Laser welding method suitable for connection of magnesium alloy and medical titanium alloy heterogeneous metal wires

Through laser welding technology, the problem of difficulty in connecting magnesium/titanium heterogeneous wires is solved, the degradability and efficient connection of the anchor end of the vascular stent are achieved, the mechanical strength and corrosion resistance of the joint are improved, and the endovascular damage is solved risk.

CN118926678AActive Publication Date: 2024-11-12THE AFFILIATED CENT HOSPITAL OF DALIAN UNIV OF TECH (DALIAN CENT HOSPITAL) +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410982308.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-12
Estimated Expiration
2044-07-22

AI Technical Summary

Technical Problem

Welding between magnesium/titanium heterogeneous metal wires is difficult, especially when the material thickness is less than 1mm, the overlap gap is high, resulting in difficulty in connecting and unable to form an effective connection, which affects the degradation of the anchored end of the vascular stent and the endovascular membrane. protection.

Method used

Using laser welding method, pulsed laser and continuous laser are carried out simultaneously, combined with high-purity argon protection, diode continuous laser and Nd:YAG pulse laser are used to weld magnesium alloy and medical titanium alloy wire, and welding parameters such as current, Frequency, power and offset for efficient connection.

Benefits of technology

The stable connection between magnesium alloy and medical titanium alloy wire is achieved, providing the degradability of the anchor end of the vascular stent, reducing the risk of damage to the end of the vascular membrane, and improving the corrosion resistance and mechanical strength of the joint.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926678A_ABST
    Figure CN118926678A_ABST
Patent Text Reader

Abstract

The invention relates to the field of connection (welding) of heterogeneous materials, in particular to a laser welding method suitable for connection of magnesium alloy and medical titanium alloy heterogeneous metal wires. Pretightening force needs to be applied to the metal wire through a clamp, shielding gas needs to be introduced in the welding process, and metal is prevented from being oxidized. And the connection between the two heterogeneous metal wires is realized by changing related parameters of the laser. The welding joints are connected together through diffusion of elements, and the tensile strength of the welding joints can reach 62-74 MPa. The laser welding method is adopted, the lap joint mode is utilized, welding of the metal wires made of the heterogeneous materials is achieved, and a feasible scheme is provided for solving the problem that the front end of the intravascular stent is degradable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of connection (welding) of heterogeneous materials, and in particular relates to a laser welding method suitable for connecting heterogeneous metal wires of magnesium alloy and medical titanium alloy. Background Art

[0002] Aortic dissection is caused by a rupture in the aortic intima, through which blood enters the middle layer of the aortic wall, forming a dissection hematoma, which gradually extends and peels off the intima and middle layer of the aorta. Currently, the main treatment for aortic dissection is endovascular repair, which effectively reduces the pressure on the blood vessel wall and reduces the risk of aortic rupture by inserting a covered stent at the lesion and sealing the primary rupture of the dissection.

[0003] The medical device used in aortic endovascular repair is usually a covered stent, which is fixed to the lesion site by an anchoring device at the front end. Usually, the anchoring device is 10-20% larger than the diameter of the aorta. After endothelialization, the fixing effect of the anchoring device at the front end of the stent disappears, but the pressure of the larger diameter on the inner wall of the blood vessel will cause damage to the vascular endothelium and cause new ruptures. Therefore, a covered stent with a degradable anchoring device is developed. Compared with the traditional covered stent, the anchoring end of the stent can be degraded after endothelialization, which can effectively reduce the damage of the front fixing component to the inner wall of the blood vessel, and reduce the damage and long-term risks of the anchoring end of the permanently implanted stent to the human blood vessels.

[0004] In clinical practice, covered stents are usually woven from medical titanium alloy wires. In order to achieve endothelialization and degradation of the stent anchoring end, a section of biodegradable metal material can be connected to the front end of the medical titanium alloy wire, which will serve as the anchoring end. Magnesium alloy is selected as this biodegradable metal material because of its excellent biocompatibility and its rapid endothelialization and low thrombogenicity when used as a vascular stent material.

[0005] Compared with traditional methods such as adhesive connection and mechanical connection, laser welding can provide better joint corrosion resistance and mechanical strength. However, due to the large differences in the physical, chemical and metallurgical properties of magnesium and titanium, the welding of magnesium and titanium heterogeneous metals is difficult. There is currently no research on the welding of magnesium and titanium heterogeneous metal wires, and all research is on the welding between magnesium and titanium heterogeneous metal plates. Compared with the welding of plate brackets, the welding between metal wires has very high requirements on the lap gap tolerance. When the thickness of the connected material is less than 1mm, the gap between the connected materials cannot exceed 10% of the thickness of the thinnest material, otherwise the connection will not be formed.

[0006] Therefore, in order to develop a degradable stent graft with a front anchoring device, a laser welding method suitable for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires is proposed. Summary of the invention

[0007] The purpose of the present invention is to provide a laser welding method suitable for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires. The method is used to make a partially degradable stent braided wire, which can be braided into a vascular stent with a degradable anchor end to solve the problems raised in the above background.

[0008] To achieve the above object, the present invention provides the following technical solutions:

[0009] A laser welding method for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires, comprising the following steps:

[0010] Step 1: Grind the magnesium alloy wire with sandpaper to remove the surface oxide, and use acetone to clean and remove the surface grease; soak the medical titanium alloy wire in acid to remove the surface oxide layer, and use acetone to clean and remove the surface grease.

[0011] Step 2: Process the clamp for clamping the metal wire by wire cutting.

[0012] Step 3: The joint of the magnesium alloy wire and the titanium alloy wire is in the form of overlap, and the two wires are fixed by a clamp. The clamp can adjust the overlap gap of the two wires by applying a clamping force.

[0013] Step 4: Welding is performed simultaneously using pulse laser and continuous laser. The current of the pulse laser is 65-85A, the defocus amount is 130-180mm, the welding speed is 2.8-3.0m / min, the power is 30-50W, and the frequency is 30-50Hz; the power of the continuous laser is 20-60W, and both the pulse laser and the continuous laser are offset to one side of the magnesium alloy wire by 0.1-0.3mm.

[0014] Furthermore, high-purity argon gas is used to protect the welding area during the welding process, and a diode continuous laser and a Nd:YAG pulse laser are used to weld the two heterogeneous metal wires.

[0015] Furthermore, the chemical composition and mass percentage of the magnesium alloy are Y: 3-4.1%, Re: 3-4%, Zr: 0.3-1%, and the rest is Mg.

[0016] Furthermore, the titanium alloy is a medical titanium alloy, and its chemical composition and mass percentage are Ni: 50-60%, Zr: 0.1-1%, Nb: 0.1-0.5%, and the rest is Ti.

[0017] Furthermore, the wavelength of the continuous laser is 980 nm.

[0018] Furthermore, the wavelength of the pulse laser is 1064 nm.

[0019] Furthermore, during the welding process, pulse laser and continuous laser are performed simultaneously.

[0020] The beneficial effects of the present invention are as follows: the welding of two heterogeneous metal wires is achieved by laser welding, which provides a feasible solution to the problem of the degradability of the front end of the vascular stent. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a welding schematic diagram;

[0022] Figure 2 is a schematic diagram of the fixture;

[0023] Figure 3 It is the microstructure of the weld;

[0024] Figure 4 is the element distribution in the weld.

[0025] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the present invention will be described with reference to specific embodiments below. It should be noted that these embodiments are merely descriptive and do not limit the present invention in any way. DETAILED DESCRIPTION

[0026] The following will be combined with the accompanying drawings in the embodiments of the present invention to fully and clearly describe the technical solutions in the embodiments of the present invention. The described embodiments are only part of the embodiments of the present invention, not all of the embodiments.

[0027] Example 1

[0028] First, the surfaces of magnesium alloy wire (Y: 4.05%, Re: 3%, Zr: 0.52%, and the rest is Mg) and medical titanium alloy wire (Ni: 56.3%, Nb: 0.5%, Zr: 0.47%, and the rest is Ti) were cleaned: the magnesium alloy wire was polished with sandpaper to remove the surface oxide, and the surface grease was removed by washing with acetone; the medical titanium alloy wire was immersed in acid to remove the surface oxide layer, and the surface grease was removed by washing with acetone.

[0029] Then, the clamp for clamping the wire is processed by wire cutting. The joint of the magnesium alloy wire and the titanium alloy wire is in the form of overlap, and the two wires are fixed by a clamp. The clamp is used to apply a pre-tightening force to the wire, and the welding is carried out by pulse laser and continuous laser at the same time. High-purity argon gas is used to protect the welding area during welding. The two heterogeneous metal wires are welded by diode continuous laser and Nd:YAG pulse laser. When the current of the pulse laser is 70A, the magnesium alloy wire and the medical titanium alloy wire with a diameter of 0.5mm are welded. At the same time, the frequency of the pulse laser is 30Hz, the continuous laser power is 40W, the power of the pulse laser is 32W, the welding speed of the pulse laser is 2.8m / min, the defocus of the pulse laser is 145mm, and the pulse laser and the continuous laser are both offset by 0.2mm to one side of the magnesium alloy wire. The wavelength of the continuous laser is 980nm, and the wavelength of the pulse laser is 1064nm. The obtained wire welding material can be used to obtain a heterogeneous alloy joint with a tensile strength of 62.47 MPa (tensile test conditions: at room temperature, a tensile testing machine is used to perform a mechanical property test at a tensile speed of 1 mm / min).

[0030] Example 2

[0031] First, the surfaces of magnesium alloy wire (Y: 4.05%, Re: 3%, Zr: 0.52%, and the rest is Mg) and medical titanium alloy wire (Ni: 56.3%, Nb: 0.5%, Zr: 0.47%, and the rest is Ti) were cleaned: the magnesium alloy wire was polished with sandpaper to remove the surface oxide, and the surface grease was removed by washing with acetone; the medical titanium alloy wire was immersed in acid to remove the surface oxide layer, and the surface grease was removed by washing with acetone.

[0032] Then, a clamp for clamping the metal wire is processed by wire cutting. The joints of the magnesium alloy wire and the titanium alloy wire are in the form of overlap, and the two wires are fixed with a clamp. A pre-tightening force is applied to the metal wire with a clamp, and welding is performed by using pulsed laser and continuous laser simultaneously. High-purity argon gas is used to protect the welding area during the welding process. A diode continuous laser and a Nd:YAG pulse laser are used to weld the two heterogeneous metal wires. When the frequency of the pulse laser is 40Hz, the magnesium alloy wire and the medical titanium alloy wire with a diameter of 0.5mm are welded. At the same time, the current of the pulse laser is 70A, and the other welding parameters are the same as in Example 1. The obtained wire welding material can be used to obtain a heterogeneous alloy joint with a tensile strength of 68.72MPa (the tensile test conditions are the same as in Example 1)

[0033] Example 3

[0034] First, the surfaces of magnesium alloy wire (Y: 4.05%, Re: 3%, Zr: 0.52%, and the rest is Mg) and medical titanium alloy wire (Ni: 56.3%, Nb: 0.5%, Zr: 0.47%, and the rest is Ti) were cleaned: the magnesium alloy wire was polished with sandpaper to remove the surface oxide, and the surface grease was removed by washing with acetone; the medical titanium alloy wire was immersed in acid to remove the surface oxide layer, and the surface grease was removed by washing with acetone.

[0035] Then, the clamp for clamping the metal wire is processed by wire cutting. The joint of the magnesium alloy wire and the titanium alloy wire is in the form of overlap, and the two wires are fixed by a clamp. A pre-tightening force is applied to the metal wire by the clamp, and welding is carried out by pulse laser and continuous laser simultaneously. High-purity argon gas is used to protect the welding area during the welding process. A diode continuous laser and a Nd:YAG pulse laser are used to weld the two heterogeneous metal wires. When the current of the pulse laser is 75A, the magnesium alloy wire and the medical titanium alloy wire with a diameter of 0.5mm are welded. At the same time, the frequency of the pulse laser is 40Hz, and the other welding parameters are the same as in Example 1. The obtained wire welding material can be used to obtain a heterogeneous alloy joint with a tensile strength of 72.68MPa (the tensile test conditions are the same as in Example 1).

[0036] Example 3 Microstructure Figure 3 The element distribution is shown in Figure 4 As shown by Figure 4 It can be seen that the two heterogeneous metals are connected through element diffusion.

[0037] Although the embodiments of the present invention have been described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.

Claims

1. A laser welding method suitable for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires, characterized in that: The following steps are involved: Step 1: Grind the magnesium alloy wire with sandpaper to remove the oxide on the surface, and use acetone to remove the grease on the surface; soak the medical titanium alloy wire in acid to remove the oxide layer on the surface, and use acetone to remove the grease on the surface; Step 2: Process the fixture for clamping the metal wire by wire cutting; Step 3: The joint of the magnesium alloy wire and the titanium alloy wire is in the form of overlap, and the two wires are fixed by a clamp; the clamp can adjust the overlap gap of the two wires by applying a clamping force; Step 4: Welding is performed simultaneously using pulse laser and continuous laser. The current of the pulse laser is 65-85A, the defocus amount is 130-180mm, the welding speed is 2.8-3.0m / min, the power is 30-50W, and the frequency is 30-50Hz; the power of the continuous laser is 20-60W, and both the pulse laser and the continuous laser are offset to one side of the magnesium alloy wire by 0.1-0.3mm.

2. A laser welding method suitable for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires according to claim 1, characterized in that: During the welding process, high-purity argon gas is used to protect the welding area, and diode continuous laser and Nd:YAG pulse laser are used to weld two heterogeneous metal wires.

3. The laser welding method for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires according to claim 1, characterized in that: The chemical composition and mass percentage of the magnesium alloy are Y: 3-4.1%, Re: 3-4%, Zr: 0.3-1%, and the rest is Mg.

4. The laser welding method for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires according to claim 1, characterized in that: The titanium alloy is a medical titanium alloy, and its chemical composition and mass percentage are Ni: 50-60%, Zr: 0.1-1%, Nb: 0.1-0.5%, and the rest is Ti.

5. The laser welding method for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires according to claim 1, characterized in that: The wavelength of the continuous laser is 980 nm.

6. The laser welding method for connecting magnesium alloy and medical titanium alloy heterogeneous metal wires according to claim 1, characterized in that: The wavelength of the pulse laser is 1064 nm.

Citation Information

Patent Citations

  • Laser offset welding method suitable for magnesium / steel and magnesium / titanium

    CN102091872A

  • Interface reaction regulation method for dissimilar material welding through bifocus laser beam

    CN105215550A

  • Magnesium / titanium laser melting braze welding method assisted by nickel-plated layer

    CN106270878A

  • Lap welding method for magnesium / steel dissimilar metal automobile door

    CN116197537A

  • Heterogeneous joint welding system and welding method based on uniform temperature field

    CN116551174A