UV printing ink applied to glass laser cutting process protection and preparation method thereof

By optimizing the resin system of UV ink, combined with modified epoxy acrylate, water-soluble acrylate and hydroxyacrylate monomers and other raw materials, the problem of insufficient flatness and light transmittance of traditional inks when laser cutting glass is solved, and high Adhesion and rapid removal avoid glass edge cracks and improve cutting accuracy and efficiency.

CN118931253AInactive Publication Date: 2024-11-12HUIZHOU BESTER CHEM CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411049932.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the existing laser cutting glass process, traditional UV protection inks are difficult to meet the requirements of high light transmittance and flatness after cutting. At the same time, strong acidic or alkaline defiling agents may affect the strength of the glass, resulting in edge cracks.

Method used

Use modified epoxy acrylate, water-soluble acrylate and hydroxyacrylate monomers and other raw materials, combined with photoinitiators, defoamers and leveling agents, optimize the resin system, and control the addition amount and viscosity of modified epoxy acrylate. , hydroxyacrylate monomer and epoxy silane coupling agent are introduced to ensure high adhesion, flatness and rapid removal of the ink layer.

Benefits of technology

The high light transmittance and flatness of the ink layer after curing is achieved, which avoids the damage to the glass by strong acid and alkali defiling, improves the accuracy and efficiency of laser cutting, and is suitable for the industrial production of high-end glass products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004974625200000041
    Figure BDA0004974625200000041
  • Figure BDA0004974625200000051
    Figure BDA0004974625200000051
  • Figure BDA0004974625200000061
    Figure BDA0004974625200000061
Patent Text Reader

Abstract

The invention relates to the technical field of C09D11 / 00, in particular to UV printing ink applied to glass laser cutting process protection and a preparation method of the UV printing ink. The preparation raw materials at least comprise 20-40 parts of modified epoxy acrylate, 30-50 parts of water-soluble acrylate, 20-25 parts of a hydroxyl acrylate monomer, 1-5 parts of a photoinitiator, 0.1-2 parts of a defoaming agent, 0.01-0.1 part of a flatting agent and 0.1-3 parts of an adherence promoter, the flatness and light transmittance of a cured ink layer are guaranteed at the same time, rapid film stripping is achieved under the condition that the strength of glass is not affected, and the service life of the film is prolonged. And the actual application requirement of the laser cutting process is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of C09D11 / 00, and in particular to a UV ink used for protecting a glass laser cutting process and a preparation method thereof. Background Art

[0002] Laser cutting is a high-precision cutting technology that uses laser beams to heat and evaporate materials, thereby achieving precise cutting of materials. Compared with traditional CNC cutting (CNC), laser cutting has the advantages of high precision, high speed, and no need for secondary processing. Therefore, it has been widely used in the industrial field and has a good market development trend. In the field of mobile phones and tablets, high-end mobile phone series of well-known brands such as Apple, Samsung, and Huawei have increasingly higher requirements for the precision of the size of the front and back covers of the glass. The traditional CNC process is limited by efficiency and precision and is difficult to meet. Therefore, major mobile phone brands have been developing and deploying laser cutting technology.

[0003] In the process of laser cutting glass cover plates, in order to prevent scratches during the process, a temporary protective oil will be applied on both sides of the glass before cutting. This protective oil adopts a roller coating process with ultraviolet UV curing. The cured ink layer needs to have good flatness, high transmittance, weak acid or neutral solution removal and other characteristics, so as to maximize the laser cutting process yield. Therefore, the present invention intends to develop a temporary protective ink suitable for laser cutting process molding, which protects against scratches and edge collapse during the process, and is used to improve the efficiency of high-end cover glass laser cutting, which therefore puts higher requirements on the protective oil. The Chinese patent (publication number CN 114231080A) discloses a high-transmittance UV roller coating protective ink. By optimizing the ink formula system, the transmittance of the obtained ink layer can reach 88.2%, but the flatness of the ink layer needs to be further improved, and the subsequent film removal needs to be carried out in a 5% sodium hydroxide solution at a temperature of 80°C, which may have an adverse effect on the strength of the glass. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a UV ink for protecting the glass laser cutting process, while ensuring the flatness and light transmittance of the ink layer after curing, and realizing rapid film fading without affecting the strength of the glass, thereby meeting the actual application requirements of the laser cutting process.

[0005] The present invention provides a UV ink for protecting a glass laser cutting process. The raw materials for preparing the UV ink include at least 20-40 parts of modified epoxy acrylate, 30-50 parts of water-soluble acrylate, 20-25 parts of hydroxy acrylate monomer, 1-5 parts of photoinitiator, 0.1-2 parts of defoamer, 0.01-0.1 parts of leveling agent and 0.1-3 parts of adhesion agent, by weight.

[0006] As a preferred technical solution, the hydroxy acrylate monomer is selected from at least one of 2-hydroxyethyl acrylate, 2,3-dihydroxypropyl acrylate, hydroxypropyl acrylate, 2-hydroxypropyl acrylate, and hydroxyethyl methacrylate, preferably hydroxyethyl methacrylate (HEMA).

[0007] As a preferred technical solution, the modified epoxy acrylate is at least one of modified bisphenol A epoxy acrylate and fatty acid modified epoxy acrylate, preferably modified bisphenol A epoxy acrylate.

[0008] As a preferred technical solution, the viscosity of the modified epoxy acrylate at 60° C. is 3000-8000 cps, preferably 3000-6200 cps.

[0009] As a preferred technical solution, the water-soluble acrylate is a water-soluble polyester acrylate, and the viscosity of the water-soluble polyester acrylate is 1000-5000 cps, preferably 1000-3000 cps.

[0010] Preferably, the functional group number (theoretical value) of the water-soluble polyester acrylate is 2-8, preferably 2.

[0011] As a preferred technical solution, based on the total weight of raw materials for preparing UV ink, the added amount of the modified epoxy acrylate is ≥25%, preferably 30-40%.

[0012] The ink provided by the present invention needs to be used for temporary process protection of high-end cover glass laser cutting technology, so it is particularly necessary to ensure the flatness of the ink layer after curing, the light transmittance of the ink layer, and the ease of removal. During the exploration process, it was found that by optimizing the system to be a resin system of modified bisphenol A epoxy acrylate and water-soluble polyester acrylate, and controlling the addition amount of modified epoxy acrylate to be ≥25%, the provided UV ink has high adhesion to the glass surface after curing, and the ink will not fall off during the laser cutting process. The cured ink layer can be removed using a weak acid deinking agent, avoiding strong acid and strong alkali solutions from affecting the strength of the glass, resulting in cracks on the edge of the glass after laser cutting.

[0013] The present invention introduces hydroxy acrylate monomers so that the fluidity of the ink provided meets the requirements of the subsequent roller coating process, further improves the adhesion of the ink layer, and the ink layer after curing has good flatness, with an RA value of ≤0.5. In particular, when 20-25 parts of hydroxyethyl methacrylate are introduced, the ink layer obtained after curing has the best flatness, with an RA value of up to 0.3.

[0014] As a preferred technical solution, the photoinitiator is selected from at least one of the photoinitiator 184, the photoinitiator TPO, and the photoinitiator 1173; preferably, it is a combination of the photoinitiator 184, the photoinitiator TPO, and the photoinitiator 1173. Preferably, the mass ratio of the photoinitiator 184, the photoinitiator TPO, and the photoinitiator 1173 is (2-4): 1: 1. The ink system provided by the present invention simultaneously introduces the photoinitiator 184, the photoinitiator TPO, and the photoinitiator 1173 to initiate polymerization, so that the ink layer is quickly cured.

[0015] As a preferred technical solution, the defoamer is a polymer defoamer that does not contain silicone, preferably Tego 920 defoamer or BYK 011 defoamer.

[0016] As a preferred technical solution, the leveling agent is a polyether siloxane copolymer, preferably at least one of Digo 450 leveling agent or Digo 100 leveling agent, preferably Digo 450 leveling agent.

[0017] The present invention optimizes the combination of defoaming agent and leveling agent, especially introduces Tego 920 defoaming agent or BYK 011 defoaming agent in combination with Tego 450 leveling agent or Tego 100 leveling agent, so as to ensure the flatness and light transmittance of the ink layer after curing.

[0018] As a preferred technical solution, the adhesive is a silane coupling agent containing an epoxy group, preferably γ-glycidyloxypropyltrimethoxysilane and / or γ-(2,3-epoxypropyloxy)propyltriethoxysilane, and most preferably γ-glycidyloxypropyltrimethoxysilane.

[0019] In addition, based on the preferred resin system, the present invention further introduces a silane coupling agent containing an epoxy group, especially γ-glycidyloxypropyltrimethoxysilane, to ensure that the adhesion of the ink layer on the glass surface reaches 5B, meet the laser cutting requirements, and improve the yield of glass products.

[0020] The UV ink provided by the present invention has a light transmittance of up to 88%, while traditional UV roller-coated protective ink can only reach 80%, which greatly improves the light transmittance and makes the laser cutting size more precise. The roller coating process is combined with UV curing, which has high construction efficiency and can be operated by automated lines, making it easy to realize large-scale industrial production and promotion.

[0021] On the other hand, the present invention provides a method for preparing UV ink for glass laser cutting process protection, which comprises at least the following steps: adding modified epoxy acrylate, water-soluble acrylate, hydroxy acrylate monomer, photoinitiator, defoamer, leveling agent and adhesion agent into a container in sequence under stirring, stirring and dispersing the materials again after they are completely added, and filtering to obtain the ink.

[0022] Beneficial Effects

[0023] 1. The present invention provides a UV ink for protecting the glass laser cutting process, which ensures the flatness and light transmittance of the ink layer after curing, realizes rapid film fading without affecting the strength of the glass, and meets the actual application requirements of the laser cutting process.

[0024] 2. The present invention optimizes the system to be a resin system of modified bisphenol A epoxy acrylate and water-soluble polyester acrylate, and controls the addition amount of modified epoxy acrylate to be ≥25%, so that after the provided UV ink is cured, the adhesion on the glass surface is high, the ink will not fall off during the laser cutting process, and the cured ink layer can be removed by a weak acid deinking agent, thereby avoiding the strong acid and strong alkali solution affecting the strength of the glass, resulting in cracks on the edge of the glass after laser cutting.

[0025] 3. The present invention introduces hydroxy acrylate monomers to ensure that the fluidity of the ink provided meets the requirements of the subsequent roller coating process, further improves the adhesion of the ink layer, and the ink layer has good flatness after curing, with an RA value of ≤0.5. In particular, when 20-25 parts of hydroxyethyl methacrylate are introduced, the ink layer has the best flatness after curing, and the RA value can reach 0.3.

[0026] 4. The present invention optimizes the combination of defoaming agent and leveling agent, especially introduces Tego 920 defoaming agent or BYK 011 defoaming agent in combination with Tego 450 leveling agent or Tego 100 leveling agent, so as to ensure the flatness and light transmittance of the ink layer after curing.

[0027] 5. Based on the preferred resin system, the present invention further introduces a silane coupling agent containing an epoxy group, especially γ-glycidyloxypropyltrimethoxysilane, to ensure that the adhesion of the ink layer on the glass surface reaches 5B, meet the requirements of laser cutting, and improve the yield of glass products.

[0028] 6. The UV ink provided by the present invention has a light transmittance of up to 88%, while traditional UV roller-coated protective ink can only reach 80%, which greatly improves the light transmittance and makes the laser cutting size more precise. The roller coating process is combined with UV curing, which has high construction efficiency and can be operated by automated lines, making it easy to realize large-scale industrial production and promotion. DETAILED DESCRIPTION

[0029] Examples 1-6

[0030] Embodiments 1-6 of the present invention provide a UV ink for protection in a glass laser cutting process. The raw materials for its preparation are shown in Table 1 in parts by weight.

[0031] Table 1

[0032]

[0033]

[0034] On the other hand, Examples 1-6 of the present invention provide a method for preparing UV ink for glass laser cutting process protection, comprising the following steps: adding modified epoxy acrylate, water-soluble acrylate, hydroxy acrylate monomer, photoinitiator, defoamer, leveling agent, and adhesion agent into a container in sequence at a dispersion speed of 300 rpm; after the materials are completely added, stirring and dispersing at a dispersion speed of 300 rpm for 60 minutes, and filtering through a 200-mesh filter to obtain the ink.

[0035] Performance Testing

[0036] The UV ink provided in the embodiment and the commercially available UV protective ink (Rongda photosensitive TX-1108) were respectively roll-coated onto the surface of the glass plate, and after UV curing, a (18±2um) thick ink layer was obtained. The ink layer was subjected to the performance test shown in Table 2. The test results are shown in Table 2.

[0037] (1) The deinking time test method is as follows: Examples 1-6 use weak acid solution (PH=3) for deinking at 50°C, and the control example uses 5% NaOH aqueous solution for deinking at 80°C, and the time required for complete deinking is tested.

[0038] (2) The surface hardness test method is as follows: GB / T 6739-1996 Paints and varnishes - Determination of film hardness by pencil method.

[0039] (3) The test method for glass surface adhesion is as follows: Use a sharp blade to draw a 2mm×2mm grid in the designated area, and each line penetrates the ink to the substrate. Use a dust-free cloth or brush to clean the surface debris, use Japanese plant-based adhesive tape to stick the small grid and flatten it, squeeze out the bubbles, and press statically for more than 5 seconds. The product remains motionless, and the tape is quickly pulled up vertically to observe the peeling of the paint film on the adhesive tape and the product. (5B-the edge of the incision is smooth, and there is no peeling at the edge of the grid; 4B-there is small peeling at the intersection of the incision, and the actual damage in the grid area does not exceed 5%; 3B-there is peeling at the edge and / or intersection of the incision, and its area is greater than 5% but less than 15%; 2B-there is partial peeling or large peeling along the edge of the incision, and / or part of the grid is peeled off in whole pieces, and the peeled area exceeds 15% but less than 35%; 1B-there is partial peeling or large peeling along the edge of the incision, and / or part of the grid is peeled off in whole pieces, and the peeled area exceeds 35% but less than 65%; 0B-there is partial peeling or large peeling along the edge of the incision, and / or part of the grid is peeled off in whole pieces, and the peeled area exceeds 65%).

[0040] (3) The light transmittance test method is: use an IR ink hole transmittance tester for testing, and set the wavelength to 550nm.

[0041] (4) The surface roughness test method is: using a surface roughness tester for testing.

[0042] Table 2

[0043]

Claims

1. A UV ink for protecting glass laser cutting process, characterized in that: The raw materials for its preparation include at least 20-40 parts of modified epoxy acrylate, 30-50 parts of water-soluble acrylate, 20-25 parts of hydroxy acrylate monomer, 1-5 parts of photoinitiator, 0.1-2 parts of defoamer, 0.01-0.1 parts of leveling agent and 0.1-3 parts of adhesion agent by weight.

2. The UV ink for glass laser cutting process protection according to claim 1 is characterized in that: The hydroxy acrylate monomer is selected from at least one of 2-hydroxyethyl acrylate, 2,3-dihydroxypropyl acrylate, hydroxypropyl acrylate, 2-hydroxypropyl acrylate, and hydroxyethyl methacrylate.

3. The UV ink for glass laser cutting process protection according to claim 1 or 2, characterized in that: The modified epoxy acrylate is at least one of modified bisphenol A epoxy acrylate and fatty acid modified epoxy acrylate; preferably, the water-soluble acrylate is water-soluble polyester acrylate.

4. The UV ink for glass laser cutting process protection according to claim 3 is characterized in that: The modified epoxy acrylate has a viscosity of 3000-8000 cps at 60°C.

5. The UV ink for glass laser cutting process protection according to claim 4 is characterized in that: Based on the total weight of raw materials for preparing UV ink, the added amount of the modified epoxy acrylate is ≥25%.

6. The UV ink for glass laser cutting process protection according to claim 5, characterized in that: The photoinitiator is selected from at least one of photoinitiator 184, photoinitiator TPO, and photoinitiator 1173.

7. The UV ink for glass laser cutting process protection according to claim 5, characterized in that: The defoamer is a polymer-type defoamer that does not contain silicone.

8. The UV ink for glass laser cutting process protection according to claim 7, characterized in that: The leveling agent is a polyether siloxane copolymer.

9. The UV ink for glass laser cutting process protection according to claim 8, characterized in that: The adhesive agent is a silane coupling agent containing an epoxy group.

10. A method for preparing UV ink for glass laser cutting process protection according to any one of claims 1 to 9, characterized in that: The method comprises at least the following steps: adding modified epoxy acrylate, water-soluble acrylate, hydroxy acrylate monomer, photoinitiator, defoamer, leveling agent and adhesion agent into a container in sequence under stirring, stirring and dispersing the materials again after they are completely added, and filtering to obtain the product.

Citation Information

Patent Citations

  • Ultraviolet-curable acid-resistant glass protection ink and preparation method thereof

    CN105968938A

  • UV-curing glass protecting ink with fragment stripping and preparation method thereof

    CN107298891A

  • UV protecting printing ink, glass substrate and water cutting method of substrate

    CN109777191A

  • Ultraviolet curing ink and application thereof

    CN111748236A

  • High-transmittance UV roller coating protective ink and preparation method thereof

    CN114231080A