Crack propagation life analysis method for motor rotor structure
By establishing a finite element model, calculating stress strength factors and making corrections, and combining with the Paris formula for integral calculation, the defects of assuming no initial cracks in the existing technology are solved, and the precise crack propagation life analysis of the motor rotor structure is achieved, providing More accurate lifespan assessment.
Patent Information
- Application Number
- CN202410964598.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-18
- Publication Date
- 2024-11-12
AI Technical Summary
The existing method for fatigue life analysis of motor rotor structures assumes that the structure has no initial crack defects, which leads to the calculation results that are too optimistic when the initial cracks exist and cannot accurately reflect the actual life of the structure.
A method that includes establishing a finite element model, calculating the stress strength factor at the crack tip, performing polynomial fitting, correcting the crack geometry and plastic zones, calculating critical crack sizes and integrating calculations through the Paris formula. Extended lifespan.
The life calculation of the motor rotor structure under the presence of initial cracks is realized, providing accurate and fast crack propagation life analysis, filling the gap that cannot be accurately calculated by high-period and low-period fatigue analysis methods.
Smart Images

Figure CN118940567A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a crack life analysis method for a motor rotor structure, which is suitable for motors and large motors and belongs to the technical field of motor structure analysis. Background Art
[0002] The motor rotor structure will be subjected to alternating loads caused by frequent starting and stopping during its service life. If the rotor structure suffers from fatigue fracture during its service life, it will bring immeasurable losses to safe production. Fatigue damage is a continuous process. The motor rotor components are inside the stator. It is very difficult to monitor fatigue damage online or regularly during its service life. In addition, the brittle fracture of the structure caused by fatigue crack propagation is often sudden. Therefore, it is necessary to conduct crack propagation life analysis on the motor rotor structure during the motor design stage to ensure the normal and stable operation of the motor during its service life.
[0003] In the past, the calculation of motor structure fatigue life mostly adopted high-cycle fatigue or low-cycle fatigue analysis methods. This type of fatigue analysis assumes that there are no initial crack defects in the structure, and calculates the fatigue life of the intact structure from crack initiation to final failure. If there are initial crack defects in the structure, the life calculated by high-cycle or low-cycle fatigue analysis methods cannot reflect the actual situation of the structure, and often leads to overly optimistic conclusions. Summary of the invention
[0004] Aiming at the problem that the fatigue life calculation of motor structure in the past often leads to overly optimistic conclusions, a crack propagation life analysis method for motor rotor structure is proposed. The method is simple to operate and can realize crack propagation life analysis with standardized calculation methods and processes.
[0005] The technical solution of the present invention is:
[0006] A crack growth life analysis method for a motor rotor structure comprises the following steps:
[0007] Step 1: Establish a finite element model of the motor rotor structure with crack characteristics. The crack tip uses a stress singular unit, and the crack direction is perpendicular to the first principal stress direction at the cracking position.
[0008] Step 2: Based on the finite element model of step 1, the stress intensity factor at the crack tip under various crack depths is calculated as a physical quantity for evaluating the stress field intensity at the crack tip, and a polynomial expression of the stress intensity factor with the crack depth as the independent variable is obtained through polynomial fitting;
[0009] Step 3: Use the crack geometry correction function and the plastic zone correction function to correct the stress intensity factor expression in step 2;
[0010] Step 4: Calculate the critical crack size when the rotor structure fails. The critical crack size can be calculated based on the fracture toughness or yield strength of the material, and the smaller value is removed;
[0011] Step 5: Calculate the crack growth life of the rotor structure by taking the definite integral of the Paris crack growth rate formula, where the lower limit of the definite integral is the initial crack size and the upper limit is the critical crack size;
[0012] The specific steps are as follows:
[0013] Step 1: Establish a finite element numerical simulation model based on the actual structure of the motor. To ensure the accuracy of the calculation, a 2D 8-node isoparametric unit or a 3D 20-node isoparametric unit is used for modeling. First, the stress distribution of the rotor structure without cracks is calculated by finite element method to determine the stress concentration position of the rotor structure and the first principal stress s at the stress concentration position. 1 Then, the crack feature is established at the maximum principal stress position of the structure. The crack feature starts from the surface of the structure and goes deep into the structure. The crack surface is closely related to the first principal stress s at this position. 1 Vertical; In order to accurately represent the stress singularity at the crack tip, a circle of units around the crack tip uses stress singular units, and the midpoint of the unit around the crack tip is located at 1 / 4 of the unit edge and biased to one side of the crack tip; a circle of stress singular units around the crack tip, the unit radial size ≤ a / 8, a is the crack depth, and the unit circumferential angle is between 30° and 40°;
[0014] Step 2: Determine the crack tip stress intensity factor K for the specific structure of the motor rotor I (a) Functional expression: First, the internal displacement, stress and strain field distribution of the structure under the action of external loads are calculated by finite element method, and then the finite element results are post-processed by displacement extrapolation method or J integral method to determine the stress intensity factor at the crack tip; the stress intensity factor of the structure under different crack sizes is calculated multiple times, and the stress intensity factor K is converted into I Fitted into a deterministic function expression K with crack size a as the independent variable I (a);
[0015] Displacement Extrapolation Method:
[0016] According to the linear elastic theory, near the structural crack tip, the displacement perpendicular to the crack surface has the following analytical expression:
[0017]
[0018] In formula (1), v is displacement; G is the shear modulus of the material; μ is the Poisson's ratio of the material; K IIis the stress intensity factor of the sliding crack; r and θ are the polar radial and circumferential coordinate components with the crack tip as the origin, respectively; the above formula is a plane strain solution, and μ is replaced by The plane stress solution of displacement can be obtained; according to the above formula (1), on the crack surface, θ = ±180°, then the displacement perpendicular to the crack surface can be expressed as:
[0019]
[0020] According to the structural displacement field obtained by finite element analysis, the stress intensity factor K at the tearing crack tip can be calculated: I for:
[0021]
[0022] In formula (3), |Δv| is the relative displacement of the node on the crack surface at a distance r from the crack tip in the direction perpendicular to the crack surface. To improve the calculation accuracy, a node at a distance r from the crack tip can be selected on the crack surface. 1 and r 2 The relative displacements of the two positions are |Δv 1 | and |Δv 2 |; then the coefficients A and B can be obtained from these two points, so that There are the following expressions:
[0023]
[0024] According to the above formula (4), the crack tip can be extrapolated to:
[0025]
[0026] Finally, the stress intensity factor K at the crack tip can be calculated: I for:
[0027]
[0028] J-integral method:
[0029] In fracture mechanics, the J integral is used as an average measure of the strain field near the crack tip. When the volume force inside the integral path is zero and the force on the crack surface is zero, the J integral can be expressed as:
[0030]
[0031] Where, Γ is an integral path around the crack tip in the counterclockwise direction; W is the strain energy density; is the stress vector pointing outward along the normal direction on the integration path; is the displacement vector on the integral path; x and y are the coordinate components along the crack propagation direction and perpendicular to the crack propagation direction in the rectangular coordinate system with the crack tip as the origin; s is the arc length of the integral path; the J integral has the invariance of the integral path, and the result of the J integral calculation is the same for any path around the crack tip in a counterclockwise direction; because the finite element analysis obtains an approximate solution to the structural physical field, the J integral calculated based on the finite element results will have certain differences under different paths, but this difference is small when the finite element mesh density is sufficient; for the linear elastic plane strain model, the J integral and the stress intensity factor at the crack tip have the following relationship:
[0032]
[0033] Where E is the elastic modulus of the material; for the plane stress model, the above equation (8) can be divided by 1-μ 2 The relationship between J integral and stress intensity factor is obtained; most engineering structures are dominated by opening cracks, that is, K II =0, then the stress intensity factor K I It can be directly calculated by J integral:
[0034]
[0035] Step 3: Stress intensity factor function expression K I (a) Modification; Considering the influence of crack geometry and crack tip plastic zone on stress intensity factor, the stress intensity factor expression K in step 2 is modified I (a) Perform crack geometry correction and plastic zone correction; the calculation formula of the crack geometry correction coefficient is:
[0036]
[0037] Where R is the ratio of the short axis a to the long axis b of the crack ellipse; the plastic zone correction factor is calculated using the following formula:
[0038]
[0039] In the formula, σ Y is the yield strength of the material; σ is the far-end stress of the crack, which is calculated by the following equivalent formula:
[0040]
[0041] Substituting the distal stress σ expressed in the above formula into the plastic zone correction formula, the calculation formula of the plastic zone correction coefficient with the crack depth a as the independent variable is obtained:
[0042]
[0043] The corrected stress intensity factor expression is:
[0044] K′ I (a) = F 2 ·F 3 (a) K I (a) (14)
[0045] Step 4: Determine the critical crack size a of the structure cr ; Critical crack size a cr It can be determined according to the two modes of structural brittle fracture failure or local yield failure, and the smaller value of the two modes is taken; according to the failure mode of brittle fracture, when the structure fails due to brittle fracture:
[0046] K′ I (a cr1 )=K IC (15)
[0047] According to the local yield failure mode, when the structure fails due to yield:
[0048] σ(a cr2 )=σ Y (16)
[0049] The above two equations can be used to calculate the critical crack size a under the two failure modes: cr1 and a cr2 ; Take the smaller value of the two as the final critical crack size, that is,
[0050] a cr =min(a cr1 , a cr2 ) (17)
[0051] Step 5: Calculate the crack growth life of the motor rotor structure; by taking the definite integral of the Paris formula representing the crack growth rate in fracture mechanics, we can calculate the structure from the initial crack a i Extend to critical crack a cr Crack growth life:
[0052]
[0053] Where N is the structural crack growth life, a i is the initial crack size, C[ΔK I (a)] m It is the length of crack extension in one load cycle, that is, the crack growth rate. C and m are parameters determined by the material and are measured through experiments.
[0054] Preferably, in step 2, the calculation of the stress intensity factor at the crack tip can also use commercial finite element software to automatically calculate the stress intensity factor at the crack tip; finite element software with this function can directly derive the value of the stress intensity factor at the crack tip.
[0055] Preferably, the polynomial fitting in step 2 and the critical crack size a in step 4 are cr1 The solution can be achieved with the help of Python, Mat lab or MathCAD tools.
[0056] The beneficial effects of the present invention are:
[0057] The method provided by the present invention overcomes the shortcomings of other technologies and can achieve accurate and rapid analysis of the crack propagation life of the motor rotor structure.
[0058] The present invention has the advantages that the crack propagation life calculation of various motor rotor components can be completed, the implementation is simple, the calculation is accurate, and the analysis efficiency can be greatly improved by standardizing the calculation method and process.
[0059] The present invention proposes a method for establishing a functional expression of the stress intensity factor at the crack tip of the motor rotor structure, and then conservatively determines the critical crack size when the structure fails through multiple failure modes, and finally calculates the crack growth life of the rotor structure by integrating the crack growth rate formula. The advantage of the present invention is that it realizes the life calculation of the motor rotor structure under the condition of the presence of initial cracks, filling the gap that the previous high-cycle and low-cycle fatigue analysis methods cannot accurately calculate the crack growth life when the structure has initial cracks. BRIEF DESCRIPTION OF THE DRAWINGS
[0060] Figure 1 It is a schematic diagram of an open crack and a partial enlargement under the action of bidirectional stress of the present invention;
[0061] Figure 2 The cantilever beam structure with a single-side crack and a partially enlarged schematic diagram of the present invention;
[0062] Figure 3 It is a schematic diagram of the first principal stress distribution field of a cantilever beam with a single-side crack of the present invention;
[0063] Figure 4 It is a schematic diagram of the polynomial fitting of the stress intensity factor of the present invention;
[0064] Figure 5 A schematic diagram of crack geometry correction of the stress intensity factor of the present invention;
[0065] Figure 6 It is a schematic diagram of the plastic zone correction of the stress intensity factor of the present invention;
[0066] Figure 7 It is a schematic diagram of the bending stress of the residual effective cross section of the cantilever beam of the present invention. DETAILED DESCRIPTION
[0067] The present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments. This embodiment is implemented based on the technical solution of the present invention, and provides a detailed implementation method and specific operation process, but the protection scope of the present invention is not limited to the following embodiments.
[0068] Step 1: Establish a finite element numerical simulation model based on the actual structure of the motor rotor. To ensure the accuracy of the calculation, the model is built using a second-order isoparametric unit with a mid-node. First, calculate the stress distribution of the rotor structure when there is no crack, determine the stress concentration position of the structure and the first principal stress s at the stress concentration position. 1 Considering conservative evaluation, the crack characteristics are established at the stress concentration position of the structure. The crack characteristics start from the surface of the structure and go deep into the structure. The crack surface is consistent with the first principal stress s at this position. 1 Vertical. In order to accurately represent the stress singularity at the crack tip, a circle of units around the crack tip uses a stress singular unit, which is characterized by the midpoint of the unit around the crack tip being located at 1 / 4 of the unit edge and biased to one side of the crack tip. The radial dimension of the stress singular unit around the crack tip is ≤ a / 8, a is the crack depth, and the circumferential angle of the unit is between 30° and 40°.
[0069] Step 2: Determine the stress intensity factor K at the crack tip in the rotor structure I Function expression. After the finite element calculation is completed, the stress intensity factor at the crack tip can be determined by post-processing the displacement field or stress field near the crack tip. The displacement extrapolation method and the J integral method are easy to implement in engineering, and you can choose one of them.
[0070] Displacement Extrapolation Method:
[0071] According to the linear elastic theory, near the structural crack tip, the displacement perpendicular to the crack surface has the following analytical expression:
[0072]
[0073] In formula (1), v is displacement; G is the shear modulus of the material; μ is the Poisson's ratio of the material; K II is the stress intensity factor of the sliding crack; r and θ are the polar radial and circumferential coordinate components with the crack tip as the origin. The above formula is a plane strain solution. Replace μ in the formula with The plane stress solution of displacement can be obtained. According to the above formula (1), on the crack surface, θ = ±180°, then the displacement perpendicular to the crack surface can be expressed as:
[0074]
[0075] According to the structural displacement field obtained by finite element analysis, the stress intensity factor K at the tearing crack tip can be calculated. I for:
[0076]
[0077] In formula (3), |Δv| is the relative displacement of the node at a distance r from the crack tip on the crack surface in the direction perpendicular to the crack surface. To improve the calculation accuracy, a node at a distance r from the crack tip can be selected on the crack surface. 1 and r 2 The relative displacements of the two positions are |Δv 1 | and |Δv 2 |. From these two points, we can get the coefficients A and B, so that There are the following expressions:
[0078]
[0079] According to the above formula (4), the crack tip can be extrapolated to:
[0080]
[0081] Finally, the stress intensity factor K at the crack tip can be calculated: I for:
[0082]
[0083] J-integral method:
[0084] In fracture mechanics, the J integral is used as an average measure of the strain field near the crack tip. When the volume force inside the integral path is zero and the force on the crack surface is zero, the J integral can be expressed as:
[0085]
[0086] Where, Γ is an integral path around the crack tip in the counterclockwise direction; W is the strain energy density; is the stress vector pointing outward along the normal direction on the integration path; is the displacement vector on the integration path; x and y are the coordinate components along the crack propagation direction and perpendicular to the crack propagation direction in the rectangular coordinate system with the crack tip as the origin; s is the arc length of the integration path. The J integral has the invariance of the integration path, and the result of the J integral calculation is the same for any path around the crack tip in a counterclockwise direction. Because the finite element analysis obtains an approximate solution to the structural physical field, the J integral calculated based on the finite element results will have certain differences under different paths, but this difference is small when the finite element mesh density is sufficient. For the linear elastic plane strain model, the J integral and the stress intensity factor at the crack tip have the following relationship:
[0087]
[0088] Where E is the elastic modulus of the material. For the plane stress model, the above equation (8) can be divided by 1-μ 2 The relationship between J integral and stress intensity factor is obtained. Most engineering structures are dominated by opening cracks, i.e., K II =0, then the stress intensity factor K I It can be directly calculated by J integral:
[0089]
[0090] Some commercial finite element software can automatically calculate the stress intensity factor at the crack tip based on the finite element results using the above two methods. If the finite element analysis uses finite element software with this function, the stress intensity factor value at the crack tip can also be directly derived.
[0091] When calculating the crack growth life, what is needed is the function K of the stress intensity factor with the crack depth a as the independent variable. I (a). To determine K I (a) The specific form of the function requires repeating the above calculation process, establishing crack features of different depths at the same position and direction of the rotor structure, and calculating the corresponding stress intensity factor values, and finally obtaining a set of stress intensity factor values corresponding to different crack depths. By fitting this set of data with a polynomial, the functional expression of the stress intensity factor K can be obtained: I (a). Polynomial fitting can be implemented with the help of tools such as Python, Matlab or MathCAD.
[0092] Step 3: Stress intensity factor function K I (a) The correction includes the crack geometry correction and the plastic zone correction, both of which need to be corrected.
[0093] Crack geometry correction: The stress intensity factor calculated based on the plane model assumes that the crack runs through the entire structure. In actual motor rotor structures, cracks that run through the entire structure rarely appear. The shape of the crack is mostly close to an ellipse, with the short axis in the crack propagation direction and the long axis perpendicular to the crack propagation direction. Crack geometry correction factor F 2 The following formula (10) is used for calculation:
[0094]
[0095] Among them, R is the ratio of the minor axis to the major axis of the crack ellipse. For most cracks in the motor rotor structure, R is between 0.2 and 0.5.
[0096] Plastic zone correction: The stress intensity factor calculation in step 2 is based on the results of linear elastic finite element analysis, but metal materials will inevitably form a plastic zone near the crack tip due to stress concentration. In order to consider the influence of the plastic zone, it is necessary to perform a plastic zone correction on the stress intensity factor. Plastic zone correction factor F 3 The following formula (11) is used for calculation:
[0097]
[0098] In the formula, σ Y is the yield strength of the material; σ is the far-end stress of the crack, which is equivalently calculated by the following formula (12):
[0099]
[0100] Substituting equation (12) into equation (11), the expression of the plastic zone correction factor is obtained as a function of the crack depth a: 3 (a):
[0101]
[0102] Finally, the functional expression of the modified stress intensity factor is:
[0103] K′ I (a) = F 2 ·F 3 (a) K I (a) (14)
[0104] Step 4: Calculate the critical crack size a at which the rotor structure fails cr . Critical crack size a cr It indicates the crack depth when the rotor structure fails. The failure mode is different and the critical crack size a cr The calculation method of the critical crack size a is also different. The critical crack size a can be calculated according to the following failure mode cr .
[0105] Structural brittle fracture failure: Fracture toughness K is used in fracture mechanics IC Indicates the material's ability to resist brittle fracture, fracture toughness K IC is a material property measured experimentally. I <K IC When the stress intensity factor K I =K IC When the structure is brittle fractured, the crack depth at this time is the critical crack size a in the brittle failure mode. cr1 Therefore, the following equation (15) can be used:
[0106] K′ I (a cr1 )=K IC (15)
[0107] Calculate the critical crack size a cr1 The expansion form of formula (15) is relatively complex and can be solved with the help of tools such as Python, Matlab or MathCAD.
[0108] Local yield failure of the structure: As the crack expands, the remaining effective area of the structure gradually decreases. When the average stress on the remaining effective area reaches the yield strength σ Y When the structure fails due to insufficient bearing capacity, the crack depth is the critical crack size a under fatigue failure mode. cr2 The average stress σ(a cr2 ), it is necessary to calculate according to the specific force mode such as tension, torsion or bending. When yield failure occurs, there are:
[0109] σ(a cr2 )=σ Y (16)
[0110] According to the above formula (16), the critical crack size under the local yield failure mode can be determined by setting the maximum stress of the structure equal to the yield strength. The critical crack size a can be calculated as cr2 .
[0111] The critical crack sizes calculated by the two failure modes are different. The smaller value of the two is taken as the final critical crack size, that is:
[0112] a cr =min(a cr1 , a cr2 ) (17)
[0113] Step 5: Calculate the crack growth life of the motor rotor structure. The Paris formula for crack growth rate in fracture mechanics is as follows:
[0114]
[0115] In the above formula, N is the number of cycles (i.e., the structural crack growth life); It represents the length of crack extension in one load cycle, i.e. the crack extension rate; C and m are parameters determined by the material and are measured through experiments. The definite integral of formula (18) is made with respect to the crack size a, and the lower limit of the integral is the initial crack size a i , which can be the actual existing crack size in the structure or the minimum crack size that can be detected by nondestructive testing equipment; the upper limit of the integral is the critical crack size a determined in step 4 cr The calculated structural crack growth life N is:
[0116]
[0117] In this embodiment, Figure 2 As shown, a cantilever beam with a height of h = 20 mm and a length of l = 100 mm is shown. The left end of the cantilever beam is fixed, and the right end is subjected to a concentrated force of 500 N. The structure is made of steel, and there is a single-side crack in the middle of the cantilever beam. It is used as the analysis object of this embodiment.
[0118] like Figure 3 As shown in the figure, the displacement, stress, and strain physical field distribution of the cantilever beam under the concentrated force is first obtained by finite element analysis, and then the stress intensity factor at the crack tip is calculated using the displacement extrapolation method or the J integral method. The stress intensity factor values of different crack depths are repeatedly calculated, and the functional expression of the stress intensity factor K is obtained by polynomial fitting. I (a) If Figure 4 As shown. For the stress intensity factor function K I (a) Perform crack geometry correction and plastic zone correction to obtain the corrected stress intensity factor function K′ I (a). Determine the critical crack size of the cantilever beam and finally calculate the crack growth life of the structure by taking the definite integral of the Paris crack growth rate formula.
[0119] The specific operations are:
[0120] Step 1: Create Figure 2The finite element model shown uses a planar 8-node isoparametric unit to ensure the accuracy of the calculation. In order to accurately represent the stress singularity at the crack tip, a circle of units around the crack tip uses a stress singular unit, which is characterized in that the mid-node of the unit around the crack tip is located at 1 / 4 of the unit edge and biased to one side of the crack tip. The radial dimension of the circle of stress singular units surrounding the crack tip is 1 / 8 of the crack depth, and the circumferential angle of the unit is 30°. A concentrated force of 500N is applied to the free end face of the cantilever beam, and a fixed constraint is applied to the fixed end. The stress field of the cantilever beam is obtained by finite element calculation, as shown in Figure 3 shown.
[0121] Step 2: Determine the stress intensity factor K at the crack tip in the beam I Function expression. The results obtained by finite element calculation can be post-processed, and the displacement extrapolation method or J integral method can be used to determine the stress intensity factor of different crack sizes. Repeat step 1 and the above steps to establish crack sizes of different depths for calculation, establish a cantilever beam model with different crack depths, and calculate the corresponding stress intensity factor. Figure 4 As shown, the function of the stress intensity factor with crack depth a as the independent variable is finally obtained through polynomial fitting:
[0122] K I (a) = 3.78a 3 -51.86a 2 +428.9a+314.57
[0123] Step 3: Stress intensity factor function K I (a) is modified. Step 2 uses the plane strain model to calculate the stress intensity factor, assuming that the crack runs through the entire structure. In actual engineering structures, through cracks rarely occur. The shape of the crack is mostly close to an ellipse, with the short axis in the crack propagation direction and the long axis perpendicular to the crack propagation direction, such as Figure 5 The ratio of the minor axis to the major axis of a common elliptical crack in engineering is between 0.2 and 0.5. Usually, R = 0.1 is used as a conservative design. The crack geometry correction coefficient is calculated by formula (10):
[0124]
[0125] In addition, step 2 uses linear elastic analysis to calculate the stress intensity factor, but metal materials will inevitably produce a plastic zone at the crack tip due to stress concentration, such as Figure 6 As shown. In order to consider the influence of the plastic zone, the stress intensity factor needs to be corrected for the plastic zone. The plastic zone correction factor is calculated using the following formula (11):
[0126]
[0127] In the formula, σ Y is the yield strength of the material, which is 730MPa; σ is the distal stress of the crack. According to the general expression of the stress intensity factor at the crack tip subjected to the distal stress:
[0128]
[0129] It can be calculated equivalently:
[0130]
[0131] Therefore, the distal stress is also a function of the crack depth a. Substituting it into the plastic zone correction coefficient formula, we can get
[0132]
[0133] Finally, the corrected stress intensity factor expression is obtained:
[0134] K′ I (a) = F 2 ·F 3 (a) K I (a)
[0135] Step 4: Determine the critical crack size a of the structure cr . Critical crack size a cr It can be determined based on the two modes of structural brittle fracture failure or local yield failure, and the smaller value of the two modes is taken.
[0136] First, the critical crack size a is calculated according to the failure mode of brittle fracture. cr1 The fracture toughness of the cantilever beam material is measured by the test When the stress intensity factor of the cantilever beam reaches the fracture toughness, the structure fails due to brittle fracture, that is, when the structure fails due to brittle fracture:
[0137] K′ I (a cr1 )=K IC
[0138] Solving this nonlinear equation can determine the critical crack size of the embodiment structure as a cr1 =12.15mm.
[0139] Then, the critical crack size a is calculated based on the local yield failure mode cr2 .like Figure 7 As shown, when the crack size is a cr2 When the effective remaining section height of the cantilever beam is ha cr2 When the maximum bending stress of the cantilever beam reaches the yield strength, the structure fails due to yielding, that is, when the structure produces local yielding, there is:
[0140]
[0141] It can be calculated that the critical crack size of the cantilever beam when it fails is a cr2 =5.67mm. This embodiment adopts the bending yield failure of the cantilever beam structure, and determines the critical crack size according to the bending stress formula. For other structures subjected to tension, torsion or combined loads, the corresponding mechanical formula can be used to calculate the structural stress, and the critical crack size under the local yield failure mode can be determined by setting the maximum stress of the structure equal to the yield strength.
[0142] The critical crack size of the cantilever beam structure of the final embodiment is:
[0143] a cr =min(a cr1 , a cr2 )=min(12.15,5.67)=5.67mm
[0144] Step 5: Calculate the crack growth life of the structure. The Paris formula for crack growth rate is:
[0145]
[0146] The parameter that determines the crack growth rate of the cantilever beam material in the above formula can be measured according to the standard test method for measuring fatigue crack growth rate in ASTM E647-1995, which is C = 1.3 × 10 -10 MPa -2.25 mm -0.125 and m = 2.25. Assume that the initial crack size of the cantilever beam is a i =1.27mm, then the crack growth life of the structure can be calculated by taking the definite integral of the Paris formula as:
[0147]
[0148] The calculation results show that the cantilever beam in the embodiment grows from an initial crack of 1.27 mm to a critical crack of 5.67 mm at failure, and its crack growth life is about 3549 load cycles.
[0149] The above-mentioned embodiment only expresses one implementation mode of the present invention, and its description is relatively specific and detailed, but it cannot be understood as limiting the scope of the invention patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.
Claims
1. A crack growth life analysis method for a motor rotor structure, characterized in that: The following steps are involved: Step 1: Establish a finite element model of the motor rotor structure with crack characteristics. The crack tip uses a stress singular unit, and the crack direction is perpendicular to the first principal stress direction at the cracking position. Step 2: Based on the finite element model of step 1, the stress intensity factor at the crack tip under various crack depths is calculated as a physical quantity for evaluating the stress field intensity at the crack tip, and a polynomial expression of the stress intensity factor with the crack depth as the independent variable is obtained through polynomial fitting; Step 3: Use the crack geometry correction function and the plastic zone correction function to correct the stress intensity factor expression in step 2; Step 4: Calculate the critical crack size when the rotor structure fails. The critical crack size can be calculated based on the fracture toughness or yield strength of the material, and the smaller value is removed; Step 5: Calculate the crack growth life of the rotor structure by taking the definite integral of the Paris crack growth rate formula, where the lower limit of the definite integral is the initial crack size and the upper limit is the critical crack size; The specific steps are as follows: Step 1: Establish a finite element numerical simulation model according to the actual structure of the motor. To ensure the accuracy of the calculation, a 2D 8-node isoparametric unit or a 3D 20-node isoparametric unit is used for modeling. First, the stress distribution of the rotor structure when there is no crack is calculated by finite element method to determine the stress concentration position of the rotor structure and the direction of the first principal stress s1 at the stress concentration position. Then, a crack feature is established at the maximum principal stress position of the structure. The crack feature starts from the surface of the structure and penetrates into the structure. The crack surface is perpendicular to the first principal stress s1 at this position. To accurately represent the stress singularity at the crack tip, a circle of units around the crack tip uses a stress singular unit. The midpoint of the unit around the crack tip is located at 1 / 4 of the unit edge and is biased to one side of the crack tip. The radial size of the stress singular unit around the crack tip is ≤a / 8, a is the crack depth, and the circumferential angle of the unit is between 30° and 40°. Step 2: Determine the crack tip stress intensity factor K for the specific structure of the motor rotor I (a) Functional expression: First, the internal displacement, stress and strain field distribution of the structure under the external load is calculated by finite element method, and then the stress intensity factor at the crack tip is determined by post-processing the finite element results through displacement extrapolation method or J-integral method; The stress intensity factor of the structure at different crack sizes is calculated multiple times, and the stress intensity factor K is converted into I Fitted into a deterministic function expression K with crack size a as the independent variable I (a); Displacement Extrapolation Method: According to the linear elastic theory, near the structural crack tip, the displacement perpendicular to the crack surface has the following analytical expression: In formula (1), v is displacement; G is the shear modulus of the material; μ is the Poisson's ratio of the material; K II is the stress intensity factor of the sliding crack; r and θ are the polar radial and circumferential coordinate components with the crack tip as the origin, respectively; the above formula is a plane strain solution, and μ is replaced by The plane stress solution of displacement can be obtained; according to the above formula (1), on the crack surface, θ = ±180°, then the displacement perpendicular to the crack surface can be expressed as: According to the structural displacement field obtained by finite element analysis, the stress intensity factor K at the tearing crack tip can be calculated: I for: In formula (3), |Δv| is the relative displacement of the node on the crack surface at a distance r from the crack tip in the direction perpendicular to the crack surface. To improve the calculation accuracy, two points at a distance r1 and r2 from the crack tip can be selected on the crack surface, and their relative displacements are set to |Δv1| and |Δv2| respectively. Then, the coefficients A and B can be obtained from these two points, so that There are the following expressions: According to the above formula (4), the crack tip can be extrapolated to: Finally, the stress intensity factor K at the crack tip can be calculated: I for: J-integral method: In fracture mechanics, the J integral is used as an average measure of the strain field near the crack tip. When the volume force inside the integral path is zero and the force on the crack surface is zero, the J integral can be expressed as: Where, Γ is an integral path around the crack tip in the counterclockwise direction; W is the strain energy density; is the stress vector pointing outward along the normal direction on the integration path; is the displacement vector on the integral path; x and y are the coordinate components along the crack propagation direction and perpendicular to the crack propagation direction in the rectangular coordinate system with the crack tip as the origin; s is the arc length of the integral path; the J integral has the invariance of the integral path, and the result of the J integral calculation is the same for any path around the crack tip in a counterclockwise direction; because the finite element analysis obtains an approximate solution to the structural physical field, the J integral calculated based on the finite element results will have certain differences under different paths, but this difference is small when the finite element mesh density is sufficient; for the linear elastic plane strain model, the J integral and the stress intensity factor at the crack tip have the following relationship: Where E is the elastic modulus of the material; for the plane stress model, the above equation (8) can be divided by 1-μ 2 The relationship between J integral and stress intensity factor is obtained; most engineering structures are dominated by opening cracks, that is, K II =0, then the stress intensity factor K I It can be directly calculated by J integral: Step 3: Stress intensity factor function expression K I (a) Modification; Considering the influence of crack geometry and crack tip plastic zone on stress intensity factor, the stress intensity factor expression K in step 2 is modified I (a) Perform crack geometry correction and plastic zone correction; the calculation formula of the crack geometry correction coefficient is: Where R is the ratio of the short axis a to the long axis b of the crack ellipse; the plastic zone correction factor is calculated using the following formula: In the formula, σ Y is the yield strength of the material; σ is the far-end stress of the crack, which is calculated by the following equivalent formula: Substituting the distal stress σ expressed in the above formula into the plastic zone correction formula, the calculation formula of the plastic zone correction coefficient with the crack depth a as the independent variable is obtained: The corrected stress intensity factor expression is: <h2 style=";text-align:left;direction:ltr">K′<h2 style=";text-align:left;direction:ltr"> I <h2 style=";text-align:left;direction:ltr"> (a)=F2·F3(a)·K<h2 style=";text-align:left;direction:ltr"> I <h2 style=";text-align:left;direction:ltr"> (a) (14) Step 4: Determine the critical crack size a of the structure cr ; Critical crack size a cr It can be determined according to the two modes of structural brittle fracture failure or local yield failure, and the smaller value of the two modes is taken; according to the failure mode of brittle fracture, when the structure fails due to brittle fracture: K′ I (a cr1 )=K IC (15) According to the local yield failure mode, when the structure fails due to yield: σ(a cr2 )=s Y (16) The above two equations can be used to calculate the critical crack size a under the two failure modes: cr1 and a cr2 ; Take the smaller value of the two as the final critical crack size, that is, in cr =min(a) cr1 ,in cr2 ) (17) Step 5: Calculate the crack growth life of the motor rotor structure; by taking the definite integral of the Paris formula representing the crack growth rate in fracture mechanics, we can calculate the structure from the initial crack a i Extend to critical crack a cr Crack growth life: Where N is the structural crack growth life, a i is the initial crack size, C[ΔK I (a)] m It is the length of crack extension in one load cycle, that is, the crack growth rate. C and m are parameters determined by the material and are measured through experiments.
2. The crack growth life analysis method for a motor rotor structure according to claim 1, characterized in that: In step 2, the stress intensity factor at the crack tip can also be calculated using commercial finite element software to automatically calculate the stress intensity factor at the crack tip; finite element software with this function can directly derive the value of the stress intensity factor at the crack tip.
3. The crack growth life analysis method for a motor rotor structure according to claim 1, characterized in that: Polynomial fitting in step 2, critical crack size a in step 4 cr1 The solution can be achieved with the help of Python, Matlab or MathCAD tools.
Citation Information
Cited By
Method, device and equipment for evaluating residual strength of compressor impeller
CN119337535A
Repair structure crack propagation tracking measurement correction method based on intelligent coating
CN122594679A
A method for measuring and correcting the propagation of structural cracks based on smart coatings
CN122594679B