Tundish and continuous casting method using same
By designing a structure of a dike and porous portion with wall and eaves in the tundra, combined with appropriate inactive gas flow rate and prefabricated refractory, the problems of poor inclusion floating effect and molten steel pollution in the prior art are solved. , achieving efficient improvement in the cleanliness of molten steel.
Patent Information
- Application Number
- CN202380033072.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-26
- Filing Date
- 2023-03-16
- Publication Date
- 2024-11-08
AI Technical Summary
In the prior art, it is difficult to effectively remove non-metallic inclusions in the molten steel during the casting process, and excessive gas injection will lead to contamination of the molten steel, and the inclusions will not float up the inclusions or have high cost.
A tundra is designed, including a dike with a wall and an eaves. The bottom of the dike has a porous part and a gas inlet pipe. By adjusting the flow rate of inactive gas and setting prefabricated refractories, the up-floating separation of inclusions is promoted and the middle is prevented. The slag is wrapped in.
It effectively inhibits the short-circuit flow of the molten steel, promotes the up-floating separation of inclusions, improves the cleanliness of molten steel, and avoids molten steel pollution and cost increase.
Smart Images

Figure CN118922261A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a tundish and a continuous casting method using the tundish, wherein the tundish is used to relay molten metal injected from a ladle and supply the molten metal to a casting mold in a continuous casting process, and can efficiently remove non-metallic inclusions in the molten metal injected into the tundish. Background Art
[0002] In order to produce high-quality steel materials, it is required to further improve the high cleanliness technology of molten steel. Non-metallic inclusions such as Al2O3 in molten steel, which are deoxidation products, become the cause of defects after rolling, so they need to be separated and removed as much as possible before casting. The tundish has the function of floating and separating the non-metallic inclusions that flow out with the molten steel when pouring molten steel from the ladle. The larger the floating separation ratio, the higher the cleanliness of molten steel can be produced.
[0003] So far, methods for efficiently floating and separating inclusions in a tundish have been proposed. For example, Patent Document 1 discloses a technique for promoting the floating effect of inclusions by a method for manufacturing clean steel, wherein the tundish is divided into a steel receiving area for receiving molten steel from a ladle and a quasi-static area of steel having an outlet toward a mold, and a perforated weir extending from the bottom to a position higher than the surface of the molten steel is provided in the tundish, and the molten steel is supplied by immersing an injection nozzle from the ladle in the molten steel in the steel receiving area.
[0004] Patent document 2 discloses the following technology: a tundish which is divided into a steel receiving side and an outlet side by a perforated weir having holes connected to a bottom wall, wherein a lower weir with an open top is provided on the outlet side of the perforated weir, and the shape of the tundish, the position of the weir, the shape of the hole and the position of the hole are optimized.
[0005] In addition, Patent Document 3 discloses the following technology: a weir with flow holes is provided midway between the injection position from the ladle and the outflow port to the casting mold, and a specified amount of inert gas is blown into the bottom of the ladle on the outflow port side of the weir to enhance the effect of floating inclusions.
[0006] Prior art literature Patent Literature Patent Document 1: Japanese Patent Application Laid-Open No. 53-6231 Patent Document 2: Japanese Patent Application Laid-Open No. 10-216909 Patent Document 3: Japanese Patent Application Publication No. 2011-143449 Summary of the invention
[0007] Problems to be solved by the invention
[0008] However, the above-mentioned prior art has the following problems.
[0009] In the technology described in Patent Document 1, a hole for extracting excess steel is provided on the bottom side of the tundish with a perforated weir. After the inclusions in the molten steel pass near the bottom of the perforated weir, the inclusions may flow out due to the short-circuit flow flowing toward the molten steel outlet near the bottom of the tundish.
[0010] In the technology of Patent Document 2, inclusions in molten steel are promoted to float up by the lower weir after passing through the perforated weir, but the floating effect is insufficient. In addition, since molten steel remains on the steel receiving side of the lower weir after casting, the excess steel cost may increase.
[0011] In the technology of Patent Document 3, although the inclusion floating effect is improved by blowing inert gas, the inclusion floating effect is small unless the gas volume ratio of the gas in the molten steel is increased. On the contrary, if the gas flow rate is increased, the surface of the molten steel shakes when the bubbles burst, and the tundish slag existing on the surface of the molten steel may be involved, causing the molten steel to be contaminated.
[0012] The present invention has been made in view of the above circumstances, and an object of the present invention is to provide a tundish capable of effectively and inexpensively promoting the floating of inclusions contained in molten steel poured from a ladle into a tundish, and to propose a continuous casting method using the tundish.
[0013] Technical solutions to solve problems
[0014] The tundish of the present invention for solving the above-mentioned problems is characterized in that a weir is provided between a molten steel injection part and a molten steel outflow port, the molten steel injection part is a position where the molten steel injection flow from the ladle collides with the bottom of the tundish, the molten steel outflow port is a position where the molten steel flows out from the tundish to the mold, the weir has a wall portion and an eaves portion, the wall portion surrounds the molten steel injection part from four sides and extends upward from the bottom of the tundish, the eaves portion protrudes toward the molten steel injection part side in the horizontal direction at the upper end of the wall portion, the weir has one or more notches continuous from the wall portion to the eaves portion, a first porous portion is provided at the bottom of the refractory surrounded by the wall portion, a first gas introduction pipe is provided in the weir and in the refractory including the first porous portion, the first gas introduction pipe is connected to the first porous portion, and the tundish further optionally has a bottom refractory at the bottom of the tundish between the weir and the molten steel outflow port, the bottom refractory having a second porous portion and a second gas introduction pipe connected to the second porous portion.
[0015] In addition, the tundish involved in the present invention also has a prefabricated refractory, which has a third gas introduction pipe inside and is installed on the wall of the tundish. The third gas introduction pipe is connected to the first gas introduction pipe or the second gas introduction pipe, or extends from the first gas introduction pipe or the second gas introduction pipe, which can become a more preferred solution.
[0016] The continuous casting method according to the present invention is characterized in that, using the tundish, the inert gas flow rate R1 per unit area of the bottom of the weir is adjusted to 0.02 to 1.0 NL / (s·m 2 ) in the range of , while blowing inert gas into molten steel from the first porous portion through the first gas inlet pipe, the steel slab is continuously cast by casting from the tundish to the mold.
[0017] In addition, the continuous casting method according to the present invention further adjusts the inert gas flow rate R2 per unit area to 0.1 to 10 NL / (s·m 2 ) range, and blowing inert gas into the molten steel from the second porous portion through the second gas inlet pipe, which can become a more preferred solution.
[0018] Effects of the Invention
[0019] According to the tundish of the present invention, the short-circuit flow of molten steel injected from the ladle flowing at the bottom of the tundish can be suppressed and the flow can be changed to flow upward, thereby promoting the floating separation of inclusions. In addition, the rising of bubbles from the porous part of the weir can promote the floating separation of inclusions.
[0020] The tundish according to the present invention is preferred because it can further promote the floating separation of inclusions before flowing into the mold by blowing bubbles into the molten steel from the porous portion of the bottom refractory provided between the weir and the molten steel outlet.
[0021] In addition, the tundish of the present invention is also provided with a prefabricated refractory, so that a device for blowing gas from a porous portion provided at the bottom of the weir or the bottom of the tundish can be easily installed, and the prefabricated refractory has a gas introduction pipe inside and is installed on the wall of the tundish. Therefore, it is possible to suppress the operation obstruction caused by poor installation, there is no danger of steel leakage, etc., it is safe, and therefore it is preferred.
[0022] According to the continuous casting method of the present invention, since the above-mentioned tundish is used, the amount of inactive gas injected from the bottom of the weir and the bottom of the tundish is within an appropriate range, so that the floating separation of inclusions is sufficient, and the entrapment of tundish slag from the surface of molten steel can be suppressed. Therefore, high-cleanliness steel can be easily produced. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 1 and 2 are cross-sectional views schematically showing a tundish according to an embodiment of the present invention, wherein (a) is a cross-sectional view taken along the arrow AA, (b) is a cross-sectional view taken along the arrow BB, and (c) is a cross-sectional view taken along the arrow CC. Figure 2 This is a graph showing the effect of the inert gas flow rate R1 per unit area of the bottom of the weir on the number of inclusions flowing out into the steel slab. Figure 3 This is a graph showing the effect of the inert gas flow rate R2 per unit area of the porous portion of the refractory provided at the bottom of the tundish on the amount of inclusions flowing out into the steel slab. Figure 4 This is a graph showing the number of inclusions flowing out of steel slabs cast under the gas injection conditions shown in Table 1. DETAILED DESCRIPTION
[0024] The following is a detailed description of the embodiments of the present invention. In addition, the drawings are schematic and sometimes different from reality. In addition, the following embodiments illustrate the device and method for implementing the technical idea of the present invention, and do not specify the structure as the following structure. That is, the technical idea of the present invention can be modified in various ways within the technical scope described in the claims.
[0025] The tundish according to one embodiment of the present invention is schematically shown in Figure 1 . Figure 1 (a) is the sectional view taken along the AA line. Figure 1 (b) is the cross-sectional view from the BB direction. Figure 1 (c) is a cross-sectional view taken along the CC direction. The tundish 1 of this embodiment is an intermediate container used in the continuous casting of steel, and is used to inject molten steel in the ladle into the continuous casting mold. The tundish 1 is, for example, a substantially rectangular container with an open top surface. Molten steel is supplied from the ladle (not shown) via the injection nozzle 2. Figure 1 In the example of FIG. 1 , the stored molten steel is supplied to a casting mold (not shown) from two molten steel outlets 3 provided at the bottom.
[0026] In this embodiment, a weir 4 is provided between a molten steel injection portion 2a, where the molten steel injection flow from the ladle collides with the bottom 1a of the tundish, and a molten steel outlet 3, where the molten steel flows out from the tundish 1 to the mold. The weir 4 includes a wall portion 4a that surrounds the molten steel injection portion 2a from all sides and extends upward from the bottom 1a of the tundish; and an eaves portion 4b that protrudes horizontally from the upper end of the wall portion 4a toward the molten steel injection portion 2a. The weir 4 includes one or more notches that are continuous from the wall portion 4a to the eaves portion 4b. The weir 4 includes a first porous portion 4d at the refractory bottom 4c surrounded by the wall portion 4a, and a first gas introduction pipe 5a connected to the first porous portion 4d in the weir and in the refractory including the first porous portion 4d. The first porous portion 4d preferably occupies 15% or more of the total area of the refractory bottom 4c surrounded by the wall portion 4a of the weir 4. The upper limit is not limited, but is preferably not set near the collision point of the molten steel injection flow from the ladle.
[0027] By forming such a structure, the short-circuit flow of the molten steel injected from the ladle flowing at the bottom 1a of the tundish can be suppressed, and the flow is changed to upward, thereby promoting the floating separation of inclusions. In addition, by blowing inert gas from the first porous portion 4d, non-metallic inclusions can be captured in the inert gas bubbles, further promoting the floating separation. By providing the first porous portion 4d at the refractory bottom 4c of the molten steel injection portion 2a, due to the shear force caused by the high-speed injection flow toward the horizontal direction due to the collision with the refractory bottom 4c, the gas bubbles separated from the first porous portion 4d are miniaturized, and the effect of increasing the probability of capturing inclusions can be obtained.
[0028] Figure 2 The graph shows the inert gas flow rate R1 [NL / (s·m 2 )] on the number of inclusions flowing out of the steel casting. For the number of inclusions flowing out of the steel casting, five samples were taken from the two widest faces of the rectangular steel billet, the observation surface was polished, and the number of inclusions larger than 10μm in the steel billet was evaluated by the number of inclusions per unit area under a microscope. Figure 2 It is clear that when R1 is less than 0.02NL / (s·m 2 ) is not preferred because the inclusions in the tundish have a small floating effect. On the other hand, when R1 exceeds 1.0NL / (s·m 2 ) is too much gas injection, which increases the entrapment of tundish slag, and is therefore not preferred. Therefore, the inert gas flow rate R1 per unit area at the bottom of the weir 4 needs to be adjusted to 0.02 to 1.0 NL / (s·m 2 Preferably, the inert gas flow rate R1 is 0.02 to 0.2 NL / (s·m2 ) range.
[0029] For the supply of the inert gas to the first porous portion 4d, it is preferred to provide a prefabricated refractory 6 having a third gas introduction pipe 5c inside and installed on the wall of the tundish 1, wherein the third gas introduction pipe 5c is connected to or extends from the first gas introduction pipe 5a provided on the weir 4. Thus, the installation of the refractory to the tundish becomes simple, and the operation obstruction caused by poor installation can be suppressed.
[0030] In the present embodiment, it is preferred that a refractory 7 is optionally provided at the bottom 1a of the tundish between the weir 4 and the molten steel outlet 3, and the refractory 7 has a second porous portion 7a and a second gas inlet pipe 5b connected to the second porous portion 7a. It is preferred that a prefabricated refractory 6 is provided, and the prefabricated refractory 6 has a third gas inlet pipe 5c inside and is installed on the wall of the tundish 1, and the third gas inlet pipe 5c is connected to the second gas inlet pipe 5b or is formed by extending the second gas inlet pipe 5b. The refractory 7 and the prefabricated refractory 6 can also be integrally formed. The refractory 7 is preferably arranged to cross the entire bottom 1a of the tundish in a direction orthogonal to the flow of molten steel, and the flow of molten steel is the flow of molten steel injection flow from the ladle toward the molten steel outlet 3 to the mold. It is possible to generate a flow toward the surface of the tundish in the same way as the lower weir to promote the floating separation of inclusions. In addition, as Figure 1 As shown, an upper weir 8 may be provided upstream of the refractory 7 having the second porous portion 7a, that is, on the steel receiving side receiving molten steel from the ladle. This can prevent the inclusions floating on the steel receiving side from flowing out to the injection side into the mold.
[0031] Figure 3 The graph in FIG. 2 shows the inert gas flow rate R2 [NL / (s·m 2 )] and the number density of inclusions in the billet. Figure 3 The test was conducted without blowing inert gas from the first porous portion 4d provided in the weir 4. The inclusions were evaluated in the same manner as described above. Figure 3 It is clear that when R2 is less than 0.1NL / (s·m 2 ) is not preferred because the floating effect of inclusions in the tundish is small. On the other hand, when R2 exceeds 10NL / (s·m 2 ) is too much gas injection amount, and the entrapment of tundish slag becomes large, which is not preferred. Therefore, the inert gas flow rate R2 per unit area of the second porous portion 7a is preferably adjusted to 0.1 to 10 NL / (s·m 2 ) range.
[0032] It is preferable to form the refractory material 7 including the second porous portion 7 a integrally with the prefabricated refractory material 6 attached to the wall of the tundish 1 because the maintenance time of the tundish can be shortened.
[0033] The first porous portion 4d and the second porous portion 7a can be made by firing spherical particles mainly composed of alumina at 1600°C or above. The average pore diameter of the first porous portion 4d and the second porous portion 7a is preferably 20 to 120 μm. The average pore diameter can be specified by mercury intrusion method, etc., according to JIS R 1655:2003. By setting the average pore diameter to this range, the diameter of the bubbles blown into the molten steel can be controlled within a specified range, which is effective in suppressing the entanglement of slag.
[0034] Example
[0035] 300 tons of molten steel was placed in a ladle after oxygen blowing in a converter and vacuum degassing in an RH type vacuum degassing device. Figure 1 The tundish 1 shown in the figure is poured into the casting mold and continuous casting is performed. In the tundish 1, the inert gas flow rate R1 [NL / (s·m 2 )] and the inert gas flow rate R2 per unit area of the second porous portion 7a of the refractory 7 provided between the weir 4 and the outlet 3 [NL / (s·m 2 )]. The number density of inclusions in the steel billets after each treatment was investigated in the same manner as above. The results are shown in a graph. Figure 4 .
[0036] [Table 1]
[0037] Processing number 1 is a conventional example in which R1 and R2 are set to 0. Processing numbers 2 to 4 are invention examples in which an appropriate amount of inert gas is blown only from the first porous portion 4d at the bottom of the weir 4. Processing numbers 5 to 8 are reference examples in which an appropriate amount of inert gas is blown only from the second porous portion 7a at the bottom of the tundish provided between the weir 4 and the outlet 3. Processing numbers 9 to 12 are invention examples in which an appropriate amount of inert gas is blown by combining the two. Processing numbers 13 to 16 are comparative examples in which the amount of inert gas blown deviates from the appropriate range. Figure 4 As a result, it can be seen that in the invention example in which the inert gas was blown in an appropriate range, the cleanliness of the steel billet was significantly improved compared with the conventional example and the comparative example.
[0038] In this specification, "L" as a unit of volume means 10 -3 m 3The symbol “N” recorded in the volume of a gas represents the volume at a temperature of 0°C and a pressure of 101325 Pa as a standard state.
[0039] Description of symbols 1 Tundish 1a Tundish bottom 2 Injection nozzle 2a Molten steel injection part 3 Molten steel outlet 4 dykes 4a Wall 4b Brim 4c Refractory bottom 4d (First) porous part 5a (First) Gas inlet pipe 5b (Second) Gas inlet pipe 5c (Third) Gas inlet pipe 6 Prefabricated refractory 7 Refractory (including porous parts) 7a (Second) porous portion 8 Go up the dike.
Claims
1. A tundish, comprising a weir between a molten steel injection portion and a molten steel outflow port, wherein the molten steel injection portion is a position where the molten steel injection flow from the ladle collides with the bottom of the tundish, and the molten steel outflow port is a position where the molten steel flows out of the tundish into a casting mold, wherein the weir comprises a wall portion and an eaves portion, wherein the wall portion surrounds the molten steel injection portion from all sides and extends upward from the bottom of the tundish, and the eaves portion protrudes horizontally toward the molten steel injection portion at an upper end portion of the wall portion, The dam has one or more continuous gaps from the wall to the eaves, a first porous portion is provided at the bottom of the refractory surrounded by the wall, a first gas introduction pipe is provided in the dam and in the refractory including the first porous portion, and the first gas introduction pipe is connected to the first porous portion. The tundish may further include a bottom refractory at a bottom of the tundish between the weir and the molten steel outlet, the bottom refractory having a second porous portion and a second gas introduction pipe connected to the second porous portion.
2. The tundish according to claim 1, wherein: The tundish further includes a prefabricated refractory having a third gas introduction pipe inside and mounted on a wall of the tundish, wherein the third gas introduction pipe is connected to the first gas introduction pipe or the second gas introduction pipe, or extends from the first gas introduction pipe or the second gas introduction pipe.
3. A continuous casting method, using the tundish according to claim 1 or 2, wherein the inert gas flow rate R1 per unit area at the bottom of the weir is adjusted to 0.02 to 1.0 NL / (s·m 2 ) in the range of , while blowing inert gas into molten steel from the first porous portion through the first gas inlet pipe, the steel slab is continuously cast by casting from the tundish to the mold.
4. The continuous casting method according to claim 3, wherein: The inert gas flow rate R2 per unit area is adjusted to 0.1 to 10 NL / (s•m 2 ) range, and blow inert gas into the molten steel from the second porous portion through the second gas introduction pipe.