3D printing high-strength circular steel tube short column local geometric defect measurement and evaluation method
By making rubber replicas and performing three-dimensional scanning, combining curve and surface fitting methods, the local geometric defects of 3D printed high-strength steel round tube short columns were evaluated, and the problem of inability to scan the inner surface was solved, achieving high-precision geometric defect evaluation and Process optimization provides a foundation for component design.
Patent Information
- Application Number
- CN202411241062.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-12
AI Technical Summary
The 3D printed high-strength steel round tube short column has irregular geometric morphology due to process reasons during the additive manufacturing process, especially the inner surface cannot be effectively scanned, which makes it difficult to evaluate local geometric defects and affects the failure mode under axial pressure.
A method for measuring and evaluating local geometric defects of short columns of 3D printed high-strength round steel pipes is proposed. By making rubber replicas and cutting them, a three-dimensional scanner captures the geometric features of the outer surface and part of the inner surface, and verifying the scanning accuracy with Archimedes' principle , calculate point cloud data to determine local geometric defects, and evaluate deviations through curve and surface fitting methods, optimizing the process until specification limits are met.
The problem of scanning blind spots in the inner surface of the short column of the circular tube is solved, the accuracy and accuracy of measurement is ensured, the cross-section and surface geometric parameters are comprehensively evaluated, the design foundation is provided, and the application of other tube components is broadened.
Smart Images

Figure CN118937340A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel structure and additive manufacturing evaluation, and is a method for measuring and evaluating local geometric defects of 3D printed high-strength round steel pipe short columns. Background Art
[0002] With the development of the steel structure field, 3D printed high-strength steel will be favored by more and more designers due to its unique advantages. In the additive manufacturing process, WAAM has a higher deposition rate, lower equipment and raw material costs, and fewer restrictions on the workplace and forming size. It is suitable for the manufacture of large metal components in the construction engineering field, providing an effective way for intelligent construction.
[0003] Circular tube short columns generally refer to circular tube components with a slenderness ratio of no more than 8. In actual engineering, they are mainly subjected to axial compression, and their failure form is often local buckling. 3D printed circular tube short columns have irregular geometric morphology due to process reasons, so it is necessary to conduct geometric analysis on them.
[0004] The local geometric defects of short column components have a significant impact on their failure mode under axial compression. In the past, several longitudinal lines were taken for WAAM short columns, but this method easily ignored the maximum deviation of the longitudinal lines that were not taken. Therefore, it is necessary to propose a new evaluation method for local geometric defects of 3D printed circular tube short columns.
[0005] 3D laser scanning has high accuracy, but for round tube components with small size or large aspect ratio, there are scanning blind areas on the inner surface. Summary of the invention
[0006] In view of the shortcomings of the prior art, the present invention proposes a method for measuring and evaluating local geometric defects of 3D printed high-strength round steel tube short columns, and solves the problem that the inner surface of 3D printed high-strength steel round tube short columns cannot be scanned.
[0007] The present invention provides a method for measuring and evaluating local geometric defects of a 3D printed high-strength round steel tube short column. The present invention provides the following technical solutions:
[0008] A method for measuring and evaluating local geometric defects of 3D printed high-strength round steel tube short columns comprises the following steps:
[0009] Step 1: Replicate the 3D printed high-strength steel tube short column to obtain a refined coating sample;
[0010] Step 2: Perform geometric scanning and result verification on the refined coating sample;
[0011] Step 3: Perform three-dimensional analysis on the scanned short tube column and the refined coating sample to determine the point cloud data;
[0012] Step 4: Process the point cloud data obtained in step 3 to calculate local geometric defects;
[0013] Step 5: Evaluate local geometric defects and optimize the process until they are satisfied.
[0014] Preferably, the step 1 is specifically:
[0015] A mold of a 3D printed high-strength steel round tube short column with a ratio of 1:1 silicone material is made, and the mold is filled with resin molding material. After the resin is cured, the round tube short column replica is taken out and cut to obtain a resin replica of the 3D printed high-strength steel round tube short column. The replica is a refined coating sample of the 3D printed high-strength steel round tube short column.
[0016] Preferably, the step 2 is specifically:
[0017] The outer surface and part of the inner surface geometric features of the refined coating samples of the 3D printed high-strength steel round tube stubs were captured by a 3D scanner, and the geometric features of the refined coating samples of the cut 3D printed high-strength steel round tube stubs were captured. The mass of the round tube stub replica was measured using an electronic balance, and the volume of the round tube stub was measured using 3D model processing software. The accuracy of the 3D scanning method was verified using the Archimedes principle.
[0018] Preferably, the step 3 is specifically:
[0019] The two halves of the refined coated sample were spliced together, a reference plane was taken every 0.2 mm, the intersection line of the reference plane and the replica was calculated to obtain the contour line, the contour line was imported to generate point cloud data, and then the typical geometric parameters of each cross-section were calculated to obtain the geometric characteristics of the 3D printed high-strength steel round tube short column.
[0020] Preferably, the centroid deviation e of each section is calculated x 、e y , length b, width h, circumference C, and cross-sectional area A, and then determine the geometric unevenness of the specimen caused by printing technology.
[0021] Preferably, the step 4 is specifically:
[0022] Step 4.1: First calculate the local geometric defects at the cross-section level, use the curve fitting method to fit the circular curve equations of the inner and outer surfaces of each cross-section, calculate the radial deviation Δρ between each point cloud data and the fitting line, and use the adjacent average method for smoothing to eliminate the maximum deviation caused by the printing process that does not need to be considered. The local geometric defects at the cross-section level ω c It is the maximum absolute value of the internal and external surface deviations;
[0023] Step 4.2: Calculate the local geometric defects at the surface level, use the Origin surface fitting method to fit the cylindrical surface equation of the point cloud, and calculate the radial deviation Δρ between each point cloud data and the fitting surface.
[0024] The neighboring average method is used for smoothing to eliminate the maximum deviation caused by the printing process that does not need to be considered. The local geometric defects at the surface level ω p It is the maximum absolute value of the internal and external surface deviations;
[0025] Step 4.3: Take the above two defect values ω c ,ω p The maximum value of is taken as the local geometric defect of 3D printed high-strength steel round tube short column ω 0 .
[0026] Preferably, the step 5 is specifically:
[0027] The obtained initial local geometric defect amplitude is evaluated and compared with the limit value b / 100 in the European steel structure code. If the code limit is met, subsequent axial compression tests are carried out; if the limit is not met, the process needs to be adjusted and optimized until it is met.
[0028] A 3D printed high-strength steel round tube short column geometry measurement and local defect assessment system, the system comprising:
[0029] A refined coating sample preparation module, wherein the refined coating sample preparation module replicates a 3D printed high-strength steel round tube short column to obtain a refined coating sample;
[0030] A geometric scanning module, which performs geometric scanning on the refined coating sample and verifies the result;
[0031] An analysis module, wherein the analysis module performs a three-dimensional analysis on the scanned round tube short column refined coating sample to determine point cloud data of the refined coating sample;
[0032] A geometric defect calculation module, wherein the geometric defect calculation module processes the point cloud data obtained in step 3 to calculate local geometric defects;
[0033] An evaluation module evaluates the acquired local geometric defects and adjusts the optimization process until the defects are satisfied.
[0034] A computer-readable storage medium stores a computer program, which is executed by a processor to implement a method for measuring and evaluating local geometric defects of 3D-printed high-strength round steel pipe short columns.
[0035] A computer device comprises a memory and a processor, wherein the memory stores a computer program, and when the processor executes the computer program, a method for measuring and evaluating local geometric defects of a 3D printed high-strength round steel pipe short column is implemented.
[0036] The present invention has the following beneficial effects:
[0037] Compared with the prior art, the present invention has the following advantages:
[0038] The present invention proposes a method for measuring and evaluating local geometric defects of 3D printed high-strength round steel tube short columns. The first step of the present invention solves the problem of scanning blind spots on the inner surface of the round tube short column. By making a rubber replica and cutting the replica, the accuracy of the rubber replica is verified based on the scanned part, and the accuracy of the 3D scan is verified by using the mass density method, thereby ensuring the correctness of the method.
[0039] The third step of the present invention fully considers the geometric parameters of the cross section to characterize the variation properties of the circular tube cross section, and further explains the geometric unevenness of the 3D printed high-strength steel circular tube short column.
[0040] The fourth step of the present invention proposes a method for evaluating local geometric defects of such specimens, which is more comprehensive than the previous technology.
[0041] The present invention provides a basis for the design of such components by evaluating the geometric properties and local geometric defects of 3D printed high-strength steel round tube short columns. This method can be extended to other tubular components and can also be used for components manufactured by other processes. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0043] Figure 1 It is a specific flow chart of the local geometric defect evaluation method of 3D printed high-strength steel round tube short column of the present invention;
[0044] Figure 2 It is the resin replica production process;
[0045] Figure 3 is a schematic diagram of scanning using a 3D handheld scanner;
[0046] Figure 4 It is the point cloud data obtained by 3D scanning and the corresponding fitting surface;
[0047] Figure 5 is a schematic diagram of an embodiment of a method for evaluating local geometric defects of a 3D printed high-strength steel round tube short column (including nominal cross-sectional dimensions);
[0048] Figure 6 This is a schematic diagram of the processing of the contour line of a 3D printed high-strength steel round tube short column;
[0049] Figure 7 is a scatter plot of the deviations of the geometric parameters of the embodiment and the rubber replica;
[0050] Figure 8 is the result of geometric parameter analysis of the embodiment;
[0051] Fig. 9 is the local geometric defect before smoothing;
[0052] Fig.10 is the local geometric defect after smoothing;
[0053] Fig.11 is the local geometric defect before smoothing;
[0054] Fig.12 is the local geometric defect after smoothing. DETAILED DESCRIPTION
[0055] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0056] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0057] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0058] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0059] The present invention is described in detail below in conjunction with specific embodiments. Specific embodiment one:
[0061] according to Figure 1 – Fig.12 As shown, the specific optimization technical solution adopted by the present invention to solve the above technical problems is: the present invention relates to a method for measuring and evaluating local geometric defects of 3D printed high-strength round steel pipe short columns.
[0062] A method for measuring and evaluating local geometric defects of 3D printed high-strength round steel tube short columns comprises the following steps:
[0063] Step 1: Replicate the 3D printed high-strength steel tube short column to obtain a refined coating sample;
[0064] Step 2: Perform geometric scanning and result verification on the refined coating sample;
[0065] Step 3: Perform three-dimensional analysis on the scanned short tube column and the refined coating sample to determine the point cloud data of the refined coating sample;
[0066] Step 4: Process the point cloud data obtained in step 3 to calculate local geometric defects;
[0067] Step 5: Evaluate local geometric defects and optimize the process until they are satisfied. Specific embodiment 2:
[0069] The difference between the second embodiment of the present invention and the first embodiment is that:
[0070] The step 1 is specifically as follows:
[0071] A mold for 3D printed high-strength steel round tube short columns with a 1:1 silicone material is made, and the mold is filled with resin molding material. After the resin is cured, the round tube short column replica is taken out and cut to obtain a resin replica of the 3D printed high-strength steel round tube short column, that is, a refined coating sample of the 3D printed high-strength steel round tube short column is obtained.
[0072] The first step of the present invention solves the problem of a scanning blind area on the inner surface of a short cylindrical tube. A rubber replica is made and cut open, and the accuracy of the rubber replica is verified based on the scanned portion. The accuracy of the 3D scan is verified using a mass density method, thereby ensuring the correctness of the method. Specific embodiment three:
[0074] The difference between the third embodiment of the present invention and the second embodiment is that:
[0075] The step 2 is specifically as follows:
[0076] The outer surface and part of the inner surface geometric features of the refined coating samples of the 3D printed high-strength steel round tube stubs were captured by a 3D scanner, and the geometric features of the refined coating samples of the cut 3D printed high-strength steel round tube stubs were captured. The mass of the round tube stub replica was measured using an electronic balance, and the volume of the round tube stub was measured using 3D model processing software. The accuracy of the 3D scanning method was verified using the Archimedes principle. Specific embodiment four:
[0078] The difference between the fourth embodiment of the present invention and the third embodiment is that:
[0079] The step 3 is specifically as follows:
[0080] The two halves of the refined coated sample were spliced together, a reference plane was taken every 0.2 mm, the intersection line of the reference plane and the replica was calculated to obtain the contour line, the contour line was imported to generate point cloud data, and then the typical geometric parameters of each cross-section were calculated to obtain the geometric characteristics of the 3D printed high-strength steel round tube short column.
[0081] The third step of the present invention fully considers the geometric parameters of the cross section to characterize the variation properties of the circular tube cross section, and further explains the geometric unevenness of the 3D printed high-strength steel circular tube short column. Specific embodiment five:
[0083] The difference between the fifth embodiment of the present invention and the fourth embodiment is that:
[0084] The two halves of the refined coated sample were spliced together, a reference plane was taken every 0.2 mm, the intersection line of the reference plane and the replica was calculated to obtain the contour line, the contour line was imported to generate point cloud data, and then the typical geometric parameters of each cross-section were calculated to obtain the geometric characteristics of the 3D printed high-strength steel round tube short column. Specific embodiment six:
[0086] The difference between the sixth embodiment of the present invention and the fifth embodiment is that:
[0087] Calculate the centroid deviation e of each section x 、e y, length b, width h, circumference C, and cross-sectional area A, and then determine the geometric unevenness of the specimen caused by printing technology. Specific embodiment seven:
[0089] The difference between the seventh embodiment of the present invention and the sixth embodiment is that:
[0090] The step 4 is specifically as follows:
[0091] Step 4.1: First, calculate the local geometric defects at the cross-section level. Use the curve fitting method to fit the circular curve equations of the inner and outer surfaces of each cross-section, calculate the radial deviation Δρ between each point cloud data and the fitting line, and use the adjacent average method for smoothing to eliminate the maximum deviation caused by the printing process that does not need to be considered. The local geometric defects at the cross-section level ω c It is the maximum absolute value of the internal and external surface deviations;
[0092] Step 4.2: Calculate the local geometric defects at the surface level, use the Origin surface fitting method to fit the cylindrical surface equation of the point cloud, calculate the radial deviation Δρ between each point cloud data and the fitting surface, use the adjacent average method for smoothing to eliminate the maximum deviation caused by the printing process that does not need to be considered, and the local geometric defects at the surface level ω p It is the maximum absolute value of the internal and external surface deviations;
[0093] Step 4.3: Take the above two defect values ω c ,ω p The maximum value of is taken as the local geometric defect of 3D printed high-strength steel round tube short column ω 0 .
[0094] The fourth step of the present invention proposes a method for evaluating local geometric defects of such specimens, which is more comprehensive than the previous technology.
[0095] The present invention provides a basis for the design of such components by evaluating the geometric properties and local geometric defects of 3D printed high-strength steel round tube short columns. This method can be extended to other tubular components and can also be used for components manufactured by other processes. Specific embodiment eight:
[0097] The difference between the eighth embodiment of the present invention and the seventh embodiment is that:
[0098] The present invention provides a 3D printed high-strength steel round tube short column geometry measurement and local defect assessment system, the system comprising:
[0099] A refined coating sample preparation module, wherein the refined coating sample preparation module replicates a 3D printed high-strength steel round tube short column to obtain a refined coating sample;
[0100] A geometric scanning module, which performs geometric scanning on the refined coating sample and verifies the result;
[0101] An analysis module, wherein the analysis module performs a three-dimensional analysis on the scanned round tube short column refined coating sample to determine point cloud data of the refined coating sample;
[0102] A geometric defect calculation module, wherein the geometric defect calculation module processes the point cloud data obtained in step 3 to calculate local geometric defects;
[0103] An evaluation module evaluates the acquired local geometric defects and adjusts the optimization process until the defects are satisfied. Specific embodiment nine:
[0105] The difference between the ninth embodiment of the present invention and the eighth embodiment is that:
[0106] The present invention provides a computer-readable storage medium having a computer program stored thereon, the program being executed by a processor to implement a method for measuring and evaluating local geometric defects of a 3D-printed high-strength round steel pipe short column. Specific embodiment ten:
[0108] The difference between the tenth embodiment of the present invention and the ninth embodiment is that:
[0109] The present invention provides a computer device, comprising a memory and a processor, wherein the memory stores a computer program, and when the processor executes the computer program, a method for measuring and evaluating local geometric defects of a 3D printed high-strength round steel pipe short column is implemented. Specific embodiment eleven:
[0111] The difference between the eleventh embodiment of the present invention and the tenth embodiment is that:
[0112] As an example, Figure 5 A method for measuring and evaluating local geometric defects of a 3D printed high-strength round steel tube short column comprises the following steps:
[0113] Step 1: Make a mold for 3D printing high-strength steel round tube short column with a silicone material ratio of 1:1. Fill it with resin mold material, and after the resin is cured, take out the short tube replica and cut it to get the resin replica of the 3D printed high-strength steel round tube short column, such as Figure 2 shown.
[0114] Step 2: Geometric scanning and result verification: Use a 3D scanner to capture the geometric features of the outer surface and part of the inner surface of the 3D printed high-strength steel tube short column, and capture the geometric features of the cut tube short column replica. Use an electronic balance to measure the mass of the tube short column replica, use 3D model processing software to measure the volume of the tube short column, and use Archimedes' principle to verify the accuracy of the 3D scanning method.
[0115] In this embodiment, a HandySCAN 3D handheld scanner is used for three-dimensional scanning, and its accuracy can reach 0.025 mm. After obtaining the STL file, the volume of the specimen is directly analyzed in UG and the Archimedean principle is used to verify the accuracy of the scanning.
[0116] Step 3: Import the scanned replica of the short tube into the 3D analysis software, join the two halves of the replica, take a reference plane every 0.2 mm, calculate the intersection of the reference plane and the replica to get the contour line. Import the contour line into the simulation software to generate point cloud data such as Figure 4 Then the typical geometric parameters of each section are calculated to obtain the geometric characteristics of the 3D printed high-strength steel round tube short column.
[0117] In this embodiment, the contour line of the test piece along the length direction is obtained in the UG software, and then the point cloud data of the contour line is extracted in the simulation software for subsequent processing and calculation.
[0118] In this embodiment, the schematic diagram of processing contour lines in the simulation software is as follows: Figure 6 As shown, this embodiment calculates the centroid deviation e of each cross section. x 、e y , length b, width h, circumference C, cross-sectional area A, and then judge the geometric unevenness of the test piece caused by printing technology. The calculation method of this embodiment is: according to the coordinates of the point cloud in the simulation software, according to the calculation formula in Table 1.
[0119] Table 1 Calculation formula of geometric parameters
[0120]
[0121] Step 3 in this embodiment also includes verification of the accuracy of the rubber replica, and the specific method is: verify the deviation δ between the geometric parameters of the length b, width h, perimeter C, and cross-sectional area A of this embodiment except the scanning blind area and the geometric parameters of the rubber replica ABS The calculation results of this embodiment are as follows Figure 7 As shown, the calculated average error is 0.79%, which verifies the feasibility of using rubber replicas for geometric analysis of 3D printed high-strength steel circular tube short columns and solves the problem that the inner surface of the circular tube component cannot be scanned.
[0122] After verifying the accuracy of the replica in step 3 of this embodiment, the geometric parameters length b, width h, perimeter C, and cross-sectional area A are further calculated. The calculation results of this embodiment are as follows: Figure 8 As shown, it is shown that the surface geometric fluctuations of 3D printed high-strength steel circular tube short columns are large, which provides a basis for the design of such components.
[0123] Step 4: Process the point cloud data obtained in step 3 to calculate local geometric defects.
[0124] (1) First, calculate the local geometric defects at the cross-section level, and use the curve fitting method to fit the circular curve equations of the inner and outer surfaces of each cross-section respectively: Figure 4 As shown, calculate each point cloud data (x 0 ,y 0 ) and the fitting line (x 1 ,y 1 ) between the radial deviation Δρ 1 , the adjacent average method is used in the simulation software for smoothing to eliminate some maximum deviations caused by the printing process that do not need to be considered, and the local geometric defects at the cross-sectional level ω c It is the maximum absolute value of the above-mentioned internal and external surface deviations.
[0125]
[0126] ω c =Δρ 1,max
[0127] In this embodiment, local geometric defects at the cross-sectional level are calculated, such as Fig. 9 As shown in the figure, the radial deviation between the arc line of each cross section and the actual point cloud is calculated, and then these deviations are smoothed using the adjacent average method in the simulation software to eliminate some maximum deviations that do not need to be considered due to the printing process. In this way, the local geometric defects obtained are more accurate, such as Fig.10 shown.
[0128] (2) Then calculate the local geometric defects at the surface level and use the Origin surface fitting method to fit the cylindrical surface equation of the point cloud. Figure 4 , calculate each point cloud data (x 0 ,y 0 ) and the fitting surface (x 2 ,y 2 ) between the radial deviation Δρ 2 , the adjacent average method is used in the simulation software for smoothing to eliminate some maximum deviations caused by the printing process that do not need to be considered, and the local geometric defects at the cross-sectional level ω p It is the maximum absolute value of the above-mentioned internal and external surface deviations.
[0129]
[0130] ω p =Δρ 2,max
[0131] In this embodiment, local geometric defects at the surface level are calculated, such as Fig.11 As shown in the figure, the radial deviation between the fitted cylindrical surface of each section and the actual point cloud is calculated, and then these deviations are smoothed using the adjacent average method in the simulation software to eliminate some maximum deviations that do not need to be considered due to the printing process. In this way, the local geometric defects obtained are more accurate, such as Fig.12 shown.
[0132] (3) Take the above two defect values ω c ,ω p The maximum value of is taken as the local geometric defect of 3D printed high-strength steel round tube short column ω 0 , check whether the local geometric defects meet the limit value b / 100 in the European standard. If the limit value is met, the subsequent axial compression test is carried out. If the limit value is not met, the process needs to be adjusted and optimized until it is met.
[0133] In this embodiment, a 15×15 mm window is used for adjacent smoothing processing. Specific embodiment twelve:
[0135] The difference between the twelfth embodiment of the present invention and the eleventh embodiment is that:
[0136] The present invention comprises the following steps:
[0137] Step 1: Make a mold for 3D printing high-strength steel round tube short column with a silicone material ratio of 1:1. Fill it with resin mold material, and after the resin is cured, take out the short tube replica and cut it to get the resin replica of the 3D printed high-strength steel round tube short column, such as Figure 2 shown.
[0138] Step 2: Geometric scanning and result verification. The outer surface and part of the inner surface geometric features of the 3D printed high-strength steel round tube short column are captured by a 3D scanner. Figure 3 The geometric features of the cut short cylinder replica were captured. The mass of the short cylinder replica was measured using an electronic balance, the volume of the short cylinder was measured using 3D model processing software, and the accuracy of the 3D scanning method was verified using the Archimedean principle.
[0139] Step 3: Import the scanned replica of the short tube into the 3D analysis software, join the two halves of the replica, take a reference plane every 0.2 mm, calculate the intersection of the reference plane and the replica to get the contour line. Import the contour line into the simulation software to generate point cloud data such as Figure 4Then the typical geometric parameters of each section are calculated to obtain the geometric characteristics of the 3D printed high-strength steel round tube short column.
[0140] Step 4: Process the point cloud data obtained in step 3 to calculate local geometric defects.
[0141] (1) First, calculate the local geometric defects at the cross-section level, and use the curve fitting method to fit the circular curve equations of the inner and outer surfaces of each cross-section respectively: Figure 4 As shown, the radial deviation Δρ between each point cloud data and the fitting line is calculated, and the adjacent average method is used for smoothing in the simulation software to eliminate some maximum deviations that do not need to be considered due to the printing process, and the local geometric defects ω at the cross-sectional level c It is the maximum absolute value of the above-mentioned internal and external surface deviations.
[0142] (2) Then calculate the local geometric defects at the surface level and use the Origin surface fitting method to fit the cylindrical surface equation of the point cloud. Figure 4 , calculate the radial deviation Δρ between each point cloud data and the fitting surface, and use the adjacent average method for smoothing in the simulation software to eliminate some maximum deviations that do not need to be considered due to the printing process, and the local geometric defects at the surface level ω p It is the maximum absolute value of the above-mentioned internal and external surface deviations.
[0143] (3) Take the above two defect values ω c ,ω p The maximum value of is taken as the local geometric defect of 3D printed high-strength steel round tube short column ω 0 .
[0144] Step 5: Evaluate the initial local geometric defect amplitude obtained and compare it with the limit value b / 100 in the European Steel Structure Code. If it meets the limit value, conduct subsequent axial compression tests. If it does not meet the limit value, adjust the optimization process until it meets the limit value.
[0145] The point cloud data obtained in the third step is processed to calculate the local geometric defects.
[0146] Preferably, step one is to make a resin replica of the 3D printed high-strength steel round tube short column, thereby solving the problem that the inner surface of the round tube component cannot be scanned.
[0147] Preferably, step 2 is to verify (1) the accuracy of the 3D scanning technology and (2) the accuracy of the resin replica.
[0148] The mass of the 3D printed short cylindrical column replica was measured using an electronic balance, and the volume of the replica was calculated based on the mass m of the resin. This was compared with the volume obtained using the three-dimensional scanning method in the third step to verify the accuracy of the 3D scanning technology.
[0149] When scanning 3D printed short cylindrical tubes, some inner surfaces cannot be scanned by 3D scanning technology. To solve this problem, the resin replica is scanned instead. In order to verify the manufacturing accuracy of the resin replica and the feasibility of this method, the geometric data obtained by the third step of scanning are compared, and then the manufacturing accuracy of the resin replica is verified.
[0150] Preferably, in step three, an STL file of a replica of a short cylindrical tube is obtained, which is imported into a 3D modeling software for model assembly. After verifying the accuracy of the 3D scanning technology and the replica, contour lines are taken every 0.2 mm, and then these contour lines are imported into the simulation software for subsequent geometric analysis.
[0151] Calculate the centroid deviation e of each section in the simulation software x 、e y , length b, width h, circumference C, and cross-sectional area A, and then determine the geometric unevenness of the specimen caused by printing technology.
[0152] As a preferred method, step 4 proposes two types of local geometric defects: local geometric defects at the cross-section level and local geometric defects at the surface level, and proposes a local defect evaluation method.
[0153] In the description of this specification, the description of reference terms such as "one embodiment", "some embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or N embodiments or examples in a suitable manner. In addition, those skilled in the art can combine and combine the different embodiments or examples described in this specification and the features of different embodiments or examples without contradiction. In addition, the terms "first" and "second" are used only for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, the features defined as "first" and "second" can explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "N" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined. Any process or method description in the flowchart or otherwise described herein can be understood to represent a module, fragment or portion of code including one or more executable instructions for implementing the steps of a custom logic function or process, and the scope of the preferred embodiment of the present invention includes other implementations, in which the functions may not be performed in the order shown or discussed, including in a substantially simultaneous manner or in a reverse order according to the functions involved, which should be understood by a person skilled in the art of the art to which the embodiments of the present invention belong. The logic and / or steps represented in the flowchart or otherwise described herein, for example, can be considered as a sequenced list of executable instructions for implementing the logic function, can be specifically implemented in any computer-readable medium for use by an instruction execution system, device or device (such as a computer-based system, a system including a processor or other system that can fetch instructions from an instruction execution system, device or device and execute instructions), or in combination with these instruction execution systems, devices or devices. For the purpose of this specification, "computer-readable medium" can be any device that can contain, store, communicate, propagate or transmit programs for use by an instruction execution system, device or device or in combination with these instruction execution systems, devices or devices. More specific examples (a non-exhaustive list) of computer-readable media include the following: an electrical connection having one or N wirings (electronic device), a portable computer disk case (magnetic device), a random access memory (RAM), a read-only memory (ROM), an erasable and programmable read-only memory (EPROM or flash memory), a fiber optic device, and a portable compact disk read-only memory (CDROM).In addition, the computer readable medium can even be paper or other suitable medium on which the program can be printed, because the program can be obtained electronically, for example, by optically scanning the paper or other medium, then editing, interpreting or processing in other suitable ways as necessary, and then storing it in a computer memory. It should be understood that the various parts of the present invention can be implemented with hardware, software, firmware, or a combination thereof. In the above-mentioned embodiment, N steps or methods can be implemented with software or firmware stored in a memory and executed by a suitable instruction execution system. For example, if implemented with hardware, as in another embodiment, any one of the following technologies known in the art or their combination can be used to implement: a discrete logic circuit with a logic gate circuit for implementing a logic function for a data signal, a dedicated integrated circuit with a suitable combination of logic gate circuits, a programmable gate array (PGA), a field programmable gate array (FPGA), etc.
[0154] The above is only a preferred implementation of a method for measuring and evaluating local geometric defects of a 3D printed high-strength round steel tube short column. The protection scope of a method for measuring and evaluating local geometric defects of a 3D printed high-strength round steel tube short column is not limited to the above embodiment. All technical solutions under this idea belong to the protection scope of the present invention. It should be pointed out that for those skilled in the art, several improvements and changes without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A method for measuring and evaluating local geometric defects of 3D-printed high-strength round steel tube short columns, characterized by: The following steps are involved: Step 1: Replicate the 3D printed high-strength steel tube short column to obtain a refined coating sample; Step 2: Perform geometric scanning and result verification on the refined coated sample and 3D printed high-strength steel circular tube short column; Step 3: Perform three-dimensional analysis on the scanned short tube and refined coating sample to determine the point cloud data; Step 4: Process the point cloud data obtained in step 3 to calculate local geometric defects; Step 5: Evaluate local geometric defects and optimize the process until they are satisfied.
2. The method according to claim 1, wherein: The step 1 is specifically as follows: A mold for 3D-printed high-strength steel round tube short columns with a 1:1 silicone material is made and filled with resin molding material. After the resin solidifies, the short tube column replica is taken out and cut open to obtain a resin replica of the 3D-printed high-strength steel round tube short column. The replica is the refined coating sample of the 3D-printed high-strength steel round tube short column.
3. The method according to claim 2, wherein: The step 2 is specifically as follows: The geometric features of the outer surface and part of the inner surface of the refined coated sample of the 3D printed high-strength steel circular tube short column were captured by a 3D scanner, and the geometric features of the refined coated sample of the cut 3D printed high-strength steel circular tube short column were captured. The mass of the circular tube short column replica was measured using an electronic balance, and the volume of the circular tube short column was measured using 3D model processing software. The accuracy of the 3D scanning method was verified using the Archimedes principle.
4. The method according to claim 3, wherein: The step 3 is specifically as follows: The two halves of the refined coated sample were spliced together, and a reference plane was taken every 0.2 mm. The intersection line between the reference plane and the replica was calculated to obtain the contour line. The contour line was imported into the generated point cloud data, and then the typical geometric parameters of each cross-section were calculated to obtain the geometric characteristics of the 3D printed high-strength steel circular tube short column.
5. The method according to claim 4, wherein: Calculate the centroid deviation e of each section x 、e y , length b, width h, circumference C, and cross-sectional area A, and then judge the geometric unevenness of the specimen caused by printing technology.
6. The method according to claim 5, wherein: The step 4 is specifically as follows: Step 4.1: Calculate the local geometric defects at the cross-section level. Use the curve fitting method to fit the circular curve equations of the inner and outer surfaces of each cross-section, calculate the radial deviation Δρ between each point cloud data and the fitting line, and use the adjacent average method for smoothing to eliminate the maximum deviation caused by the printing process that does not need to be considered. The local geometric defects at the cross-section level ω c It is the maximum absolute value of the deviation between the inner and outer surfaces; Step 4.2: Calculate the local geometric defects at the surface level. Use the Origin surface fitting method to fit the cylindrical surface equation of the point cloud. Calculate the radial deviation Δρ between each point cloud data and the fitted surface. Use the adjacent average method for smoothing to eliminate the maximum deviation caused by the printing process that does not need to be considered. The local geometric defects at the surface level ω p It is the maximum absolute value of the deviation between the inner and outer surfaces; Step 4.3: Take the two defect values ω c 、ω p The maximum value of is taken as the local geometric defect ω0 of the 3D printed high-strength steel circular tube short column.
7. The method according to claim 6, wherein: The step 5 is specifically as follows: The obtained initial local geometric defect amplitude is evaluated and compared with the limit value b / 100 in the European Steel Structure Code. If the code limit is met, subsequent axial compression tests are carried out; When the limit is not met, the process needs to be adjusted and optimized until it is met.
8. A system for measuring and evaluating local geometric defects of 3D-printed high-strength round steel tube short columns, characterized by: The system comprises: A refined coating sample preparation module, which replicates a 3D-printed high-strength steel round tube short column to obtain a refined coating sample; A geometric scanning module, which performs geometric scanning on the refined coating sample and verifies the results; An analysis module, wherein the analysis module performs a three-dimensional analysis on the scanned circular tube short column refined coating sample to determine point cloud data of the refined coating sample; A geometric defect calculation module, which processes the point cloud data obtained in step 3 to calculate local geometric defects; An evaluation module evaluates the acquired local geometric defects and adjusts the optimization process until the defects are satisfied.
9. A computer-readable storage medium having a computer program stored thereon, characterized in that: The program is executed by a processor to implement the method according to claims 1-7.
10. A computer device comprising a memory and a processor, wherein the memory stores a computer program, wherein: The processor implements the method of claims 1-7 when executing the computer program.