Method for producing phosphoric acid

Through acid treatment and multiple purification steps on bone tissue, the problem of efficient recovery of phosphoric acid from bone tissue was successfully solved, providing a sustainable phosphoric acid supply source that replaces phosphate ores, and achieving efficient phosphoric acid recovery and purification.

CN118922379APending Publication Date: 2024-11-08KINKI UNIVERSITY
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202380024553.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-01
Filing Date
2023-02-28
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The prior art is difficult to effectively recover phosphoric acid and to recycle phosphoric acid from bone tissue to replace phosphoric ore, which solves the dependence of phosphoric acid supply and environmentally friendly needs.

Method used

By acid treatment on the bone tissue, an acid extract is obtained, and then alkali is added to form calcium phosphate. Then acid is added to remove calcium ions. Calcium precipitation is removed using a composition composed of sulfate, carbonate or bicarbonate. The purification process is repeated to Improve the purity of phosphoric acid.

Benefits of technology

The efficient recovery of phosphoric acid from bone tissue is achieved, providing a sustainable source of phosphoric acid supply to replace phosphoric ores, improving the purity and recovery of phosphoric acid, suitable for agricultural and industrial use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118922379A_ABST
    Figure CN118922379A_ABST
Patent Text Reader

Abstract

Provided is a novel method for producing phosphoric acid. A method for producing phosphoric acid according to one aspect of the present invention includes the following steps. (a) A step in which bone tissue is subjected to an acid treatment to obtain an acid extract. And (b) a step for adding an alkali to the obtained acid extract to obtain precipitated calcium phosphate. And (c) adding an acid to the obtained calcium phosphate precipitate to obtain a calcium phosphate solution. And (d) a step in which one or more salts selected from the group consisting of sulfates, carbonates, and bicarbonate are added to the obtained calcium phosphate solution, and precipitated calcium is removed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for producing phosphoric acid. Background Art

[0002] Phosphoric acid is a material widely used in agriculture and industry. Phosphoric acid is usually produced using phosphate rock as a raw material, but technologies for recovering phosphoric acid from waste have also been developed. For example, Patent Document 1 discloses a method for recovering phosphoric acid from feces and urine and sludge in a septic tank. Patent Document 2 discloses a method for recovering phosphoric acid from steelmaking slag.

[0003] Patent Document 1: Japanese Patent Application Publication No. 2017-196619 Patent Document 2: Japanese Patent Application Publication No. 2011-213558 Summary of the invention Technical problem to be solved by the invention

[0004] Bone tissue contains about 33% phosphoric acid based on the weight before drying. Therefore, if phosphoric acid can be recovered from bone tissue, waste bones generated in slaughterhouses and the like may become a huge source of phosphoric acid. This is very ideal for Japan, which relies on imports for all its phosphate rock needs. Therefore, it is required to develop a method for recovering phosphoric acid from bone tissue.

[0005] One object of the present invention is to provide a novel method for producing phosphoric acid. Solutions to technical problems

[0006] <1> A method for producing phosphoric acid comprises the following steps: (a) treating the bone tissue with acid to obtain an acid extract; (b) adding alkali to the obtained acid extract to obtain precipitated calcium phosphate; (c) adding acid to the obtained calcium phosphate precipitate to obtain a calcium phosphate solution; and (d) a step of adding one or more selected from the group consisting of sulfates, carbonates, and bicarbonates to the obtained calcium phosphate solution to remove precipitated calcium. <2> The production method according to <1>, further comprising a step of pre-treating the bone tissue before the step (a), The pretreatment is at least one selected from the group consisting of heating the bone tissue, heating the bone tissue under pressure, and irradiating the bone tissue with microwaves. <3> The manufacturing method according to <1> or <2>, After the step (d), the method further includes removing anions and cations other than phosphate ions and hydrogen ions. <4> The production method according to any one of <1> to <3>, The above steps (b) and (c) are repeated two or more times. <5> The production method according to any one of <1> to <4>, In the above step (a), the bone tissue is subjected to an acid treatment using at least one selected from the group consisting of nitric acid, hydrochloric acid, formic acid, and sulfuric acid. <6> The production method according to any one of <1> to <5>, In the above step (d), sulfuric acid is not added to the calcium phosphate solution. Effects of the Invention

[0007] According to one aspect of the present invention, a novel method for producing phosphoric acid is provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Figure 1 This is a flowchart showing an example of a method for producing a fertilizer according to one embodiment of the present invention. Figure 2 It is a flowchart showing another example of the method for producing a fertilizer according to one embodiment of the present invention. Figure 3 This is a flow chart showing an example of a method for producing phosphoric acid according to one embodiment of the present invention. Figure 4 This figure shows the results of treating bone tissue obtained by acid-treating pig bones with nitric acid with protease. Figure 5 This is a diagram showing the results of treating bone tissue obtained by acid-treating pig bones with nitric acid or hydrochloric acid with thaumarinase. Figure 6 This is a graph showing the results of preparing osteolytic solution A using various acids and proteases without solution exchange. Figure 7 This is a graph showing the results of an experiment to investigate the effect of acid extracts on plant growth. Figure 8 This is a diagram showing the results of an experiment to examine the effects of an acid extract, a protease treatment solution, or a bone dissolving solution A on plant growth. Fig. 9 This is a graph showing the results of an experiment comparing the effects of osteolytic solution A and a commercially available culture solution on plant growth. Fig.10This is a graph showing the results of an experiment comparing the effects of osteolytic solution A and a commercially available culture solution on plant growth. Fig.11 This is a graph showing the results of an experiment comparing changes in the expression levels of genes related to stress tolerance between bone dissolving solution A and commercially available liquid fertilizers. Fig.12 This is a graph showing the results of an experiment comparing changes in the expression levels of genes related to stress tolerance between bone dissolving solution A and commercially available liquid fertilizers. Fig.13 This is a graph showing the effect of pretreatment of bone tissue on the amount of phosphoric acid contained in the acid extract. Fig.14 This is a diagram showing the results of electrophoresis analysis of protein components contained in the acid extract. Fig.15 This is a graph showing the results of preparing protease treatment solutions using various proteases. Fig.16 This is a diagram showing the results of electrophoresis analysis of protein components contained in a protease-treated solution. Fig.17 This is a graph showing the results of preparing osteolytic solution A using various acids and proteases without solution exchange. Fig.18 The graph shows the analysis results of genes with expression changes in new shoots and leaves grown for 5 days after application of bone dissolving solution B or commercially available liquid fertilizer. Fig.19 The graph shows the analysis results of genes with expression changes in the roots of new shoots grown for 5 days after application of a mixed solution of bone dissolving solution B and commercial liquid fertilizer or commercial liquid fertilizer alone. Fig. 20 The graph shows the analysis results of genes with expression changes in new shoots and leaves grown for 5 days after application of a mixed solution of bone dissolving solution B and commercial liquid fertilizer or commercial liquid fertilizer alone. Fig.21 The figure shows the dissolution curve of the extraction of phosphoric acid using commercially available bone powder as a raw material. Fig. 22 This is a graph showing the results of producing liquid fertilizer using commercially available bone meal as a raw material. Neuroenzyme F3G was used as a protease. Fig.23 This is a graph showing the results of producing liquid fertilizer using commercially available bone meal as a raw material. Papain was used as a protease. DETAILED DESCRIPTION

[0009] [1. Method for producing fertilizer] A method for producing a fertilizer according to one aspect of the present invention includes one or more of the following steps 1 to 3. In one embodiment, the method for producing a fertilizer further includes the following step 4. Hereinafter, step 2, step 3, step 4, and step 1 will be described in detail in this order.

[0010] Step 1: A step of treating bone tissue with a solution containing both an acid and a protease to produce a fertilizer from the obtained bone-dissolving solution A. Step 2: A step of treating bone tissue with acid and producing a fertilizer from the obtained acid extract. Step 3: A step of treating the acid-treated bone tissue with protease to produce a fertilizer from the obtained protease-treated solution. Step 4: A step of mixing the acid extraction solution and the protease treatment solution to produce a fertilizer from the obtained bone dissolving solution B.

[0011] [1.1. Step 2] Step 2 is a step of treating the bone tissue with acid and producing a fertilizer from the obtained acid extract. In step 2, inorganic components are mainly separated from the bone tissue and eluted into the acid extract. Fertilizer is produced from the obtained acid extract. The acid extract itself can be used as fertilizer, or the bone dissolving solution B mixed with the protease treatment solution can be used as fertilizer.

[0012] The bone tissue for step 2 can be derived from any organism. Examples of organisms include mammals, birds, amphibians, and fish. In order to mass-produce fertilizers, it is preferred to obtain a large amount of bone tissue as a raw material for fertilizers, for example, preferably bone tissue of poultry (cows, pigs, sheep, chickens, etc.). Before the bone tissue is treated with acid, it can be chopped or crushed in advance. In this way, the decomposition of the bone tissue can be carried out more efficiently, so the manufacturing time can sometimes be shortened.

[0013] The acid for treating the bone tissue in step 2 is not particularly limited. Examples of acids include hydrochloric acid, nitric acid, formic acid, sulfuric acid, and trichloroacetic acid. Acidic decalcification solutions such as Plank-Rychlo solutions may also be used. From the viewpoint of easy availability, it is preferred to select one or more of the group consisting of nitric acid, hydrochloric acid, formic acid, and sulfuric acid. From the viewpoint of the recovery efficiency of phosphoric acid, it is preferred to select one or more of the group consisting of hydrochloric acid, sulfuric acid, and nitric acid, and more preferably to select one or more of the group consisting of hydrochloric acid and nitric acid. From the viewpoint of the recovery efficiency of calcium, it is preferred to select one or more of the group consisting of hydrochloric acid and formic acid. Two or more acids may also be mixed and used in an appropriate ratio.

[0014] In step 2, the bone tissue may be treated with an acid using a solution obtained by diluting an acid in a solvent. Examples of the solvent include water, lower alcohols, glycerol, propylene-1,2-diol, and 1,3-propylene glycol. Two or more solutions may be mixed at an appropriate ratio for use.

[0015] The concentration of the acid can be appropriately determined according to the volume of the bone tissue to be treated with the acid. When the volume of the bone tissue is small, it can be treated with a low concentration of acid. When the volume of the bone tissue is large, it is preferred to use a high concentration of acid. When the acid treatment is performed with a low concentration of acid, it is preferred to treat the micronized bone tissue. However, even when the volume of the bone tissue is large, if the acid concentration is increased and the immersion is prolonged, the inorganic components can be fully extracted. For example, when the volume of the bone tissue is several cm 3 When the crushed bone material is as the raw material, the lower limit of the concentration of the acid in step 2 may be 0.6 mol / L or more, 0.7 mol / L or more, 0.8 mol / L or more, or 0.9 mol / L or more. The upper limit of the concentration of the acid in step 2 may be 2.0 mol / L or less, 1.5 mol / L or less, 1.0 mol / L or less, or 0.9 mol / L or less. If the concentration of the acid is within the above range, the inorganic component can be efficiently extracted, and since the acid concentration is not too high, the cost of neutralizing the acid extract can be reduced.

[0016] Examples of preferred acid concentrations when the micronized bone tissue is subjected to acid treatment are as follows. When the acid is nitric acid, the lower limit of the concentration of nitric acid is preferably 0.6 mol / L or more, and more preferably 0.7 mol / L or more. The upper limit of the concentration of nitric acid is preferably 1.0 mol / L or less, and more preferably 0.9 mol / L or less. When the acid is hydrochloric acid, the lower limit of the concentration of hydrochloric acid is preferably 0.8 mol / L or more, and more preferably 0.9 mol / L or more. The upper limit of the concentration of hydrochloric acid is preferably 1.2 mol / L or less, and more preferably 1.1 mol / L or less. When the acid is formic acid, the lower limit of the concentration of formic acid is preferably 0.8 mol / L or more, and more preferably 0.9 mol / L or more. The upper limit of the concentration of formic acid is preferably 1.2 mol / L or less, and more preferably 1.1 mol / L or less. When the acid is sulfuric acid, the lower limit of the concentration of sulfuric acid is preferably 0.8 mol / L or more, and more preferably 0.9 mol / L or more. The upper limit of the concentration of sulfuric acid is preferably 1.2 mol / L or less, and more preferably 1.1 mol / L or less. However, the above concentration is an example of a preferred concentration when the bone tissue is micronized, and when a larger bone tissue is used as a raw material, the acid concentration can be further increased.

[0017] For example, when the volume is several cm 3When the following bone crushed material is used as the raw material, the lower limit of the extraction time in step 2 is preferably 6 hours or more, more preferably 8 hours or more, and further preferably 10 hours or more. The upper limit of the extraction time in step 2 is preferably 48 hours or less, more preferably 24 hours or less, and further preferably 14 hours or less. If the extraction time is within the above range, the inorganic components contained in the bone tissue can be fully extracted.

[0018] For example, when the volume is several cm 3 When the following bone crushing material is used as the raw material, the temperature of the acid treatment in step 2 is preferably 5 to 60°C. If the acid treatment is performed within the above temperature range, the generation of unpleasant odors accompanying the acid treatment can be reduced. Therefore, the site selection conditions for the fertilizer manufacturing plant become loose. In addition, in order to adjust the temperature condition to below 60°C, no expensive special equipment is required, and the temperature can be kept constant by using a water bath or an incubator.

[0019] In step 2, in addition to the acid, a chelating agent capable of capturing calcium ions may be added. Alternatively, in step 2, the bone tissue may be treated with a chelating agent before or after the acid treatment (the solutions may or may not be exchanged during the acid treatment and the chelating agent treatment). Examples of chelating agents include ethylenediaminetetraacetic acid (EDTA, CAS registration number: 60-00-4), ethylene glycol diaminetetraacetic acid (EGTA, CAS registration number: 67-42-5), and ethylenediamine-N, N'-disuccinic acid (EDDS, CAS registration number: 20846-91-7). In step 2, the pH of the solution containing the chelating agent is preferably 6.0 to 8.0. For example, when a volume of several cm 3 When the crushed bone material is as the raw material, the lower limit of the concentration of the chelating agent in step 2 may be 0.1 mol / L or more, 0.2 mol / L or more, 0.3 mol / L or more, or 0.4 mol / L or more. The upper limit of the concentration of the chelating agent in step 2 may be 0.9 mol / L or less, 0.8 mol / L or less, 0.7 mol / L or less, or 0.6 mol / L or less.

[0020] In step 2, at least a portion of the calcium may be removed after the acid treatment. Examples of methods for removing calcium include a method of neutralizing the acid extract (generating calcium phosphate precipitation), a method of adding sulfuric acid or a sulfate (precipitation of calcium sulfate), a method of adding carbonic acid or a carbonate (precipitation of calcium carbonate or calcium hydrogen carbonate), and a method of adding a hydrogen carbonate (precipitation of calcium carbonate or calcium hydrogen carbonate).

[0021] If the pretreatment step described later is performed, the phosphoric acid concentration of the acid extract obtained in step 2 tends to increase. The concentration of phosphoric acid contained in the acid extract may be, for example, 280 mM or more, 300 mM or more, or 320 mM or more.

[0022] [1.2. Step 3] Step 3 is a step of treating the acid-treated bone tissue with protease and producing a fertilizer from the obtained protease treatment solution. The obtained protease treatment solution is used to produce a fertilizer. The protease treatment solution itself can be used as a fertilizer, or the bone dissolving solution B mixed with the acid extract can be used as a fertilizer.

[0023] The protease used in step 3 is not particularly limited. Examples of the protease include serine protease, cysteine ​​protease, aspartic acid protease, glutamic acid protease, and metalloprotease.

[0024] Specific examples of proteases include trypsin [EC 3.4.21.4], chymotrypsin [EC 3.4.21.1], [EC 3.4.21.2], pepsin [EC 3.4.23.1], colicin [EC 3.4.23.19], papain [EC 3.4.22.2], ficin [EC 3.4.22.3], thaumatin [EC 3.4.22.14], bromelain [EC 3.4.22.32], cathepsin B [EC 3.4.22.1], cathepsin H [EC 3.4.22.16], cathepsin K [EC 3.4.22.38], cathepsin L [EC 3.4.22.15], cathepsin S [EC 3.4.22.27], thermolysin [EC 3.4.24.27].

[0025] As the protease, commercially available enzyme preparations can be used. Examples of such preparations include neuroenzyme F3G (derived from Rhizopus niveus), orientase AY (derived from Aspergillus niger), tetrazyme (derived from Aspergillus niger), Sumizyme AP (derived from Aspergillus niger), Denapsin 2P (derived from the genus Aspergillus), proline protease (derived from Aspergillus niger), Maxipro AFP (derived from Aspergillus niger), protease S "Amano" G (derived from Bacillus stearothermophilus), protease N "Amano" G (derived from Bacillus subtilis), protease NL "Amano" (derived from Bacillus subtilis), protease A "Amano" G (derived from Aspergillus oryzae), umami-enhancing enzyme (derived from Aspergillus oryzae), protease P "Amano" 3G (derived from Aspergillus melleus), Protease M "Amano" SD (derived from Aspergillus oryzae), Peptidase R (derived from Rhizopus oryzae). Alternatively, chemically synthesized enzymes, enzymes produced by genetic engineering methods, and enzymes extracted from organisms can be used.

[0026] The protease used in step 3 is preferably a protease having an optimum pH of 1.5 to 8.0. Examples of the protease having an optimum pH of 1.5 to 8.0 include protease S "Amano" G (optimum pH: 7.0 to 8.5), protease N "Amano" G (optimum pH: 6.0 to 7.5), protease NL "Amano" (optimum pH: 6.5 to 7.5), protease A "Amano" G (optimum pH: 6.0 to 7.5), umami-enhancing enzyme (optimum pH: 6.0 to 7.5), protease M "Amano" G (optimum pH: 3.0 to 6.5), Protease P "Amano" 3G (optimum pH: 7.0-8.0), peptidase R "Amano" (optimum pH: 6.0-8.0), kiwi proteinase (optimum pH: 2.5-7.5), papain (optimum pH: 4.0-9.0), pepsin (optimum pH: 1.5-3.0), neuroenzyme F3G (optimum pH: 3.0-5.0), trypsin (optimum pH: 7.0-9.0), chymotrypsin (optimum pH: 7.0-9.0). The protease used is more preferably a protease with an optimum pH of 1.5-5.0. Examples of proteases having an optimum pH of 1.5 to 5.0 include protease M "Amano" (optimum pH: 3.0 to 6.5), kiwi protease (optimum pH: 2.5 to 7.5), papain (optimum pH: 4.0 to 9.0), pepsin (optimum pH: 1.5 to 3.0), and neuroenzyme F3G (optimum pH: 3.0 to 5.0). The protease used is more preferably a protease having an optimum pH of 1.5 to 4.0. Examples of proteases having an optimum pH of 1.5 to 4.0 include kiwi protease (optimum pH: 2.5 to 7.5), pepsin (optimum pH: 1.5 to 3.0), and neuroenzyme F3G (optimum pH: 3.0 to 5.0).

[0027] The concentration of the protease in step 3 can be appropriately set. The lower limit of the protease concentration may be 2 mg / L or more or 10 mg / L or more. The upper limit of the protease concentration may be 100 mg / L or less or 50 mg / L or less.

[0028] The temperature and pH in step 3 can be set appropriately. From the perspective of improving treatment efficiency, it is preferably consistent with the optimum temperature and optimum pH of the protease used. As an example of the temperature of the reaction system in step 3, 20 to 60°C can be cited. The lower limit of the temperature of the reaction system in step 2 can be more than 10°C, more than 20°C, more than 25°C, more than 30°C, more than 35°C, more than 40°C, more than 45°C, more than 50°C or more than 55°C. The upper limit of the temperature of the reaction system in step 2 can be less than 60°C or less than 55°C.

[0029] In step 3, a salt may be added to the reaction system. The substrate specificity of the protease may sometimes change depending on the concentration of the salt added to the reaction system. Therefore, by adding a salt to the reaction system, the components contained in the obtained protease treatment solution can be changed.

[0030] As examples of salts added to the reaction system in step 3, chloride salts can be cited. As examples of chloride salts, NaCl, KCl, LiCl, and MgCl2 can be cited. The lower limit of the concentration of the salt added to the reaction system in step 3 can be more than 0 mmol / L, more than 20 mmol / L, more than 100 mmol / L, more than 150 mmol / L, more than 200 mmol / L, more than 500 mmol / L, more than 1000 mmol / L, more than 1500 mmol / L, and more than 2000 mmol / L. The upper limit of the concentration of the salt added to the reaction system in step 3 can be less than 4000 mmol / L or less than 2000 mmol / L.

[0031] In one embodiment, the size of the peptide fragment generated in step 3 is less than 10,000 Da, less than 8,000 Da, less than 6,000 Da or less than 4,000 Da. The peptide fragments cut to this size are likely to lose their physiological activity. In addition, the peptide fragments cut to this size are easily absorbed by plants as nutrients, and sometimes act as active ingredients of fertilizers. In one embodiment, the peptide fragment is derived from one or more peptide fragments selected from the group consisting of type I collagen, α-2-HS-glycoprotein, periostin, biglycan and SPARC.

[0032] [1.3. Step 4] Step 4 is a step of mixing the acid extract obtained in step 2 and the protease treatment solution obtained in step 3 to produce a fertilizer from the obtained bone dissolving solution B. Fertilizer is produced from the obtained bone dissolving solution B. In step 4, the mixing ratio of the acid extract and the protease treatment solution is not particularly limited. The mixing ratio can be appropriately selected so that the obtained bone dissolving solution B has a desired composition.

[0033] [1.4. Step 1] Step 1 is a step of treating bone tissue with a solution containing both an acid and a protease to produce a fertilizer from the obtained bone dissolving solution A. In step 1, the acid treatment in step 2 and the protease treatment in step 3 are performed simultaneously. In step 1, it is not necessary to exchange solutions during the acid treatment and the protease treatment.

[0034] In step 1, the order of contacting the bone tissue with the acid and the protease is not particularly limited. For example, the following order can be mentioned. Among these orders, order 1 is preferred. Procedure 1: Immerse bone tissue in a solution containing an acid, and after a predetermined time, add a protease to the solution. Before adding the protease, the pH of the solution may be adjusted to the optimal pH of the protease. Procedure 2: The bone tissue is immersed in a solution containing a protease, and after a predetermined period of time, an acid is added to the solution. Sequence 3: Prepare a solution containing both acid and protease, and immerse the bone tissue in the solution.

[0035] Regarding the preferred conditions for the acid treatment and protease treatment in step 1, the descriptions in Sections [1.1] and [1.2] are cited.

[0036] [1.5. Other processes] The method for producing fertilizer according to one embodiment of the present invention may include steps that are generally performed in the production of fertilizers in addition to steps 1 to 4. Examples of such steps include a pretreatment step, a component addition step, a drying step, a pulverization step, a coating granulation step, and a packaging step.

[0037] The pretreatment step is a step before step 1 or step 2. In the pretreatment step, the bone tissue as a raw material is pretreated. By performing the pretreatment step, the amount of phosphoric acid extracted from the bone tissue can be increased (see Example 4).

[0038] In one embodiment, the bone tissue is heated in the pretreatment step. The heating temperature may be 30° C. or 40° C. or 100° C. or 80° C. or less. The bone tissue may be heated while being immersed in an acid.

[0039] In one embodiment, in the pretreatment step, the bone tissue is heated under pressure. The pressure at this time may be 200 kPa or more or 1 MPa or more; 500 MPa or less or 800 MPa or less. The heating temperature at this time may be 10°C or more or 50°C or more; 120°C or less or 200°C or less.

[0040] In one embodiment, in the pretreatment process, the bone tissue is irradiated with microwaves. Heating, heating under pressure, and microwave irradiation may also be performed in any combination. Among them, microwave irradiation is more preferred as a pretreatment process because the effect can be obtained in a short time. The microwave irradiation time may be more than 5 seconds, more than 10 seconds, or more than 15 seconds; less than 10 minutes, less than 7 minutes, or less than 5 minutes.

[0041] If the pretreatment step is performed, the protein contained in the bone tissue is denatured. Therefore, the fertilizer obtained by the pretreatment step contains denatured protein (or its fragment). The denatured protein (or its fragment) loses the inherent physiological activity of the protein.

[0042] The component adding step is a step of adding additional fertilizer components. If the component adding step is provided, a fertilizer having a preferred composition corresponding to the plant to be cultivated can be manufactured. Examples of fertilizer components added in the component adding step include potassium components (potassium oxide, potassium hydroxide, potassium chloride, potassium sulfate, etc.), nitrogen components (urea, ammonium nitrate, etc.), magnesium components (magnesium phosphate, magnesium chloride, magnesium sulfate, etc.), vitamins, manganese, boron, iron, copper, zinc, and molybdenum. In addition, the acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B may be mixed with other fertilizers (inorganic fertilizers, organic fertilizers, etc.).

[0043] The drying step is a step of removing excess water from the acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B. Through the drying step, a solid or paste-like fertilizer is obtained. The solid fertilizer can also be cut and crushed into a size and shape that is easy to apply as needed.

[0044] The coating granulation process is a process of coating and granulating solid fertilizers. For example, if fertilizers are coated with silicate compounds, the fertilizer effect period can be adjusted, or phosphorus and calcium can be prevented from being fixed, or the loss of fertilizers can be prevented, or the damage of fertilizers caused by impact can be prevented.

[0045] The packaging process is a process of packaging the acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B in a container so that it can be circulated or sold as a fertilizer. In the packaging process, the acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B can also be combined with instructions for using them as fertilizers. The instructions can be printed on the container or prepared separately from the fertilizer packaged as a physical or electronic file. The instructions can record the prescription of the fertilizer, the method of fertilization, the period of fertilization, the target crop, etc.

[0046] [1.6. Exemplary method for producing fertilizer] An example of a method for producing a fertilizer according to an embodiment of the present invention will be described below based on an exemplary flowchart.

[0047] Figure 1 1 is an exemplary flow chart showing a manufacturing method including step 2, step 3 and / or step 4. In the flow chart, an acid extract is obtained by going through step S1, step S2, step S3 and step S4. In addition, a protease treatment solution is obtained by going through step S1, step S2 and step S5. Furthermore, the acid extract and the protease treatment solution are passed through step S6 to obtain a bone dissolving solution B. The acid extract, the protease treatment solution and the bone dissolving solution B can all be used as components of fertilizers or mixed fertilizers. Since the acid extract contains phosphoric acid, which is an essential nutrient for plants, it can also be used as a fertilizer itself.

[0048] In step S1, the bone tissue is pretreated. Step S1 is an optional step and may not be performed. By pretreating the bone tissue, the amount of phosphoric acid contained in the acid extract can be increased. This step is as described in Section [1.5].

[0049] In step S2, the bone tissue is treated with acid. The supernatant obtained in step S2 is an acid extract. If fertilizer is produced from the acid extract, it is the above-mentioned step 2. The acid treatment of bone tissue is as described in section [1.1].

[0050] In step S3, a sulfate, a carbonate or a bicarbonate is added. Step S3 is an optional step and may not be implemented. Through step S3, the calcium ions contained in the acid extract are precipitated as calcium sulfate, calcium carbonate or calcium bicarbonate. Examples of sulfates include sodium sulfate, potassium sulfate, ammonium sulfate and magnesium sulfate. Examples of carbonates include potassium carbonate and ammonium carbonate. Examples of bicarbonates include potassium bicarbonate. Preferably, the sulfate is selected from one or more of the group consisting of potassium sulfate, ammonium sulfate and magnesium sulfate. Preferably, the carbonate is potassium carbonate. Preferably, the bicarbonate is potassium bicarbonate. If these sulfates, carbonates or bicarbonates are used, potassium, magnesium and / or ammonium will be contained in the acid extract. These components are important nutrients for plants.

[0051] In step S4, the acid extract is neutralized with an alkali. Step S4 is an optional step and may not be implemented. Step S4 restores the acid extract from acidic to near neutral. Examples of alkalis that can be used include sodium hydroxide and potassium hydroxide. Among them, if potassium hydroxide is used, the acid extract contains potassium ions. Potassium ions are important nutrients for plants, so it is preferably neutralized with potassium hydroxide.

[0052] In step S5, the acid-treated bone tissue is treated with protease. The treatment solution obtained in step S5 is a protease-treated solution. If fertilizer is produced from the protease-treated solution, it is the above-mentioned step 3. Protease Treatment of Bone Tissue Acid Treatment is as described in Section [1.2].

[0053] In step S6, the acid extraction solution and the protease treatment solution are mixed. In this way, a bone dissolving solution B is obtained. If a fertilizer is produced from the bone dissolving solution B, it is the above-mentioned step 4. The preparation of the bone dissolving solution B is as described in section [1.3].

[0054] Figure 2 : is an exemplary flow chart showing a production method including step 1. In this flow chart, bone dissolving solution A is obtained through step S1, step S7, step S3, and step S4. Bone dissolving solution A can be used as a fertilizer or a component of a mixed fertilizer.

[0055] Since steps S1 , S3 , and S4 are as described above, their repeated description will be omitted.

[0056] In step S7, the bone tissue is treated with both acid and protease. In this way, a bone dissolving solution A is obtained. If a fertilizer is produced from the bone dissolving solution A, it is the above-mentioned step 1. The preparation of the bone dissolving solution A is as described in section [1.4].

[0057] 〔2. Fertilizer〕 [2.1. Fertilizers determined by manufacturing method] The fertilizer involved in one aspect of the present invention is a fertilizer obtained by the method for producing the fertilizer involved in one aspect of the present invention. Therefore, the fertilizer involved in one aspect of the present invention comprises an acid extract, a protease treatment solution, an osteolytic solution A or an osteolytic solution B. Among them, the fertilizer comprising the osteolytic solution A or the osteolytic solution B is preferred because it has a higher growth promoting effect on the plant body.

[0058] The lower limit of the proportion of the acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B in the total weight of the fertilizer can be 0.01 weight % or more, 0.05 weight % or more, 0.1 weight % or more, 0.5 weight % or more, 1 weight % or more, 5 weight % or more, 10 weight % or more, 20 weight % or more, 30 weight % or more, 40 weight % or more, 50 weight % or more, 60 weight % or more, 70 weight % or more, 80 weight % or more or 90 weight % or more. The upper limit of the proportion of the acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B in the total weight of the fertilizer is 100 weight %. In one embodiment, the fertilizer consists only of the acid extract, protease treatment solution, bone dissolving solution A, bone dissolving solution B, or any mixture thereof.

[0059] The composition of fertilizer can be changed suitably as required. For example, a part or all of phosphorus and calcium can be converted into monocalcium phosphate or calcium citrate. If set as such composition, then can regulate fertilizer effect period, to supply phosphorus and calcium with the growth stage of plant body.

[0060] Fertilizer can be solid fertilizer or liquid fertilizer. Since acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B are obtained in liquid form, they can be easily processed into liquid fertilizer. According to the method for manufacturing fertilizer involved in one embodiment of the present invention, since the components of bone tissue (for example, all the components of bone tissue) can be dissolved, it is expected to obtain a liquid fertilizer rich in components useful for plant growth. In addition, the existing bone-derived solid fertilizer (bone meal) is slow-acting and is mostly used for soil improvement after several years. On the contrary, if it is a liquid fertilizer, quick-acting properties can be expected. Furthermore, bone meal is not suitable for hydroponic cultivation. On the contrary, liquid fertilizer can be suitable for use in hydroponic cultivation. In addition, liquid fertilizer also has the advantage that it can also be easily applied to foliar spreading.

[0061] Fertilizers may also contain ingredients other than acid extract, protease treatment solution, bone dissolving solution A or bone dissolving solution B. Examples of such ingredients include acidic fertilizers, alkaline fertilizers, and other common fertilizers. Examples of acidic fertilizers include ammonium sulfate, superphosphate, potassium sulfate, aluminum sulfate, peat moss, black soil, ash, and alum. Examples of alkaline fertilizers include plant ash, lime nitrogen, Chilean saltpeter, fish fertilizer leaf mold, magnesia lime, organic lime, slaked lime, lime nitrogen, limestone, cement, baking soda, shells, rice husks, and smoked charcoal. Examples of other common fertilizers include rice straw, bark, and molasses. Free amino acids (gamma-aminobutyric acid, etc.), plant growth hormones (auxin, etc.), and trace elements (magnesium, sulfur, iron, manganese, zinc, copper, boron, molybdenum, etc.) may also be included.

[0062] [2.2. Fertilizers determined by composition] The fertilizer involved in one aspect of the present invention includes bone tissue degradation products. Therefore, most of them include type I collagen, osteocalcin, α-2-HS-glycoprotein, periostin, biglycan, SPARC or their degradation peptides as the main organic components of bone tissue. These components are difficult to be included in the fertilizer obtained by other manufacturing methods. Therefore, the possibility that the fertilizer containing type I collagen, osteocalcin, α-2-HS-glycoprotein, biglycan, SPARC, their degradation peptides, or their combination is a fertilizer manufactured by the manufacturing method involved in one embodiment of the present invention is high.

[0063] In one embodiment, the fertilizer comprises one or more peptide fragments derived from the group consisting of free type I collagen, α-2-HS-glycoprotein, periostin, biglycan and SPARC. In the method for manufacturing the fertilizer according to one embodiment of the present invention, the protease treatment of bone tissue is sometimes included (step S5 and step S7). The position of the peptide chain cut by the protease is inherently determined by the protease. Therefore, if a specific protein is treated with a specific protease, the peptide fragments produced by the treatment are uniquely determined. Since the molecular weight of each fragment is different, it is possible to determine the protein before the protease treatment from the peptide fragments contained in the fertilizer, for example, according to mass spectrometry. Therefore, those skilled in the art can judge whether the peptide fragments contained in the fertilizer are derived from one or more peptide fragments selected from the group consisting of free type I collagen, α-2-HS-glycoprotein, periostin, biglycan and SPARC.

[0064] Table 1 shows examples of peptide fragments that can be detected by LC-MS / MS. This peptide fragment is a peptide fragment that may appear when the fertilizer is analyzed without being treated with trypsin. Since it is not treated with trypsin, the C-terminus of the peptide fragment is an amino acid other than Lys or Arg.

[0065]

Table 1

[0066] In one embodiment, the peptide fragments derived from one or more peptides selected from the group consisting of type I collagen, α-2-HS-glycoprotein, periostin, biglycan and SPARC have no physiological activity. In the method for producing a fertilizer according to one embodiment of the present invention, multiple steps in which the protein may lose its physiological activity are included. One is a pretreatment step. In the pretreatment step, the bone tissue is heated, heated under pressure, or microwaves are irradiated to the bone tissue, so that the protein is denatured and loses its physiological activity. Another is the protease treatment in step 1 and step 3. The protein treated with the protease becomes fragments and loses its original physiological activity.

[0067] In one embodiment, the size of the peptide fragment derived from one or more of the group consisting of free type I collagen, α-2-HS-glycoprotein, periostin, biglycan and SPARC is less than 10,000 Da, less than 8,000 Da, less than 6,000 Da or less than 4,000 Da. The peptide fragment cut to this size has a high probability of losing physiological activity. In addition, the peptide fragment cut to this size is easily absorbed by plants as nutrition, and sometimes acts as an active ingredient of fertilizer.

[0068] In the present specification, "physiological activities of type I collagen, α-2-HS-glycoprotein, periostin, biglycan and SPARC" are as follows. The fragments derived from them lose their physiological activities means that they do not have the following activities. Physiological activity of type I collagen: self-association to form fibers under physiological conditions. Physiological activity of α-2-HS-glycoprotein: Binding to calcium ions. · Physiological activity of periostin: It functions as a cell adhesion molecule of osteoblast precursor cells. ·Physiological activity of biglycan: Binds to type I collagen. Physiological activity of SPARC: Promotes the synthesis of type I collagen in cultured dermal fibroblasts.

[0069] In one embodiment, the fertilizer contains phosphoric acid. In the method for producing the fertilizer according to one embodiment of the present invention, if the pretreatment step is performed, the concentration of phosphoric acid contained in the fertilizer tends to be higher. The concentration of phosphoric acid contained in the fertilizer may be, for example, 280 mM or more, 300 mM or more, or 320 mM or more.

[0070] In one embodiment, the fertilizer comprises both peptide fragments derived from one or more selected from the group consisting of type I collagen, α-2-HS-glycoprotein, periostin, biglycan, and SPARC, and phosphoric acid.

[0071] [3. Method for producing phosphoric acid] Another aspect of the present invention relates to a method for producing phosphoric acid using bone tissue as a raw material. The method for producing phosphoric acid includes, for example, a calcium phosphate purification step and a calcium removal step.

[0072] As an example of the step of producing calcium phosphate, the following procedure can be mentioned. 1. An alkaline solution is added to the acid extract obtained in step 2 for neutralization. Thus, a precipitate is obtained. 2. Add an acid solution (such as hydrochloric acid aqueous solution) to the precipitate to make the precipitate soluble again. 3. Repeat 1 and 2 to purify calcium phosphate.

[0073] In the removal process of calcium, calcium is removed by adding a chelating agent in the calcium phosphate solution of purification. As other examples, calcium can be precipitated as calcium sulfate or calcium carbonate by adding more than one selected from the group consisting of sulfate, carbonate and bicarbonate in the solution of calcium phosphate of purification. As the example of sulfate, carbonate and bicarbonate, sodium sulfate, potassium sulfate, ammonium sulfate, magnesium sulfate, sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, ammonium carbonate or a mixture of any multiple components thereof can be enumerated. The reagent added to the calcium phosphate solution can be directly added in the form of powder, or can be added in the form of solution (aqueous solution etc.). The above method can also be applied to acidic solution and room temperature, so calcium can be easily removed.

[0074] [3.1. Exemplary method for producing phosphoric acid] As a method for producing phosphoric acid from bone tissue, two production methods can be considered. One is a production method of burning bones into ashes and purifying phosphoric acid from the ashes. In the process of purifying phosphoric acid from ashes, the existing method of purifying phosphoric acid from phosphate ore is adopted. However, this production method consumes a lot of energy and the output of CO2 also increases, so it is not suitable for the realization of SDGs.

[0075] Another manufacturing method is Figure 3 The method is illustrated in the flowchart of FIG. In addition to phosphate, bone tissue also contains inorganic components such as calcium and organic components such as collagen. Figure 3 In the illustrated method, phosphoric acid is dissolved in steps S11 and S12, and components other than phosphoric acid and calcium are removed in steps S13 and S14. Steps S13 and S14 can be repeated, and the number of repetitions can be appropriately set. In step S15, sulfate, carbonate or bicarbonate is added to remove calcium. Calcium sulfate, calcium carbonate or calcium bicarbonate produced in step S15 can be used as agricultural fertilizer or industrial raw material. Below, each step is described in detail.

[0076] In step S11, the bone tissue is pretreated. Step S11 is an optional step and may not be performed. By pretreating the bone tissue, the amount of phosphoric acid contained in the acid extract can be increased. This step is the same as step S1 above, and the details are as described in section [1.5].

[0077] In step S12, the bone tissue is treated with acid. This step obtains an acid extract. This step is the same as step S2 above, and the conditions for the acid treatment are described in section [1.1].

[0078] In step S13, the acid extract is neutralized with an alkali. In step S13, the phosphate ions contained in the acid extract are precipitated as calcium phosphate, so that the components derived from the bone inclusions are contained in the supernatant. Therefore, phosphoric acid can be purified by recovering the precipitate. Examples of the alkali that can be used include sodium hydroxide and potassium hydroxide.

[0079] In step S14, an acid is added to the precipitated calcium phosphate. Thus, the precipitated calcium phosphate is dissolved again. Examples of the acid that can be used include hydrochloric acid, nitric acid, and formic acid.

[0080] Steps S13 and S14 may be repeated. By repeating these steps, the purity of phosphoric acid increases. The number of times steps S13 and S14 may be repeated may be, for example, two or more times, three or more times, four or more times, or five or more times. From the viewpoint of economic efficiency, the number of times steps S13 and S14 may be repeated may be, for example, 10 or less times. After repeating steps S13 and S14, before entering step S15, a necessary number of cleaning treatments may be performed to wash away unnecessary components contained in the calcium phosphate precipitate with pure water.

[0081] In step S15, sulfate, carbonate or bicarbonate is added to the calcium phosphate solution. The calcium ions in the solution are thus precipitated as calcium sulfate, calcium carbonate or calcium bicarbonate. The precipitated calcium sulfate, calcium carbonate or calcium bicarbonate is removed by centrifugation or the like. As examples of sulfates, one or more selected from sodium sulfate, potassium sulfate, ammonium sulfate and magnesium sulfate can be cited. As examples of carbonates, one or more selected from sodium carbonate, potassium carbonate and ammonium carbonate can be cited. As examples of bicarbonates, one or more selected from sodium bicarbonate and potassium bicarbonate can be cited. In addition, any combination of two or more of sulfates, carbonates and bicarbonates is also possible. In step S15, adding sulfate instead of sulfuric acid has the following advantages. Since no liquid is added, the volume increase of the reaction system can be reduced. Since the reaction system does not become strongly acidic, the amount of base required for neutralization is small. High security. ·High calcium removal rate.

[0082] The amount of sulfate, carbonate or bicarbonate added in step S15 can be appropriately set by those skilled in the art. The input amount of sulfate, carbonate or bicarbonate can be, for example, the concentration of sulfate, carbonate or bicarbonate in the reaction system is more than 0.2M, more than 0.4M, more than 0.6M, more than 0.8M or more than 1.0M. The more input amount of sulfate, carbonate or bicarbonate, the more residual calcium can be reduced. The upper limit of the input amount of sulfate, carbonate or bicarbonate can be, for example, the concentration of sulfate in the reaction system is less than 3.0M, less than 2.0M or 1.0M.

[0083] In operation S15, due to the solubility product, a small amount of sulfate ion, carbonate ion or bicarbonate ion remains in the supernatant. When removing these ions, carbonate ion or bicarbonate ion is converted into carbon dioxide by heating, so it can be easily removed. Therefore, the salt added in operation S15 is preferably selected from one or more of the group consisting of carbonate and bicarbonate.

[0084] In step S16, the supernatant after calcium removal is purified. The supernatant sometimes contains cations such as sodium ions contained in sulfate, anions such as chloride ions. By adsorbing these ions on, for example, ion exchange resins, high-purity phosphoric acid can be obtained. If carbonate ions or bicarbonate ions are contained, they can be converted into carbon dioxide by heating, so that the ions can be removed outside the system.

[0085] The present invention is not limited to the above-mentioned embodiments, and various modifications can be made within the scope of the claims. Embodiments obtained by appropriately combining technical means disclosed in different embodiments are also included in the technical scope of the present invention. [Example]

[0086] [Example 1: Preparation of fertilizer containing bone tissue degradation products] [Example 1-1: Preparation of acid extract using nitric acid and component analysis] The bone tissue was treated with nitric acid in the following procedure to obtain an acid extract. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKA TUBE MILL 100, IKA JAPAN Co., Ltd.). 2. Add 40 mL of nitric acid aqueous solution to 3 g of wet weight of pig bones and immerse at 20°C. The concentration of the nitric acid aqueous solution is 0.3 mol / L, 0.5 mol / L, 0.75 mol / L or 1.0 mol / L. The immersion time is 12 hours, 24 hours or 48 hours. 3. Recover the supernatant as the acid extract.

[0087] [Example 1-2: Preparation of acid extract using hydrochloric acid and component analysis] The bone tissue was treated with hydrochloric acid in the following procedure to obtain an acid extract. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKA TUBE MILL 100, IKA JAPAN Co., Ltd.). 2. Add 35 mL of hydrochloric acid aqueous solution to 2 g of wet weight of pig bones and immerse at 20°C. The concentration of the hydrochloric acid aqueous solution is 0.3 mol / L, 0.5 mol / L or 1.0 mol / L. The immersion time is 6 hours, 12 hours or 24 hours. 3. Recover the supernatant as the acid extract.

[0088] [Example 1-3: Preparation of acid extract using formic acid and component analysis] The bone tissue was treated with formic acid in the following procedure to obtain an acid extract. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKA TUBE MILL 100, IKA JAPAN Co., Ltd.). 2. Add 35 mL of formic acid aqueous solution to 2 g of wet weight of pig bones and immerse at 20°C. The concentration of formic acid aqueous solution is 0.3 mol / L, 0.5 mol / L or 1.0 mol / L. The immersion time is 6 hours, 12 hours or 24 hours. 3. Recover the supernatant as the acid extract.

[0089] [Example 1-4: Preparation of acid extract using sulfuric acid and component analysis] The bone tissue was treated with sulfuric acid in the following procedure to obtain an acid extract. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKA TUBE MILL 100, IKA JAPAN Co., Ltd.). 2. Add 35 mL of sulfuric acid aqueous solution to 2 g of wet weight of pig bones and immerse at 20°C. The concentration of sulfuric acid aqueous solution is 0.3 mol / L, 0.5 mol / L or 1.0 mol / L. The immersion time is 6 hours, 12 hours or 24 hours. 3. Recover the supernatant as the acid extract.

[0090] Table 2 shows the results of total phosphorus analysis of the obtained acid extract. The component analysis was entrusted to Kurita Analysis Center Co., Ltd. Table 2 shows the results of total phosphorus (mg) per 1g of bone wet weight. The analysis results were summarized using each acid according to the concentration of nitric acid, hydrochloric acid, formic acid or sulfuric acid and the immersion time. It shows that most of the phosphorus can be recovered in about 24 hours regardless of the acid aqueous solution. In addition, it is shown that phosphorus can be fully recovered when the acid concentration is about 1 mol / L. Among the four acids studied, hydrochloric acid and sulfuric acid have high phosphorus recovery efficiency. As can be seen from Table 2, about 100 mg of phosphorus can be recovered from 1g of bone tissue.

[0091]

Table 2

[0092] Table 3 shows the results of total calcium analysis of the obtained acid extract. The component analysis was entrusted to Kurita Analysis Center Co., Ltd. Table 3 shows the results of total calcium (mg) per 1g of bone wet weight. The analysis results were summarized using each acid according to the concentration of nitric acid, hydrochloric acid, formic acid, and sulfuric acid and the immersion time. It shows that in aqueous solutions of nitric acid, hydrochloric acid, and formic acid, most of the calcium can be recovered in about 24 hours. In addition, in aqueous sulfuric acid, free calcium forms insoluble calcium sulfate. Therefore, as a result of the analysis, the calcium concentration is low, but in fact, calcium is dissolved from the bone tissue. It shows that calcium can be fully recovered when the acid concentration is about 1 mol / L. Among the four acids studied, hydrochloric acid and formic acid have high calcium recovery efficiency. As can be seen from Table 3, about 200 mg of calcium can be recovered from 1g of bone tissue.

[0093]

Table 3

[0094] [Example 1-5: Preparation of protease treatment solution] The acid-treated bone tissue obtained in Example 1-2 was immersed in a treatment solution containing the following two proteases. The conditions for the protease treatment were protease concentration: 2% (w / w), temperature: 50°C, and pH: optimal pH. Protease 1: Neuroenzyme F3G (Amano Enzyme Co., Ltd., protease derived from Rhizopus niveus filamentous fungi) Protease 2: Pepsin (Sigma Aldrich, aspartic protease)

[0095] The results are shown in Figure 4 .exist Figure 4 In the figure, A represents the result of treatment with protease 1, and B represents the result of treatment with protease 2. The treatment time was 3.5 hours, 19 hours, or 24 hours. The results of visually confirming the transparency of the treatment solution and the residual bone tissue are as follows. After 3.5 hours: In the system treated with either protease, bone tissue almost disappeared. · After 24 hours: In the system treated with any protease, the bone tissue completely disappeared and the transparency of the protease treatment solution also increased.

[0096] Thus, it was found that a protease-treated solution can be obtained by treating the acid-treated bone tissue with a commercially available protease.

[0097] [Example 1-6: Preparation and component analysis of protease treatment solution] A protease-treated solution was obtained according to the following procedure. 1. The bone tissue was immersed in a 1 mol / L nitric acid aqueous solution or a hydrochloric acid aqueous solution for 48 hours for acid treatment. 2. The obtained treated solution is separated into an acid extract and bone tissue residue, and the acid extract is transferred to another container. 3. Add 0.1 mol / L citric acid buffer (pH 3.5) to the bone tissue residue. The amount added is 10 mL per 1 g of initial bone weight. 4. Pre-treat kiwifruit protease (cysteine ​​protease derived from kiwifruit) by contacting it with 20 mmol / L phosphate buffer (pH 6.5) containing 10 mmol / L dithiothreitol and 5 mmol / L ethylenediaminetetraacetic acid at 25°C for 90 minutes. 5. Add activated kiwifruit protease to the reaction system obtained in 3 to perform protease treatment. The treatment conditions are temperature: 20°C or 50°C, pH: 3.5 (adjusted with 100 mmol / L phosphate buffer), and time: 3 days.

[0098] The results are shown in Figure 5 In the system treated with either nitric acid or hydrochloric acid, bone tissue almost disappeared when the reaction temperature was 50°C.

[0099] The obtained protease-treated solution was passed through a 100 μm filter to obtain a filtrate from which fine insoluble matter had been removed. The results of component analysis of the filtrate are shown in Table 4 (values ​​converted per 1 g of bone wet weight are shown). The component analysis was commissioned to Kurita Analysis Center Co., Ltd.

[0100]

Table 4

[0101] [Example 1-7: Preparation and component analysis of bone dissolving solution A] The osteolytic solution A was prepared in one step without solution exchange between the acid treatment and the protease treatment. The specific procedure is as follows. 1. The bone tissue was acid-treated by immersing it in a 1 mol / L nitric acid aqueous solution, a hydrochloric acid aqueous solution, a formic acid aqueous solution or a sulfuric acid aqueous solution for 48 hours. 2. Add citric acid buffer (pH 3.5) to the reaction system to make the final concentration 0.1 mol / L. 3. Adjust to the optimum pH of the protease with 5N NaOH and 5N HCl. Specifically, adjust the pH of kiwifruit protease to 3.5, pepsin to 3.0, and neuroenzyme F3G to 3.0. 4. Each protease was added to 1% (w / w). The reaction conditions of the protease were 4 days at 50°C. It should be noted that kiwifruit protease (cysteine ​​protease derived from kiwifruit) was pretreated with 20 mmol / L phosphate buffer (pH 6.5) containing 10 mmol / L dithiothreitol and 5 mmol / L ethylenediaminetetraacetic acid at 25°C for 90 minutes.

[0102] The results are shown in Figure 6 In any system, if the reaction temperature is 50°C, the bone tissue becomes smaller. In this way, the bone dissolving solution A is obtained from the bone tissue in one step without intervening solution exchange between the acid treatment and the protease treatment. In particular, the combination of pepsin and hydrochloric acid or nitric acid dissolves the bone tissue well, and the remaining bone tissue is extremely small.

[0103] The obtained bone dissolving solution A was passed through a 100 μm filter to obtain a filtrate from which fine insoluble matter was removed. The results of measuring the calcium concentration of the filtrate are shown in Table 5 (showing the value converted per 1 g of bone wet weight). The calcium was measured using a compact calcium ion meter LAQUAtwin-Ca-11 (Horiba Advanced Technology Co., Ltd.).

[0104]

Table 5

[0105] [Example 1-8: Extraction of phosphoric acid] Crudely purified phosphoric acid was obtained from bone tissue according to the following procedure. 1. The bone tissue was acid-treated by immersing it in a 1 mol / L nitric acid aqueous solution, a hydrochloric acid aqueous solution, a formic acid aqueous solution or a sulfuric acid aqueous solution for 48 hours. 2. Add 0.15 volume of 5N NaOH to the reaction system, mix thoroughly, and let stand at room temperature for 1 hour. Thus, a white solution is obtained. 3. The obtained solution was centrifuged at 10,000 g for 10 minutes at room temperature, and the supernatant was removed. The same amount of 1N HCl as that added in step 1 was added to the white precipitate and mixed thoroughly. Thus, a transparent solution was obtained. 4. Add Na2SO4, K2SO4, MgSO4, (NH4)2SO4, Na2CO3 or NaHCO3 in an amount equal to the calcium concentration in the reaction system, mix thoroughly, and let stand at room temperature for 1 hour. Thus, a white solution is obtained. 5. The obtained solution was centrifuged at 10,000 g for 10 minutes at room temperature to remove the supernatant. The obtained transparent solution contained phosphoric acid.

[0106] By immersing bone tissue in sulfuric acid, a phosphoric acid solution in which calcium is removed to some extent can be obtained. However, the processing volume of sulfuric acid increases, and the solution becomes strongly acidic, and then there are many impurities, making it difficult to purify. On the other hand, according to the above-mentioned process, a solution containing phosphoric acid with high purity can be easily obtained.

[0107] [Example 2: Growth evaluation and component analysis of plants grown with fertilizer containing bone tissue degradation products] [Materials and Methods] 1. Radish (Raphanus sativus L) seeds (Takii Seedlings Co., Ltd.) were sown on wet paper towels and left to stand at 22°C in the dark for 2 days to allow the seeds to germinate. 2. The obtained plant body was transplanted into a polyurethane cube (2 cm×2 cm×2 cm) for hydroponic cultivation. 3. Immerse the acid extract, protease treatment solution or bone dissolving solution A in the polyurethane cube and let it grow for 5 days. The light conditions during this period are photosynthetically active photon flux density: about 150 μmol / m 2 s, light period: 16 hours, dark period: 8 hours. A fluorescent lamp for cultivation of cultivated plants (BR-A, NEC Lighting Co., Ltd.) was used as the light source. 4. Perform growth evaluation and component analysis on the grown plants. Specifically, the analysis is as follows. Fresh weight of aboveground part: The plant body was cut at the boundary between the hypocotyl and the root, and the weight of the hypocotyl side was measured. · Dry weight of aboveground part: The plant part for which the fresh weight was measured was dried in an oven at 80° C. for 2 days, and then the weight was measured. Above-ground moisture content: calculated based on the difference between the above-ground fresh weight and the above-ground dry weight. Leaf area: The cotyledons of the plants were captured using a scanner and the leaf area was measured using ImageJ. Total polyphenol content: 50 mg of cotyledons were crushed in a 90% methanol solution, and the total polyphenol content was measured by the Folin phenol method using the supernatant obtained by centrifugation.

[0108] [Results and Investigation] (1) Effect of acid extract concentration on growth Plants were grown under the condition of applying the acid extract diluted 500 times or 2000 times. The results are shown in Figure 7 The fresh weight of the aboveground part of the plant grown by using the acid extract diluted 500 times increased compared with the control plant. From this result, it can be seen that the acid extract diluted about 500 times has a growth-promoting effect on the plant. In subsequent experiments, the acid extract diluted 500 times and the protease treatment solution were used.

[0109] (2) Effects of acid extract, protease treatment solution, or osteolytic solution A on growth Plants were grown under the following six conditions, and the fresh weights of the aboveground parts were compared. · Water only (control) · Application of unheated protease treatment solution (protease treatment solution 1) ·Protease treatment solution heated at 50°C (Protease treatment solution 2) · Apply acid extract ·Administering a bone dissolving solution A mixed with a protease treatment solution 1 and an acid extract ·Administering a bone dissolving solution A mixed with protease treatment solution 2 and acid extraction solution The results are shown in Figure 8 . The plants treated with protease treatment solution 1 and protease treatment solution 2 showed promoted growth compared with the control. Similarly, the plants treated with acid extract also showed promoted growth compared with the control (this is shown in (1)). Furthermore, the plants treated with bone dissolving solution A, which is a mixture of protease treatment solution and acid extract, showed a higher growth promoting effect compared with the control. From the results, it can be seen that both acid extract and protease treatment solution have a growth promoting effect on plants. Furthermore, it can be seen that the growth promoting effect of bone dissolving solution A on plants is higher than the growth promoting effect produced by acid extract or protease treatment solution alone.

[0110] (3) Comparison of effects with commercially available culture media The growth promoting effect of the bone dissolving solution A and the commercially available culture solution was compared. As the commercially available culture solution, a culture solution prepared by diluting the A prescription of OAT Greenhouse (OAT Agrio Co., Ltd.) to 1 / 6 was used. By this dilution, the nitrate ion concentration was adjusted to the same as that of the bone dissolving solution A (about 600 ppm).

[0111] The results are shown in Figure 8 , 9 The growth of plants treated with commercially available culture solution was promoted to the same extent as that of plants treated with bone dissolving solution A. The growth promoting effect of plants treated with both bone dissolving solution A and culture solution was further improved compared with plants treated with either of them alone. This suggests that the growth promoting effect of commercially available culture solution can be further improved by using bone dissolving solution A.

[0112] The water content of the aboveground part of the plant body increased by applying the bone dissolving solution A, and further increased by adding both the bone dissolving solution A and the culture solution. The total polyphenol content per cotyledon increased by applying the bone dissolving solution A, and further increased by applying both the bone dissolving solution A and the culture solution. This may be due to the promotion of plant growth, resulting in an increase in cotyledon weight.

[0113] [Example 3: Analysis of RNA expression in plants 1] [Total RNA extraction from plants] 1. Radish (Raphanus sativus L) seeds (Takii Seedlings Co., Ltd.) were sown on wet paper towels and left to stand in the dark at 100% humidity and 22°C for 2 days to allow the seeds to germinate. 2. Transplant the obtained plant body into a polyurethane sponge. The polyurethane sponge is impregnated with any one of (1) water, (2) bone dissolving solution A, (3) commercially available liquid fertilizer, or (4) a mixture of bone dissolving solution A and commercially available liquid fertilizer. 3. The plants were grown at 22°C for 1 day, 3 days or 5 days. The light conditions during this period were: light intensity: about 100 μmol / m 2 s, light period: 16 hours, dark period: 8 hours. A fluorescent lamp for cultivation of cultivated plants (BR-A, NEC Lighting Co., Ltd.) was used as the light source. 4. Collect about 0.1 g of leaf and root tissue from the growing plant, put them in a mortar and add liquid nitrogen immediately after collection, and grind them while the tissues are frozen. 5. Total RNA was extracted from the ground tissue using RNeasy Plant Mini Kit (Qiagen). 6. The concentration of total RNA in the aqueous solution was determined using the Qubit RNA HS Assay Kit (Thermo Fisher Scientific) and a fluorophotometer (Qubit-4). In addition, the absorbance (A) at 230 nm, 260 nm, and 280 nm was measured by a spectrophotometer. 230 , A 260 and A 280 ) to investigate the purity of the extracted RNA.

[0114] The results are shown in Table 6. From the start of culture to the fifth day, 13.2 to 88.2 μg of total RNA was extracted from about 0.1 g of leaves of the plant. 8.4 to 43.8 μg of total RNA was extracted from about 0.1 g of roots of the plant. 260 / A 280 The value was about 2.0, confirming that there was no problem with the purity of the RNA.

[0115]

Table 6

[0116] [Preparation of RNA sequencing library and RNA sequence analysis using next generation sequencer] The preparation of cDNA library from total RNA extracted from the sprouts and the analysis of gene expression using a next-generation sequencer were commissioned to Ascent Corporation. The analysis procedure was as follows. 1. The quality of the extracted total RNA (RNA degradation degree) was evaluated using BioAnalyzer (Agilent Technologies). 2. From the extracted total RNA, polyA-mRNA was concentrated using beads bound to polyT oligo DNA. 3. Use reverse transcriptase to make a cDNA library. 4. The base sequence of cDNA was determined using a next-generation sequencer (DNBSEQ-G400, MGI tech). Thus, the base sequence of the expressed mRNA was comprehensively determined (RNAseq analysis). The assembly of the sprout gene was performed using Stringtie software. At this time, the entire genomic base sequence of the sprout published in the database of the Kazusa DNA Research Institute (http: / / radish.kazusa.or.jp) was referenced.

[0117] [Analysis of genes with changing expression levels] 1. Based on the FPKM value (fragments per kilobase of exon per million reads mapped), genes whose expression levels significantly changed due to different cultivation conditions were identified. The FPKM value was obtained by correcting the reads of each gene with the length of the transcript. The identification was performed using DESeq2 software. 2. Comprehensively determine the genes (DEGs) whose expression levels are significantly increased or decreased. The analysis results are presented by volcano plots. The expression levels were compared in four groups: (1) water only, (2) bone dissolving solution A, (3) commercial liquid fertilizer, and (4) a mixture of bone dissolving solution A and commercial liquid fertilizer. Identify genes whose expression levels are significantly increased or decreased in group (2) or (4). 3. GOseq software was used to perform GO enrichment analysis on the identified expression change genes, thereby analyzing the biological functions of the expression change genes.

[0118] [Quantitative RT-PCR] Five genes closely related to stress tolerance were used as target genes, and the expression of the genes was investigated by quantitative RT-PCR. As target genes, glutathione S-transferase τ19 (GSTU19), catalase 2 (CAT2), auxin transporter-like protein 2-1 (LAX2-1), glutathione S-transferase 12 (GST12) and calmodulin 5 (CaM5) were used. The specific order is as follows. 1. Total RNA was extracted from leaves and roots of plants grown by applying (1) water, (2) bone dissolving solution A, (3) commercially available liquid fertilizer, or (4) a mixture of bone dissolving solution A and commercially available liquid fertilizer. 2. Reverse transcriptase reaction (RT reaction) was performed using random primers. PrimeScript RT Master Mix (Takara Bio Co., Ltd.) was used as the reverse transcriptase. 3. Quantitative PCR was performed on the target gene. In the quantitative PCR, a specific primer pair and TB Green Premix Ex Taq II (Takara Bio Co., Ltd.) were used with 2.0 ng of cDNA as a template. As an instrument for performing quantitative PCR, Thermal Cycler Dice Real Time System TP850 (Takara Bio Co., Ltd.) was used.

[0119] In quantitative RT-PCR, the expression level of each target gene was normalized to the expression level of the actin gene. The base sequences of the primer pairs used for amplification of the target gene and the actin gene are shown in Table 7 (SEQ ID NOs. 1 to 12 from the top).

[0120]

Table 7

[0121] [result] The expression level of the gene encoding glutathione S-transferase τ19 (GSTU-19) was not detected before transplantation into the polyurethane sponge. Similarly, at the 1st day after transplantation, it was not detected in the leaves and roots of the plants grown in the system containing (1) water, (2) bone dissolving solution A, and (3) commercially available liquid fertilizer. However, at the 1st day after transplantation, the expression level of GSTU-19 increased significantly in the leaves and roots of the plants grown in the system containing a mixture of (4) bone dissolving solution A and commercially available liquid fertilizer ( Fig.11 Similarly, at the 1st day after transplantation, the expression levels of genes encoding catalase 2 (CAT2), auxin transporter-like protein 2-1 (LAX2-1), glutathione S-transferase 12 (GST12), and calmodulin 5 (CaM5) in the leaves of plants grown in a system containing a mixture of (4) bone dissolving solution A and commercially available liquid fertilizer increased significantly ( Fig.12 ).

[0122] Thus, it is shown that if the fertilizer involved in one embodiment of the present invention is used in combination with an existing liquid fertilizer, the expression of genes related to stress tolerance of plants is promoted. This result suggests that the stress tolerance of plants can be improved by using the fertilizer involved in one embodiment of the present invention in combination with an existing liquid fertilizer.

[0123] [Example 4: Improving the extraction rate of phosphoric acid by pretreatment] It was confirmed that the amount of phosphoric acid contained in the acid extract increased by pre-treating the bone tissue. Specifically, the acid extract was prepared according to the following procedure, and the amount of phosphoric acid contained was quantified. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKATUBE MILL 100, IKA JAPAN Co., Ltd.). 2. 5 g of ground pig bones were subjected to any of the following pretreatments (1) to (5). (1) No treatment (2) Immerse in 30 mL of nitric acid (1 mol / L) at 50°C for 1 day (3) Expose to 500W microwave for 30 seconds (4) Irradiate with 500W microwave for 60 seconds (5) Irradiate with 500W microwave for 120 seconds 3. Add 30 mL of nitric acid (1 mol / L) to the pig bones of (1) and (3) to (5). Immerse the pig bones of (1) to (5) in 30 mL of nitric acid at 20°C for 48 hours while shaking (100 rpm). In this way, the bone tissue is decalcified. 4. Recover the supernatant as the acid extract. 5. The phosphate concentration was measured using Malachite Green Phosphate Assay Kit (BioAssay Systems). The measurement method was in accordance with the manual attached to the product. During the measurement, the supernatant was diluted with distilled water.

[0124] [result] The results are shown in Fig.13 . Phosphoric acid was extracted from the bone tissue (2) pretreated by heating at 50°C in an amount 1.18 times greater than that from the bone tissue (1) not pretreated. In addition, phosphoric acid was extracted from the bone tissues (3) to (5) pretreated by microwave irradiation in an amount up to 1.26 times greater than that from the bone tissue (1) not pretreated.

[0125] It can be seen from this that the amount of phosphoric acid extracted from the acid extract increases by performing appropriate pretreatment. In particular, microwave irradiation is completed in a short time, does not require heating, can be applied to large bone tissues, and can further increase the extraction rate of phosphoric acid, so it is a preferred method.

[0126] [Example 5: Analysis of protein components contained in acid extract] The protein components contained in the acid extract were analyzed according to the following procedure. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKA TUBE MILL 100, IKA JAPAN Co., Ltd.). 2. Add 30 mL of hydrochloric acid (1 mol / L) to 2 g of wet weight of pig bones, and immerse at 20°C for 48 hours while shaking (100 rpm). In this way, the bone tissue is decalcified. 4. Recover the supernatant as the acid extract. 5. The obtained acid extracts were prepared as (1) a stock acid extract, (2) a 1 / 2 diluted acid extract, and (3) a 1 / 4 diluted acid extract. 6. Add an appropriate amount of 1 mol / L NaOH solution to make the pH neutral. 5. Add an equal amount of dithiothreitol as a reducing agent and heat at 95°C for 10 minutes. 6. Electrophoresis was performed by a conventional method using 5% polyacrylamide gel (for high molecular weight components) and 12.5% ​​polyacrylamide gel (for low molecular weight components).

[0127] [result] The results are shown in Fig.14 As a control sample, type I collagen, a protein contained in large quantities in bones, and a molecular weight marker were subjected to electrophoresis using the same gel. As can be seen from the figure, no protein with a molecular weight of more than 10,000 Da that was stained by a highly sensitive silver staining kit was detected from the acid extract. In other words, it can be seen that the acid extract contains almost no protein components. It is believed that the reason is that due to the treatment with hydrochloric acid, which is a strong acid, the peptide bonds of the protein are cut and become low-molecular peptides and amino acids.

[0128] [Example 6: Preparation of protease treatment solution and protein component analysis] [Example 6-1: Preparation of protease treatment solution] A protease-treated solution was obtained according to the following procedure. 1. The bone tissue was immersed in a 1 mol / L hydrochloric acid aqueous solution for 48 hours for acid treatment. 2. The obtained treated solution is separated into an acid extract and bone tissue residue, and the acid extract is transferred to another container. 3. Add 0.1 mol / L citric acid buffer (pH 3.5) to the bone tissue residue. The amount added is 10 mL per 1 g of initial bone weight. 4. The obtained bone tissue residue was immersed in a treatment solution containing the following three proteases. The conditions for the protease treatment were as follows: protease concentration: 2% (w / w), temperature: 50°C, and pH: optimal pH. ·Proleather FG-F (Amano Enzyme Co., Ltd., derived from Bacillus sp.) ·Protease P "Amano" 3G (Amano Enzyme Co., Ltd., derived from Aspergillus melleus) Protease M "Amano" SD (Amano Enzyme Co., Ltd., derived from Aspergillus oryzae)

[0129] [result] The appearance of the treatment solution is shown in Fig.15 . For reference, the results of Example 1-5 (neurase F3G and pepsin) and Example 1-6 (kiwifruit protease) are also shown. As can be seen from the figure, even the protease bone decomposition residue discussed in this example is decomposed to obtain a protease treatment solution. It should be noted that precipitation was observed in the protease treatment solution obtained in this example, but it is believed that this is the precipitation of calcium salts caused by the liquid being close to neutral. According to the results of Example 6-2 described later, it can be said that the protein contained in the bone decomposition residue is fully decomposed by protease treatment.

[0130] [Example 6-2: Analysis of protein components contained in protease treatment solution] In the same manner as in Examples 1-5, 1-6 and 6-1, a protease treatment solution was prepared using the following protease. Pepsin (Sigma Aldrich, aspartic protease) · Peptidase R (Amano Enzyme Co., Ltd., derived from Rhizopus genus) ·Protease P "Amano" 3G (Amano Enzyme Co., Ltd., derived from Aspergillus melleus) ·Proleather FG-F (Amano Enzyme Co., Ltd., derived from Bacillus sp.) Neuroenzyme F3G (Amano Enzyme Co., Ltd., derived from Rhizopus niveus) Protease M "Amano" SD (Amano Enzyme Co., Ltd., derived from Aspergillus oryzae) Kiwifruit enzyme (derived from kiwi fruit, cysteine ​​protease)

[0131] The obtained protease treatment solution was diluted 10-fold (lane A) or 5-fold (lane B) and subjected to electrophoresis using 16% polyacrylamide gel. The electrophoresed proteins were silver stained. As a control sample, a solution to which only the enzyme was added (lane C) was also subjected to electrophoresis.

[0132] The results are shown in Fig.16 As shown in the figure, any protease treatment solution contains protein components with different molecular weights from the enzyme (lane C). In other words, no matter which protease is used for treatment, the protein contained in the bone tissue residue is decomposed. The decomposed peptides are used by the plant as a nutrient source.

[0133] [Example 7: Recovery of Phosphoric Acid from Bone Tissue] Phosphoric acid was recovered as a precipitate from the acid extract according to the following procedure. In addition, the recovery rate of phosphoric acid was calculated. 1. Pork bones obtained from a slaughterhouse were finely pulverized using a grinder (IKATUBE MILL 100, IKA JAPAN Co., Ltd.). 2. Soak the crushed pig bones in 1N nitric acid aqueous solution or 1N hydrochloric acid aqueous solution for 48 hours. 3. Recover the supernatant to obtain the acid extract. 4. To 0.5 mL of the acid extract, 30 μL, 50 μL, 70 μL, 100 μL or 120 μL of a 5N sodium hydroxide aqueous solution was added and the mixture was allowed to stand at room temperature for 1 hour to precipitate phosphoric acid. 5. Separate the reaction solution into supernatant and precipitate by centrifugation. 6. Add 0.5 mL of 1N hydrochloric acid aqueous solution to the precipitate to redissolve the phosphoric acid. 7. The phosphoric acid content in the re-dissolved solution of the precipitate obtained in step 5 and the supernatant obtained in step 4 was measured. The measurement was performed using Malachite Green Phosphate Assay Kit (BioAssay Systems). In addition, the phosphoric acid recovery rate was calculated based on the phosphoric acid content in the acid extract obtained in step 3.

[0134]

Table 8

[0135] [result] The results are shown in Table 8. In the acid extract using nitric acid, if the amount of NaOH aqueous solution added is 100 μL or more, more than 70% of phosphoric acid can be recovered as a precipitate. On the other hand, if the amount of NaOH aqueous solution added is 120 μL, the phosphoric acid contained in the supernatant is reduced to about 10%. In the acid extract using hydrochloric acid, if the amount of NaOH aqueous solution added is 70 μL or more, more than 70% of phosphoric acid can be recovered as a precipitate. On the other hand, if the amount of NaOH aqueous solution added is 100 μL, the phosphoric acid contained in the supernatant is reduced to about 10%. In this way, by adding an appropriate amount of NaOH aqueous solution to the acid extract, phosphoric acid can be recovered and roughly purified as a precipitate.

[0136] Incidentally, the content of phosphoric acid in the acid extract using nitric acid was 24.6 mg. This is equivalent to 34.7% of the wet weight (71 mg) of the pig bones used in step 2. In addition, the content of phosphoric acid in the acid extract using hydrochloric acid was 15.1 mg. This is equivalent to 20.2% of the wet weight (74.5 mg) of the pig bones used in step 2. Since phosphoric acid accounts for 25 to 35% of the weight of the bone tissue before drying, a maximum of 99% (=34.7 / 35×100) of phosphoric acid can be extracted by preparing the acid extract.

[0137] [Example 8: Purification of phosphoric acid by adding sulfate] [Example 8-1: Discussion on the recovery rate of phosphoric acid in the supernatant] Calcium was removed from the redissolved solution of the phosphoric acid precipitate obtained in Example 7 in the form of calcium sulfate precipitate according to the following procedure. 1. A redissolved solution of phosphoric acid precipitate was prepared in the same manner as in Example 7. The acid used in step 2 of Example 7 was 1N nitric acid aqueous solution or 1N hydrochloric acid aqueous solution. The amount of 5N sodium hydroxide aqueous solution added in step 4 of Example 7 was 100 μL. 2. Add sulfuric acid or sulfate (sodium sulfate, potassium sulfate, ammonium sulfate or magnesium sulfate). The amount of sulfuric acid or sulfate added is an amount that the final concentration is 0.4M, 0.6M, 0.8M or 1.0M. 3. Remove the generated calcium sulfate precipitate by centrifugation. 4. Determine the weight of phosphoric acid contained in the supernatant. The determination was performed using the Malachite Green Phosphate Assay Kit (BioAssay Systems). In addition, the phosphoric acid recovery rate was calculated based on the phosphoric acid content in the precipitate (the precipitate obtained in step 5 of Example 7) produced by adding sodium hydroxide aqueous solution to the acid extract before adding sulfuric acid or sulfate.

[0138]

Table 9

[0139] [result] The results are shown in Table 9. It is known that if the concentration of sulfate is appropriately set, sulfate can also achieve the same degree of phosphoric acid recovery as sulfuric acid. In addition, at a low concentration of 0.4M, there is a tendency that the phosphoric acid concentration obtained by the addition of sulfate is slightly higher than the phosphoric acid concentration obtained by the addition of sulfuric acid. Importantly, the addition of sulfate can not only reduce the volume of the system compared to the addition of sulfuric acid, but also the concentration of the phosphoric acid obtained is about 1.5 times higher. In this regard, the method involved in one embodiment of the present invention is a useful method for purifying phosphoric acid. Furthermore, when the technology is put into practical use, it is preferred that the addition amount of sulfuric acid or sulfate is small, which once again proves the effectiveness of the calcium removal effect of sulfate.

[0140] The use of sulfates instead of sulfuric acid in the precipitation of calcium has the following advantages. Phosphoric acid concentration is about 1.5 times higher. Since no liquid is added, the volume increase of the reaction system can be reduced. Since the reaction system does not become strongly acidic, the amount of base required for neutralization is small. High security.

[0141] [Example 8-2: Study on the ability to remove calcium from the supernatant] The calcium content in the supernatant obtained in step 4 of Example 8-1 was measured. LAQUAtwin-Ca-11 was used for the measurement. In addition, the calcium content in the precipitate (the precipitate obtained in step 5 of Example 7) produced by adding a sodium hydroxide aqueous solution to the acid extract before adding sulfuric acid or sulfate was used as a reference to calculate the calcium residual rate.

[0142]

Table 10

[0143] [result] The results are shown in Table 10. If compared at the same concentration, the calcium residual rate of sulfate is generally lower than that of sulfuric acid. For example, in an experimental system in which 0.4M sodium hydroxide was added after acid treatment with hydrochloric acid, the amount of calcium in the solution was 1,210μg in the case of H2SO4, while it was 155-270μg in the case of sulfate. In other words, in terms of calcium removal capacity under this condition, the calcium removal capacity of sulfate is up to 7.8 times higher. In addition, it is important to compare the solution to which sulfate was added with the solution to which sulfuric acid was added, the volume of the former solution was about 1 / 2 of the latter, and the calcium concentration of the former solution was reduced to about 1 / 2 of the latter solution. In other words, by adding sulfate, calcium that is not necessary for purifying phosphoric acid can be efficiently removed.

[0144] When comparing the acids used in the acid treatment, the calcium residual rate in the acid treatment using hydrochloric acid was lower than that in the acid treatment using nitric acid. The system in which 1M potassium sulfate was added to the acid extract treated with hydrochloric acid was the most effective in removing calcium.

[0145] Table 11 shows the result based on table 9,10, calculates the value of the relative ratio (%) of calcium amount (mg) / phosphoric acid amount (mg).Although phosphoric acid can also be recovered by adding sulfuric acid, at any concentration, the residual amount of calcium is more than the experimental system with added sulfate.On the other hand, it is also shown that if sulfate is added to recover phosphoric acid, then compared with the experimental system with added sulfuric acid, the residual amount of calcium significantly decreases, and the recovery of phosphoric acid is relatively high.Like this, by adding appropriate sulfate, the residual amount of calcium can be reduced to 0.2 weight % when the recovery of phosphoric acid is not reduced.Therefore, it can be said that in the purification of phosphoric acid extracted from bone tissue, compared with sulfuric acid, sulfate is preferably used.

Table 11

[0146] [Example 8-3: Study on the leakage rate of phosphoric acid into the precipitate] The phosphoric acid content in the calcium sulfate precipitate obtained in step 3 of Example 8-1 was measured according to the following procedure. 1. Add EDTA (pH 7.4) and 5N sodium hydroxide to the calcium sulfate precipitate to redissolve it. 2. Determine the phosphoric acid content in the obtained solution. The determination was performed using Malachite Green Phosphate Assay Kit (BioAssay Systems). In addition, the phosphoric acid leakage rate was calculated based on the phosphoric acid content in the precipitate (the precipitate obtained in step 5 of Example 7) produced by adding sodium hydroxide aqueous solution to the acid extract before adding sulfuric acid or sulfate.

[0147]

Table 12

[0148] [result] The results are shown in Table 12. As can be seen from the table, if the concentration of sulfate is appropriately adjusted, the phosphoric acid content in the calcium sulfate precipitate can be reduced to the same level as sulfuric acid. If the concentration of sulfate is 0.4M, the phosphoric acid leakage can be sufficiently reduced.

[0149] [Example 8-4: Discussion of Total Phosphoric Acid Recovery Rate] The total amount of the phosphoric acid recovery rate in the supernatant discussed in Example 8-1 and the phosphoric acid leakage rate to the precipitate discussed in Example 8-3 was discussed. The phosphoric acid contained in the precipitate may be recovered by washing the precipitate. For example, the phosphoric acid contained in the precipitate can be recovered by washing the precipitate (calcium sulfate) with pure water. Therefore, the more the total phosphoric acid content, the more potential amount of phosphoric acid that can be recovered.

[0150]

Table 13

[0151] [result] The results are shown in Table 13. It can be seen that if the concentration is appropriately adjusted, even sulfate can achieve a phosphoric acid recovery rate comparable to that of sulfuric acid. The total recovery rate of the acid extract using hydrochloric acid is high, but the absolute phosphoric acid content of the acid extract using hydrochloric acid and the acid extract using nitric acid is comparable.

[0152] [Example 9: Analysis of RNA expression in plants 2] [Creation of cDNA library and analysis of gene expression using next-generation sequencer] The same procedure as in Example 3 was followed.

[0153] [Analysis of genes with changing expression levels] The same procedure as in Example 3 was followed. The expression levels were compared in two groups: bone dissolving solution B vs. commercial liquid fertilizer, and a mixed solution of bone dissolving solution B and commercial liquid fertilizer vs. commercial liquid fertilizer.

[0154] [result] Fig.18This is the analysis result of the expression change genes in the leaves of new shoots cultivated for 5 days after applying bone dissolving solution B or commercially available liquid fertilizer. There are 1,568 genes whose FPKM values ​​increased by more than 2 times. There are 1,654 genes whose FPKM values ​​decreased by less than half. Therefore, the expression levels of a total of 3,222 genes changed. The result of GO enrichment analysis showed that among the genes with changed expression levels, there were 65 genes related to growth control, 44 genes related to photosynthesis, and 26 genes related to light collection in the photochemical system I of photosynthesis.

[0155] Fig.19 This is the analysis result of the expression change genes in the roots of new shoots cultivated for 5 days with only a mixture of bone dissolving solution B and commercial liquid fertilizer or commercial liquid fertilizer. There are 766 genes whose FPKM values ​​increase by more than 2 times. There are 1,235 genes whose FPKM values ​​decrease to less than one-half. Therefore, the expression levels of a total of 2,001 genes change. The result of GO enrichment analysis is that among the genes with changed expression levels, there are 17 genes related to nitrate assimilation, 16 genes related to the elongation of root hairs, and 12 genes related to the uptake of nitrate.

[0156] Fig. 20 It is the analysis result of the expression change genes in the leaves of new shoots cultivated for 5 days with only a mixture of bone dissolving solution B and commercial liquid fertilizer or commercial liquid fertilizer. There are 582 genes whose FPKM values ​​increase to more than 2 times. There are 662 genes whose FPKM values ​​decrease to less than one-half. Therefore, the expression levels of a total of 1,244 genes change. The result of GO enrichment analysis is that among the genes with expression changes, there are 32 genes related to the response to abscisic acid (plant hormone), 13 genes related to the elongation of root hairs, and 6 genes related to the promotion of germination.

[0157] according to Figures 18 to 20 The results shown show that the bone dissolving solution B changes the gene expression of the new shoots. In particular, the expression of the gene group related to the tissue growth of the leaves and roots, photosynthesis in the leaves, and nutrient absorption in the roots is greatly changed.

[0158] [Example 10: Study on the efficiency of calcium ion removal by addition of sulfate] By adding sulfate to the redissolved solution of the phosphate precipitate, calcium ions are removed in the form of calcium carbonate precipitates. The calcium ion content in the supernatant after the precipitate is measured to investigate the calcium removal efficiency. The specific procedure is as follows. 1. A redissolved solution of phosphoric acid precipitate was prepared in the same manner as in Example 7. The acid used in step 2 of Example 7 was a 1N aqueous hydrochloric acid solution. The amount of the 5N aqueous sodium hydroxide solution added in step 4 of Example 7 was 100 μL. 2. Add liquid sulfuric acid (H2SO4) or solid sulfate (Na2SO4, K2SO4, Mg2SO4 and (NH4)2SO4). The amount of sulfuric acid or sulfate added is such that the final concentration is 0.4M. 3. Remove the generated calcium sulfate precipitate by centrifugation. 4. Determine the weight (mg) of calcium ions contained in the supernatant. The determination of calcium ions was carried out under precise measurement conditions using a high-speed ion chromatograph IC-8100EX (Tosoh Corporation) connected to a TSKgelSuperIC-Cation HSII (4.6mm ID×10cm). A mixture of 3.0mmol / L of methanesulfonic acid and 2.7mmol / L of 18-crown ether-6 was used as the eluent. The measurement temperature was 40°C, the flow rate was 1.0mL / min, and the injection volume was 30μL. The conductivity (μS) was measured, and the regression equation was obtained from the area of ​​the standard substance to determine the calcium ion concentration. The calcium ion content of each sample (30μL) was calculated from the calcium ion concentration.

[0159]

Table 14

[0160] [result] The results are shown in Table 14. The system with the addition of liquid sulfuric acid not only increased the overall volume of the system, but also had the lowest calcium ion removal rate of 73%. In the system with the addition of solid sulfate, the overall volume of the system increased less, and the calcium ion removal rate was as high as 91-94%. In addition, since sulfuric acid, which is a strong acid, is not used, the method of adding sulfate is also safe. Furthermore, by appropriately increasing or decreasing the amount of sulfate added, the desired concentration of calcium can also be retained.

[0161] When phosphoric acid or fertilizer containing phosphoric acid is produced from bone tissue, calcium ions contained in the bone tissue become a reason for reducing the recovery of phosphoric acid. This is because, in the neutral region, calcium ions combine with phosphate ions to form calcium phosphate precipitation. Therefore, it is desirable to remove calcium ions by precipitation, which can be removed smoothly by the addition of sulfate.

[0162] Potassium ions, magnesium ions or ammonium ions contained in sulfate are components necessary for plant growth. Therefore, when potassium sulfate, magnesium sulfate or ammonium sulfate is used as sulfate, the fertilizer can contain components necessary for plant growth. Alternatively, even if the alkali added in step 4 of Example 7 is changed from sodium hydroxide to potassium hydroxide, the fertilizer can contain components necessary for plant growth. If such a manufacturing method is adopted, a fertilizer with improved value can be manufactured.

[0163] [Example 11: Purification of phosphoric acid by adding carbonate] Calcium was removed from the redissolved solution of the phosphoric acid precipitate obtained in Example 7 in the form of calcium carbonate precipitate according to the following procedure. 1. A redissolved solution of phosphoric acid precipitate was prepared in the same manner as in Example 7. The acid used in step 1 of Example 7 was 1N aqueous nitric acid solution or 1N aqueous hydrochloric acid solution. The amount of 5N aqueous sodium hydroxide solution added in step 4 of Example 7 was 100 μL. 2. Add carbonate (solid sodium bicarbonate or sodium carbonate). The amount of sodium bicarbonate added is an amount that the final concentration is 0.4 M. The amount of sodium carbonate added is an amount that the final concentration is 0.6 M. 3. Remove the generated calcium carbonate precipitate by centrifugation. 4. Determine the concentration (ppm) of phosphate ions contained in the supernatant. The determination of phosphate ions was carried out under precise measurement conditions using a high-speed ion chromatograph IC-8100EX (Tosoh Corporation) connected to a TSKgel SuperIC-Anion HS (4.6mm ID×10cm). A mixture of 7.5mmol / L sodium bicarbonate and 0.8mmol / L sodium carbonate was used as the eluent. The measurement temperature was 40°C, the flow rate was 1.5mL / min, and the injection volume was 30μL. The conductivity (μS) was measured, and the regression equation was obtained from the area of ​​the standard substance to determine the phosphate ion concentration. The phosphate ion concentration of each sample (30μL) was calculated from the phosphate ion concentration.

[0164]

Table 15

[0165] [result] The results are shown in Table 15. By adding carbonate, calcium ions are precipitated as calcium carbonate, and phosphate ions remain in the supernatant. For example, in a system in which sodium bicarbonate is added to an acid extract using hydrochloric acid, the supernatant contains 9,000 ppm or more of phosphoric acid. The carbonate ions remaining in the supernatant are converted into carbon dioxide when heated, so they can be easily removed.

[0166] [Example 12: Removal of cations contained in sulfate] [Example 12-1: Removal of sodium ions or potassium ions] The cations (sodium ions or potassium ions) contained in the sulfate added to remove the calcium ions are removed in the following order: Specifically, the sodium ions or potassium ions are adsorbed using a strong cation exchange gel. 1. TSKgel SP-TOYOPEARL 650M gel (Tosoh Corporation) was decanted with pure water and filled into a micro spin column (GE Healthcare). 2. Add an appropriate amount of the supernatant after adding sulfate and removing calcium sulfate to the upper layer of the gel. 3. Pass the gel through the supernatant by centrifugation using a benchtop centrifuge. Collect the flow-through fraction through the gel. 3. The content (mg) of sodium ions or potassium ions contained in the flow-through fraction was measured. The sodium ion was measured using LAQUAtwin-Na-11 (Horiba Advanced Technologies Co., Ltd.). The potassium ion was measured using LAQUAtwin-K-11 (Horiba Advanced Technologies Co., Ltd.).

[0167]

Table 16

[0168] [result] The results are shown in Table 16. The supernatant after calcium sulfate precipitation by adding sodium sulfate or potassium sulfate contains sodium ions or potassium ions. These ions can be removed by strong cation exchange gel. Specifically, sodium ions are removed by 83%, and potassium ions are removed by 86%. By repeatedly circulating to the strong cation exchange gel, more cations can be removed.

[0169] Thus, it is shown that in the method of adding sulfate, the cations added as sulfate can be removed by the strong cation exchange gel. However, in the case of making fertilizer from bone tissue, potassium ions, magnesium ions and ammonium ions are important nutrients for plant growth, so they do not need to be removed.

[0170] [Example 12-2: Removal of magnesium ions or ammonium ions] The cations (magnesium ions or ammonium ions) contained in the sulfate added to remove the calcium ions are removed in the following order: Specifically, the magnesium ions or ammonium ions are adsorbed using a strong cation exchange gel. 1. TSKgel SP-TOYOPEARL 650M gel (Tosoh Corporation) was decanted with pure water and filled into a micro spin column (GE Healthcare). 2. Add an appropriate amount of the supernatant after adding sulfate and removing calcium sulfate to the upper layer of the gel. 3. Pass the gel through the supernatant by centrifugation using a benchtop centrifuge. Collect the flow-through fraction through the gel. 3. Determine the content (μg) of magnesium ions, ammonium ions or calcium ions contained in the flow fraction. The ion concentration was determined using a high-speed ion chromatograph IC-8100EX (Tosoh Corporation) connected to a TSKgel SuperIC-Cation HSII (4.6mm ID×10cm) under precise measurement conditions. A mixture of 3.0mmol / L of methanesulfonic acid and 2.7mmol / L of 18-crown ether-6 was used as the eluent. The measurement temperature was 40°C, the flow rate was 1.0mL / min, and the injection volume was 30μL. The conductivity (μS) was measured, and the regression equation was obtained from the area of ​​the standard substance to determine the calcium ion concentration. The ion content of each sample (30μL) was calculated from the ion concentration.

[0171]

Table 17

[0172] [result] The results are shown in Table 17. It is shown that magnesium ions, ammonium ions and calcium ions can be removed from the supernatant by contacting with the strong cation exchange gel. More cations including calcium ions can be removed by repeatedly circulating to the strong cation exchange gel. This suggests that the purity of phosphoric acid can be improved.

[0173] [Example 13: Purification of Phosphoric Acid from Commercially Available Bone Powder] Commercially available steamed bone meal (Omiya Green Service Co., Ltd.) was solubilized in the following procedure to recover phosphoric acid. 1. Add 10 mL of sulfuric acid (1N), hydrochloric acid (1N) or nitric acid (1N) to 1 g of steamed bone meal and shake at 25°C for 19 hours. 2. Use a centrifuge to separate the obtained acid extract into supernatant and precipitate. 3. Add 0.1 mL of NaOH aqueous solution (5N) to 0.5 mL of the supernatant and shake for 1 hour. 4. Separate the reaction solution into supernatant and precipitate by centrifugation. 5. Add an appropriate amount of hydrochloric acid (1N) to the precipitate to dissolve it. 6. Repeat steps 3 to 5 multiple times. Then, the precipitate was dissolved in 0.5 mL of hydrochloric acid (0.4 N). Thus, a precipitate solution in which phosphoric acid was concentrated was obtained. 7. Determine the anion content in the obtained precipitate solution. The measurement is carried out under precise measurement conditions using a high-speed ion chromatograph IC-8100EX (Tosoh Corporation) connected to a TSKgel SuperIC-Anion HS (4.6mm ID×10cm). A mixture of 7.5mmol / L sodium bicarbonate and 0.8mmol / L sodium carbonate is used as the eluent. The measurement temperature is 40°C, the flow rate is 1.5mL / min, and the injection volume is 30μL. Measure the conductivity (μS), and calculate the regression equation from the area of ​​the standard substance to determine the anion ion concentration. Calculate the anion content of each sample (30μL) from the anion ion concentration.

[0174]

Table 18

[0175] [result] The results are shown in Table 18 and Fig.21 . Even if commercially available steamed bone powder (bone tissue that has been heated under high pressure) is used as a raw material, phosphoric acid can be efficiently and relatively safely recovered by the method for producing phosphoric acid involved in one embodiment of the present invention. According to Table 18, the recovery efficiency of phosphoric acid using an acid extract using hydrochloric acid or nitric acid is higher than that using an acid extract using sulfuric acid. The phosphoric acid recovery efficiency of the system using hydrochloric acid or nitric acid is 3.2 to 3.4 times that of the system using sulfuric acid.

[0176] This is also Fig.21 According to the elution curve of the ion chromatogram shown in the figure, in the system using hydrochloric acid or nitric acid, anions other than phosphate ions are almost not contained except chloride ions (hydrochloric acid is used in step 5 to dissolve the precipitate). On the other hand, in the system using sulfuric acid, sulfate ions are detected in addition to phosphate ions.

[0177] The results of this example show that phosphoric acid can be extracted from commercially available bone powder (bone tissue that has been heated under pressure). This proves that the method for producing phosphoric acid according to one embodiment of the present invention is a sustainable technology with low energy cost and less environmental damage than the method for recovering phosphoric acid from phosphate rock or dried sewage sludge.

[0178] [Example 14: Preparation of protease treatment solution from commercially available bone powder] Commercially available steamed bone meal (Omiya Green Service Co., Ltd.) was solubilized in the following procedure to prepare a protease treatment solution. 1. Add 10 mL of sulfuric acid (1N), hydrochloric acid (1N) or nitric acid (1N) to 1 g of steamed bone meal and shake at 25°C for 24 hours. 2. Use a centrifuge to separate the obtained acid extract into a supernatant (acid extract) and a precipitate (bone residue) for recovery. 3. Add 10 mL of 0.1 mol / L citric acid buffer (pH 3) or 0.1 mol / L Tris hydrochloric acid buffer (pH 8) to the precipitate. 4. Follow Figure 1 S5 of the invention is used to prepare a protease treatment solution from the precipitate. As a protease, neuroenzyme F3G (Amano Enzyme Co., Ltd.) or papain W-40 (Amano Enzyme Co., Ltd.) is used, and the treatment is carried out in the same order as in Example 1-5. Specifically, it is as follows. Neuroenzyme F3G system: protease concentration = 1% (w / w) of initial bone weight, buffer = citric acid buffer (pH 3), temperature = 37°C, immersion time = 3 days Papain W-40 system: protease concentration = 1% (w / w) of initial bone weight, buffer = Tris hydrochloric acid buffer (pH 8), temperature = 37°C, immersion time = 3 days 5. Centrifuge the reaction solution to separate the precipitate and the supernatant.

[0179] [result] The results are shown in Fig. 22 , 23 . Commercially available steamed bone meal is a mixture of pig bones and chicken bones that have been heat-treated under high pressure. Even if this bone meal is used as a raw material, a protease-treated liquid can be prepared by the method for manufacturing a fertilizer involved in one embodiment of the present invention. The protease-treated liquid can be used as a fertilizer itself, and can also be used as a raw material for bone dissolving solution B. Liquid fertilizers can be expected to have a quick-acting plant growth effect that solid bone meal cannot. In addition, liquid fertilizers can also be used in hydroponic cultivation and foliar spreading.

[0180] Regarding the protease treatment using the neuroenzyme F3G, the bone residues treated with hydrochloric acid were almost completely dissolved by the protease treatment. The bone residues treated with nitric acid were completely dissolved by the protease treatment. White precipitates were also observed after the protease treatment of the bone residues treated with sulfuric acid. This precipitate was considered to be calcium sulfate, and it is believed that at least a part of the protein component was decomposed.

[0181] About the protease treatment using papain W-40, the bone residue after acid treatment with hydrochloric acid or nitric acid is almost completely dissolved by protease treatment. The bone residue after acid treatment with sulfuric acid is also observed to have a white precipitate after protease treatment. This precipitate is considered as calcium sulfate, and it is believed that at least a part of the protein component is decomposed.

[0182] As can be seen from the above results, when the protease treatment solution is obtained using an acid extract using sulfuric acid as a raw material, it is sometimes necessary to remove the precipitate by centrifugation. When the protease treatment solution is obtained using an acid extract using hydrochloric acid or nitric acid as a raw material, it is not necessary to remove the precipitate. From this point of view, it is preferred to use hydrochloric acid or nitric acid in the acid treatment process. In addition, for the centrifugal supernatant of the solution after the protease treatment, what has been acid-treated with sulfuric acid is transparent, and what has been acid-treated with nitric acid or hydrochloric acid is turbid. As can be seen from the results, in order to more completely decompose bone residues, it is more preferred to carry out acid treatment with hydrochloric acid or nitric acid. However, it should be noted that sulfuric acid can also be used to prepare the protease treatment solution.

[0183] [Example 15: Determination of peptide concentration in acid extract using commercially available bone powder as raw material] An acid extract was prepared from commercially available steamed bone powder (Omiya Green Service Co., Ltd.) according to the following procedure. The peptide concentration contained in the acid extract was measured. 1. Add 10 mL of sulfuric acid (1N), hydrochloric acid (1N) or nitric acid (1N) to 1 g of steamed bone meal and shake at 25°C for 24 hours. 2. Use a centrifuge to separate the obtained acid extract into a supernatant and a precipitate. Recover the supernatant as the acid extract. 3. Add 0.4 mol / L potassium hydroxide aqueous solution to 0.5 mL of the supernatant to precipitate discrete calcium. 4. Determine the peptide concentration in the supernatant obtained by removing the precipitate from the reaction solution obtained in step 3. The determination was performed using a protein assay BCA kit (product number 297-73101, Fujifilm Wako). The determination method was in accordance with the product manual. The absorbance at 540 nm was measured. The higher the absorbance, the higher the peptide concentration. 5. Recover the precipitate from the reaction solution obtained in step 3. At this time, only the system treated with hydrochloric acid or nitric acid in step 1 is recovered. 6. Use 1N hydrochloric acid to completely dissolve the precipitate. Then, add 0.4 mol / L potassium hydroxide again to precipitate calcium phosphate. Repeat this dissolution-precipitation process three times. 7. In step 6, after the first and third repetitions, the peptide concentration in the supernatant after removing the precipitate from the reaction solution was measured. The measurement was performed using a protein assay BCA kit (product number 297-73101, Fujifilm Wako). The measurement method was in accordance with the product manual. The absorbance at 540 nm was measured. The higher the absorbance, the higher the peptide concentration.

[0184]

Table 19

[0185] [result] The results are shown in Table 19. Peptides were detected in the acid extract prepared using commercially available steamed bone powder as a raw material. The peptide concentration increased in the order of the acid extract treated with hydrochloric acid, the acid extract treated with sulfuric acid, and the acid extract treated with nitric acid. This result shows that a large amount of peptides are contained in the acid extract treated with hydrochloric acid in particular. Peptides are organic components contained in bone tissue. Therefore, it is suggested that the acid extract contains a component that brings about a plant growth effect.

[0186] In Example 5, it was shown that the acid extract contained almost no protein component stained by the silver staining kit (see also Fig.14 ) As for the reason, in Example 5, it was presumed that the peptide bonds of the protein were cleaved to form low-molecular peptides and amino acids. This example confirms this presumption.

[0187] Peptides become impurities in the production of phosphoric acid. It is known that peptides as impurities are formed by repeating the dissolution-precipitation process of calcium phosphate ( Figure 3 As shown in Table 19, by repeating the dissolution-precipitation process three times, the peptide concentration was reduced to 1 / 100. From this result, it can be seen that the peptide can be successfully removed from the acid extraction solution treated with hydrochloric acid or nitric acid, and the phosphoric acid concentration can be increased. [Possibility of Industrial Application]

[0188] The present invention can be used for the production of phosphoric acid, etc.

Claims

1. A method for producing phosphoric acid, comprising the following steps: (a) treating the bone tissue with acid to obtain an acid extract; (b) adding alkali to the obtained acid extract to obtain precipitated calcium phosphate; (c) adding acid to the obtained calcium phosphate precipitate to obtain a calcium phosphate solution; and (d) a step of adding one or more selected from the group consisting of sulfates, carbonates, and bicarbonates to the obtained calcium phosphate solution to remove precipitated calcium.

2. The method according to claim 1, further comprising, before step (a), a step of pre-treating the bone tissue. The pretreatment is at least one selected from the group consisting of heating the bone tissue, heating the bone tissue under pressure, and irradiating the bone tissue with microwaves.

3. The production method according to claim 1, further comprising, after the step (d), a step of removing anions and cations other than phosphate ions and hydrogen ions.

4. The production method according to claim 1, wherein the step (b) and the step (c) are repeated two or more times.

5. The production method according to claim 1, wherein in the step (a), the bone tissue is acid-treated with one or more selected from the group consisting of nitric acid, hydrochloric acid, formic acid and sulfuric acid.

6. The production method according to claim 1, wherein in the step (d), sulfuric acid is not added to the calcium phosphate solution.

Citation Information

Patent Citations

  • Method for extracting biological sclerotin calcium phosphate

    CN101429531A

  • Method for preparing high pure phosphoric acid from calcium hydrogen phosphate

    CN102992288A

  • Process for producing wet method phosphoric acid by medium low grade phosphorus mine

    CN1792776A

  • Method for producing phosphoric acid from bone, and method and device for employing phosphoric acid produced from bone in the fermentation of sugar

    WO2011115302A1