Fine processing method for firing talcum powder by using rotary kiln

Through the refined processing method of talc powder fired by rotary kiln, the problems of low efficiency and uneven quality of traditional talc powder processing methods are solved, and the efficient production of talc powder with uniform particle size and high purity is achieved, which is suitable for a variety of industrial applications.

CN118929680APending Publication Date: 2024-11-12LIAONING SANSHAN ENERGY SAVING NEW MATERIALS CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411003366.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Traditional talc processing methods are inefficient and uneven product quality.

Method used

The refined processing method of rotary kiln firing talc powder is used, including raw material preparation, water pressure balling, rotary kiln sintering and fine-graining steps. By controlling the ratio, temperature and time of raw materials, efficient production of talc powder is achieved.

Benefits of technology

It improves the production efficiency and product quality of talc powder, has uniform particle size and high purity, and is suitable for a variety of industrial applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a fine processing method for firing talcum powder by using a rotary kiln, which comprises the following steps: step 1) raw material preparation: taking two raw materials according to the mass ratio of talc to silica being 2: 1, mixing, grinding into powder, and sieving with a 200-mesh sieve to obtain fine powder for later use; (2) adding water to press balls, namely taking the fine powder, adding a proper amount of water to enable the humidity of the fine powder to reach a state suitable for ball pressing, and pressing the wet fine powder into balls at the temperature of 50 DEG C; (3) sintering in a rotary kiln: feeding the pressed spherical material into the rotary kiln for sintering, and enabling the spherical material to be subjected to chemical reaction at high temperature, so as to obtain a talcum powder sintered body; and 4) fine crushing: performing fine crushing on the obtained talcum powder sintered body, and sieving with a 200-mesh sieve to obtain a finished product. According to the fine processing method of the talcum powder, the production efficiency and the product quality of the talcum powder are effectively improved, and the obtained talcum powder is uniform in particle size, high in purity and suitable for various industrial applications.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a processing technology for non-metallic minerals, in particular to a fine processing method for sintering talc powder using a rotary kiln. Background Art

[0002] Talc is a white, soft, hydrophobic mineral that belongs to the magnesium silicate structure containing crystal water. It consists of three layers: two silicon-containing layers sandwiched between a magnesium oxide layer or a magnesium hydroxide layer;

[0003] The three-layer structure of talc crystals is in a perfect electrical balance, which makes it carry little or no charge. The lack of charge makes talc a non-polar or hydrophobic mineral, which allows it to better adsorb on other hydrophobic substances such as adhesives and resins. Therefore, talc is widely used as a resin and adhesive control agent.

[0004] As an important industrial raw material, talc is widely used in many fields. However, traditional talc processing methods usually include mining, crushing, grinding, screening and packaging, but often have problems of low efficiency and uneven product quality. Summary of the invention

[0005] The technical problem to be solved by the present invention is to overcome the defects of the above-mentioned technology and provide a refined processing method for sintering talc powder by using a rotary kiln.

[0006] In order to solve the above technical problems, the technical solution provided by the present invention is a fine processing method of talcum powder fired by a rotary kiln, comprising the following steps:

[0007] Step 1) Raw material preparation: according to the mass ratio of talc to silica being 2:1, take the two raw materials, mix them and grind them into powder, pass through a 200-mesh sieve to obtain fine powder for later use;

[0008] Step 2) adding water to press balls: take the fine powder and add an appropriate amount of water to make the moisture of the fine powder reach a state suitable for pressing balls, and press the wet fine powder into balls at a temperature of 50°C;

[0009] Step 3) Rotary kiln sintering: The pressed spherical material is sent into a rotary kiln for sintering, so that the spherical material undergoes a chemical reaction at high temperature to obtain a talc sintered body;

[0010] Step 4) Fine grinding: The obtained talc powder sintered body is finely ground and passed through a 200-mesh sieve to obtain a finished product.

[0011] Furthermore, the specific operation of grinding into powder in step 1 is to first use a jaw crusher to crush the stone into smaller pieces, then use a cone crusher to crush it again, and finally send it to a Raymond mill for grinding.

[0012] Furthermore, the weight ratio of the amount of water added in step 2 to the fine powder is 3-7:1; and the humidity of the fine powder is 40-70%.

[0013] Furthermore, in step 3, the temperature of the rotary kiln is 1000-1150° C., and the sintering time is 1-2 hours.

[0014] The present invention also provides talcum powder prepared by the above-mentioned fine processing method.

[0015] The advantages of the present invention over the prior art are as follows: the refined processing method of talcum powder provided by the present invention effectively improves the production efficiency and product quality of talcum powder by accurately controlling key parameters such as raw material ratio, processing temperature and time, and the prepared talcum powder has uniform particle size and high purity and is suitable for a variety of industrial applications. DETAILED DESCRIPTION

[0016] The following is a further detailed description of the refined processing method of talc powder fired in a rotary kiln according to the present invention in conjunction with the embodiments.

[0017] Example 1

[0018] A fine processing method for talcum powder fired by a rotary kiln comprises the following steps:

[0019] Step 1) Raw material preparation: Take talc and silica in a mass ratio of 2:1, first use a jaw crusher to crush the raw stone into small pieces, then use a cone crusher to crush, and finally use a Raymond mill to grind, pass through a 200-mesh sieve, and obtain fine powder for standby use;

[0020] Step 2) adding water to press balls: according to the ratio of the amount of water added to the weight of the fine powder being 5:1, take 100 kg of fine powder and add 50 kg, mix well, and press into balls using a ball press at 50°C;

[0021] Step 3) Rotary kiln sintering: The pressed spherical material is fed into a rotary kiln and sintered at 1100° C. for 1.5 hours to obtain a talc sintered body;

[0022] Step 4) Fine grinding: The sintered body is finely ground and passed through a 200-mesh sieve again to obtain finished talcum powder.

[0023] The talcum powder obtained in Example 1 was tested for whiteness, silicon dioxide, manganese oxide, calcium oxide, ferric oxide, and aluminum oxide content, and compared with the index data of the first-class product in the industry index, as shown in the table below:

[0024] Test items 200 mesh talcum powder First-class product quality indicators Whiteness(%) 95.7 ≥94 <![CDATA[SiO2(%)]]> 62.5 ≥60 CaO(%) 0.35 ≤0.5 <![CDATA[Fe2O3(%)]]> 0.21 ≤0.3 <![CDATA[Al2O3(%)]]> 0.33 ≤0.4 MgO(%) 33.5 ≥30

[0025] The refined processing method of talcum powder provided by the present invention effectively improves the production efficiency and product quality of talcum powder by accurately controlling key parameters such as raw material ratio, processing temperature and time. The prepared talcum powder has uniform particle size and high purity and is suitable for various industrial applications.

[0026] The present invention and its implementation methods are described above, and such description is not restrictive. In short, if ordinary technicians in the field are inspired by it, without departing from the purpose of the invention, they can design structures and embodiments similar to the technical solution without creativity, which should all fall within the protection scope of the present invention.

Claims

1. A fine processing method for talcum powder using a rotary kiln, characterized in that: The following steps are involved: Step 1) Raw material preparation: according to the mass ratio of talc to silica being 2:1, take the two raw materials, mix them and grind them into powder, pass through a 200-mesh sieve to obtain fine powder for later use; Step 2) adding water to press balls: take the fine powder and add an appropriate amount of water to make the moisture of the fine powder reach a state suitable for pressing balls, and press the wet fine powder into balls at a temperature of 50°C; Step 3) Rotary kiln sintering: The pressed spherical material is sent into a rotary kiln for sintering, so that the spherical material undergoes a chemical reaction at high temperature to obtain a talc sintered body; Step 4) Fine grinding: The obtained talc powder sintered body is finely ground and passed through a 200-mesh sieve to obtain a finished product.

2. The method for finely processing talc powder by using a rotary kiln to burn according to claim 1, characterized in that: The specific operation of grinding into powder in step 1 is to first use a jaw crusher to break the stone into smaller pieces, then use a cone crusher to crush it again, and finally send it to a Raymond mill for grinding.

3. The fine processing method of talc powder fired by a rotary kiln according to claim 1, characterized in that: The weight ratio of the amount of water added in step 2 to the fine powder is 3-7:1; the humidity of the fine powder is 40-70%.

4. The fine processing method of talc powder fired by a rotary kiln according to claim 1, characterized in that: In step 3, the temperature of the rotary kiln is 1000-1150° C., and the sintering time is 1-2 hours.

5. A talcum powder prepared by the fine processing method according to any one of claims 1 to 4.

Citation Information

Patent Citations

  • Preparation method for low-cost and high-whiteness calcined talcum

    CN109279615A

  • Preparation method of low-cost high-whiteness calcined talc

    CN112408967A

  • High temperature wear-resistant ceramic glaze, high temperature wear-resistant ceramic coating layer preform, manufacturing method and use thereof

    JP2022184544A

  • Preparation method for low-cost and high-whiteness calcined talc

    WO2020082528A1