System and method for resource utilization of sulfur-rich tail gas
Through a simplified sulfur-rich exhaust resource utilization system, spray absorption and negative pressure flash evaporation technology, the problems of complex systems, high energy consumption and safety hazards in the existing technology are solved, and efficient and low-cost resource utilization is achieved , the obtained concentrated H2SO4 and calcium sulfate precipitation have high added value and achieves zero wastewater and zero waste slag emissions.
Patent Information
- Application Number
- CN202411007659.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing sulfur-rich exhaust resource utilization technology has problems such as complex system processes, high energy consumption, high cost and safety hazards.
A system for resource utilization of sulfur-rich exhaust gas is designed, including lime water supply device, oxidized air source, spray absorption device, clarifier, heat exchanger and flash separator, through spray absorption and negative pressure flash Technology, using the waste heat of sulfur-rich exhaust gas to cool down and concentrate sulfuric acid, simplify the process flow, reduce energy consumption, and use safe and reliable lime water as an absorber.
It realizes efficient, safe and low-cost resource utilization of sulfur-rich exhaust gas, reduces operating costs, and improves exhaust gas utilization. The recovered concentrated H2SO4 and calcium sulfate precipitation have high added value, achieving zero wastewater and zero waste slag emissions.
Smart Images

Figure CN118925467A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of resource processing of sulfur-rich tail gas, and in particular to a system and method for resource utilization of sulfur-rich tail gas. Background Art
[0002] There are a lot of pollutants such as SO2, NOx, dust, and dioxins in the exhaust gas from sintering of steel plants, coal-fired exhaust gas from thermal power plants, exhaust gas from large boilers, and various smelting exhaust gases. The activated coke desulfurization and denitrification process uses the adsorption characteristics of the activated coke itself to achieve efficient and coordinated removal of pollutants including dust, dioxins, SO2, and NOx. After the dioxins in the flue gas are enriched by the activated coke, the high temperature and catalytic action in the regeneration tower destroy the oxygen groups between the benzene rings and crack them into harmless substances, without the need to add additional dioxin removal equipment. The activated coke dry flue gas purification technology is widely used in the fields of chemical industry, nonferrous metallurgy, and steel production. Therefore, it has become an urgent problem to achieve the reduction of sulfur dioxide emissions and resource recovery of the regenerated gas released during the regeneration of activated coke without generating secondary pollutants such as wastewater and waste residue.
[0003] The concentration of SO2 in activated coke regeneration gas is extremely high, and the prospect of resource utilization is great. The current mainstream process is to convert SO2 into value-added products such as elemental sulfur, thionyl chloride, and ammonium sulfate to achieve resource utilization of waste gas. However, due to the limited use of elemental sulfur and the high investment costs of thionyl chloride and ammonium sulfate, the treatment of steel sintering flue gas and coal-fired boiler tail gas urgently needs to develop a treatment method that can achieve high added value and zero waste emission resource utilization of sulfur-rich tail gas.
[0004] However, the current technology for resource utilization of sulfur-rich tail gas has several shortcomings: first, the process system is complicated, and most of the time it needs to be treated by distillation, rectification and other methods, which not only increases the investment cost and operating energy consumption, but also increases the system failure rate; second, the energy consumption is high; third, the treatment raw materials use substances such as ammonia water or sodium sulfite, among which flammable and explosive fuels such as ammonia water pose a safety hazard, and the cost of sodium sulfite is high. Summary of the invention
[0005] The purpose of the present invention is to overcome the problems of the prior art in that the system process for resource utilization of sulfur-rich tail gas is complex, the energy consumption is high, the cost is high, and there are potential safety hazards, and to provide a system and method for resource utilization of sulfur-rich tail gas.
[0006] In order to achieve the above-mentioned object, the present invention provides a system for resource utilization of sulfur-rich tail gas, which includes a lime water supply device, an oxidation air source, a spray absorption device, a clarifier, a heat exchanger and a flash separator; the spray absorption device is provided with a washing section and an oxidation section from top to bottom;
[0007] The sulfur-rich tail gas is cooled in the heat exchanger, and the cooled sulfur-rich tail gas is reversely contacted with lime water from a lime water supply device in the washing section of the spray absorption device to obtain clean flue gas and washing slurry. The washing slurry is oxidized by oxidizing air from an oxidizing air source in the oxidation section, and the oxidized washing slurry is subjected to solid-liquid separation in the clarifier. The supernatant obtained by the solid-liquid separation is transported to the flash separator for negative pressure flash evaporation, and the sulfuric acid solution obtained at the lower part of the flash separator is circulated into the heat exchanger to exchange heat with the sulfur-rich tail gas in the heat exchanger, and then returned to the flash separator for negative pressure flash evaporation.
[0008] Preferably, the system further comprises a condenser, in which the steam from the flash separator is condensed into water and then returned to the spray absorption device or the lime water supply device for utilization.
[0009] Preferably, the sulfur-rich tail gas is activated coke regeneration gas.
[0010] Preferably, the system further comprises a circulation pump for circulating the sulfuric acid solution between the flash separator and the heat exchanger.
[0011] Preferably, the system further comprises a concentrated sulfuric acid storage tank for collecting concentrated sulfuric acid from the flash separator.
[0012] A second aspect of the present invention provides a method for resource utilization of sulfur-rich tail gas, the method comprising the following steps:
[0013] (1) The sulfur-rich tail gas is transported to a heat exchanger and cooled to 80-120°C;
[0014] (2) transporting the cooled sulfur-rich tail gas and lime water to a spray absorption device for contact reaction to obtain a washing slurry and clean flue gas, and the washing slurry undergoes an oxidation reaction under the action of oxidizing air;
[0015] (3) passing the oxidized washing slurry into a clarifier for solid-liquid separation to obtain a supernatant and a calcium sulfate precipitate;
[0016] (4) The supernatant is passed into a flash separator for negative pressure flash evaporation to obtain steam and sulfuric acid solution, the sulfuric acid solution is circulated into the heat exchanger to exchange heat with the sulfur-rich tail gas in the heat exchanger, and then returned to the flash separator for negative pressure flash evaporation, and the cycle is repeated to obtain concentrated sulfuric acid and steam.
[0017] Preferably, in step (1), the sulfur-rich tail gas is activated coke regeneration gas.
[0018] Preferably, in step (1), the volume fraction of sulfur dioxide in the sulfur-rich tail gas is not higher than 30%.
[0019] Preferably, the method further comprises: condensing the steam obtained in step (3), and using the water obtained by condensation to prepare the lime water in step (2).
[0020] Preferably, in step (2), the concentration of calcium hydroxide in the lime water is 15-25wt%.
[0021] Compared with the prior art, the system and method for resource utilization of sulfur-rich tail gas described in the present invention have the following advantages:
[0022] 1. Through the design of the process flow, the system of the present invention requires fewer devices and simplifies the resource utilization process.
[0023] 2. The system provided by the present invention can utilize the waste heat of high-temperature sulfur-rich tail gas (above 400°C), and utilize the waste heat of the sulfur-rich tail gas (inside the system) to continuously flash the supernatant (dilute H2SO4) to obtain concentrated H2SO4, while cooling the sulfur-rich tail gas to achieve the conditions for spray absorption; this process does not require the introduction of additional heat sources, thereby reducing operating costs.
[0024] 3. The present invention selects safe, reliable, and easily available lime water as the absorbent. Compared with ammonia water, it is safer, and compared with Na2SO3, it has a lower cost and better effect, and has the prospect of large-scale application.
[0025] 4. The concentrated H2SO4 product and calcium sulfate precipitate obtained by resource recovery of the present invention, wherein the concentrated H2SO4 has a higher added value, is widely used in laboratories and industrial production, and has a good market prospect; the calcium sulfate precipitate can enter the coal yard or other subsequent resource recovery process. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the system for resource utilization of sulfur-rich tail gas proposed by the present invention.
[0027] Description of Reference Numerals
[0028] 1-lime water supply device; 2-oxidizing air source; 3-spray absorption device; 4-clarifier; 5-heat exchanger; 6-flash separator; 7-condenser; 8-circulation pump; 9-sludge pump; 10-concentrated sulfuric acid collection device;
[0029] 31- washing section; 32- oxidation section. DETAILED DESCRIPTION
[0030] The specific implementation of the present invention is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described here is only used to illustrate and explain the present invention, and is not used to limit the present invention.
[0031] The endpoints and any values of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.
[0032] The present invention provides a system for resource utilization of sulfur-rich tail gas. Figure 1 The system comprises a lime water supply device 1, an oxidation air source 2, a spray absorption device 3, a clarifier 4, a heat exchanger 5 and a flash separator 6, wherein the spray absorption device 3 is provided with a washing section 31 and an oxidation section 32 from top to bottom;
[0033] The sulfur-rich tail gas is cooled in the heat exchanger 5, and the cooled sulfur-rich tail gas is reversely contacted with the lime water from the lime water supply device 1 in the washing section 31 of the spray absorption device 3 to obtain clean flue gas and washing slurry. The washing slurry is oxidized by the oxidizing air from the oxidizing air source 2 in the oxidation section 32. The oxidized washing slurry is subjected to solid-liquid separation in the clarifier 4, and the supernatant obtained by the solid-liquid separation is transported to the flash separator 6 for negative pressure flash evaporation. The sulfuric acid solution obtained at the lower part of the flash separator 6 is circulated into the heat exchanger 5 to exchange heat with the sulfur-rich tail gas in the heat exchanger 5, and then returned to the flash separator 6 for negative pressure flash evaporation.
[0034] In the present invention, negative pressure flash evaporation refers to the process in which a high-pressure sulfuric acid solution enters a relatively low-pressure container and, due to a sudden decrease in pressure, the sulfuric acid solution is converted into saturated steam and concentrated sulfuric acid solution at a portion of the container pressure.
[0035] At present, when sulfur-rich tail gas is used as a resource, it is mostly necessary to cool the sulfur-rich tail gas (about 400°C) and then treat it, which wastes heat energy. The system provided by the present invention can make full use of the waste heat of sulfur-rich tail gas, reduce the temperature of sulfur-rich tail gas, and increase the temperature of circulating dilute H2SO4 solution (supernatant) at the same time, so that the dilute H2SO4 can continuously evaporate water under negative pressure flash evaporation conditions and condense into concentrated H2SO4, without introducing external heat source, saving energy consumption.
[0036] In the present invention, the specific source of the sulfur-rich tail gas is not limited, as long as it contains sulfur dioxide that can be recycled. In a specific embodiment, the sulfur-rich tail gas can be steel plant sintering tail gas, thermal power plant coal-fired tail gas, large boiler tail gas, various smelting tail gas or desulfurized activated coke regeneration gas.
[0037] In a preferred embodiment, the sulfur-rich tail gas is desulfurized activated coke regeneration gas, which contains fewer impurities and a higher sulfur dioxide content, and has greater prospects for resource utilization.
[0038] In the present invention, the activated coke regeneration gas refers to: steel sintering flue gas or coal-fired boiler tail gas entering the desulfurization and denitrification tower containing activated coke for desulfurization and denitrification treatment. The adsorption characteristics of the activated coke itself can achieve efficient synergistic removal of pollutants including dust, dioxins, SO2 and NOx. After the activated coke in the desulfurization and denitrification tower is saturated with adsorption, the activated coke is conveyed to the regeneration tower by a conveyor. The activated coke adsorbed with pollutants is heated to 450°C in the regeneration tower to release SO2, and the SO2 gas is carried out by N2. The gas obtained at this time is the activated coke regeneration gas.
[0039] In the present invention, the washing section 31 of the spray absorption device 3 refers to the area where the sulfur-rich tail gas contacts the lime water. In the washing section 31, the following reactions are carried out:
[0040] 2SO2+Ca(OH)2=Ca(HSO3)2
[0041] In order to improve the reaction efficiency, in a preferred embodiment, the middle and lower part of the spray absorption device 3 is the sulfur-rich tail gas inlet, and the upper part is provided with a spray layer, so that the cooled sulfur-rich tail gas enters from the middle and lower part of the spray absorption device 3 and flows upward, and the spray layer located at the upper part of the spray absorption device 3 is sprayed with lime water, and the cooled sulfur-rich tail gas and lime water are cyclically sprayed and countercurrently washed to obtain clean flue gas and washing slurry. Among them, the washing slurry falls into the lower part of the spray absorption device 3, and the clean flue gas is discharged from the top of the spray absorption device 3.
[0042] In the present invention, the oxidation section of the spray absorption device 3 refers to the area where the washing slurry is located at the lower part of the spray absorption device 3. The oxidation air from the oxidation air source 2 is introduced into the oxidation section 32 (i.e., the washing slurry) to force oxidation of the washing slurry. Specifically, the following reaction is carried out in the oxidation section 32:
[0043] Ca(HSO3)2+O2=CaSO4↓+H2SO4
[0044] In a specific embodiment, the spray absorption device 3 is a spray absorption tower.
[0045] In the present invention, the washing slurry is subjected to solid-liquid separation in the clarifier 4 to obtain a supernatant and a CaSO4 precipitate. In a specific embodiment, the clarifier 4 is a high-efficiency integrated clarifier 4.
[0046] In a specific embodiment, the system further includes a circulation pump 8 for circulating the sulfuric acid solution between the flash separator 6 and the heat exchanger 5, so that the sulfuric acid solution can exchange heat with the sulfur-rich tail gas in the heat exchanger 5 to heat the sulfuric acid solution, thereby improving the efficiency of the flash evaporation.
[0047] In a preferred embodiment, the system further comprises a condenser 7, in which the steam from the flash separator 6 is condensed into water, and then returned to the spray absorption device 3 or the lime water supply device 1 for use. It can be understood that the design of the present invention is not limited to this, and the condensed water can also be used for other water-demanding ends in the system, so that water can be fully utilized and zero wastewater discharge can be achieved.
[0048] In a specific embodiment, the system further comprises a concentrated sulfuric acid collecting device 10 for collecting concentrated sulfuric acid from the flash separator 6 .
[0049] In the present invention, the sulfuric acid solution circulates between the heat exchanger 5 and the flash separator 6, and evaporates continuously until concentrated sulfuric acid is obtained. The present invention does not limit the specific concentration of the concentrated sulfuric acid, and can be designed according to actual working conditions and needs. The present invention does not limit how to control the flash separator 6 to obtain the concentrated sulfuric acid of the desired concentration, and can be achieved by changing the vacuum degree of the flash gas, connecting multiple flash separators in series, etc., which are all conventional control means in the art.
[0050] In a specific embodiment, a control valve (not shown in the figure) is provided at the bottom of the flash separator 6, and the control valve is interlocked with the density meter. When the concentrated sulfuric acid at the bottom of the flash separator 6 reaches the required concentration and corresponding density, the control valve is opened to allow the concentrated sulfuric acid at the bottom of the flash separator 6 to pass into the concentrated sulfuric acid collecting device 10 for collection.
[0051] In the present invention, lime water and the sulfur-rich tail gas after cooling are circulated and sprayed in the spray absorption device 3, countercurrent washing is performed, and then the washing slurry obtained is forcibly oxidized by oxidizing air, and the oxidized washing slurry is filtered and precipitated in the clarifier 4 to obtain a dilute H2SO4 solution (supernatant), and the supernatant enters the negative pressure flash separator 6, and circulates between the flash separator 6 and the heat exchanger 5, so that the waste heat of the sulfur-rich tail gas is used to flash the dilute H2SO4 solution to obtain a concentrated H2SO4 solution for resource utilization, and the purified tail gas meets the discharge standards. In addition, the CaSO4 precipitate is pumped into the coal yard or other subsequent resource treatment through the sludge pump 9, and the steam discharged from the upper part of the flash evaporation is condensed through the condenser 7 and circulated for water replenishment and flushing water for the entire system, effectively achieving zero wastewater and zero waste residue discharge.
[0052] The present invention also provides a method for resource utilization of sulfur-rich tail gas, which comprises the following steps:
[0053] (1) The sulfur-rich tail gas is transported to a heat exchanger and cooled to 80-120°C;
[0054] (2) The cooled sulfur-rich tail gas and lime water are transported to a spray absorption device for contact reaction to obtain a washing slurry and clean flue gas, and the washing slurry is oxidized under the action of oxidizing air;
[0055] (3) passing the oxidized washing slurry into a clarifier for solid-liquid separation to obtain a supernatant and a calcium sulfate precipitate;
[0056] (4) The supernatant is passed into a flash separator for negative pressure flash evaporation to obtain steam and sulfuric acid solution, the sulfuric acid solution is circulated into the heat exchanger to exchange heat with the sulfur-rich tail gas in the heat exchanger, and then returned to the flash separator for negative pressure flash evaporation, and the cycle is repeated to obtain concentrated sulfuric acid and steam.
[0057] In the method of the present invention, in step (1), the sulfur-rich tail gas is desulfurized activated coke regeneration gas.
[0058] The present invention does not particularly limit the specific content of sulfur dioxide in the sulfur-rich tail gas in step (1). In order to achieve better treatment effect and more stable system operation, in a preferred embodiment, in step (1), the volume fraction of sulfur dioxide in the sulfur-rich tail gas is not higher than 30%, and more preferably 10-30%.
[0059] The present invention does not limit the concentration of the lime water in step (2), and can be designed according to actual working conditions. In a specific embodiment, in step (2), the concentration of calcium hydroxide in the lime water is 15-25wt%.
[0060] The present invention also does not limit the dosage relationship between the sulfur-rich tail gas, lime water and oxidizing air, and can be designed according to actual conditions, as long as the calcium hydroxide in the lime water and the oxygen in the oxidizing air are slightly excessive, the sulfur dioxide in the sulfur-rich tail gas can be fully absorbed, and the obtained clean flue gas can be directly discharged into the atmosphere.
[0061] In the present invention, oxidizing air refers to air filtered by an oxidizing blower. The present invention has no particular restrictions on the composition and source of the oxidizing air, and it can be conventional oxidizing air in the art.
[0062] In the method described in the present invention, in step (2), the clean flue gas obtained by removing sulfur dioxide meets the emission standards and can be directly discharged into the atmosphere.
[0063] In the current sulfur-rich tail gas resource utilization process, the process system flow is complicated, and most of them need to be treated by distillation, rectification and other methods, which not only increases the investment cost and operating energy consumption, but also increases the system failure rate. The process provided by the present invention simplifies the resource utilization process through the waste heat utilization technology of sulfur-rich tail gas, the technology of negative pressure flash evaporation concentration of H2SO4, the lime water circulation spray countercurrent washing technology, and the design of the clarifier 4 solid-liquid separation technology, with low energy consumption, low cost, high safety, and ensures the stable operation of the system. At the same time, the tail gas utilization rate is high, and the recovered products have high added value.
[0064] The process provided by the present invention can completely treat sulfur-rich tail gas in a harmless, reduced and resource-based manner. The process uses the waste heat of the sulfur-rich tail gas to cool it down and enter the spray absorption device 3, and then wash it in countercurrent with lime water (Ca(OH)2 solution). The clean flue gas with sulfur dioxide removed is discharged into the atmosphere, and the washing slurry enters the clarifier 4. After precipitation and clarification, the supernatant (dilute H2SO4) enters the negative pressure flash separator 6. The obtained sulfuric acid solution is circulated between the flash separator 6 and the heat exchanger 5, and the waste heat of the sulfur-rich tail gas is used as a heat source for flash evaporation. After continuous evaporation, concentrated H2SO4 is obtained at the bottom of the flash separator 6 and enters the concentrated sulfuric acid collection device 10 for external transportation to realize the resource utilization of the sulfur-rich tail gas. Steam is discharged from the upper part of the flash separator 6 and condensed into water through the condenser 7, which can be circulated for water replenishment and flushing water for the entire system, thereby realizing zero wastewater discharge. This process makes full use of the waste heat of sulfur-rich tail gas, improves tail gas utilization, reduces investment and operating costs, and reduces energy consumption. The resource-based products have high added value and good market prospects. At the same time, it achieves zero wastewater and zero waste residue emissions to reduce secondary pollution.
[0065] The present invention will be described in detail below through examples, but the protection scope of the present invention is not limited thereto.
[0066] The experimental methods in the following examples, unless otherwise specified, are all conventional methods in the art. The experimental materials used in the following examples, unless otherwise specified, are all commercially available.
[0067] Example 1
[0068] Reference Figure 1 The system shown performs the operations of this embodiment.
[0069] In this embodiment, the contents (volume fractions) of the main components in the sulfur-rich tail gas are shown in Table 1 below.
[0070] Table 1
[0071] Serial number project Numeric 1 <![CDATA[SO2, %(dry)]]> ≤25.26 2 <![CDATA[SO3,%(dry)]]> ≤0.25 3 <![CDATA[NH3, %(dry)]]> ≤4.23 4 HCL, % (dry) ≤1.8 5 HF,%(dry) ≤0.12 6 <![CDATA[CO2, %(dry)]]> ≤6.28 7 <![CDATA[N2,% (dry)]]> ≥62.06 8 <![CDATA[H2O, %(wet)]]> 36.41
[0072] The sulfur-rich tail gas with a temperature of 300-400°C is firstly heat-exchanged with the circulating sulfuric acid solution through the tubular heat exchanger 5 to reduce the temperature of the sulfur-rich tail gas to about 100°C;
[0073] The sulfur-rich tail gas after cooling enters from the lower part of the spray absorption device 3 and flows upward. The lime water (mass concentration is 20%) from the lime water supply device 1 is sprayed from the spray layer arranged at the upper part of the spray absorption device 3. The sulfur-rich tail gas after cooling and the lime water are circulated and sprayed and countercurrently washed in the washing section 31 to obtain clean flue gas and a washing slurry located in the oxidation section 32. The oxidizing air from the oxidizing air source 2 is introduced into the washing slurry to force oxidation under the action of the oxidizing air.
[0074] The oxidized washing slurry is passed into the clarifier 4 for solid-liquid separation to obtain a supernatant and a solid filter residue CaSO4, wherein the CaSO4 precipitate (i.e., hydrated gypsum) is pumped into the coal yard or other subsequent resource treatment through the sludge pump 9, and the supernatant (dilute H2SO4) enters the negative pressure flash separator 6 for negative pressure flash evaporation to obtain steam and sulfuric acid solution. The sulfuric acid solution located at the lower part of the flash separator 6 is circulated between the heat exchanger 5 and the flash separator 6 via the circulation pump 8. After multiple cycles of heat exchange and flash evaporation, the solution at the bottom of the flash tank reaches a certain concentration and enters the concentrated sulfuric acid collection device 10; the steam obtained by flash evaporation in the flash separator 6 is passed into the condenser 7 to condense into water, which can be used for water replenishment and flushing water for the entire system to achieve system adaptive water balance.
[0075] According to the test, in this embodiment, the utilization rate of sulfur dioxide in the sulfur-rich tail gas is 95-99%;
[0076] The concentration of concentrated H2SO4 at the outlet of the flash separator 6 is 70-80wt%;
[0077] The solid content of the CaSO4 precipitate at the outlet of the clarifier 4 is 25wt%. If the finished gypsum is obtained after cyclone and vacuum dehydration treatment, its moisture content is ≤10wt%, which can be directly sold as a product.
[0078] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.
Claims
1. A system for resource utilization of sulfur-rich tail gas, characterized in that: The system comprises a limewater supply device (1), an oxidizing air source (2), a spray absorption device (3), a clarifier (4), a heat exchanger (5) and a flash separator (6), wherein the spray absorption device (3) is provided with a washing section (31) and an oxidation section (32) from top to bottom; The sulfur-rich tail gas is cooled in the heat exchanger (5), and the cooled sulfur-rich tail gas is reversely contacted with lime water from the lime water supply device (1) in the washing section (31) of the spray absorption device (3) to obtain clean flue gas and washing slurry. The washing slurry is oxidized by oxidation air from the oxidation air source (2) in the oxidation section (32). The oxidized washing slurry is subjected to solid-liquid separation in the clarifier (4), and the supernatant obtained by the solid-liquid separation is transported to the flash separator (6) for negative pressure flash evaporation. The sulfuric acid solution obtained at the lower part of the flash separator (6) is circulated into the heat exchanger (5) to exchange heat with the sulfur-rich tail gas in the heat exchanger (5), and then returned to the flash separator (6) for negative pressure flash evaporation.
2. The system according to claim 1, characterized in that The system further comprises a condenser (7), in which the steam from the flash separator (6) is condensed into water and then returned to the spray absorption device (3) or the lime water supply device (1) for utilization.
3. The system according to claim 1, characterized in that The sulfur-rich tail gas is activated coke regeneration gas.
4. The system according to claim 1, characterized in that The system further comprises a circulation pump (8) for circulating the sulfuric acid solution between the flash separator (6) and the heat exchanger (5).
5. The system according to claim 1, characterized in that The system further comprises a concentrated sulfuric acid collecting device (10) for collecting concentrated sulfuric acid from the flash separator (6).
6. A method for resource utilization of sulfur-rich tail gas, characterized in that: The method comprises the following steps: (1) The sulfur-rich tail gas is transported to a heat exchanger and cooled to 80-120°C; (2) transporting the cooled sulfur-rich tail gas and lime water to a spray absorption device for contact reaction to obtain a washing slurry and clean flue gas, and the washing slurry undergoes an oxidation reaction under the action of oxidizing air; (3) passing the oxidized washing slurry into a clarifier for solid-liquid separation to obtain a supernatant and a calcium sulfate precipitate; (4) The supernatant is passed into a flash separator for negative pressure flash evaporation to obtain steam and sulfuric acid solution, the sulfuric acid solution is circulated into the heat exchanger to exchange heat with the sulfur-rich tail gas in the heat exchanger, and then returned to the flash separator for negative pressure flash evaporation, and the cycle is repeated to obtain concentrated sulfuric acid and steam.
7. The method according to claim 6, characterized in that In step (1), the sulfur-rich tail gas is activated coke regeneration gas.
8. The method according to claim 6, characterized in that In step (1), the volume fraction of sulfur dioxide in the sulfur-rich tail gas is not higher than 30%.
9. The method according to claim 6, characterized in that The method further comprises: condensing the steam obtained in step (3), and using the water obtained by condensation to prepare the lime water in step (2).
10. The method according to claim 6, characterized in that In step (2), the concentration of calcium hydroxide in the lime water is 15-25wt%.
Citation Information
Patent Citations
Process and device for desulphurizing flue gas by lime-gypsum method
CN101703861A
Method and apparatus for removing sulfur dioxide from sulfuric acid industrial tail gas, and for recovering sulfuric acid
CN102228776A
Method and device for removing sulfur dioxide in industrially-sintered flue gas and recovering gypsum
CN102949923A
Apparatus for concentrating ammonium sulfate slurry by using flue gas enthalpy
CN106938146A
Device for preparing sulfuric acid by using discharged sulfur dioxide as raw material
CN204474329U