, and n represents the exponent of the nonlinear relationship between green body change and pressure. By selecting the appropriate pressing pressure P, it can be ensured that the final product has the expected density, which is crucial to ensure the performance of ceramic materials. Since C and n are parameters related to material properties, experimental determination of these parameters can better understand the behavior of the material and optimize the pressing process accordingly. This helps to reduce trial and error costs and improve production efficiency. In addition, by accurately evaluating the pressure, defects such as voids and cracks inside the green body can be effectively reduced, the density and uniformity of the green body can be improved, and the quality of the final product can be significantly improved by precisely controlling the density.

[0061] S20, obtaining characteristic parameters of the ceramic body and a database generated according to the historical ceramic preparation process, performing cluster analysis on the characteristic parameters and the database, and obtaining an initial firing plan for the ceramic body, wherein the initial firing plan includes a reference temperature change curve and a reference holding time for each firing stage.

[0062] First of all, the firing stage is mainly divided into the following stages:

[0063] Drying: During this stage, the ceramic body is left at room temperature to remove most of the water in it. This process can occur naturally or be accelerated by heating.

[0064] Bisque firing: After being completely dried, the ceramic body is placed in a kiln for preliminary firing, usually called bisque firing or first firing. The temperature is generally between 900 and 1100 degrees Celsius. The purpose of bisque firing is to harden the ceramic body and make it stronger for subsequent processing such as glazing.

[0065] Glazing: After bisque firing, the ceramic body is coated with a layer of glaze. Glaze is a glassy material that melts at high temperatures to form a smooth and waterproof surface.

[0066] Glaze firing: The glazed ceramic body is placed back into the kiln for a second firing, this time usually at a higher temperature, which can reach over 1000 to 1300 degrees Celsius. During the glaze firing process, the glaze melts and combines with the ceramic surface to form a shiny surface.

[0067] The firing temperature control curve is usually designed including:

[0068] Preheating stage: from room temperature to low temperature. This stage is mainly to remove moisture from the blank to avoid cracking. The temperature rise rate should not be too fast. A holding time can be set to ensure uniform heating.

[0069] Sintering stage: According to the material characteristics, the temperature is gradually raised to the firing temperature. This stage is the critical period for the physical and chemical changes of the ceramic material. The appropriate heating rate and firing temperature need to be determined based on the sintering characteristics of the material.

[0070] Insulation stage: After reaching the predetermined firing temperature, maintain it for a certain period of time to ensure sufficient sintering and enhance the mechanical strength and stability of the ceramic. The insulation time is adjusted according to the type and thickness of the ceramic.

[0071] Cooling stage: Slowly cool down to prevent the product from generating stress and cracking due to sudden temperature changes. Especially for large or thick-walled products, special attention should be paid to the cooling rate.

[0072] In this embodiment, the characteristic parameters of the ceramic body are first obtained. Preferably, the characteristic parameters include the material type, actual density and theoretical density of the ceramic body. The material type determines the basic chemical composition of the body. The actual density is obtained by measuring the mass and volume of the body. The theoretical density is the density value when the material is fully densified, which can usually be found in the material manual.

[0073] Then, a database generated based on the historical ceramic preparation process is obtained. When building this database, historical data needs to be obtained from literature, experimental records or other sources. Then data preprocessing is performed, including cleaning the data, removing outliers, and unifying units and formats. Finally, key features related to the ceramic firing process, such as temperature curves, holding time, etc., are extracted, and the initial body density and the finished product density after firing are recorded for different ceramic material types.

[0074] Furthermore, the characteristic parameters are clustered with the database to obtain the initial firing plan of the ceramic body.

[0075] In the present embodiment, any clustering algorithm such as K-means, hierarchical clustering or DBSCAN can be used to cluster based on characteristics such as material type, actual density and theoretical density. When clustering, the number of clusters is first determined, and then the data points in the database are assigned to different clusters. According to the clustering results, the corresponding production process in the database can be found to obtain the initial firing scheme. Specifically, the initial firing scheme includes a reference temperature change curve and a reference insulation time for each firing stage. The reference temperature curve is defined based on the typical temperature change pattern of each cluster. The reference insulation time is determined based on the average insulation time of each stage in the historical data. The firing process is divided into three stages: heating, insulation and cooling, and the reference temperature and time of each stage are given.

[0076] S30, obtaining an actual temperature change curve of the ceramic in the current firing stage and a corresponding reference temperature change curve as the actual curve and the reference curve; using wavelet transform to extract the temperature change trends of the actual curve and the reference curve to divide the actual curve and the reference curve into multiple curve segments.

[0077] Specifically, the current firing stage is first determined, for example, the bisque firing stage, and then the temperature change during the firing process is monitored in real time by a sensor, and the actual temperature data change curve over time is recorded, and based on the initial firing scheme obtained after the aforementioned cluster analysis, a reference temperature change curve of the bisque firing stage is matched therefrom. For the convenience of description, the actual temperature change curve and the corresponding reference temperature change curve are referred to as the actual curve and the reference curve, respectively.

[0078] Furthermore, wavelet transform technology is used to extract the main trend of the temperature change curve. Wavelet transform can capture the local characteristics of the signal and is very suitable for processing such non-stationary signals. According to the results of wavelet transform, the actual curve and the reference curve are divided into multiple curve segments. Each segment represents a main trend of temperature change.

[0079] See also Figure 2 , Figure 2 A comparative analysis chart of the reference curve and the actual curve is provided. Figure 2 In the figure, curve ABCD represents the reference curve of temperature variation over time, while abcd represents the actual curve of temperature variation over time. The main features of the two variation curves can be extracted through wavelet transformation to determine the trend, thereby dividing the reference curve and the actual curve into three segments, where the trends of the AB and ab segments are both rising; the BC and bc segments are falling, and the CD and cd segments are rising.

[0080] S40, determining a first change trend of each curve segment in the actual curve and a second change trend of each curve segment in the reference curve; calculating trend similarity between the first change trend and the second change trend, and calculating data similarity of each temperature data on the actual curve and the reference curve, and determining target similarity based on trend similarity and data similarity.

[0081] like Figure 2 As shown, the actual curve and the reference curve are each divided into three segments. For each curve segment in the actual curve, its temperature change trend is determined, which is the first change trend; for each curve segment in the reference curve, its temperature change trend is determined, which is the second change trend. To compare the trends of the two curve segments, the correlation coefficient or Euclidean distance can be used to calculate the cosine similarity. If the change trend of the actual curve and the reference curve in a certain time period is obviously inconsistent, it may indicate an abnormality. Further, the key data points of the two curve segments are compared, such as Figure 2Take the endpoints A, B and the middle point on the AB segment; take the endpoints a, b and the middle point on the ab segment, calculate the mean square error (MSE) or mean absolute error (MAE) of these three temperature points respectively, and determine the data matching similarity based on the calculation results. If the data matching degree between the actual curve and the reference curve in a certain time period is low, it may indicate anomalies. Finally, determine the target similarity based on the trend similarity and data similarity. You can use the weighted average method to determine a comprehensive target similarity. For example, you can assign different weights to the trend similarity and data similarity, and then calculate the weighted average as the final target similarity.

[0082] In this embodiment, the trend similarity reflects the closeness of the temperature change trend between the actual firing process and the reference firing scheme. The data similarity reflects the closeness between the actual temperature data and the reference temperature data. By combining these two situations, the continuous temperature change and the discrete key point temperature difference are considered, so that the difference between the actual firing process and the reference theoretical process can be accurately evaluated, and then it can be judged whether the firing process meets expectations.

[0083] S50: Determine whether the target similarity is greater than a first preset threshold.

[0084] S60: If the target similarity is greater than a first preset threshold, the next firing stage is executed according to the initial firing scheme.

[0085] The first preset threshold is usually a number close to 1, for example, it can be 0.95. If the target similarity is greater than the first preset threshold, it means that the temperature change during actual firing is very close to the temperature change curve of the reference curve. At this time, it means that there is no special abnormality in the firing process. The firing process of the next firing stage can be executed according to the reference temperature change curve and the insulation time of the next stage in the initial firing plan.

[0086] Therefore, this embodiment uses the characteristic parameters of the ceramic body and the historical database for cluster analysis to obtain an initial firing plan suitable for the current body, so that a reference can be quickly provided for the current firing plan to make it more consistent with the characteristics of the actual body. The trend of the actual temperature change curve and the reference curve is extracted through wavelet transform, so as to accurately divide the curve segments. When comparing the reference curve and the actual curve, the temperature trends of different curve segments can be more finely compared, so as to more accurately find deviations and match the corresponding processing strategies, thereby improving the firing accuracy and accelerating the process efficiency.

[0087] In addition, when comparing the reference curve and the actual curve, the present invention will compare the similarity of the change trend of each curve segment, and will also combine the data similarity of the discrete temperature points in the curve segment, so as to determine the target similarity according to the trend similarity and the data similarity, and compare the target similarity with the first preset threshold after obtaining it. If it is greater than the first preset threshold, it means that the current actual firing temperature is normal, and the next firing stage can be executed according to the initial firing scheme. By real-time monitoring of the actual temperature change and comparing it with the reference curve, deviations can be found in time and adjusted. By considering the similarity of continuous trend changes and the similarity of discrete values, the difference between the actual curve and the reference curve can be analyzed more accurately. This provides a reliable basis for decision-making in the actual firing process and enhances process energy efficiency.

[0088] The above embodiment takes into account the case where the target similarity is greater than the first preset threshold. In other embodiments, if the target similarity is less than or equal to the first preset threshold, it is necessary to further consider whether to adjust the firing parameters to remedy the defects caused by abnormal temperature changes, or to directly abandon the current firing process to avoid wasting more resources.

[0089] See also Figure 3 In one embodiment, the method further comprises:

[0090] S70, if the target similarity is less than or equal to the first preset threshold, calculating the deviation between the target similarity and the first preset threshold, and determining whether the deviation is within a preset range;

[0091] S80, if yes, optimize the reference temperature change curve and reference holding time of the next firing stage in the initial firing scheme, and execute the next firing stage according to the optimized firing scheme;

[0092] S90: If not, stop the firing process of the current ceramic body and replace it with a new ceramic body for firing.

[0093] It is understandable that if the temperature change is minor, such as a slight deviation from the set temperature but still within the acceptable range, then firing can usually continue. In this case, the temperature abnormality may not have a significant impact on the quality of the final product. Because in order to compensate for the defects that may be caused by the current temperature deviation, the reference temperature change curve and reference holding time of the next firing stage will be adjusted, and then the next firing stage will be executed according to the adjusted firing plan.

[0094] Specifically, when optimizing, first analyze whether the cause of the deviation is due to the temperature change trend or the problem with the temperature data itself. If the deviation is mainly caused by trend mismatch, it can be optimized by adjusting the temperature change rate. For example, if the actual temperature rises too fast, the heating rate of the next stage can be appropriately reduced; vice versa. If the deviation is mainly due to temperature data mismatch, it can be optimized by fine-tuning the insulation time and temperature value. For example, if the actual temperature is lower than the reference temperature, the insulation time can be increased in the next stage; if it is higher than the reference temperature, the insulation time can be reduced. Therefore, the specific tuning strategy can be as follows:

[0095] 1) Heating rate adjustment:

[0096] If the heating rate of the actual curve is faster than that of the reference curve, the heating rate of the next stage can be slowed down.

[0097] If the heating rate of the actual curve is slower than that of the reference curve, the heating rate of the next stage can be accelerated.

[0098] 2) Adjustment of holding time:

[0099] If the temperature of the actual curve is too low, the insulation time of the next stage can be extended.

[0100] If the temperature of the actual curve is too high, the insulation time of the next stage can be shortened.

[0101] 3) Temperature adjustment:

[0102] If the temperature of a certain stage in the entire firing process continues to be low, the maximum sintering temperature of the next stage can be appropriately increased.

[0103] If the temperature in a certain stage continues to be too high, the maximum sintering temperature of the next stage can be appropriately lowered.

[0104] The above tuning process is for situations where the deviation is within the preset range. However, if the temperature changes abnormally, such as the temperature is much higher or lower than the set value, or the temperature drops or rises suddenly, this may have a negative impact on the structure and performance of the ceramic. At this time, in order to prevent waste of resources, the firing process of the current ceramic body can be stopped and replaced with a new ceramic body for firing.

[0105] In this embodiment, when it is found that the deviation range is controllable, it is remedied by adjusting the parameters of the next stage. Conversely, if the deviation is uncontrollable, there is no need to continue to waste manpower and material resources to replace the new body and re-fire it. In this way, the quality of the finished ceramic product can be predicted in advance, and it can be replaced in time when the firing problem is irreversible, avoiding waste of energy, thereby greatly improving the process energy efficiency of ceramic processing.

[0106] See also Figure 4In one embodiment, before executing the next firing stage according to the optimized firing scheme, the method further includes:

[0107] S801, obtaining a ceramic product image after the current firing stage is completed, and performing denoising, image enhancement and grayscale processing on the ceramic product image to obtain a grayscale image.

[0108] Image acquisition: Use a camera or other imaging device to capture an image of the ceramic product after firing.

[0109] Denoising: Remove random noise from the image through filtering algorithms (such as Gaussian filtering, median filtering, etc.) to improve the accuracy of subsequent processing.

[0110] Image enhancement: Improve the clarity and contrast of the image through contrast enhancement, histogram equalization and other technologies to facilitate subsequent feature extraction.

[0111] Grayscale processing: Convert color images into grayscale images to simplify the complexity of image processing while retaining sufficient detail information for analysis.

[0112] Therefore, through denoising and enhancement processing, the quality of the image can be significantly improved, making the subsequent feature extraction more accurate. Grayscale processing simplifies the image processing flow, reduces the computational complexity, and helps to improve the processing speed of the entire system.

[0113] S802, extracting features from the grayscale image, including texture features, edge features, and spectral features; inputting the extracted features into a preset RNN model for defect recognition, and generating recognition results;

[0114] Texture features: Extract texture information from images through methods such as gray-level co-occurrence matrix (GLCM) and local binary pattern (LBP).

[0115] Edge features: Use Canny edge detection, Sobel operator and other techniques to detect edges in the image.

[0116] Spectral characteristics: Although grayscale images have no color information, the spectral characteristics can be indirectly reflected by the grayscale value distribution, such as through histogram analysis.

[0117] The extracted features are input into the pre-trained recurrent neural network (RNN) model, and the memory capacity of the RNN model is used to capture the sequence relationship between features, perform defect recognition, and thus determine the defect type and location. The RNN model can effectively capture the sequence dependency between image features, thus improving the accuracy of defect recognition.

[0118] S803: Compensate the optimized firing scheme according to the recognition result.

[0119] See also Figure 5 In one embodiment, compensating the optimized firing scheme according to the recognition result includes:

[0120] S8031. Determine the defect type according to the recognition result, where the defect type includes cracks, bubbles and uneven color;

[0121] S8032, performing correlation analysis on the defect type and the reference temperature change curve and reference holding time of the current firing stage in the initial firing scheme, and screening out target defect types with correlation greater than a second preset threshold;

[0122] S8033. Determine the firing temperature and holding time to be adjusted according to the target defect type, and compensate the optimized firing scheme according to the firing temperature and holding time to be adjusted.

[0123] In this embodiment, correlation analysis can be performed using the Pearson correlation coefficient. By identifying the defect type and performing correlation analysis, the relationship between the specific defect type and the firing parameters is clarified, thereby screening out defects with high correlation with the reference temperature change curve and the reference insulation time, and performing targeted parameter tuning and compensation.

[0124] For example, cracks are usually related to too high a cooling rate, and the holding time can be appropriately increased or the cooling rate can be reduced. Bubbles may be related to insufficient moisture removal, which can be improved by adjusting the heating rate or increasing the holding time. Uneven color may be caused by uneven temperature distribution, which can be solved by optimizing the temperature curve. Defects can be compensated for the parameters adjusted in the above embodiments, further improving the accuracy of temperature change control and holding time.

[0125] In one embodiment, the method further comprises:

[0126] After all firing stages are completed to obtain a finished ceramic product, the quality parameters of the current finished ceramic product are obtained, and the initial firing plan for the next ceramic production is determined according to the quality parameters;

[0127] The quality parameters of the finished ceramic product include dimensional change, porosity and tensile strength.

[0128] In this embodiment, in order to study and analyze the firing control process of this time, the quality parameters of the current ceramic finished product are also obtained to determine the initial firing plan for the next ceramic production according to the quality parameters.

[0129] Specifically, the initial firing plan for the next ceramic production is determined based on the quality parameters, including:

[0130] Establish a multi-objective optimization function for firing temperature, holding time and heating rate, and establish corresponding constraints based on dimensional change, porosity and tensile strength;

[0131] The multi-objective optimization function is solved according to the firefly algorithm, and the initial firing plan for the next ceramic production is determined according to the solution result.

[0132] In this embodiment, the parameter optimization process is as follows:

[0133] 1) Establish a multi-objective optimization function:

[0134] f=f(T,t,v)

[0135] Where T, t, and v represent the firing temperature, holding time, and heating rate, respectively.

[0136] 2) Determine the parameter relationship between dimensional change ΔL, porosity ε, and tensile strength σ:

[0137] ΔL=aT+bt+c

[0138] ε=d-gT

[0139] σ=-pε-qT 2

[0140] According to the dimensional change ΔL, porosity ε, and tensile strength σ, the corresponding constraints are recommended:

[0141] ΔL min ≤ΔL≤ΔL max

[0142] ε tar -τ≤ε≤ε tar +τ

[0143] σ min ≤σ

[0144] In the formula, a, b, c, d, g, p, q are all constant terms; ΔL min , ΔL max are the minimum and maximum sizes allowed to change, ε tar represents the ideal value of porosity, τ represents the allowable fluctuation error of porosity, σ min Indicates the minimum tensile strength.

[0145] Furthermore, the firefly algorithm is used to solve the multi-objective function:

[0146] Initialization step: Set the initial firing temperature T, holding time t and heating rate v as the initial firing plan, and initialize the firefly positions, including the firefly population, the number of processors, the number of assigned tasks, the light absorption coefficient, and the spatial distance between two fireflies;

[0147] Position update step: According to the initialized firefly position, calculate the firefly brightness through the objective function; update the firefly position according to the firefly brightness, including controlling the common fireflies to move according to the adaptive step size, the moving direction is determined by the firefly with the largest fluorescent brightness, and controlling the optimal firefly to find the current optimal solution to move;

[0148] Iteration step: determine whether the number of iterations reaches a first preset threshold. If not, repeat the position update step until the number of iterations reaches the first preset threshold, and output the global optimal solution.

[0149] In summary, after obtaining the finished ceramic product, this embodiment will obtain the quality parameters of the current finished ceramic product, establish constraints based on the quality parameters, establish constraints based on the temperature, insulation time and heating rate in the firing plan, and determine the initial firing plan before the next ceramic firing by optimizing. Through this self-learning feedback control and adjustment mechanism, the quality of ceramic firing is continuously improved, and ultimately the yield rate of the entire ceramic firing process is greatly improved.

[0150] Those skilled in the art will appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professional and technical personnel can use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of the present invention.

[0151] Those skilled in the art can clearly understand that, for the convenience and brevity of description, the specific working processes of the systems, devices and units described above can refer to the corresponding processes in the aforementioned method embodiments, and will not be repeated here. Those skilled in the art can also clearly understand that the descriptions of the various embodiments of the present invention have different focuses. For the convenience and brevity of description, the same or similar parts may not be repeated in different embodiments. Therefore, for parts not described or not described in detail in a certain embodiment, refer to the records of other embodiments.

Claims

1. A method for controlling process parameters of ceramic production, characterized in that: The method comprises: A ball mill is used to prepare a ceramic blank, and the prepared blank is pressed and formed to obtain a ceramic body; Acquire characteristic parameters of the ceramic body and a database generated according to a historical ceramic preparation process, perform cluster analysis on the characteristic parameters and the database, and obtain an initial firing scheme for the ceramic body, wherein the initial firing scheme includes a reference temperature change curve and a reference holding time at each firing stage; Obtaining an actual temperature change curve of the ceramic in the current firing stage and a corresponding reference temperature change curve as an actual curve and a reference curve; extracting the temperature change trends of the actual curve and the reference curve by wavelet transform, so as to divide the actual curve and the reference curve into a plurality of curve segments; Determine a first change trend of each curve segment in the actual curve and a second change trend of each curve segment in the reference curve; calculate the trend similarity of the first change trend and the second change trend, and calculate the data similarity of each temperature data on the actual curve and the reference curve, and determine the target similarity according to the trend similarity and the data similarity; It is determined whether the target similarity is greater than a first preset threshold value. If the target similarity is greater than the first preset threshold value, the next firing stage is executed according to the initial firing scheme.

2. The ceramic production process parameter control method according to claim 1, characterized in that: The method further comprises: If the target similarity is less than or equal to a first preset threshold, calculating a deviation between the target similarity and the first preset threshold, and determining whether the deviation is within a preset range; If yes, the reference temperature change curve and the reference holding time of the next firing stage in the initial firing plan are optimized, and the next firing stage is executed according to the optimized firing plan; If not, the firing process of the current ceramic body is stopped and a new ceramic body is replaced for firing.

3. The ceramic production process parameter control method according to claim 2, characterized in that: Before executing the next firing stage according to the optimized firing plan, the method further includes: Acquire the ceramic product image after the current firing stage is completed, perform denoising, image enhancement and grayscale processing on the ceramic product image to obtain a grayscale image; Extract features from grayscale images, including texture features, edge features, and spectral features; input the extracted features into the preset RNN model for defect recognition and generate recognition results; The optimized firing scheme is compensated according to the identification results.

4. The ceramic production process parameter control method according to claim 3, characterized in that: The method of compensating the optimized firing scheme according to the identification result includes: Determining defect types according to the recognition results, wherein the defect types include cracks, bubbles, and uneven colors; Performing correlation analysis on the defect type and the reference temperature change curve and reference holding time of the current firing stage in the initial firing scheme, and screening out the target defect type with a correlation greater than a second preset threshold value; The firing temperature and holding time to be adjusted are determined according to the target defect type, and the optimized firing scheme is compensated according to the firing temperature and holding time to be adjusted.

5. The ceramic production process parameter control method according to claim 1, characterized in that: The pressure during the compression molding is: P=C(ρ g -p0) n In the formula, P represents pressure, C represents the response degree of the ceramic blank to pressure, and ρ g represents the target density of the ceramic body after pressing, ρ0 represents the density of the ceramic body before pressing, and n represents the relationship between the density of the body and the pressure, satisfying 2≤n≤5.

6. The ceramic production process parameter control method according to claim 1, characterized in that: The characteristic parameters include the material type and actual density of the ceramic body and the theoretical density of the finished ceramic product.

7. The ceramic production process parameter control method according to claim 1, characterized in that: The method further comprises: After all firing stages are completed to obtain a finished ceramic product, the quality parameters of the current finished ceramic product are obtained, and the initial firing plan for the next ceramic production is determined according to the quality parameters; The quality parameters of the finished ceramic product include dimensional change, porosity and tensile strength.

8. The ceramic production process parameter control method according to claim 7, characterized in that: Determine the initial firing plan for the next ceramic production according to the quality parameters, including: Establish a multi-objective optimization function for firing temperature, holding time and heating rate, and establish corresponding constraints based on dimensional change, porosity and tensile strength; The multi-objective optimization function is solved according to the firefly algorithm, and the initial firing plan for the next ceramic production is determined according to the solution result.

Citation Information

Patent Citations

  • Preparation method of controllable-porosity porous silicon carbide ceramic

    CN104193395A

  • Temperature parameter curve control method and system for normal-pressure sintering ceramic furnace

    CN111623624A

  • Kiln control method based on visual identification and kiln capable of automatically adjusting temperature

    CN117109324A

  • Production method of high-strength anti-pollution domestic ceramic

    CN117623735A

  • Device and method for preparing composite material

    CN117654325A

Cited By

  • Ceramic sintering optimization method and system based on dynamic monitoring

    CN119494277A

  • Ceramic-based double-sided printed circuit board and manufacturing method thereof

    CN119697884A

  • Ceramic-based double-sided printed circuit board and manufacturing method thereof

    CN119697884B

  • Triphenylphosphine oxide recovery method suitable for industrial production

    CN120004948A

  • Accurate standard-free quantification method based on automatic identification and matching of different matrixes

    CN120507382A