Method for realizing rapid enrichment and detection of nano plastic based on aggregate micro-droplet SERS (Surface Enhanced Raman Scattering) platform

Through the condensed micro droplet SERS platform combining silver sol and condenser, the problems of insufficient sensitivity and high detection cost in the detection of nanoplastics in the prior art are solved, and fast and effective nanoplastic detection is achieved, with low detection limit and simple operation. .

CN118937304AActive Publication Date: 2024-11-12NORTHEAST FORESTRY UNIV
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411039489.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-12
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

In the prior art, the method of detecting nanoplastics by combining SERS technology with condensers with enriched properties has not been reported, and the sensitivity of detection in water is not sufficient, so a complex SERS composite substrate is required, which is difficult to prepare and high cost. , affects detection efficiency.

Method used

The combined silver sol and condenser are used to prepare a condensed micro droplet SERS platform through vortex shock, achieving rapid enrichment detection of nanoplastics, which is simple and efficient in operation.

Benefits of technology

The rapid enrichment detection of nanoplastics is achieved, with a low detection limit. The linear range of polystyrene nanoplastics is 5×10-8g/L~0.5g/L, with short processing time, simple and efficient operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118937304A_ABST
    Figure CN118937304A_ABST
Patent Text Reader

Abstract

The invention discloses a method for realizing rapid enrichment detection of nano-plastics based on a condensate micro-droplet SERS (Surface Enhanced Raman Scattering) platform, and relates to a method for rapidly enriching and detecting nano-plastics. The invention aims to solve the problem that a method for detecting substances by combining an SERS (Surface Enhanced Raman Scattering) technology and a condensation body with enrichment performance does not exist at present. The preparation method specifically comprises the following steps: 1, synthesizing silver sol; step 2, preparing a condensation body; step 3, preparing a condensation body SERS platform; adding the silver sol obtained in the step 1 into the aggregate solution obtained in the step 3, and carrying out vortex oscillation to obtain an aggregate micro-droplet SERS substrate detaining silver nanoparticles; step 4, detecting the nano plastic; and adding a polystyrene microsphere solution into the condensed liquid drop SERS platform obtained in the step 3, carrying out vortex oscillation for 10 seconds, and then carrying out SERS measurement. The invention belongs to the technical field of hydrophobic pollutant detection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for rapid enrichment and detection of nano plastics, belonging to the technical field of hydrophobic pollutant detection. Background Art

[0002] In recent years, plastic pollution has become one of the most pressing environmental issues, seriously affecting human health. Nano-scale plastic particles have structural stability, large specific surface area, provide abundant adsorption sites for pollutants in the environment, and high hydrophobicity makes them an effective carrier for transporting various persistent organic pollutants. Effective technology for detecting nanoplastics is a necessary prerequisite for protecting human health and ecological safety. Among the existing methods for detecting nanoplastics, mass spectrometry is a destructive detection method that will damage the sample. Infrared method is sensitive to water molecules and is not suitable for water environment detection. Raman spectroscopy is fast and simple to operate and will not cause damage to the object being measured, but the direct use of ordinary Raman spectroscopy in water is not sensitive enough. It is necessary to introduce surface enhanced Raman spectroscopy (SERS) method to prepare a variety of SERS composite substrates to detect nanoplastics. However, the preparation of composite substrates is difficult and expensive, which increases the time cost of detection. The preparation method of metal sol SERS substrate is simple and inexpensive. Agglomerates are a liquid-liquid phase separation phenomenon, which has the performance of enriching substances from the surrounding environment, increasing the local concentration of substances, and improving the detection limit. The formation of aggregates achieves simultaneous enrichment of the SERS substrate and the detected object, but research on detecting substances using this method has not been reported yet. Summary of the invention

[0003] The present invention aims to solve the problem that there is no method for detecting substances by combining SERS technology with agglomerates with enrichment performance, and further proposes a method for realizing rapid enrichment and detection of nanoplastics based on agglomerate micro-droplet SERS platform.

[0004] The technical solution adopted by the present invention to solve the above problems is: the steps of the present invention include:

[0005] Step 1, synthesizing silver sol;

[0006] Step 2, preparing agglomerates;

[0007] Step 3, preparing a condensate SERS platform; adding the silver sol obtained in step 1 to the condensate solution obtained in step 3, and vortexing to obtain a condensate micro-droplet SERS substrate with silver nanoparticles captured;

[0008] Step 4, detecting nanoplastics; adding the polystyrene microsphere solution to the condensate droplet SERS platform obtained in step 3, vortexing for 10 seconds, and then performing SERS measurement.

[0009] Furthermore, step 1 specifically includes:

[0010] Step 101, heating the silver nitrate solution to a slight boil under stirring;

[0011] Step 102, adding a 1% by mass aqueous solution of trisodium citrate, keeping the mixture in a boiling state, and continuing stirring for 1 hour until the color changes from gray-green to gray-white;

[0012] Step 103, cooling the solution to room temperature while stirring to obtain silver sol.

[0013] Furthermore, step 2 specifically includes:

[0014] Step 201, preparing a polydiallyl dimethyl ammonium chloride solution: dissolving the polydiallyl dimethyl ammonium chloride in a phosphate buffer solution to prepare a 1-10 mg / mL polydiallyl dimethyl ammonium chloride solution;

[0015] Step 202, preparing a polyacrylic acid solution: dissolving polyacrylic acid in a phosphate buffer solution to prepare a 1-10 mg / mL polyacrylic acid solution;

[0016] Step 203: Add the solution prepared in step 201 to the solution prepared in step 202, and oscillate using a vortex oscillator for 20 to 30 seconds to obtain an agglomerate.

[0017] Furthermore, the amounts of the substances in step 1 are in the following proportions: 0.036 g of silver nitrate is dissolved in 200 mL of deionized water; 4 mL of a 1% sodium citrate aqueous solution.

[0018] Furthermore, the pH of the phosphate buffer solution in step 2 is 8.0.

[0019] Furthermore, in step 2, the concentration of the aqueous solution of polydiallyl dimethyl ammonium chloride is 1 to 10 mg / mL, and the concentration of the aqueous solution of polyacrylic acid is 1 to 10 mg / mL.

[0020] Furthermore, in step 203, the volume ratio of the polydiallyl dimethyl ammonium chloride solution to the polyacrylic acid solution is 2:1.

[0021] Furthermore, the amounts of the substances in step 3 are in the following proportions: 10 μL of polydimethylammonium chloride solution, 5 μL of polyacrylic acid solution, and 8 μL of silver sol.

[0022] Furthermore, the amounts of the substances in step 4 are in the following proportions: 2 μL of polystyrene microsphere solutions of different concentrations and 23 μL of coacervate solution.

[0023] Furthermore, in step 4, the continuous SERS measurement was performed with a data collection time of 10 s, accumulated once, and a power of 10 mW.

[0024] The beneficial effects of the present invention are:

[0025] 1. The present invention constructs a SERS detection platform for aggregates with enrichment performance, which is simple to operate and highly efficient;

[0026] 2. The enrichment process of the SERS substrate and the substance to be detected can be completed within 1 minute, and the processing time is short;

[0027] 3. The linear range of the polystyrene nanoplastic of the present invention is 5×10 -8 g / L~0.5g / L (0.05ppb~500ppm), low detection limit. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 is an optical microscope image of the agglomerate obtained in Example;

[0029] Figure 2 is a dark field microscope image of the agglomerate obtained in Example;

[0030] Figure 3 is an optical microscope image of the condensate SERS platform obtained in Example;

[0031] Figure 4 is a dark field microscope image of the condensate SERS platform obtained in Example;

[0032] Figure 5 is a graph showing the variation of SERS intensity of nanoplastics in the embodiment with concentration;

[0033] Figure 6 is a linear relationship diagram between the SERS intensity and the concentration ratio of the nanoplastics in the embodiment;

[0034] Figure 7 is a schematic diagram of the SERS spectrum of polystyrene microspheres;

[0035] Figure 8 It is a schematic diagram of the linear relationship between the intensity ratio and the logarithm of the concentration. Example

[0036] Embodiment 1:

[0037] 1. Synthesis of Silver Sol

[0038] Take 0.036g AgNO3 and dissolve it in 200ml deionized water, stir and heat it in an oil bath until it is slightly boiling (slightly bubbling without stirring, and slightly lower the temperature of the oil bath to prevent violent boiling after bubbling), then quickly add 4mL of 1% sodium citrate aqueous solution by mass, stir at 100°C until the solution turns gray-green, continue to stir and heat at 85°C for 1 hour until the color turns gray-white, and cool the solution to room temperature while stirring to obtain a silver sol;

[0039] 2. Preparation of Agglomerates

[0040] Preparation of polydiallyl dimethyl ammonium chloride solution: dissolve 10 mg of polydiallyl dimethyl ammonium chloride in 1 mL of phosphate buffer solution to prepare a 10 mg / mL polydiallyl dimethyl ammonium chloride solution;

[0041] Wherein, the concentration of phosphate buffer solution is 0.05 mol / L, and the pH is 8.0;

[0042] Preparation of polyacrylic acid solution: dissolve 10 mg of polyacrylic acid in 1 mL of phosphate buffer solution to prepare a 10 mg / mL polyacrylic acid solution;

[0043] Wherein, the concentration of phosphate buffer solution is 0.05 mol / L, and the pH is 8.0;

[0044] 10 μL of the polydiallyl dimethyl ammonium chloride solution was added to 5 μL of the polyacrylic acid solution, and the mixture was shaken for 30 seconds using a vortex shaker to obtain a coacervate solution;

[0045] like Figure 1 As shown, it can be seen that the condensate is a spherical droplet with regular shape;

[0046] like Figure 2 As shown, it can be seen that the interior of the condensate is hollow;

[0047] 3. Construction of the Condensate SERS Platform

[0048] During the preparation of the aggregates in step 2, 8 μL of the silver sol solution synthesized in step 1 was added, and the solution was shaken for 30 seconds using a vortex shaker to obtain an aggregate micro-droplet SERS detection platform enriched with silver nanoparticles;

[0049] like Figure 3 As shown, it can be seen that silver nanoparticles have been successfully enriched inside the agglomerate, the color of the agglomerate becomes darker, and the contrast increases;

[0050] like Figure 4 As shown, it can be seen that bright spots originating from silver nanoparticles appear inside the agglomerate, indicating the successful enrichment of silver nanoparticles.

[0051] 4. Detection of Nanoplastics at Different Concentrations

[0052] The polystyrene microsphere stock solution with an initial concentration of 0.5 g / L and a particle size of 20 nm was diluted step by step with water to obtain polystyrene microsphere solutions of different concentrations (0.5 g / L to 5×10 -8 g / L);

[0053] 2 μL of polystyrene microsphere solutions of different concentrations were added to 23 μL of the newly prepared condensate SERS platform solution and vortexed for 10 s to obtain condensate microdroplets enriched with polystyrene microspheres, and then continuous SERS measurements were performed immediately.

[0054] The data acquisition time was 10 s, accumulated once, and the power was 10 mW. The instrument used was a confocal micro-Raman spectrometer (RTS2-301-DL) purchased from Beijing Zhuoli Hanguang Instrument Co., Ltd.;

[0055] like Figure 5 As shown, it can be seen that granular substances appear inside the agglomerates, indicating that the polystyrene microspheres are successfully enriched inside the agglomerates;

[0056] like Figure 6 As shown in the figure, it can be seen that the SERS signal of the polystyrene microspheres inside the agglomerates is higher than that outside the agglomerates, indicating that the polystyrene microspheres are effectively enriched inside the agglomerates;

[0057] like Figure 7 As shown, the concentration range is 0.5g / L~5×10 -8 SERS spectra of polystyrene microspheres with a concentration of 500 ppm to 0.05 ppb, where 1004 cm -1 The ratio of peak intensities varies with concentration;

[0058] like Figure 8 As shown, 1004cm -1 There is a linear relationship between the intensity ratio and the logarithmic value of the concentration, and the regression coefficient is (R 2 =0.975).

[0059] The above is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with this profession can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent replacement and improvement made to the above embodiments without departing from the content of the technical solution of the present invention, based on the technical essence of the present invention, within the spirit and principles of the present invention, still fall within the protection scope of the technical solution of the present invention.

Claims

1. A method for rapid enrichment and detection of nanoplastics based on the condensate microdroplet SERS platform. It is characterized in that Specifically include: Step 1, synthesizing silver sol; Step 2, preparing agglomerates; Step 3, preparing a condensate SERS platform; adding the silver sol obtained in step 1 to the condensate solution obtained in step 3, and vortexing to obtain a condensate micro-droplet SERS substrate with silver nanoparticles captured; Step 4, detecting nanoplastics; adding the polystyrene microsphere solution to the condensate droplet SERS platform obtained in step 3, vortexing for 10 seconds, and then performing SERS measurement.

2. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that Step 1 specifically includes: Step 101, heating the silver nitrate solution to a slight boil under stirring; Step 102, adding a 1% by mass aqueous solution of trisodium citrate, keeping the mixture in a boiling state, and continuing stirring for 1 hour until the color changes from gray-green to gray-white; Step 103, cooling the solution to room temperature while stirring to obtain silver sol.

3. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that Step 2 specifically includes: Step 201, preparing a polydiallyl dimethyl ammonium chloride solution: dissolving the polydiallyl dimethyl ammonium chloride in a phosphate buffer solution to prepare a 1-10 mg / mL polydiallyl dimethyl ammonium chloride solution; Step 202, preparing a polyacrylic acid solution: dissolving polyacrylic acid in a phosphate buffer solution to prepare a 1-10 mg / mL polyacrylic acid solution; Step 203: Add the solution prepared in step 201 to the solution prepared in step 202, and oscillate using a vortex oscillator for 20 to 30 seconds to obtain an agglomerate.

4. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that The amounts of the substances in step 1 are in the following proportions: 0.036 g of silver nitrate is dissolved in 200 mL of deionized water; 4 mL of a 1% sodium citrate aqueous solution.

5. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that The pH of the phosphate buffer solution in step 2 is 8.

0.

6. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that In step 2, the concentration of the aqueous solution of polydiallyl dimethyl ammonium chloride is 1 to 10 mg / mL, and the concentration of the aqueous solution of polyacrylic acid is 1 to 10 mg / mL.

7. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 3, It is characterized in that In step 203 , the volume ratio of the polydiallyl dimethyl ammonium chloride solution to the polyacrylic acid solution is 2:

1.

8. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that The amounts of the substances in step 3 are in the following proportions: 10 μL of polydimethylammonium chloride solution, 5 μL of polyacrylic acid solution, and 8 μL of silver sol.

9. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that The amounts of the substances in step 4 are in the following proportions: 2 μL of polystyrene microsphere solutions of different concentrations and 23 μL of coacervate solution.

10. The method for rapid enrichment and detection of nanoplastics based on the condensate micro-droplet SERS platform according to claim 1, It is characterized in that In step 4, the continuous SERS measurement was performed with a data collection time of 10 s, accumulated once, and a power of 10 mW.

Citation Information

Patent Citations

  • Method for preparing mesoporous silica by taking anionic surfactant as template

    CN103449453A

  • Method for preparation of SERS active substrate based on layer-by-layer self-assembly and detection of crystal violet

    CN108387568A

  • Preparation method and application of hydrogel flexible SERS (Surface Enhanced Raman Scattering) substrate

    CN115791750A

  • Polymer gel material for collecting water in atmosphere and preparation method of polymer gel material

    CN118027508A