Through the dimerization and cooxidation reaction of hexafluoropropylene, combined with expandable graphite and chitosan grafted hydroglue, the preparation of high-purity perfluorohexanone is achieved, solving the low yield and equipment requirements in the prior art High problems improve fire extinguishing performance and safety.
Patent Information
- Application Number
- CN202411426007.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-14
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing perfluorohexanone preparation methods have problems such as low yield of crude product, poor selectivity, many side reactions, high equipment requirements and difficult raw material synthesis, especially intermediate products are heat-sensitive and flammable, resulting in high equipment requirements.
Hexafluoropropylene is used for dimerization, and the polyhydric glue grafted with expandable graphite and chitosan is added. Through the co-oxidation reaction of hydrogen and oxygen, combined with isomerization catalytic reaction, the purification process is finally carried out to obtain high-purity perfluorohexyl ketone.
It improves the fire extinguishing performance and adaptability of perfluorohexanone, reduces cost and environmental pollution, enhances storage and transportation safety, and does not require the addition of solvents, and has lower reaction temperature and pressure.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of organic chemical synthesis preparation, and in particular to a preparation method of perfluorohexanone. Background Art
[0002] Perfluorohexanone is a transparent, colorless, odorless chemical substance. It is liquid at room temperature and has electrical insulation in both gaseous and liquid states. Due to its good fire extinguishing performance, large safety margin and excellent environmental performance, it has become a new generation of environmentally friendly clean fire extinguishing agent and an ideal substitute for Halon-1301, Halon-1211 and HFC-227ea. Perfluorohexanone is widely used in portable fire extinguishers and full flooding fire extinguishing systems. The latent heat of vaporization of perfluorohexanone is 1 / 25 of that of water, the vaporization rate is 50 times that of water, and it has a higher gas phase pressure, which helps perfluorohexanone to quickly change from liquid phase to gas phase and distribute to the protected area when sprayed from the nozzle of the fire extinguishing system.
[0003] Most of the prior art uses hexafluoropropylene as a raw material, a polar aprotic solvent as a medium, and a metal fluoride as a catalyst. The typical synthesis step is that hexafluoropropylene and hexafluoropropylene oxide react at 20-25° C. in the presence of a cesium fluoride catalyst to obtain perfluorohexanone. However, the crude product yield of this synthesis route is only 34.6%, the selectivity is poor, and there are many side reactions. The synthesis route of perfluorohexanone of 3M Company is: in an autoclave reactor, with ether as a reaction medium under sewage conditions, hexafluoropropylene and perfluoropropionyl fluoride are reacted under the action of potassium chloride to obtain a crude perfluorohexanone product, and then the impurity trimer and a small amount of hexafluoropropylene dimer are removed by a simple distillation or rectification method. Although the product yield is high, the synthesis of the raw material perfluoropropionyl fluoride is relatively difficult. In addition, the intermediate product of perfluorohexanone, perfluoro-2-methyl-2-pentene, is very sensitive to heat and highly flammable. U.S. Patents No. US4377717 and US4296265 introduce a method for synthesizing perfluoro-2-methyl-2-pentene using hexafluoropropylene as a raw material, without solvent, and using metal fluoride, activated carbon, and metal fluoride attached to activated carbon as a catalyst. This method has the characteristics of high temperature and high pressure, and has high requirements for equipment. Therefore, it is necessary to provide a production process for perfluorohexanone with low reaction temperature, low equipment requirements and high yield. Summary of the invention
[0004] The object of the present invention is to provide a method for preparing perfluorohexanone to solve the problems raised in the above background technology.
[0005] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a method for preparing perfluorohexanone, comprising the following steps: S1, first preparing two identical reaction containers, and adding hexafluoropropylene into the reaction container and then introducing a catalyst filled therein to carry out dimerization reaction to obtain perfluoro-2-methyl-2-pentene; S2, adding expandable graphite and chitosan-grafted polyhydrogel to the perfluoro-2-methyl-2-pentene obtained in the reaction container in step S1, and fully mixing and stirring to obtain a new compound to improve its performance and application effect; S3, introducing hydrogen and oxygen into the mixed compound in step S2 to mix them in a mixing molar ratio of 2:3:3, and obtaining a mixed gas after sufficient reaction; S4, introducing the mixed gas in step S3 into another reaction container filled with another catalyst to carry out a co-oxidation reaction to obtain an epoxide; S5, adding a new catalyst to the epoxide in step S4 to carry out an isomerization catalytic reaction to obtain a crude perfluorohexanone product; S6, finally purifying the crude perfluorohexanone product obtained in step S5.
[0006] As a preferred technical solution of the present invention, the reaction temperature of the dimerization reaction in step S1 is 40-110° C., and the reaction pressure is 6-12 MPa.
[0007] As a preferred technical solution of the present invention, the reaction temperature of the oxidation reaction in step S4 is 180-240° C., and the reaction pressure is 3-10 MPa.
[0008] As a preferred technical solution of the present invention, in step S5, the temperature of the reactor point is controlled at 20°C to 40°C for reaction, and the reaction pressure is between 7-14 MPa.
[0009] As a preferred technical solution of the present invention, the purification treatment in step S6 is to purify perfluorohexanone by reacting the crude perfluorohexanone product with a nucleophilic reagent at 20~100°C in the presence of a catalyst. After the reaction, the mixed product is separated and then distilled to obtain perfluorohexanone with a purity of more than 99.9%.
[0010] Compared with the prior art, the present invention has the following beneficial effects:
[0011] (1) The present invention is a method for preparing perfluorohexanone. The method for preparing perfluorohexanone provided by the present invention adds expandable graphite and chitosan grafted polyhydrogel, which plays a role in adjusting solubility, improving dispersibility and stability during the process, so that the fire extinguishing performance of perfluorohexanone can be significantly improved, and at the same time, its adaptability and effect in different application environments can be improved.
[0012] (2) The present invention is a method for preparing perfluorohexanone. The perfluorohexanone prepared by the method for preparing perfluorohexanone provided by the present invention is purified. This method does not require the addition of solvents, greatly reduces costs and environmental pollution problems, and improves safety during fire extinguishing. Moreover, the purified perfluorohexanone has a higher fire extinguishing agent safety limit value and a lower vapor pressure, which helps to improve the safety of its storage and transportation. DETAILED DESCRIPTION
[0013] A method for preparing perfluorohexanone according to an embodiment of the present invention comprises the following steps:
[0014] S1. First, prepare two identical reaction containers, add hexafluoropropylene into the reaction containers, and then introduce a catalyst filled therein to perform a dimerization reaction to obtain perfluoro-2-methyl-2-pentene;
[0015] S2, adding expandable graphite and chitosan-grafted polyhydrogel to the perfluoro-2-methyl-2-pentene obtained in the reaction container in step S1, and mixing and stirring to obtain a new compound to improve its performance and application effect;
[0016] S3, introducing hydrogen and oxygen into the mixed compound in step S2 to mix them in a molar ratio of 2:3:3, and obtaining a mixed gas after sufficient reaction;
[0017] S4, passing the mixed gas at the midpoint of step S3 into another reaction container filled with another catalyst to carry out a co-oxidation reaction to obtain an epoxide;
[0018] S5, adding a new catalyst to the epoxide in step S4 to carry out an isomerization catalytic reaction to obtain a crude perfluorohexanone product;
[0019] S6, finally purifying the crude perfluorohexanone product obtained in step S5;
[0020] In this embodiment, the reaction temperature of the dimerization reaction in step S1 is 40-110°C, and the reaction pressure is 6-12MPa. The reaction temperature of the oxidation reaction in step S4 is 180-240°C, and the reaction pressure is 3-10MPa. In step S5, the reactor point temperature is controlled at 20°C to 40°C for reaction, and the reaction pressure is between 7-14MPa.
[0021] In this embodiment, the purification treatment in step S6 is to purify perfluorohexanone by reacting the crude perfluorohexanone product with a nucleophilic reagent at 20~100°C in the presence of a catalyst. After the reaction is completed, the mixed product is separated and then distilled to obtain perfluorohexanone with a purity of more than 99.9%.
[0022] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing perfluorohexanone, It is characterized in that The following steps are involved: S1. First, prepare two identical reaction containers, add hexafluoropropylene into the reaction container, and then introduce a catalyst filled therein to carry out a dimerization reaction to obtain perfluoro-2-methyl-2-pentene; S2. Add expandable graphite and chitosan-grafted polyhydrogel to the perfluoro-2-methyl-2-pentene obtained in the reaction container in step S1, mix and stir them thoroughly to obtain a new compound to improve its performance and application effect; S3. Add hydrogen and oxygen to the mixed compounds in step S2 to mix them in a molar ratio of 2:3:3, and obtain a mixed gas after sufficient reaction; S4. Pass the mixed gas in step S3 into another reaction container filled with another catalyst to carry out a co-oxidation reaction to obtain an epoxide; S5. Add a new catalyst to the epoxide in step S4 to carry out an isomerization catalytic reaction to obtain a crude perfluorohexanone product; S6. Finally, purify the crude perfluorohexanone product obtained in step S5.
2. A method for preparing perfluorohexanone according to claim 1, It is characterized in that The reaction temperature of the dimerization reaction in step S1 is 40-110° C., and the reaction pressure is 6-12 MPa.
3. A method for preparing perfluorohexanone according to claim 1, It is characterized in that The reaction temperature of the oxidation reaction in step S4 is 180-240° C., and the reaction pressure is 3-10 MPa.
4. A method for preparing perfluorohexanone according to claim 1, It is characterized in that In step S5, the temperature of the reactor point is controlled at 20°C to 40°C for reaction, and the reaction pressure is between 7-14 MPa.
5. A method for preparing perfluorohexanone according to claim 1, It is characterized in that The purification treatment in step S6 is to purify perfluorohexanone by reacting the crude perfluorohexanone product with a nucleophilic reagent at 20-100° C. in the presence of a catalyst. After the reaction, the mixed product is separated and then distilled to obtain perfluorohexanone with a purity of more than 99.9%.
Citation Information
Patent Citations
Preparation method and application of perfluoro hexanone
CN107501038A
Multifunctional perfluorohexanone fire extinguishing agent and preparation method thereof
CN113509679A
Preparation method of perfluorohexanone
CN116854574A
Purification method of perfluorohexanone
CN116969825A
Catalyst system and preparation method therefor and use thereof
WO2024138976A1