Double-sided asynchronous thermal diffusion method and device for nickel pre-plated steel strip

By using double-sided asynchronous thermal diffusion method in pre-plated nickel steel strips, a temperature gradient is formed and heat treatment is optimized, the problem of insufficient bonding force of the iron-nickel diffusion layer is solved, corrosion resistance and safety are improved, and "iron leakage" is avoided Phenomenon.

CN118932165APending Publication Date: 2024-11-12HUBEI ENG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411015514.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing heat treatment technology can easily lead to the iron-nickel diffusion layer in pre-nickel steel strips, resulting in the problem of the nickel-plated layer being disconnected or "iron leakage", especially when the double-sided non-equal thickness is not guaranteed. Force and corrosion resistance.

Method used

The double-sided asynchronous heat diffusion method of pre-plating steel belt is adopted to form a temperature gradient through single-sided preheating treatment, and then the overall heat treatment is carried out in the heating furnace to form an iron-nickel diffusion layer with significant differences, and the heat treatment environment and parameters are optimized to enhance the binding force. .

Benefits of technology

It effectively improves the corrosion resistance and use safety of pre-plated nickel steel strips, avoids the "iron leakage" phenomenon, ensures stronger bonding force of the iron-nickel diffusion layer, and improves the service performance of the battery case.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118932165A_ABST
    Figure CN118932165A_ABST
Patent Text Reader

Abstract

The invention discloses a double-sided asynchronous thermal diffusion method for a pre-nickel-plated steel strip. The method comprises the following steps: S1, mounting and preparing the pre-nickel-plated steel strip with two unequal-thickness surfaces; s2, single-face preheating treatment is conducted on the nickel pre-plated steel strip with the two faces unequal in thickness; s3, carrying out heat diffusion treatment on the pre-nickel-plated steel strip with two unequal-thickness surfaces; and S4, cooling and rolling of the double-sided unequal-thickness pre-nickel-plated steel strip. The invention further discloses a pre-nickel-plated steel strip double-face asynchronous heat diffusion device which comprises a pre-nickel-plated steel strip and further comprises an uncoiling mechanism, a preheating box, a heating furnace, an exhaust box, a cooling box and a coiling mechanism which are sequentially distributed. The device further comprises a pressure regulating mechanism. According to the method, the single-face preheating treatment and the overall heat treatment process are conducted on the double-face unequal-thickness pre-nickel-plated steel strip, iron-nickel diffusion layers with remarkable difference are formed on the double faces of the steel strip, the corrosion resistance of the pre-nickel-plated steel strip is effectively improved, and the use safety and the service performance of a pre-nickel-plated product are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of pre-nickel-plated materials, in particular to a method and a device for double-sided asynchronous thermal diffusion of a pre-nickel-plated steel strip. Background Art

[0002] With the rapid development of the new energy vehicle industry, the demand for high-performance batteries is also growing. Pre-nickel-plated steel strips have now become the preferred structural material for cylindrical battery shells, especially the 48 series large cylindrical batteries. During the stamping process of the pre-nickel-plated steel plate, the steel strip will undergo huge plastic deformation, and strong friction will occur between the stamping die, which can easily cause the nickel plating on the steel strip to crack or detach. Due to the complexity of the battery working environment, including temperature changes, chemical corrosion and other factors, the corrosion process of the steel strip may be accelerated, thereby affecting the safety and stability of the battery. Therefore, the use of heat treatment after pre-nickel plating is an effective way to enhance the bonding strength between the nickel plating layer and the steel strip, which can improve the service performance of the steel shell.

[0003] In the existing heat treatment technology, if the heat treatment temperature, time and heating / cooling methods are not well controlled, the iron-nickel diffusion layer is prone to be too thin or too thick, resulting in insufficient bonding strength, and then the nickel plating layer detaches or "iron leaks". Especially when the pre-nickel plating thickness on both sides of the steel plate is very different, the iron-nickel diffusion layer on one side is not effectively formed, while the "iron leak" problem has already occurred on the other side. The traditional tunnel resistance furnace heating method is also difficult to avoid the occurrence of the above problems. Summary of the invention

[0004] The present invention provides a method and device for double-sided asynchronous thermal diffusion of a pre-nickel-plated steel strip, which can effectively improve the corrosion resistance of double-sided non-uniform thickness pre-plated steel strips, and can solve at least one of the above-mentioned technical problems.

[0005] In order to solve the above technical problems, the present invention adopts the following technical solutions:

[0006] A method for double-sided asynchronous thermal diffusion of a pre-nickel-plated steel strip comprises the following steps:

[0007] S1: Installation and preparation of double-sided pre-nickel-plated steel strips with unequal thickness: Wind the double-sided pre-nickel-plated steel strips with unequal thickness on the unwinding mechanism, distinguish between thick and thin sides, and ensure that the thin side of the pre-nickel-plated steel strips unwinding and stretching along the unwinding direction faces the condensation pipe in the preheating box, and the thick side faces the gas guide plate in the preheating box;

[0008] S2: Single-sided preheating treatment of pre-nickel-plated steel strip with non-uniform thickness on both sides: the free end of the pre-nickel-plated steel strip after unwinding passes into the preheating box, and the air inlet channel of the preheating box passes high-temperature gas to the thick side of the pre-nickel-plated steel strip via the gas guide plate. The thin side of the pre-nickel-plated steel strip is pressed against the condensation pipe under the pressure of the pressure regulating mechanism, and the thin side of the pre-nickel-plated steel strip is cooled and the thick side is heated, forming a temperature gradient in the plate;

[0009] S3: Thermal diffusion treatment of pre-nickel-plated steel strip with non-uniform thickness on both sides: the free end of the pre-nickel-plated steel strip after single-side preheating is passed through the preheating box into the heating furnace, and both sides are heated by the heating tube, so that diffusion layers are quickly formed on both sides of the plate;

[0010] S4: Cooling and winding of double-sided pre-nickel-plated steel strip with non-uniform thickness: the free end of the pre-nickel-plated steel strip after thermal diffusion treatment passes through the exhaust box and the cooling box in sequence from the heating furnace, and the mixed gas after passing through the preheating box and the multiple heating furnaces is discharged through the exhaust channel of the exhaust box, and the cooling box introduces cooling gas to prevent oxidation to the pre-nickel-plated steel strip through the cooling gas channel. The free end of the pre-nickel-plated steel strip after cooling treatment is connected to the winding mechanism, and the winding mechanism rotates the pre-nickel-plated steel strip along the winding direction to wind it up.

[0011] Further, in S1, the unwinding speed of the unwinding mechanism and the winding speed of the winding mechanism are adjusted according to the distance between them and are always equal;

[0012] In S2, the flow rate of the high-temperature gas introduced into the air inlet channel is controllable, the flow rate of the condensate introduced into the condensation pipeline is controllable, and the pressure of the pre-nickel-plated steel strip pressed by the pressure regulating mechanism is adjustable and monitored in real time by the pressure sensor;

[0013] In S3, the heating temperature in the heating furnace is controllable, and the speed at which the pre-nickel-plated steel strip travels in the heating furnace is adjustable;

[0014] In S4, the exhaust speed of the exhaust channel and the intake speed of the intake channel are both controllable and always equal, the flow rate of the cooling gas flowing into the cooling gas channel is controllable, and the flow rate of the cooling gas is positively correlated with the rewinding speed of the unwinding mechanism or the rewinding mechanism.

[0015] A double-sided asynchronous thermal diffusion device for a pre-nickel-plated steel strip, suitable for the double-sided asynchronous thermal diffusion method for a pre-nickel-plated steel strip, comprises a pre-nickel-plated steel strip, and also comprises an unwinding mechanism, a preheating box, a heating furnace, an exhaust box, a cooling box and a winding mechanism which are sequentially distributed;

[0016] The pre-nickel-plated steel strip is a double-sided non-uniform thickness steel strip, with a thick side and a thin side, one side being a thick side and the other side being a thin side, and is wound on the unwinding mechanism, and after the free end of the pre-nickel-plated steel strip is drawn out, it passes through the preheating box, the heating furnace, the exhaust box and the cooling box in sequence, and enters the winding mechanism;

[0017] Condensation pipes and gas guide plates are arranged horizontally and in parallel with each other inside the preheating box, condensate liquid flows in the condensation pipe, the air inlet channel of the preheating box points to the gas guide plate, and high-temperature gas is introduced, the free end of the pre-nickel-plated steel strip passes horizontally between the condensation pipe and the gas guide plate, the thin side faces the condensation pipe, and the thick side faces the gas guide plate, the pre-nickel-plated steel strip forms a temperature gradient in the preheating box;

[0018] It also includes a pressure regulating mechanism, which is used to compress the pre-nickel-plated steel strip and fit it to the condensation pipe.

[0019] Furthermore, the pressure regulating mechanism includes a support seat, a motor, a coupling, a screw rod, a guide column, a bracket and a roller shaft;

[0020] The motor is mounted on the support seat, and the output power shaft of the motor is fixed to the screw via the coupling. The screw passes through the bottom of the bracket vertically and in the center, and is threadedly engaged with the bracket. There are multiple guide columns, which are distributed in a ring shape on the support seat with the screw as the center, and vertically pass through the bottom of the bracket. The roller is horizontally rotatably mounted on the top of the bracket, and the bracket has a movement stroke for driving the roller to move up and down along the screw. The roller is used to press and fit the pre-nickel-plated steel strip to the condensation pipe, and a pressure sensor for real-time pressure measurement is installed on the roller.

[0021] Furthermore, there are two pressure regulating mechanisms, which are respectively installed at the inlet end of the preheating box and the outlet end of the exhaust box.

[0022] Furthermore, the heating furnace has multiple furnace walls, all of which are made of thermal insulation material, are connected to each other one by one, and are located between the preheating box and the exhaust box. Two rows of heating tubes are installed at upper and lower intervals inside the heating furnace. The pre-nickel-plated steel strip passes between the two rows of heating tubes, and an electric control box electrically connected to the heating tubes is installed on the heating furnace.

[0023] Furthermore, an exhaust channel is provided on the exhaust box, and the exhaust channel is used to discharge the mixed gas after passing through the preheating box and the multiple heating furnaces. The exhaust channel is connected to an exhaust pump, and the air intake channel is connected to an air intake pump. The exhaust speed of the exhaust pump and the air intake speed of the air intake pump are both controllable and always equal.

[0024] Furthermore, a cooling gas channel is provided on the cooling box, and the cooling gas channel is used to introduce cooling gas for preventing oxidation of the pre-nickel-plated steel strip, and the flow rate of the cooling gas is controllable.

[0025] Furthermore, the inlet / outlet ends of the preheating box, the inlet / outlet ends of the heating furnace, the inlet / outlet ends of the exhaust box and the inlet / outlet ends of the cooling box are all at the same horizontal height, and the pre-nickel-plated steel strip horizontally passes through the preheating box, multiple heating furnaces, the exhaust box and the cooling box in sequence.

[0026] Furthermore, it also includes a tensioning wheel mechanism, which has two tensioning wheel mechanisms, which are respectively installed at the output end of the unwinding mechanism and the input end of the winding mechanism. The pre-nickel-plated steel strip passes through the tensioning wheel mechanism, and the tensioning wheel mechanism is used to adjust the tensioning force on the pre-nickel-plated steel strip.

[0027] The beneficial effects of the present invention are embodied in:

[0028] 1. The present invention performs a single-sided preheating treatment process on a pre-nickel-plated steel strip with non-uniform thickness on both sides. After a temperature gradient with a large temperature difference is formed in the steel strip, an overall heat treatment process is performed to form an iron-nickel diffusion layer with significant differences on both sides of the steel strip, thereby effectively improving the corrosion resistance of the pre-nickel-plated steel strip and pre-nickel-plated products, such as battery shells.

[0029] 2. The present invention further ensures that the heat-treated iron-nickel diffusion layer has stronger bonding strength and no "iron leakage" phenomenon by optimizing the heat treatment environment and parameters, thereby improving the safety of use and service performance of the pre-nickel-plated products. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The drawings described herein are used to provide further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute improper limitations on the present application.

[0031] Figure 1 The present invention is a flowchart of a method for double-sided asynchronous thermal diffusion of a pre-nickel-plated steel strip according to an embodiment of the present invention.

[0032] Figure 2 It is a SEM comparison picture of the thin side and the thick side of the double-sided pre-nickel-plated steel strip with unequal thickness before and after being treated in the embodiment of the present invention.

[0033] Figure 3 It is a schematic diagram of the overall structure of an embodiment of the present invention.

[0034] Figure 4 It is a schematic diagram of the internal gas flow of the local structure of an embodiment of the present invention.

[0035] Figure 5 Schematic diagram of a condensation pipeline according to an embodiment of the present invention.

[0036] Figure 6 Schematic diagram of a voltage regulating mechanism according to an embodiment of the present invention.

[0037] Figure 7 It is a structural block diagram of a computer device according to an embodiment of the present invention.

[0038] The components in the accompanying drawings are marked as follows: 1. unwinding mechanism; 2. tensioning wheel mechanism; 3. pressure regulating mechanism; 4. preheating box; 401. air inlet channel; 5. condensation pipe; 6. gas guide plate; 7. heating furnace; 701. heating tube; 702. electric control box; 8. exhaust box; 801. exhaust channel; 9. cooling box; 901. cooling gas channel; 10. winding mechanism; 11. pre-nickel-plated steel strip; 12. support seat; 13. motor; 1301. output power shaft; 14. coupling; 15. screw; 16. guide column; 17. bracket; 18. roller. DETAILED DESCRIPTION

[0039] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. In the absence of conflict, the embodiments in this application and the features in the embodiments can be combined with each other. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0040] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative position relationship, movement, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly. In addition, the meaning of "and / or" appearing in the full text includes three parallel solutions. Taking "A and / or B" as an example, it includes solution A, solution B, or solutions that satisfy both A and B. In addition, "multiple" means more than two.

[0041] See also Figure 1 The embodiment of the present invention also provides a method for double-sided asynchronous heat diffusion of a pre-nickel-plated steel strip, comprising the following steps:

[0042] S1: Installation and preparation of the pre-nickel-plated steel strip 11 with non-uniform thickness on both sides: Wind the pre-nickel-plated steel strip 11 with non-uniform thickness on both sides on the unwinding mechanism 1, distinguish the thick side and the thin side, and ensure that the thin side of the pre-nickel-plated steel strip 11 unwinding and stretching along the unwinding direction faces the condensation pipe 5 in the preheating box 4, and the thick side faces the gas guide plate 6 in the preheating box 4;

[0043] S2: Single-sided preheating treatment of the pre-nickel-plated steel strip 11 with non-uniform thickness on both sides: the free end of the pre-nickel-plated steel strip 11 after unwinding passes through the preheating box 4, and the air inlet channel 401 of the preheating box 4 passes high-temperature gas to the thick side of the pre-nickel-plated steel strip 11 through the gas guide plate 6. The thin side of the pre-nickel-plated steel strip 11 is pressed against the condensation pipe 5 under the pressure of the pressure regulating mechanism 3, and the thin side of the pre-nickel-plated steel strip 11 is cooled and the thick side is heated, forming a temperature gradient in the plate;

[0044] S3: Thermal diffusion treatment of the pre-nickel-plated steel strip 11 with non-uniform thickness on both sides: the free end of the pre-nickel-plated steel strip 11 after single-side preheating is passed through the preheating box 4 into the heating furnace 7, and both sides are heated by the heating tube 701, so that diffusion layers are quickly formed on both sides of the plate;

[0045] S4: Cooling and winding of double-sided non-uniform thickness pre-nickel-plated steel strip 11: the free end of the pre-nickel-plated steel strip 11 after thermal diffusion treatment passes through the exhaust box 8 and the cooling box 9 in sequence from the heating furnace 7, and the mixed gas after passing through the preheating box 4 and the multiple heating furnaces 7 is discharged through the exhaust channel 801 of the exhaust box 8, and the cooling box 9 introduces cooling gas to prevent oxidation to the pre-nickel-plated steel strip 11 through the cooling gas channel 901. The free end of the pre-nickel-plated steel strip 11 after cooling treatment is connected to the winding mechanism 10, and the winding mechanism 10 rotates the pre-nickel-plated steel strip 11 along the winding direction for winding.

[0046] The present invention targets pre-nickel-plated steel strips with non-uniform thickness on both sides, performs a single-sided preheating treatment process, forms a temperature gradient with a large temperature difference in the steel strip, and then performs an overall heat treatment process to form iron-nickel diffusion layers with significant differences on both sides of the steel strip, thereby effectively improving the corrosion resistance of the pre-nickel-plated steel strip and pre-nickel-plated products, such as battery shells. At the same time, by optimizing the heat treatment environment and parameters, it is further ensured that the bonding force of the heat-treated iron-nickel diffusion layer is stronger and there is no "iron leakage" phenomenon, thereby improving the use safety and service performance of the pre-nickel-plated products.

[0047] In the present invention, the single-sided preheating treatment is completed by cooling the thin surface of the pre-nickel-plated steel strip and heating the thick surface, thereby forming a temperature gradient with a large temperature difference in the pre-nickel-plated steel strip. According to Fick's law, temperature is a decisive factor affecting the diffusion rate and diffusion flux. When the diffusion coefficient of the material is the same, the higher the temperature, the higher the diffusion rate. The temperature difference between the two-sided pre-nickel-plated layers leads to a difference in diffusion rate, and within the same diffusion time, the difference in diffusion rate also leads to a difference in diffusion flux. The diffusion flux of the nickel layer on the high-temperature side is larger, so the thickness of the iron-nickel alloy layer formed is thicker, and similarly the thickness of the iron-nickel alloy layer finally formed on the low-temperature side is thinner. Utilizing this method, a pre-nickel-plated steel strip with different thicknesses of iron-nickel alloy layers on both sides can be formed during a single thermal diffusion treatment.

[0048] See also Figure 1 In this embodiment, in S1, the unwinding speed of the unwinding mechanism 1 and the rewinding speed of the rewinding mechanism 10 are adjusted according to the distance between them. Generally, the unwinding speed and the rewinding speed are set to 1 m·s -1 ~5m·s -1 , and are always equal to avoid damage to the pre-nickel-plated steel strip 11;

[0049] In S2, the flow rate of the high-temperature gas introduced into the air inlet channel 401 is controllable, the flow rate of the condensate introduced into the condensation pipe 5 is controllable, the pressure of the pressure regulating mechanism 3 pressing the pre-nickel-plated steel strip 11 is adjustable and monitored in real time by the pressure sensor, and the high-temperature gas is selected to be a gas that can prevent the pre-nickel-plated steel strip 11 from being oxidized, such as nitrogen, inert gas, etc. The temperature of the high-temperature gas is usually set between 600°C and 1000°C, and the flow rate of the high-temperature gas is usually set to 0.2m·s -1 ~10m·s -1 The condensing liquid should be a liquid with good fluidity and large specific heat capacity, such as water at room temperature, aqueous solution with additives, etc. The flow rate of the condensing liquid is usually set to 0.1m·s -1 ~3m·s -1 , the pressure applied by the pressure regulating mechanism 3 to the pre-nickel-plated steel strip 11 is usually set within 50Pa to 500Pa;

[0050] In S3, the heating temperature in the heating furnace 7 is controllable, the speed at which the pre-nickel-plated steel strip 11 travels in the heating furnace 7 is adjustable, the temperature of the heating tube 701 in the heating furnace 7 is usually set between 500° C. and 900° C., and the movement speed of the pre-nickel-plated steel strip 11 in the plurality of heating furnaces 7 is usually set to 1 m·s -1 ~5m·s -1 ;

[0051] In S4, the exhaust speed of the exhaust channel 801 and the intake speed of the intake channel 401 are both controllable and constant, and the flow rate of the cooling gas flowing into the cooling gas channel 901 is controllable. The cooling gas is selected from a gas that can prevent the pre-nickel-plated steel strip 11 from being oxidized, such as nitrogen, inert gas, etc. The flow rate of the cooling gas is usually set to 0.2 m·s -1 ~3m·s -1 , and the flow rate of the cooling gas is positively correlated with the unwinding and winding speed of the unwinding mechanism 1 or the winding mechanism 10. The higher the unwinding and winding speed of the pre-nickel-plated steel strip 11, the greater the flow rate of the cooling gas, and vice versa. It should be noted that during operation, cooling gas should be introduced into the cooling box 9 in advance to fully discharge the air in the box in advance. The ventilation time is generally set to 1h~5h, and ensure that the cooling gas channel 901 is always ventilated to the cooling box 9.

[0052] The present invention will be further described below with reference to a specific embodiment:

[0053] In this embodiment, the pre-nickel-plated steel strip 11 is selected, and the chemical composition of its steel matrix is ​​(mass percentage): C content 4.7%, Si content 1.3%, Mn content 1.1%, P content 0.9%, S content 0.9%, and the rest is Fe. The thickness of the steel strip is 0.8 mm and the width is 250 mm. The steel strip is pre-nickel-plated, and the nickel plating thickness on both sides is 4 μm and 8 μm respectively.

[0054] The above-mentioned pre-nickel-plated steel strip 11 coil is installed in the unwinding mechanism 1 of the present application, and the free end of the steel strip coil is passed through the tensioning wheel mechanism 2, the preheating box 4, the heating furnace 7, the exhaust box 8 and the cooling box 9 in sequence, and finally connected to the winding mechanism 10.

[0055] The parameters of each component in the device are adjusted, specifically: the tension of the tensioning wheel mechanism 2 is adjusted to 12N, the high-temperature gas introduced into the preheating box 4 is set to 820°C nitrogen, and the flow rate of the high-temperature gas is set to 6m·s -1 , cool water at room temperature is introduced into the condensation pipe 5, and the flow rate of the cool water at room temperature is 0.5 m·s -1 , adjust the pressure of the pressure regulating mechanism 3 on the pre-nickel-plated steel strip 11 to 85Pa. After the pre-nickel-plated steel strip 11 is subjected to single-sided preheating treatment in the preheating box 4, a temperature gradient is formed inside the plate, and the plate enters the heating furnace 7. The length of the heating furnace 7 is set to 4 sections, the temperature in the furnace is set to 700°C, and the movement speed of the pre-nickel-plated steel strip 11 in the heating furnace 7 is 1.5m·s -1 After the pre-nickel-plated steel strip 11 is heated in the heating furnace 7, a heat diffusion layer is quickly formed on both sides and enters the exhaust box 8. The exhaust box 8 also has the same flow rate as the high-temperature gas, that is, 6m·s -1 The mixed gas after passing through the preheating box 4 and the heating furnace 7 is extracted, and then the pre-nickel-plated steel strip 11 enters the cooling box 9, and the flow rate of the cooling box 9 is 2m·s -1 The steel strip is cooled by nitrogen and finally coiled.

[0056] See also Figure 2 , the microstructure of the pre-nickel-plated steel strip 11 after the above treatment is analyzed. The scanning electron microscope (SEM) in the figure is taken by backscattered electron imaging, wherein (a) is a detection image of the thin alloy layer of the untreated pre-nickel-plated steel strip, (b) is a detection image of the thick alloy layer of the untreated pre-nickel-plated steel strip, (c) is a detection image of the thin alloy layer of the treated pre-nickel-plated steel strip, and (d) is a detection image of the thick alloy layer of the treated pre-nickel-plated steel strip. Figure 2It can be seen that after double-sided asynchronous thermal diffusion treatment, thermal diffusion occurs on both sides of the pre-nickel-plated steel strip to form an iron-nickel alloy layer, but the thickness of the iron-nickel alloy layer on the two sides is different. The thickness of the iron-nickel alloy layer on the thin side of the pre-nickel-plated steel strip (thickness of 4μm) is about 2μm, and the thickness of the iron-nickel alloy layer on the thick side of the pre-nickel-plated steel strip (thickness of 8μm) is about 4μm, thereby forming steel strips with different diffusion layer thicknesses. After the above treatment, not only is it ensured that a sufficient iron-nickel diffusion layer is formed on the thick side of the pre-nickel-plated steel strip, but the "iron leakage" phenomenon on the thin side of the pre-nickel-plated steel strip is also avoided, thereby effectively improving the corrosion resistance of the pre-nickel-plated steel strip.

[0057] See also Figure 3-Figure 4 , the embodiment of the present invention provides a double-sided asynchronous heat diffusion device for pre-nickel-plated steel strip, which is applicable to the double-sided asynchronous heat diffusion method for pre-nickel-plated steel strip, including a pre-nickel-plated steel strip 11, and also including an unwinding mechanism 1, a preheating box 4, a heating furnace 7, an exhaust box 8, a cooling box 9 and a winding mechanism 10 which are sequentially distributed;

[0058] The pre-nickel-plated steel strip 11 is a double-sided non-uniform thickness steel strip, with one side being a thick side and the other side being a thin side, and is wound on the unwinding mechanism 1, and after the free end of the pre-nickel-plated steel strip 11 is drawn out, it passes through the preheating box 4, the heating furnace 7, the exhaust box 8 and the cooling box 9 in sequence, and enters the winding mechanism 10;

[0059] The interior of the preheating box 4 is horizontally parallel and spaced apart with condensation pipes 5 and gas guide plates 6, the condensation pipes 5 are filled with condensate, the air inlet channel 401 of the preheating box 4 points to the gas guide plate 6, and high-temperature gas is introduced, the free end of the pre-nickel-plated steel strip 11 horizontally passes through between the condensation pipe 5 and the gas guide plate 6, the thin side faces the condensation pipe 5, and the thick side faces the gas guide plate 6, the pre-nickel-plated steel strip 11 forms a temperature gradient in the preheating box 4;

[0060] It also includes a pressure regulating mechanism 3 , which is used to press the pre-nickel-plated steel strip 11 and fit it to the condensation pipe 5 .

[0061] The present invention targets pre-nickel-plated steel strips with non-uniform thickness on both sides, performs a single-sided preheating treatment process, forms a temperature gradient with a large temperature difference in the steel strip, and then performs an overall heat treatment process to form iron-nickel diffusion layers with significant differences on both sides of the steel strip, thereby effectively improving the corrosion resistance of the pre-nickel-plated steel strip and pre-nickel-plated products, such as battery shells. At the same time, by optimizing the heat treatment environment and parameters, it is further ensured that the bonding force of the heat-treated iron-nickel diffusion layer is stronger and there is no "iron leakage" phenomenon, thereby improving the use safety and service performance of the pre-nickel-plated products.

[0062] In the present invention, the single-sided preheating treatment is completed by cooling the thin surface of the pre-nickel-plated steel strip and heating the thick surface, thereby forming a temperature gradient with a large temperature difference in the pre-nickel-plated steel strip. According to Fick's law, temperature is a decisive factor affecting the diffusion rate and diffusion flux. When the diffusion coefficient of the material is the same, the higher the temperature, the higher the diffusion rate. The temperature difference between the two-sided pre-nickel-plated layers leads to a difference in diffusion rate, and within the same diffusion time, the difference in diffusion rate also leads to a difference in diffusion flux. The diffusion flux of the nickel layer on the high-temperature side is larger, so the thickness of the iron-nickel alloy layer formed is thicker, and similarly the thickness of the iron-nickel alloy layer finally formed on the low-temperature side is thinner. Utilizing this method, a pre-nickel-plated steel strip with different thicknesses of iron-nickel alloy layers on both sides can be formed during a single thermal diffusion treatment.

[0063] See also Figure 6 In this embodiment, the pressure regulating mechanism 3 includes a support seat 12, a motor 13, a coupling 14, a screw 15, a guide column 16, a bracket 17 and a roller 18;

[0064] The motor 13 is installed on the support base 12, and the output power shaft 1301 of the motor 13 is fixed to the screw rod 15 via the coupling 14. The screw rod 15 vertically passes through the bottom of the bracket 17 in the center and is threadedly matched with the bracket 17. There are multiple guide columns 16, which are distributed in a ring shape on the support base 12 with the screw rod 15 as the center, and vertically pass through the bottom of the bracket 17. The roller 18 is horizontally rotatably installed on the top of the bracket 17. The bracket 17 has a movement stroke that drives the roller 18 to move up and down along the screw rod 15. The roller 18 is used to press and fit the pre-nickel-plated steel strip 11 to the condensation pipe 5, and a pressure sensor for real-time pressure measurement is installed on the roller 18.

[0065] In this design, the motor 13 drives the output power shaft 1301 to rotate, and under the action of the coupling 14, the screw 15 rotates synchronously with the output power shaft 1301. Under the action of the threaded engagement, the bracket 17 should rotate synchronously with the screw 15, but under the limiting action of the guide column 16, the bracket 17 cannot rotate, but rises and falls along the length direction of the screw 15, thereby driving the roller 18 on the top to rise and fall synchronously, thereby realizing the adjustment of the pressure of the pre-nickel-plated steel strip 11 by the roller 18. At the same time, the pressure sensor is used to monitor the pressure in real time and transmit it to the remote end for inspection by the technician;

[0066] It should be noted that the above-mentioned pressing force should be based on the premise that it does not affect the normal friction and sliding of the pre-nickel-plated steel strip 11 against the surface of the roller 18.

[0067] See also Figure 3-Figure 4 In this embodiment, there are two pressure regulating mechanisms 3, which are respectively installed at the inlet end of the preheating box 4 and the outlet end of the exhaust box 8. With this design, when the pre-nickel-plated steel strip 11 is processed in the box or in the furnace, the two pressure regulating mechanisms 3 located in the unwinding direction and the winding direction respectively press and compact it, which ensures that the pre-nickel-plated steel strip 11 can be close to the condensation pipe 5 during the single-sided preheating process, which is conducive to the formation of a temperature gradient in the plate, and ensures that the pre-nickel-plated steel strip 11 will not be deformed in the box or in the furnace, which is conducive to the normal processing.

[0068] See also Figure 3-Figure 4 In this embodiment, the heating furnace 7 has multiple furnace walls, which are made of heat-insulating materials, connected one by one, and located between the preheating box 4 and the exhaust box 8. Two rows of heating tubes 701 are installed in the upper and lower intervals inside the heating furnace 7. The pre-nickel-plated steel strip 11 passes through the two rows of heating tubes 701, and an electric control box 702 electrically connected to the heating tubes 701 is installed on the heating furnace 7. With this design, the heating furnace 7 can be selected as a resistance heating furnace, which is usually set to 3 to 8 sections, and other forms can also be selected. No specific restrictions are made here. In this application, the heating temperature in the heating furnace 7 and the speed of the pre-nickel-plated steel strip 11 passing through the heating furnace 7 are controllable and adjustable. Generally, the temperature of the heating tube 701 in the heating furnace 7 is set to between 500°C and 900°C, and the movement speed of the pre-nickel-plated steel strip 11 in the multiple heating furnaces 7 is set to 1m·s -1 ~5m·s -1 In this way, the pre-nickel-plated steel strip 11 which has undergone single-sided preheating treatment and formed a temperature gradient inside the plate has completed the thermal diffusion treatment.

[0069] See also Figure 3-Figure 4 In this embodiment, an exhaust channel 801 is provided on the exhaust box 8. The exhaust channel 801 is used to exhaust the mixed gas after passing through the preheating box 4 and the multiple heating furnaces 7. The exhaust channel 801 is connected to the exhaust pump, and the intake channel 401 is connected to the intake pump. The exhaust speed of the exhaust pump and the intake speed of the intake pump are both controllable and always equal. With this design, the high-temperature gas introduced into the preheating box 4 through the intake channel 401 is selected from gases that can prevent the pre-nickel-plated steel strip 11 from oxidizing, such as nitrogen, inert gas, etc., and the temperature of the high-temperature gas is usually set between 600°C and 1000°C, and the flow rate is usually set to 0.2m·s -1 ~10m·s -1 Therefore, the exhaust velocity of the exhaust channel 801 is usually set to 0.2 m·s -1 ~10m·s -1 ;

[0070] It should be noted that during operation, high-temperature gas should be introduced into the preheating box 4 in advance to fully exhaust the air in the box. The ventilation time is generally set to 1h to 5h, and it is ensured that the air inlet channel 401 is always ventilated to the preheating box 4.

[0071] See also Figure 3-Figure 4 In this embodiment, a cooling gas channel 901 is provided on the cooling box 9, and the cooling gas channel 901 is used to pass cooling gas to prevent oxidation of the pre-nickel-plated steel strip 11, and the flow rate of the cooling gas is controllable. In this design, since the temperature of the pre-nickel-plated steel strip 11 after the heating treatment in the heating furnace 7 is relatively high, it needs to be cooled before it can be rolled up. The cooling gas is selected to be a gas that can prevent oxidation of the pre-nickel-plated steel strip 11, such as nitrogen, inert gas, etc. The flow rate of the cooling gas is usually set to 0.2m·s -1 ~3m·s -1 , and the flow rate of the cooling gas is positively correlated with the unwinding and reeling speed of the unwinding mechanism 1 or the rewinding mechanism 10. The higher the rewinding and reeling speed of the pre-nickel-plated steel strip 11, the greater the flow rate of the cooling gas, and vice versa;

[0072] It should be noted that during operation, cooling gas should be introduced into the cooling box 9 in advance to fully exhaust the air in the box. The ventilation time is generally set to 1h to 5h, and ensure that the cooling gas channel 901 is always ventilated to the cooling box 9.

[0073] See also Figure 3-Figure 4 In this embodiment, the inlet / outlet end of the preheating box 4, the inlet / outlet end of the heating furnace 7, the inlet / outlet end of the exhaust box 8 and the inlet / outlet end of the cooling box 9 are all at the same horizontal height, and the pre-nickel-plated steel strip 11 horizontally passes through the preheating box 4, the plurality of heating furnaces 7, the exhaust box 8 and the cooling box 9 in sequence. This design ensures that the pre-nickel-plated steel strip 11 is always in a horizontally stretched state during the processing and maintains a certain tension. At the same time, the unwinding end of the unwinding mechanism 1 in the unwinding direction and the winding end of the winding mechanism 10 in the winding direction should also be maintained at the same horizontal height as the above-mentioned inlet / outlet ends to avoid deformation or damage to the plate during the unwinding or winding process of the pre-nickel-plated steel strip 11.

[0074] See also Figure 3In this embodiment, it also includes a tensioning wheel mechanism 2, which has two tensioning wheel mechanisms 2, which are respectively installed at the output end of the unwinding mechanism 1 and the input end of the winding mechanism 10. The pre-nickel-plated steel strip 11 passes through the tensioning wheel mechanism 2, and the tensioning wheel mechanism 2 is used to adjust the tensioning force on the pre-nickel-plated steel strip 11. In this design, the tensioning wheel mechanism 2 is respectively installed in the unwinding direction and the winding direction. By adjusting the tensioning force of the tensioning wheel mechanism 2, it is ensured that the pre-nickel-plated steel strip 11 is kept in a tensioned state during the treatment process, thereby improving the effect of the single-sided preheating treatment and the thermal diffusion treatment. In general, the tensioning force of the tensioning wheel mechanism 2 is set to 5N to 100N.

[0075] See also Figure 7 An embodiment of the present invention further provides a computer device, including a memory and a processor, wherein the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the above method.

[0076] It is understandable that the system, device and storage medium provided in the embodiments of the present invention correspond to the method provided in the embodiments of the present invention, and the explanation, examples and beneficial effects of the relevant contents can refer to the corresponding parts in the above methods.

[0077] It should be noted that those of ordinary skill in the art can understand that all or part of the steps implemented in the embodiments of the present invention can be implemented in whole or in part by software, hardware, firmware or any combination thereof. When implemented using software, it can be implemented in whole or in part in the form of a computer program product. The computer program product includes one or more computer instructions. When the computer program instructions are loaded and executed on a computer, the process or function described in the embodiment of the present application is generated in whole or in part. The computer may be a general-purpose computer, a special-purpose computer, a computer network, or other programmable device. The computer instructions may be stored in a computer-readable storage medium, or transmitted from one computer-readable storage medium to another computer-readable storage medium, for example, the computer instructions may be transmitted from a website site, computer, server or data center by wired (e.g., coaxial cable, optical fiber, digital subscriber line (DSL)) or wireless (e.g., infrared, wireless, microwave, etc.) mode to another website site, computer, server or data center. The computer-readable storage medium may be any available medium that a computer can access or a data storage device such as a server or data center that includes one or more available media integrated. The available medium may be a magnetic medium (eg, a floppy disk, a hard disk, a magnetic tape), an optical medium (eg, a DVD), or a semiconductor medium (eg, a solid state disk (SSD)).

[0078] In summary, the present invention conducts a single-sided preheating treatment process for pre-nickel-plated steel strips with non-uniform thickness on both sides, forms a temperature gradient with a large temperature difference in the steel strip, and then conducts an overall heat treatment process to form iron-nickel diffusion layers with significant differences on both sides of the steel strip, thereby effectively improving the corrosion resistance of the pre-nickel-plated steel strips and pre-nickel-plated products, such as battery shells. At the same time, by optimizing the heat treatment environment and parameters, it is further ensured that the bonding force of the heat-treated iron-nickel diffusion layer is stronger and there is no "iron leakage" phenomenon, thereby improving the safety of use and service performance of the pre-nickel-plated products.

[0079] It should be understood that the examples and implementation modes described herein are for illustrative purposes only and are not intended to limit the present invention. Those skilled in the art may make various modifications or changes based on the examples and implementation modes. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. A method for double-sided asynchronous thermal diffusion of pre-nickel-plated steel strip, characterized in that: The following steps are involved: S1: Installation and preparation of a pre-nickel-plated steel strip (11) with unequal thickness on both sides: Winding the pre-nickel-plated steel strip (11) with unequal thickness on both sides on the unwinding mechanism (1), distinguishing between thick and thin sides, and ensuring that the thin side of the pre-nickel-plated steel strip (11) unwinding and stretching along the unwinding direction faces the condensation pipe (5) in the preheating box (4), and the thick side faces the gas guide plate (6) in the preheating box (4); S2: Single-sided preheating treatment of a pre-nickel-plated steel strip (11) with non-uniform thickness on both sides: the free end of the pre-nickel-plated steel strip (11) after unwinding passes into the preheating box (4), and the air inlet channel (401) of the preheating box (4) passes high-temperature gas to the thick side of the pre-nickel-plated steel strip (11) via the gas guide plate (6). The thin side of the pre-nickel-plated steel strip (11) is pressed against the condensation pipe (5) by the pressure regulating mechanism (3), and the thin side of the pre-nickel-plated steel strip (11) is cooled and the thick side is heated, thereby forming a temperature gradient in the plate; S3: thermal diffusion treatment of a pre-nickel-plated steel strip (11) with non-uniform thickness on both sides: the free end of the pre-nickel-plated steel strip (11) after single-side preheating is passed from the preheating box (4) into a heating furnace (7), and both sides are heated by a heating tube (701), so that a diffusion layer is quickly formed on both sides of the plate; S4: Cooling and winding of double-sided pre-nickel-plated steel strip (11) with non-uniform thickness: the free end of the pre-nickel-plated steel strip (11) after thermal diffusion treatment passes through the exhaust box (8) and the cooling box (9) in sequence from the heating furnace (7), and the mixed gas after being mixed with the preheating box (4) and multiple heating furnaces (7) is discharged through the exhaust channel (801) of the exhaust box (8), and the cooling box (9) introduces cooling gas to prevent oxidation to the pre-nickel-plated steel strip (11) through the cooling gas channel (901). The free end of the pre-nickel-plated steel strip (11) after cooling treatment is connected to the winding mechanism (10), and the winding mechanism (10) rotates the pre-nickel-plated steel strip (11) along the winding direction to wind it up.

2. The method for double-sided asynchronous thermal diffusion of pre-nickel-plated steel strip according to claim 1, characterized in that: In S1, the unwinding speed of the unwinding mechanism (1) and the rewinding speed of the rewinding mechanism (10) are adjusted according to the distance between them and are always equal; In S2, the flow rate of the high-temperature gas introduced into the air inlet channel (401) is controllable, the flow rate of the condensate liquid introduced into the condensation pipe (5) is controllable, and the pressure of the pressure regulating mechanism (3) pressing the pre-nickel-plated steel strip (11) is adjustable and monitored in real time by a pressure sensor; In S3, the heating temperature in the heating furnace (7) is controllable, and the speed at which the pre-nickel-plated steel strip (11) travels in the heating furnace (7) is adjustable; In S4, the exhaust speed of the exhaust channel (801) and the intake speed of the intake channel (401) are both controllable and constantly equal, the flow rate of the cooling gas flowing into the cooling gas channel (901) is controllable, and the flow rate of the cooling gas is positively correlated with the unwinding and rewinding speed of the unwinding mechanism (1) or the rewinding mechanism (10).

3. A double-sided asynchronous thermal diffusion device for pre-nickel-plated steel strip, suitable for the double-sided asynchronous thermal diffusion method for pre-nickel-plated steel strip as claimed in any one of claims 1 to 2, comprising a pre-nickel-plated steel strip (11), characterized in that: It also includes an unwinding mechanism (1), a preheating box (4), a heating furnace (7), an exhaust box (8), a cooling box (9) and a winding mechanism (10) which are sequentially arranged; The pre-nickel-plated steel strip (11) is a double-sided unequal thickness steel strip, with one side being a thick side and the other side being a thin side, and is wound on the unwinding mechanism (1), and after the free end of the pre-nickel-plated steel strip (11) is drawn out, it passes through the preheating box (4), the heating furnace (7), the exhaust box (8) and the cooling box (9) in sequence, and enters the winding mechanism (10); The interior of the preheating box (4) is provided with condensation pipes (5) and gas guide plates (6) arranged horizontally and in parallel with each other at intervals. Condensate liquid flows in the condensation pipe (5). The air inlet channel (401) of the preheating box (4) points to the gas guide plate (6) and passes high-temperature gas. The free end of the pre-nickel-plated steel strip (11) passes horizontally between the condensation pipe (5) and the gas guide plate (6), with the thin surface facing the condensation pipe (5) and the thick surface facing the gas guide plate (6). The pre-nickel-plated steel strip (11) forms a temperature gradient in the preheating box (4); It also comprises a pressure regulating mechanism (3), and the pressure regulating mechanism (3) is used to press the pre-nickel-plated steel strip (11) and make it fit onto the condensation pipe (5).

4. The double-sided asynchronous thermal diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: The pressure regulating mechanism (3) comprises a support seat (12), a motor (13), a coupling (14), a screw rod (15), a guide column (16), a bracket (17) and a roller shaft (18); The motor (13) is mounted on the support seat (12); the output power shaft (1301) of the motor (13) is fixed to the screw (15) via the coupling (14); the screw (15) vertically passes through the bottom of the bracket (17) in the center and is threadedly matched with the bracket (17); the guide pillars (16) are provided in plurality, which are respectively distributed in a ring shape on the support seat (12) with the screw (15) as the center of the circle and vertically pass through the bottom of the bracket (17); the roller (18) is horizontally rotatably mounted on the top of the bracket (17); the bracket (17) has a movement stroke for driving the roller (18) to move up and down along the screw (15); the roller (18) is used to press the pre-nickel-plated steel strip (11) and fit it to the condensation pipe (5); and a pressure sensor for real-time pressure measurement is installed on the roller (18).

5. The double-sided asynchronous thermal diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: The pressure regulating mechanisms (3) are provided with two, which are respectively installed at the inlet end of the preheating box (4) and the outlet end of the exhaust box (8).

6. The double-sided asynchronous thermal diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: The heating furnace (7) has a plurality of furnace walls, all of which are made of heat-insulating materials, are connected to each other, and are located between the preheating box (4) and the exhaust box (8). Two rows of heating tubes (701) are installed in the upper and lower parts of the heating furnace (7). The pre-nickel-plated steel strip (11) passes through between the two rows of heating tubes (701). An electric control box (702) electrically connected to the heating tubes (701) is installed on the heating furnace (7).

7. The double-sided asynchronous thermal diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: The exhaust box (8) is provided with an exhaust channel (801), and the exhaust channel (801) is used to exhaust the mixed gas after passing through the preheating box (4) and the plurality of heating furnaces (7). The exhaust channel (801) is connected to an exhaust pump, and the intake channel (401) is connected to an intake pump. The exhaust speed of the exhaust pump and the intake speed of the intake pump are both controllable and always equal.

8. The double-sided asynchronous heat diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: The cooling box (9) is provided with a cooling gas channel (901), and the cooling gas channel (901) is used to pass cooling gas to prevent oxidation of the pre-nickel-plated steel strip (11), and the flow rate of the cooling gas is controllable.

9. The double-sided asynchronous heat diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: The inlet / outlet ends of the preheating box (4), the inlet / outlet ends of the heating furnace (7), the inlet / outlet ends of the exhaust box (8) and the inlet / outlet ends of the cooling box (9) are all at the same horizontal height, and the pre-nickel-plated steel strip (11) horizontally passes through the preheating box (4), the plurality of heating furnaces (7), the exhaust box (8) and the cooling box (9) in sequence.

10. The double-sided asynchronous thermal diffusion device for pre-nickel-plated steel strip according to claim 3, characterized in that: It also includes a tensioning wheel mechanism (2), wherein the tensioning wheel mechanism (2) has two members, which are respectively installed at the output end of the unwinding mechanism (1) and the input end of the rewinding mechanism (10), and the pre-nickel-plated steel strip (11) passes through the tensioning wheel mechanism (2). The tensioning wheel mechanism (2) is used to adjust the tensioning force on the pre-nickel-plated steel strip (11).