Mass transfer and self-bonding preparation method of micron-sized chip

By designing special structures for Micro-LED chips and driver substrates, using external forces to drive self-growth interconnection and metal self-growth interconnection technology in electroless plating solution, the problems of uniformity and alignment accuracy in traditional bonding technology are solved, and efficient Micro-nano-scale alignment and electrical connection improve huge transfer efficiency and yield.

CN118919626APending Publication Date: 2024-11-08JINJIANG BOGAN ELECTRONIC TECH CO LTD
0 Cites 0 Cited by

Patent Information

Application Number
CN202411004146.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-08

Smart Images

  • Figure CN118919626A_ABST
    Figure CN118919626A_ABST
Patent Text Reader

Abstract

The invention relates to a micron-sized chip mass transfer and self-bonding preparation method, and belongs to the technical field of integrated circuits and photoelectric display. The micron-sized chip is provided with a special structure, the target substrate bonded with the micron-sized chip is provided with a special structure array for bearing the corresponding micron-sized chip, and the micron-sized chip and the special structure array corresponding to the micron-sized chip on the target substrate are driven by external force to realize self-growth interconnection and achieve the purpose of self-bonding. According to the method disclosed by the invention, firm bonding of a physical structure and good electrical connection can be realized, and micro-nano-scale high-precision alignment can be realized in a chip self-bonding preparation process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of integrated circuits and optoelectronic displays, and in particular relates to a method for mass transfer and self-bonding preparation of micron-level chips. Background Art

[0002] Display technology is the third largest manufacturing industry in my country. Display technology has developed from CRT (cathode ray tube) display to LCD (liquid crystal) display and OLED (organic light emitting diode) display. The next generation of display technology - highly integrated semiconductor information display (HISID) will develop towards high integration, ultra-high resolution, immersive high interactivity and true three-dimensional. Interactive and true three-dimensional future information display requires high density and high integration of light sources. Compared with traditional LCD display and OLED display, inorganic light-emitting devices Micro-LED with light-emitting units less than 30μm will play an irreplaceable role in future display technology with the advantages of lower power consumption, wider color gamut, longer life, faster response speed and stronger thermal stability. Micro-LED arrays with micron-sized pixels can not only serve as high-density light sources, but also integrate detectors to sense and collect spatial three-dimensional environment and human motion information in real time to achieve high interactivity. In addition, Micro-LED can also be widely used in the fields of high-performance display devices such as smartphones / watches, high-end TVs, in-vehicle / airborne displays, flexible displays and transparent displays.

[0003] Micro-LED needs to overcome a series of problems to gain an absolute position in future displays, especially the mass transfer technology used for full-colorization and the bonding of Micro-LED chips to the driver substrate. Micro-LED chips and driver substrates are electrically and physically connected through the flip-chip bonding process. In traditional flip-chip bonding technology, metal bumps provide both electrical and physical bonding between chip layers and between chip layers and driver substrate layers. This technology usually has the following problems:

[0004] 1. The uniformity of the metal bump structure is very high. The high temperature and high pressure conditions in the bump bonding process will cause the metal bump to expand, deform, and be damaged; during the evaporation and reflow process of the metal bump, the height and shape of the metal bump are inconsistent; the stability, integrity and uniformity (especially the height) of the metal bump structure affect the physical and electrical connection between the chip and the driver substrate.

[0005] 2. Bonding alignment accuracy. The pick and place operation of chips in full-color mass transfer technology and the connection between the pixels of Micro-LED chips and the pixels of the driver substrate require extremely high alignment accuracy. In particular, the period of the light-emitting unit of Micro-LED chips used in AR / VR technology is less than 10μm, requiring the alignment accuracy of metal bumps to be lower than the micron level. Summary of the invention

[0006] The purpose of the present invention is to overcome the above-mentioned problems and provide a method for mass transfer and self-bonding preparation of micron-level chips, which can achieve firm physical structure bonding and good electrical connection, and the chip self-bonding preparation process can achieve high-precision alignment at the micro-nano level.

[0007] To achieve the above-mentioned purpose, the technical solution of the present invention is: a method for mass transfer and self-bonding preparation of micron-level chips, the micron-level chip has a special structure, and the target substrate bonded thereto has a special structural array for receiving the corresponding micron-level chip, and the micron-level chip and the special structural array of the corresponding micron-level chip on the target substrate are driven by external force to achieve self-growth interconnection and achieve the purpose of self-bonding.

[0008] In one embodiment of the present invention, the special structure of the micron-level chip refers to a micron-level structure attached to the micron-level chip formed by micron-level processing, and the target substrate has a special structure array for receiving the corresponding micron-level chip, which refers to a micron-level structure array formed on the target substrate by micron-level processing according to the structural characteristics of the micron-level chip and is conducive to receiving the corresponding micron-level chip.

[0009] In one embodiment of the present invention, the micron-level chip is a mixture of one or more of MicroLED, micron-level IC chip, micro-nano sensor device, micron-level energy management device, micron-level photoelectric conversion device, micron-level driving chip, and micron-level signal transmission device.

[0010] In one embodiment of the present invention, the target substrate is a substrate substrate having a mixture of one or more of CMOS circuits, thin film transistor circuits, transistor circuit matrices, and IC circuit matrices.

[0011] In one embodiment of the present invention, the substrate itself is a mixture of one or more of a glass substrate, a silicon substrate, a sapphire substrate, a PCB, a quartz substrate, and a flexible organic material substrate.

[0012] In one embodiment of the present invention, the external driving force is a mixture of one or more of mechanical force (including pressure), electricity, magnetism, gravity, impact force caused by viscosity change caused by temperature change, laser-guided viscosity reduction impact force, and impact force caused by laser peeling.

[0013] In one embodiment of the present invention, the self-bonding is based on metal self-growth interconnection in a chemical plating solution.

[0014] In one embodiment of the present invention, the self-bonding specifically includes the following steps:

[0015] 1) Prepare the plating solution for wettability;

[0016] 2) Wetting properties of special micron-scale chips;

[0017] 3) The surface wettability of the special structure array of the target substrate corresponding to the micron-level chip is adjusted so that the special structure array of the target substrate can receive the corresponding micron-level chip, realize the self-growth and interconnection of metal bumps and have good ohmic contact at the same time.

[0018] In one embodiment of the present invention, in step 1), the wettability of the plating solution is prepared by adding a surfactant to a mixed or alloy plating solution of one or more of copper, nickel, chromium, indium, tin, silver, gold, tungsten, titanium, and platinum, wherein the surfactant is a non-ionic surfactant, including: alkylphenol polyoxyethylene ether, fatty acid polyoxyethylene ester, long-chain fatty alcohol polyoxyethylene ether, polyoxyethylene alkylamide, polyoxyethylene alkylamine and polyethers, and the added concentration is 1-500 mg / L.

[0019] In one embodiment of the present invention, the special structure of the micron-level chip specifically refers to a structure that increases buoyancy, which helps to reduce the acceleration of the micron-level chip under gravity, resulting in excessive impact force when the micron-level chip is bonded to the target substrate; the target substrate bonded thereto has a special structural array that can accommodate the corresponding micron-level chip, specifically refers to an array formed by a container shape or a structure that fixes the micron-level chip.

[0020] Compared with the prior art, the present invention has the following beneficial effects: The present invention realizes simple physical bonding between the micron-scale chip and the driving substrate through a special structure. The electrodes of the chip and the electrodes of the driving substrate realize a firm physical structure bonding and have a good electrical connection at the same time by self-bonding. The chip self-bonding preparation process can realize high-precision alignment and bonding at the micro-nano level. Compared with the existing hot pressing or laser welding technology, the bonding technology of the present invention, since the electrodes of the micron-scale chip and the electrodes of the driving substrate do not need to be in direct contact during pre-bonding, but are physically and electrically connected through subsequent self-bonding, it no longer requires very precise alignment and strict requirements for very high parallelism in large areas, which can greatly reduce the requirements for transfer accuracy, and can realize large-area mass transfer and bonding, thereby improving the transfer efficiency and yield of the chip. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1It is a schematic diagram of the Micro-LED structure of the preferred embodiment 1 of the present invention.

[0022] Figure 2 It is a schematic diagram of a driving substrate according to a preferred embodiment of the present invention.

[0023] Figure 3 This is a schematic diagram of conventional chip from laser peeling to laser transfer to bonding.

[0024] Figure 4 It is a schematic diagram of a driving substrate according to a second preferred embodiment of the present invention. DETAILED DESCRIPTION

[0025] The technical solution of the present invention is described in detail below in conjunction with the accompanying drawings.

[0026] It should be noted that the following detailed descriptions are illustrative and are intended to provide further explanation of the present application. Unless otherwise specified, all technical and scientific terms used herein have the same meanings as those commonly understood by those skilled in the art to which the present application belongs.

[0027] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present application; as used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, they indicate the presence of features, steps, operations, devices, components and / or their combinations.

[0028] The present invention provides a method for mass transfer and self-bonding preparation of micron-level chips. The micron-level chip has a special structure, and the target substrate bonded thereto has a special structural array for receiving the corresponding micron-level chip. The micron-level chip and the special structural array of the corresponding micron-level chip on the target substrate are driven by external force to achieve self-growth interconnection and achieve the purpose of self-bonding.

[0029] Example 1

[0030] like Figure 1 As shown, the first embodiment of the present invention provides a method for wettability adjustment of the special structure of the Micro-LED chip. The special structure of the Micro-LED chip refers to a structure attached to the Micro-LED chip formed by micro-nano processing. A structure that increases buoyancy helps to reduce the impact force when the chip is bonded to the substrate due to acceleration of the chip under gravity. The above structure helps to more accurately control the bonding of the Micro-LED chip and the thin-film transistor circuit substrate under the drive of the laser peeling impact force.

[0031] like Figure 2As shown, the present invention adjusts the surface wettability of the thin film transistor circuit substrate structure so that the structure can receive the Micro-LED chip, realize the self-growth and interconnection of metal bumps and have good ohmic contact at the same time. The metal self-growth interconnection refers to the self-growth interconnection of nickel metal bumps, and the target substrate is a thin film transistor circuit substrate; the substrate itself is a mixture of one or more of a sapphire substrate, a quartz substrate, and a flexible organic material substrate. The thin film transistor circuit substrate has a special structure array that can receive the corresponding Micro-LED chip. It refers to a micro-nano structure array that is formed on the thin film transistor circuit substrate through micro-nano processing according to the structural characteristics of the chip, which is conducive to receiving the chip. Specifically, it refers to a container-shaped structure array. The above-mentioned structure array helps to more accurately control the bonding of the Micro-LED chip and the thin film transistor circuit substrate under the impact force of laser peeling.

[0032] Driven by the impact force of laser stripping, the Micro-LED chip is knocked off the sapphire substrate onto the thin-film transistor circuit substrate of the container-shaped structure array filled with chemical nickel plating solution, and is embedded with the container-shaped structure, so that the Micro-LED chip and the array structure on the thin-film transistor circuit substrate can achieve self-growth interconnection and self-bonding. The self-bonding is based on the metal self-growth interconnection in the chemical plating solution, including: 1) wettability adjustment of the plating solution; 2) wettability adjustment of the special structure of the micron-level chip; 3) surface wettability adjustment of the target substrate structure, so that the target substrate structure can receive the micron-level chip, achieve metal bump self-growth and interconnection, and have good ohmic contact at the same time. The metal self-grown interconnection comprises: the wettability of the plating solution in step 1) is prepared by adding a surfactant to a mixed or alloy plating solution of one or more of copper, nickel, chromium, indium, tin, silver, gold, tungsten, titanium, and platinum, wherein the surfactant is a non-ionic surfactant, including: alkylphenol polyoxyethylene ether, fatty acid polyoxyethylene ester, long-chain fatty alcohol polyoxyethylene ether, polyoxyethylene alkylamide, polyoxyethylene alkylamine, and polyethers, etc., and the added concentration is 1-500 mg / L.

[0033] Today’s mass transfer and bonding solutions include Figure 3 As shown, firstly, the chip array 1 is formed by laser peeling off the sapphire substrate of COW (Chip on Wafer) to transfer the chip to the temporary transfer substrate 1, and then the chip array 2 is formed by transferring the chip from the temporary transfer substrate 1 to the transfer substrate 2 according to the pixel pitch arrangement requirement, and the chip array 2 is bonded to the drive substrate from the transfer substrate 2 by heat pressing or laser. The self-bonding method of Example 1 of the present invention saves the intermediate steps, realizes the integration of the peeling of the chip and the sapphire substrate to the transfer and bonding of the drive substrate, and greatly improves the efficiency of mass transfer.

[0034] Example 2

[0035] like Figure 4 As shown, the second embodiment of the present invention provides a method for adjusting the surface wettability of a thin film transistor (TFT) circuit substrate structure, so that the structure can receive and fix the Micro-LED chip, realize the self-growth and interconnection of metal bumps and have good ohmic contact at the same time. The metal self-growth interconnection is a nickel metal bump self-growth interconnection, and the target substrate is a thin film transistor circuit; the substrate itself is a mixture of one or more of a sapphire substrate, a quartz substrate, and a flexible organic material substrate. The thin film transistor circuit substrate has a special structure array corresponding to the Micro-LED chip, which refers to a micro-nano structure that is formed on the thin film transistor circuit substrate through micro-nano processing according to the characteristics of the chip structure and is conducive to receiving the chip, and specifically refers to a structure for fixing the Micro-LED chip. The above structure not only helps to more accurately control the bonding of the Micro-LED chip and the thin film transistor circuit substrate under pressure drive, but also helps to avoid the short circuit between the positive and negative electrodes of the Micro-LED chip during the bonding process, and can indirectly compensate for a certain alignment deviation, thereby improving the bonding yield.

[0036] After the Micro-LED chip is fixed on the thin-film transistor circuit substrate with a special structure under the driving force of pressure, it is then placed in a chemical nickel plating solution with a certain temperature and wettability, so that the Micro-LED chip and the array structure on the thin-film transistor circuit substrate can achieve self-growth interconnection and achieve the purpose of self-bonding. The self-bonding is based on the metal self-growth interconnection in the chemical plating solution, including: 1) wettability adjustment of the plating solution; 2) wettability adjustment of the special structure of the micron-level chip; 3) surface wettability adjustment of the target substrate structure, so that the target substrate structure can receive the micron-level chip, achieve self-growth and interconnection of metal bumps and have good ohmic contact at the same time. The metal self-grown interconnection comprises: the wettability of the plating solution in step 1) is prepared by adding a surfactant to a mixed or alloy plating solution of one or more of copper, nickel, chromium, indium, tin, silver, gold, tungsten, titanium, and platinum, wherein the surfactant is a non-ionic surfactant, including: alkylphenol polyoxyethylene ether, fatty acid polyoxyethylene ester, long-chain fatty alcohol polyoxyethylene ether, polyoxyethylene alkylamide, polyoxyethylene alkylamine, and polyethers, etc., and the added concentration is 1-500 mg / L.

[0037] The above is only a preferred embodiment of the present invention, and does not limit the present invention in other forms. Any technician familiar with the profession may use the above disclosed technical content to change or modify it into an equivalent embodiment with equivalent changes. However, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the technical solution of the present invention still belongs to the protection scope of the technical solution of the present invention.

Claims

1. A method for mass transfer and self-bonding of micron-scale chips. It is characterized in that The micron-level chip has a special structure, and the target substrate bonded to it has a special structural array for receiving the corresponding micron-level chip. Driven by external force, the micron-level chip and the special structural array of the corresponding micron-level chip on the target substrate achieve self-growth interconnection and achieve the purpose of self-bonding.

2. A method for mass transfer and self-bonding of micron-scale chips according to claim 1, It is characterized in that The special structure of the micron-level chip refers to a micron-level structure attached to the micron-level chip formed by micron-level processing, and the target substrate has a special structure array that can accommodate the corresponding micron-level chip, which refers to a micron-level structure array that is formed on the target substrate by micron-level processing according to the structural characteristics of the micron-level chip and is conducive to accommodating the corresponding micron-level chip.

3. A method for mass transfer and self-bonding of micron-scale chips according to claim 1, It is characterized in that The micron-level chip is a mixture of one or more of MicroLED, micron-level IC chip, micro-nano-level sensor device, micron-level energy management device, micron-level photoelectric conversion device, micron-level driving chip, and micron-level signal transmission device.

4. A method for mass transfer and self-bonding of micron-scale chips according to claim 1, It is characterized in that The target substrate is a substrate substrate having a mixture of one or more of CMOS circuits, thin film transistor circuits, transistor circuit matrices, and IC circuit matrices.

5. A method for mass transfer and self-bonding of micron-scale chips according to claim 4, It is characterized in that The substrate itself is a mixture of one or more of a glass substrate, a silicon substrate, a sapphire substrate, a PCB, a quartz substrate, and a flexible organic material substrate.

6. A method for mass transfer and self-bonding of micron-scale chips according to claim 1, It is characterized in that The external force driving is a mixture of one or more of mechanical force, electric force, magnetic force, gravity, impact force caused by viscosity change due to temperature change, laser-guided viscosity reduction impact force, and impact force caused by laser stripping.

7. A method for mass transfer and self-bonding of micron-scale chips according to claim 1, It is characterized in that The self-bonding is based on the self-growth interconnection of metal in a chemical plating solution.

8. A method for mass transfer and self-bonding of micron-scale chips according to claim 7, It is characterized in that The self-bonding specifically comprises the following steps: 1) Prepare the plating solution for wettability; 2) Wetting properties of special micron-scale chips; 3) The surface wettability of the special structure array of the target substrate corresponding to the micron-level chip is adjusted so that the special structure array of the target substrate can receive the corresponding micron-level chip, realize the self-growth and interconnection of metal bumps and have good ohmic contact at the same time.

9. A method for mass transfer and self-bonding of micron-scale chips according to claim 8, It is characterized in that In step 1), the wettability of the plating solution is prepared by adding a surfactant to a mixed or alloy plating solution of one or more of copper, nickel, chromium, indium, tin, silver, gold, tungsten, titanium, and platinum. The surfactant is a non-ionic surfactant, including: alkylphenol polyoxyethylene ether, fatty acid polyoxyethylene ester, long-chain fatty alcohol polyoxyethylene ether, polyoxyethylene alkylamide, polyoxyethylene alkylamine and polyethers, and the added concentration is 1-500 mg / L.

10. A method for mass transfer and self-bonding of micron-scale chips according to claim 1 or 2, It is characterized in that The special structure of the micron-level chip specifically refers to a structure that increases buoyancy, which helps to reduce the acceleration of the micron-level chip under gravity, resulting in excessive impact force when the micron-level chip is bonded to the target substrate; the target substrate bonded thereto has a special structural array that can accommodate the corresponding micron-level chip, specifically refers to an array formed by a container shape or a structure that fixes the micron-level chip.