Preparation method of semiconductor device and semiconductor device
By forming a doped region structure with deep injection light doping and shallow injection heavy doping on the semiconductor epitaxial chip, the problem of large contact resistance of silicon carbide electronic devices is solved, and the switching speed of the device is improved and power consumption is reduced.
Patent Information
- Application Number
- CN202410866042.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-11-08
AI Technical Summary
The contact resistance of silicon carbide electronic devices is large, which limits device performance, especially in power devices, which accounts for a high proportion of on-resistance, which affects speed and power consumption.
By forming a specific doped region structure on the semiconductor epitaxial chip, including deep implantation of light doped and shallow implantation of heavily doped regions, the Schottky barrier width is reduced, thereby improving contact resistance and on-resistance.
It effectively reduces device leakage, improves switching speed and reduces power consumption.
Smart Images

Figure CN118919551A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a method for preparing a semiconductor device and a semiconductor device thereof. Background Art
[0002] Silicon carbide has excellent properties such as wide band gap, high critical electric field, high thermal conductivity and high electron saturation velocity, and is the most prominent candidate for the next generation of power semiconductor devices. Currently, most of the mature processes used for silicon-based, such as ion implantation, thermal oxidation, self-aligned silicide and other technologies have been used in silicon carbide power devices and have achieved considerable development. At present, there are still many significant technical difficulties, such as the optimal properties of silicon carbide materials, and obtaining low contact resistance and high reliability ohmic contacts is one of the key technical issues limiting the performance of silicon carbide electronic devices.
[0003] With the continuous advancement of technology and market demand, power devices may also continue to miniaturize following a trend similar to Moore's Law. Among them, contact resistance will face a greater test, accounting for more than 50% of the entire device on-resistance (the contact resistance of 30nm contact CD in silicon base accounts for more than 60% of the total resistance), seriously affecting the speed and power consumption of power devices.
[0004] Therefore, it is very important to improve the contact resistance characteristics of the device. Summary of the invention
[0005] The semiconductor device manufacturing method and semiconductor device provided in the present application can solve the problem of large on-resistance of the device.
[0006] In order to solve the above technical problems, a technical solution adopted in the present application is: providing a method for preparing a semiconductor device, comprising:
[0007] Providing a semiconductor epitaxial wafer, wherein the semiconductor epitaxial wafer has a first conductivity type;
[0008] forming a first doping region, a second doping region, a third doping region, a fourth doping region and a fifth doping region on the semiconductor epitaxial wafer;
[0009] Wherein, the first doped region extends from the first surface of the semiconductor epitaxial wafer along a first direction; the first doped region has a second conductivity type, and the first direction is a direction extending from the first surface of the semiconductor epitaxial wafer toward the inside of the semiconductor epitaxial wafer;
[0010] The second doping region and the third doping region are both arranged in the first doping region, the third doping region extends from the first surface along the first direction, the second doping region is located below the third doping region and is connected to the third doping region; the ion doping concentration of the third doping region is greater than the ion doping concentration of the second doping region, and the second doping region and the third doping region both have the first conductivity type;
[0011] The fourth doping region and the fifth doping region are both arranged in the first doping region, the fifth doping region extends from the first surface along the first direction, the fourth doping region is located below the fifth doping region and is connected to the fifth doping region; and the fourth doping region is parallel to and connected to the second doping region, and the fifth doping region is parallel to and connected to the third doping region, the ion doping concentration of the fifth doping region is greater than the ion doping concentration of the fourth doping region, and the fourth doping region and the fifth doping region both have the second conductivity type.
[0012] In order to solve the above technical problems, another technical solution adopted by the present application is: to provide a semiconductor device, comprising:
[0013] A semiconductor epitaxial wafer, wherein the semiconductor epitaxial wafer has a first conductivity type;
[0014] A first doped region extends from the first surface of the semiconductor epitaxial wafer along a first direction; the first doped region has a second conductivity type, and the first direction is a direction extending from the first surface of the semiconductor epitaxial wafer toward the inside of the semiconductor epitaxial wafer;
[0015] a second doping region and a third doping region, wherein the second doping region and the third doping region are both arranged in the first doping region, the third doping region extends from the first surface along the first direction, the second doping region is located below the third doping region and is connected to the third doping region; the ion doping concentration of the third doping region is greater than the ion doping concentration of the second doping region, and the second doping region and the third doping region both have a first conductivity type;
[0016] A fourth doping region and a fifth doping region, wherein the fourth doping region and the fifth doping region are both arranged in the first doping region, the fifth doping region extends from the first surface along the first direction, the fourth doping region is located below the fifth doping region and is connected to the fifth doping region; and the fourth doping region is parallel to and connected to the second doping region, the fifth doping region is parallel to and connected to the third doping region, the ion doping concentration of the fifth doping region is greater than the ion doping concentration of the fourth doping region, and the fourth doping region and the fifth doping region both have a second conductivity type.
[0017] Different from the prior art, the beneficial effect of the present application is that in the preparation method of the semiconductor device provided by the present application, a third doping region with an ion doping concentration greater than that of the second doping region is formed above the second doping region to form a second doping region with deep injection and light doping and a third doping region with shallow injection and heavy doping are formed, and a fifth doping region with an ion doping concentration greater than that of the fourth doping region is formed above the fourth doping region to form a fourth doping region with deep injection and light doping and a fifth doping region with shallow injection and heavy doping are formed; the shallow injection and heavy doping structure of the third doping region and the fifth doping region can reduce the Schottky barrier width, thereby improving the contact resistance and on-resistance of the device, and is beneficial to reducing device leakage, thereby increasing the switching speed of the device and reducing power consumption. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work, among which:
[0019] Figure 1 A schematic flow chart of a method for manufacturing a semiconductor device according to a first embodiment of the present application;
[0020] Figure 2 for Figure 1 A partial flow diagram of an embodiment of step S2;
[0021] Figure 3 for Figure 1 A partial flow diagram of an embodiment of step S2;
[0022] Figure 4 for Figure 3 A flowchart of an embodiment of step S223;
[0023] Figure 5 for Figure 1 A partial flow diagram of an embodiment of step S2;
[0024] Figure 6 for Figure 4 A schematic flow chart of an embodiment of step S25;
[0025] Figure 7 Figure 1 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S1;
[0026] Figure 8 for Figure 2A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S21;
[0027] Fig. 9 for Figure 2 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S22;
[0028] Fig.10 for Figure 4 A schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S231;
[0029] Fig.11 for Figure 4 A schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S232;
[0030] Fig.12 This is a schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S241;
[0031] Fig.13 for Figure 6 A schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S251;
[0032] Fig.14 for Figure 6 A schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S252;
[0033] Fig.15 This is a schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S261;
[0034] Fig.16 A schematic flow chart of another implementation of the method for manufacturing a semiconductor device provided in the first embodiment of the present application;
[0035] Fig.17 for Fig.16 A schematic flow chart of an embodiment of step S5;
[0036] Fig.18 for Fig.16 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S3;
[0037] Fig.19 for Fig.16 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S4;
[0038] Fig. 20 for Fig.17 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S51;
[0039] Fig.21 for Fig.17A schematic diagram of a structure of a portion of an intermediate product of an embodiment after step S52;
[0040] Fig. 22 A partial structural schematic diagram of a semiconductor device provided in the second embodiment of the present application. Description of the drawings:
[0042] First embodiment:
[0043] Semiconductor epitaxial wafer-11; substrate-111; silicon carbide epitaxial layer-112; first doping region-12; second doping region-13; third doping region-14; fourth doping region-15; fifth doping region-16; gate structure-17; ohmic contact metal-18; titanium metal layer-181; first cobalt metal layer-182; silicon layer-183; second cobalt metal layer-184;
[0044] The first region to be doped-A1; the first sub-region-121; the second sub-region-122; the second region to be doped-A2; the third region to be doped-A3;
[0045] A first doping prefabricated region-130; a second doping prefabricated region-150; a third doping prefabricated region-120;
[0046] First mask pattern-B1; second mask pattern-B2; silicon dioxide layer-B21; polysilicon layer-B22; third mask pattern-B3; fourth mask pattern-B4;
[0047] The first opening is C1; the second opening is C2; the third opening is C3; the fourth opening is C4.
[0048] Second embodiment:
[0049] Semiconductor epitaxial wafer-21; substrate-211; silicon carbide epitaxial layer-212; first doping region-22; second doping region-23; third doping region-24; fourth doping region-25; fifth doping region-26; ohmic contact metal-27; insulating layer-28; gate structure-291; source structure-292; drain structure 293. DETAILED DESCRIPTION
[0050] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0051] The terms "first", "second", "third" in this application are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Thus, the features defined as "first", "second", "third" can expressly or implicitly include at least one of the features. In the description of this application, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined. In the embodiments of this application, all directional indications (such as up, down, left, right, front, back...) are only used to explain the relative position relationship, movement, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication also changes accordingly. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device comprising a series of steps or units is not limited to the steps or units listed, but optionally also includes steps or units that are not listed, or optionally also includes other steps or units inherent to these processes, methods, products or devices.
[0052] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0053] The present application is described in detail below with reference to the accompanying drawings and embodiments.
[0054] See also Figure 1-Figure 6 , Figure 1 A schematic flow chart of a method for manufacturing a semiconductor device according to a first embodiment of the present application; Figure 2 for Figure 1 A partial flow diagram of an embodiment of step S2; Figure 3 for Figure 2 A schematic flow chart of an embodiment of step S21; Figure 4 for Figure 1 A partial flow diagram of an embodiment of step S2;
[0055] Figure 5 for Figure 4 A schematic flow chart of an embodiment of step S23; Figure 6 for Figure 1 A partial flow chart of an embodiment of step S2 in FIG.
[0056] See also Figure 1 The first embodiment of the present application provides a method for preparing a semiconductor device, comprising:
[0057] Step S1: providing a semiconductor epitaxial wafer 11.
[0058] The semiconductor epitaxial wafer 11 has a first conductivity type, which is one of a P-type doped semiconductor and an N-type doped semiconductor.
[0059] See Figure 7 In one embodiment, the semiconductor epitaxial wafer 11 is a silicon carbide (SiC) semiconductor epitaxial wafer, and the semiconductor epitaxial wafer 11 includes a substrate 111 and an epitaxial layer 112 grown on the substrate 111. The surface of the epitaxial layer 112 facing away from the substrate 111 is defined as the first surface of the semiconductor epitaxial wafer 11.
[0060] Furthermore, a number of regions to be doped are defined on the semiconductor epitaxial wafer 11 , and the regions to be doped are used for ion doping, such as P-type ion doping and N-type ion doping, to form corresponding functional regions in the semiconductor epitaxial wafer.
[0061] In some embodiments, P-type ions include but are not limited to B+ or Al + etc.; N-type ions include but are not limited to N + , P + 、As + wait.
[0062] In the present application, the several regions to be doped include several third regions to be doped A3 extending from the first surface of the semiconductor epitaxial wafer 11 along the first direction, and each third region to be doped A3 includes parallel and connected first regions to be doped A1 and second regions to be doped A2, and the first regions to be doped A1 and the second regions to be doped A2 both extend from the first surface of the semiconductor epitaxial wafer 11 along the first direction.
[0063] It should be noted that the first direction is a direction extending from the first surface of the semiconductor epitaxial wafer 11 toward the inside of the semiconductor epitaxial wafer 11 .
[0064] Step S2 : forming a first doping region 12 , a second doping region 13 , a third doping region 14 , a fourth doping region 15 and a fifth doping region 16 on the semiconductor epitaxial wafer 11 .
[0065] The first doped region 12 extends from the first surface of the semiconductor epitaxial wafer 11 along the first direction; the first doped region 12 has a second conductivity type; the second conductivity type is the other of a P-type doped semiconductor and an N-type doped semiconductor.
[0066] The second doping region 13 and the third doping region 14 are both disposed in the first doping region 12, the third doping region 14 extends from the first surface along the first direction, the second doping region 13 is located below the third doping region 14 and is connected to the third doping region 14; the ion doping concentration of the third doping region 14 is greater than the ion doping concentration of the second doping region 13, and the second doping region 13 and the third doping region 14 both have the first conductivity type;
[0067] The fourth doping region 15 and the fifth doping region 16 are both arranged in the first doping region 12, the fifth doping region 16 extends from the first surface along the first direction, the fourth doping region 15 is located below the fifth doping region 16 and is connected to the fifth doping region 16; and the fourth doping region 15 is parallel to and connected to the second doping region 13, and the fifth doping region 16 is parallel to and connected to the third doping region 14, the ion doping concentration of the fifth doping region 16 is greater than the ion doping concentration of the fourth doping region 15, and the fourth doping region 15 and the fifth doping region 16 both have the second conductivity type.
[0068] Specifically, in the method for preparing a semiconductor device provided in the present application, a third doping region 14 having an ion doping concentration greater than that of the second doping region 13 is formed above the second doping region 13 to form a second doping region 13 that is lightly doped by deep injection and a third doping region 14 that is heavily doped by shallow injection, and a fifth doping region 16 having an ion doping concentration greater than that of the fourth doping region 15 is formed above the fourth doping region 15 to form a fourth doping region 15 that is lightly doped by deep injection and a fifth doping region 16 that is heavily doped by shallow injection; the shallowly injected heavily doped structure of the third doping region 14 and the fifth doping region 16 can reduce the Schottky barrier width, thereby improving the contact resistance and on-resistance of the device, and is beneficial to reducing device leakage, thereby increasing the switching speed of the device and reducing power consumption.
[0069] In one embodiment, see Figure 2 , forming a first doped region 12 on a semiconductor epitaxial wafer 11, comprising:
[0070] Step S21: forming a third mask pattern B3 on the first surface of the semiconductor epitaxial wafer 11, wherein the third mask pattern B3 has two third openings C3 spaced apart at positions corresponding to the third region A3 to be doped, and the positions of the two third openings C3 correspond one-to-one to the positions of the two spaced apart first sub-regions 121 in the third region A3 to be doped.
[0071] In some embodiments, the material of the third mask pattern B3 includes silicon dioxide (SiO2) or polysilicon (Poly). The third opening C3 can be formed by an etching process, for example, dry etching the mask layer forming the third mask pattern B3 to form the third mask pattern B3 having the third opening C3.
[0072] Specific combination Figure 8 The two third openings C3 are respectively disposed near two opposite sides of the third region to be doped A3, and the portion of the third mask pattern B3 between the two third openings C3 forms a shielding portion (not marked in the figure).
[0073] Step S22: using the two third openings C3 to perform ion doping of the second conductivity type on the two first sub-regions 121 to form two third doping pre-regions 120 spaced apart in the third region to be doped A3.
[0074] In the embodiment of the present application, the second conductivity type is P type, and the second conductivity type ion doping of the two first sub-regions 121 includes: implanting Al into the two first sub-regions 121 at a high temperature (for example, 400° C.-600° C.) + , so as to form two third doping pre-regions 120 distributed at intervals in the third area to be doped A3.
[0075] Specific combination Fig. 9 .
[0076] It can be understood that due to the existence of the shielding portion, after step S22, after the third region to be doped A3 is doped using the third mask pattern B3, two third doping pre-regions 120 spaced apart are formed in the third region to be doped A3.
[0077] In other embodiments, the third mask pattern B3 has an opening at a position corresponding to the third region to be doped A3, and the opening completely exposes the third region to be doped A3. In this embodiment, after the second conductive type ion doping is performed using the third mask pattern B3, since there is no shielding portion on the third region to be doped A3, the complete first doping region 12 can be formed at one time.
[0078] In one embodiment, see Figure 3 , forming a second doping region 13 and a third doping region 14 on the semiconductor epitaxial wafer 11, including:
[0079] Step S23 : performing ion doping of the first conductivity type on the first to-be-doped region A1 of the semiconductor epitaxial wafer 11 to form a first doping pre-region 130 .
[0080] In the embodiment of the present application, the first conductivity type is N type, and the first conductivity type ion doping of the first to-be-doped region A1 includes: implanting N into the first to-be-doped region A1 at a high temperature (eg, 400° C.-600° C.) + , so as to form a first doping pre-region 130 in the first area to be doped A1.
[0081] Specific combination Fig.11 .
[0082] Step S24: performing ion doping of the first conductive type on a portion of the first doping prefabricated region 130 close to the first surface to form a third doping region 14 in the first doping prefabricated region 130 ; wherein the portion of the first doping prefabricated region 130 other than the third doping region 14 serves as the second doping region 13 .
[0083] In the embodiment of the present application, the portion of the first doping prefabricated region 130 close to the first surface is further doped for a second time. Specifically, N is continuously implanted into the portion of the first doping prefabricated region 130 close to the first surface under high temperature conditions. + , P + 、As + Plasma is applied to form a shallowly implanted heavily doped third doping region 14 in a portion of the first doping prefabricated region 130 close to the first surface, and a portion of the first doping prefabricated region 130 other than the third doping region 14 serves as the second doping region 13 .
[0084] Specific combination Fig.12 .
[0085] Specifically, by performing in-situ secondary doping on the first area to be doped A1, a second doping area 13 deeply injected and lightly doped and a third doping area 14 shallowly injected and heavily doped are formed in the first area to be doped A1. Specifically, the third doping area 14 shallowly injected and heavily doped can reduce the Schottky barrier width of the device, thereby improving the contact resistance and on-resistance of the device, and is beneficial to reducing the leakage of the device, thereby increasing the switching speed of the device and reducing power consumption.
[0086] In one embodiment, see Figure 4 , step S23 specifically includes:
[0087] Step S231 : forming a first mask pattern B1 on the first surface of the semiconductor epitaxial wafer 11 , wherein the first mask pattern B1 has a first opening C1 at a position corresponding to the first region to be doped A1 .
[0088] In one embodiment, see Fig.10 After two third doping pre-regions 120 are formed and spaced apart from each other, the first mask pattern B1 is grown using the third mask pattern B3.
[0089] In some embodiments, the material of the first mask pattern B1 may be the same as the material of the third mask pattern B3. The first opening C1 may be formed by an etching process, for example, dry etching is performed on the mask layer forming the first mask pattern B1 to form the first mask pattern B1 having the first opening C1. It can be understood that since the first mask pattern B1 is formed by self-aligned growth using the third mask pattern B3, the first mask pattern B1 forms the first opening C1 at the position corresponding to each third opening C3, and the first opening C1 is smaller than the opening size of the third opening C3. Each first opening C1 corresponds to a first region A1 to be doped.
[0090] Specifically, the third mask pattern B3 has two third openings C3 spaced apart at positions corresponding to the third region to be doped A3 . The third mask pattern B3 can also be used as a substrate for the first mask pattern B1 to be formed subsequently, thereby simplifying the process of forming the first doping prefabricated region 130 .
[0091] Step S232: using the first opening C1 and adopting the first implantation energy and the first ion doping concentration, perform ion doping of the first conductivity type on the first to-be-doped region A1 of the semiconductor epitaxial wafer 11 to form a first doping prefabricated region 130 .
[0092] In some embodiments, the first ion doping concentration is 1e12-1e15 / cm 2 .
[0093] In the embodiment of the present application, at a high temperature (eg, 400° C.-600° C.), N is implanted into the first to-be-doped region A1 using the first opening C1 with a first implantation energy and a first ion doping concentration. + , so as to form a first doping pre-region 130 in the first area to be doped A1.
[0094] Specific combination Fig.11 Specifically, after step S232 , two first doping prefabricated regions 130 spaced apart from each other are formed in each third doping prefabricated region 120 .
[0095] Further, step S24 specifically includes:
[0096] Step S241 : using the first opening C1 and adopting the second implantation energy and the second ion doping concentration, ion doping of the first conductivity type is performed on a portion of the first doping prefabricated region 130 close to the first surface to form a third doping region 14 in the first doping prefabricated region 130 .
[0097] The second injection energy is less than the first injection energy; and the second ion doping concentration is greater than the first ion doping concentration.
[0098] It can be understood that the ion doping depth is positively correlated with the implantation energy. Therefore, in order to make the extension depth of the third doping region 14 along the first direction smaller than the extension depth of the second doping region 13 along the first direction, in the present application, the second implantation energy is smaller than the first implantation energy. In one embodiment, the second implantation energy is 30-70keV.
[0099] In order to make the ion doping concentration of the third doping region 14 greater than the ion doping concentration of the second doping region 13, the second ion doping concentration is 1e13-1e16 / cm 2 .
[0100] Specific combination Fig.12 In the embodiment of the present application, the first opening C1 is used to continue to implant N into the portion of the first doped prefabricated region 130 close to the first surface under high temperature conditions. + , P + or As + Plasma is applied to form a shallowly implanted heavily doped third doping region 14 in a portion of the first doping prefabricated region 130 close to the first surface, and a portion of the first doping prefabricated region 130 other than the third doping region 14 is used as the second doping region 13 .
[0101] Specifically, the first mask pattern B1 is used to perform in-situ secondary doping on the first area to be doped A1 to form a second doping region 13 with deep injection and light doping and a third doping region 14 with shallow injection and heavy doping. The formation of the third doping region 14 does not require an additional mask pattern, which can save process steps and optimize device performance.
[0102] In one embodiment, see Figure 5 , forming a fourth doping region 15 and a fifth doping region 16 on the semiconductor epitaxial wafer 11, including:
[0103] Step S25: Perform ion doping of the second conductivity type on the second doping region A2 of the semiconductor epitaxial wafer 11 to form a second doping prefabricated region 150; wherein the second doping region A2 extends from the first surface of the semiconductor epitaxial wafer 11 along the first direction, and the second doping region A2 is parallel to and connected to the first doping region A1.
[0104] In the embodiment of the present application, the second conductive type ion doping of the second doped region A2 includes: implanting Al into the second doped region A2 at a high temperature (eg, 400° C.-600° C.) + , so as to form a second doping pre-region 150 in the second area to be doped A2.
[0105] Specific combination Fig.14 .
[0106] Step S26: performing ion doping of the second conductivity type on a portion of the second doping prefabricated region 150 close to the first surface to form a fifth doping region 16 in the second doping prefabricated region 150 ; wherein the portion of the second doping prefabricated region 150 other than the fifth doping region 16 serves as a fourth doping region 15 .
[0107] In the embodiment of the present application, the second doping prefabricated region 150 is further doped with a secondary doping at a portion close to the first surface. Specifically, the second doping prefabricated region 150 is further doped with B+ or Al at a high temperature. + Plasma is applied to form a fifth doping region 16 which is heavily doped by shallow implantation in a portion of the second doping prefabricated region 150 close to the first surface, and a portion of the second doping prefabricated region 150 other than the fifth doping region 16 serves as a fourth doping region 15 .
[0108] Specific combination Fig.15 .
[0109] Specifically, by performing in-situ secondary doping on the second area to be doped A2, a fourth doping area 15 with deep injection and light doping and a fifth doping area 16 with shallow injection and heavy doping are formed in the second area to be doped A2. Specifically, the fifth doping area 16 with shallow injection and heavy doping can reduce the Schottky barrier width of the device, thereby improving the contact resistance and on-resistance of the device, and is beneficial to reducing the leakage of the device, thereby increasing the switching speed of the device and reducing power consumption.
[0110] In one embodiment, see Figure 6 , step S25 specifically includes:
[0111] Step S251 : forming a second mask pattern B2 on the first surface of the semiconductor epitaxial wafer 11 , wherein the second mask pattern B2 has a second opening C2 at a position corresponding to the second region to be doped A2 .
[0112] In some embodiments, the material of the second mask pattern B2 may be the same as that of the first mask pattern B1 and the third mask pattern B3. The second opening C2 may be formed by an etching process, for example, by dry etching the mask layer forming the second mask pattern B2 to form a second mask pattern B2 having a second opening C2, and the second opening C2 exposes the second doped region A2.
[0113] In one embodiment, forming the second mask pattern B2 on the first surface of the semiconductor epitaxial wafer 11 includes: after the third doping region 14 and the second doping region 13 are formed, removing the first mask pattern B1 and forming the second mask pattern B2 on the first surface of the semiconductor epitaxial wafer 11 .
[0114] Specific combination Fig.13In some embodiments, wet etching or dry etching is used to remove the first mask pattern B1.
[0115] Specifically, by removing the first mask pattern B1 before forming the second doping prefabricated region 150 , it is possible to prevent the first mask pattern B1 from affecting the preparation of the mask pattern (ie, the second mask pattern B2 ) for subsequently forming the second doping prefabricated region 150 .
[0116] Step S252 : using the second opening C2 and adopting a third implantation energy and a third ion doping concentration, perform ion doping of the second conductivity type on the second to-be-doped region A2 of the semiconductor epitaxial wafer 11 to form a second doping prefabricated region 150 .
[0117] In some embodiments, the third ion doping concentration is 1e12-1e14 / cm 2 .
[0118] Specific combination Fig.14 In the embodiment of the present application, under high temperature (eg, 400° C.-600° C.), Al is implanted into the second to-be-doped region A2 using the second opening C2 with the third implantation energy and the third ion doping concentration. + , so as to form a second doping pre-region 150 in the second area to be doped A2.
[0119] In this step, due to the diffusion characteristics of ions, the second conductive type ions in the second doping prefabricated region 150 also diffuse to the second sub-region 122 in the third area to be doped A3 which does not correspond to the two third openings C3, so as to form a continuous first doping region 12 together with the two third doping prefabricated regions 120.
[0120] The second sub-region 122 is located between the two first sub-regions 121 and is connected to the two first sub-regions 121 respectively.
[0121] The area of the first doped region 12 located below the second doped pre-region 150 can be used as a channel region (MOS channel) of the device.
[0122] Further, step S26 specifically includes:
[0123] Step S261 : using the second opening C2 and adopting a fourth implantation energy and a fourth ion doping concentration, perform ion doping of the second conductivity type on a portion of the second doping prefabricated region 150 close to the first surface to form a fifth doping region 16 in the second doping prefabricated region 150 .
[0124] The fourth implantation energy is less than the third implantation energy; and the fourth ion doping concentration is greater than the third ion doping concentration.
[0125] It can be understood that the ion doping depth is positively correlated with the implantation energy. Therefore, in order to make the extension depth of the fifth doping region 16 along the first direction smaller than the extension depth of the fourth doping region 15 along the first direction, in the present application, the fourth implantation energy is smaller than the third implantation energy. In one embodiment, the fourth implantation energy is 30-70keV.
[0126] In order to make the ion doping concentration of the fifth doping region 16 greater than the ion doping concentration of the fourth doping region 15, the fourth ion doping concentration is 1e12-1e15 / cm 2 .
[0127] Specific combination Fig.15 In the embodiment of the present application, the second opening C2 is used to continue to implant B+ or Al into the portion of the second doping prefabricated region 150 close to the first surface under high temperature conditions. + Plasma is applied to form a fifth doping region 16 which is heavily doped by shallow implantation in a portion of the second doping prefabricated region 150 close to the first surface, and a portion of the second doping prefabricated region 150 other than the fifth doping region 16 serves as a fourth doping region 15 .
[0128] Specifically, the second region to be doped A2 is in-situ re-doped using the second mask pattern B2 to form a fourth doped region 15 with deep injection and light doping and a fifth doped region 16 with shallow injection and heavy doping. The formation of the fifth doped region 16 does not require an additional mask pattern, which can save process steps and optimize device performance.
[0129] See also Figure 16-Figure 21 , Fig.16 A schematic flow chart of another implementation of the method for manufacturing a semiconductor device provided in the first embodiment of the present application; Fig.17 for Fig.16 A schematic flow chart of an embodiment of step S5; Fig.18 for Fig.16 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S3; Fig.19 for Fig.16 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S4; Fig. 20 for Fig.17 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S51; Fig.21 for Fig.17 A schematic diagram of the structure of a portion of an intermediate product of an embodiment after step S52.
[0130] In one embodiment, the second mask pattern B2 includes a silicon dioxide layer B21 and a polysilicon layer B22. Fig.16 , the method for preparing the semiconductor device further comprises:
[0131] Step S3 : patterning the second mask pattern B2 to form a plurality of gate structures 17 .
[0132] In one embodiment, the gate structure 17 may be obtained by photolithography and dry etching the second mask pattern B2.
[0133] See Fig.18 , wherein each gate structure 17 extends from an edge of a first doping region 12 not covered by the third doping region 14 to an edge of another adjacent first doping region 12 not covered by the third doping region 14 .
[0134] Specifically, in the embodiment of the present application, by setting the second mask pattern B2 to include a stacked silicon dioxide layer B21 and a polysilicon layer B22, the second mask pattern B2 is made to have the same material and film layer structure as the gate structure 17 of the device, so that the gate structure 17 is formed using the second mask pattern B2, which can save preparation processes and thus save costs.
[0135] In one embodiment, the method for preparing a semiconductor device further includes:
[0136] Step S4 : forming a fourth mask pattern B4 on the first surface of the semiconductor epitaxial wafer 11 , wherein the fourth mask pattern B4 has a fourth opening C4 at a position corresponding to the fifth doping region 16 , and the fourth opening C4 also extends to at least a portion of the third doping region 14 connected to the fifth doping region 16 .
[0137] See Fig.19 The material of the fourth mask pattern B4 includes but is not limited to silicon dioxide, polysilicon, nitrogen dioxide, BPSG (boro-phospho-silicate glass), etc.
[0138] Specifically, the fourth mask pattern B4 can be formed by photolithography, development, etching, etc. The fourth opening C4 serves as an ohmic contact window of the device.
[0139] Step S5: forming an ohmic contact metal 18 in the fourth opening C4.
[0140] Specifically, the ohmic contact metal 18 is formed on the first surface of the semiconductor epitaxial wafer 11, and the ohmic contact metal 18 forms an ohmic contact with the fifth doping region 16 and the third doping region 14. Due to the shallow injection heavy doping structure of the third doping region 14 and the fifth doping region 16, the Schottky barrier width formed by the ohmic contact metal 18 and the third doping region 14 and the fifth doping region 16 can be reduced, thereby improving the device contact resistance and on-resistance, and is beneficial to reducing device leakage, thereby increasing the device switching speed and reducing power consumption.
[0141] In one embodiment, the ohmic contact metal 18 includes metal silicide, and the metal elements in the metal silicide include cobalt and titanium. Fig.17 , step S5 specifically includes:
[0142] Step S51 : depositing a titanium (Ti) metal layer 181 , a first cobalt (Co) metal layer 182 , a silicon (Si) layer 183 and a second cobalt (Co) metal layer 184 in sequence in the fourth opening C4 to form a prefabricated structure of the ohmic contact metal 18 .
[0143] See Fig. 20 , wherein the titanium metal layer 181 is deposited on the first surface of the semiconductor epitaxial wafer, and the titanium metal layer 181 has a first thickness, and the first thickness is 5-20 nm. For example, the first thickness is 5 nm, 10 nm, 15 nm or 20 nm, etc., which is selected according to actual needs.
[0144] The first cobalt metal layer 182 is deposited on the titanium metal layer 181, and the first cobalt metal layer 182 has a second thickness, and the second thickness is 30-200 nm. For example, the second thickness is 30 nm, 60 nm, 80 nm, 110 nm, 140 nm, 170 nm or 200 nm, etc., which is selected according to actual needs.
[0145] The silicon layer 183 is deposited on the first cobalt metal layer 182, and the silicon layer 183 has a third thickness, and the third thickness is 10-100 nm. For example, the third thickness is 10 nm, 30 nm, 60 nm, 80 nm or 100 nm, etc., which is selected according to actual needs.
[0146] The second cobalt metal layer 184 is deposited on the silicon layer 183, and the second cobalt metal layer 184 has a fourth thickness, and the fourth thickness is 20-200 nm. For example, the fourth thickness is 20 nm, 60 nm, 100 nm, 140 nm, 170 nm or 200 nm, etc., which is selected according to actual needs.
[0147] Step S52 : performing high temperature annealing treatment on the semiconductor epitaxial wafer with the prefabricated structure formed with the ohmic contact metal 18 to form the ohmic contact metal 18 .
[0148] See Fig.21Specifically, a titanium metal layer 181 and a first cobalt metal layer 182 are sequentially deposited in the fourth opening C4, and the titanium metal layer 181 and the first cobalt metal layer 182 are annealed at high temperature to form Ti-Co silicide, which helps to inhibit the diffusion of CoSi2 into the body to form good encapsulation, and further a silicon layer 183 and a second cobalt metal layer 184 are sequentially deposited on the first cobalt metal layer 182. When the prefabricated structure of the ohmic contact metal 18 is annealed at high temperature, the silicon layer 183 can provide more Si sources, and the Co element in the second cobalt metal layer 184 can diffuse downward to form a more uniform and dense CoSi, which helps to promote the formation of a denser and more uniform CoSi2 on the SiC surface, thereby facilitating the formation of an ohmic contact metal 18 that is resistant to high temperatures and has good high-temperature stability.
[0149] See also Fig. 20 In one embodiment, step S52 specifically includes:
[0150] Step S521: performing a first high temperature annealing treatment on the semiconductor epitaxial wafer having the prefabricated structure formed with the ohmic contact metal 18 at a first temperature.
[0151] Step S522: performing a second high temperature annealing treatment on the semiconductor epitaxial wafer after the first high temperature annealing treatment at a second temperature to form an ohmic contact metal.
[0152] In one embodiment, the first temperature is 300-500°C; the second temperature is 600-800°C.
[0153] Specifically, the first high temperature annealing helps to promote the alloying of the metal and semiconductor interface or form a low-impedance metallization layer, thereby reducing the resistance of the ohmic contact, and the second high temperature annealing can further optimize the alloy composition or the structure of the metal layer to ensure more stable contact performance. In addition, multiple annealing helps to optimize the characteristics of the metal and semiconductor interface, and the ohmic contact metal 18 after two high temperature annealing treatments can show higher thermal stability.
[0154] In one embodiment, after step S52, the residual metal is removed by a wet method.
[0155] Specifically, compared with the traditional process of using nickel (Ni) metal as the ohmic contact metal 18, NiSi is easily transformed into a high-resistance phase NiSi2 after high temperature >750°C, and the resistivity doubles, and it is easy to diffuse downward after high temperature, thereby increasing the leakage channel; in the present application, Co is treated at a high temperature of more than 600°C to form a low-resistivity CoSi2, and has good stability at high temperature and no line width effect. Ti is added to form Ti-Co silicide, which helps to inhibit the diffusion of CoSi2 into the body and thus form a good encapsulation. At the same time, Si / Co film is deposited on the Co surface (Si can provide more Si sources, and Co diffuses downward to form a more uniform and dense CoSi), which helps to promote the formation of a denser and more uniform CoSi2 on the SiC surface, thereby obtaining an ohmic contact metal 18 that is more resistant to high temperatures and has better high-temperature stability than Ni. The resistivity of the ohmic contact metal 18 can reach below 1e-6Ω·cm2, thereby improving the contact resistance and on-resistance of the device, and is beneficial to reducing device leakage, thereby increasing the device switching speed and reducing power consumption.
[0156] The following is a method for preparing a semiconductor device provided in a specific embodiment of the present application:
[0157] Step S101: After SiC (equivalent to the semiconductor epitaxial wafer 11) undergoes a series of preparation processes to the intermediate product (equivalent to the two third doping prefabricated regions 120) of PW (equivalent to the first doping region 12), the non-implanted region (i.e., the second sub-region 122) is blocked by a masking layer ((SiO2 / Poly)). Then a self-aligned masking layer (equivalent to the first mask pattern B1) is grown for the implantation of the N+ region (equivalent to the first doping prefabricated region 130), and dry etching is performed. The region of the third region to be doped A3 blocked by the masking layer is used as a MOS channel (device channel).
[0158] Step S102: Dry etching to obtain a self-aligned N+ implantation region for forming N-type doping. At this time, high temperature (500°C) ion implantation is performed to implant N+ implantation regions with the first doping prefabricated region 130 as the BSL (reference). + In addition, an additional low-energy, high-doping concentration N++ ion implantation (e.g. N + , P + 、As + The N++ heavily doped region (equivalent to the third doped region 14) is formed by the N+ region except the third doped region 14 as the second doped region 13. In this way, the shallow doping concentration is increased, the Schottky barrier width (SBW) is reduced, and the specific contact resistance, on-resistance, junction leakage and channel leakage are reduced.
[0159] Step S103: removing the SiC surface masking layer (ie, removing the first mask pattern B1 ) by wet etching.
[0160] Step S104: re-grow a masking layer (SiO2, Poly, etc.) (equivalent to the second mask pattern B2) on the surface for subsequent P+ ion implantation.
[0161] Step S105: P+ high temperature (500°C) ion implantation (Al+) forms P-type doping (equivalent to the second doping prefabricated region 150), and in addition, an additional low energy and high doping concentration P++ ion (B + or Al + ) is injected to form a P++ heavily doped region (equivalent to the fifth doping region 16), thereby increasing the shallow doping concentration, improving the later specific contact resistance, on-resistance and reducing junction leakage, and then high-temperature ion activation is used to achieve N and P type region doping.
[0162] Step S106: growing gate oxide (SiO2) and Poly on the entire first surface of the semiconductor epitaxial wafer 11 to manufacture a MOSgate structure (equivalent to the gate structure 17).
[0163] Step S107: Obtain the MOS Gate structure by photolithography and dry etching, and the Gate and PW overlay regions are the channel of the MOS, that is, the PW region below the gate structure 17 is the channel region of the device.
[0164] Step S108: growing an ILD dielectric layer (SiO2, BPSG) (equivalent to the fourth mask pattern B4).
[0165] Step S109: holes for forming OC (equivalent to the ohmic contact metal 18) are obtained by photolithography and dry etching, and over etching (10-50 nm) helps to achieve a larger contact area and reduce contact resistance.
[0166] Step S110: Ti (5-20 nm), Co (30-200 nm), Si (10-100 nm), and Co (20-200 nm) are sequentially deposited in the holes for subsequent formation of an OC layer.
[0167] Step S111: forming an ohmic contact metal 18 through high temperature annealing RTP1 (300-500° C.) and RTP2 (600-800° C.), and then removing the metal remaining on the SiC surface by wet method.
[0168] Specifically, compared with the traditional Ni-based metal silicide, NiSi is easily transformed into high-resistance phase NiSi2 after high temperature >750℃, and its resistivity doubles. It is also easy to diffuse downward after high temperature, increasing the leakage channel. Co forms low-resistivity CoSi2 after high-temperature treatment above 600℃, and has good stability at high temperature and no line width effect. Adding Ti to form Ti-Co silicide helps to inhibit the diffusion of CoSi2 into the body, thereby forming good encapsulation. At the same time, Si / Co film is deposited on the Co surface (Si can provide more Si sources, and Co diffuses downward to form a more uniform and dense CoSi), which helps to promote the formation of denser and more uniform CoSi2 on the SiC surface.
[0169] See also Fig. 22 , Fig. 22 This is a partial structural schematic diagram of a semiconductor device provided in the second embodiment of the present application. The second embodiment of the present application provides a semiconductor device, including: a semiconductor epitaxial wafer 21, a first doping region 22, a second doping region 23, a third doping region 24, a fourth doping region 25 and a fifth doping region 26.
[0170] The semiconductor epitaxial wafer 21 has a first conductivity type. In one embodiment, the semiconductor epitaxial wafer 21 is a silicon carbide (SiC) semiconductor epitaxial wafer 21, and the semiconductor epitaxial wafer 21 includes a substrate 211 and an epitaxial layer 212 grown on the substrate 211. The surface of the epitaxial layer 212 facing away from the substrate 211 is defined as the first surface of the semiconductor epitaxial wafer 21.
[0171] Among them, the first doped region 22 extends from the first surface of the semiconductor epitaxial wafer 21 along the first direction; the first doped region 22 has a second conductivity type, and the first direction is the direction from the first surface of the semiconductor epitaxial wafer 21 toward the inside of the semiconductor epitaxial wafer 21, that is, the first direction is the direction from the epitaxial layer 212 toward the substrate 211.
[0172] Among them, the second doping region 23 and the third doping region 24 are both arranged in the first doping region 22, the third doping region 24 extends from the first surface along the first direction, the second doping region 23 is located below the third doping region 24 and connected to the third doping region 24; the ion doping concentration of the third doping region 24 is greater than the ion doping concentration of the second doping region 23, and the second doping region 23 and the third doping region 24 both have the first conductivity type.
[0173] Among them, the fourth doping region 25 and the fifth doping region 26 are both arranged in the first doping region 22, the fifth doping region 26 extends from the first surface along the first direction, the fourth doping region 25 is located below the fifth doping region 26 and is connected to the fifth doping region 26; and the fourth doping region 25 is parallel to and connected to the second doping region 23, and the fifth doping region is parallel to and connected to the third doping region 24, the ion doping concentration of the fifth doping region 26 is greater than the ion doping concentration of the fourth doping region 25, and the fourth doping region 25 and the fifth doping region 26 both have the second conductivity type.
[0174] The first conductivity type is one of a P-type doped semiconductor and an N-type doped semiconductor, and the second conductivity type is the other of a P-type doped semiconductor and an N-type doped semiconductor, which can be selected according to actual needs.
[0175] Specifically, the semiconductor device provided by the present application forms a third doping region 24 that is heavily doped by in-situ shallow injection above the second doping region 23, and forms a fifth doping region 26 that is heavily doped by in-situ shallow injection above the fourth doping region 25. The third doping region 24 and the fifth doping region 26 that are heavily doped by in-situ shallow injection can reduce the Schottky barrier width of the device, thereby improving the contact resistance and on-resistance of the device, and are beneficial to reducing the leakage of the device, thereby increasing the switching speed of the device and reducing power consumption.
[0176] In one embodiment, the semiconductor device has a plurality of first doping regions 22 disposed at intervals. In the same first doping region 22 , the number of second doping regions 23 and the number of third doping regions 24 are both two, and the number of fourth doping regions 25 and the number of fifth doping regions 26 are both one.
[0177] Specifically, the two third doping regions 24 are opposite and spaced apart, the fifth doping region 26 is located between the two third doping regions 24 and is connected to both third doping regions 24 , and the depth of the fifth doping region 26 extending along the first direction is the same as the depth of the two third doping regions 24 extending along the first direction.
[0178] The two second doping regions 23 are respectively located below the two third doping regions 24, the fourth doping region 25 is located between the two second doping regions 23 and is connected to both second doping regions 23; and the depth of the fourth doping region 25 extending along the first direction is the same as the depth of the two second doping regions 23 extending along the first direction.
[0179] In some embodiments, the ion doping concentration of each doping region in the semiconductor device needs to be designed according to the required device characteristics. For example, the ion doping concentration of the first doping region 22 is 1e11-1e14 / cm 2 For example, the ion doping concentration of the first doping region 22 may be 1e11 / cm 2 , 1e11 / cm 2, 1e13 / cm 2 , or 1e14 / cm 2 wait.
[0180] For example, the ion doping concentration of the second doping region 23 is 1e12-1e15 / cm 2 For example, the ion doping concentration of the second doping region 23 may be 1e12 / cm 2 , 1e13 / cm 2 , 1e14 / cm 2 , or 1e15 / cm 2 wait.
[0181] For example, the ion doping concentration of the third doping region 24 is 1e13-1e16 / cm 2 For example, the ion doping concentration of the third doping region 24 may be 1e13 / cm 2 , 1e14 / cm 2 , 1e15 / cm 2 , or 1e16 / cm 2 wait.
[0182] For example, the ion doping concentration of the fourth doping region 25 is 1e12-1e14 / cm 2 For example, the ion doping concentration of the fourth doping region 25 may be 1e12 / cm 2 , 1e13 / cm 2 or 1e14 / cm 2 wait.
[0183] For example, the ion doping concentration of the fifth doping region 26 is 1e12-1e15 / cm 2 For example, the ion doping concentration of the fifth doping region 26 may be 1e12 / cm 2 , 1e13 / cm 2 , 1e14 / cm 2 , or 1e15 / cm 2 wait.
[0184] Specifically, the ion doping concentration of the third doping region 24 is set to (1e13-1e16 / cm 2 ) is greater than the ion doping concentration of the second doping region 23 (1e12-1e15 / cm 2 ), the third doping region 24 with shallow implantation and heavy doping can reduce the Schottky barrier width of the device, thereby improving the contact resistance and on-resistance of the device, and is conducive to reducing the leakage of the device, thereby increasing the switching speed of the device and reducing power consumption. The ion doping concentration of the fifth doping region 26 is set to (1e12~1e15 / cm 2 ) is greater than the ion doping concentration of the fourth doping region 25 (1e12-1e14 / cm 2), the shallowly implanted heavily doped fifth doping region 26 can reduce the Schottky barrier width of the device, thereby improving the contact resistance and on-resistance of the device, and is beneficial to reducing the leakage of the device, thereby increasing the switching speed of the device and reducing power consumption.
[0185] In one embodiment, the semiconductor device further includes an ohmic contact metal 27 , wherein the ohmic contact metal 27 is disposed on the first surface of the semiconductor epitaxial wafer 21 , and the ohmic contact metal 27 is located on the fifth doping region 26 , and is also located on at least a portion of the third doping region 24 connected to the fifth doping region 26 .
[0186] The ohmic contact metal 27 includes metal silicide, and the metal elements in the metal silicide include cobalt and titanium.
[0187] Specifically, cobalt silicide (CoSi2) has a low resistivity, good stability at high temperatures, no line width effect, and the metal silicide contains titanium (Ti), which helps to inhibit the diffusion of cobalt silicide into the semiconductor epitaxial layer 11, thereby obtaining an ohmic contact metal 27 that is more resistant to high temperatures and has better high temperature stability than Ni.
[0188] In one embodiment, the metal silicide is TiCoSi2-x. The metal silicide includes a buffer layer 271 and a conductive layer 272, wherein the buffer layer 271 is disposed on the first surface of the semiconductor epitaxial layer 11, and the buffer layer 271 is located on the fifth doping region 26, and is also located on at least a portion of the third doping region 24 connected to the fifth doping region 26, and the buffer layer 271 is a titanium layer. The conductive layer 272 is disposed on the surface of the buffer layer 271 away from the semiconductor epitaxial layer 11, and the conductive layer 272 includes cobalt silicide.
[0189] Specifically, the ohmic contact metal 27 is formed by high temperature annealing of a titanium metal layer, a first cobalt metal layer, a silicon layer, and a second cobalt metal layer sequentially formed on the fifth doping region 26 and a portion of the third doping region 24. The titanium layer does not participate in the reaction, but mainly plays a role in buffering and adhering the first cobalt metal layer, the silicon layer, and the second cobalt metal layer to form cobalt silicide by high temperature annealing. The cobalt silicide is used as an ohmic contact metal for transmitting electrical signals.
[0190] Specifically, compared with the traditional process of using nickel (Ni) metal as ohmic contact metal, NiSi is easy to become high-resistance phase NiSi2 after high temperature >750℃, and the resistivity doubles, and it is easy to diffuse downward after high temperature, thereby increasing the leakage channel; while Co forms low-resistivity CoSi2 after high-temperature treatment above 600℃, and has good stability at high temperature and no line width effect. Ti is added to form Ti-Co silicide, which helps to inhibit the diffusion of CoSi2 into the body and thus form good encapsulation. At the same time, Si / Co film is deposited on the Co surface (Si can provide more Si sources, and Co diffuses downward to form a more uniform and dense CoSi), which helps to promote the formation of denser and more uniform CoSi2 on the SiC surface, thereby obtaining an ohmic contact metal 27 that is more resistant to high temperature and has better high-temperature stability than Ni, and the resistivity of the ohmic contact metal 27 can reach 1e-6Ω·cm 2 The following further improves the device contact resistance and on-resistance, and helps to reduce device leakage, thereby increasing the device switching speed and reducing power consumption.
[0191] Furthermore, the semiconductor device also includes an insulating layer 28 for device insulation, and an electrode structure for electrical connection with an external device, wherein the electrode structure includes a gate structure 291 , a source structure 292 and a drain structure 293 .
[0192] The above description is only an implementation method of the present application, and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A method for preparing a semiconductor device, characterized in that: include: Providing a semiconductor epitaxial wafer, wherein the semiconductor epitaxial wafer has a first conductivity type; forming a first doping region, a second doping region, a third doping region, a fourth doping region and a fifth doping region on the semiconductor epitaxial wafer; Wherein, the first doped region extends from the first surface of the semiconductor epitaxial wafer along a first direction; the first doped region has a second conductivity type, and the first direction is a direction extending from the first surface of the semiconductor epitaxial wafer toward the inside of the semiconductor epitaxial wafer; The second doping region and the third doping region are both arranged in the first doping region, the third doping region extends from the first surface along the first direction, the second doping region is located below the third doping region and is connected to the third doping region; the ion doping concentration of the third doping region is greater than the ion doping concentration of the second doping region, and the second doping region and the third doping region both have the first conductivity type; The fourth doping region and the fifth doping region are both arranged in the first doping region, the fifth doping region extends from the first surface along the first direction, the fourth doping region is located below the fifth doping region and is connected to the fifth doping region; and the fourth doping region is parallel to and connected to the second doping region, and the fifth doping region is parallel to and connected to the third doping region, the ion doping concentration of the fifth doping region is greater than the ion doping concentration of the fourth doping region, and the fourth doping region and the fifth doping region both have the second conductivity type.
2. The preparation method according to claim 1, characterized in that: The forming of the second doping region and the third doping region on the semiconductor epitaxial wafer comprises: Performing ion doping of a first conductivity type on a first region to be doped of the semiconductor epitaxial wafer to form a first doping prefabricated region; wherein the first region to be doped extends from a first surface of the semiconductor epitaxial wafer along the first direction; Performing ion doping of the first conductivity type on a portion of the first doping prefabricated region close to the first surface to form the third doping region in the first doping prefabricated region; wherein the portion of the first doping prefabricated region other than the third doping region serves as the second doping region; The forming of the fourth doping region and the fifth doping region on the semiconductor epitaxial wafer comprises: Performing ion doping of a second conductivity type on a second region to be doped of the semiconductor epitaxial wafer to form a second doping prefabricated region; wherein the second region to be doped extends from the first surface of the semiconductor epitaxial wafer along a first direction, and the second region to be doped is parallel to and connected to the first region to be doped; The second conductive type ion doping is performed on a portion of the second doping prefabricated region close to the first surface to form the fifth doping region in the second doping prefabricated region; wherein the portion of the second doping prefabricated region other than the fifth doping region serves as the fourth doping region.
3. The preparation method according to claim 2, characterized in that: The step of performing ion doping of a first conductivity type on the first to-be-doped region of the semiconductor epitaxial wafer to form a first doping prefabricated region includes: forming a first mask pattern on a first surface of the semiconductor epitaxial wafer, wherein the first mask pattern has a first opening at a position corresponding to the first region to be doped; Using the first opening and adopting a first implantation energy and a first ion doping concentration, ion doping of a first conductivity type is performed on a first region to be doped of the semiconductor epitaxial wafer to form the first doping prefabricated region; The step of performing ion doping of the first conductivity type on a portion of the first doped prefabricated region close to the first surface to form the third doped region in the first doped prefabricated region includes: Using the first opening and adopting a second implantation energy and a second ion doping concentration, ion doping of the first conductivity type is performed on a portion of the first doping prefabricated region close to the first surface, so as to form the third doping region in the first doping prefabricated region; Among them, the second injection energy is less than the first injection energy; and the second ion doping concentration is greater than the first ion doping concentration.
4. The preparation method according to claim 3, characterized in that: The step of performing ion doping of a second conductivity type on the second to-be-doped region of the semiconductor epitaxial wafer to form a second doping prefabricated region includes: forming a second mask pattern on the first surface of the semiconductor epitaxial wafer, wherein the second mask pattern has a second opening at a position corresponding to the second region to be doped; Using the second opening and adopting a third implantation energy and a third ion doping concentration, ion doping of a second conductivity type is performed on the second to-be-doped region of the semiconductor epitaxial wafer to form the second doping prefabricated region; The step of performing ion doping of the second conductivity type on a portion of the second doped prefabricated region close to the first surface to form the fifth doped region in the second doped prefabricated region includes: Using the second opening and adopting a fourth implantation energy and a fourth ion doping concentration, ion doping of a second conductivity type is performed on a portion of the second doping prefabricated region close to the first surface, so as to form the fifth doping region in the second doping prefabricated region; Among them, the fourth injection energy is less than the third injection energy; and the fourth ion doping concentration is greater than the third ion doping concentration.
5. The preparation method according to claim 4, characterized in that: The semiconductor epitaxial wafer further includes a third region to be doped, the third region to be doped extending from the first surface of the semiconductor epitaxial wafer along the first direction, and the first region to be doped and the second region to be doped are both located in the third region to be doped; Forming a first doped region on the semiconductor epitaxial wafer, comprising: forming a third mask pattern on the first surface of the semiconductor epitaxial wafer, wherein the third mask pattern has two third openings spaced apart at positions corresponding to the third region to be doped, and positions of the two third openings correspond one-to-one to positions of two first sub-regions spaced apart in the third region to be doped; Performing ion doping of the second conductivity type on the two first sub-regions by using the two third openings, so as to form two third doping prefabricated regions distributed at intervals in the third region to be doped; Among them, the second conductive type ions in the second doping prefabricated region are also diffused to the second sub-region in the third region to be doped, the position of which does not correspond to the two third openings, so as to form a continuous first doping region together with the two third doping prefabricated regions, wherein the second sub-region is located between the two first sub-regions and is respectively connected to the two first sub-regions.
6. The preparation method according to claim 5, characterized in that: After two third doping prefabricated regions distributed at intervals are formed, the first mask pattern is grown using the third mask pattern; The forming of a second mask pattern on the first surface of the semiconductor epitaxial wafer comprises: After the third doping region and the second doping region are formed, the first mask pattern is removed, and a second mask pattern is formed on the first surface of the semiconductor epitaxial wafer.
7. The preparation method according to any one of claims 1 to 6, characterized in that: The preparation method further comprises: forming a fourth mask pattern on the first surface of the semiconductor epitaxial wafer, wherein the fourth mask pattern has a fourth opening at a position corresponding to the fifth doping region, and the fourth opening also extends to at least a portion of the third doping region connected to the fifth doping region; An ohmic contact metal is formed in the fourth opening, wherein the ohmic contact metal is formed on the first surface of the semiconductor epitaxial wafer, the ohmic contact metal comprises metal silicide, and the metal elements in the metal silicide comprise cobalt and titanium.
8. The preparation method according to claim 7, characterized in that: The step of forming an ohmic contact metal in the fourth opening comprises: Depositing a titanium metal layer, a first cobalt metal layer, a silicon layer and a second cobalt metal layer in the fourth opening in sequence to form a prefabricated structure of the ohmic contact metal, wherein the titanium metal layer is deposited on the first surface of the semiconductor epitaxial wafer; The semiconductor epitaxial wafer formed with the prefabricated structure is subjected to high temperature annealing treatment to form the ohmic contact metal.
9. The preparation method according to claim 8, characterized in that: The thickness of the titanium metal layer is 5-20 nm; The thickness of the first cobalt metal layer is 30-200 nm; The thickness of the silicon layer is 10-100 nm; The thickness of the second cobalt metal layer is 20-200 nm.
10. The preparation method according to claim 8, characterized in that: The step of performing high temperature annealing on the semiconductor epitaxial wafer having the prefabricated structure to form the ohmic contact metal comprises: Performing a first high-temperature annealing treatment on the semiconductor epitaxial wafer having the prefabricated structure at a first temperature; Performing a second high temperature annealing treatment on the semiconductor epitaxial wafer after the first high temperature annealing treatment at a second temperature to form the ohmic contact metal; Wherein, the first temperature is 300-500°C, and the second temperature is 600-800°C.
11. A semiconductor device, characterized in that: include: A semiconductor epitaxial wafer, wherein the semiconductor epitaxial wafer has a first conductivity type; A first doped region extending from a first surface of the semiconductor epitaxial wafer along a first direction; The first doped region has a second conductivity type, and the first direction is a direction extending from the first surface of the semiconductor epitaxial wafer toward the inside of the semiconductor epitaxial wafer; a second doping region and a third doping region, wherein the second doping region and the third doping region are both arranged in the first doping region, the third doping region extends from the first surface along the first direction, the second doping region is located below the third doping region and is connected to the third doping region; the ion doping concentration of the third doping region is greater than the ion doping concentration of the second doping region, and the second doping region and the third doping region both have a first conductivity type; A fourth doping region and a fifth doping region, wherein the fourth doping region and the fifth doping region are both arranged in the first doping region, the fifth doping region extends from the first surface along the first direction, the fourth doping region is located below the fifth doping region and is connected to the fifth doping region; and the fourth doping region is parallel to and connected to the second doping region, the fifth doping region is parallel to and connected to the third doping region, the ion doping concentration of the fifth doping region is greater than the ion doping concentration of the fourth doping region, and the fourth doping region and the fifth doping region both have a second conductivity type.
12. The semiconductor device according to claim 11, characterized in that In the first doping region, the number of the second doping region and the number of the third doping region are both two, and the number of the fourth doping region and the number of the fifth doping region are both one; The two third doping regions are arranged opposite to each other and spaced apart, the fifth doping region is located between the two third doping regions and is connected to both the third doping regions, and the depth of the fifth doping region extending along the first direction is the same as the depth of the two third doping regions extending along the first direction; The two second doping regions are respectively located below the two third doping regions, the fourth doping region is located between the two second doping regions and is connected to both second doping regions; and the depth of the fourth doping region extending along the first direction is the same as the depth of the two second doping regions extending along the first direction.
13. The semiconductor device according to claim 11, characterized in that The ion doping concentration of the first doping region is 1e11-1e14 / cm 2 ; The ion doping concentration of the second doping region is 1e12-1e15 / cm 2 ; The ion doping concentration of the third doping region is 1e13-1e16 / cm 2 ; The ion doping concentration of the fourth doping region is 1e12-1e14 / cm 2 ; The ion doping concentration of the fifth doping region is 1e12-1e15 / cm 2 .
14. The semiconductor device according to any one of claims 11 to 13, characterized in that: The semiconductor device further comprises: An ohmic contact metal is disposed on the first surface of the semiconductor epitaxial layer, and the ohmic contact metal is located on the fifth doping region and also on at least a portion of the third doping region connected to the fifth doping region; Wherein, the ohmic contact metal includes metal silicide, and the metal elements in the metal silicide include cobalt and titanium.
15. The semiconductor device according to claim 14, characterized in that The metal silicide is TiCoSi2-x; The metal silicide comprises: a buffer layer, the buffer layer being disposed on the first surface of the semiconductor epitaxial layer, and the buffer layer being located on the fifth doping region and also being located on at least a portion of the third doping region connected to the fifth doping region, the buffer layer being a titanium layer; A conductive layer is provided on a surface of the buffer layer away from the semiconductor epitaxial layer, and the conductive layer comprises cobalt silicide.