Preparation process of electronic-grade ammonium acetate
Through the neutralization reaction of acetic acid and ammonia water and subsequent treatment steps, high-purity ammonium acetate was successfully prepared, which solved the problem of high metal impurities content in the prior art, met the processing needs of nano-scale integrated circuits, and achieved low cost and Environmentally friendly industrial production.
Patent Information
- Application Number
- CN202410848100.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-27
- Publication Date
- 2024-11-12
AI Technical Summary
The high content of metal impurities in existing ammonium acetate products leads to easy disassembly, leakage current and breakdown in integrated circuit manufacturing, affecting the reliability and life of the circuit, especially in nano-scale integrated circuit processing.
After neutralization reaction of acetic acid and ammonia water, it is subjected to under reduced pressure distillation and concentration, the crystallization temperature and stirring conditions are controlled, and combined with centrifugal washing and drying steps, an ultra-clean high-purity ammonium acetate with a content of more than 99% and a metal impurity less than 5 ppb was prepared.
The preparation of high-purity ammonium acetate is realized, which meets the processing needs of nano-scale integrated circuits, reduces production costs, and is simple and suitable for large-scale production, avoiding human contact and environmental pollution.
Smart Images

Figure CN118930428A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of chemical synthesis, and in particular to a preparation process of electronic grade ammonium acetate. Background Art
[0002] Ammonium acetate, also known as ammonium acetate, is a white crystal with an acetic acid smell. As an organic salt, it can be used in meat preservatives, pharmaceuticals, and analytical reagents. It can also be used as a corrosion inhibitor and additive in silicon wafer etching solutions, electroplating solutions, cleaning agents and other electronics industries.
[0003] In the process of industrial production, transportation and storage of ammonium acetate, due to reasons such as raw materials and equipment, it is inevitable that some impurities such as dust particles, metal ions, and unreacted raw materials will be introduced into the product. The presence of these impurities, especially metal ions, can easily lead to the generation of staggered layers, thereby increasing the risk of leakage current, breakdown, and reducing the life of carriers. Therefore, for integrated circuits with smaller line widths, a few metal ions or dust particles are enough to scrap the entire circuit. Due to the rapid development of the integrated circuit (IC) industry, the requirements for the content of various electronic-grade reagents are also getting higher and higher. From the perspective of technological trends, meeting the processing needs of nano-scale integrated circuits is the development direction of electronic-grade reagents.
[0004] At present, the ammonium acetate on the market mainly focuses on high content and low moisture, and pays less attention to metal trace impurities. Therefore, it is of great significance to develop a preparation method of electronic grade ammonium acetate with low metal impurities suitable for the IC industry. Summary of the invention
[0005] In order to solve the technical problems of low ammonium acetate content and high metal impurity content in the prior art, the present invention aims to provide a preparation process of electronic-grade ammonium acetate. The present invention obtains an electronic-grade ammonium acetate product with high content and low metal impurity content through the preparation process. The method is simple in process and suitable for large-scale production.
[0006] The method first synthesizes an ammonium acetate solution through a neutralization reaction of acetic acid and ammonia water, concentrates the solution and then cools it for crystallization, and after centrifugation, washing and drying, an ultra-clean and high-purity electronic-grade ammonium acetate product with a content of more than 99% and metal impurities less than 5 ppb can be obtained.
[0007] Specifically, the present invention provides a preparation process of electronic grade ammonium acetate, the preparation process comprising the following steps: Step 1: Into the acetic acid solution, an excess of ammonia water is introduced to completely neutralize the solution to produce a mixed solution of ammonium acetate and ammonia water; Step 2: distilling the mixed solution in step 1 under reduced pressure to remove excess ammonia water and obtain a concentrated solution of a certain concentration; Step 3: crystallizing the concentrated solution of step 2, controlling the crystallization temperature in the system, and obtaining ammonium acetate slurry after cooling and crystallization; Step 4: After centrifugation and washing, the crystal slurry obtained in step 3 is subjected to filtrate and ammonium acetate crystals are obtained; Step 5: Drying the ammonium acetate crystals obtained in step 4 to obtain an electronic grade ammonium acetate product.
[0008] The above steps provide a preparation process for electronic grade ammonium acetate. In the step 1, preferably, the acetic acid used is industrial grade acetic acid with a content greater than 99%, the ammonia water used is industrial grade ammonia water with a concentration of 27% to 29%, and the endpoint pH of the neutralization reaction is 7 to 7.5.
[0009] In the step 1, preferably, the synthesis temperature is controlled to be lower than 40° C. by introducing circulating cooling water into the interlayer of the synthesis reactor.
[0010] In the step 1, preferably, the pipe for introducing the ammonia water needs to be submerged below the liquid level of the acetic acid solution, and the ammonia water is slowly added to the acetic acid solution and continuously stirred at a stirring speed of 100-200 rpm / min, and the flow rate of the added ammonia water is 0.4-0.5 kg / min; through this operation, not only can the volatilization of ammonia gas be prevented and the loss of ammonia water be reduced, but also the ammonia water and acetic acid can be fully contacted to promote the reaction.
[0011] The above provides a process for preparing electronic grade ammonium acetate. In the step 2, preferably, the vacuum degree of the reduced pressure concentration is less than -0.08 MPa.
[0012] In the step 2, preferably, the temperature of the reduced pressure concentration is controlled at 40-70°C.
[0013] More preferably, the concentration temperature is 50-60°C.
[0014] By concentrating under reduced pressure, aqueous ammonia can be quickly removed to obtain concentrated ammonium acetate solution.
[0015] In the step 2, preferably, after concentration under reduced pressure, the concentration of ammonium acetate is controlled at 75-80%, and the distilled ammonia solution can be recycled to step 1. By controlling the concentration of the ammonium acetate concentrate, ammonium acetate with a higher yield and content can be obtained.
[0016] The above provides a preparation process for electronic grade ammonium acetate. In the step 3, preferably, the starting crystallization temperature of ammonium acetate is 60-70° C., and the ending crystallization temperature is 10-20° C. At this temperature, ammonium acetate crystals are well precipitated.
[0017] In the step 3, preferably, the temperature for adding the seed crystals is 45-60° C., and the amount of the seed crystals added is 0.5-1% of the mass of the crystallization solution; the addition of the seed crystals promotes the precipitation of ammonium acetate crystals.
[0018] In the step 3, preferably, the cooling rate during the crystallization of ammonium acetate is 2-10°C / h.
[0019] More preferably, the cooling rate is 4-8°C / h, and the temperature is slowly lowered to allow crystals to precipitate slowly and obtain better uniformity.
[0020] In the step 3, preferably, the stirring speed during the crystallization of ammonium acetate is 50-200 r / min.
[0021] The above provides a preparation process for electronic grade ammonium acetate. In the step 4, preferably, the washing is centrifugal spray washing, the spray flow rate is 0.01~0.5L / s, and the spray time is 10~60s.
[0022] The above provides a preparation process for electronic grade ammonium acetate. In the step 5, preferably, the crystals are washed and then vacuum dried at 45-55° C. for 4-12 hours.
[0023] More preferably, the drying time of the crystals is 6 to 8 hours.
[0024] The invention obtains an ultra-clean and high-purity electronic-grade ammonium acetate product by controlling the reaction conditions of acetic acid and ammonia water and the crystallization conditions of ammonium acetate, so as to meet the processing requirements of nano-scale integrated circuits.
[0025] Compared with the prior art, the advantages of the present invention are: 1. The present invention provides a preparation process of ultra-clean high-purity electronic-grade ammonium acetate, which is simple to operate and easy to industrialize. The product content is greater than 99%, and the metal impurity content is less than 5 ppb, which meets the requirements of electronic-grade ammonium acetate.
[0026] 2. In the synthesis process of the present invention, the pipeline for passing ammonia water should be submerged below the liquid level of the sulfuric acid solution to allow it to fully contact and undergo a neutralization reaction, thereby reducing the thermal decomposition of ammonia water in the air and reducing the loss of ammonia water; at the same time, in the concentration process, the concentrated ammonia water can be recycled, effectively reducing costs and realizing industrial production.
[0027] 3. The entire preparation process of the present invention is a fully enclosed low-temperature system, which avoids the stimulation of acetic acid and ammonia water to the human body during the synthesis process, and the production process is gentle and pollution-free.
[0028] 4. In the centrifugal washing process, the present invention utilizes high-speed centrifugation and spray washing to quickly separate the filtrate attached to the surface of the ammonium acetate crystals, thereby obtaining a purer ammonium acetate product; at the same time, high-speed centrifugation can effectively reduce the free water in the ammonium acetate crystals and shorten the subsequent drying time. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The present invention will be further described below in conjunction with the accompanying drawings and embodiments: Figure 1 The present invention is a production process flow chart of electronic grade ammonium acetate. DETAILED DESCRIPTION
[0030] In the following examples and comparative examples, the content of ammonium acetate was determined by potentiometric titration or near infrared, and the content of metal ion impurities was detected by ICP-MS.
[0031] Example 1 A process for preparing electronic grade ammonium acetate comprises the following steps: Step 1: Add 10kg of 99.89% industrial grade glacial acetic acid to a 30L double-layer reactor, connect the circulating water, adjust the cooling device, and set the external circulating water temperature to about 5°C. When the acetic acid solution in the reactor cools down to below 25°C, turn on the stirring, and slowly add 29% ammonia water at a flow rate of 0.4g / min at a stirring speed of 150r / min. Control the reaction temperature not to exceed 40°C. When the pH value of the mixed solution reaches 7.5, stop adding ammonia water to complete the neutralization reaction; Step 2: After the reaction is completed, the circulating water temperature is increased to 65°C, stirred at a stirring speed of 150r / min for 30min, the vacuum pump is turned on to make the system vacuum degree <-0.08mPa, and the reduced pressure is concentrated to the concentration of ammonium acetate of 78-80%; Step 3: After the concentration is complete, turn off the vacuum pump, raise the reaction system to normal pressure, and adjust the stirring speed to 50r / min; at this time, the initial crystallization temperature of the solution is 65°C, adjust the program temperature control device, adjust the cooling rate of the circulating water to 4°C / h, and when the temperature drops to 55°C, add 0.1kg of ammonium acetate seeds to induce crystallization. When the solution temperature drops to 15°C, the crystallization process is terminated to obtain ammonium acetate slurry; Step 4: After the crystallization is completed, the slurry is placed in a centrifuge to centrifuge and separate the filtrate. After the filtrate is completely separated, it is sprayed with pure water for washing for 30 seconds at a flow rate of 0.02L / s, and centrifuged at high speed until the washing liquid is completely separated to obtain ammonium acetate crystals; Step 5: Place the ammonium acetate crystals in a vacuum drying oven and dry at 50° C. for 4 hours to obtain electronic grade ammonium acetate product.
[0032] Example 2 A process for preparing electronic grade ammonium acetate comprises the following steps: Step 1: Add 10kg of 99.91% industrial grade glacial acetic acid to a 30L double-layer reactor, connect the circulating water, adjust the cooling device, and set the external circulating water temperature to about 5°C. When the acetic acid solution in the reactor cools down to below 25°C, turn on the stirring, and slowly add 25.5% ammonia water at a flow rate of 0.5kg / min at a stirring speed of 150r / min. Control the reaction temperature not to exceed 40°C. When the pH value of the mixed solution reaches 7.5, stop adding ammonia water to complete the neutralization reaction; Step 2: After the reaction is complete, increase the circulating water temperature to 65°C, maintain the stirring speed at 150r / min for 30min, and turn on the vacuum pump to make the system vacuum degree <-0.08mPa, and reduce the pressure to concentrate to the concentration of ammonium acetate of 78~80%; Step 3: After the concentration is complete, turn off the vacuum pump, raise the reaction system to normal pressure, and maintain the stirring speed at 150r / min. At this time, the initial crystallization temperature of the solution is 65°C. Adjust the program temperature control device and adjust the cooling rate of the circulating water to 6°C / h. When the temperature drops to 55°C, add 0.1kg of ammonium acetate seeds to induce crystallization. When the solution temperature drops to 15°C, the crystallization process is terminated to obtain ammonium acetate slurry; Step 4: After the crystallization is completed, the crystal slurry is placed in a centrifuge to centrifuge and separate the filtrate. After the filtrate is completely separated, it is sprayed with pure water at a flow rate of 0.02L / s for 30s, and centrifuged at high speed until the washing liquid is completely separated to obtain ammonium acetate crystals; Step 5: Place the ammonium acetate crystals in a vacuum drying oven and dry at 50° C. for 4 hours to obtain electronic grade ammonium acetate product.
[0033] Example 3 A process for preparing electronic grade ammonium acetate comprises the following steps: Step 1: Add 10kg of 99.89% industrial grade glacial acetic acid to a 30L double-layer reactor, connect the circulating water, adjust the cooling device, and set the external circulating water temperature to about 5°C. When the acetic acid solution in the reactor cools down to below 25°C, turn on the stirring, and slowly add 29% ammonia water at a flow rate of 0.5kg / min at a stirring speed of 100r / min. Control the reaction temperature not to exceed 50°C. When the pH value of the mixed solution reaches 7.5, stop adding ammonia water to complete the neutralization reaction; Step 2: After the reaction is completed, the temperature is raised to 60°C, and the mixture is stirred at a stirring speed of 100 r / min for 30 min. Subsequently, the mixture is concentrated under reduced pressure at a vacuum degree of <-0.08 mPa to a concentration of ammonium acetate of 75-77%; Step 3: After the concentration is complete, turn off the vacuum pump, raise the reaction system to normal pressure, and maintain the stirring speed at 100r / min. At this time, the initial crystallization temperature of the solution is 60°C. Adjust the program temperature control device and adjust the cooling rate of the circulating water to 5°C / h. When the temperature drops to 50°C, add 0.1kg of ammonium acetate seeds to induce crystallization. When the solution temperature drops to 10°C, end the crystallization process to obtain ammonium acetate slurry; Step 4: After the crystallization is completed, the slurry is placed in a centrifuge to centrifuge and separate the filtrate. After the filtrate is completely separated, it is sprayed with pure water for washing for 30 seconds at a flow rate of 0.02L / s, and centrifuged at high speed until the washing liquid is completely separated to obtain ammonium acetate crystals; Step 5: Place the ammonium acetate crystals in a vacuum drying oven and dry at 50° C. for 4 hours to obtain electronic grade ammonium acetate product.
[0034] Example 4 A process for preparing electronic grade ammonium acetate comprises the following steps: Step 1: Add 10kg of 99.89% industrial grade glacial acetic acid to a 30L double-layer reactor, connect the circulating water, adjust the cooling device, and set the external circulating water temperature to about 5°C. After the acetic acid solution in the reactor cools down to below 25°C, turn on the stirring, and slowly add 29% ammonia water at a flow rate of 0.4kg / min at a stirring speed of 200r / min. Control the reaction temperature not to exceed 40°C. When the pH value of the mixed solution reaches 7.5, stop adding ammonia water to complete the neutralization reaction; Step 2: After the reaction is completed, the temperature is raised to 70°C, and the mixture is stirred at a stirring speed of 200 r / min for 30 min. Subsequently, the mixture is concentrated under reduced pressure at a vacuum degree of <-0.08 mPa to a concentration of ammonium acetate of 78-80%; Step 3: After the concentration is complete, turn off the vacuum pump, raise the reaction system to normal pressure, and maintain the stirring speed at 200r / min. At this time, the initial crystallization temperature of the solution is 70°C. Adjust the program temperature control device and adjust the cooling rate of the circulating water to 8°C / h. When the temperature drops to 60°C, add 0.1kg of ammonium acetate seeds to induce crystallization. When the solution temperature drops to 10°C, the crystallization process is terminated to obtain ammonium acetate slurry; Step 4: After the crystallization is completed, the slurry is placed in a centrifuge to centrifuge and separate the filtrate. After the filtrate is completely separated, it is sprayed with pure water for washing for 30 seconds at a flow rate of 0.02L / s, and centrifuged at high speed until the washing liquid is completely separated to obtain ammonium acetate crystals; Step 5: Place the ammonium acetate crystals in a vacuum drying oven and dry at 50° C. for 4 hours to obtain electronic grade ammonium acetate product.
[0035] Example 5 Based on Example 1-2, the synthesis stirring speed, the flow rate of ammonia water in step 1 and the use of condensed water throughout the process were changed to investigate the effects of different stirring speeds, ammonia water flow rates and condensed water on the actual amount of ammonia water introduced and the content of metal impurities. The experimental results are shown in Table 1.
[0036] Table 1 Effects of stirring speed, flow rate and condensed water on ammonia feed and metal impurities
[0037] From the comparison of the results in Table 1, it can be seen that when the stirring speed is 100-200 r / min and the flow rate is 0.4-0.5 kg / min, the neutralization reaction temperature is controlled by external circulating condensed water, and the actual amount of ammonia water used is not much different from the theoretical input amount, the content of ammonium acetate is higher than 99%, and the content of metal ions is lower than 5 ppb; in the synthesis process, the stirring speed is too fast or too slow, the flow rate of ammonia water is too fast or too slow, and the temperature control without adding condensed water will increase the amount of ammonia water used, which will lead to an increase in metal impurities in the mixed solution of ammonium acetate and ammonia water during the synthesis process, and finally lead to a slight increase in metal impurities in the finished ammonium acetate.
[0038] Example 6 Based on Example 2-3, the concentration of the concentrated ammonium acetate in step 2 was controlled to investigate the effects of different concentrated ammonium acetate concentrations on the ammonium acetate yield and the content of metal impurities. The experimental results are shown in Table 2.
[0039] Table 2 Effect of the concentration of concentrated ammonium acetate on the content of ammonium acetate and metal impurities
[0040] From the comparison of the results in Table 2, it can be seen that when the concentration of ammonium acetate in the concentrated solution is between 75% and 80%, the yield and content of ammonium acetate are relatively good; when the concentration of the concentrated solution is lower than 75%, the supersaturation range is low and the final yield is reduced; when the concentration of the concentrated solution is higher than 80%, the crystallization process is unstable, and the nuclear explosion crystallization phenomenon is prone to occur when the temperature is lowered, resulting in the inability of ammonium acetate crystals to grow well, and the yield has not increased significantly, but the crystal content is reduced and the metal impurity content is increased.
[0041] Example 7 Based on Example 1 and Example 4, the crystallization temperature, cooling rate and stirring rate in step 3 were changed to investigate the effects of different crystallization start and end temperatures and cooling rates on the ammonium acetate yield and metal impurity content. The experimental results are shown in Table 3.
[0042] Table 3 Effect of crystallization start and end temperature, stirring rate and cooling rate on ammonium acetate yield and content
[0043] From the comparison of the results in Table 3, it can be seen that if the initial crystallization temperature is too high, the crystallization time will be prolonged, and the crystal yield, purity, and metal impurity removal will not be significantly improved. If the initial crystallization temperature is too low, the crystallization will be unstable, and nuclear explosion will easily occur, and the metal impurities in the crystal will increase. During the crystallization process, if the cooling rate is too slow or too fast, it will affect the crystal growth state. If the cooling rate is too fast, the crystal will grow rapidly, and the metal impurities in the crystal will increase. At the same time, due to the large temperature difference between the inside and outside of the kettle, the crystal will grow along the wall, and the inner wall of the crystal will stick to the wall, reducing the overall yield; if the cooling rate is too slow, the crystal will grow slowly, the crystal size will be larger, and the metal impurities will be reduced, but the crystal will also sink to the bottom, reducing the overall yield. Secondly, during the crystallization process, the stirring speed also has a significant impact on the crystallization process. If the stirring speed is too slow, the crystal cannot be dispersed in the entire solution system, and the crystal will sink to the bottom and harden after growing larger; if the stirring speed is too fast, the shear force of the paddle on the crystal will increase, the crystal will be more easily damaged, and secondary nucleation will be induced, and the metal impurities in the crystal will increase. Therefore, when the starting crystallization temperature is controlled at 60~70°C, the ending crystallization temperature is controlled at 10~20°C, the cooling rate is controlled at 4~8°C / h, and the stirring rate is controlled at 50~200rpm / min, the quality of the obtained ammonium acetate is good, and the content of metal impurities is lower than 5ppb.
[0044] Comparative Example 1 Based on Example 1, the stirring flow rate during the synthesis in step 1 is 50 r / min, and the rest is the same as Example 1.
[0045] Comparative Example 2 Based on Example 1, the stirring flow rate during the synthesis in step 1 is 300 r / min, and the rest is the same as Example 1.
[0046] Comparative Example 3 Based on Example 2, the flow rate of adding ammonia water in step 1 is 0.2 kg / min, and the rest is the same as Example 2.
[0047] Comparative Example 4 Based on Example 2, the flow rate of adding ammonia water in step 1 is 0.8 kg / min, and the rest is the same as Example 2.
[0048] Comparative Example 5 Based on Example 2, no condensed water cooling is introduced during step 1, and the rest is the same as Example 2.
[0049] Comparative Example 6 Based on Example 3, the mixed solution in step 2 is concentrated under reduced pressure to a concentration of ammonium acetate of 70-74%, and the rest is the same as Example 3.
[0050] Comparative Example 7 Based on Example 3, the mixed solution in step 2 is concentrated under reduced pressure to a concentration of ammonium acetate of 80-85%, and the rest is the same as Example 3.
[0051] Comparative Example 8 Based on Example 1, the crystallization starting temperature in step 3 is 75°C, and the rest is the same as Example 1.
[0052] Comparative Example 9 Based on Example 4, the crystallization starting temperature in step 3 is 55°C, and the rest is the same as Example 4.
[0053] Comparative Example 10 Based on Example 1, the cooling rate of the circulating water in step 3 is 2°C / h, and the rest is the same as Example 1.
[0054] Comparative Example 11 Based on Example 1, the cooling rate of the circulating water in step 3 is 10°C / h, and the rest is the same as Example 1.
[0055] Comparative Example 12 Based on Example 1, the stirring rate during the crystallization process in step 3 is 20 r / min, and the rest is the same as Example 1.
[0056] Comparative Example 13 Based on Example 1, the stirring rate during the crystallization process in step 3 is 300 r / min, and the rest is the same as Example 1.
[0057] It can be seen from the above embodiments and comparative examples that by controlling the reaction conditions and crystallization conditions, the content of the electronic-grade ammonium acetate product obtained by the preparation method of the present invention is greater than 99%, the metal impurity content is less than 5 ppb, and the yield is good. However, under other conditions in the comparative example, the requirements of product content, yield and metal impurity content cannot be met; it can be seen that the present invention provides an ultra-clean and high-purity electronic ammonium acetate product that meets the needs of the IC industry.
[0058] The above embodiments are only preferred technical solutions of the present invention and should not be regarded as limiting the present invention. The protection scope of the present invention shall be the technical solutions recorded in the claims, including equivalent replacement solutions of the technical features in the technical solutions recorded in the claims. That is, equivalent replacement improvements within this scope are also within the protection scope of the present invention.
Claims
1. A process for preparing electronic grade ammonium acetate, characterized in that: The preparation process includes synthesis, crystallization, centrifugal washing and drying, and specifically comprises the following steps: Step 1: Add excess ammonia water into the acetic acid solution to completely neutralize it to obtain a mixed solution of ammonium acetate and ammonia water; Step 2: distilling the mixed solution in step 1 under reduced pressure to remove excess ammonia water and obtain a concentrated solution of a certain concentration; Step 3: crystallizing the concentrated solution of step 2, controlling the crystallization temperature in the system, and obtaining ammonium acetate slurry after cooling and crystallization; Step 4: After centrifugation and washing of the crystal slurry obtained in step 3, a filtrate and ammonium acetate crystals are obtained; Step 5: Drying the ammonium acetate crystals obtained in step 4 to obtain an electronic grade ammonium acetate product.
2. The preparation process according to claim 1, characterized in that: In step 1, the acetic acid used is industrial grade acetic acid with a content greater than 99%; the ammonia water used is industrial grade ammonia water with a concentration of 27% to 29%, and the endpoint pH of the synthesis reaction is 7 to 7.
5.
3. The preparation process according to claim 1, characterized in that: In step 1, the synthesis temperature is controlled to be lower than 40° C. by introducing circulating cooling water into the interlayer of the synthesis reactor.
4. The preparation process according to claim 1, characterized in that: In step 1, the pipe for introducing ammonia water needs to be submerged below the liquid surface of the acetic acid solution. The ammonia water is slowly added to the acetic acid solution and stirred continuously. The stirring speed is 100-200 rpm / min, and the flow rate of the added ammonia water is 0.4-0.5 kg / min.
5. The preparation method according to claim 1, characterized in that: In step 2, the vacuum degree of the reduced pressure concentration is less than -0.08MPa, the concentration temperature is controlled at 40-70°C, and the concentration of ammonium acetate after concentration is 75-80%.
6. The preparation process according to claim 1, characterized in that: In step 3, the starting crystallization temperature of the ammonium acetate is 60-70°C, the ending crystallization temperature is 10-20°C, the temperature for adding the seed crystals is 45-60°C, and the amount of the seed crystals added is 0.5-1% of the mass of the crystallization solution.
7. The preparation process according to claim 1, characterized in that: In step 3, the cooling rate during crystallization of ammonium acetate is 2~10℃ / h, and the stirring speed during crystallization is 50~200 r / min.
8. The preparation process according to claim 1, characterized in that: In step 4, the washing is centrifugal spray washing, the spray flow rate is 0.01~0.05L / s, and the spray time is 10~60s.
9. The preparation process according to claim 1, characterized in that: In step 5, the drying temperature of the ammonium acetate crystals is 45-55° C., and the drying time is 4-12 hours.
10. The preparation process according to any one of claims 1 to 9, characterized in that: The purity of the electronic grade ammonium acetate is greater than 99%, and the metal ion impurities are all less than 5 ppb.