Manufacturing method for embedding cavity in base material layer of embedded substrate
The non-circular cavity is made through Plasma equipment and rapid etching and copper biting technology, and the built-in circuit is made by combining Sputter E-less and additive methods, which solves the shortcomings of cavity and circuit production in the existing technology, and achieves precise control and lightweightness. The volume demand of short electronic products.
Patent Information
- Application Number
- CN202410139685.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-27
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-09-27
AI Technical Summary
The existing circuit board production technology cannot effectively produce non-circular cavity and embedded circuits, and the depth control of embedded components is inaccurate, making it difficult to meet the volume requirements of thin and short electronic products.
Plasma equipment and rapid etching and copper biting technology are used to make embedded cavity of different sizes and shapes on the substrate layer, and embedded circuits are made through Sputter E-less and additive methods to ensure precise control of line width and thickness.
It realizes efficient production of non-circular cavity and embedded circuit, improves the depth control accuracy of embedded components, and meets the volume requirements of thin and short electronic products.
Smart Images

Figure CN118921845A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of circuit board manufacturing, and in particular relates to a manufacturing method of an embedded substrate in which a cavity is embedded in a base material layer. Background Art
[0002] In recent years, electronic products have been widely used in daily work and life, and light, thin and small electronic products are becoming more and more popular. As the main component of electronic products, flexible circuit boards occupy a large space of electronic products, so the volume of flexible circuit boards largely affects the volume of electronic products. Large-volume flexible circuit boards are bound to be difficult to meet the trend of light, thin, short and small electronic products.
[0003] In the manufacturing process of existing circuit boards, the cavity is made by drilling in the substrate layer, which is only suitable for the production of circular cavities and cannot control the depth of the embedded components. Summary of the invention
[0004] The main purpose of the present invention is to provide a method for manufacturing an embedded substrate by embedding a cavity in a base material layer, so as to overcome the shortcomings of the prior art.
[0005] In order to achieve the above-mentioned invention object, the technical solution adopted by the present invention includes:
[0006] According to a first aspect of an embodiment of the present invention, there is provided a method for manufacturing an embedded substrate in which a cavity is embedded in a base material layer, comprising the following steps:
[0007] P1. Select a BT substrate containing an upper attached copper layer and a lower attached copper layer as a base material layer, and remove the upper attached copper layer and the lower attached copper layer on the surface of the base material layer.
[0008] P2, opening a through hole on the substrate layer, and making a resin plug on the through hole;
[0009] P3, forming a first metal copper layer on the upper surface and the lower surface of the substrate layer respectively;
[0010] P4, opening a window on the first metal copper layer, and opening an embedded cavity on the substrate layer corresponding to the window;
[0011] P5. placing the magnetic material assembly in the embedded cavity and fixing it;
[0012] P6. Remove the first metal copper layer on the upper surface and the lower surface of the substrate layer, attach a first ABF to the surface of the substrate layer, and press the first ABF into the embedded cavity and the surface of the substrate layer;
[0013] P7. Disposing a second metal copper layer on the first ABF, and opening a window on the second metal copper layer;
[0014] P8, opening an embedded circuit cavity on the first ABF and the substrate layer corresponding to the window opening;
[0015] P9, removing the second metal copper layer, and providing a third metal copper layer on the surface of the first ABF and the buried circuit cavity;
[0016] P10, thickening the third metal copper layer until the embedded circuit cavity is filled;
[0017] P11, remove the third metal copper layer and the first ABF to form an embedded circuit;
[0018] P12, attaching a second ABF on the surface of the substrate layer, providing a fourth metal copper layer on the second ABF, and making circuit openings on the fourth metal copper layer;
[0019] P13, opening a conducting blind hole at the circuit window, wherein the conducting blind hole penetrates the second ABF and is connected to the embedded circuit;
[0020] P14, making an embedded circuit slot at the conductive blind hole, and removing the fourth metal copper layer;
[0021] P15, a fourth metal copper layer is provided on the surface of the second ABF and the inner buried line slot, the inner buried line slot is filled and the fourth metal copper layer is thickened to form an outer layer circuit build-up layer;
[0022] P16. Remove the fourth electroplated copper layer.
[0023] Furthermore, in step P1, a via layer is opened on the substrate layer by mechanical or laser processing.
[0024] Further, the step P2 comprises:
[0025] (1) In the opened via hole layer, a layer of metal copper is coated on the surface of the substrate layer and the hole wall by electroplating process;
[0026] (2) Filling the via layer with insulating resin material through a resin plugging process;
[0027] (3) Use a brushing device to brush off the resin material and the copper metal on the surface of the substrate layer that protrudes beyond the above-mentioned plugging hole.
[0028] At this time, there are only substrate layer materials and resin plugging holes.
[0029] Furthermore, the step P3 includes: forming a layer of metal copper on the surface of the substrate layer through a Sputter E-less process.
[0030] Further, the step P4 comprises:
[0031] (1) Covering the light-transmissive dry film on the copper layer where the embedded cavity is to be made by a hot pressing process, and exposing and developing the position where the embedded component cavity is to be made;
[0032] (2) Use a rapid etching method to etch away the unprotected copper layer, exposing the underlying substrate layer;
[0033] (3) using a plasma device to dig a cavity for an embedded component in the substrate layer at a position not protected by the copper layer, and when the plasma device acts on the substrate layer, the substrate layer material is decomposed downward;
[0034] (4) The remaining dry film covering the metal copper layer in step (1) is removed, and only the metal copper on the base material layer and the buried cavity remain on the surface of the substrate.
[0035] Furthermore, in step (3), the substrate layer material is decomposed downwards, and according to the size and shape of the magnetic component, the thickness is based on the thickness of the embedded component required by the customer + / - 5um.
[0036] Furthermore, the step P5 includes: picking up a magnetic material attached to the tape, and placing it into the cavity after position alignment; when placing it into the cavity, the position deviation must be less than + / -5um.
[0037] Furthermore, the step P6 comprises:
[0038] (1) removing the metal copper described in step P3 by rapid etching;
[0039] (2) taking two portions of dielectric ABF dry film materials, and attaching the ABF dry film to the upper and lower surfaces of the substrate layer through a lamination and hot pressing process, so that the upper and lower surfaces of the substrate layer are covered with a layer of ABF dry film and the buried cavity space on the upper surface of the substrate layer is filled at the same time;
[0040] Further, the step P7 comprises:
[0041] (1) gradually plating a layer of metal copper on the surface of the ABF described in step P6 by a Sputter E-less process;
[0042] (2) A light-transmitting dry film is attached to the thin copper layer on both sides through a lamination and hot pressing process, and a circuit pattern is produced on the dry film through a UV exposure machine. Subsequently, exposure and development are performed to reveal the position of the inner layer circuit groove;
[0043] (3) Use a fast etching method to etch away the unprotected copper layer, exposing the ABF dielectric layer underneath;
[0044] Furthermore, the step P8 includes: using a plasma device to act on the light-transmitting ABF dry film to decompose the ABF material downwards, and continuously decompose the resin material of the substrate layer downwards to form the position of the embedded wiring groove.
[0045] Furthermore, the step P9 comprises:
[0046] (1) using a rapid etching method to remove the copper metal described in step P7(1);
[0047] (2) Through the Sputter E-less process, a layer of metal copper is gradually plated on the cavity and ABF surface in step P7(2).
[0048] Furthermore, the step P10 includes: making an embedded inner layer circuit by an additive method, thickening the metal copper in the above step P9 (2), and filling the embedded circuit groove to form an embedded circuit.
[0049] Compared with the prior art, the advantages of the present invention include:
[0050] (1) The present invention provides a method for manufacturing an embedded substrate by embedding a cavity in a base material layer. Unlike the previous drilling operation method which can only produce circular embedded cavities, the plasma device can operate embedded cavities of different sizes and shapes on the ABF dielectric material, and the thickness can be more effectively controlled than laser or mechanical drilling.
[0051] (2) It is difficult to make embedded circuits in the existing substrate layer. The present invention provides a method for making embedded circuits in the substrate layer, and the width and thickness of the embedded circuits can be better controlled. BRIEF DESCRIPTION OF THE DRAWINGS
[0052] By reading the detailed description of the preferred embodiment below, various other advantages and benefits will become clear to those of ordinary skill in the art. The accompanying drawings are only used for the purpose of illustrating the preferred embodiment and are not considered to be limitations of the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings.
[0053] Figure 1 It is a schematic diagram of the structure of a substrate layer in a typical embodiment of the present invention;
[0054] Figure 2 It is a schematic diagram of the structure of making a resin plug hole on a through hole in a typical embodiment of the present invention;
[0055] Figure 3 It is a schematic structural diagram of forming a first metal copper layer on the surface of a substrate layer in a typical embodiment of the present invention;
[0056] Figure 4aIt is a structural schematic diagram of a typical embodiment of the present invention in which an embedded cavity is provided on a substrate layer corresponding to a window opening;
[0057] Figure 4b It is a schematic structural diagram of a typical embodiment of the present invention in which a buried cavity is opened on a substrate layer corresponding to a window opening by a plasma device; Figure 5 It is a schematic diagram of a structure in which a magnetic material is placed in a cavity in a typical embodiment of the present invention;
[0058] Figure 6 It is a schematic diagram of a structure in which a first ABF is attached to the surface of the substrate layer in a typical embodiment of the present invention;
[0059] Figure 7a It is a schematic structural diagram of a typical embodiment of the present invention in which a second metal copper layer is disposed on a first ABF;
[0060] Figure 7b It is a schematic diagram of a structure in which a window is opened on the second metal copper layer in a typical embodiment of the present invention;
[0061] Figure 8 A schematic diagram of the structure of the position of the internal buried wire routing groove in a typical embodiment of the present invention;
[0062] Figure 9a It is a schematic diagram of a structure in which the second metal copper layer is removed in a typical embodiment of the present invention;
[0063] Figure 9b It is a schematic structural diagram of a typical embodiment of the present invention in which a third metal copper layer is provided on the surface of the first ABF and the embedded circuit cavity;
[0064] Fig.10 It is a schematic diagram of a structure in which a cavity for buried circuits is filled in a typical embodiment of the present invention;
[0065] Fig.11 It is a schematic diagram of a structure in which the third metal copper layer and the first ABF are removed to form an embedded circuit in a typical embodiment of the present invention;
[0066] Fig.12 This is a schematic diagram of a structure in which a fourth metal copper layer is disposed on a first ABF and a circuit window is made on the fourth metal copper layer in a typical embodiment of the present invention;
[0067] Fig.13 It is a structural schematic diagram of a typical embodiment of the present invention in which a conducting blind hole is provided at a circuit window;
[0068] Fig.14a It is a schematic diagram of the structure of making an embedded circuit slot at a conductive blind hole in a typical embodiment of the present invention;
[0069] Fig.14bIt is a schematic diagram of a structure in which the fourth metal copper layer is removed in a typical embodiment of the present invention; Fig.15 It is a schematic diagram of a structure for forming an outer circuit build-up layer in a typical embodiment of the present invention;
[0070] Fig.16 It is a schematic structural diagram of removing the fourth electroplated copper layer in a typical embodiment of the present invention;
[0071] Markings in the figure: substrate layer 101, resin plug hole 102, first metal copper layer 103, buried cavity 104, magnetic material 105, first ABF 106, second metal copper layer 107, window 108, third metal copper layer 109, second ABF 110, fourth metal copper layer 111, fourth electroplated copper layer 112. DETAILED DESCRIPTION
[0072] In view of the deficiencies in the prior art, the inventor of this case has proposed the technical solution of the present invention after long-term research and extensive practice. The technical solution, its implementation process and principle will be further explained as follows.
[0073] The present invention is further described in detail below in conjunction with specific embodiments, and the examples provided are only for illustrating the present invention, rather than for limiting the scope of the present invention. The examples provided below can be used as a guide for further improvements by those of ordinary skill in the art, and do not constitute a limitation of the present invention in any way.
[0074] The experimental methods in the following examples, unless otherwise specified, are all conventional methods, and are performed according to the techniques or conditions described in the literature in the field or according to the product instructions. The materials, reagents, etc. used in the following examples, unless otherwise specified, can all be obtained from commercial channels.
[0075] An embodiment of the present invention provides a method for manufacturing an embedded substrate by embedding a cavity in a base material layer, comprising the following steps:
[0076] P1. Select a BT substrate containing an upper attached copper layer and a lower attached copper layer as the base material layer 101, and remove the upper attached copper layer and the lower attached copper layer on the surface of the base material layer 101; in a specific implementation, a BT substrate without an upper attached copper layer and a lower attached copper layer can also be directly selected as the base material layer 101; Figure 1 As shown;
[0077] P2, opening a through hole on the substrate layer 101, and making a resin plug hole 102 on the through hole; Figure 2 Specifically, the steps include:
[0078] (1) In the opened via hole layer, a layer of metal copper is coated on the surface of the substrate layer 101 and the hole wall by electroplating process;
[0079] (2) Filling the via layer with insulating resin material through a resin plugging process;
[0080] (3) Use a brushing device to brush off the resin material and the metal copper on the surface of the substrate layer 101 that protrude beyond the above-mentioned plugging holes. At this time, only the substrate layer 101 material and the resin plugging holes are left.
[0081] P3, forming a first metal copper layer 103 on the upper surface and the lower surface of the substrate layer 101 respectively; forming the first metal copper layer 103 on the surface of the substrate layer 101 through the Sputter E-less process; Figure 3 shown.
[0082] P4, opening a window 108 on the first metal copper layer 103, and opening an embedded cavity 104 on the substrate layer 101 corresponding to the window 108; Figure 4a and 4b Specifically, the steps include:
[0083] (1) Covering the light-transmissive dry film on the copper layer where the embedded cavity 104 is to be made by a hot pressing process, and exposing and developing the position where the embedded component cavity is to be made;
[0084] (2) using a rapid copper etching method to etch away the unprotected copper layer, thereby exposing the underlying substrate layer 101;
[0085] (3) using a plasma device to dig the embedded component cavity of the substrate layer 101 at a position not protected by the copper layer, and when the plasma device acts on the substrate layer 101, the material of the substrate layer 101 is decomposed downward;
[0086] (4) The remaining dry film covering the metal copper layer in step (1) is removed, and only the metal copper on the base material layer 101 and the buried cavity 104 remain on the surface of the substrate.
[0087] P5. Place the magnetic material 105 component in the embedded cavity 104 and fix it; specifically, pick up a magnetic material 105 attached to the tape, and after positioning, put it into the cavity; when placing it in the cavity, the position deviation must be less than + / -5um; Figure 5 shown.
[0088] P6, removing the first metal copper layer 103 on the upper and lower surfaces of the substrate layer 101, attaching a first ABF 106 on the surface of the substrate layer 101, and pressing the first ABF 106 into the embedded cavity 104 and the surface of the substrate layer 101; Figure 6 Specifically, the steps include:
[0089] P7, disposing a second metal copper layer 107 on the first ABF 106, and opening a window 108 on the second metal copper layer 107; Figure 7a As shown, a second metal copper layer is disposed on the first ABF; as Figure 7b As shown, a schematic diagram of a structure in which a window is opened on the second metal copper layer;
[0090] P8. An embedded circuit cavity is formed on the first ABF 106 and the substrate layer 101 corresponding to the window 108. Specifically, the plasma device acts on the light-transmitting ABF dry film to decompose the ABF material downwards, and continuously decomposes the resin material of the substrate layer 101 downwards to form an embedded circuit groove position. Specifically, the substrate layer 101 material is decomposed downwards, and the thickness is based on the size and shape of the magnetic component and is greater than the thickness of the embedded component required by the customer by + / - 5um. Figure 8 shown.
[0091] P9, remove the second metal copper layer 107, and set a third metal copper layer 109 on the surface of the first ABF 106 and the embedded circuit cavity;
[0092] Figure 9a A schematic diagram of the structure for removing the second metal copper layer; Figure 9b A schematic diagram of a structure for providing a third metal copper layer on the surface of the first ABF and the buried circuit cavity; specifically, the following steps are included:
[0093] (1) using a rapid etching method to remove the copper metal described in step P7(1);
[0094] (2) Through the Sputter E-less process, a layer of metal copper is gradually plated on the cavity and ABF surface in step P7(2).
[0095] P10, thickening the third metal copper layer 109 until the embedded circuit cavity is filled; Fig.10 Specifically, it includes making an embedded inner layer circuit by an additive method, thickening the metal copper in step P9 (2) above, filling the embedded circuit groove to form an embedded circuit.
[0096] P11, remove the third metal copper layer 109 and the first ABF 106 to form an embedded circuit, such as Fig.11 As shown;
[0097] P12, attaching a second ABF 110 to the surface of the substrate layer 101, providing a fourth metal copper layer 111 on the second ABF 110, and making a circuit opening 108 on the fourth metal copper layer 111, as shown in FIG. Fig.12 As shown;
[0098] P13, a conducting blind hole is opened at the circuit opening 108, and the conducting blind hole passes through the second ABF 110 and is connected to the embedded circuit, such as Fig.13 As shown;
[0099] P14, making an embedded circuit slot at the conductive blind hole, and removing the fourth metal copper layer 111; Fig.14a A schematic diagram of the structure of making an embedded circuit slot at a conductive blind hole; Fig.14b A schematic diagram of the structure for removing the fourth metal copper layer;
[0100] P15, a fourth electroplated copper layer 112 is provided on the surface of the second ABF 110 and the inner buried line slot, the inner buried line slot is filled and the fourth electroplated copper layer 112 is thickened to form an outer layer circuit build-up layer; Fig.15 Specifically, the steps include:
[0101] (1) The outer line trench and via hole trench in the outer ABF are made by two plasma equipments. The via hole trench needs to be connected downward to the inner line copper layer. The width and depth of the outer line trench in the ABF need to meet the customer's line width and copper thickness specifications of + / -5um.
[0102] (2) After forming the wiring trench and the via layer, a thin copper layer is formed on the surface of the via and the ABF dielectric layer through an E-less process;
[0103] (3) The outer buried circuit copper layer is produced through the build-up electroplating process, and the hole layer is filled simultaneously.
[0104] P16, removing the fourth electroplated copper layer 112, such as Fig.16 Specifically, it includes brushing off the electroplated copper on the upper and lower surfaces through the CMP (Chemical Mechanical Plating) process to form an outer layer buried circuit.
[0105] The above are only some embodiments of the present invention. It should be pointed out that for ordinary technicians in this field, other modifications and improvements can be made without departing from the creative concept of the present invention, which all belong to the protection scope of the present invention.
Claims
1. A method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer, characterized in that: The following steps are involved: P1. Select a BT substrate containing an upper attached copper layer and a lower attached copper layer as a base material layer, and remove the upper attached copper layer and the lower attached copper layer on the surface of the base material layer; P2, opening a through hole on the substrate layer, and making a resin plug on the through hole; P3, forming a first metal copper layer on the upper surface and the lower surface of the substrate layer respectively; P4, opening a window on the first metal copper layer, and opening an embedded cavity on the substrate layer corresponding to the window; P5. placing the magnetic material assembly in the embedded cavity and fixing it; P6. Remove the first metal copper layer on the upper surface and the lower surface of the substrate layer, attach a first ABF to the surface of the substrate layer, and press the first ABF into the embedded cavity and the surface of the substrate layer; P7. Disposing a second metal copper layer on the first ABF, and opening a window on the second metal copper layer; P8, opening an embedded circuit cavity on the first ABF and the substrate layer corresponding to the window opening; P9, removing the second metal copper layer, and providing a third metal copper layer on the surface of the first ABF and the buried circuit cavity; P10, thickening the third metal copper layer until the embedded circuit cavity is filled; P11, remove the third metal copper layer and the first ABF to form an embedded circuit; P12, attaching a second ABF on the surface of the substrate layer, providing a fourth metal copper layer on the second ABF, and making circuit openings on the fourth metal copper layer; P13, opening a conducting blind hole at the circuit window, wherein the conducting blind hole penetrates the second ABF and is connected to the embedded circuit; P14, making an embedded circuit slot at the conductive blind hole and removing the fourth metal copper layer; P15, a fourth metal copper layer is provided on the surface of the second ABF and the inner buried line slot, the inner buried line slot is filled and the fourth metal copper layer is thickened to form an outer layer circuit build-up layer; P16. Remove the fourth electroplated copper layer.
2. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: In step P2, a via layer is opened on the substrate layer by mechanical or laser processing.
3. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: The step P3 comprises: Using the Sputter E-less process, a layer of metallic copper is formed on the surface of the substrate layer.
4. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: The step P4 comprises: (1) Covering the light-transmissive dry film on the copper layer where the embedded cavity is to be made by a hot pressing process, and exposing and developing the position where the embedded component cavity is to be made; (2) Use a rapid etching method to etch away the unprotected copper layer, exposing the underlying substrate layer; (3) using a plasma device to dig a cavity for an embedded component in the substrate layer at a position not protected by the copper layer, and when the plasma device acts on the substrate layer, the substrate layer material is decomposed downward; (4) The remaining dry film covering the copper layer in step (1) is removed, and only the metal copper on the base material layer and the buried cavity remain on the surface of the substrate.
5. The method for manufacturing an embedded substrate having a cavity and an embedded circuit embedded in a base material layer according to claim 4, It is characterized in that In step (3), the substrate layer material is decomposed downwards, and according to the size and shape of the magnetic component, the thickness is based on the thickness of the embedded component required by the customer + / - 5um.
6. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: The step P5 includes: picking up a magnetic material attached to the tape, and placing it into the cavity after positioning.
7. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: The step P7 comprises: (1) gradually plating a layer of metal copper on the surface of the ABF described in step P6 by a Sputter E-less process; (2) A light-transmitting dry film is attached to the thin copper layer on both sides through a lamination and hot pressing process, and a circuit pattern is produced on the dry film through a UV exposure machine. Subsequently, exposure and development are performed to reveal the position of the inner layer circuit groove; (3) Use a fast copper etching method to etch away the unprotected copper layer, exposing the ABF dielectric layer underneath.
8. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: The step P8 includes: using a plasma device to act on the light-transmissive ABF dry film to decompose the ABF material downwards, and continuously decompose the resin material of the substrate layer downwards to form a location for an internally embedded wiring groove.
9. The method for manufacturing an embedded substrate with a cavity embedded in a base material layer according to claim 8, characterized in that: The width and depth of the buried wiring trench in the resin material of the substrate layer must meet the customer's line width and copper thickness specifications of + / -5um.
10. The method for manufacturing an embedded substrate by embedding a cavity and an embedded circuit in a base material layer according to claim 1, characterized in that: The step P15 comprises: (1) The outer layer line grooves and via holes are made in the outer layer ABF by two plasma equipments. The via holes need to be connected downward to the inner layer line copper layer; (2) After forming the wiring trench and the via layer, a thin copper layer is formed on the surface of the via and the ABF dielectric layer through an E-less process; (3) The outer buried circuit copper layer is produced through the build-up electroplating process, and the hole layer is filled simultaneously.
Citation Information
Patent Citations
Embedded circuit board and manufacturing method thereof
CN102123566A
Circuit board, semiconductor device mfg. method, and electroplating system
CN1387239A
Method of manufacturing printed circuit board
KR1020100049842A
Printed circuit board and manufacturing method thereof
KR1020140113009A
Cited By
Conduction alignment method of base material layer embedded magnetic material
CN120786820A