Preparation method of matrix pressure sensor
By using IC process and hole plug structure in thin film pressure sensors, the lattice density is improved and the space requirements are reduced, the problem of low lattice density in the existing technology is solved, and the efficient manufacturing and multiple matrix pressure sensors are realized. application.
Patent Information
- Application Number
- CN202411152780.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-08-21
AI Technical Summary
The low lattice density of existing thin film pressure sensors leads to large sensor space requirements, limiting their application.
By providing the first substrate and the second substrate, a bonding medium is formed and through the pore column is filled with a strained layer with a thickness higher than the bonding medium, removing the isolation layer to form a cavity, and forming a hole plug at the pore position to seal the cavity, Matrix pressure sensors are manufactured using IC process.
The sensor lattice density is improved, the space requirements are reduced, and the manufacturing process of matrix pressure sensors is reliable and stable, and it supports the application of resistive and capacitive matrix pressure sensors.
Smart Images

Figure CN118936691A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductors, and in particular to a method for preparing a matrix pressure sensor. Background Art
[0002] Pressure sensors are commonly used in touch screens, robot perception, medical equipment, etc. By arranging multiple pressure sensors in a matrix, pressure changes at multiple points can be detected simultaneously, providing a high-resolution pressure distribution map.
[0003] At present, thin-film pressure sensors are all made based on printing technology, and the interface part adopts piercing cold-pressed terminals. Due to the influence of its manufacturing process and interface, multiple pressure sensor chips can only be packaged into a dot matrix at the back end, which has the problem of large sensor space requirements and low dot matrix density, which greatly limits the application of thin-film pressure sensors.
[0004] Therefore, how to increase the density of sensor arrays while reducing sensor space requirements has become a technical problem that the industry urgently needs to solve. Summary of the invention
[0005] The present invention provides a method for preparing a matrix pressure sensor, which solves the technical problem of how to increase the sensor dot density and reduce the sensor space requirement.
[0006] According to a first aspect of the present invention, an embodiment of the present invention provides a method for preparing a matrix pressure sensor, comprising:
[0007] Step S1: providing a first substrate and a second substrate;
[0008] Step S2: forming a first bonding medium on the surface of the first substrate;
[0009] Step S3: bonding the first substrate and the second substrate via the first bonding medium;
[0010] Step S4: forming a hole column on the surface of the second substrate, wherein the hole column penetrates the second substrate and the first bonding medium;
[0011] Step S5: depositing an isolation layer on the sidewall of the hole column;
[0012] Step S6: filling a strain layer in the pore column, wherein the thickness of the strain layer is greater than the thickness of the first bonding medium;
[0013] Step S7: removing the isolation layer and the first bonding medium to form a cavity;
[0014] Step S8: forming a hole plug at the position where the hole column is located in the second substrate to seal the cavity.
[0015] Optionally, the step S5 includes:
[0016] Step S51: depositing an isolation material layer on the second substrate, wherein the isolation material layer covers the surface of the pore column and covers other areas of the second substrate;
[0017] Step S52: etching the isolation material layer on the surface of the second substrate and the isolation material layer at the bottom of the hole column to form the isolation layer.
[0018] Optionally, forming the hole plug in step S8 includes:
[0019] The second substrate at the hole column is subjected to epitaxy to form a first epitaxial layer, and the hole column is sealed to form a hole plug at the position where the hole column is located in the second substrate.
[0020] Optionally, after step S8, the method further includes:
[0021] The first mask layer is removed.
[0022] Optionally, step S6 includes:
[0023] The first substrate at the bottom of the hole column is epitaxially grown to form the strained layer.
[0024] Optionally, a material of the strain layer is different from a material of the isolation layer.
[0025] Optionally, the material of the strained layer includes single crystal silicon, silicon germanium and phosphorus silicon.
[0026] Optionally, the cross-sectional length of the strain layer is 1 nm to 10 um.
[0027] Optionally, after step S8, the method further includes:
[0028] A first metal plate and a second metal plate are deposited on the first substrate and the second substrate respectively, wherein the first metal plate corresponds to an upper surface of the cavity, and the second metal plate corresponds to a lower surface of the cavity.
[0029] Compared with the prior art, the technical solution of the embodiment of the present invention has the following beneficial effects:
[0030] In the preparation method of the matrix pressure sensor of the technical solution of the present invention, the IC process is used to manufacture the matrix pressure sensor, by providing a first substrate and a second substrate; forming a first bonding medium on the surface of the first substrate; bonding the first substrate and the second substrate through the first bonding medium; forming a hole column on the surface of the second substrate, the hole column penetrates the second substrate and the first bonding medium; depositing an isolation layer on the side wall of the hole column; filling the hole column with a strain layer, the thickness of the strain layer is higher than the thickness of the first bonding medium; removing the isolation layer and the first bonding medium to form a cavity; forming a hole plug at the position where the hole column is located on the second substrate to seal the cavity, so that the manufacturing process of the present invention is reliable and stable, and the sensor dot density formed on the substrate is high, while reducing the sensor space requirement.
[0031] Furthermore, the present invention utilizes the change in the cross-section of the strain layer when subjected to stress, or the deformation of the upper and lower plates of the cavity when subjected to stress, so that the matrix pressure sensor manufactured by the present invention can be used as both a resistive matrix pressure sensor and a capacitive matrix pressure sensor. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0033] Figure 1 is a schematic flow chart of a method for preparing a matrix pressure sensor in one embodiment of the present invention;
[0034] Figure 2 to Figure 4 FIG. 1 is a schematic diagram of the manufacturing process of a matrix pressure sensor according to an embodiment of the present invention. Figure 1 ;
[0035] Figure 5 is a schematic flow chart of a method for preparing a matrix pressure sensor in another embodiment of the present invention;
[0036] Figure 6 FIG. 1 is a schematic diagram of the manufacturing process of a matrix pressure sensor according to an embodiment of the present invention. Figure 2 ;
[0037] Figure 7 is a schematic flow chart of a method for preparing a matrix pressure sensor in another embodiment of the present invention;
[0038] Figure 8 to Figure 15 FIG. 1 is a schematic diagram of the manufacturing process of a matrix pressure sensor according to an embodiment of the present invention. Figure 2 ;
[0039] Figure 16-17 1 is a schematic diagram of the principle of a matrix pressure sensor according to an embodiment of the present invention;
[0040] Figures 18 to 20 FIG. 1 is a schematic diagram of the manufacturing process of a matrix pressure sensor according to an embodiment of the present invention. Figure 3 ;
[0041] Description of reference numerals:
[0042] 101- first substrate;
[0043] 201- second substrate;
[0044] 301-first mask layer;
[0045] 401-isolating material layer;
[0046] 402-Isolation layer;
[0047] 501-hole column;
[0048] 502- strain layer;
[0049] 60-medium support beam;
[0050] 601-first medium support beam;
[0051] 602-second medium support beam;
[0052] 603- dielectric layer;
[0053] 701- first epitaxial layer;
[0054] 801- first metal plate;
[0055] 802- Second metal plate. DETAILED DESCRIPTION
[0056] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0057] The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0058] The technical solution of the present invention is described in detail with specific embodiments below. The following specific embodiments can be combined with each other, and the same or similar concepts or processes may not be described in detail in some embodiments.
[0059] As described in the background art, it is difficult to increase the sensor array density and reduce the sensor space requirement when manufacturing a pressure sensor in the prior art.
[0060] In view of this, the present invention provides a method for preparing a matrix pressure sensor, which comprises providing a first substrate and a second substrate; forming a first bonding medium on the surface of the first substrate; bonding the first substrate and the second substrate through the first bonding medium; forming a hole column on the surface of the second substrate, the hole column penetrating the second substrate and the first bonding medium; depositing an isolation layer on the side wall of the hole column; filling the hole column with a strain layer, the thickness of the strain layer being higher than the thickness of the first bonding medium; removing the isolation layer and the first bonding medium to form a cavity; forming a hole plug at the position where the hole column is located on the second substrate to seal the cavity. The present invention uses IC technology to manufacture a matrix pressure sensor, and while the process is reliable and stable, the density of the sensor dot matrix formed on the substrate is high, and the sensor space requirement is reduced.
[0061] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0062] Please refer to Figure 1 The present invention proposes a method for preparing a matrix pressure sensor, comprising:
[0063] Step S1: providing a first substrate and a second substrate;
[0064] Step S2: forming a first bonding medium on the surface of the first substrate;
[0065] Step S3: bonding the first substrate and the second substrate via the first bonding medium;
[0066] Step S4: forming a hole column on the surface of the second substrate, wherein the hole column penetrates the second substrate and the first bonding medium;
[0067] Step S5: depositing an isolation layer on the sidewall of the hole column;
[0068] Step S6: filling a strain layer in the pore column, wherein the thickness of the strain layer is greater than the thickness of the first bonding medium;
[0069] Step S7: removing the isolation layer and the first bonding medium to form a cavity;
[0070] Step S8: forming a hole plug at the position where the hole column is located in the second substrate to seal the cavity.
[0071] It can be seen that the present invention manufactures the matrix pressure sensor by utilizing the IC process. While the process is reliable and stable, the density of the sensor dot matrix formed on the substrate is relatively high, and the sensor space requirement is reduced.
[0072] Please refer to Figure 2 to Figure 20 , shows a structural schematic diagram of the preparation process of the matrix pressure sensor according to an embodiment of the present invention.
[0073] Please refer to Figure 2 , providing a first substrate 101 and a second substrate 201.
[0074] As an example, the first substrate 101 and the second substrate 201 can both be silicon substrates. Of course, the present invention is not limited to this, and SOI substrates, ceramic substrates, etc. can also be used. According to the needs of actual applications, the substrate materials used by the first substrate 101 and the second substrate 201 can also be different. Technicians in this field can use appropriate materials according to design requirements.
[0075] It should be understood that the thickness of the first substrate 101 and the thickness of the second substrate 201 in the embodiment of the present invention may be the same, or appropriate thicknesses may be selected according to needs.
[0076] Please refer to Figure 3 , a first bonding medium 102 is formed on the surface of the first substrate 101 .
[0077] In the embodiment of the present invention, the material of the first bonding medium 102 is silicon oxide, but the present invention is not limited thereto, and those skilled in the art may select a suitable material as the bonding medium as needed, for example, silicon nitride, polysilicon, silicon carbide, etc.
[0078] Please refer to Figure 4, the first substrate 101 and the second substrate 201 are bonded through the first bonding medium 102 .
[0079] Please continue to refer to Figure 1 , executing step S4: forming a hole column on the surface of the second substrate, wherein the hole column penetrates the second substrate and the first bonding medium.
[0080] In one implementation, please refer to Figure 5 , the step S4 includes:
[0081] Step S41: forming a first mask layer on the second substrate;
[0082] Step S42: performing a first patterning on the first mask layer to form a first patterned mask layer;
[0083] Step S43: using the first patterned mask layer as a mask and the interface between the first bonding medium and the first substrate as an etching stop layer, etching the second substrate and the first bonding medium in sequence to form the hole column.
[0084] Now combined Figure 6 Provide explanation.
[0085] Please refer to Figure 6 , a first mask layer 301 is formed on the second substrate 201, and the first mask layer 301 is patterned for the first time to form a first patterned mask layer, and the first patterned mask layer is used as a mask and the interface between the first bonding medium 102 and the first substrate 101 is used as an etching stop layer, and the second substrate 201 and the first bonding medium 102 are etched in sequence to form the hole column 501.
[0086] Please continue to refer to Figure 1 , execute step S5: deposit an isolation layer on the side wall of the hole column.
[0087] In one implementation, please refer to Figure 7 , the step S5 comprises:
[0088] Step S51: depositing an isolation material layer on the second substrate, wherein the isolation material layer covers the surface of the pore column and covers other areas of the second substrate;
[0089] Step S52: etching the isolation material layer on the surface of the second substrate and the isolation material layer at the bottom of the hole column to form the isolation layer.
[0090] Now combined Figure 8-Figure 9 Provide explanation.
[0091] Please refer to Figure 8, an isolation material layer 401 is deposited on the second substrate 201 , and the isolation material layer 401 covers the surface of the pore column 501 and covers other areas of the second substrate 201 .
[0092] The isolation material layer 401 can be regarded as a thin film, and its material can be nitride, silicon oxynitride or silicon oxide, etc. The present invention is not limited to this, and those skilled in the art can select a suitable material as needed.
[0093] Please refer to Fig. 9 , the isolation material layer 401 on the surface of the second substrate 201 and the isolation material layer 401 at the bottom of the hole column 501 are etched to form the isolation layer 402.
[0094] In a specific implementation, the isolation material layer 401 on the surface of the second substrate 201 and the isolation material layer 401 at the bottom of the hole column 501 are dry-etched to form the isolation layer 402 .
[0095] Please refer to Fig.10 , a strain layer 502 is filled in the hole column 501 , and the thickness of the strain layer 502 is higher than the thickness of the first bonding medium 102 .
[0096] In the embodiment of the present invention, the material of the strained layer 502 is different from the material of the isolation layer 402. For example, the material of the strained layer 502 may be single crystal silicon, germanium silicon, phosphorus silicon, and the like.
[0097] Taking the material of the strained layer 502 as single crystal silicon as an example, in one embodiment, the method of filling the strained layer in the hole column in step S6 includes:
[0098] The first substrate at the bottom of the hole column is epitaxially grown to form the strained layer.
[0099] In practical applications, the present invention can select a suitable cross-section of the single crystal silicon column according to the sensitivity of pressure. The smaller the cross-sectional area, the greater the deformation when receiving pressure and the higher the sensitivity. In a specific implementation, the cross-sectional length of the strain layer 502 is 1nm~10um.
[0100] Please refer to Fig.11 , remove the isolation layer 402 and the first bonding medium 102 to form a cavity.
[0101] In one implementation, the isolation layer 402 and the first bonding medium 102 may be removed by a dry etching process or a wet etching process.
[0102] After this process, the top view of the matrix pressure sensor can be as follows: Fig.12 As shown, the matrix pressure sensor further includes a dielectric support beam 60 , and the dielectric support beam 60 surrounds the periphery of the matrix pressure sensor.
[0103] In other embodiments, please refer to Fig.13 , the dielectric support beam 60 includes a first dielectric support beam 601, a dielectric layer 603 and a second dielectric support beam 602;
[0104] The dielectric layer 603 is located between the first dielectric support beam 601 and the second dielectric support beam 602 .
[0105] Of course, the present invention does not limit the top shape of the matrix pressure sensor, and those skilled in the art can select a suitable structure as needed.
[0106] Please continue to refer to Figure 1 , executing step S8: forming a hole plug at the position where the hole column is located in the second substrate to seal the cavity.
[0107] In one embodiment, the method for forming the hole plug in step S8 includes:
[0108] The second substrate at the hole column is subjected to epitaxy to form a first epitaxial layer, and the hole column is sealed to form a hole plug at the position where the hole column is located in the second substrate.
[0109] Now combined Fig.14 Provide explanation.
[0110] Please refer to Fig.14 , epitaxially grow the second substrate 201 at the hole column 501 to form a first epitaxial layer 701 , and seal the hole column 501 to form a hole plug at the position where the hole column 501 is located in the second substrate 201 .
[0111] It should be understood that the present invention does not limit whether the material of the first epitaxial layer 701 is the same as that of the second substrate 201 .
[0112] Please refer to Fig.15 , remove the first mask layer 301.
[0113] exist Fig.15 In the matrix pressure sensor formed by the example of , the pressure can be measured by resistance, that is, the deformation of the column of the strain layer 502 is controlled to change greatly during measurement, and the volume of the cavity changes slightly; its schematic diagram can be as follows Fig.16 As shown, Fig.16 R bodyIt can be understood as the resistance of the column of the strain layer 502. Specifically, when the sensor is subjected to external force, the column of the strain layer 502 is deformed, its cross-sectional area increases, and the output resistance decreases. When the external force is removed, the deformation of the column of the strain layer 502 disappears, and the original shape is restored, the cross-sectional area decreases, and the output resistance of the sensor increases.
[0114] In other application modes, pressure can also be measured by capacitance, that is, when measuring, the deformation change of the column of the strain layer 502 is controlled to be small, and the change of the cavity volume is large; its principle diagram can be as follows Fig.17 As shown. Fig.17 In the example, it can be seen that for the resistive array pressure sensor, the connection between adjacent rows and columns has the function of parallel capacitance in addition to the on-resistance.
[0115] In actual work, Fig.17 When the sensing unit in the example is turned on, its parallel capacitor stores charge. When switching to another sensing unit, the charge of the capacitor corresponding to the unit needs time to discharge. The discharge time is determined by the RC network composed of resistors and capacitors. The specific design application depends on the product requirements.
[0116] In practical applications, if the pressure is measured by capacitance, the thickness of the second substrate 201 can be appropriately reduced, or a metal layer can be deposited between the upper plate and the lower plate to enhance the effect of capacitance change.
[0117] Specifically, please refer to Fig.18 A first metal plate 801 and a second metal plate 802 are deposited on the first substrate 101 and the second substrate 201 respectively, wherein the first metal plate 801 corresponds to the upper surface of the cavity, and the second metal plate 802 corresponds to the lower surface of the cavity.
[0118] In practical applications, the deposition of the first metal plate 801 and the second metal plate 802 can be completed after step S2 and before step S3 .
[0119] By controlling the thickness of the first metal plate, the sensitivity of capacitive sensing can also be controlled. In a specific implementation, the thickness of the first metal plate 801 can be controlled after the above bonding process. For example, the thickness of the first metal plate 801 can be reduced by a CMP process.
[0120] Considering that when etching the first metal plate 801, the exposed second substrate 201 may be lost, Fig.18 In the example, the surface of the strain layer 502 is flush with the surface of the second substrate 201, which does not affect the actual use effect.
[0121] The top view of the matrix pressure sensor for measuring pressure by capacitance can be shown as follows: Fig.19 As shown, the matrix pressure sensor further includes a dielectric support beam 60 , and the dielectric support beam 60 surrounds the matrix pressure sensor.
[0122] In other embodiments, please refer to Fig. 20 , the dielectric support beam 60 includes a first dielectric support beam 601, a dielectric layer 603 and a second dielectric support beam 602;
[0123] The dielectric layer 603 is located between the first dielectric support beam 60 and the second dielectric support beam 60 .
[0124] It can be seen that the present invention utilizes the change in the cross-section of the strain layer when subjected to force, or the deformation of the upper and lower plates of the cavity when subjected to force, so that the matrix pressure sensor manufactured by the present invention can be used as both a resistive matrix pressure sensor and a capacitive matrix pressure sensor.
[0125] In summary, the embodiment of the present invention utilizes the IC process to manufacture a matrix pressure sensor, by providing a first substrate and a second substrate; forming a first bonding medium on the surface of the first substrate; bonding the first substrate and the second substrate through the first bonding medium; forming a hole column on the surface of the second substrate, the hole column penetrating the second substrate and the first bonding medium; depositing an isolation layer on the side wall of the hole column; filling the hole column with a strain layer, the thickness of the strain layer being higher than the thickness of the first bonding medium; removing the isolation layer and the first bonding medium to form a cavity; forming a hole plug at the position where the hole column is located on the second substrate to seal the cavity, so that the manufacturing process of the present invention is reliable and stable, and the sensor dot matrix density formed on the substrate is high, while reducing the sensor space requirement.
[0126] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for preparing a matrix pressure sensor, characterized in that: include: Step S1: providing a first substrate and a second substrate; Step S2: forming a first bonding medium on the surface of the first substrate; Step S3: bonding the first substrate and the second substrate via the first bonding medium; Step S4: forming a hole column on the surface of the second substrate, wherein the hole column penetrates the second substrate and the first bonding medium; Step S5: depositing an isolation layer on the sidewall of the hole column; Step S6: filling a strain layer in the pore column, wherein the thickness of the strain layer is greater than the thickness of the first bonding medium; Step S7: removing the isolation layer and the first bonding medium to form a cavity; Step S8: forming a hole plug at the position where the hole column is located in the second substrate to seal the cavity.
2. The method for preparing a matrix pressure sensor according to claim 1, characterized in that: The step S4 includes: Step S41: forming a first mask layer on the second substrate; Step S42: performing a first patterning on the first mask layer to form a first patterned mask layer; Step S43: using the first patterned mask layer as a mask and the interface between the first bonding medium and the first substrate as an etching stop layer, etching the second substrate and the first bonding medium in sequence to form the hole column.
3. The method for preparing a matrix pressure sensor according to claim 2, characterized in that: The step S5 includes: Step S51: depositing an isolation material layer on the second substrate, wherein the isolation material layer covers the surface of the pore column and covers other areas of the second substrate; Step S52: etching the isolation material layer on the surface of the second substrate and the isolation material layer at the bottom of the hole column to form the isolation layer.
4. The method for preparing a matrix pressure sensor according to claim 3, characterized in that: The forming of the hole plug in step S8 includes: The second substrate at the hole column is subjected to epitaxy to form a first epitaxial layer, and the hole column is sealed to form a hole plug at the position where the hole column is located in the second substrate.
5. The method for preparing a matrix pressure sensor according to claim 4, characterized in that: After step S8, the method further includes: The first mask layer is removed.
6. The method for preparing a matrix pressure sensor according to claim 1, characterized in that: Step S6 includes: The first substrate at the bottom of the hole column is epitaxially grown to form the strained layer.
7. The method for preparing a matrix pressure sensor according to claim 1, characterized in that: The material of the strain layer is different from that of the isolation layer.
8. The method for preparing a matrix pressure sensor according to claim 6, characterized in that: The material of the strained layer includes single crystal silicon, silicon germanium and phosphorus silicon.
9. The method for preparing a matrix pressure sensor according to claim 6, characterized in that: The cross-sectional length of the strain layer is 1 nm to 10 um.
10. The method for preparing a matrix pressure sensor according to any one of claims 1 to 6, characterized in that: After step S8, the method further includes: A first metal plate and a second metal plate are deposited on the first substrate and the second substrate respectively, wherein the first metal plate corresponds to an upper surface of the cavity, and the second metal plate corresponds to a lower surface of the cavity.
Citation Information
Patent Citations
A sensor device and a method
CN103226024A
Capacitive and tactile sensors and related sensing methods
CN111051834A
Three-dimensional force sensing array sensor based on piezoelectric unit and pressure calculation method
CN111157151A
Array type pressure measuring device
CN112880902A
Array MEMS piezoresistive tactile sensor packaging design method
CN117819471A
Cited By
Pressure sensor chip and preparation method thereof
CN121364034A