Antistatic T-shirt production process
Through the anti-static T-shirt production process, the spraying and textile technology of composite conductive fibers and silver-plated fibers are used to solve the static problem of T-shirts, reduce safety hazards, and achieve safer daily use.
Patent Information
- Application Number
- CN202410792099.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-19
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing T-shirts will produce static electricity after autumn, which may accidentally hurt others during contact and crackle when taking off clothes, which poses a safety hazard.
Adopt antistatic T-shirt production process, by selecting antistatic fabrics, composite conductive fibers, blended yarns, silver-plated fibers, spraying, textile, dyeing tank treatment, cutting and printing, and finally sewing them into T-shirts manually to ensure that Fabric anti-static.
It reduces the generation of static electricity and reduces safety risks, allowing people to get closer to T-shirts, improving safety in daily life.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of T-shirt production, and in particular to a production process of an antistatic T-shirt. Background Art
[0002] Existing T-shirts will generate a lot of static electricity after autumn, which may accidentally hurt each other when people touch them. In addition, when the T-shirt is taken off, it will make crackling sounds, and there are certain safety hazards.
[0003] Therefore, we proposed an antistatic T-shirt production process to solve the above problems. Summary of the invention
[0004] The purpose of the present invention is to solve the shortcomings of the prior art and to propose an antistatic T-shirt production process.
[0005] A production process for antistatic T-shirts, characterized in that it comprises the following steps:
[0006] S1: Before producing antistatic T-shirts, you first need to select the processing fabrics of the T-shirts. In the existing process of selecting an antistatic fabric for production and processing, you first need to take a piece of polyester resin and conductive masterbatch through the following processes: slicing → pulse conveyor → wet slicing large silo → pulse conveyor → pre-crystallizer → drying tower → extruder → melt distribution pipe → spinning box → metering pump → composite spinning assembly → side blowing → bundling oiling → winding → chemical fiber to obtain a composite conductive fiber with PET as the matrix;
[0007] S2: Secondly, blended yarn needs to be prepared. First, a certain amount of composite conductive fiber and cotton fiber are torn loose by hand, and then put into a small wool mixing machine for full mixing for 20-25 minutes. Then, the mixed fiber is fed into a small carding machine for carding into a web and strips, and then the conductive fiber blended yarn is obtained by a small spinning machine;
[0008] S3: Next, the electrostatic material is pretreated, water and antistatic agent are mixed in a ratio of 3:1 to prepare a mixture, the mixture is sprayed on the conductive fiber blended yarn, and the sprayed conductive fiber blended yarn is left to stand for 20-25 hours;
[0009] S4: Next, prepare the silver-plated fiber blended yarn. First, manually loosen the silver-plated staple fibers, add a spinning aid in a ratio of 2:1, fully mix, and place for 5-8 hours. Then, feed the conductive fiber blended yarn into a carding machine together with the conductive fiber blended yarn to form a raw sliver. Then, the yarn is passed through a roving machine for 20-30 minutes, and then through a spinning machine for 10-15 minutes. Finally, the silver-plated fiber blended yarn is wound on a bobbin machine for 5-10 minutes.
[0010] S5: Then, a textile treatment is performed to weave the silver-plated fiber blended yarn into knitted fabrics with different weft knitted patterns on a weft knitted single-sided jacquard circular machine;
[0011] S6: Put the knitted grey fabric into the dyeing vat after being prepared, inject water according to the weight of the grey fabric, beat the grey fabric into the dyeing vat, and inject dye and auxiliary agent into the dyeing vat through the dyeing vat barrel. The ratio of dye and auxiliary agent is 3:1. Heat the dyeing vat at 100-110℃ and pressure of 1.5-2.5Mpa, keep warm for 30-40 minutes, cool down to 70-80℃, and the cylinder pressure is 0.1-0.2Mpa. Open the cylinder cover to wash the sample water out of the cylinder, and dehydrate the grey fabric;
[0012] S7: Next, the grey cloth is subjected to antistatic post-treatment, firstly, the fabric is placed in the finishing liquid and soaked at room temperature for 30 to 40 minutes, then rolled dry, with a rolling rate of 60 to 75%, and finally dried at a drying temperature of 165 to 170°C;
[0013] S8: Next, the grey fabric is shaped. First, the fabric is soaked in water with sodium chloride added at 30-55°C for 65-85 minutes; then an oxidant is added, and the temperature of the oxidation process is maintained at 55-65°C for 40-50 minutes; then a softener is added, and the temperature of the softening process is maintained at 35-40°C for 20-30 minutes; then a reducing agent is added, and the temperature of the reduction process is maintained at 40-50°C for 30-38 minutes, to obtain the prepared antistatic fabric;
[0014] S9: Next, the antistatic fabric is cut to the required size by a cutting machine, and the style can be designed by an automatic cutting bed;
[0015] S10: After the fabric is cut into the required shape, the fabric is printed by a printing machine, and the reactive dye gravure ink is directly sprayed onto the designed pattern formed on the PET film, and then the pattern on the PET film is transferred to the fabric;
[0016] S11: Next, the fabric is sewn into a T-shirt shape by human labor using a sewing machine. When the sewing is completed, the extra thread ends during the sewing process are manually removed, and the sewing machine is quality inspected to obtain a complete antistatic T-shirt.
[0017] Preferably, in S1, the conductive masterbatch comprises the following raw materials in parts by mass: polypropylene (PP): 100-120 parts, conductive carbon black: 10-20 parts, carbon black dispersant: 5-12 parts, processing aid: 20-30 parts, magnetite powder: 12-14 parts.
[0018] Preferably, in S2, the rotation speed of the small carding machine is 25-30 r / min, and the mixing ratio of the composite conductive fiber and the cotton fiber is 1:1.
[0019] Preferably, in S3, the volume of water is 11 to 21 times the volume of the antistatic agent, and the weight of the mixture accounts for 10% to 25% of the total weight of the nylon fiber raw material and the mixture.
[0020] Preferably, in S7, the components of the finishing liquid and the weight percentage of each component are: 5-12% polyurethane resin, 13-23% softener, 0.1-0.3% fatty alcohol polyoxyethylene ether, 1.5-3.5% citric acid, and the rest is water.
[0021] Preferably, in S8, the mass ratio of sodium chloride to fabric is about 1:180, the mass ratio of oxidant to fabric is 1:110, the mass ratio of softener to fabric is 1:100, and the mass ratio of reducing agent to fabric is 1:120.
[0022] Preferably, in S9, the model of the cutting machine is QY-650TH, and the maximum cutting thickness of the cutting machine is 1-3 mm.
[0023] Preferably, in S11, the needle pitch of the sewing machine is 2.5-4 mm, the sewing thickness is 0.8-2 mm, the thread head pressure is 2-4 kg, and the thread head tension setting accuracy is -0.2-0.2 kg.
[0024] The beneficial effects of the present invention are as follows: the antistatic material required for the antistatic T-shirt is pre-treated and post-treated, and then woven and dyed to obtain the fabric required for preparing the T-shirt, and then the antistatic fabric is cut and printed, and finally the fabric is sewn into the required T-shirt by manpower using a sewing machine, so that the entire T-shirt can be anti-static, certain safety hazards are reduced, and people can have closer contact in daily life. DETAILED DESCRIPTION
[0025] The present invention will be further explained below in conjunction with specific embodiments.
[0026] Example 1
[0027] S1: Before producing antistatic T-shirts, it is necessary to first select the processing fabrics of the T-shirts. In the existing process of selecting an antistatic fabric for production and processing, it is first necessary to take a piece of polyester resin and conductive masterbatch through the following process: slicing → pulse conveyor → large wet slicing silo → pulse conveyor → pre-crystallizer → drying tower → extruder → melt distribution pipe → spinning box → metering pump → composite spinning component → side blowing → bundling oiling → winding → chemical fiber to obtain a composite conductive fiber with PET as the matrix; in S1, the conductive masterbatch includes the following raw materials in parts by mass: polypropylene (PP): 100 parts, conductive carbon black: 10 parts, carbon black dispersant: 5 parts, processing aid: 20 parts, magnetite powder: 12 parts.
[0028] S2: Secondly, blended yarn needs to be prepared. First, a certain amount of composite conductive fiber and cotton fiber are torn loose by hand, and then put into a small wool mixing machine for thorough mixing for 20 minutes. Then, the mixed fibers are fed into a small carding machine for combing into a net and strips, and then the conductive fiber blended yarn is obtained by a small spinning machine. In S2, the rotation speed of the small carding machine is 2r / min, and the mixing ratio of the composite conductive fiber and the cotton fiber is 1:1.
[0029] S3: Next, the electrostatic material is pretreated. Water and an antistatic agent are mixed in a ratio of 3:1 to form a mixture, and the mixture is sprayed on the conductive fiber blended yarn. The sprayed conductive fiber blended yarn is then left to stand for 20 hours. In S3, the volume of water is 11 times the volume of the antistatic agent, and the weight of the mixture accounts for 10% of the total weight of the nylon fiber raw material and the mixture.
[0030] S4: Next, the silver-plated fiber blended yarn is prepared. First, the silver-plated short fibers are loosened manually, a spinning aid is added in a ratio of 2:1, and the mixture is fully mixed and placed for 5 hours. The mixture is then fed into a carding machine together with the conductive fiber blended yarn to form a raw sliver. The yarn is then spun by a roving machine for 20 minutes, spun by a spinning machine for 10 minutes, and finally wound by a bobbin winder for 5 minutes to form the silver-plated fiber blended yarn.
[0031] S5: Then, a textile treatment is performed to weave the silver-plated fiber blended yarn into knitted fabrics with different weft knitted patterns on a weft knitted single-sided jacquard circular machine;
[0032] S6: Put the knitted grey fabric into the dyeing vat after being prepared, inject water according to the weight of the grey fabric, beat the grey fabric into the dyeing vat, and inject dye and auxiliary agent into the dyeing vat through the dyeing vat barrel. The ratio of dye and auxiliary agent is 3:1. Heat the dyeing vat at 100°C and 1.5Mpa, keep warm for 30 minutes, cool down to 70°C, and the cylinder pressure is 0.1Mpa. Open the cylinder cover to wash the sample water out of the cylinder, and dehydrate the grey fabric;
[0033] S7: Next, the grey cloth is subjected to antistatic post-treatment. The fabric is first immersed in the finishing liquid at room temperature for 30 minutes, then rolled dry with a rolling rate of 60%, and finally dried at a temperature of 165°C. In S7, the components of the finishing liquid and the weight percentage of each component are: 5% polyurethane resin, 13% softener, 0.1% fatty alcohol polyoxyethylene ether, 1.5% citric acid, and the rest is water.
[0034] S8: Next, the grey cloth is shaped. First, the fabric is soaked in water with sodium chloride at 30°C for 65 minutes; then an oxidant is added, and the temperature of the oxidation process is maintained at 55°C for 40 minutes; then a softener is added, and the temperature of the softening process is maintained at 35°C for 20 minutes; then a reducing agent is added, and the temperature of the reduction process is maintained at 40°C for 30 minutes to obtain the prepared antistatic fabric; in S8, the mass ratio of sodium chloride to fabric is about 1:180, the mass ratio of the oxidant to fabric is 1:110, the mass ratio of the softener to fabric is 1:100, and the mass ratio of the reducing agent to fabric is 1:120.
[0035] S9: Next, the antistatic fabric is cut to the required size by a cutting machine, and the style can be designed by an automatic cutting bed; in S9, the model of the cutting machine is QY-650TH, and the maximum cutting thickness of the cutting machine is 1mm.
[0036] S10: After the fabric is cut into the required shape, the fabric is printed by a printing machine, and the reactive dye gravure ink is directly sprayed onto the designed pattern formed on the PET film, and then the pattern on the PET film is transferred to the fabric;
[0037] S11: Next, the fabric is sewn into a T-shirt shape using a sewing machine by manpower. When the sewing is completed, the extra thread ends during the sewing process are manually removed, and the sewing machine is quality inspected to obtain a complete anti-static T-shirt. In S11, the needle length of the sewing machine is 2.5mm, the sewing thickness is 0.8mm, the thread pulling pressure is 2kg, and the thread pulling force setting accuracy is -0.2kg.
[0038] Example 2
[0039] S1: Before producing antistatic T-shirts, it is necessary to first select the processing fabrics of the T-shirts. In the existing method of selecting an antistatic fabric for production and processing, it is first necessary to take a piece of polyester resin and conductive masterbatch through the following process: slicing → pulse conveyor → large wet slicing silo → pulse conveyor → pre-crystallizer → drying tower → extruder → melt distribution pipe → spinning box → metering pump → composite spinning component → side blowing → bundling oiling → winding → chemical fiber to obtain a composite conductive fiber with PET as the matrix; in S1, the conductive masterbatch includes the following raw materials in parts by mass: polypropylene (PP): 110 parts, conductive carbon black: 15 parts, carbon black dispersant: 8 parts, processing aid: 25 parts, magnetite powder: 13 parts.
[0040] S2: Secondly, blended yarn needs to be prepared. First, a certain amount of composite conductive fiber and cotton fiber are torn loose by hand, and then put into a small wool mixing machine for full mixing for 20-25 minutes. Then, the mixed fibers are fed into a small carding machine for carding into a net and strips, and then the conductive fiber blended yarn is obtained by a small spinning machine. In S2, the rotation speed of the small carding machine is 28r / min, and the mixing ratio of the composite conductive fiber and the cotton fiber is 1:1.
[0041] S3: Next, the electrostatic material is pretreated. Water and an antistatic agent are mixed in a ratio of 3:1 to form a mixture, and the mixture is sprayed on the conductive fiber blended yarn. The sprayed conductive fiber blended yarn is then left to stand for 22.5 hours. In S3, the volume of water is 17 times the volume of the antistatic agent, and the weight of the mixture accounts for 18% of the total weight of the nylon fiber raw material and the mixture.
[0042] S4: Next, the silver-plated fiber blended yarn is prepared. First, the silver-plated short fibers are manually loosened, a spinning aid is added in a ratio of 2:1, and the mixture is fully mixed and placed for 6 hours. The mixture is then fed into a carding machine together with the conductive fiber blended yarn to form a raw sliver. The yarn is then passed through a roving machine for 25 minutes, a spinning machine for 13 minutes, and finally a winding machine for 8 minutes to form the silver-plated fiber blended yarn.
[0043] S5: Then, a textile treatment is performed to weave the silver-plated fiber blended yarn into knitted fabrics with different weft knitted patterns on a weft knitted single-sided jacquard circular machine;
[0044] S6: Put the knitted grey fabric into the dyeing vat after being prepared, and add water according to the weight of the grey fabric. Then, put the grey fabric into the dyeing vat, and inject dye and auxiliary agent into the dyeing vat through the dyeing vat barrel. The ratio of dye and auxiliary agent is 3:1. Heat the dyeing vat at 105℃ and 2Mpa, and keep it warm for 35 minutes. Then cool it down to 75℃ and the pressure of the vat is 0.15Mpa. Open the vat cover, wash the sample water out of the vat, and dehydrate the grey fabric.
[0045] S7: Next, the grey cloth is subjected to antistatic post-treatment. The fabric is first immersed in the finishing liquid at room temperature for 35 minutes, then rolled dry with a rolling rate of 37%, and finally dried at a temperature of 168°C. In S7, the components of the finishing liquid and the weight percentage of each component are: 10% polyurethane resin, 18% softener, 0.2% fatty alcohol polyoxyethylene ether, 2.5% citric acid, and the rest is water.
[0046] S8: Next, the grey cloth is shaped. First, the fabric is soaked in water with sodium chloride at 40°C for 75 minutes; then an oxidant is added, and the temperature of the oxidation process is maintained at 60°C for 45 minutes; then a softener is added, and the temperature of the softening process is maintained at 38°C for 25 minutes; then a reducing agent is added, and the temperature of the reduction process is maintained at 45°C for 34 minutes to obtain the prepared antistatic fabric; in S8, the mass ratio of sodium chloride to fabric is about 1:180, the mass ratio of the oxidant to fabric is 1:110, the mass ratio of the softener to fabric is 1:100, and the mass ratio of the reducing agent to fabric is 1:120.
[0047] S9: Next, the antistatic fabric is cut to the required size by a cutting machine, and the style can be designed by an automatic cutting bed; in S9, the model of the cutting machine is QY-650TH, and the maximum cutting thickness of the cutting machine is 2mm.
[0048] S10: After the fabric is cut into the required shape, the fabric is printed by a printing machine, and the reactive dye gravure ink is directly sprayed onto the designed pattern formed on the PET film, and then the pattern on the PET film is transferred to the fabric;
[0049] S11: Next, the fabric is sewn into a T-shirt shape by human labor using a sewing machine. When the sewing is completed, the extra thread ends during the sewing process are manually removed, and the sewing machine is quality inspected to obtain a complete anti-static T-shirt. In S11, the needle length of the sewing machine is 3.5mm, the sewing thickness is 1.5mm, the thread pulling pressure is 3kg, and the thread pulling force setting accuracy is 0.1kg.
[0050] Example 3
[0051] S1: Before producing antistatic T-shirts, it is necessary to first select the processing fabrics of the T-shirts. In the existing method of selecting an antistatic fabric for production and processing, it is first necessary to take a piece of polyester resin and conductive masterbatch through the following process: slicing → pulse conveyor → large wet slicing silo → pulse conveyor → pre-crystallizer → drying tower → extruder → melt distribution pipe → spinning box → metering pump → composite spinning component → side blowing → bundling oiling → winding → chemical fiber to obtain a composite conductive fiber with PET as the matrix; in S1, the conductive masterbatch includes the following raw materials in parts by mass: polypropylene (PP): 120 parts, conductive carbon black: 20 parts, carbon black dispersant: 12 parts, processing aid: 30 parts, magnetite powder: 14 parts.
[0052] S2: Secondly, blended yarn needs to be prepared. First, a certain amount of composite conductive fiber and cotton fiber are torn loose by hand, and then put into a small wool mixing machine for thorough mixing for 25 minutes. Then, the mixed fibers are fed into a small carding machine for combing into a net and strips, and then the conductive fiber blended yarn is obtained by a small spinning machine. In S2, the rotation speed of the small carding machine is 30r / min, and the mixing ratio of the composite conductive fiber and the cotton fiber is 1:1.
[0053] S3: Next, the electrostatic material is pretreated. Water and an antistatic agent are mixed in a ratio of 3:1 to form a mixture, and the mixture is sprayed on the conductive fiber blended yarn. The sprayed conductive fiber blended yarn is then left to stand for 25 hours. In S3, the volume of water is 21 times the volume of the antistatic agent, and the weight of the mixture accounts for 25% of the total weight of the nylon fiber raw material and the mixture.
[0054] S4: Next, the silver-plated fiber blended yarn is prepared. First, the silver-plated short fibers are loosened manually, a spinning aid is added in a ratio of 2:1, and the mixture is fully mixed and placed for 8 hours. The mixture is then fed into a carding machine together with the conductive fiber blended yarn to form a raw sliver. The yarn is then spun on a roving machine for 30 minutes, spun on a spinning machine for 15 minutes, and finally wound on a bobbin winder for 10 minutes to form the silver-plated fiber blended yarn.
[0055] S5: Then, a textile treatment is performed to weave the silver-plated fiber blended yarn into knitted fabrics with different weft knitted patterns on a weft knitted single-sided jacquard circular machine;
[0056] S6: Put the knitted grey fabric into the dyeing vat after being prepared, and add water according to the weight of the grey fabric. Then, put the grey fabric into the dyeing vat, and inject dye and auxiliary agent into the dyeing vat through the dyeing vat barrel. The ratio of dye and auxiliary agent is 3:1. Heat the dyeing vat at 110℃ and 2.5Mpa, keep it warm for 40 minutes, cool it down to 80℃, and the pressure of the vat is 0.2Mpa. Open the vat cover, wash the sample water out of the vat, and dehydrate the grey fabric.
[0057] S7: Next, the grey cloth is subjected to antistatic post-treatment, firstly, the fabric is immersed in the finishing liquid at room temperature for 40 minutes, then rolled dry with a rolling rate of 75%, and finally dried at a drying temperature of 170°C; in S7, the components of the finishing liquid and the weight percentage of each component are: 12% polyurethane resin, 23% softener, 0.3% fatty alcohol polyoxyethylene ether, 3.5% citric acid, and the rest is water.
[0058] S8: Next, the grey cloth is shaped. First, the fabric is soaked in water with sodium chloride added at 55°C for 85 minutes; then an oxidant is added, and the temperature of the oxidation process is maintained at 65°C for 50 minutes; then a softener is added, and the temperature of the softening process is maintained at 40°C for 30 minutes; then a reducing agent is added, and the temperature of the reduction process is maintained at 50°C for 38 minutes to obtain the prepared antistatic fabric; in S8, the mass ratio of sodium chloride to fabric is about 1:180, the mass ratio of the oxidant to fabric is 1:110, the mass ratio of the softener to fabric is 1:100, and the mass ratio of the reducing agent to fabric is 1:120.
[0059] S9: Next, the antistatic fabric is cut to the required size by a cutting machine, and the style can be designed by an automatic cutting bed; in S9, the model of the cutting machine is QY-650TH, and the maximum cutting thickness of the cutting machine is 3mm.
[0060] S10: After the fabric is cut into the required shape, the fabric is printed by a printing machine, and the reactive dye gravure ink is directly sprayed onto the designed pattern formed on the PET film, and then the pattern on the PET film is transferred to the fabric;
[0061] S11: Next, the fabric is sewn into a T-shirt shape using a sewing machine manually. When the sewing is completed, the extra thread ends during the sewing process are manually removed, and the sewing machine is quality inspected to obtain a complete anti-static T-shirt. In S11, the stitch length of the sewing machine is 4mm, the sewing thickness is 2mm, the thread pulling pressure is 4kg, and the thread pulling force setting accuracy is 0.2kg.
[0062] Before producing antistatic T-shirts, a piece of polyester resin and conductive masterbatch must be prepared through the following processes: slicing → pulse conveyor → large wet slicing bin → pulse conveyor → pre-crystallizer → drying tower → extruder → melt distribution pipe → spinning box → metering pump → composite spinning assembly → side blowing → bundling oiling → winding → chemical fiber to obtain composite conductive fiber with PET as the matrix;
[0063] Further, to prepare blended yarn, a certain amount of composite conductive fiber and cotton fiber are first torn loose by hand, and then put into a small wool mixing machine for full mixing for 25 minutes, and then the mixed fiber is fed into a small carding machine for carding into a web and strips, and then the conductive fiber blended yarn is obtained by a small spinning machine;
[0064] Furthermore, the electrostatic material is pretreated, water and an antistatic agent are mixed in a ratio of 3:1 to prepare a mixture, the mixture is sprayed on the conductive fiber blended yarn, and the sprayed conductive fiber blended yarn is left to stand for 245 hours;
[0065] Furthermore, the silver-plated fiber blended yarn is prepared by manually loosening the silver-plated staple fibers, adding a spinning aid in a ratio of 2:1, and fully mixing and standing for 8 hours, and then feeding the conductive fiber blended yarn into a carding machine together with the conductive fiber blended yarn to form a raw sliver, and then passing through a roving machine for 30 minutes of roving, a spinning machine for 15 minutes of spun yarn, and finally winding the yarn through a winding machine for 10 minutes to form the silver-plated fiber blended yarn, and then performing a textile treatment, and knitting the silver-plated fiber blended yarn on a weft knitting single-sided jacquard large circular machine into a knitted fabric with different weft knitting patterns;
[0066] Further, the knitted grey fabric is put into the dyeing vat, water is added according to the weight of the grey fabric, the grey fabric is beaten into the dyeing vat, dye and auxiliary agent are beaten into the dyeing vat through the dyeing vat barrel, the ratio of dye and auxiliary agent is 3:1, the dyeing vat is heated to 110°C, the pressure is 2.5Mpa, and the temperature is kept for 40 minutes, and the temperature is cooled to 80°C, the cylinder pressure is 0.2Mpa, the cylinder cover is opened, the sample water is washed out of the cylinder, and the grey fabric is dehydrated;
[0067] Further, the grey cloth is subjected to antistatic post-treatment, firstly, the fabric is immersed in the finishing liquid at room temperature for 40 minutes, then rolled dry, the rolling rate is 75%, and finally dried at 170°C; next, the grey cloth is shaped, firstly, the fabric is immersed in 55°C water with sodium chloride added for 85 minutes; then, an oxidant is added, and the oxidation process temperature is maintained at 65°C for 50 minutes; then, a softener is added, and the softening process temperature is maintained at 40°C for 30 minutes; then, a reducing agent is added, and the reduction process temperature is maintained at 50°C for 38 minutes, to obtain the prepared antistatic fabric;
[0068] Furthermore, the antistatic fabric is cut to the required size by a cutting machine, and the style can be designed by an automatic cutting bed; after the fabric is cut to the required shape, it is printed by a printing machine, and the reactive dye gravure ink is directly sprayed onto the designed pattern formed on the PET film, and then the pattern on the PET film is transferred to the fabric; then the fabric is sewn into a T-shirt shape using a sewing machine by manpower, and when the sewing is completed, the extra thread ends during the sewing process are manually subtracted, and the sewing machine is quality inspected to obtain a complete antistatic T-shirt.
[0069] In the present invention, the antistatic material required for the antistatic T-shirt is pre-treated and post-treated, and then woven and dyed to obtain the fabric required for preparing the T-shirt, and then the antistatic fabric is cut and printed, and finally the fabric is sewn into the required T-shirt by manpower using a sewing machine, so that the entire T-shirt can be anti-static, certain safety hazards are reduced, and people can have closer contact in daily life.
[0070] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A production process for antistatic T-shirts, It is characterized in that The following steps are involved: S1: Before producing antistatic T-shirts, you first need to select the processing fabrics of the T-shirts. In the existing process of selecting an antistatic fabric for production and processing, you first need to take a piece of polyester resin and conductive masterbatch through the following processes: slicing → pulse conveyor → wet slicing large silo → pulse conveyor → pre-crystallizer → drying tower → extruder → melt distribution pipe → spinning box → metering pump → composite spinning assembly → side blowing → bundling oiling → winding → chemical fiber to obtain a composite conductive fiber with PET as the matrix; S2: Secondly, blended yarn needs to be prepared. First, a certain amount of composite conductive fiber and cotton fiber are torn loose by hand, and then put into a small wool mixing machine for full mixing for 20-25 minutes. Then, the mixed fiber is fed into a small carding machine for carding into a web and strips, and then the conductive fiber blended yarn is obtained by a small spinning machine; S3: Next, the electrostatic material is pretreated, water and antistatic agent are mixed in a ratio of 3:1 to prepare a mixture, the mixture is sprayed on the conductive fiber blended yarn, and the sprayed conductive fiber blended yarn is left to stand for 20-25 hours; S4: Next, prepare the silver-plated fiber blended yarn. First, manually loosen the silver-plated staple fibers, add a spinning aid in a ratio of 2:1, fully mix, and place for 5-8 hours. Then, feed the conductive fiber blended yarn into a carding machine together with the conductive fiber blended yarn to form a raw sliver. Then, the yarn is passed through a roving machine for 20-30 minutes, and then through a spinning machine for 10-15 minutes. Finally, the silver-plated fiber blended yarn is wound on a bobbin machine for 5-10 minutes. S5: Then, a textile treatment is performed to weave the silver-plated fiber blended yarn into knitted fabrics with different weft knitted patterns on a weft knitting single-sided jacquard circular machine; S6: Put the knitted grey fabric into the dyeing vat after being prepared, inject water according to the weight of the grey fabric, beat the grey fabric into the dyeing vat, and inject dye and auxiliary agent into the dyeing vat through the dyeing vat barrel. The ratio of dye and auxiliary agent is 3:
1. Heat the dyeing vat at 100-110℃ and pressure of 1.5-2.5Mpa, keep warm for 30-40 minutes, cool down to 70-80℃, and the cylinder pressure is 0.1-0.2Mpa. Open the cylinder cover to wash the sample water out of the cylinder, and dehydrate the grey fabric; S7: Next, the grey cloth is subjected to antistatic post-treatment, firstly, the fabric is placed in the finishing liquid and soaked at room temperature for 30 to 40 minutes, then rolled dry, with a rolling rate of 60 to 75%, and finally dried at a drying temperature of 165 to 170°C; S8: Next, the grey fabric is shaped. First, the fabric is soaked in water with sodium chloride added at 30-55°C for 65-85 minutes; then an oxidant is added, and the temperature of the oxidation process is maintained at 55-65°C for 40-50 minutes; then a softener is added, and the temperature of the softening process is maintained at 35-40°C for 20-30 minutes; then a reducing agent is added, and the temperature of the reduction process is maintained at 40-50°C for 30-38 minutes, to obtain the prepared antistatic fabric; S9: Next, the antistatic fabric is cut to the required size by a cutting machine, and the style can be designed by an automatic cutting bed; S10: After the fabric is cut into the required shape, the fabric is printed by a printing machine, and the reactive dye gravure ink is directly sprayed onto the designed pattern formed on the PET film, and then the pattern on the PET film is transferred to the fabric; S11: Next, the fabric is sewn into a T-shirt shape by human labor using a sewing machine. When the sewing is completed, the extra thread ends during the sewing process are manually removed, and the sewing machine is quality inspected to obtain a complete antistatic T-shirt.
2. The antistatic T-shirt production process according to claim 1, It is characterized in that In S1, the conductive masterbatch is made of the following raw materials in parts by mass: polypropylene (PP): 100-120 parts, conductive carbon black: 10-20 parts, carbon black dispersant: 5-12 parts, processing aid: 20-30 parts, magnetite powder: 12-14 parts.
3. The antistatic T-shirt production process according to claim 1, It is characterized in that In the S2, the rotation speed of the small carding machine is 25-30r / min, and the mixing ratio of the composite conductive fiber and the cotton fiber is 1:
1.
4. The antistatic T-shirt production process according to claim 1, It is characterized in that In S3, the volume of water is 11 to 21 times the volume of the antistatic agent, and the weight of the mixture accounts for 10% to 25% of the total weight of the nylon fiber raw material and the mixture.
5. The antistatic T-shirt production process according to claim 1, It is characterized in that In S7, the components of the finishing liquid and the weight percentage of each component are: 5-12% polyurethane resin, 13-23% softener, 0.1-0.3% fatty alcohol polyoxyethylene ether, 1.5-3.5% citric acid, and the rest is water.
6. The antistatic T-shirt production process according to claim 1, Features In the S8, the mass ratio of sodium chloride to fabric is about 1:180, the mass ratio of oxidant to fabric is 1:110, the mass ratio of softener to fabric is 1:100, and the mass ratio of reducing agent to fabric is 1:
120.
7. The antistatic T-shirt production process according to claim 1, Features ,In the S9, the model of the cutting machine is QY-650TH, and the maximum cutting thickness of the cutting machine is 1-3mm.
8. The antistatic T-shirt production process according to claim 1, Features In the S11, the needle length of the sewing machine is 2.5-4mm, the sewing thickness is 0.8-2mm, the thread head pressure is 2-4kg, and the thread head tension setting accuracy is -0.2-0.2kg.