Post-corrosion modeling method for metal surface with any initial morphology
By combining measurement and geometric measurement in corrosion environments with Monte Carlo method, the outline of the metal surface after corrosion is generated, and the problem of difficult to model irregular surfaces and inverse modeling in the prior art is solved, and the surface after corrosion is realized The accurate geometric modeling and surface roughness considerations improve the accuracy and efficiency of simulation results.
Patent Information
- Application Number
- CN202410999905.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-24
AI Technical Summary
The prior art is difficult to accurately model the irregular surface of the metal structure after corrosion, and the reverse modeling method has problems of poor accuracy and low efficiency, which cannot effectively reflect the surface roughness characteristics after corrosion, affecting the stress distribution analysis of structural parts.
By measuring the average corrosion depth and surface roughness parameters in a corrosion environment based on steel standard samples, combining geometric measurements and Monte Carlo method, the surface profile after corrosion is generated, and each point is moved along the method direction to determine the post-corrosion position, so as to achieve arbitrary Post-corrosion geometric modeling of the initial morphology metal surface.
Accurate modeling of the surface morphology after corrosion is achieved, which can quickly reflect the roughness characteristics of the metal structure after corrosion, and is suitable for irregular and regular surfaces, improving the accuracy and efficiency of simulation results.
Smart Images

Figure CN118937195A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for modeling a metal surface with arbitrary initial morphology after corrosion, and in particular to a method for geometric modeling of a corrosion surface taking into account the initial morphology of the metal surface and the roughness of the surface after corrosion. Background Art
[0002] Steel structures are widely used in various engineering structures such as long-span steel bridges, offshore platforms, and offshore wind power plants due to their advantages such as light weight and high strength. During their service life, these structures will be degraded by environmental corrosion, which will endanger the safety of the structure. Therefore, it is necessary to study the mechanical properties of steel structures after corrosion. However, corrosion tests have problems such as high economic cost, long time consumption, and limited specimen size. Therefore, it is necessary to carry out numerical analysis of the mechanical properties of corroded steel structures. The accurate establishment of the geometric model of the metal surface after corrosion is the basis for the finite element refinement analysis of corroded steel structures. At present, most of the modeling methods for the surface of steel structures after corrosion do not consider the roughness characteristics of the surface after corrosion, and cannot accurately reflect the morphological characteristics of the metal surface after corrosion, which will lead to the simulation results being unable to accurately reflect the influence of local corrosion characteristics on the stress distribution of structural parts. At the same time, most of the existing post-corrosion modeling methods can only be applied to regular geometric models and are difficult to apply to irregular surfaces, which makes it difficult to establish the post-corrosion morphology of metal structures such as welded structures, complex components, and additive manufacturing. The post-corrosion modeling method based on inverse modeling is difficult to separate from the corrosion test, and has problems such as poor accuracy and low efficiency. Therefore, in order to accurately establish the geometric model of the metal structure surface after corrosion, it is necessary to establish a corrosion surface geometric modeling method that takes into account the initial morphology of the metal surface and the surface roughness after corrosion. Summary of the invention
[0003] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a method for geometric modeling of a corrosion surface that takes into account the initial morphology of the metal surface and the roughness of the surface after corrosion. The method can be applied to the post-corrosion modeling of any initial surface, and can accurately reflect the roughness characteristics of the surface morphology after corrosion, thereby realizing the rapid modeling of the surface after corrosion of metal structural parts. The present invention can be used for the initial surface post-corrosion geometric modeling of irregular surfaces based on scanning coordinate information, and can also be used for the initial surface post-corrosion geometric modeling of regular surfaces based on feature point coordinate information.
[0004] The present invention provides a method for modeling a metal surface after corrosion with any initial morphology, comprising:
[0005] (a) Based on the average corrosion depth d of a standard steel sample, i.e. a small steel sample with a flat surface, after exposure to a corrosive environment for a time t u And surface roughness parameter S a ,S q ,S z, determine the development of surface corrosion characteristics over time, including d u -t,S a -d u ,S q -d u ,S z -d u ; wherein the S a ,S q ,S z They are the arithmetic mean height, root mean square height and maximum depth respectively;
[0006] (b) Determine the surface corrosion characteristics, including the average rust depth d, based on the exposure time t of the metal surface in the corrosive environment u And surface roughness parameter S a ,S q ,S z ;
[0007] (c) Based on the geometric measurement results, determine the initial surface profile and the surface profile length l, and determine the points P on the surface profile i Length of the path from the endpoint l i With point P i Coordinate (x i ,y i ) corresponding relationship;
[0008] (d) Based on the surface roughness parameter S a ,S q ,S z , through the Monte Carlo method, the length l of the path from the end point on the cross-sectional profile length l is generated i Each point P i Random corrosion amount d i ;
[0009] (e) Calculate the initial surface contour at each point P i The corresponding normal direction n i , establish each point P i Geometric information matrix G i =(x i ,y i ,l i ,n i );
[0010] (f) For each point P along the surface contour path i Along its normal direction n i The movement corresponds to the random corrosion amount d i , determine P i Move point P' i Coordinate (x' i ,y' i ), point P' iThat is the post-corrosion point P i Corresponding position.
[0011] According to a specific implementation method, in step (a), a small steel sheet sample with a flat surface is used to calibrate the development law of corrosion characteristics, and its geometric dimensions and mass need to be measured before being exposed to a corrosive environment.
[0012] According to a specific implementation method, in step (a), S a ,S q ,S z are the arithmetic mean height, root mean square height and maximum depth respectively. For the metal surface obtained by the corrosion exposure test, it can be calculated based on the following formula
[0013] According to a specific implementation method, in step (a), when it is impossible to carry out corrosion exposure test, the corrosion characteristic development law can be determined by existing metal environmental corrosion data. Among them, for structural steel, the corrosion rate can be determined according to "Atmospheric Corrosion of Metals and Alloys Part 1: Classification, Determination and Evaluation" (GB / T 19292.1-2018); the corrosion morphology characteristics can be calculated according to the following formula:
[0014] S a =0.0077×w+0.0031
[0015] S q =0.0096×w+0.0015
[0016] S z =0.0592×w+0.0544
[0017] Among them, w is the corrosion rate, w = (m0-m1) / m0, m0 is the initial mass, m1 is the mass after corrosion;
[0018] According to a specific implementation method, in step (a), according to different corrosion exposure time t corrosion characteristics d u ,S a ,S q ,S z , establish S a ,S q ,S z The average corrosion depth d u The corresponding relationship between
[0019] According to a specific implementation method, in step (b), the exposure time t is the exposure time of the established surface in the corrosive environment, which is the service life of the evaluated structural component;
[0020] According to a specific implementation method, in step (b), according to the d established in step (a), u -t relationship, determine the average corrosion depth d after corrosion u According to the S established in step (a) a -d u ,S q -d u ,S z -d u Relationship, determine the surface roughness parameter S after corrosion a ,S q ,S z ;
[0021] According to a specific implementation method, in the step (c), the initial surface profile is geometrically measured, and for surfaces with complex surface morphology, the coordinate information of each point on the surface profile can be obtained by laser scanning or other methods;
[0022] According to a specific implementation method, in step (c), the initial surface profile is geometrically measured. For a regular geometric surface, only the endpoint coordinates can be input, and interpolation is performed between the endpoints to obtain N data points P i The initial coordinate information of
[0023] According to a specific implementation method, in the step (c), the initial cross section is simplified into multiple broken lines by inputting the initial contour through the endpoint coordinates. The number of data points N in each broken line can be determined by the broken line length l. The number of data points N will affect the modeling accuracy of the surface contour after corrosion Δ=l / N. For modeling of the rough surface after corrosion, in order to ensure the authenticity of the morphology, it is recommended that Δ is not greater than 0.02mm;
[0024] According to a specific implementation method, in step (c), each point P on the surface profile i Length of the path from the endpoint l i is the distance from the end point of the section along the initial surface contour to point P i Circumference of the surface contour within the range;
[0025] According to a specific implementation method, in step (d), a one-dimensional rough surface is generated by a Monte Carlo method to generate a one-dimensional rough surface sample with a length of l and N data points. The generated rough surface corrosion feature d u ,S a ,S q ,S z Consistent with the parameters determined in claim 5, the longitudinal coordinates of each point on the rough surface are i Random corrosion amount d i ,i=1~N;
[0026] According to a specific implementation method, in step (d), the corrosion amount d of each point on the surface profile l is determined by step
[025] . i ,The number of corrosion points on the contour l is N, i = 1~N;
[0027] According to a specific implementation method, in step (e), each point P on the surface profile l is determined i Normal n i , and each point P i The geometric information is stored in the geometric information matrix G i =(x i ,y i ,l i ,n i ), i=1~N;
[0028] According to a specific implementation method, in step (f), it is considered that the corrosion develops in the direction perpendicular to the metal surface toward the inside of the metal matrix, that is, at each point P along the surface contour path i Along its normal direction n i Movement corresponding to corrosion amount d i , determine P i After moving P' i Point coordinates (x' i ,y' i ), point P' i That is the post-corrosion point P i Corresponding position.
[0029] The beneficial effects of the present invention include: the method can take into account any initial morphology of metal surfaces during the corrosion development process, and realize geometric modeling of surfaces with complex initial morphology after corrosion; the method can take into account surface roughness during corrosion modeling, and reflect the evolution of corrosion morphology during the corrosion process. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 A flow chart of a post-corrosion modeling method for metal surfaces with arbitrary initial morphology;
[0032] Figure 2 This is a schematic diagram of corrosion of a standard small steel sheet;
[0033] Figure 3 It is a schematic diagram of the average corrosion depth development;
[0034] Figure 4 It is a schematic diagram of the corrosion morphology development;
[0035] Figure 5 is a schematic diagram of the initial outline;
[0036] Figure 6 is the path length l i Schematic diagram;
[0037] Figure 7 is the random corrosion amount d i Schematic diagram;
[0038] Figure 8 is the normal n of each point on the surface contour i Schematic diagram;
[0039] Fig. 9 P i and P' i Schematic diagram;
[0040] Fig.10 This is a schematic diagram of the cross-sectional profile after corrosion. DETAILED DESCRIPTION
[0041] The present invention will be further described below in conjunction with the accompanying drawings.
[0042] The present invention discloses a method for modeling a metal surface with any initial morphology after corrosion. The specific process is as follows: Figure 1 The first step is to calculate the average corrosion depth d after exposure time t in a corrosive environment based on a standard steel sample, i.e. a small steel sample with a flat surface. u And surface roughness parameter S a ,S q ,S z , determine the development of corrosion characteristics over time, including d u -t,S a -d u ,S q -d u ,S z -d u ; The second step is to determine the corrosion characteristics of the metal surface based on the exposure time t in the corrosive environment, including the average corrosion depth d u And surface roughness parameter S a ,S q ,S z ; The third step is to determine the initial surface profile and the surface profile length l based on the geometric measurement results, and determine the points P on the surface profile i Length of the path from the endpoint l i Its coordinates (x i ,y i ) correspondence; the fourth step, based on the roughness parameter S a ,S q ,S z , through the Monte Carlo method, the length l of the path from the end point on the cross-sectional profile length l is generated i Each point P i Random corrosion amount d i ; Step 5: Calculate each point P on the initial surface contour iThe corresponding normal direction n i , establish each point P i Geometric information matrix G i =(x i ,y i ,l i ,n i ); Step 6: align each point P along the surface contour path i Along its normal direction n i Movement corresponding to corrosion amount d i , determine P i After moving P' i Point coordinates (x' i ,y' i ), point P' i That is the post-corrosion point P i Corresponding position.
[0043] Corrosion test of small steel sheet with flat surface Figure 2 shown.
[0044] The average corrosion depth of structural steel develops over time. Figure 3 shown.
[0045] Corrosion characteristics d according to different corrosion exposure time t u ,S a ,S q ,S z , establish S a ,S q ,S z The average corrosion depth d u The corresponding relationship, such as Figure 4 As shown;
[0046] According to the established d u -t relationship, determine the average corrosion depth d after corrosion u ; According to the S established in step (a) a -d u ,S q -d u ,S z -d u Relationship, determine the surface roughness parameter S after corrosion a ,S q ,S z ;
[0047] Perform geometric measurements on the initial surface profile and establish the initial profile, such as Figure 5 For surfaces with complex morphology, the coordinate information of each point on its surface contour can be obtained by laser scanning or other methods; for regular geometric surfaces, only the endpoint coordinates can be input, and interpolation between the endpoints can be performed to obtain N data points P iThe initial coordinate information of
[0048] The initial section is simplified into multiple polylines by inputting the initial contour through the endpoint coordinates. The number of data points N in each polyline segment can be determined by the polyline length l. The number of data points N will affect the modeling accuracy of the surface contour after corrosion Δ=l / N. For modeling of the rough surface after corrosion, in order to ensure the authenticity of the morphology, it is recommended that Δ is not greater than 0.02mm;
[0049] Each point P on the surface contour i Length of the path from the endpoint l i is the distance from the end point of the section along the initial surface contour to point P i The perimeter of the surface contour within the range, such as Figure 6 As shown;
[0050] The Monte Carlo method is used to generate a one-dimensional rough surface, and a one-dimensional rough surface sample with a length of l and N data points is generated. The generated rough surface corrosion feature d u ,S a ,S q ,S z Consistent with the parameters determined in claim 5, the longitudinal coordinates of each point on the rough surface are i Random corrosion amount d i ,i=1~N, such as Figure 7 As shown;
[0051] Determine the points P on the surface profile l i Normal n i ,like Figure 8 As shown, each point P i The geometric information is stored in the geometric information matrix G i =(x i ,y i ,l i ,n i ), i=1~N;
[0052] Consider that corrosion develops in the direction perpendicular to the metal surface toward the inside of the metal matrix, that is, along the surface contour path, the i Along its normal direction n i Movement corresponding to corrosion amount d i , determine P i After moving P' i Point coordinates (x' i ,y' i ), point P' i That is the post-corrosion point P i Corresponding position, such as Fig. 9 As shown;
[0053] Determine the cross-sectional profile after corrosion, such as Fig.10 As shown;
[0054] The method can take into account any metal surface with initial morphology during the corrosion development process, and realize geometric modeling of the surface with complex initial morphology after corrosion;
[0055] The method can take into account the surface roughness in the corrosion modeling process and reflect the evolution of the corrosion morphology during the corrosion process.
Claims
1. A method for modeling a metal surface after corrosion with arbitrary initial morphology, characterized in that: The post-corrosion surface established by the method can accurately reflect the roughness characteristics of the metal surface in the actual corrosion environment and can be applied to any initial morphology surface; the method comprises: (a) Based on the average corrosion depth d of a standard steel sample, i.e. a small steel sample with a flat surface, after exposure to a corrosive environment for a time t u And surface roughness parameter S a ,S q ,S z , determine the development of corrosion characteristics over time, including d u -t,S a -d u ,S q -d u ,S z -d u ; wherein the S a ,S q ,S z They are the arithmetic mean height, root mean square height and maximum depth respectively; (b) Determine the surface corrosion characteristics, including the average corrosion depth d, based on the exposure time t of the metal surface in the corrosive environment u And surface roughness parameter S a ,S q ,S z ; (c) Based on the geometric measurement results, determine the initial surface profile and the surface profile length l, and determine the points P on the surface profile i Length of the path from the endpoint l i With point P i Coordinate (x i ,y i ) corresponding relationship; (d) Based on the surface roughness parameter S a ,S q ,S z , through the Monte Carlo method, the path length l from the end point on the surface contour length l is generated i Each point P i Random corrosion amount d i ; (e) Calculate the initial surface contour at each point P i The corresponding normal direction n i , establish each point P i Geometric information matrix G i =(x i ,y i ,l i ,n i ); (f) For each point P along the surface contour path i Along its normal direction n i The movement corresponds to the random corrosion amount d i , determine P i Move point P' i Coordinate (x' i ,y' i ), point P' i That is the post-corrosion point P i Corresponding position.
2. The method according to claim 1, characterized in that In step (a), the small steel sheet sample with a flat surface is used to calibrate the development law of corrosion characteristics, and its geometric dimensions and mass need to be measured before being exposed to the corrosive environment; Alternatively, when it is not possible to conduct a corrosion exposure test in step (a), the development law of corrosion characteristics can be determined through existing metal environmental corrosion data; Alternatively, the surface roughness parameter S in step (a) a ,S q ,S z Calculated based on the following formula: S z =|max(Z(x,y))-min(Z(x,y))|.
3. The method according to claim 1, characterized in that The exposure time t in step (b) is the exposure time of the established surface in the corrosive environment, according to the d established in step (a). u -t relationship, determine the average corrosion depth d after corrosion u According to the S established in step (a) a -d u ,S q -d u ,S z -d u Relationship, determine the surface roughness parameter S after corrosion a ,S q ,S z。 4. The method according to claim 1, characterized in that In step (c), the initial surface profile is geometrically measured. For surfaces with complex surface morphology, the coordinate information of each point on the surface profile can be obtained by laser scanning or other methods; Alternatively, in step (c), the initial surface profile is geometrically measured. For a regular geometric surface, only the endpoint coordinates can be input, and interpolation is performed between the endpoints to obtain N data points P i The initial coordinate information of Alternatively, in step (c), each point P on the surface profile i Length of the path from the endpoint l i is the distance from the end point of the section along the initial surface contour to point P i The perimeter of the surface contour within the range.
5. The method according to claim 1, characterized in that In the step (d), a one-dimensional rough surface is generated by the Monte Carlo method, and a one-dimensional rough surface sample with a length of l and N data points is generated. The generated rough surface corrosion feature d u ,S a ,S q ,S z Consistent with the corresponding parameters determined in claim 5, the longitudinal coordinates of each point on the rough surface are i Random corrosion amount d i , where i=1~N.
6. The method according to claim 5, characterized in that In the step (d), the corrosion amount d of each point on the surface profile l is determined i , the number of corrosion points on the contour l is N, where i = 1~N.
7. The method according to claim 1, characterized in that In the step (e), each point P on the surface profile l is determined i Normal n i , and each point P i The geometric information is stored in the geometric information matrix G i =(x i ,y i ,l i ,n i ), i=1~N.
8. The method according to claim 1, characterized in that In the step (f), it is considered that the corrosion develops in the direction perpendicular to the metal surface toward the inside of the metal matrix, that is, the surface contour path is perpendicular to the surface contour path of each point P. i Along its normal direction n i Movement corresponding to corrosion amount d i , determine P i Move point P' i Coordinate (x' i ,y' i ), point P' i That is the post-corrosion point P i Corresponding position.
9. The method according to any one of claims 1 to 8, characterized in that: The method can take into account any metal surface with initial morphology during the corrosion development process, and realize geometric modeling of a surface with complex initial morphology after corrosion.
10. The method according to any one of claims 1 to 8, characterized in that: The method can take into account the surface roughness in the corrosion modeling process and reflect the evolution of the corrosion morphology during the corrosion process.
Citation Information
Patent Citations
Finite element numerical simulation and parameter analysis method for fatigue after corrosion of metal material
CN113177272A
Method for establishing metal surface corrosion prediction model based on corrosion probability
CN113791023A
Rust steel simulation method based on surface random roughness
CN114757074A
Method for evaluating corrosion depth of structural steel based on three-dimensional shape scanning
CN117664918A
Metal structure corrosion fatigue coupling life simulation method based on cellular automaton and continuum mechanics
CN118351990A