Preparation method of improved long-acting energy porcelain

Through the improved preparation method of long-acting energy porcelain, using specific components and process processing, the problem of the effect attenuation of existing energy porcelain in cup applications is solved, achieving longer-lasting energy release and higher durability. Reduced environmental pollution.

CN118930236APending Publication Date: 2024-11-12FUJIAN XIA SHANG ZHOU ANCIENT CELADON TECHNOLOGY CO LTD +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411135535.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

When used as a cup, the existing energy porcelain has a significant effect on the stored objects, and it is difficult to exert its special effects stably for a long time.

Method used

Using the preparation method of improved long-acting energy porcelain, processed through specific formulations and processes, including the use of agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethylcellulose, polyvinyl alcohol and Components such as talc powder and other components are formed by mechanical stirring and firing.

Benefits of technology

The prepared energy porcelain has more lasting energy release characteristics, is stronger and more durable, and reduces the use or emissions of harmful substances to the environment, which is in line with the modern green production concept.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of ceramics, in particular to a preparation method of improved long-acting energy porcelain, which is prepared from the following components in percentage by weight: 10 to 20 parts of agate extract, 1.1 to 2.5 parts of wollastonite extract, 1 to 2 parts of aluminum oxide, 1.8 to 2 parts of activated carbon extract, 5 to 8 parts of kaolin extract, 0.2 to 0.7 part of carboxymethyl cellulose, 1 to 2 parts of polyvinyl alcohol, 1 to 1.2 parts of talcum powder and a proper amount of distilled water. Compared with the prior art, the energy ceramic prepared by the method has a more lasting energy release characteristic in the aspect of performance and can stably exert the special effect for a long time, the product is higher in strength and more durable compared with existing various types of ceramic, in addition, the preparation method can reduce the use or emission of substances harmful to the environment, and the energy ceramic is more environment-friendly. The modern green production concept is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of ceramics, and in particular to a method for preparing an improved long-acting energy porcelain. Background Art

[0002] Energy porcelain is a ceramic product with unique characteristics. It uses advanced technology and integrates a variety of special materials. It has received some attention in the field of health preservation.

[0003] The invention patent with application number 201410202740.3 discloses an energy porcelain, which is characterized in that, measured by weight, the porcelain material formula of the energy device is as follows: 20-30 parts of quartz stone, 25-35 parts of potassium feldspar, 10-15 parts of kaolin, 5-10 parts of water, 1-5 parts of silver, 1-5 parts of titanium, 1-5 parts of tin, 1-5 parts of silicone, 1-5 parts of potassium, 1-5 parts of magnesium, 1-5 parts of calcium, 1-5 parts of zinc, 1-5 parts of germanium, 1-5 parts of Brazilian tourmaline, 1-5 parts of medical stone, 1-5 parts of volcanic rock, 1-5 parts of old stove soil, 1-5 parts of magnetite, and 1-5 parts of inorganic salt minerals.

[0004] The application aims to solve the problem: "Therefore, if a container can be provided that can change the water quality so that the water in the container meets the WHO standards for high-quality drinking water, it will help humans prevent diseases, improve their physical fitness, and prevent various diseases. This porcelain utensil will have great social and economic significance."

[0005] However, at present, when energy porcelain is used to make cups, its positive effect on the contents is particularly attenuated; To this end, we proposed a method for preparing an improved long-lasting energy porcelain. Summary of the invention

[0006] In view of the above-mentioned shortcomings of the prior art, the present invention provides a method for preparing an improved long-acting energy porcelain, which solves the technical problems raised in the above-mentioned background technology.

[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions: In the first aspect, an improved long-lasting energy porcelain is composed of the following components by weight percentage: 10 to 20 parts of agate extract, 1.1 to 2.5 parts of wollastonite extract, 1 to 2 parts of aluminum oxide, 1.8 to 2 parts of activated carbon extract, 5 to 8 parts of kaolin extract, 0.2 to 0.7 parts of carboxymethyl cellulose, 1 to 2 parts of polyvinyl alcohol, 1 to 1.2 parts of talc and an appropriate amount of distilled water.

[0008] Furthermore, the preparation method of the agate extract is: Take agate raw stones of not less than the formula percentage, sort the agate raw stones with a transparency of not less than 50% and no through cracks based on machine vision, and rinse them with a high-pressure water gun; put the rinsed agate raw stones into a crusher for crushing, set the crusher running time to 20-30min, and set the crushing end speed of the crusher to 1000-2000 rpm; pass the crushed agate raw stones through a 2000-3000 mesh sieve, and use a magnetic separator to eliminate metal substances in the powder from the sieved agate raw stone powder; use a dryer to receive the agate raw stone powder after the metal powder elimination treatment, use the dryer to dry the agate raw stone powder, set the dryer drying time to 15-30min, set the drying temperature to 90-110 degrees Celsius, and the obtained is recorded as agate extract.

[0009] Furthermore, the agate raw material for preparing the agate extract is selected from any one of natural agate or artificial synthetic agate; The humidity of the agate extract is not more than 10%.

[0010] Furthermore, the preparation method of the wollastonite extract is: Take silica lime of not less than the formula percentage, wash and crush the silica lime, so that the particle size of the washed and crushed silica lime is 1-3 cm; put the obtained silica lime into a magnetic separator to eliminate magnetic substances; put the silica lime with the magnetic substances eliminated into an acid solution, set the reaction time to 2-4 hours, and set the reaction dimension to 51-79 degrees Celsius; use clean water to rinse the silica lime after the reaction and send it into a vacuum filter for filtration to separate the solid silica lime, which is recorded as wollastonite extract.

[0011] Furthermore, the acid solution used in the silica lime reaction is selected from dilute hydrochloric acid or dilute sulfuric acid, and the ratio of the acid solution to the silica lime is 2 / 1; When the silica lime is washed with clean water after the reaction, the silica lime is spread flat and the thickness is not more than 1 cm.

[0012] Furthermore, the aluminum oxide is selected from Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-Any one of aluminum oxide; The aluminum oxide is selected by default Type - Alumina.

[0013] Furthermore, the activated carbon extract is activated carbon powder, the activated carbon powder is sieved through 2500-2700 mesh, and the surface porosity of each activated carbon molecule in the activated carbon powder is not less than 75%.

[0014] Furthermore, the preparation method of the kaolin extract is: Take kaolin of not less than the formula percentage, and crush the kaolin ore until it can pass through a 200-mesh sieve; put the crushed kaolin powder into a stirring tank, add distilled water in a ratio of 1:4 to 1:6 to obtain a slurry; use a mechanical stirring device to stir the obtained slurry, set the stirring speed to 200 to 300 rpm, and set the stirring time to 30 to 45 minutes; let the stirred slurry stand for 2 to 3 hours; after standing, skim off the suspended matter without stirring the precipitate; further put the skimmed solution and precipitate into a centrifuge for dehydration, set the centrifuge speed to 1200 to 1400 rpm, set the centrifuge running time to 20 to 25 minutes, and put the obtained dehydrated precipitate into a drying device for drying, set the drying temperature to 80 to 100 degrees Celsius, until the water content of the dehydrated precipitate is less than 5%, and the result is recorded as kaolin extract.

[0015] Furthermore, the carboxymethyl cellulose is selected from high-polymerization degree carboxymethyl cellulose; The high-polymerization-degree carboxymethyl cellulose is prepared by any one of a solvent method, a water-based method, and a kneading method, and the high-polymerization-degree carboxymethyl cellulose is prepared by the water-based method by default; The higher the density of the raw material for preparing the high-polymerization degree carboxymethyl cellulose, the later the preparation method, such as the solvent method, the water medium method, or the kneading method, is selected.

[0016] In a second aspect, a method for preparing an improved long-acting energy porcelain comprises the following steps: Step 1: Accurately weigh each raw material according to the above formula, and save each raw material for later use; Step 2: adding agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethyl cellulose, polyvinyl alcohol, and talc into distilled water and mechanically stirring; Step 3: The mixture obtained in step 2 is recorded as clay; Step 4: The clay is kneaded into a predetermined shape and fired to obtain the improved long-lasting energy porcelain.

[0017] Compared with the known public technology, the technical solution provided by the present invention has the following beneficial effects: The present invention provides a method for preparing an improved long-lasting energy porcelain. The energy porcelain prepared by the preparation method has a more lasting energy release characteristic in terms of performance, and can stably exert its special efficacy for a long time. Secondly, the product itself is stronger and more durable than various types of existing ceramics. In addition, the preparation method may reduce the use or emission of substances harmful to the environment, which is in line with the concept of modern green production. DETAILED DESCRIPTION

[0018] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0019] The present invention will be further described below in conjunction with the embodiments.

[0020] Embodiment 1: The preparation method of an improved long-acting energy porcelain of this embodiment is composed of the following components: 10-20 parts of agate extract, 1.1-2.5 parts of wollastonite extract, 1-2 parts of aluminum oxide, 1.8-2 parts of activated carbon extract, 5-8 parts of kaolin extract, 0.2-0.7 parts of carboxymethyl cellulose, 1-2 parts of polyvinyl alcohol, 1-1.2 parts of talc and an appropriate amount of distilled water; The preparation method of agate extract is as follows: Take agate raw stones of not less than the formula percentage, sort the agate raw stones with a transparency of not less than 50% and no through cracks based on machine vision, and rinse them with a high-pressure water gun; put the rinsed agate raw stones into a crusher for crushing, set the crusher running time to 20-30 minutes, and set the crushing end speed of the crusher to 1000-2000 revolutions / min; pass the crushed agate raw stones through a 2000-3000 mesh sieve, and use a magnetic separator to eliminate metal substances in the powder from the screened agate raw stone powder; use a dryer to receive the agate raw stone powder after the metal powder elimination treatment, use the dryer to dry the agate raw stone powder, set the drying time of the dryer to 15-30 minutes, and set the drying temperature to 90-110 degrees Celsius, and the obtained is recorded as agate extract; The agate raw material for preparing the agate extract is selected from any one of natural agate or artificial synthetic agate; The humidity of agate extract shall not exceed 10%; The preparation method of wollastonite extract is: Take silica lime of not less than the formula percentage, wash and crush the silica lime, so that the particle size of the washed and crushed silica lime is 1-3 cm; put the obtained silica lime into a magnetic separator to eliminate magnetic substances; put the silica lime with magnetic substances eliminated into an acid solution, set the reaction time to 2-4 hours, and set the reaction dimension to 51-79 degrees Celsius; use clean water to rinse the silica lime after the reaction and send it into a vacuum filter for filtration to separate the solid silica lime, which is recorded as wollastonite extract; The acid solution used for the silica lime reaction is selected from either dilute hydrochloric acid or dilute sulfuric acid, and the ratio of the acid solution to the silica lime is 2 / 1; When the silica lime is washed with clean water after reaction, the silica lime is spread flat, and the thickness is no more than 1 cm; Alumina selection Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-Any one of aluminum oxide; Alumina is selected by default Type - Alumina; Activated carbon extract is activated carbon powder, which is sieved through 2500-2700 mesh, and the surface porosity of each activated carbon molecule in the activated carbon powder is not less than 75%; The preparation method of kaolin extract is as follows: Take kaolin of not less than the formula percentage, and crush the kaolin ore until it can pass through a 200-mesh sieve; put the crushed kaolin powder into a stirring tank, add distilled water in a ratio of 1:4 to 1:6, and obtain a slurry; use a mechanical stirring device to stir the obtained slurry, set the stirring speed to 200 to 300 rpm, and set the stirring time to 30 to 45 minutes; let the stirred slurry stand for 2 to 3 hours; after standing, skim off the suspended matter without stirring the precipitate; further put the skimmed solution and precipitate into a centrifuge for dehydration, set the centrifuge speed to 1200 to 1400 rpm, set the centrifuge running time to 20 to 25 minutes, and put the obtained dehydrated precipitate into a drying device for drying, set the drying temperature to 80 to 100 degrees Celsius, until the water content of the dehydrated precipitate is less than 5%, and the result is recorded as a kaolin extract; Carboxymethyl cellulose uses high-polymerization degree carboxymethyl cellulose; The high-polymerization degree carboxymethyl cellulose is prepared by any one of the solvent method, water medium method and kneading method. The water medium method is selected as the default method for preparing the high-polymerization degree carboxymethyl cellulose. The higher the density of the raw material for preparing high-polymerization degree carboxymethyl cellulose, the later the preparation method, such as solvent method, water medium method or kneading method, is selected.

[0021] A method for preparing an improved long-acting energy porcelain comprises the following steps: Step 1: Accurately weigh each raw material according to the above formula, and save each raw material for later use; Step 2: adding agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethyl cellulose, polyvinyl alcohol, and talc into distilled water and mechanically stirring; Step 3: The mixture obtained in step 2 is recorded as clay; Step 4: The clay is kneaded into a predetermined shape and fired to obtain the improved long-lasting energy porcelain.

[0022] Embodiment 2: A method for preparing an improved long-acting energy porcelain, comprising the following components: 10 parts of agate extract, 1.1 parts of wollastonite extract, 1 part of aluminum oxide, 1.8 parts of activated carbon extract, 5 parts of kaolin extract, 0.2 parts of carboxymethyl cellulose, 1 part of polyvinyl alcohol, 1 part of talc powder and an appropriate amount of distilled water; The preparation method of agate extract is as follows: Take agate raw stones of not less than the formula percentage, sort the agate raw stones with a transparency of not less than 50% and no through cracks based on machine vision, and wash them with a high-pressure water gun; put the washed agate raw stones into a crusher for crushing, set the crusher running time to 20 minutes, and set the crushing end speed of the crusher to 1000 revolutions / min; pass the crushed agate raw stones through a 2000-mesh sieve, and use a magnetic separator to eliminate metal substances in the powder from the screened agate raw stone powder; use a dryer to receive the agate raw stone powder after the metal powder elimination treatment, use the dryer to dry the agate raw stone powder, set the drying time of the dryer to 15 minutes, and set the drying temperature to 90 degrees Celsius, and the obtained powder is recorded as agate extract; The agate raw material for preparing the agate extract is selected from any one of natural agate or artificial synthetic agate; The humidity of agate extract shall not exceed 10%; The preparation method of wollastonite extract is: Take silica lime of not less than the formula percentage, wash and crush the silica lime, so that the particle size of the washed and crushed silica lime is 1 cm; put the silica lime obtained into a magnetic separator to eliminate magnetic substances; put the silica lime with magnetic substances eliminated into an acid solution, set the reaction time to 2 hours, and set the reaction dimension to 51 degrees Celsius; use clean water to rinse the silica lime after the reaction and send it into a vacuum filter for filtration to separate the solid silica lime, which is recorded as wollastonite extract; The acid solution used for the silica lime reaction is selected from either dilute hydrochloric acid or dilute sulfuric acid, and the ratio of the acid solution to the silica lime is 2 / 1; When the silica lime is washed with clean water after reaction, the silica lime is spread flat, and the thickness is no more than 1 cm; Alumina selection Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-Any one of aluminum oxide; Alumina is selected by default Type - Alumina; Activated carbon extract is activated carbon powder, which is sieved through a 2500-mesh sieve, and the surface porosity of each activated carbon molecule in the activated carbon powder is not less than 75%; The preparation method of kaolin extract is as follows: Take kaolin of not less than the formula percentage, and crush the kaolin ore until it can pass through a 200-mesh sieve; put the crushed kaolin powder into a stirring tank, add 1:6 distilled water to obtain a slurry; use a mechanical stirring device to stir the obtained slurry, set the stirring speed to 200 rpm, and set the stirring time to 30 minutes; let the stirred slurry stand for 2 hours; after standing, skim off the suspended matter without stirring the precipitate; further put the skimmed solution and precipitate into a centrifuge for dehydration, set the centrifuge speed to 1200 rpm, set the centrifuge running time to 20 minutes, put the obtained dehydrated precipitate into a drying device for drying, set the drying temperature to 80 degrees Celsius, until the water content of the dehydrated precipitate is less than 5%, and the result is recorded as kaolin extract; Carboxymethyl cellulose uses high-polymerization degree carboxymethyl cellulose; The high-polymerization degree carboxymethyl cellulose is prepared by any one of the solvent method, water medium method and kneading method. The water medium method is selected as the default method for preparing the high-polymerization degree carboxymethyl cellulose. The higher the density of the raw material for preparing high-polymerization degree carboxymethyl cellulose, the later the preparation method, such as solvent method, water medium method or kneading method, is selected.

[0023] A method for preparing an improved long-acting energy porcelain comprises the following steps: Step 1: Accurately weigh each raw material according to the above formula, and save each raw material for later use; Step 2: adding agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethyl cellulose, polyvinyl alcohol, and talc into distilled water and mechanically stirring; Step 3: The mixture obtained in step 2 is recorded as clay; Step 4: The clay is kneaded into a predetermined shape and fired to obtain the improved long-lasting energy porcelain.

[0024] Embodiment 3: A method for preparing an improved long-acting energy porcelain, comprising the following components: 20 parts of agate extract, 2.5 parts of wollastonite extract, 2 parts of aluminum oxide, 2 parts of activated carbon extract, 5-8 parts of kaolin extract, 0.7 parts of carboxymethyl cellulose, 2 parts of polyvinyl alcohol, 1.2 parts of talc and an appropriate amount of distilled water; The preparation method of agate extract is as follows: Take agate raw stones of not less than the formula percentage, sort the agate raw stones with a transparency of not less than 50% and no through cracks based on machine vision, and wash them with a high-pressure water gun; put the washed agate raw stones into a crusher for crushing, set the crusher running time to 30 minutes, and set the crushing end speed of the crusher to 2000 revolutions / min; pass the crushed agate raw stones through a 3000-mesh sieve, and use a magnetic separator to eliminate metal substances in the powder from the screened agate raw stone powder; use a dryer to receive the agate raw stone powder after the metal powder elimination treatment, use the dryer to dry the agate raw stone powder, set the drying time of the dryer to 30 minutes, set the drying temperature to 110 degrees Celsius, and the obtained is recorded as agate extract; The agate raw material for preparing the agate extract is selected from any one of natural agate or artificial synthetic agate; The humidity of agate extract shall not exceed 10%; The preparation method of wollastonite extract is: Take silica lime of not less than the formula percentage, wash and crush the silica lime, so that the particle size of the washed and crushed silica lime is 3 cm; put the silica lime obtained into a magnetic separator to eliminate magnetic substances; put the silica lime with magnetic substances eliminated into an acid solution, set the reaction time to 4 hours, and set the reaction dimension to 79 degrees Celsius; use clean water to rinse the silica lime after the reaction and send it into a vacuum filter for filtration to separate the solid silica lime, which is recorded as wollastonite extract; The acid solution used for the silica lime reaction is selected from either dilute hydrochloric acid or dilute sulfuric acid, and the ratio of the acid solution to the silica lime is 2 / 1; When the silica lime is washed with clean water after reaction, the silica lime is spread flat, and the thickness is no more than 1 cm; Alumina selection Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-Any one of aluminum oxide; Alumina is selected by default Type - Alumina; Activated carbon extract is activated carbon powder, which is sieved through a 2700-mesh sieve, and the surface porosity of each activated carbon molecule in the activated carbon powder is not less than 75%; The preparation method of kaolin extract is as follows: Take kaolin of not less than the formula percentage, and crush the kaolin ore until it can pass through a 200-mesh sieve; put the crushed kaolin powder into a stirring tank, add 1:6 distilled water to obtain a slurry; use a mechanical stirring device to stir the obtained slurry, set the stirring speed to 300 rpm, and set the stirring time to 45 minutes; let the stirred slurry stand for 3 hours; after standing, skim off the suspended matter without stirring the precipitate; further put the skimmed solution and precipitate into a centrifuge for dehydration, set the centrifuge speed to 1400 rpm, set the centrifuge running time to 25 minutes, put the obtained dehydrated precipitate into a drying device for drying, set the drying temperature to 100 degrees Celsius, until the water content of the dehydrated precipitate is less than 5%, and the result is recorded as kaolin extract; Carboxymethyl cellulose uses high-polymerization degree carboxymethyl cellulose; The high-polymerization degree carboxymethyl cellulose is prepared by any one of the solvent method, water medium method and kneading method. The water medium method is selected as the default method for preparing the high-polymerization degree carboxymethyl cellulose. The higher the density of the raw material for preparing high-polymerization degree carboxymethyl cellulose, the later the preparation method, such as solvent method, water medium method or kneading method, is selected.

[0025] A method for preparing an improved long-acting energy porcelain comprises the following steps: Step 1: Accurately weigh each raw material according to the above formula, and save each raw material for later use; Step 2: adding agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethyl cellulose, polyvinyl alcohol, and talc into distilled water and mechanically stirring; Step 3: The mixture obtained in step 2 is recorded as clay; Step 4: The clay is kneaded into a predetermined shape and fired to obtain the improved long-lasting energy porcelain.

[0026] Embodiment 4: A method for preparing an improved long-acting energy porcelain, comprising the following components: 15 parts of agate extract, 1.35 parts of wollastonite extract, 1.5 parts of aluminum oxide, 1.9 parts of activated carbon extract, 6 parts of kaolin extract, 0.4 parts of carboxymethyl cellulose, 1.5 parts of polyvinyl alcohol, 1.1 parts of talc and an appropriate amount of distilled water; The preparation method of agate extract is as follows: Take agate raw stones of not less than the formula percentage, sort the agate raw stones with a transparency of not less than 50% and no through cracks based on machine vision, and rinse them with a high-pressure water gun; put the rinsed agate raw stones into a crusher for crushing, set the crusher running time to 25 minutes, and set the crushing end speed of the crusher to 1300 revolutions / min; pass the crushed agate raw stones through a 2500-mesh sieve, and use a magnetic separator to eliminate metal substances in the powder from the screened agate raw stone powder; use a dryer to receive the agate raw stone powder after the metal powder elimination treatment, use the dryer to dry the agate raw stone powder, set the drying time of the dryer to 23 minutes, set the drying temperature to 100 degrees Celsius, and the obtained is recorded as agate extract; The agate raw material for preparing the agate extract is selected from any one of natural agate or artificial synthetic agate; The humidity of agate extract shall not exceed 10%; The preparation method of wollastonite extract is: Take silica lime of not less than the formula percentage, wash and crush the silica lime, so that the particle size of the washed and crushed silica lime is 2 cm; put the obtained silica lime into a magnetic separator to eliminate magnetic substances; put the silica lime with magnetic substances eliminated into an acid solution, set the reaction time to 3 hours, and set the reaction dimension to 60 degrees Celsius; use clean water to rinse the silica lime after the reaction and send it into a vacuum filter for filtration to separate the solid silica lime, which is recorded as wollastonite extract; The acid solution used for the silica lime reaction is selected from either dilute hydrochloric acid or dilute sulfuric acid, and the ratio of the acid solution to the silica lime is 2 / 1; When the silica lime is washed with clean water after reaction, the silica lime is spread flat, and the thickness is no more than 1 cm; Alumina selection Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-Any one of aluminum oxide; Alumina is selected by default Type - Alumina; Activated carbon extract is activated carbon powder, which is sieved through a 2600-mesh sieve, and the surface porosity of each activated carbon molecule in the activated carbon powder is not less than 75%; The preparation method of kaolin extract is as follows: Take kaolin of not less than the formula percentage, and crush the kaolin ore until it can pass through a 200-mesh sieve; put the crushed kaolin powder into a stirring tank, add 1:5 distilled water to obtain a slurry; use a mechanical stirring device to stir the obtained slurry, set the stirring speed to 250 rpm, and set the stirring time to 40 minutes; let the stirred slurry stand for 2.5 hours; after standing, skim off the suspended matter without stirring the precipitate; further put the skimmed solution and precipitate into a centrifuge for dehydration, set the centrifuge speed to 1300 rpm, set the centrifuge running time to 22 minutes, and put the obtained dehydrated precipitate into a drying device for drying, set the drying temperature to 90 degrees Celsius, until the water content of the dehydrated precipitate is less than 5%, and the result is recorded as kaolin extract; Carboxymethyl cellulose uses high-polymerization degree carboxymethyl cellulose; The high-polymerization degree carboxymethyl cellulose is prepared by any one of the solvent method, water medium method and kneading method. The water medium method is selected as the default method for preparing the high-polymerization degree carboxymethyl cellulose. The higher the density of the raw material for preparing high-polymerization degree carboxymethyl cellulose, the later the preparation method, such as solvent method, water medium method or kneading method, is selected.

[0027] A method for preparing an improved long-acting energy porcelain comprises the following steps: Step 1: Accurately weigh each raw material according to the above formula, and save each raw material for later use; Step 2: adding agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethyl cellulose, polyvinyl alcohol, and talc into distilled water and mechanically stirring; Step 3: The mixture obtained in step 2 is recorded as clay; Step 4: The clay is kneaded into a predetermined shape and fired to obtain the improved long-lasting energy porcelain.

[0028] In summary, the energy porcelain prepared by the preparation method in the above embodiment has performance that enables the energy porcelain to have more lasting energy release characteristics, and can stably exert its special effects for a long time. Secondly, the product itself is stronger and more durable than various types of existing ceramics. In addition, the preparation method may reduce the use or emission of substances harmful to the environment, which is in line with the concept of modern green production.

[0029] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. Such modifications or replacements will not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. An improved long-lasting energy porcelain, characterized in that: Calculated by weight percentage, it is composed of the following components: 10 to 20 parts of agate extract, 1.1 to 2.5 parts of wollastonite extract, 1 to 2 parts of aluminum oxide, 1.8 to 2 parts of activated carbon extract, 5 to 8 parts of kaolin extract, 0.2 to 0.7 parts of carboxymethyl cellulose, 1 to 2 parts of polyvinyl alcohol, 1 to 1.2 parts of talc and an appropriate amount of distilled water.

2. The improved long-lasting energy porcelain according to claim 1, characterized in that: The preparation method of the agate extract is: Take agate raw stones with a percentage not less than the formula, sort the agate raw stones with a transparency of not less than 50% and no through cracks based on machine vision, and use a high-pressure water gun to wash them; The washed agate raw stone is put into a grinder for crushing, the grinder operation time is set to 20-30 minutes, and the grinding end speed of the grinder is set to 1000-2000 revolutions per minute; the crushed agate raw stone is passed through a 2000-3000 mesh sieve, and the agate raw stone powder obtained by screening is passed through a magnetic separator to eliminate metal substances in the powder; a dryer is used to receive the agate raw stone powder after the metal powder elimination treatment, and the agate raw stone powder is dried in the dryer, the drying time of the dryer is set to 15-30 minutes, and the drying temperature is set to 90-110 degrees Celsius, and the obtained is recorded as agate extract.

3. The improved long-lasting energy porcelain according to claim 2, characterized in that: The agate raw material for preparing the agate extract is selected from any one of natural agate or artificial synthetic agate; The humidity of the agate extract is not more than 10%.

4. The improved long-lasting energy porcelain according to claim 1, characterized in that: The preparation method of the wollastonite extract is: Take silica lime of not less than the formula percentage, wash and crush the silica lime, so that the particle size of the washed and crushed silica lime is 1-3 cm; put the obtained silica lime into a magnetic separator to eliminate magnetic substances; put the silica lime with the magnetic substances eliminated into an acid solution, set the reaction time to 2-4 hours, and set the reaction dimension to 51-79 degrees Celsius; use clean water to rinse the silica lime after the reaction and send it into a vacuum filter for filtration to separate the solid silica lime, which is recorded as wollastonite extract.

5. The improved long-lasting energy porcelain according to claim 4, characterized in that: The silica lime reaction acid solution used in the dilute hydrochloric acid or dilute sulfuric acid in any one, the configuration ratio of the acid solution to silica lime is 2 / 1; When the silica lime is washed with clean water after the reaction, the silica lime is spread flat and the thickness is not more than 1 cm.

6. The improved long-lasting energy porcelain according to claim 1, characterized in that: The aluminum oxide is selected from Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-alumina, Type-Alumina any one; The aluminum oxide is selected by default Type - Alumina.

7. The improved long-lasting energy porcelain according to claim 1, characterized in that: The activated carbon extract is activated carbon powder, the activated carbon powder is sieved through 2500-2700 meshes, and the surface porosity of each activated carbon molecule in the activated carbon powder is not less than 75%.

8. The improved long-lasting energy porcelain according to claim 1, characterized in that: The preparation method of the kaolin extract is: Take kaolin of not less than the formula percentage, and crush the kaolin ore until it can pass through a 200-mesh sieve; put the crushed kaolin powder into a stirring tank, add distilled water in a ratio of 1:4 to 1:6 to obtain a slurry; use a mechanical stirring device to stir the obtained slurry, set the stirring speed to 200 to 300 rpm, and set the stirring time to 30 to 45 minutes; let the stirred slurry stand for 2 to 3 hours; after standing, skim off the suspended matter without stirring the precipitate; further put the skimmed solution and precipitate into a centrifuge for dehydration, set the centrifuge speed to 1200 to 1400 rpm, set the centrifuge running time to 20 to 25 minutes, and put the obtained dehydrated precipitate into a drying device for drying, set the drying temperature to 80 to 100 degrees Celsius, until the water content of the dehydrated precipitate is less than 5%, and the result is recorded as kaolin extract.

9. The improved long-lasting energy porcelain according to claim 1, characterized in that: The carboxymethyl cellulose is selected from high-polymerization degree carboxymethyl cellulose; The high-polymerization-degree carboxymethyl cellulose is prepared by any one of a solvent method, a water-based method, and a kneading method, and the high-polymerization-degree carboxymethyl cellulose is prepared by the water-based method by default; The higher the density of the raw material for preparing the high-polymerization degree carboxymethyl cellulose, the later the preparation method, such as the solvent method, the water medium method, or the kneading method, is selected.

10. A method for preparing an improved long-acting energy porcelain, the method being a method for preparing an improved long-acting energy porcelain as claimed in any one of claims 1 to 9, characterized in that: The following steps are involved: Step 1: Accurately weigh each raw material according to the above formula, and save each raw material for later use; Step 2: adding agate extract, wollastonite extract, alumina, activated carbon extract, kaolin extract, carboxymethyl cellulose, polyvinyl alcohol, and talc into distilled water and mechanically stirring; Step 3: The mixture obtained in step 2 is recorded as clay; Step 4: The clay is kneaded into a predetermined shape and fired to obtain the improved long-lasting energy porcelain.

Citation Information

Patent Citations

  • Thermal insulation agate porcelain and preparation method thereof

    CN110078487A

  • Ceramic artware and preparation method thereof

    CN113087506A

  • Health-preserving mineral porcelain

    CN114276119A

  • Preparation method of environment-friendly functional ceramic

    CN114349473A

  • Energy porcelain and manufacturing process therefor

    WO2015172701A1