Technological method for forming environment-friendly high-strength composite tray through one-time compression molding
Through the primary molding process and material ratio optimization, the problems of pallet deformation and low strength are solved, and high-strength, continuous use and cost-saving environmentally friendly composite pallets are achieved, suitable for pallet molding and transportation.
Patent Information
- Application Number
- CN202410937621.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-12
AI Technical Summary
The existing pallets are prone to deform during use and cannot achieve overall movement, resulting in poor separation and use effects. Due to separate molding, fiber reinforcement cannot be effectively increased, and the strength is low, resulting in disposable products and high usage costs.
By adopting a one-time molding process, the LFT mixed mass is grasped by a robot and glued it to the heated PP prepreg belt and entered the mold. During the press mold clamping process, the PP prepreg belt softens and the LFT mixed mass flows, forming The curved structure improves the strength of the pallet and achieves integrated molding through the material ratio of 20%-30% phenolic resin, 40% fiber, 40% polypropylene resin, and 15% glass fiber reinforcement.
It improves the strength and integrity of the pallet, realizes the continuous use of the pallet, reduces the cost of use, and uses lightweight high-strength basalt fibers and composite particles through the LFTD production line, simplifies the process, enhances the load-bearing capacity, and saves storage and transportation space.
Smart Images

Figure CN118927664A_ABST
Abstract
Description
Technical Field
[0001] The present invention specifically relates to the technical field of composite material pallet processing, and specifically to a process method for one-time compression molding of an environmentally friendly high-strength composite material pallet. Background Art
[0002] A pallet is a horizontal platform device used for packaging, stacking, handling and transporting goods and products as a unit load. As a kind of packaging equipment similar to containers, pallets are now widely used in production, transportation, warehousing and circulation. Pallets are important loading, unloading, storage and transportation equipment in the process of logistics operations. They play a huge role in modern logistics when used with forklifts. At present, pallets can be divided into five types according to material classification: wooden pallets, steel pallets, plastic pallets, composite material pallets and paper pallets. At present, most pallets are PP injection molded, which are molded separately by compression molding and welding. This cannot effectively increase fiber reinforcement and has low strength. This will cause the pallet to deform during use and cannot effectively achieve continuous use of the pallet. This makes the pallet a disposable product, resulting in increased use costs. After searching, Chinese patent publication number CN202123216687.7 discloses an anti-deformation injection molded pallet cover; comprising a cover body and a card body, the card body is connected to the cover body, the cover body is provided with a plurality of grooves and a plurality of mounting grooves, a tensioner buckle is provided in the mounting groove, and a clamping rib is provided on the peripheral side of the card body; Although the tray in the above patent can achieve the effect of supporting the load, it is not integrally formed, so the tray cannot be effectively moved as a whole during use. In this way, the tray may be separated during use, and the effect of use cannot be effectively guaranteed; Therefore, we provide a process method for one-time compression molding of environmentally friendly high-strength composite material pallets; after the robot withdraws, the press closes the mold and performs compression molding. The PP prepreg is not easy to flow due to the long glass fiber length, while the LFT mixed agglomerate flows to fill the entire cavity. Since the LFT mixed agglomerate was previously adhered to the top of the PP prepreg, a portion of the LFT mixed agglomerate will be retained on the top of the PP prepreg, and a portion will also be retained below it. In this way, the PP prepreg is basically placed in the middle of the pallet. The rapid downward pressure of the press, due to the softening of the PP prepreg and the time required for the flow of the LFT mixed agglomerate, during the process of the press closing the mold, the PP prepreg will not be horizontally regular in the pallet, but will have a certain curve. This structural form, on the contrary, further improves the strength of the entire pallet; after the pallet is cooled and formed, a thermoplastic composite material pallet is obtained. Summary of the invention
[0003] The purpose of the present invention is to provide a process for molding an environmentally friendly high-strength composite material pallet by one-time compression molding. Since the LFT mixed agglomerate material is previously adhered to the top of the PP prepreg tape, a portion of the LFT mixed agglomerate material will be retained on the top of the PP prepreg tape, and a portion will also be retained below it. In this way, the PP prepreg tape is basically placed in the middle of the pallet. The rapid downward pressure of the press, due to the softening of the PP prepreg tape and the time required for the flow of the LFT mixed agglomerate material, during the process of the press closing the mold, the PP prepreg tape will not be horizontal and regular in the pallet, but will have a certain curve. Such a structural form, on the contrary, further improves the strength of the entire pallet. After the pallet is cooled and formed, a thermoplastic composite material pallet is obtained; to solve the problems raised in the above background technology.
[0004] To achieve the above object, the present invention provides the following technical solutions: The environmentally friendly high-strength composite material pallet is molded in one step, and the pallet includes a base and a carrier plate; the pallet is set in an integrated manner; it is composed of 20%-30% phenolic resin, 40% fiber, 40% polypropylene resin, 15% glass fiber reinforcement, and 5% additives; Preferably, the additive is one or more of a curing agent, a release agent, and a pigment. Preferably, after the headlight is placed on the fixing frame through the protective gear, the headlight is transferred through the moving assembly to place the headlight inside the detection assembly; Preferably, the fiber is one of wood fiber or bamboo fiber; Preferably, the phenolic resin is one or more of phenol, cresol, formaldehyde and acetaldehyde; Preferably, the preparation process of the glass fiber reinforcement comprises the following steps: Step 1: Mix 50% - 60% silicon dioxide, 10% - 25% aluminum oxide, 1% - 10% magnesium oxide and 5% - 10% boron oxide; Step 2: In order to improve the performance and processing properties of glass fiber, a small amount of metal oxides and fluorides may also be added; Step 3: Mixing the mixed glass fiber reinforcement with phenolic resin and polypropylene resin; Step 4: Mixing the glass fiber reinforcement with the phenolic resin and the fiber; Mixing the glass fiber reinforcement with the polypropylene resin and the fiber; Step 5: After the mixing is completed, the LFT mixed mass is grabbed by a robot and moved downward. After being attached with the heated PP prepreg tape, the chain quickly exits the mold. Preferably, the manipulator places the LFT mass and prepreg tape in the mold cavity within 5 seconds; the heating in the mold cavity is 500°C-800°C; Preferably, the reaction temperature in step 1 is 60°-75°; the reaction temperature in step 2 is 80°-120°; Preferably, the process for one-time compression molding of an environmentally friendly high-strength composite material pallet comprises the following steps: Step 1: Use the robot to grab the LFT mixed mass and move it down. After sticking it to the heated PP prepreg tape, the chain quickly withdraws from the top of the mold; Step 2: The heat-insulating LFT mixed mass can provide heat to the PP prepreg and quickly enter the mold. Under the wrapping of the mold, the heat loss can be further reduced. Step 3: After the robot withdraws, the press closes the mold and presses it into shape. The PP prepreg is not easy to flow due to the long length of the glass fiber, while the LFT mixed mass flows and fills the entire cavity; Step 4: The press machine is pressed down quickly. Due to the softening of the PP prepreg tape and the time required for the LFT mixed mass material to flow, the PP prepreg tape has a certain curve in the tray mold during the press mold closing process; Step 5: After the tray is cooled and formed, a thermoplastic composite tray is obtained; Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention optimizes the ratio of the pallet material. During the process of the press mold closing, the PP prepreg tape will not be horizontal and regular in the pallet, but will have a certain curve. Such a structural form further improves the strength of the entire pallet. After the pallet is cooled and formed, a thermoplastic composite material pallet is obtained. 2. The composite material pallet of the present invention is molded once using the LFTD production line, and uses lightweight and high-strength basalt fiber and composite material particles, which are melted and mixed by special equipment to form an integrated structure; this pallet is easy to form, has a simple process, and has a strong load-bearing capacity. The greater advantage of this structural design and molding is that it can fully utilize the granular and sheet-shaped finished products of thermoplastic composite materials as well as the scraps of corners, machine heads, etc. for processing; it can be stacked for storage and transportation, saving storage and transportation space. BRIEF DESCRIPTION OF THE DRAWINGS
[0005] Figure 1 It is a schematic diagram of the three-dimensional structure of the present invention.
[0006] Figure 2 For the present invention Figure 1 Top view of the .
[0007] Figure 3 for Figure 1 Side view of.
[0008] In the figure: 1-support beam, 2-carrier plate. DETAILED DESCRIPTION
[0009] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0010] See also Figure 1-3 In the embodiment of the present invention, an environmentally friendly high-strength composite material pallet is molded in one step, and the pallet includes a base and a carrier plate; the pallet is arranged in an integrated manner; it is composed of 20%-30% phenolic resin, 40% fiber, 40% polypropylene resin, 15% glass fiber reinforcement, and 5% additives; Specifically, the additive is one or more of a curing agent, a release agent, and a pigment; Preferred; the fiber is one of wood fiber or bamboo fiber The phenolic resin is one or more of phenol, cresol, formaldehyde and acetaldehyde; By adopting the above technical solution and optimizing the ratio of the pallet material, during the process of the press mold closing, the PP prepreg tape will not be horizontal and regular in the pallet, but will have a certain curve. This structural form will further improve the strength of the entire pallet. After the pallet is cooled and formed, a thermoplastic composite material pallet is obtained; Furthermore, the preparation process of the glass fiber reinforcement comprises the following steps: Step 1: Mix 50% - 60% silicon dioxide, 10% - 25% aluminum oxide, 1% - 10% magnesium oxide and 5% - 10% boron oxide; Step 2: In order to improve the performance and processing properties of glass fiber, a small amount of metal oxides and fluorides may also be added; Step 3: Mixing the mixed glass fiber reinforcement with phenolic resin and polypropylene resin; Step 4: Mixing the glass fiber reinforcement with the phenolic resin and the fiber; Mixing the glass fiber reinforcement with the polypropylene resin and the fiber; Step 5: After the mixing is completed, the LFT mixed mass is grabbed by a robot and moved downward. After being attached with the heated PP prepreg tape, the chain quickly exits the mold. The manipulator places the LFT mass and prepreg tape in the mold cavity within 5 seconds; the heating in the mold cavity is 500°C-800°C; The reaction temperature in step 1 is 60°-75°; the reaction temperature in step 2 is 80°-120°; The process for molding an environmentally friendly high-strength composite material pallet in one-step molding comprises the following steps: Step 1: Use the robot to grab the LFT mixed mass and move it down. After sticking it to the heated PP prepreg tape, the chain quickly withdraws from the top of the mold; Step 2: The heat-insulating LFT mixed mass can provide heat to the PP prepreg and quickly enter the mold. Under the wrapping of the mold, the heat loss can be further reduced. Step 3: After the robot withdraws, the press closes the mold and presses it into shape. The PP prepreg is not easy to flow due to the long length of the glass fiber, while the LFT mixed mass flows and fills the entire cavity; Step 4: The press machine is pressed down quickly. Due to the softening of the PP prepreg tape and the time required for the LFT mixed mass material to flow, the PP prepreg tape has a certain curve in the tray mold during the press mold closing process; Step 5: After the tray is cooled and formed, a thermoplastic composite tray is obtained; By adopting the above technical solution, the composite material pallet is molded in one step using the LFTD production line, using lightweight and high-strength basalt fiber and composite material particles, which are melted and mixed by special equipment to form an integrated structure. This pallet is easy to form, has a simple process, and has a strong load-bearing capacity. The greater advantage of this structural design and molding is that it can make full use of thermoplastic composite granular and sheet products as well as corners, machine heads and other scraps for processing. Its specific structure can be stacked for storage and transportation, saving storage and transportation space.
[0011] The working principle of the present invention is: a robot is used to grab the LFT mixed mass material and move it downward, and after it is glued to the heated PP prepreg tape, the chain quickly withdraws from the top of the mold; the robot places the LFT mass material and the prepreg tape in the mold cavity within 5 seconds, so that the insulated LFT mixed mass material can provide heat to the PP prepreg tape and quickly enter the mold. Under the wrapping of the mold, the heat loss can also be further reduced.
[0012] After the robot withdraws, the press closes the mold and performs compression molding. The PP prepreg is not easy to flow due to the long glass fiber length, while the LFT mixed agglomerate flows to fill the entire cavity. Since the LFT mixed agglomerate was previously attached to the top of the PP prepreg, a portion of the LFT mixed agglomerate will be retained on the top of the PP prepreg, and a portion will also be retained below it. In this way, the PP prepreg is basically placed in the middle of the tray. The rapid downward pressure of the press, due to the softening of the PP prepreg and the time required for the LFT mixed agglomerate to flow, during the process of the press closing the mold, the PP prepreg will not be horizontal and regular in the tray, but will have a certain curve. This structural form, on the contrary, further improves the strength of the entire tray. After the tray is cooled and formed, a thermoplastic composite tray is obtained; It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.
[0013] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. One-time compression molding of environmentally friendly high-strength composite material pallets, characterized by The pallet includes a base and a carrier plate; the pallet is arranged in an integrated manner; it is composed of 20%-30% phenolic resin, 40% fiber, 40% polypropylene resin, 15% glass fiber reinforcement, and 5% additives.
2. The process for forming an environmentally friendly high-strength composite material pallet by one-step compression molding according to claim 1 is characterized in that: The additive is one or more of a curing agent, a release agent and a pigment.
3. The process for forming an environmentally friendly high-strength composite material pallet by one-step compression molding according to claim 1 is characterized in that: The fiber is one of wood fiber or bamboo fiber.
4. The process for forming an environmentally friendly high-strength composite material pallet by one-step compression molding according to claim 1 is characterized in that: The phenolic resin is one or more of phenol, cresol, formaldehyde and acetaldehyde.
5. The one-time compression molded environmentally friendly high-strength composite material pallet according to claim 4; characterized in that: The preparation process of the glass fiber reinforcement comprises the following steps: Step 1: Use 50% - 60% silicon dioxide, 10% - 25% aluminum oxide, 1% - 10% magnesium oxide and 5% - 10% boron oxide to mix; Step 2: In order to improve the performance and processing properties of glass fiber, a small amount of metal oxides and fluorides may also be added; Step 3: Mixing the mixed glass fiber reinforcement with phenolic resin and polypropylene resin; Step 4: Mixing the glass fiber reinforcement with the phenolic resin and the fiber; Mixing the glass fiber reinforcement with the polypropylene resin and the fiber; Step 5: After the mixing is completed, the LFT mixed mass is grabbed by a robot and moved downward. After being attached with the heated PP prepreg tape, the chain quickly withdraws from the top of the mold.
6. The one-time compression molded environmentally friendly high-strength composite material pallet according to claim 2; characterized in that: The robot places the LFT mass and prepreg tape in the mold cavity within 5 seconds; the heating in the mold cavity is 500°C-800°C.
7. The one-time compression molded environmentally friendly high-strength composite material pallet according to claim 6; characterized in that: The reaction temperature in step 1 is 60°-75°; the reaction temperature in step 2 is 80°-120°.
8. The process for forming an environmentally friendly high-strength composite material pallet by one-time compression molding according to any one of claims 1 to 7, characterized in that: The following steps are involved: Step 1: Use the robot to grab the LFT mixed mass and move it down. After sticking it to the heated PP prepreg tape, the chain quickly withdraws from the top of the mold; Step 2: The heat-insulating LFT mixed mass can provide heat to the PP prepreg and quickly enter the mold. Under the wrapping of the mold, the heat loss can be further reduced. Step 3: After the robot withdraws, the press closes the mold and presses it into shape. The PP prepreg is not easy to flow due to the long length of the glass fiber, while the LFT mixed mass flows and fills the entire cavity; Step 4: The press machine is pressed down quickly. Due to the softening of the PP prepreg tape and the time required for the LFT mixed mass material to flow, the PP prepreg tape has a certain curve in the tray mold during the press mold closing process; Step 5: After the tray is cooled and formed, a thermoplastic composite tray is obtained.
Citation Information
Patent Citations
Anti-deformation injection molding tray cover
CN217533834U