Thin film capable of reducing blue light transmission and preparation method

Through the preparation of the erythromycin film, the blue light absorption capacity of its specific range is used to solve the problems of reduced light transmittance and high cost in the existing anti-blue light technology, and efficient absorption of 400-500nm blue light is achieved, providing economic and environmental protection The solution and maintains good physical and chemical stability.

CN118930986APending Publication Date: 2024-11-12SOUTH CHINA UNIV OF TECH ZHUHAI INST OF MODERN IND INNOVATION +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411183753.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Existing blue light-proof methods such as adding blue light barrier coatings or filters have problems such as decreasing light transmittance, color distortion, high manufacturing costs and complex processes, and broad-spectrum absorbers will affect the transmission of other light.

Method used

Using the bamboo erythromycin film, by combining the bamboo erythromycin with film-forming materials and functional additives, a film with strong blue light absorption capacity and good stability is prepared in a specific range, and fixed to the substrate by solution deposition or spraying. In addition, selective absorption of 400-500nm blue light is achieved.

Benefits of technology

Effectively reduce blue light transmission and provide economical and environmentally friendly solutions. The rosin film is highly specific and efficient for blue light, has good physical and chemical stability, is not easily affected by the environment for long-term use, and is simple in process and low in cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930986A_ABST
    Figure CN118930986A_ABST
Patent Text Reader

Abstract

The invention relates to the field of optical materials and health protection, and discloses a hypocrellin-containing film and a preparation method thereof, which can be applied to reduction of blue light transmission. The thin film is composed of hypocrellin, a film forming material and a fixing base material. The preparation method comprises the following steps: (1) respectively preparing a hypocrellin solution and a membrane material solution; (2) adding the hypocrellin solution into the film-forming material solution, uniformly mixing, and uniformly coating a fixed base material with the obtained mixed solution; and (3) drying the coated base material at a relatively low temperature to form a film. The hypocrellin has relatively strong absorption capability on blue light of 400-500nm, and can effectively reduce blue light transmission, so that eye health is protected. The obtained film is good in visible light permeability and meanwhile has good selective absorption performance on blue light.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a preparation method of a hypocrellin film and application of the film in reducing blue light transmission, belonging to the field of optical biomaterials and health protection. Background Art

[0002] For OLED, AMOLED, LCD and other display screens and other light sources, high-energy short-wave blue light with a wavelength between 400-500nm may cause irreversible damage to human eyes and skin. Long-term exposure to blue light may cause digital eye fatigue and cause oxidative damage to retinal cells, thereby increasing the risk of eye diseases. In addition, some spectra in blue light may cause problems such as dry skin, pigmentation and photoaging.

[0003] Hypocrellin is a lipophilic perylenequinone compound extracted from natural Hypocrellin, which includes Hypocrellin A, B, C and D. The five-ring conjugated system of Hypocrellin gives it excellent photosensitivity, so it is often used in photodynamic therapy. Compared with other photosensitizing compounds, Hypocrellin has low dark toxicity and is degradable. In addition, Hypocrellin can be produced greenly through biological fermentation, avoiding harmful byproducts that may be produced in traditional chemical synthesis processes.

[0004] Most of the current anti-blue light methods rely on adding blue light blocking coatings or filters. Taking glasses as an example, the anti-blue light principle is to coat the lenses with a blue light reflecting film, or add blue light absorbers such as lutein, curcumin, and melanin to the substrate to reduce the damage to the eyes by reflecting or absorbing blue light. However, these methods are often accompanied by problems such as decreased transmittance, color distortion, high manufacturing costs, and complex preparation processes. In addition, the above three pigments have a wide absorption spectrum. While blocking blue light, they will also reduce the transmission of other light, thereby affecting transmittance and color rendering.

[0005] In contrast, as a biosynthesized natural ingredient, the film of hypocrellin has the advantages of good stability, narrow absorption spectrum and green production. Introducing hypocrellin into the field of blue light protection can effectively reduce blue light transmission and provide a more economical and environmentally friendly solution. Summary of the invention

[0006] In view of the problems mentioned in the prior art, the present invention proposes a new type of hypocrellin film, which utilizes the absorption capacity of hypocrellin for blue light in a specific range to prepare an environmentally friendly, stable and transmittance-free blue light-proof film. The film can effectively reduce blue light transmission and provide a more economical and environmentally friendly solution for the field of optical materials and health protection.

[0007] The present invention is achieved through the following technical solutions.

[0008] A film for reducing blue light transmission, characterized in that the film comprises hypocrellin and a film-forming material. Further, the hypocrellin is selected from hypocrellin A, B, C, D or a mixture of any two or more thereof.

[0009] Furthermore, the film-forming material can be a mixture of one or more materials, including but not limited to agarose, polyvinyl alcohol, resin and other inert organic or inorganic materials that can provide similar effects. Furthermore, the film also contains a plasticizer, an ultraviolet absorber or other functional additives to further enhance the film performance.

[0010] Furthermore, the film can be fixed on a substrate, and the substrate includes plastic, acrylic, glass, and resin.

[0011] Furthermore, the thin film can be prepared by solution deposition, spin coating, spray coating, dip coating or chemical vapor deposition.

[0012] Specifically, the method for preparing the film comprises the following steps:

[0013] Step 1) pre-treating the substrate: selecting a substrate, soaking the substrate in an anhydrous ethanol solution, taking it out after soaking, and drying it at room temperature;

[0014] Step 2) preparing a hypocrellin solution and a film-forming material solution: taking hypocrellin, adding it to an anhydrous ethanol solution, filtering after ultrasonic vibration to obtain a hypocrellin-ethanol solution; taking another film-forming material and dissolving it in deionized water to obtain a film-forming material solution;

[0015] Step 3) Film: Mix the hypocrellin-ethanol solution and the film-forming material solution in proportion to obtain a hypocrellin-film solution, then add glycerol and stir at room temperature; apply the stirred hypocrellin-film solution to the substrate described in step 1), and dry the coated substrate to obtain a hypocrellin film. Preferably, the coating method includes solution deposition, spin coating, spray coating, dip coating or chemical vapor deposition.

[0016] Preferably, the method for preparing the film comprises the following steps:

[0017] Step 1) pre-treating the substrate: select a substrate, soak the substrate in an anhydrous ethanol solution for 60-120 minutes, take it out after soaking, and dry it at room temperature;

[0018] Step 2) preparing a hypocrellin solution and a film-forming material solution: taking hypocrellin, adding it to an anhydrous ethanol solution at a mass ratio of 1:3000-4000, and filtering after ultrasonic vibration for 30-60 minutes to obtain a hypocrellin-ethanol solution; taking another film-forming material, dissolving it in deionized water at a mass ratio of 1:50-100 to obtain a film-forming material solution;

[0019] Step 3) Film: Mix the hypocrellin-ethanol solution and the film-forming material solution in proportion to obtain a hypocrellin-film solution containing 10-1000 μg / mL of hypocrellin, then add glycerol with a volume ratio of 0.5-1.0%, and stir at room temperature for 15-30 minutes; apply the stirred hypocrellin-film solution to the substrate described in step 1), and place the coated substrate at 30-40°C and dry for 12-18 hours to obtain a stable and uniform hypocrellin film.

[0020] More specifically, the preparation method comprises the following steps:

[0021] Step 1: Substrate pretreatment.

[0022] Select an inert material with a smooth surface, such as a plastic plate, as the substrate for fixing the film. Soak the substrate in anhydrous ethanol for 60-120 minutes, take it out and place it in a clean and cool place to dry for later use. This step is to remove dust and stains attached to the surface of the substrate to prevent it from affecting the formation of the film.

[0023] Step 2: Preparation of Hypocrellin Solution and Membrane Material Solution

[0024] With anhydrous ethanol or dimethyl sulfoxide as solvent, add crude hypocrellin into the solvent at a mass ratio of 1:3000-4000, perform ultrasonic vibration for 30-60 minutes to dissolve the pigment, and filter to obtain hypocrellin-ethanol solution. The selected solvent must have good hypocrellin solubility and be compatible with the aqueous membrane solution, otherwise hypocrellin will not be evenly distributed in the membrane material.

[0025] Take another suitable solid substrate powder, dissolve it in deionized water at a mass ratio of 1:50-100 to prepare a membrane material solution.

[0026] Step 3: Thin film.

[0027] Mix the hypocrellin solution and the membrane material solution in proportion to obtain a hypocrellin-membrane solution containing 0-1000 μg / mL hypocrellin, and stir at room temperature for 15-30 minutes. Apply the hypocrellin-membrane solution after stirring to the substrate described in step 1, and the coating method includes but is not limited to solution deposition, spin coating, spray coating, dip coating or chemical vapor deposition. Place the coated substrate at 30-40°C and dry for 12-18 hours to obtain a stable and uniform hypocrellin film.

[0028] This step may vary depending on the composition of the selected membrane material. For example, when the membrane material is polyvinyl alcohol, 0.5%-1% by volume of glycerol may be added. Glycerol can act as a plasticizer to enhance the flexibility and tensile strength of the membrane.

[0029] Step 4: Optical performance test. Use a spectrometer to test the blue light absorption capacity of the bamboo red fungus film in step 3. The detection light source can be a white light source such as LED, LCD or sunlight, or a blue light source. Analyze the spectral data, calculate the blue light absorption rate of the film in the wavelength range of 400-500nm, and evaluate its anti-blue light effect. The calculation formula is: relative absorption rate of blue light = (1-S HA / S CK )*100%, where S HA and S CK They are the spectral areas of the hypocrellin coating and the blank coating within a specific wavelength range, respectively.

[0030] The beneficial effects achieved by the present invention mainly include but are not limited to the following aspects:

[0031] The hypocrellin film of the present invention has high specificity and high efficiency in absorbing blue light, wherein the hypocrellin can selectively absorb blue light with a wavelength between 400-500nm, thereby effectively reducing the impact of blue light on human eyes and skin. In addition, the film has good physical and chemical stability, can maintain the anti-blue light effect in long-term use, and is not easily affected by the environment. The hypocrellin film has the characteristics of simple manufacturing process and low cost, so that it has a wider application prospect. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Attached Figure 1 Schematic diagram of the structural formula of hypocrellin, wherein a to d are the structural formulas of hypocrellin A, hypocrellin B, hypocrellin C and hypocrellin D respectively;

[0033] Attached Figure 2 Spectra of the films with different contents of hypocrellin prepared in Example 1 of the present invention under 300 Lux LCD;

[0034] Attached Figure 3 This is a spectrum diagram of the thin film with different contents of hypocrellin prepared in Example 2 of the present invention under 1200 Lux blue light. DETAILED DESCRIPTION

[0035] This section will describe the technical solutions in the embodiments of the present invention in detail. It should be understood that the embodiments are only used to illustrate the present invention and are not intended to limit the scope of the present invention. Based on these embodiments, those skilled in the art can understand and implement other embodiments without performing creative work, and these embodiments are all within the scope of protection of the present invention. In the embodiments of the present invention, unless otherwise stated, the experimental steps are routine operations, and all reagents can be purchased from the market.

[0036] Example 1

[0037] Preparation of hypocrellin A thin film based on plastic substrate and its blue light absorption effect under LCD.

[0038] Soak a circular plastic substrate with a diameter of 60 mm in anhydrous ethanol for 60-120 minutes, then take it out and place it in a clean and cool place to dry for use. Accurately weigh 15 mg of cypermethrin A and dissolve it in 40 mL of anhydrous ethanol, and ultrasonically vibrate it in a closed container for 60 minutes to obtain a cypermethrin A-ethanol solution. Take another beaker, add accurately weighed 0.45 g of agarose and 30 mL of deionized water, and microwave heating for 1 minute to fully dissolve the agarose to obtain an agarose solution. Take multiple 10 mL centrifuge tubes, add 0, 600, 1200, and 1800 μL of cypermethrin A-ethanol solution, respectively, and then add agarose solution to 6 mL, and quickly shake it evenly. Take 5 mL of the mixed solution and evenly apply it on the plastic substrate. After cooling and forming at room temperature, place it at 37 ° C and dry it for 15 hours to obtain cypermethrin A films with different contents.

[0039] The above-prepared hypocrellin A film was placed under an LCD display screen, and the film's absorption effect on blue light was detected by a spectrometer, and the degree of blue light absorption of the film was calculated by the peak area at 414-484nm. Figure 2 The calculation results in Table 1 show that the hypocrellin A film based on plastic substrate has a significant absorption effect on the blue light in the LCD display, and is positively correlated with the hypocrellin concentration in the film. When the hypocrellin content is 2.50%, the film has a 35.70% absorption rate for 414-484nm blue light, while the absorption rate for 583-800nm ​​red light is only 8.93%.

[0040] Table 1

[0041]

[0042] Example 2

[0043] Preparation of cypermethrin B film based on plastic substrate and its blue light absorption effect in the 430-580nm band.

[0044] Soak a circular plastic substrate with a diameter of 60 mm in anhydrous ethanol for 60-120 minutes, then take it out and place it in a clean and cool place to dry for use. Accurately weigh 15 mg of cypermethrin B and dissolve it in 40 mL of anhydrous ethanol, and ultrasonically vibrate it in a closed container for 60 minutes to obtain a cypermethrin B-ethanol solution. Take another beaker, add accurately weighed 0.45 g of agarose and 30 mL of deionized water, and microwave heating for 1 minute to fully dissolve the agarose to obtain an agarose solution. Take multiple 10 mL centrifuge tubes, add 0, 600, 1200, and 1800 μL of cypermethrin B-ethanol solution, respectively, and then add agarose solution to 6 mL, and quickly shake it evenly. Take 5 mL of the mixed solution and evenly apply it on the plastic substrate. After cooling and forming at room temperature, place it at 37 ° C and dry it for 15 hours to obtain cypermethrin B films with different contents.

[0045] The above-prepared hypocrellin B film was placed under a 430-583nm blue light source, and the absorption effect of the film on blue light was detected by a spectrometer, and the absorption degree of the film on blue light was calculated based on the peak area at 430-583nm. Figure 3 Calculations show that in Table 2, the film's ability to absorb blue light increases with the increase in the concentration of hypocrellin. When the content of hypocrellin B is 2.50%, the film's absorption rate for 430-583nm blue light is 40.99%.

[0046] Table 2

[0047]

[0048] Although the above describes the specific implementation of the present invention in combination with the embodiments, it is not intended to limit the scope of protection of the present invention. Those skilled in the art should understand that it should be clear to those skilled in the art that these modifications or improvements made without departing from the spirit of the present invention all fall within the scope of protection of the present invention.

Claims

1. A film for reducing blue light transmission, characterized in that: The film comprises hypocrellin and a film-forming material.

2. The film according to claim 1, characterized in that The hypocrellin is selected from hypocrellin A, B, C, D or a mixture of any two or more thereof.

3. The film according to any one of claims 1-2, characterized in that: The film-forming material can be a mixture of one or more materials, and the film-forming material includes but is not limited to agarose, polyvinyl alcohol, resin and other inert organic or inorganic materials that can provide similar effects.

4. The film according to any one of claims 1 to 3, characterized in that: The film may also contain a plasticizer, an ultraviolet absorber or other functional additives to further enhance the film properties.

5. The film according to any one of claims 1 to 4, characterized in that: The film can be fixed on a substrate, which includes plastic, acrylic, glass, and resin.

6. The film according to any one of claims 1 to 5, characterized in that: The thin film can be prepared by solution deposition, spin coating, spray coating, dip coating or chemical vapor deposition.

7. The film according to any one of claims 1 to 6, characterized in that: The method for preparing the film comprises the following steps: Step 1) pre-treating the substrate: selecting a substrate, soaking the substrate in an anhydrous ethanol solution, taking it out after soaking, and drying it at room temperature; Step 2) preparing a hypocrellin solution and a film-forming material solution: taking hypocrellin, adding it to an anhydrous ethanol solution, filtering after ultrasonic vibration to obtain a hypocrellin-ethanol solution; taking another film-forming material and dissolving it in deionized water to obtain a film-forming material solution; Step 3) Film: Mix the hypocrellin-ethanol solution and the film-forming material solution in proportion to obtain a hypocrellin-film solution, then add glycerol and stir at room temperature; apply the stirred hypocrellin-film solution to the substrate described in step 1), and dry the coated substrate to obtain a hypocrellin film.

8. The film according to claim 7, characterized in that The coating method includes solution deposition, spin coating, spray coating, dip coating or chemical vapor deposition.

9. The film according to claim 7, characterized in that The method for preparing the film comprises the following steps: Step 1) pre-treating the substrate: select a substrate, soak the substrate in an anhydrous ethanol solution for 60-120 minutes, take it out after soaking, and dry it at room temperature; Step 2) preparing a hypocrellin solution and a film-forming material solution: taking hypocrellin, adding it to an anhydrous ethanol solution at a mass ratio of 1:3000-4000, and filtering after ultrasonic vibration for 30-60 minutes to obtain a hypocrellin-ethanol solution; taking another film-forming material, dissolving it in deionized water at a mass ratio of 1:50-100 to obtain a film-forming material solution; Step 3) Film: Mix the hypocrellin-ethanol solution and the film-forming material solution in proportion to obtain a hypocrellin-film solution containing 10-1000 μg / mL of hypocrellin, then add glycerol with a volume ratio of 0.5-1.0%, and stir at room temperature for 15-30 minutes; apply the stirred hypocrellin-film solution to the substrate described in step 1), and place the coated substrate at 30-40°C and dry for 12-18 hours to obtain a stable and uniform hypocrellin film.

10. Use of the film according to any one of claims 1 to 9, characterized in that: The film reduces the transmission intensity of blue light.

Citation Information

Cited By