OLED panel single-side thinning method
Through the combination of tuffy glue and UV photosensitive film, the problem of OLED panel lacking dummy zone and sealed glue frame after cutting is solved, and the single-sided thinning and corrosion protection of the product is achieved, and the utilization rate and marketing of the product are improved.
Patent Information
- Application Number
- CN202411174591.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-11-12
AI Technical Summary
After the OLED panel is cut into the shape of a panel after production, it lacks dummy zone and closed adhesive frame, which makes it impossible to thin, and is prone to acid corrosion problems, affecting product utilization and marketing promotion.
The terminal area is sealed with tuffy glue, and the pure black PET film and UV photosensitive film are used for covering and cutting. Combined with two sealing processes, it ensures that the product is sprayed and etched with acid without dummy zone to reduce corrosion. risk.
Effectively reduce the corrosion of acid liquid lines, improve product utilization, reduce scrapping, realize single-sided thinning of OLED panels, and ensure product quality and market promotion.
Smart Images

Figure CN118946225A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of OLED, and in particular to a single-side thinning method for an OLED panel. Background Art
[0002] At present, the demand for OLED products is increasing year by year. OLED manufacturers have increased the demand for large panel QC spot checks after the array production process. All original-size large sheets are cut into panel shapes for spot checks and confirmation. Existing single-sided thinning products are only for thinning large sheet products. Large sheet products have edge dummy areas and closed plastic frames, which have technical defects for single-sided thinning of OLED panels. After the spot check, these panels have not undergone the thinning process, resulting in these products being unable to flow into the market normally.
[0003] Since the panel product has been cut, the terminal of this part of the panel is exposed due to product restrictions. The edges after cutting are all effective areas without dummy areas. Therefore, the HF acid thinning easily corrodes the product, and how to protect it becomes a problem. Therefore, it is necessary to propose a solution to solve the above technical problems. Summary of the invention
[0004] The present invention provides a single-sided thinning method for an OLED panel, which effectively solves the problem that the OLED panel cannot be thinned, effectively reduces acid corrosion of the circuit, protects the end surface and reduces corrosion, and can still perform a sealing process without a dummy area, effectively improving the utilization rate of the product and reducing the scrapping of the product.
[0005] In order to achieve the above object, the present invention adopts the following technical solution: a method for thinning a single side of an OLED panel, which specifically comprises the following steps: S1. Use tuffy glue to completely seal the terminal area of the panel product, and use QC inspection to confirm the product after sealing to ensure the airtightness of the terminal; S2, then use pure black PET film to cover part of the AA area of the TP surface; S3, then use UV photosensitive film to cover the non-thinned surface. When cutting the film, the UV photosensitive film should be 1-2mm larger than the galss edge; S4, then use tuffy glue to seal and cure the end face and sealing interface; S5. Attach the product to the etched back plate and spray it with acid; S6. After etching is completed, the UV photosensitive film and tuffy glue on the non-thinned surface are removed; S7. After the inspection is completed, the goods can be shipped normally.
[0006] Preferably, in step S1, when Tuffy glue is used to seal the OLED panel terminal, the height of the Tuffy glue is flush with the TP surface.
[0007] Preferably, in step S3, after the UV photosensitive film is coated, cutting is performed along the edge of the panel. During this process, it is necessary to avoid light and can be stored under yellow light.
[0008] Preferably, in step S1 and step S4, after sealing with tuffy glue, it needs to be left to stand for 3 hours to solidify.
[0009] Preferably, in step S5, the product is attached to the etched back plate by using a non-adhesive tape to attach and fix it through the hollow holes of the back plate, and the attachment requirement is that it must be attached along the first hole.
[0010] Preferably, in step S6, UV light irradiation is added before tearing the film; the viscosity of the UV photosensitive film before irradiation is greater than 1600g / 25mm, and the viscosity of the UV photosensitive film after irradiation is less than 10g / 25mm.
[0011] Preferably, in step S6, the light integrated amount of UV light is controlled at: 3000mj / cm².
[0012] Compared with the prior art, the present invention has the following beneficial effects: The present invention optimizes the design of the single-sided thinning process of the OLED panel, uses tuffy glue to protect the terminals, reserves a certain area for sealing when cutting after UV photosensitive film lamination, and finally uses tuffy glue for secondary sealing to complete the final sealing. In this process, the operation and specific parameters of each process flow are strictly controlled, thereby realizing the single-sided thinning method of the OLED panel, effectively improving the utilization rate of the product and reducing the scrapping of the product.
[0013] The present invention adopts the method of tuffy glue + UV photosensitive film + tuffy glue to achieve single-sided thinning of the product, and performs a single-sided thinning process on the OLED panel, effectively solving the problem that the OLED panel cannot be thinned. The acid corrosion circuit is effectively reduced by sealing twice, and the end face is protected to reduce corrosion. The sealing process can still be performed without a dummy area. The overall design is ingenious and practical. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 The present invention is a schematic flow chart of a method for thinning a single side of an OLED panel. DETAILED DESCRIPTION
[0015] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0016] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0017] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed", "provided with", etc. should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be internal communication between two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0018] Reference is now made to the accompanying drawings, wherein the purpose of each illustration is only to show certain exemplary embodiments and is not intended to limit the present invention. In each of the drawings, the same reference numerals represent the same or corresponding parts. The dimensions and proportions in each of the drawings are also only for illustration and should not be interpreted as limiting the present invention, and these dimensions may be exaggerated relative to the actual product. Example
[0019] A single-side thinning method for an OLED panel according to this embodiment specifically includes the following steps: S1. After the panel product incoming material inspection is completed, tuffy glue is used to completely seal the terminal area of the panel product. Tuffy glue has strong adhesion and no residual glue is left after tearing it off, and it has no effect on the metal wiring of the terminal. Use QC inspection to inspect and confirm the product after sealing to confirm that all the terminals are covered to ensure the airtightness of the terminals.
[0020] S2. Use pure black PET film to cover part of the AA area of the TP surface; it is convenient to tear off the film completely, and the adhesive of the pure black PET film does not contact the middle area; the pure black PET film can protect the other non-thinned surface to prevent etching erosion.
[0021] S3. Then use UV photosensitive film to cover the non-thinned surface; when cutting the film, the UV photosensitive film should be 1-2mm larger than the galss edge, that is, when cutting the film, a 1-2mm distance should be reserved at the edge of the UV photosensitive film to provide a tuffy glue sealing position.
[0022] S4, then use tuffy glue to seal and cure the end face and sealing interface; S5. Attach the product to the etching backplane and spray acid. The backplane carrier plays a role in fixing the product during the acid etching process.
[0023] S6. After etching is completed, the UV photosensitive film and tuffy glue on the non-thinned surface are removed; S7. After the inspection is completed, the goods can be shipped normally.
[0024] Specifically, in step S1, when Tuffy glue is used to seal the OLED panel terminal, the height of the Tuffy glue must be flush with the TP surface. In step S1 and step S4, after the Tuffy glue is used for sealing, it needs to be left to stand for 3 hours to solidify. The end face and the sealing interface are sealed and solidified again with Tuffy glue to prevent acid from corroding the Tuffy glue at the terminal sealing point and provide protection for the TP surface terminal from leakage.
[0025] In step S3, after the UV photosensitive film is coated, cutting is performed along the edge of the panel. During this process, light protection is required and yellow light can be used for preservation.
[0026] In step S5, the product is attached to the etching backplane by using a non-adhesive tape to attach and fix it through the hollow holes of the backplane. The attachment requirement must be along the first hole to avoid top-spray etching and allow the acid to flow away from the first hole. The backplane needs to be attached before the product is etched, mainly to ensure that the glass is fixed during the etching process and to avoid impact and shaking.
[0027] It is worth noting that in step S6, UV light irradiation is added before film tearing, and the light volume of UV light irradiation is controlled at: 3000mj / cm². This light irradiation is to reduce the viscosity of the UV photosensitive film. The UV photosensitive film is very sticky before the light irradiation. The viscosity of the UV photosensitive film before the light irradiation is greater than 1600g / 25mm, and the viscosity of the UV photosensitive film after the light irradiation is less than 10g / 25mm. There is no obvious stickiness after the light irradiation.
[0028] The pure black PET film contacts the AA area of the TP surface, mainly protecting the non-etched area from being etched by acid during the etching process; the UV photosensitive film covers the non-thinned surface of the TP, and the edge of the UV photosensitive film reserves 1-2mm distance to provide a tuffy glue sealing position. The etching backplane contacts the UV photosensitive film on the TP surface, and the acid-proof tape is attached and connected to the hollow holes on the etching carrier. Since the internal results of oled products are mainly diodes and other photosensitive equipment, in order to avoid the influence of UV light on the product box after etching, a pure black PET film must be used to avoid light.
[0029] The present invention mainly solves the OLED panel thinning method. After the product has been cut, the terminal (metal wire body) leaks out and there is no dummy area. When the product is thinned, corrosion is avoided, and unnecessary scrap and loss of such products are reduced. To this end, the present invention optimizes the design of the single-sided thinning process of the OLED panel, by using tuffy glue to protect the terminal, and reserving a certain area to provide a sealing position when cutting after UV photosensitive film coating, and finally using tuffy glue for secondary sealing to complete the final sealing, and in this process, the operation and specific parameters of each process flow are strictly controlled, so as to realize the single-sided thinning method of the OLED panel, effectively improve the utilization rate of the product, and reduce the scrapping of the product. The present invention adopts this tuffy glue + UV photosensitive film + tuffy glue method to achieve single-sided thinning of the product, and performs a single-sided thinning process on the OLED panel, effectively solving the problem that the OLED panel cannot be thinned, and effectively reduces the acid corrosion circuit situation through two times of sealing, and protects the end face to reduce corrosion. The sealing process can still be performed without a dummy area.
[0030] The above-described embodiments only express a certain implementation mode of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.
Claims
1. A method for thinning a single side of an OLED panel, characterized in that: The following steps are involved: S1. Use tuffy glue to completely seal the terminal area of the panel product, and use QC inspection to confirm the product after sealing to ensure the airtightness of the terminal; S2. Use pure black PET film to cover part of the AA area of the TP surface; S3. Then use UV photosensitive film to cover the non-thinned surface. When cutting the film, the UV photosensitive film should be 1-2mm larger than the galss edge. S4. Then, tuffy glue is used to seal and cure the end face and sealing interface; S5. Attach the product to the etched backboard and spray it with acid; S6. After etching is completed, the UV photosensitive film and tuffy glue on the non-thinned surface are removed; S7. After the inspection is completed, the goods can be shipped normally.
2. The method for thinning a single side of an OLED panel according to claim 1, wherein: In step S1, when Tuffy glue is used to seal the OLED panel terminals, the height of the Tuffy glue is flush with the TP surface.
3. The method for thinning a single side of an OLED panel according to claim 1, wherein: In step S3, after the UV photosensitive film is coated, cutting is performed along the edge of the panel. During this process, light protection is required and yellow light can be used for storage.
4. The method for thinning a single side of an OLED panel according to claim 1, wherein: In step S1 and step S4, after sealing with tuffy glue, it needs to be left to stand for 3 hours to solidify.
5. The method for thinning a single side of an OLED panel according to claim 1, wherein: In step S5, the product is attached to the etched back plate by using a non-adhesive tape to attach and fix it through the hollow holes of the back plate. The attachment requirement is that the product must be attached along the first hole.
6. The method for thinning a single side of an OLED panel according to claim 1, wherein: In step S6, UV light irradiation is added before tearing the film; the viscosity of the UV photosensitive film before irradiation is greater than 1600 g / 25 mm, and the viscosity of the UV photosensitive film after irradiation is less than 10 g / 25 mm.
7. The method for thinning a single side of an OLED panel according to claim 6, wherein: In step S6, the integrated light intensity of the UV light is controlled at 3000 mj / cm².
Citation Information
Cited By
Hybrid OLED (Organic Light Emitting Diode) single-side thinning method based on photosensitive film and black PET (Polyethylene Terephthalate) film
CN120344119A