Semiconductor device and method for forming the same
By adopting a buried gate structure in semiconductor devices and using the combination of trench and gate dielectric layers, the gate resistance increase problem caused by polysilicon double gate electrodes is solved, and the effect of improving GIDL characteristics and reducing resistance is achieved.
Patent Information
- Application Number
- CN202311759895.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-11
- Filing Date
- 2023-12-20
- Publication Date
- 2024-11-12
AI Technical Summary
When using polysilicon as a double gate electrode to improve gate drain leakage (GIDL) characteristics, the gate resistance increases due to the reduced line width of the word line, and a structure is needed to simultaneously improve the GIDL characteristics and reduce the gate resistance.
A buried gate structure is adopted, in which a trench is formed in the substrate, covering the gate dielectric layer and the fill gate electrode, the first and second gate electrodes are isolated by an oxidation-resistant layer, and a covering layer is formed in the trench to form an embedded type The buried gate structure is used to reduce resistance.
It effectively improves the GIDL characteristics, reduces the gate resistance, and improves the electrical characteristics and reliability of semiconductor devices.
Smart Images

Figure CN118943170A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to Korean Patent Application No. 10-2023-0060938, filed on May 11, 2023, which is incorporated herein by reference in its entirety. Technical Field
[0003] Embodiments of the present disclosure relate to a semiconductor device, and more particularly, to a semiconductor device including a buried gate. Background Art
[0004] With the rapid development of the electronic industry, the demand for highly integrated semiconductor devices has gradually increased. In particular, polysilicon has been used as a dual gate electrode to improve gate-induced drain leakage (GIDL) characteristics. Summary of the invention
[0005] Embodiments of the present disclosure are directed to semiconductor devices having improved electrical characteristics.
[0006] According to one embodiment of the present disclosure, a semiconductor device includes: a trench formed in a substrate; a gate dielectric layer adapted to cover a bottom surface and sidewalls of the trench; a first gate electrode adapted to gap-fill a bottom of the trench above the gate dielectric layer; a second gate electrode formed above the first gate electrode; and an anti-oxidation layer disposed at an interface between the first gate electrode and the second gate electrode.
[0007] According to one embodiment of the present invention, a method for manufacturing a semiconductor device includes: forming a trench in a substrate; covering the bottom surface and sidewalls of the trench with a gate dielectric layer; gap-filling the bottom of the trench with a first gate electrode above the gate dielectric layer; locally providing an anti-oxidation layer on the first gate electrode; forming a second gate electrode above the anti-oxidation layer and in the trench; forming a covering layer above the second gate electrode and in the trench to complete a buried gate structure; and forming a source-drain region in the substrate adjacent to the trench. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 is a plan view showing a semiconductor device according to an embodiment of the present disclosure.
[0009] Figure 2A is along Figure 1 A cross-sectional view taken along line AA' is shown.
[0010] Figure 2B is along Figure 1 A cross-sectional view taken along line BB' is shown.
[0011] FIG. 3A to FIG. 3Fis a cross-sectional view illustrating a method for manufacturing a semiconductor device according to another embodiment of the present disclosure.
[0012] Figures 4 to 6 is a cross-sectional view showing a semiconductor device according to other embodiments of the present disclosure. DETAILED DESCRIPTION
[0013] Embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. However, the present disclosure can be embodied in different forms and should not be construed as being limited to the embodiments described herein. On the contrary, these embodiments are provided so that the present disclosure will convey the scope of the present disclosure to those skilled in the art. Throughout the present disclosure, similar reference numerals refer to similar parts in the various figures and embodiments of the entire present disclosure.
[0014] The drawings are not necessarily to scale, and in some cases, the proportions may be exaggerated in order to clearly illustrate the features of the embodiments. When the dimensions of the elements described herein are referred to as "approximately", the dimensions given may vary by + / -5%. When a first layer is referred to as being "on" a second layer or "on" a substrate, it refers not only to the case where the first layer is formed directly on the second layer or substrate, but also to the case where a third layer exists between the first layer and the second layer or substrate.
[0015] Figure 1 is a plan view showing a semiconductor device 100 according to an embodiment of the present disclosure. Figure 2A is along Figure 1 A cross-sectional view taken along line AA'. Figure 2B is along Figure 1 A cross-sectional view taken along line BB'.
[0016] When polysilicon is used as a dual gate electrode to improve GIDL characteristics as described above, the gate resistance increases due to the reduction in the line width of the word line. Therefore, a structure capable of solving the increase in gate resistance while improving GIDL characteristics is required. In this regard, the present disclosure has emerged. Figure 1 , Figure 2A and Figure 2B , the semiconductor device 100 may include a substrate 101 and a buried gate structure 100G (such as a double gate structure) embedded in the substrate 101. The semiconductor device 100 may be part of a memory cell. For example, the semiconductor device 100 may be part of a dynamic random access memory (DRAM) memory cell.
[0017] The substrate 101 may be a material suitable for semiconductor processing. The substrate 101 may include a semiconductor substrate. The substrate 101 may be formed of a silicon-containing material. For example, the substrate 101 may include one or more of the following: silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 101 may also include other semiconductor materials such as germanium. The substrate 101 may include a III / V semiconductor substrate, for example, a compound semiconductor substrate such as GaAs. The substrate 101 may include a silicon-on-insulator (SOI) substrate.
[0018] An isolation layer 102 and an active region 103 may be formed in the substrate 101. The active region 103 may be defined by the isolation layer 102. The isolation layer 102 may be a shallow trench isolation (STI) region formed by a trench etching process. The isolation layer 102 may be formed by filling a shallow trench (e.g., isolation trench 102T) with a dielectric material. For example, the isolation layer 102 may include silicon oxide, silicon nitride, or a combination thereof.
[0019] like Figure 2A As shown, a trench 105 may be formed in the substrate 101. The trench 105 may be formed by using a hard mask layer 104 (see Figure 3A Description) is formed as an etching stop to etch the substrate 101. Figure 1 From the perspective of the plan view of , the trench 105 may have a line shape extending in one direction. The trench 105 may have a line shape crossing the active area 103 and the isolation layer 102. The trench 105 may have a depth shallower than the isolation trench 102T. According to another embodiment of the present disclosure, the bottom of the trench 105 may have a curvature. The trench 105 may be a space in which the buried gate structure 100G is formed, and this configuration may be referred to as a "gate trench".
[0020] The first doping region 111 and the second doping region 112 may be formed in the active region 103. The first doping region 111 and the second doping region 112 may be regions doped with conductive dopants. For example, the conductive dopant may include one or more of phosphorus (P), arsenic (As), antimony (Sb), or boron (B). The first doping region 111 and the second doping region 112 may be doped with dopants of the same conductivity type. The first doping region 111 and the second doping region 112 may be disposed in the active region 103 on both sides of the trench 105. The bottom surfaces of the first doping region 111 and the second doping region 112 may be disposed at a predetermined depth from the top surface of the active region 103. The bottom surfaces of the first doping region 111 and the second doping region 112 may be higher than the bottom surface of the trench 105. The first doping region 111 may be referred to as a "first source / drain region", and the second doping region 112 may be referred to as a "second source / drain region". A channel may be defined between the first doping region 111 and the second doping region 112 by the buried gate structure 100G. A channel may be defined along the contour of the trench 105 .
[0021] like Figure 2B As shown, the trench 105 may include a first trench T1 and a second trench T2. The first trench T1 may be formed in the active area 103. The second trench T2 may be formed in the isolation layer 102. The trench 105 may extend continuously from the first trench T1 to the second trench T2. In the trench 105, the bottom surface of the first trench T1 may be set at a level higher than the bottom surface of the second trench T2. When the isolation layer 102 is recessed, a height difference between the first trench T1 and the second trench T2 may be formed. Therefore, the second trench T2 may include a recessed region R, the bottom surface of the recessed region R being lower than the bottom surface of the first trench T1. Due to the step difference between the first trench T1 and the second trench T2, a fin 103F may be formed in the active area 103. Therefore, the active area 103 may include a fin 103F.
[0022] As described above, the fin 103F may be formed under the first trench T1, and the sidewall of the fin 103F may be exposed by the recessed isolation layer 102F. The fin 103F may be a portion in which a portion of a channel is formed. The fin 103F may be referred to as a saddle fin. The fin 103F may increase the channel width and improve electrical characteristics.
[0023] According to another embodiment of the present disclosure, the fin 103F may be omitted.
[0024] The buried gate structure 100G may include a gate dielectric layer 106 covering the bottom surface and sidewalls of the trench 105, and a gate electrode structure GE and a capping layer 110 sequentially stacked on the gate dielectric layer 106 to fill the trench 105. The gate electrode structure GE may include a stacked structure of a first gate electrode 107, an anti-oxidation layer 108, and a second gate electrode 109. The first gate electrode 107 may fill the lower portion of the trench 105 on the gate dielectric layer 106. The anti-oxidation layer 108 may be formed on the first gate electrode 107. The second gate electrode 109 may be formed on the anti-oxidation layer 108. The second gate electrode 109 may fill the middle portion of the trench 105. The capping layer 110 may fill the upper portion of the trench 105 on the second gate electrode 109. For convenience of description, the lower portion, the middle portion, and the upper portion of the trench 105 may be provided, and the thickness (or depth) of each portion may be the same as or different from each other.
[0025] For example, the gate dielectric layer 106 may include one or more of silicon oxide, silicon nitride, silicon oxynitride, high-k material, or a combination thereof. The high-k material may include a material having a dielectric constant higher than that of silicon oxide. For example, the high-k material may include a material having a dielectric constant greater than about 3.9. In another example, the high-k material may include a material having a dielectric constant greater than about 10. In another example, the high-k material may include a material having a dielectric constant of about 10 to 30. The high-k material may include at least one metal element. The high-k material may include a hafnium-containing material. For example, the hafnium-containing material may include one or more of hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, or a combination thereof. According to another embodiment of the present disclosure, for example, the high-k material may include one or more of lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, silicon zirconium oxide, silicon zirconium oxynitride, aluminum oxide, or a combination thereof. As the high-k material, other known high-k materials may be selectively used. The gate dielectric layer 106 may include a metal oxide.
[0026] An upper surface of the gate electrode structure GE may be disposed at a lower level than an upper surface of the active region 103. The first gate electrode 107 may have a shape filling a bottom portion of the trench 105.
[0027] The upper surface of the first gate electrode 107 may be disposed at a level lower than the bottom surfaces of the first doping region 111 and the second doping region 112. Therefore, the first gate electrode 107 may not overlap the first doping region 111 and the second doping region 112 in a direction parallel to the surface of the substrate 101. The first gate electrode 107 may be a metal-based material. The first gate electrode 107 may include a metal nitride. For example, the first gate electrode 107 may include titanium nitride (TiN).
[0028] According to another embodiment of the present disclosure, for example, the first gate electrode 107 may include one or more selected from the group consisting of titanium nitride (TiN), molybdenum (Mo), tantalum nitride (TaN), lanthanum (La), hafnium (Hf), tantalum (Ta), aluminum (Al), aluminum oxide (Al2O3), titanium silicon nitride (TiSiN) and tantalum silicon nitride (TaSiN) or a combination thereof, but the present disclosure is not limited thereto.
[0029] The second gate electrode 109 may partially or completely overlap the first doping region 111 and the second doping region 112 in a direction parallel to the surface of the substrate 101. The second gate electrode 109 may include the same metal nitride as the first gate electrode 107. For example, the second gate electrode 109 may include titanium nitride (TiN).
[0030] According to another embodiment of the present disclosure, for example, the second gate electrode 109 may include one or more selected from the group consisting of titanium nitride (TiN), molybdenum (Mo), tantalum nitride (TaN), lanthanum (La), hafnium (Hf), tantalum (Ta), aluminum (Al), aluminum oxide (Al2O3), titanium silicon nitride (TiSiN) and tantalum silicon nitride (TaSiN) or a combination thereof, but the present disclosure is not limited thereto.
[0031] The anti-oxidation layer 108 may be disposed between the first gate electrode 107 and the second gate electrode 109. The anti-oxidation layer 108 may be disposed at the interface between the first gate electrode 107 and the second gate electrode 109. The anti-oxidation layer 108 may not be disposed between the sidewall of the second gate electrode 109 and the gate dielectric layer 106. The anti-oxidation layer 108 may be strip-shaped. The anti-oxidation layer 108 may play a role in preventing the first gate electrode 107 and the second gate electrode 109 from being oxidized by collecting impurities (e.g., oxygen) contained in the first gate electrode 107 and the second gate electrode 109. Therefore, the degradation of the electrical characteristics of the buried gate structure 100G caused by the oxidation of the first gate electrode 107 and the second gate electrode 109 (e.g., excessive increase in work function, etc.) may be prevented. In addition, since the anti-oxidation layer 108 is disposed at the interface between the first gate electrode 107 and the second gate electrode 109, the diffusion of materials between the first gate electrode 107 and the second gate electrode 109 may be prevented, thereby ensuring the reliability of the device.
[0032] The anti-oxidation layer 108 may include a silicon-containing material. For example, the anti-oxidation layer 108 may be formed of polysilicon. The thickness of the anti-oxidation layer 108 may be less than the thickness of each of the first gate electrode 107 and the second gate electrode 109. The thickness of the anti-oxidation layer 108 may be adjusted to a thickness that can prevent material diffusion between the first gate electrode 107 and the second gate electrode 109 while allowing electrical conduction between the first gate electrode 107 and the second gate electrode 109. For example, the anti-oxidation layer 108 may have a thickness of approximately To about Thickness.
[0033] As a comparative example, when the thickness of the anti-oxidation layer 108 is formed too thin, less than about When the thickness of the anti-oxidation layer 108 exceeds about 100 mm, the oxygen collection capability may be reduced. Therefore, the anti-oxidation effect of the first gate electrode 107 and the second gate electrode 109 may be insufficient. In addition, when the thickness of the anti-oxidation layer 108 exceeds about 100 mm, the oxygen collection capability may be reduced. When the anti-oxidation layer 108 is formed in a cup shape covering the bottom surface and sidewalls of the second gate electrode 109 instead of a stripe shape, there is also a problem that the resistance of the semiconductor device increases due to the increase in the volume of the non-metallic material in the gate electrode.
[0034] The capping layer 110 may fill the upper portion of the trench 105 above the second gate electrode 109. The capping layer 110 may include a dielectric material. For example, the capping layer 110 may include one or more of silicon nitride, silicon oxide, silicon oxynitride, or a combination thereof.
[0035] Figures 4 to 6 is a cross-sectional view showing a semiconductor device according to another embodiment of the present disclosure. In addition to the first gate electrode structure, Figure 4 The semiconductor device can be Figure 2A The semiconductor device is the same as that of FIG. 1 . Except for the second gate electrode structure, Figure 5 The semiconductor device can be Figure 2A Except for the first gate electrode structure and the second gate electrode structure, Figure 6 The semiconductor device can be Figure 2A The same semiconductor devices. Figures 4 to 6 2, the same parts as the semiconductor device of FIG. Figure 2A The constituent elements are the same, so they can be simply described or omitted.
[0036] Reference Figure 4 , the semiconductor device 200 may include a substrate 101 and a buried gate structure 200G embedded in the substrate 101. The semiconductor device 200 may be a part of a memory cell. For example, the semiconductor device 200 may be a part of a DRAM memory cell.
[0037] The buried gate structure 200G may include a gate dielectric layer 106 covering the bottom surface and sidewalls of the trench 105, and a gate electrode structure GE2 and a capping layer 110 sequentially stacked on the gate dielectric layer 106 to fill the trench 105. The gate electrode structure GE2 may include a stacked structure of a first pad gate electrode 201, a first body gate electrode 202, an anti-oxidation layer 108, and a second gate electrode 109. As used herein, "body" with respect to a gate electrode refers to a gate electrode that occupies a large portion of the trench 205 compared to a pad gate electrode that is a relatively thin film present on the sidewalls of the trench.
[0038] The first pad gate electrode 201 may be a barrier layer that may prevent the material of the first body gate electrode 202 from out-diffusion. The first pad gate electrode 201 may include a metal nitride, and the first body gate electrode 202 may include a metal material. For example, the first pad gate electrode 201 may include titanium nitride, and the first body gate electrode 202 may include tungsten (W) or molybdenum (Mo).
[0039] According to another embodiment of the present disclosure, the first pad gate electrode 201 may include a material with a higher work function than the first body gate electrode 202. The first body gate electrode 202 may include a material with a lower resistance than the first pad gate electrode 201. The first pad gate electrode 201 may include a metal nitride or a metal oxide, and the first body gate electrode 202 may include a metal-based material. For example, the first pad gate electrode 201 may include titanium silicon nitride (TiSiN) or aluminum oxide (Al2O3), and the first body gate electrode 202 may include titanium nitride (TiN).
[0040] Reference Figure 5 , the semiconductor device 300 may include a substrate 101 and a buried gate structure 300G embedded in the substrate 101. The semiconductor device 300 may be a part of a memory cell. For example, the semiconductor device 300 may be a part of a DRAM memory cell.
[0041] The buried gate structure 300G may include a gate dielectric layer 106 covering the bottom surface and sidewalls of the trench 105, and a gate electrode structure GE3 and a capping layer 110 sequentially stacked on the gate dielectric layer 106 to fill the trench 105. The gate electrode structure GE3 may include a stacked structure of a first gate electrode 107, an anti-oxidation layer 108, a second pad gate electrode 301, and a second body gate electrode 302.
[0042] The second pad gate electrode 301 may be a barrier layer that may prevent the material of the second body gate electrode 302 from out-diffusion. The second pad gate electrode 301 may include a metal nitride, and the second body gate electrode 302 may include a metal material. For example, the second pad gate electrode 301 may include titanium nitride, and the second body gate electrode 302 may include tungsten (W) or molybdenum (Mo).
[0043] According to another embodiment of the present disclosure, the second pad gate electrode 301 may include a material having a higher work function than the second body gate electrode 302. The second body gate electrode 302 may include a material having a lower resistance than the second pad gate electrode 301. The second pad gate electrode 301 may include a metal nitride or a metal oxide, and the second body gate electrode 302 may include a metal-based material. For example, the second pad gate electrode 301 may include titanium silicon nitride (TiSiN) or aluminum oxide (Al2O3), and the second body gate electrode 302 may include titanium nitride (TiN).
[0044] Reference Figure 6 , the semiconductor device 400 may include a substrate 101 and a buried gate structure 400G embedded in the substrate 101. The semiconductor device 400 may be a part of a memory cell. For example, the semiconductor device 400 may be a part of a DRAM memory cell.
[0045] The buried gate structure 400G may include a gate dielectric layer 106 covering the bottom surface and sidewalls of the trench 105, and a gate electrode structure GE4 and a capping layer 110 sequentially stacked on the gate dielectric layer 106 to fill the trench 105. The gate electrode structure GE4 may include a stacked structure of a first pad gate electrode 201, a first body gate electrode 202, an anti-oxidation layer 108, a second pad gate electrode 301, and a second body gate electrode 302.
[0046] The first pad gate electrode 201 may be a barrier layer that may prevent the material of the first body gate electrode 202 from out-diffusion. The first pad gate electrode 201 may include a metal nitride, and the first body gate electrode 202 may include a metal material. For example, the first pad gate electrode 201 may include titanium nitride, and the first body gate electrode 202 may include tungsten (W) or molybdenum (Mo).
[0047] According to another embodiment of the present disclosure, the first pad gate electrode 201 may include a material with a higher work function than the first body gate electrode 202. The first body gate electrode 202 may include a material with a lower resistance than the first pad gate electrode 201. The first pad gate electrode 201 may include a metal nitride or a metal oxide, and the first body gate electrode 202 may include a metal-based material. For example, the first pad gate electrode 201 may include titanium silicon nitride (TiSiN) or aluminum oxide (Al2O3), and the first body gate electrode 202 may include titanium nitride (TiN).
[0048] The second pad gate electrode 301 may be a barrier layer that may prevent the material of the second body gate electrode 302 from out-diffusion. The second pad gate electrode 301 may include a metal nitride, and the second body gate electrode 302 may include a metal material. For example, the second pad gate electrode 301 may include titanium nitride, and the second body gate electrode 302 may include tungsten (W) or molybdenum (Mo).
[0049] According to another embodiment of the present disclosure, the second pad gate electrode 301 may include a material having a higher work function than the second body gate electrode 302. The second body gate electrode 302 may include a material having a lower resistance than the second pad gate electrode 301. The second pad gate electrode 301 may include a metal nitride or a metal oxide, and the second body gate electrode 302 may include a metal-based material. For example, the second pad gate electrode 301 may include titanium silicon nitride (TiSiN) or aluminum oxide (Al2O3), and the second body gate electrode 302 may include titanium nitride (TiN).
[0050] FIG. 3A to FIG. 3F is a cross-sectional view illustrating a method for manufacturing a semiconductor device according to various embodiments of the present disclosure. FIG. 3A to FIG. 3F Shown for manufacturing Figure 2A An example of a method of a semiconductor device is shown.
[0051] Reference Figure 3A , the isolation layer 12 may be formed in the substrate 11. The active area 13 may be defined by the isolation layer 12. The isolation layer 12 may be formed by a shallow trench isolation (STI) process. For example, the isolation trench 12T may be formed by etching the substrate 11. The isolation layer 12 may be formed by filling the isolation trench 12T with a dielectric material. The isolation layer 12 may include silicon oxide, silicon nitride, or a combination thereof. Chemical vapor deposition (CVD) or other deposition processes may be used to fill the isolation trench 12T with a dielectric material. A planarization process such as chemical mechanical polishing (CMP) may be additionally used.
[0052] A trench 15 may be formed in the substrate 11. The trench 15 may be formed in a line shape intersecting the active region 13 and the isolation layer 12. The trench 15 may be formed by an etching process of the substrate 11 using the hard mask layer 14 as an etching mask. The hard mask layer 14 may be formed on the substrate 11 and may have one or more linear openings. The hard mask layer 14 may be formed of a material having an etching selectivity relative to the substrate 11. The hard mask layer 14 may be silicon oxide, such as tetraethyl orthosilicate (TEOS). The trench 15 may be formed shallower than the isolation trench 12T. The depth of the trench 15 may increase the average cross-sectional area of the subsequent gate electrode. Therefore, the resistance of the gate electrode may be reduced. The bottom edge of the trench 15 according to another embodiment of the present disclosure may have a curvature.
[0053] Subsequently, the fin 13F may be formed. To form the fin 13F, the isolation layer 12 below the trench 15 may be selectively recessed. For the structure of the fin 13F, reference may be made to Figure 2B Fin 103F.
[0054] Subsequently, a gate dielectric layer 16 may be formed on the surface of the trench 15. Before forming the gate dielectric layer 16, etching damage on the surface of the trench 15 may be restored. For example, after forming the sacrificial oxide by thermal oxidation treatment, the sacrificial oxide may be removed. The gate dielectric layer 16 may be formed by a thermal oxidation process. The gate dielectric layer 16 may include silicon oxide. According to another embodiment of the present disclosure, the gate dielectric layer 16 may be formed by chemical vapor deposition (CVD) or atomic layer deposition (ALD). The gate dielectric layer 16 formed by the deposition method may include a high-k material, an oxide, a nitride, an oxynitride, or a combination thereof. The high-k material may include a hafnium-containing material. For example, the hafnium-containing material may include one or more of hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, or a combination thereof. According to another embodiment of the present disclosure, for example, the high-k material may include one or more of lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, silicon zirconium oxide, silicon zirconium oxynitride, aluminum oxide, or a combination thereof. As for the high-k material, other known high-k materials may be selectively used. The gate dielectric layer 16 may include a stack of silicon oxide and a high-k material. Here, the high-k material may include a material in which the amount of oxygen atoms in the same area is higher than that of silicon oxide.
[0055] Reference Figure 3B , a conductive material layer 17A may be formed over the gate dielectric layer 16 and the hard mask layer 14 to gap-fill the trench 15. The conductive material layer 17A may include a metal-based material. The conductive material layer 17A may include, for example, titanium nitride. According to another embodiment of the present disclosure, the conductive material layer 17A may include one or more selected from the group consisting of titanium nitride (TiN), molybdenum (Mo), tantalum nitride (TaN), lanthanum (La), hafnium (Hf), tantalum (Ta), aluminum (Al), aluminum oxide (Al2O3), titanium silicon nitride (TiSiN) and tantalum silicon nitride (TaSiN) or a combination thereof, but the present disclosure is not limited thereto.
[0056] Reference Figure 3C , a first gate electrode 17 filling the bottom of the trench 15 can be formed. The first gate electrode 17 can be formed by performing a recess process on the conductive material layer 17A (see Figure 3B ). The recess process may be performed by a dry etching process (eg, an etch-back process). The etch-back process may be performed using plasma.
[0057] Reference Figure 3D, an anti-oxidation layer 18 may be formed over the first gate electrode 17. The anti-oxidation layer 18 may prevent oxidation of the first gate electrode 17 by collecting oxygen remaining on the surface of the first gate electrode 17 and impurities (eg, oxygen) remaining inside the first gate electrode 17.
[0058] The anti-oxidation layer 18 may be formed by a series of processes including forming a liner of a silicon-containing material (e.g., polysilicon) along the contour of the entire surface including the upper surface of the first gate electrode 17, and then etching the silicon-containing material over the gate dielectric layer 16, so that the anti-oxidation layer 18 may be only partially disposed on the upper surface of the first gate electrode 17. The anti-oxidation layer 18 may be formed by a deposition process.
[0059] Reference Figure 3E , a second gate electrode 19 filling the middle of the trench 15 can be formed on the anti-oxidation layer 18. The second gate electrode 19 can be formed by a series of processes of forming a conductive material on the anti-oxidation layer 18 and the hard mask layer 14, and then removing a portion of the conductive material layer inside the trench 15 via a recess process. The second gate electrode 19 may include the same material as the first gate electrode 17. The second gate electrode 19 may include a metal-based material. The second gate electrode 19 may include, for example, titanium nitride. According to another embodiment of the present disclosure, the conductive material layer 17A may include one or more selected from the group including: titanium nitride (TiN), molybdenum (Mo), tantalum nitride (TaN), lanthanum (La), hafnium (Hf), tantalum (Ta), aluminum (Al), aluminum oxide (Al2O3), titanium silicon nitride (TiSiN) and tantalum silicon nitride (TaSiN) or a combination thereof, but the present disclosure is not limited thereto.
[0060] According to another embodiment of the present disclosure, the anti-oxidation layer 18 and the second gate electrode 19 may be formed by an in-situ process. Before forming the second gate electrode 19, the anti-oxidation layer 18 may be locally formed on the upper surface of the first gate electrode 17 by a treatment process using a silicon-containing source material (eg, SiH4).
[0061] Reference Figure 3F A capping layer 20 may be formed over the second gate electrode 19 to gap-fill the remaining portion of the trench 15. The capping layer 20 may include a dielectric material. For example, the capping layer 20 may include silicon nitride.
[0062] Subsequently, a process of doping impurities may be performed by an implantation technique or other doping techniques. As a result, a first doping region 21 and a second doping region 22 may be formed in the substrate 11. The first doping region 21 and the second doping region 22 may overlap all or part of the second gate electrode 19 in a direction parallel to the surface of the substrate 11. The first gate electrode 17 may not overlap the first doping region 21 and the second doping region 22 in a direction parallel to the surface of the substrate 11. The first doping region 21 and the second doping region 22 may be referred to as a first source / drain region and a second source / drain region, respectively.
[0063] According to one embodiment of the present disclosure, each gate electrode may be prevented from being oxidized by applying an anti-oxidation layer between an upper gate electrode and a lower gate electrode formed of metal electrodes.
[0064] According to one embodiment of the present disclosure, the reliability of a semiconductor device can be ensured.
[0065] Although the present disclosure has been described with respect to specific embodiments, those skilled in the art will recognize that various changes and modifications may be made without departing from the scope of the present disclosure described herein. In addition, these embodiments may be combined to form further embodiments.
Claims
1. A semiconductor device, comprising: a trench formed in the substrate; a gate dielectric layer adapted to cover the bottom surface and sidewalls of the trench; a first gate electrode adapted to gap-fill a bottom portion of the trench above the gate dielectric layer; a second gate electrode formed on the first gate electrode; as well as An anti-oxidation layer is provided at an interface between the first gate electrode and the second gate electrode.
2. The semiconductor device according to claim 1, wherein The anti-oxidation layer includes a stripe shape.
3. The semiconductor device according to claim 1, wherein The anti-oxidation layer has a thickness smaller than a thickness of each of the first gate electrode and the second gate electrode.
4. The semiconductor device according to claim 1, wherein: The anti-oxidation layer prevents diffusion of materials between the first gate electrode and the second gate electrode and has a thickness allowing electrical conduction between the first gate electrode and the second gate electrode.
5. The semiconductor device according to claim 1, wherein The anti-oxidation layer has to Thickness.
6. The semiconductor device according to claim 1, wherein The anti-oxidation layer includes a material that collects oxygen.
7. The semiconductor device according to claim 1, wherein The anti-oxidation layer includes a material containing silicon.
8. The semiconductor device according to claim 1, wherein The anti-oxidation layer includes polysilicon.
9. The semiconductor device according to claim 1, wherein: The first gate electrode and the second gate electrode include a metal material.
10. The semiconductor device according to claim 1, wherein Each of the first gate electrode and the second gate electrode includes titanium nitride.
11. The semiconductor device according to claim 1, wherein Each of the first gate electrode and the second gate electrode includes one or more selected from the following group: titanium nitride TiN, molybdenum Mo, tantalum nitride TaN, lanthanum La, hafnium Hf, tantalum Ta, aluminum Al, aluminum oxide Al2O3, titanium silicon nitride TiSiN and tantalum silicon nitride TaSiN or a combination thereof.
12. The semiconductor device according to claim 1, wherein The first gate electrode includes a stack structure including a first pad gate electrode and a first body gate electrode.
13. The semiconductor device according to claim 12, wherein: The first pad gate electrode comprises metal nitride or metal oxide, and The first body gate electrode includes a metal-based material.
14. The semiconductor device according to claim 1, wherein The second gate electrode includes a stack structure including a second pad gate electrode and a second body gate electrode.
15. The semiconductor device according to claim 14, wherein: The second pad gate electrode includes a metal nitride or a metal oxide, and the second body gate electrode includes a metal-based material.
16. The semiconductor device according to claim 1, further comprising: Source / drain regions are formed in the substrate at both sides of the trench.
17. A method for forming a semiconductor device having a buried gate structure, the method comprising: forming a trench in a substrate; covering the bottom surface and sidewalls of the trench with a gate dielectric layer; gap-filling a bottom portion of the trench over the gate dielectric layer with a first gate electrode; locally disposing an anti-oxidation layer on the first gate electrode; forming a second gate electrode on the anti-oxidation layer and in the trench; forming a capping layer on the second gate electrode and in the trench to complete the buried gate structure; as well as A source-drain region is formed in the substrate adjacent to the trench.
18. The method according to claim 17, wherein: The anti-oxidation layer includes a material that collects oxygen and protects the first gate electrode from being oxidized.
19. The method according to claim 17, wherein: The anti-oxidation layer has a range from to Thickness.
20. The method according to claim 17, wherein: The source-drain region overlaps at least a portion of the second gate electrode in a direction parallel to a surface of the substrate.