Anti-delinting simulated large fur plush fabric and weaving method thereof

Through the anti-dew removal simulation large fur plush fabric made of warp knitted, the use of specific yarn weaving structure and treatment methods, the problem of existing imitation animal fur fabrics is easily fur-lost, achieving a low-cost and efficient non-hair effect. , and improves the durability and simulation effect of the fabric.

CN118932592AActive Publication Date: 2024-11-12江苏苏美达纺织有限公司
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411271752.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-12
Estimated Expiration
2044-09-11

AI Technical Summary

Technical Problem

Existing imitation animal fur plush fabrics are prone to shedding hair and have poor durability. There are many anti-woven finishing processes and high cost. There is a lack of methods to effectively solve the hair loss problem through fabric structure.

Method used

A warp knitted anti-dewrecking simulation large fur fur fabric, including bottom layer and velvet, the bottom layer is woven from semi-matte polyester filaments and low elastic wire, and the velvet is woven from ultra-matte polyester filaments, through a specific comb The yarn pads are digitally and cross-sectional treatments to form a W-shaped structure to firmly interweave and reduce hair loss.

Benefits of technology

It achieves a low cost, low bit error rate and fast reaction anti-hair effect. The fur plush fabric produced is not easy to shed, and it is durable and has a realistic simulation effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118932592A_ABST
    Figure CN118932592A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of textile, and discloses an anti-delinting simulated large fur plush fabric and a weaving method thereof. The plush fabric is a warp knitting fabric and comprises a bottom layer and a plush layer which are sequentially arranged from bottom to top. The bottom layer is formed by weaving semi-dull polyester filament yarns and semi-dull low stretch yarns, the semi-dull polyester filament yarns account for 5-6% of the weight of the fabric, and the semi-dull low stretch yarns account for 10-15% of the weight of the fabric; the velvet layer is formed by weaving super matt polyester filaments and accounts for 80-85% of the weight of the fabric. The method provided by the invention has the advantages of few anti-linting finishing procedures, low cost, low bit error rate and high response speed, and the prepared long-wool plush fabric does not slip linting and is durable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of textiles, and in particular to an anti-shedding simulated large fur plush fabric and a weaving method thereof. Background Art

[0002] The weaving methods of plush fabrics can be divided into weaving and knitting. Since knitted products feel softer and have rich structural elasticity, and the knitting process is relatively simple to operate and has high weaving efficiency, most of the plush fabrics used for home textile decoration, clothing, etc. on the market are knitted fabrics. Compared with weft knitting, warp knitting has high efficiency and good quality in weaving multi-layer fabrics due to its machine configuration characteristics, especially the emergence of double needle bed warp knitting machines, so most plush fabrics are warp knitted fabrics. Plush fabrics imitating animal fur have always been favored by consumers and producers, and have a huge market in the fields of clothing, high-end home textiles, etc.

[0003] Based on the current market situation, the research and development focus of artificial fur plush fabrics is concentrated on expanding its functionality and aesthetics. For example, CN220297999U discloses a multi-layer functional rabbit-like plush fiber fabric, and CN219191519U discloses a coarse denier viscose rabbit-like fabric. In fact, the most important point of artificial fur should be to reduce the hair loss rate or to prevent hair loss, to be beautiful and clean, and to ensure functionality. At present, CN220157626U discloses that glue is used to reduce the hair loss rate of the fabric, and the use of glue will inevitably affect the feel of the fabric, and as the use time increases, the glue will inevitably oxidize and fall off, and this method cannot avoid hair loss, but only improves it. CN 219450171 U discloses that there is also a method of using specific equipment in the post-finishing process to reduce the hair loss of the fabric, but the purchase of new machines will inevitably increase the cost and cannot completely cure the occurrence of hair loss.

[0004] In general, the research on anti-shedding imitation animal fur plush fabrics is basically focused on post-finishing, which reduces the occurrence of hair shedding through external effects. There is relatively little research on relying on fabric structure to prevent fabric from shedding. It is urgent to develop a low-cost, high-efficiency method to achieve hair-free through fabric structure. Summary of the invention

[0005] The invention aims to solve the problems in the prior art that the imitation animal fur plush fabric is easy to shed and is not durable, and overcome the defects of multiple anti-shedding finishing processes and high cost.

[0006] In order to achieve the above-mentioned object, the first aspect of the present invention provides an anti-shedding simulated large fur plush fabric, the plush fabric is a warp knitted fabric, and comprises a bottom layer and a pile layer arranged in sequence from bottom to top;

[0007] The bottom layer is woven from semi-dull polyester filaments and semi-dull low-elastic yarns, wherein the semi-dull polyester filaments account for 5-6% of the weight of the fabric, and the semi-dull low-elastic yarns account for 10-15% of the weight of the fabric;

[0008] The fleece layer is woven from super matte polyester filaments and accounts for 80-85% of the weight of the fabric.

[0009] Preferably, the pile height of the pile layer is 70-75 mm.

[0010] The second aspect of the present invention provides a method for weaving the anti-shedding simulated large fur plush fabric as described in the first aspect of the present invention, the method comprising the following steps:

[0011] (1) placing the base yarn I on the comb bars GB1 and GB4, placing the surface yarn on the comb bar GB3, placing the base yarn II on the comb bars GB2 and GB5, and respectively setting the inlay yarn numbers of the comb bars GB1, GB2, GB3, GB4, and GB5, and then weaving according to the inlay yarn numbers to obtain a fabric embryo with a structure of base fabric I-surface yarn-base fabric II;

[0012] (2) transferring the fabric blank to a slitting machine for slitting to obtain an intermediate having single-sided fluff;

[0013] (3) Post-processing the intermediate.

[0014] Preferably, in step (1), the amount of the base yarn I on the comb bar GB1 and the comb bar GB4 is 60-65 g / m 2 .

[0015] Further preferably, in step (1), the amount of the base yarn I on the comb bar GB2 and the comb bar GB5 is 115-125 g / m 2 .

[0016] According to a particularly preferred specific implementation manner, in step (1), the yarn inlay number of the combing bar GB1 is set to 0-1-1-4 / 4-3-3-0 / / , the yarn inlay number of the combing bar GB2 is set to 1-0-0-0 / 0-1-1-1 / / , the yarn inlay number of the combing bar GB3 is set to 0-1-0-1 / 0-0-0-1 / 0-1-0-0 / / , the yarn inlay number of the combing bar GB4 is set to 1-1-1-0 / 0-0-0-1 / / , and the yarn inlay number of the combing bar GB5 is set to 3-0-0-1 / 1-4-4-3 / / .

[0017] Preferably, in step (1), the weaving condition at least satisfies: the vehicle speed is 190-210 r / min.

[0018] Further preferably, in step (1), during the weaving, the yarn padding method of the comb bar GB3 is to pad the yarn twice on one side of the needle bed, and then pad the yarn twice on the other side of the needle bed, and the cycle is repeated.

[0019] More preferably, in step (2), the conditions for the slitting process meet the following conditions: the vehicle speed is 6 to 10 m / min.

[0020] Preferably, in step (3), the post-treatment includes pre-combing, pre-ironing, hot blowing, a first combing treatment, a first ironing treatment, a second combing treatment, a second ironing treatment, shearing, and a third ironing treatment performed in sequence.

[0021] Preferably, in step (3), the pre-combing is performed by using a brushing machine, and the speed of the brushing machine is set to 5-8 m / min.

[0022] Further preferably, the pre-ironing is performed by using an ironing machine, the temperature of the ironing machine is set to 180-220° C., and the speed is controlled at 10-15 m / min.

[0023] More preferably, the hot blowing is performed by using a hot blowing machine, and the vehicle speed is controlled at 0.5-1 m / min.

[0024] Preferably, the first combing treatment is performed by using a brushing machine, and the speed of the brushing machine is set to 2-6 m / min.

[0025] Preferably, the first ironing treatment is performed by using an ironing machine, the temperature of the ironing machine is set to 100-220° C., and the speed is controlled at 6-8 m / min.

[0026] Further preferably, the second combing treatment is performed by using a brushing machine, and the speed of the brushing machine is set to 2-5 m / min.

[0027] Preferably, the second ironing treatment is performed by using an ironing machine, the temperature of the ironing machine is set to 100-220° C., and the speed is controlled at 6-8 m / min.

[0028] Preferably, the shearing condition satisfies: the vehicle speed is controlled at 4-8 m / min.

[0029] More preferably, the third ironing treatment is performed by using an ironing machine, the temperature of the ironing machine is set to 90-220° C., and the speed is controlled at 6-8 m / min.

[0030] The method for weaving anti-shedding simulated large fur plush fabric provided by the present invention also has at least the following beneficial effects:

[0031] (1) The anti-hair loss finishing method provided by the present invention has fewer steps, low cost, low bit error rate and fast response speed.

[0032] (2) The large fur plush fabric prepared by the method provided by the present invention does not shed hair and is durable.

[0033] (3) In the weaving process of the method provided by the present invention, the yarn padding method of the combing bar GB3 is to pad the yarn twice on the needle bed on one side, and then pad the yarn twice on the needle bed on the other side, and repeat this cycle. The plush structure woven by this yarn padding method is a W-shaped structure, so that the plush yarn is firmly and tightly interwoven with the base fabric, and has the characteristic of not easy to shed.

[0034] (4) The simulation effect of the large fur plush fabric produced by the method provided by the present invention is more realistic than that of acrylic.

[0035] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 It is a digital image of the yarn inlay of the combing bar GB1, combing bar GB2, combing bar GB3, combing bar GB4 and combing bar GB5 of the present invention;

[0037] Figure 2 It is a coil diagram woven by the comb bar GB1, comb bar GB2, comb bar GB3, comb bar GB4, and comb bar GB5 of the present invention. DETAILED DESCRIPTION

[0038] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0039] The present invention will be described in detail below by way of examples. In the following examples, unless otherwise specified, the raw materials are all commercially available.

[0040] In the following examples, the warp knitting machine is a double needle bed Raschel warp knitting machine purchased from Changzhou Tianhuang Warp Knitting Technology Co., Ltd., model HEBC-COM-G4.

[0041] Example 1

[0042] This example combines Figure 1 and Figure 2 A method for weaving an anti-shedding simulated large fur plush fabric is provided, the method comprising the following steps:

[0043] (1) FDY semi-dull polyester filament with a specification of 150D / 96F is used as the base yarn I, and is placed on the comb bars GB1 and GB4 of the warp knitting machine respectively; FDY super-dull polyester filament with a specification of 260D / 24F is used as the surface yarn, and is placed on the comb bar GB3 of the warp knitting machine; DTY semi-dull low-elastic yarn with a specification of 100D / 96F is used as the base yarn II, and is placed on the comb bars GB2 and GB5 of the warp knitting machine respectively; then, the inlay yarn numbers of the comb bar GB1 are designed as 0-1-1-4 / 4-3-3-0 / / on the warp knitting machine, and the inlay yarn numbers of the comb bar GB2 are designed as 0-1-1-4 / 4-3-3-0 / ... The inlay yarn number of the combing bar GB3 is 0-1-0-1 / 0-0-0-1 / 0-1-0-0 / / , the inlay yarn number of the combing bar GB4 is 1-1-1-0 / 0-0-0-1 / / , the inlay yarn number of the combing bar GB5 is 3-0-0-1 / 1-4-4-3 / / , and then weaving is performed according to the above inlay yarn numbers to obtain a fabric embryo with a structure of base fabric I-face silk-base fabric II; the weaving conditions meet: the designed pile height is 75 mm, and the machine speed is 210-220 r / min;

[0044] During the weaving process, the yarn padding method of the comb bar GB3 is to pad the yarn twice on the needle bed on one side first, and then pad the yarn twice on the needle bed on the other side, and repeat the cycle.

[0045] (2) The fabric blank is transferred to a slitting machine for slitting, so that the pile yarn layer connecting the base fabric I and the base fabric II is divided into two, and an intermediate with pile on one side is obtained; the slitting condition satisfies: the machine speed is 10 m / min.

[0046] (3) the intermediate is sequentially subjected to pre-combing, pre-ironing, hot blowing, a first combing treatment, a first ironing treatment, a second combing treatment, a second ironing treatment, shearing, and a third ironing treatment to obtain an anti-shedding simulated fur plush fabric, wherein the fabric is a warp knitted fabric, comprising a base layer and a pile layer, wherein the base layer is woven from FDY semi-dull polyester filaments with a specification of 150D / 96F, accounting for 5-6% of the weight of the fabric I, and is woven from DTY semi-dull low-elastic yarns with a specification of 100D / 96F, accounting for 10-15% of the weight of the fabric II, and the pile layer is woven on the base layer I, and is warp knitted from FDY super-dull polyester filaments with a specification of 260D / 24F, accounting for 80-85% of the weight of the fabric I, and the pile height of the pile layer I is 75 mm;

[0047] The pre-combing is carried out by using a brushing machine, firstly connecting the brushing machine I with the brushing machine II, and setting the speed of the brushing machine I and the brushing machine II to 5-8 m / min;

[0048] The pre-ironing is carried out by using an ironing machine, with the temperature of ironing machine I set to 220°C, the temperature of ironing machine II set to 210°C, the temperature of ironing machine III set to 190°C, and the temperature of ironing machine IV set to 180°C. The speed is controlled at 10-15m / min, and the pressure is kept at the maximum;

[0049] The hot blowing is carried out by using a hot blowing machine, and the speed is controlled at 0.5-1m / min to ensure that the rough surface is blown solidly;

[0050] The first combing treatment is performed by using the brushing machine I and the brushing machine II, and the speed of the brushing machine I and the brushing machine II is controlled at 2-6 m / min to ensure a strong velvety feel on the fabric surface;

[0051] The first ironing treatment is carried out by using an ironing machine, with the temperature of ironing machine I set to 220°C, the temperature of ironing machine II set to 200°C, the temperature of ironing machine III set to 180°C, the temperature of ironing machine IV set to 160°C, the temperature of ironing machine V set to 100°C, the speed is controlled at 6-8m / min, and the pressure is adjusted according to the quality of the plush surface.

[0052] Second combing treatment: the brushing machine I and brushing machine II are used, and the speed of the brushing machine I and brushing machine II is controlled at 2-5 m / min to ensure a strong velvety feel on the fabric surface;

[0053] Second ironing treatment: Use ironing machine, set the temperature of ironing machine I to 220℃, the temperature of ironing machine II to 180℃, the temperature of ironing machine III to 150-160℃, the temperature of ironing machine IV to 100℃, control the speed at 6-8m / min, and adjust the pressure according to the quality of the plush surface;

[0054] Shearing: The speed is controlled at 4-8m / min to ensure that the shearing head is smooth;

[0055] The third ironing treatment: Use ironing machine, set the temperature of ironing machine I to 220℃, the temperature of ironing machine II to 180℃, the temperature of ironing machine III to 150-160℃, the temperature of ironing machine IV to 90-100℃, control the speed at 6-8m / min, and adjust the pressure according to the quality of the plush surface.

[0056] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A kind of anti-shedding simulated large fur plush fabric, characterized in that: The plush fabric is a warp knitted fabric, and comprises a bottom layer and a plush layer arranged in sequence from bottom to top; The bottom layer is woven from semi-dull polyester filaments and semi-dull low-elastic yarns, wherein the semi-dull polyester filaments account for 5-6% of the weight of the fabric, and the semi-dull low-elastic yarns account for 10-15% of the weight of the fabric; The fleece layer is woven from super matte polyester filaments and accounts for 80-85% of the weight of the fabric.

2. The anti-shedding simulated large fur plush fabric according to claim 1, wherein: The pile height of the pile layer is 70-75 mm.

3. A method for weaving the anti-shedding simulated large fur plush fabric as claimed in claim 1 or 2, characterized in that: The method comprises the following steps: (1) placing the base yarn I on the comb bars GB1 and GB4, placing the surface yarn on the comb bar GB3, placing the base yarn II on the comb bars GB2 and GB5, and respectively setting the inlay yarn numbers of the comb bars GB1, GB2, GB3, GB4, and GB5, and then weaving according to the inlay yarn numbers to obtain a fabric embryo with a structure of base fabric I-surface yarn-base fabric II; (2) transferring the fabric blank to a slitting machine for slitting to obtain an intermediate having single-sided fluff; (3) Post-processing the intermediate.

4. The method according to claim 3, wherein: In step (1), the amount of the base yarn I on the comb bar GB1 and the comb bar GB4 is 60-65 g / m 2 ; And / or, in step (1), on the comb bar GB2 and the comb bar GB5, the amount of the base yarn I is 115-125 g / m 2 .

5. The method according to claim 3 or 4, wherein: In step (1), the yarn inlay number of the combing bar GB1 is set to 0-1-1-4 / 4-3-3-0 / / , the yarn inlay number of the combing bar GB2 is set to 1-0-0-0 / 0-1-1-1 / / , the yarn inlay number of the combing bar GB3 is set to 0-1-0-1 / 0-0-0-1 / 0-1-0-0 / / , the yarn inlay number of the combing bar GB4 is set to 1-1-1-0 / 0-0-0-1 / / , and the yarn inlay number of the combing bar GB5 is set to 3-0-0-1 / 1-4-4-3 / / .

6. The method according to claim 3 or 4, wherein: In step (1), the weaving condition at least satisfies: the vehicle speed is 190-210 r / min.

7. The method according to claim 3 or 4, wherein: In step (1), during the weaving, the yarn padding method of the comb bar GB3 is to pad the yarn twice on one side of the needle bed, and then pad the yarn twice on the other side of the needle bed, and the cycle is repeated.

8. The method according to claim 3 or 4, wherein: In step (2), the conditions for the slitting process are as follows: the vehicle speed is 6 to 10 m / min.

9. The method according to claim 3 or 4, wherein: In step (3), the post-treatment includes pre-combing, pre-ironing, hot blowing, a first combing treatment, a first ironing treatment, a second combing treatment, a second ironing treatment, shearing, and a third ironing treatment performed in sequence.

10. The method according to claim 3 or 4, wherein: In step (3), the pre-combing is performed by using a brushing machine, and the speed of the brushing machine is set to 5 to 8 m / min; And / or, the pre-ironing is performed by using an ironing machine, the temperature of the ironing machine is set to 180-220° C., and the speed is controlled at 10-15 m / min; And / or, the hot blowing is performed by using a hot blowing machine, and the speed is controlled at 0.5-1 m / min; And / or, the first combing treatment is performed by using a brushing machine, and the speed of the brushing machine is set to 2-6 m / min; And / or, the first ironing treatment is performed by using an ironing machine, the temperature of the ironing machine is set to 100-220° C., and the speed is controlled at 6-8 m / min; And / or, the second combing treatment is performed by using a brushing machine, and the speed of the brushing machine is set to 2-5 m / min; And / or, the second ironing treatment is performed by using an ironing machine, the temperature of the ironing machine is set to 100-220° C., and the speed is controlled at 6-8 m / min; And / or, the shearing conditions meet: the vehicle speed is controlled at 4-8 m / min; And / or, the third ironing treatment is performed by using an ironing machine, the temperature of the ironing machine is set to 90-220° C., and the speed is controlled at 6-8 m / min.

Citation Information

Patent Citations

  • Terylene comfortable cotton velvet woolen blanket and preparing method thereof

    CN101407972A

  • Production method of plush fabric

    CN101956292A

  • Processing method for super plush terylene carpet fabric

    CN102936793A

  • Artificial cony hair felt fiber fabric

    CN106592086A

  • Ferret-cashmere-imitating double-needle bar plush fabric and production method thereof

    CN109234905A