Method for removing COD (Chemical Oxygen Demand) from lead-zinc oxide ore flotation wastewater
Through the combined treatment of hydraulic cavitation and biological agents, the problem of removing high-salt and high-COD lead-zinc ore flotation wastewater is solved, deep purification and efficient reuse of wastewater are achieved, and treatment costs and environmental impacts are reduced.
Patent Information
- Application Number
- CN202410999205.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-24
AI Technical Summary
The existing technology is difficult to effectively treat high-salt and high COD lead-zinc ore flotation wastewater, which leads to high processing difficulties and high cost.
The pretreatment is carried out using a hydraulic cavitation device, combined with the use of oxidizing agents, acids and biological agents, and the COD in the wastewater is removed through oxidizing reactions, hydrolysis reactions and catalytic oxidizing reactions. The biologic agent is obtained from the culture of the complex bacteria of iron reducing bacteria and Bacillus, and is supported on modified biomass charcoal for catalyzing and adsorption of organic matter.
The deep purification of lead-zinc ore flotation wastewater has been achieved, the dosage and cost of medicines have been reduced, the production of toxic gases has been reduced, the reuse rate of wastewater has been improved, and the process is simple and environmentally friendly.
Smart Images

Figure CN118929946A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of industrial wastewater treatment, and in particular relates to a method for removing COD from oxidized lead-zinc ore flotation wastewater. Background Art
[0002] With the depletion of lead-zinc sulfide resources, the efficient development and utilization of lead-zinc oxide resources has become an important topic for mineral processing workers. At present, the flotation process of lead-zinc oxide ore is roughly: crushing-grinding-flotation-concentrate, tailings. During the ball milling process, an activator (sodium sulfide) is added to activate lead oxide, an inhibitor (zinc sulfate, sodium carbonate, lime) is added to inhibit sphalerite, and a collector (xanthate, black medicine, etc.) is added to complete the flotation of lead. After adjusting the pH, an activator (copper sulfate, lead nitrate, etc.) is added to activate sphalerite, and a collector (xanthate, black medicine, etc.) and a frother are added to complete the flotation of zinc sulfide minerals. Dispersants (water glass, sodium hexametaphosphate, etc.), activators (sodium sulfide, JF series activators, organic chelating agents, etc.), collectors (amines, xanthates, fatty acids, thiols, CF, CSFA, DZ-6 and other collectors) and frothers are added to complete the non-de-sludging flotation of zinc oxide minerals. The main foaming agents include pine oil, cresol oil, pine oil alcohol, methyl amyl alcohol and the like.
[0003] The reasons for the complex and difficult selection of oxidized lead-zinc ore are: the oxidation rate of lead and zinc is high and varies greatly, the mineral composition is complex and changeable, the ore structure is complex, the associated components are very unstable, and it contains a large amount of clay, iron hydroxide (limonite, etc.) and lead alum, which are very easy to muddy, making it difficult to control the flotation operation. At the same time, it contains a large amount of soluble salts (such as carbonates, sulfates, silicates and other oxides and sulfides). Soluble salts not only cause ore mud to coagulate, but also react with carbonate ions to form calcium carbonate precipitation, which covers the surface of the mineral, greatly hindering the flotation process of oxidized lead-zinc ore. Useful minerals (such as hemimorphite, smithsonite, cerussite, lead alum, etc.) and gangue minerals are complexly interlocked, intersecting, wrapping, and replacing each other, further increasing the difficulty of flotation. There are also the influence of fine minerals in the ore mud, especially in the lead oxide ore seriously impregnated with iron hydroxide, the flotation effect is extremely poor, the flotation effect of fine-grained lead oxide ore is not ideal, and the flotation activity of coarse-grained zinc oxide minerals is easy to disappear in the selection operation, causing it to fall off the tank. The dosage of reagents, especially sodium sulfide, is large. Amine collectors are sensitive to the ore mud and the dosage is large. At the same time, it is necessary to add frothers, xanthate, black medicine, ethylthiocyanate, water glass and other mineral processing reagents. Therefore, the flotation wastewater of lead zinc oxide ore has complex composition, high salt content, high COD concentration and high pH. The pH is usually around 12.0-13.0, which is strongly alkaline and difficult to handle.
[0004] At present, the commonly used methods for treating mineral processing wastewater at home and abroad include coagulation and sedimentation, oxidation, chemical precipitation, activated carbon adsorption, biological method, membrane method, etc., but these methods are difficult to complete the deep purification and reuse of wastewater at low cost and high efficiency. When the existing technology is applied to the COD removal of oxidized lead-zinc ore processing wastewater, it is suitable for low-salinity, low-COD wastewater or low-salinity, high-COD ore processing wastewater, but not suitable for the treatment of high-salinity, high-COD oxidized lead-zinc ore wastewater. Therefore, for high-salinity, high-COD oxidized lead-zinc ore processing wastewater, it is urgent to seek an efficient, reasonable, effective and practical treatment method. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a method for removing COD from flotation wastewater of oxidized lead-zinc ore in view of the limitations of the current COD removal from flotation wastewater of oxidized lead-zinc ore with high salinity and high COD.
[0006] In order to solve the above technical problems, the technical solution proposed by the present invention is:
[0007] A method for removing COD from flotation wastewater of oxidized lead-zinc ore, comprising the following steps:
[0008] (1) Pre-treating the flotation tailings of the oxidized lead-zinc ore by a hydraulic cavitation device; the flotation tailings are directly obtained by flotation without solid-liquid separation, and contain residual mineral processing agents;
[0009] (2) separating the solid and liquid of the sludge obtained by the pretreatment in step (1) to obtain mineral processing wastewater and slag;
[0010] (3) adding an oxidant to the mineral processing wastewater obtained in step (2) to carry out an oxidation reaction;
[0011] (4) adding an acid to the reaction solution of step (3) to adjust the pH and perform a hydrolysis reaction;
[0012] (5) adding a biological agent to the reaction liquid after step (4) to carry out a catalytic oxidation reaction; the biological agent comprises a bacterial liquid and a modified biochar, the bacterial liquid is obtained by culturing a composite bacterial community including iron-reducing bacteria and Bacillus, and the modified biochar is a biochar loaded with iron salts;
[0013] (6) Separating the liquid-solid-liquid after the reaction in step (5).
[0014] The residual mineral processing reagents include frothers.
[0015] The flotation tailings have a COD concentration of 2000-5000 mg / L and a TDS of ≥10 g / L.
[0016] As a further improvement, the flow rate of the flotation tailings in step (1) through the hydrodynamic cavitation device is 18 to 30 L / min.
[0017] As a further improvement, in step (4), the pH is adjusted to 4-6 and the reaction is carried out for 15-20 minutes.
[0018] As a further improvement, the amount of the biological agent added in step (5) is 0.2-1.0 g / L, and the reaction time is 15-30 min.
[0019] As a further improvement, the method for preparing the biological agent in step (5) comprises:
[0020] (a) culturing a composite bacterial community including iron-reducing bacteria and bacillus in a composite culture medium added with the mineral processing wastewater to obtain a bacterial solution;
[0021] (b) adding biochar to the iron salt solution, dispersing it evenly, and drying it to obtain modified biochar;
[0022] (c) adding the modified biochar to the bacterial solution and dispersing the modified biochar evenly to obtain the biological agent.
[0023] As a further improvement, the mass ratio of iron-reducing bacteria to Bacillus in the composite bacterial community in step (a) is 3:(6-8).
[0024] As a further improvement, the amount of biochar added in step (b) is 20% to 30% of the mass of the iron salt.
[0025] As a further improvement, the amount of modified biochar added in step (c) is 10% to 20% of the mass of the bacterial liquid.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] (1) The present invention utilizes the properties of the slurry after flotation of the oxidized lead-zinc ore to achieve the preliminary removal of COD and salt in the ore dressing slurry under the action of hydraulic cavitation. Specifically, the present invention utilizes the frother in the ore dressing reagent remaining in the ore pulp after flotation and the gravity of the ore pulp itself to strengthen the hydraulic cavitation effect, so that a local high concentration of strong oxidizing free radicals and the like are generated inside the ore pulp, thereby playing the role of activation effect. They can directly oxidize the residual ore dressing reagent in the ore pulp, thereby achieving the effect of inducing, triggering and strengthening chemical reactions. At the same time, the strong fluid mechanics shear force generated when the cavitation collapses will also break the chemical bonds on the main chain of the macromolecule to generate free radicals, thereby achieving the preliminary removal of COD in the ore pulp, greatly reducing the amount of subsequent COD removal reagents added, and reducing the cost of the reagents. Cavitation produces a mechanical effect, which can generate enough energy to break up some of the ore, clay, etc. in the ore pulp, increase the specific surface area, and increase its adsorption capacity. Through adsorption, part of the ore dressing reagent and part of the salt are removed, thereby reducing the salt in the ore pulp, which is conducive to the improvement of the subsequent oxidation efficiency.
[0028] (2) According to the properties of the wastewater, the present invention makes full use of the oxidant to form peroxy organic acid with organic matter in the wastewater in a strong alkaline environment to complete the further mineralization of COD.
[0029] (3) Adjust the pH to weak acidity, and some residual mineral processing agents will undergo molecular rearrangement or hydrolysis into small molecules, which will produce free sulfide ions.
[0030] The iron salt loaded on the biochar in the biological agent mainly undergoes precipitation reaction with the sulfur ions in the wastewater to remove the sulfur ions. At the same time, the iron salt catalyzes the residual oxidants to produce more strong oxidizing free radicals (sulfur oxide free radicals, hydroxyl free radicals or chlorine oxide free radicals, etc.), combined with the catalytic and adsorption functions of biochar and microbial metabolites (metabolites such as catalase, capsule, mucus, polysaccharides, polypeptides and proteins), it can efficiently remove organic matter in the wastewater and achieve deep COD removal; the loaded Bacillus can reduce Fe 3+ Fe 2+ , so that the loaded iron salt can achieve Fe 2+ , Fe 3+ circulation, increasing the generation rate of strong oxidative free radicals.
[0031] (4) The method for removing COD from flotation wastewater of oxidized lead-zinc ore provided by the present invention reduces the amount of alkali and acid used compared with the traditional Fenton method for removing COD, and no H 2 The production of toxic and harmful gases such as S and CO is more environmentally friendly, the COD removal efficiency is higher, and the flotation wastewater is deeply purified.
[0032] (5) The present invention performs pretreatment at the front end of the generation of ore dressing wastewater (before the solid-liquid separation of the slurry), with the concept of treating waste with waste. Compared with the existing process, the present invention is more efficient, more environmentally friendly, has low investment and operating costs, is simple to operate, and has strong impact load resistance. It can achieve efficient removal of COD in the flotation wastewater of oxidized lead-zinc ore, and the wastewater can be reused. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0034] Figure 1 It is a process flow chart of a specific embodiment of the present invention. DETAILED DESCRIPTION
[0035] In order to facilitate the understanding of the present invention, the present invention will be described more comprehensively and meticulously below in conjunction with the accompanying drawings and preferred embodiments of the present invention, but the protection scope of the present invention is not limited to the following specific embodiments.
[0036] Unless otherwise defined, all professional terms used below have the same meanings as those generally understood by those skilled in the art. The professional terms used herein are only for the purpose of describing specific embodiments and are not intended to limit the scope of protection of the present invention.
[0037] Unless otherwise specified, various raw materials, reagents, instruments and equipment used in the present invention can be purchased from the market or prepared by existing methods.
[0038] It is well known in the art that the lead-zinc oxide ore is ground and flotated to obtain concentrate and flotation tailings, and activators, collectors, frothers and other agents are added during the flotation process. The object of the method of the present invention is the flotation tailings that have not been separated from the solid and liquid (i.e., the pulp after flotation). The suspended matter in the flotation tailings mainly includes the ore components that have not been floated out, the residue of the flotation agent, the gangue minerals, the clay and other impurities.
[0039] In some embodiments, the flotation tailings of the oxidized lead-zinc ore have a COD concentration of 2000-5000 mg / L and a TDS of ≥10 g / L. In some embodiments, the flotation tailings of the oxidized lead-zinc ore have a pH of 12.3-13.3, a COD concentration of 2739-4681 mg / L, and a TDS of ≥10 g / L. 2- The content is 417-826 mg / L, and the TDS (total dissolved solids) is 13984-17530 mg / L. The mineral processing reagent is reflected in the COD concentration, and the salt is reflected in the TDS content.
[0040] like Figure 1 The method for removing COD from flotation wastewater of oxidized lead-zinc ore of the present invention comprises the following steps:
[0041] (1) The flotation tailings (ore pulp after flotation) of the oxidized lead-zinc ore are pretreated using a hydraulic cavitation device.
[0042] In some embodiments, the flow rate of the flotation tailings through the hydrodynamic cavitation device is 18-30 L / min, and the rotation speed is 2600-2900 rpm. Under the action of hydrodynamic cavitation, the flotation tailings of the oxidized lead-zinc ore are preliminarily removed of COD, reduced TDS and S 2- content.
[0043] (2) Separating the solid and liquid of the sludge obtained by pretreatment in step (1) to obtain mineral processing wastewater and slag.
[0044] (3) adding an oxidant to the mineral processing wastewater obtained in step (2) to carry out an oxidation reaction.
[0045] In some embodiments, during the oxidation reaction, the oxidant added is H 2 O 2 (20-40wt%), hypochlorite solution (8-20wt%), perchlorate solution or more, the reaction time is 30-60min. The amount of oxidant added and the COD concentration are as follows: 1ml oxidant: (100-220)mg COD.
[0046] (4) Acid is added to the reaction solution of step (3) to adjust the pH and perform a hydrolysis reaction.
[0047] In some embodiments, the pH of the wastewater is adjusted to 4-6 and the reaction is carried out for 15-20 minutes.
[0048] (5) Adding a biological agent to the reaction liquid of step (4) to carry out a catalytic oxidation reaction.
[0049] In some embodiments, in the catalytic oxidation of biological agents, the amount of biological agents added is 0.2 to 1.0 g / L, and the reaction time is 15 to 30 min.
[0050] (6) Separate the liquid and solid after the reaction in step (5). The effluent can be reused and the slag enters the tailings pond.
[0051] In some embodiments, the method for preparing the biological agent is:
[0052] (1) A composite bacterial community including iron-reducing bacteria and Bacillus is cultivated in a composite culture medium to which a small amount of the mineral processing wastewater is added to obtain a bacterial liquid.
[0053] In some embodiments, the mass ratio of iron-reducing bacteria to Bacillus in the composite bacterial community is 3:(6-8).
[0054] In some embodiments, the addition ratio of the mineral processing wastewater is 10-30% of the mass of the composite culture medium.
[0055] In some embodiments, the main components of the composite culture medium include: peptone soy broth 10.0-20.0 g / L, glucose 10.0-20.0 g / L, peptone 10.0-20.0 g / L, sodium dihydrogen phosphate 1.0-2.0 g / L, calcium chloride 1.0-2.0 g / L, biotin 3.0-4.0 g / L, and ferrous sulfate 5.0-10.0 g / L.
[0056] In some embodiments, the pH of the acclimation culture is 4.5-6.0 and the temperature is 20-35°C.
[0057] In some embodiments, the concentration of bacteria in the bacterial solution is 5.0×10 8 cfu / mL~9.0×108 cfu / mL.
[0058] (2) Preparation of modified biochar: Add biochar to the iron salt solution, disperse it evenly, and dry it at low temperature (30-40°C) to obtain the modified biochar.
[0059] In some specific embodiments, the iron salt is one or more of ferrous chloride, ferrous sulfate, ferric sulfate, polyferric sulfate, ferric chloride, ferrous nitrate, ferric nitrate, and ferrous acetate.
[0060] In some specific embodiments, the biomass charcoal is one or more of pine nut shell biomass charcoal, sawdust biomass charcoal, rice husk biomass charcoal, bagasse biomass charcoal, and coconut shell biomass charcoal.
[0061] In some specific embodiments, the concentration of the iron salt solution is 10-30 wt %, and the amount of biochar added is 20%-30% of the mass of the iron salt.
[0062] (3) Adding the modified biochar to the bacterial solution of step (1) to obtain a biomass charcoal biological preparation loaded with bacteria and modified.
[0063] In some specific embodiments, the amount of modified biochar added is 10% to 20% of the mass of the bacterial liquid.
[0064] The method for removing COD from flotation wastewater of oxidized lead-zinc ore provided by the present invention has the advantages of simple and stable process, high wastewater reuse rate, easy operation, small footprint, low cost, no secondary pollution, etc.
[0065] Example 1
[0066] The flotation tailings of a lead-zinc oxide mine were selected, with a pH of 12.9, a COD concentration of 2739 mg / L, and S 2- The content is 417mg / L and TDS is 13984mg / L.
[0067] (1) The flotation tailings of the oxidized lead-zinc ore were subjected to a hydraulic cavitation device with a rotation speed of 2600 rpm and a flow rate of 20 L / min, and a power of about 14.5 KW to achieve preliminary removal of COD. The COD concentration in the effluent was 1427 mg / L, S 2- The content was not detected, and the TDS was 6293 mg / L;
[0068] (2) The slurry from step (1) is passed through an inclined plate sedimentation tank to achieve solid-liquid separation;
[0069] (3) Add 8.0 ml / L NaClO solution (10 wt%) to the effluent (ore dressing wastewater) of step (2) and react for 30 min. The COD of the effluent is 619.9 mg / L.
[0070] (4) Add appropriate amount of sulfuric acid to the reaction solution of step (3), adjust the pH to 6, and react for 15 minutes;
[0071] (5) Add 0.2 g / L of biological agent to the reaction solution of step (4) and react for 15 min;
[0072] (6) The liquid after the reaction in step (5) enters the inclined plate sedimentation tank to achieve solid-liquid separation. The COD concentration in the effluent is 374 mg / L and can be reused. The tailings enter the tailings pond.
[0073] The preparation method of the biological preparation of this embodiment is:
[0074] (1) culturing a composite bacterial community including about 30% of iron-reducing bacteria and about 70% of bacillus in a composite medium (10.0 g / L of peptone soy broth, 10.0 g / L of glucose, 10.0 g / L of peptone, 1.0 g / L of sodium dihydrogen phosphate, 1.0 g / L of calcium chloride, 3.0 g / L of biotin, and 5.0 g / L of ferrous sulfate) to obtain a bacterial solution, wherein the pH of the acclimation culture is 5.0 and the temperature is 20° C.;
[0075] (2) Preparation of modified biochar: prepare a 10% ferric chloride + polyferric sulfate solution, add appropriate amounts of rice husk biochar and sawdust biochar, the added amount is 20% of the iron salt, and dry at low temperature (25°C) to obtain the modified biochar.
[0076] (3) The modified biochar was added to a bacterial solution containing iron-reducing bacteria and Bacillus (where the concentration of the bacteria in the bacterial solution was about 5.0×10 8 cfu / mL), dispersed evenly to obtain loaded bacteria-modified biochar, and the added amount of modified biochar was 10% of the mass of the bacterial solution.
[0077] Example 2
[0078] The flotation tailings of a lead-zinc oxide mine were selected, with a pH of 12.3, a COD concentration of 3859 mg / L, and S 2- The content is 713mg / L and TDS is 15860mg / L.
[0079] (1) The flotation tailings slurry of oxidized lead-zinc ore is passed through a hydraulic cavitation device with a controlled speed of 2800 rpm and a flow rate of 25 L / min and a power of about 15.0 KW to achieve preliminary removal of COD. The COD concentration in the effluent is 2351 mg / L, S 2- Content 0.32mg / L, TDS 8904mg / L;
[0080] (2) The slurry from step (1) is passed through an inclined plate sedimentation tank to achieve solid-liquid separation;
[0081] (3) Add 7.5 ml / L H 2 O 2 (30wt%), reaction time 30min, COD of effluent was 674mg / L;
[0082] (4) Add appropriate amount of sulfuric acid to the reaction solution of step (3), adjust the pH to 5.0, and react for 15 min;
[0083] (5) Add 0.5 g / L of biological agent to the reaction solution of step (4) and react for 30 min;
[0084] (6) The liquid after the reaction in step (5) enters the inclined plate sedimentation tank to achieve solid-liquid separation. The COD concentration in the effluent is 246 mg / L and can be reused. The tailings enter the tailings pond.
[0085] The preparation method of the biological agent is:
[0086] (1) culturing a composite bacterial community including about 30% of iron-reducing bacteria and about 70% of bacillus in a composite medium (15.0 g / L of peptone soy broth, 12.0 g / L of glucose, 15.0 g / L of peptone, 1.2 g / L of sodium dihydrogen phosphate, 1.5 g / L of calcium chloride, 3.5 g / L of biotin, and 8.0 g / L of ferrous sulfate) to obtain a bacterial solution, wherein the pH of the acclimation culture is 6.0 and the temperature is 30° C.;
[0087] (2) Preparation of modified biochar: prepare a 20% ferrous sulfate solution, add an appropriate amount of pine nut shell biochar, the added amount is 25% of the iron salt, and dry at low temperature (30° C.) to obtain the modified biochar.
[0088] (3) The modified biochar was added to a bacterial solution containing iron-reducing bacteria and Bacillus (where the concentration of the bacteria in the bacterial solution was about 7.0×10 8 cfu / mL) to obtain the loaded bacteria-modified biochar, and the added amount of the modified biochar was 15% of the mass of the bacterial solution.
[0089] Example 3
[0090] The flotation tailings of a lead-zinc oxide mine were selected, with a pH of 13.3, a COD concentration of 4681 mg / L, and S 2- The content is 826mg / L and TDS is 17530mg / L.
[0091] (1) The flotation tailings slurry of oxidized lead-zinc ore was passed through a hydraulic cavitation device with a speed of 2900 rpm and a flow rate of 25 L / min, and a power of about 15.5 KW, to achieve preliminary removal of COD, and the COD concentration in the effluent was 2549 mg / L, S2- The content was not detected, and the TDS was 9116 mg / L;
[0092] (2) The slurry from step (1) is passed through an inclined plate sedimentation tank to achieve solid-liquid separation;
[0093] (3) Add 10 ml / L H 2 O 2 (30wt%), reaction time 60min, COD of effluent was 759mg / L;
[0094] (4) Add appropriate amount of sulfuric acid to the reaction solution of step (3), adjust the pH to 5.5, and react for 15 minutes;
[0095] (5) Add 0.6 g / L of biological agent to the reaction solution of step (4) and react for 20 min;
[0096] (6) The liquid after the reaction in step (5) enters the inclined plate sedimentation tank to achieve solid-liquid separation. The COD concentration in the effluent is 362 mg / L and can be reused. The tailings enter the tailings pond.
[0097] The preparation method of the biological agent is:
[0098] (1) culturing a composite bacterial community including about 30% of iron-reducing bacteria and about 70% of bacillus in a composite medium (20.0 g / L of peptone soy broth, 20.0 g / L of glucose, 20.0 g / L of peptone, 2.0 g / L of sodium dihydrogen phosphate, 2.0 g / L of calcium chloride, 4.0 g / L of biotin, and 10.0 g / L of ferrous sulfate) to obtain a bacterial solution, wherein the pH of the acclimation culture is 6.0 and the temperature is 30° C.;
[0099] (2) Preparation of modified biochar: Prepare a 30% iron sulfate solution, add an appropriate amount of coconut shell biochar, the added amount is 30% of the iron salt, and dry at low temperature (35° C.) to obtain the modified biochar.
[0100] (3) The modified biochar was added to a bacterial solution containing iron-reducing bacteria and Bacillus (where the concentration of the bacteria in the bacterial solution was about 9.0×10 8 cfu / mL) to obtain the loaded bacteria-modified biochar, and the added amount of the modified biochar was 20% of the mass of the bacterial solution.
[0101] Comparative Example 1 Fenton method
[0102] The flotation tailings of a lead-zinc oxide mine were selected, with a pH of 13.5, a COD concentration of 4681 mg / L, and S 2- The content is 826mg / L and TDS is 17530mg / L.
[0103] (1) Add 4.5kg / m 3 Concentrated sulfuric acid is used to adjust the pH to 3.0. During this stage, a large amount of hydrogen sulfide and CO and other pungent gases are produced, and the COD concentration in the effluent is 2195 mg / L.
[0104] (2) Add 3.5kg / m 3 FeSO 4 7H 2 O and 10L / m 3 H 2 O 2 , react for 40 minutes;
[0105] (3) Add 1.8kg / m 3 NaOH, adjust pH to 7.0, hydrolyze for 15 min;
[0106] (4) Add a small amount of flocculant and let it settle for 2 hours. The effluent is turbid, with a COD concentration of 1272 mg / L, TDS of 21589 mg / L, and S 2- The content was not detected.
[0107] Comparative Example 2 Biological Agent Treatment
[0108] The flotation tailings of a lead-zinc oxide mine were selected, with a pH of 13.3, a COD concentration of 4681 mg / L, and S 2- The content is 826mg / L and TDS is 17530mg / L.
[0109] (1) Add 3.5 g / L concentrated sulfuric acid to adjust the pH to 5.5. At this stage, a large amount of hydrogen sulfide and CO and other pungent gases are produced, and the COD concentration in the effluent is 3517 mg / L;
[0110] (2) Add 0.6 g / L biological agent and react for 20 min;
[0111] (3) After the reaction in step (2), the liquid enters the inclined plate sedimentation tank to achieve solid-liquid separation. The COD concentration in the effluent is 2264 mg / L, and the TDS content is 19187 mg / L (adding sulfuric acid will increase TDS). 2- The content was not detected.
[0112] The preparation method of the biological agent is the same as that in Example 3
[0113] Comparative Example 3 Treatment of Ore Dressing Wastewater by Hydrodynamic Cavitation
[0114] The flotation tailings of a lead-zinc oxide mine were selected, with a pH of 13.3, a COD concentration of 4681 mg / L, and S 2- The content is 826mg / L and TDS is 17530mg / L.
[0115] After the slurry passes through the solid-liquid separation device, mineral processing wastewater and tailings are obtained;
[0116] The supernatant (ore dressing wastewater) enters the hydrodynamic cavitation device, with a controlled rotation speed of 2900rpm and a flow rate of 25L / min, a power of about 15.5KW, and a COD concentration of 4419mg / L in the effluent.
[0117] The above is only a preferred embodiment of the present invention and does not limit the present invention in any form. Therefore, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the scope of protection of the technical solution of the present invention.
Claims
1. A method for removing COD from flotation wastewater of oxidized lead-zinc ore, characterized in that: The steps include: (1) Pre-treating the flotation tailings of the oxidized lead-zinc ore by a hydraulic cavitation device; the flotation tailings are directly obtained by flotation without solid-liquid separation, and contain residual mineral processing agents; (2) separating the solid and liquid of the sludge obtained by the pretreatment in step (1) to obtain mineral processing wastewater and slag; (3) adding an oxidant to the mineral processing wastewater obtained in step (2) to carry out an oxidation reaction; (4) adding an acid to the reaction solution of step (3) to adjust the pH and perform a hydrolysis reaction; (5) adding a biological agent to the reaction liquid after step (4) to carry out a catalytic oxidation reaction; the biological agent comprises a bacterial liquid and a modified biochar, the bacterial liquid is obtained by culturing a composite bacterial community including iron-reducing bacteria and Bacillus, and the modified biochar is a biochar loaded with iron salts; (6) Separating the liquid-solid-liquid reaction after step (5).
2. The method for removing COD from flotation wastewater of oxidized lead-zinc ore according to claim 1, characterized in that: The residual mineral processing reagents include a frother.
3. The method for removing COD from flotation wastewater of lead-zinc oxide ore according to claim 1 or 2, characterized in that: The flotation tailings have a COD concentration of 2000-5000 mg / L and a TDS of ≥10 g / L.
4. The method for removing COD from flotation wastewater of lead-zinc oxide ore according to claim 1 or 2, characterized in that: The flow rate of the flotation tailings in step (1) through the hydrodynamic cavitation device is 18 to 30 L / min.
5. The method for removing COD from flotation wastewater of lead-zinc oxide ore according to claim 1 or 2, characterized in that: Step (4) adjust the pH to 4-6 and react for 15-20 minutes.
6. The method for removing COD from flotation wastewater of oxidized lead-zinc ore according to claim 1, characterized in that: The amount of the biological agent added in step (5) is 0.2-1.0 g / L, and the reaction time is 15-30 min.
7. The method for removing COD from flotation wastewater of oxidized lead-zinc ore according to claim 1 or 6, characterized in that: The method for preparing the biological agent in step (5) comprises: (a) culturing a composite bacterial community including iron-reducing bacteria and bacillus in a composite culture medium added with the mineral processing wastewater to obtain a bacterial solution; (b) adding biochar to the iron salt solution, dispersing it evenly, and drying it to obtain modified biochar; (c) adding the modified biochar to the bacterial solution and dispersing the modified biochar evenly to obtain the biological agent.
8. The method for removing COD from flotation wastewater of oxidized lead-zinc ore according to claim 7, characterized in that: The mass ratio of iron-reducing bacteria to Bacillus in the composite bacterial community of step (a) is 3:(6-8).
9. The method for removing COD from flotation wastewater of lead-zinc oxide ore according to claim 7, characterized in that: The amount of biochar added in step (b) is 20% to 30% of the mass of the iron salt.
10. The method for removing COD from flotation wastewater of lead-zinc oxide ore according to claim 7, characterized in that: The amount of modified biochar added in step (c) is 10% to 20% of the mass of the bacterial liquid.
Citation Information
Patent Citations
Method for synergic oxidation treatment of wastewater containing organics and heavy metal generated in mining and mineral separation
CN104478160A
Lead-zinc ore dressing wastewater treatment and recycling device and method thereof
CN109437448A
Cavitation and foaming integrated tailing flotation device
CN112495592A
Method of cavitation-acoustic weakening and disintegration of placers' clay sands
RU2426595C1
Recovery of tailings ponds
US20090020458A1
Cited By
Vulcanized slag treatment method
CN119870122A